Electrolytic capacitor element and method for producing same
By incorporating additional insulating materials wound around the electrolytic capacitor elements to cover the connection terminals and separators, the issue of separator damage from misalignment is addressed, enhancing the capacitor's quality and reducing short-circuit risks through improved alignment and tensile strength.
Patent Information
- Application Number
- PCT/JP2024/015003
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-12
- Filing Date
- 2024-04-15
- Publication Date
- 2024-11-21
AI Technical Summary
In the manufacturing of electrolytic capacitor elements, misalignment during the winding process can lead to damage of the separator by lead-out terminals, resulting in quality deterioration such as short-circuiting, due to inadequate coverage with insulating paper.
The use of additional insulating materials wound around the wound body to cover the connection terminals and separators, ensuring that the length of these insulating materials is at least three times the distance between the terminals, and possibly containing fibers, to enhance protection and prevent misalignment.
This solution effectively suppresses the risk of separator damage and quality deterioration by increasing the tensile strength of the separators and improving alignment during the winding process, thereby reducing short-circuit defects and ensuring better capacitor performance.
Smart Images

Figure JP2024015003_21112024_PF_FP_ABST
Abstract
Description
Electrolytic capacitor element and its manufacturing method
[0001] The present invention relates to an electrolytic capacitor element and a method for manufacturing the same.
[0002] For example, in an electrolytic capacitor element, a technique is known in which the connection portions between the wound anode foil and cathode foil and a pair of lead terminals are covered with insulating paper to prevent the separator between the anode foil and cathode foil from being damaged by the lead terminals (see, for example, Patent Documents 1 and 2).
[0003] JP 2006-286959 A JP 2022-40754 A
[0004] For example, in the manufacture of electrolytic capacitor elements, when winding an anode foil and a cathode foil with a separator interposed therebetween, insulating paper is placed on the separator so as to cover the connection portions between the anode foil and the cathode foil and a pair of lead terminals. However, misalignment may occur due to various factors such as the precision of the manufacturing equipment or vibration. If the connection portions are not properly covered with insulating paper due to misalignment, the separator may be damaged by the lead terminals, which may result in quality degradation such as short circuits.
[0005] The present invention has been made in view of the above-mentioned problems, and has an object to provide an electrolytic capacitor element capable of suppressing deterioration in quality, and a method for manufacturing the same.
[0006] The electrolytic capacitor element of the present invention is characterized by comprising: a wound body in which an anode foil and a cathode foil are wound with a first separator and a second separator on opposite sides of each other; an anode connection terminal connected to a first position of the anode foil; a cathode connection terminal connected to a second position of the cathode foil; a first insulating material wound within the wound body so as to face the first position and the second position on the first separator; and a second insulating material wound within the wound body so as to face the first position and the second position on the second separator, and disposed on the opposite side of the first insulating material with the anode foil and the cathode foil sandwiched therebetween.
[0007] In the electrolytic capacitor element, the length of at least one of the first insulating material and the second insulating material in the winding direction may be three times or more the distance between the anode connecting terminal and the cathode connecting terminal.
[0008] In the electrolytic capacitor element, the length of at least one of the first insulating material and the second insulating material in the winding direction may be 10 times or less the distance between the anode connecting terminal and the cathode connecting terminal.
[0009] In the electrolytic capacitor element, at least one of the first insulating material and the second insulating material may contain fibers.
[0010] In the above electrolytic capacitor element, the anode connection terminal and the cathode connection terminal may have burrs at the ends where they penetrate the anode foil and the cathode foil, respectively, and be crimp-connected to the anode foil and the cathode foil by the burrs, and at least one of the first insulating material and the second insulating material may cover the burrs of at least one of the anode foil and the cathode foil.
[0011] In the electrolytic capacitor element described above, the first insulating material may be attached to the first separator.
[0012] In the electrolytic capacitor element described above, the second insulating material may be attached to the second separator.
[0013] The method for manufacturing an electrolytic capacitor element of the present invention includes the steps of: connecting an anode connecting terminal to a first position of an anode foil; and connecting a cathode connecting terminal to a second position of a cathode foil; and winding the anode foil and the cathode foil with a first separator and a second separator on opposite sides thereof to form a wound body, wherein in the step of forming the wound body, a first insulating material is wound within the wound body so as to face the first position and the second position on the first separator; and a second insulating material is wound within the wound body on the opposite side of the first insulating material, sandwiching the anode foil and the cathode foil, so as to face the first position and the second position on the second separator.
[0014] According to the present invention, deterioration in the quality of electrolytic capacitor elements can be suppressed.
[0015] FIG. 1 is a side view showing an example of an aluminum electrolytic capacitor. FIG. 2 is a perspective view showing an example of an electrolytic capacitor element. FIG. 3 is a schematic cross-sectional view showing an example of the winding structure of a wound body taken along line A-A in FIG. 2. FIG. 4 is a cross-sectional view showing an example of the winding structure near the battledore portion. FIG. 5a is a front view of the outer surface of an anode foil unfolded in the winding direction. FIG. 5a is a front view of the outer surface of a cathode foil unfolded in the winding direction. FIG. 6a is a front view of the inner surface of an anode foil unfolded in the winding direction. FIG. 6b is a front view of the inner surface of a cathode foil unfolded in the winding direction. FIG. 7a is a front view of the outer surface of an anode foil when insulating sheets are individually placed at the positions of the anode foil and the cathode foil. FIG. 7b is a front view of the outer surface of a cathode foil when insulating sheets are individually placed at the positions of the anode foil and the cathode foil. FIG. 8 is a flowchart showing an example of a manufacturing process for an aluminum electrolytic capacitor. FIG. 9 is a diagram showing an example of the schematic configuration of a winding device that produces a wound body. FIG. 10 is a diagram showing another example of the schematic configuration of a winding device for producing a wound body.
[0016] [Embodiment] (Configuration of Aluminum Electrolytic Capacitor) Fig. 1 is a side view showing an example of an aluminum electrolytic capacitor 1. In Fig. 1, a cross section of the interior of the aluminum electrolytic capacitor 1 is shown in the right half across the center line Lc of the aluminum electrolytic capacitor 1.
[0017] The aluminum electrolytic capacitor 1 is an example of an electrolytic capacitor, specifically a conductive polymer hybrid aluminum electrolytic capacitor. The aluminum electrolytic capacitor 1 is mounted on an electronic circuit board and used for coupling, decoupling, smoothing, and the like.
[0018] The aluminum electrolytic capacitor 1 has an electrolytic capacitor element 10, a case 11, a sealing body 12, a seat plate 13, a pair of battledore portions 112, a pair of round bar portions 111, and a pair of lead portions 110. The battledore portions 112, the round bar portions 111, and the lead portions 110 are extraction electrodes of the electrolytic capacitor element 10, with the round bar portions 111 extending from the tip of the battledore portion 112 and the lead portions 110 extending from the tip of the round bar portions 111. Note that while only one of the battledore portions 112 and round bar portions 111 is shown in Figure 1, the other battledore portion 112 and round bar portion 111 are provided in a symmetrical position across the center line L.
[0019] Case 11 is made of aluminum and has a cylindrical shape with a closed upper opening. Case 11 covers electrolytic capacitor element 10 and sealing body 12 and functions as an exterior of aluminum electrolytic capacitor 1. The shape of case 11 is not limited to a cylindrical shape and may be a rectangular tube shape.
[0020] Sealing body 12 is a generally cylindrical member made of an elastic material such as butyl rubber, etc. Sealing body 12 is adjacent to electrolytic capacitor element 10 and seals the opening at the bottom of case 11.
[0021] As will be described later, the electrolytic capacitor element 10 has a configuration in which an anode foil, a cathode foil, and a separator (electrolytic paper) are stacked and wound together. A pair of battledore parts 112 are disposed inside the electrolytic capacitor element 10, and a pair of round rod parts 111 extend from the bottom of the electrolytic capacitor element 10.
[0022] The battledore portion 112, the round bar portion 111, and the lead portion 110 are made of aluminum or the like. The pair of battledore portions 112 are crimped to the anode foil and the cathode foil, respectively, and function as the anode terminal and the cathode terminal of the aluminum electrolytic capacitor 1. Each round bar portion 111 is inserted into a pair of through holes 120 formed in the sealing body 12. Note that while only one of the through holes 120 is shown in FIG. 1 , the other through hole 120 is provided at a symmetrical position across the center line L.
[0023] The lead portion 110 has a flat plate shape and is bent into an L shape, with its tip portion extending along the surface of the base plate 13. The portion of the lead portion 110 on the round bar portion 111 side is inserted into a through hole 130 in the base plate 13. The lead portion 110 is soldered to a pad on the electronic circuit board during the reflow process of the electronic circuit board.
[0024] The seat plate 13 is a plate-like member made of resin or the like, and is provided below the case 11 and the sealing member 12. The seat plate 13 supports the case 11 and the sealing member 12 relative to the electronic circuit board on which they are mounted. The seat plate 13 is provided with through holes 130 for the lead portions 110 and grooves 131 for accommodating the bent tip portions of the lead portions 110. The grooves 131 extend outward from near the center along the bottom surface of the seat plate 13. The bottom surface of the seat plate 13 serves as the mounting surface for the aluminum electrolytic capacitor 1 on the electronic circuit board, allowing the plate-like lead portions 110 to be soldered to pads on the electronic circuit board. Note that while this embodiment describes a surface-mount type aluminum electrolytic capacitor 1, the examples described below can also be applied to lead types that do not have the seat plate 13.
[0025] (Configuration of Electrolytic Capacitor Element) Fig. 2 is a perspective view showing an example of an electrolytic capacitor element 10. In Fig. 2, components common to those in Fig. 1 are assigned the same reference numerals, and their description will be omitted. Note that Fig. 2 shows a state before the lead portion 110 is bent. The electrolytic capacitor element 10 has a wound body 100 formed by winding an anode foil 101, a cathode foil 102, and separators (electrolytic paper) 103, 104, and a pair of lead electrodes 19a, 19b connected to the anode foil 101 and the cathode foil 102. The lead electrode 19a is an anode terminal, and the lead electrode 19b is a cathode terminal.
[0026] The anode foil 101 and the cathode foil 102 are formed from valve metal foils, such as aluminum, tantalum, titanium, and niobium, and alloys thereof, as well as vapor-deposited foils. The surface of the anode foil 101 is etched to increase the electrode area. This ensures that the electrolytic capacitor element 10 has a predetermined capacitance. Furthermore, an extremely thin oxide film is formed on the surface of the anode foil 101. This insulates the anode foil 101 from other components. The oxide film functions as a dielectric, allowing the electrolytic capacitor element 10 to function as a capacitor. The thickness of the anode foil 101 is, for example, 5 to 200 μm. This thickness range is preferable because it achieves an appropriate balance between the strength of the anode foil 101 and the amount of capacitance it generates.
[0027] On the other hand, no oxide film is formed on the surface of the cathode foil 102. The surface of the cathode foil 102 may also be subjected to an etching treatment. Furthermore, the surface of the cathode foil 102 may have an oxide film formed thereon, or an inorganic layer or a carbon layer formed thereon.
[0028] The separators 103 and 104 are wound while being sandwiched between the anode foil 101 and the cathode foil 102. The separators 103 and 104 are made of at least one material selected from cellulose, rayon, glass fiber, and the like. The wound body 100 is a substantially cylindrical element formed by winding the anode foil 101, the cathode foil 102, and the separators 103 and 104. In this embodiment, the height direction of the electrolytic capacitor element 10 is defined along the height of this substantially cylindrical shape. The pair of extraction electrodes 19a and 19b extend downward from the wound body 100 in the height direction. The height direction substantially coincides with the direction in which the round bar portions 111 of each extraction electrode 19a and 19b extend.
[0029] The wound body 100 is immersed in a dispersion or solution of an electrolytic solution and a conductive polymer during the manufacturing process of the aluminum electrolytic capacitor 1. This allows the electrolytic solution and the conductive polymer layer to be held in the separators 103, 104. The thickness of the separators 103, 104 is, for example, 1 to 100 μm. This thickness range is preferable because it maintains a good balance between the strength, insulating properties, porosity, and conductive material of the separators 103, 104.
[0030] The electrolyte solution may contain polyhydric alcohols, sulfone compounds, lactone compounds, carbonate compounds, diether compounds of polyhydric alcohols, monohydric alcohols, etc. These may be used alone or in combination of two or more.
[0031] The polyhydric alcohol preferably contains at least one of ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, butanediol, polyalkylene glycol, and glycerin. As the polyalkylene glycol, it is preferable to use polyethylene glycol having an average molecular weight of 200 to 1,000 or polypropylene glycol having an average molecular weight of 200 to 5,000.
[0032] Examples of lactone compounds that can be used include γ-butyrolactone and γ-valerolactone. Examples of carbonate compounds that can be used include dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate, ethylene carbonate, propylene carbonate, and fluoroethylene carbonate as a solvent. It is particularly desirable to use ethylene glycol, polyalkylene glycol, γ-butyrolactone, and sulfolane.
[0033] The electrolyte may contain a solute, such as an acid component, a base component, a salt of an acid component and a base component, a nitro compound, or a phenol compound.
[0034] The acid component may be an organic acid, an inorganic acid, or a composite compound of an organic acid and an inorganic acid. Examples of the organic acid include carboxylic acids such as phthalic acid, isophthalic acid, terephthalic acid, maleic acid, succinic acid, glutaric acid, adipic acid, benzoic acid, 4-hydroxybenzoic acid, 1,6-decanedicarboxylic acid, 1,7-octanedicarboxylic acid, and azelaic acid. Examples of the inorganic acid include boric acid, phosphoric acid, phosphorous acid, hypophosphorous acid, phosphate esters, and phosphate diesters.
[0035] Examples of the composite compound of an organic acid and an inorganic acid that can be used include borodisalicylic acid, borodisalic acid, and borodiglycolic acid.
[0036] The base component may be a primary to tertiary amine, a quaternary ammonium, a quaternized amidinium, or the like. Examples of the primary to tertiary amine that may be used include methylamine, dimethylamine, trimethylamine, ethylamine, diethylamine, triethylamine, ethylenediamine, N,N-diisopropylethylamine, tetramethylethylenediamine, hexamethylenediamine, and aniline. Examples of the quaternary ammonium that may be used include tetramethylammonium, triethylmethylammonium, and tetraethylammonium. Examples of the quaternized amidinium that may be used include ethyldimethylimidazolinium and tetramethylimidazolinium.
[0037] The conductive polymer is not particularly limited as long as it is a polymer having conductivity. For example, at least one polymer selected from the group consisting of polythiophene, polypyrrole, polyaniline, and derivatives thereof is used as the conductive polymer. Generally, polyethylenedioxythiophene (PEDOT) having at least one acid selected from the group consisting of p-toluenesulfonic acid, polystyrenesulfonic acid (PSS), etc. as a dopant is used as the conductive polymer.
[0038] (Winding structure) Figure 3 is a schematic cross-sectional view showing an example of the winding structure of the wound body 100 taken along line A-A in Figure 2. In Figure 3, components common to Figure 2 are given the same reference numerals, and their description will be omitted. Figure 3 partially shows the anode foil 101, cathode foil 102, and separators 103 and 104 wound around a substantially cylindrical winding core Ax. In the following description, the battledore 112 on the anode terminal side will be referred to as battledore 112a, and the battledore 112 on the cathode terminal side will be referred to as battledore 112b. The battledore 112a is an example of an anode connection terminal, and the battledore 112b is an example of a cathode connection terminal.
[0039] The anode foil 101 and the cathode foil 102 are wound with separators 103 and 104 on opposite sides of each other. The separators 103 and 104 are wound on opposite sides of the anode foil 101 and the cathode foil 102. The separator 103 is an example of a first separator, and the separator 104 is an example of a second separator.
[0040] The battledore 112a is crimped to position Pa on the anode foil 101, and the battledore 112b is crimped to position Pb on the cathode foil 102. Positions Pa and Pb are symmetrically positioned with respect to the winding core Ax, for example. The distance La between the battledore 112a and 112b is determined based on the design of the aluminum electrolytic capacitor 1. The plate surfaces of the battledore 112a and 112b face the outside of the electrolytic capacitor element 10 when viewed from the winding core Ax.
[0041] Battledore 112a is provided on the outer surface of anode foil 101 and is crimped to the inner surface of anode foil 101. Battledore 112b is provided on the outer surface of cathode foil 102 and is crimped to the inner surface of cathode foil 102. Separator 103 is disposed between the outer surface of anode foil 101 and the inner surface of cathode foil 102, and separator 104 is disposed between the inner surface of anode foil 101 and the outer surface of cathode foil 102.
[0042] Therefore, separator 103 faces the plate surface of battledore portion 112a and the crimped connection portion of battledore portion 112b. Separator 104 faces the plate surface of battledore portion 112b and the crimped connection portion of battledore portion 112a. Therefore, when an external force is applied to battledore portions 112a and 112b during the manufacturing process of aluminum electrolytic capacitor 1, the thinner separators 103 and 104 are, the more likely they are to be damaged at the contact portions between battledore portions 112a and 112b and the crimped connection portions on their back surfaces.
[0043] Therefore, insulating sheets 5a and 5b are wound within wound body 100 so as to face position Pa of anode foil 101 and position Pb of cathode foil 102 on separators 103 and 104, respectively. As a result, the tensile strength of separators 103 and 104 is increased compared to when insulating sheets 5a and 5b are not present, and damage to separators 103 and 104 can be suppressed even if pressure is applied to separators 103 and 104 from battledore portions 112a and 112b and the crimped connections on their back surfaces. Insulating sheet 5a is an example of a first insulating material, and insulating sheet 5b is an example of a second insulating material.
[0044] For example, the insulating sheet 5a is disposed between the separator 103 and the cathode foil 102, and the insulating sheet 5b is disposed between the separator 104 and the anode foil 101. The insulating sheets 5a and 5b contain, for example, the same fibers as those of the separators 103 and 104, or a nonwoven fabric made of a mixture of two or more fibers, so as to be able to hold a sufficient amount of electrolyte and conductive polymer. The thickness of the insulating sheets 5a and 5b is, for example, 30 (μm) or more, and the density of the insulating sheets 5a and 5b is, for example, 0.4 (g / cm 3 )
[0045] Fig. 4 is a cross-sectional view showing an example of the winding structure near the battledore 112a. Specifically, Fig. 4 shows an enlarged view of the vicinity of the battledore 112a in Fig. 2. In this example, one of the battledores 112a is shown, but the vicinity of the other battledore 112b also has a similar winding structure.
[0046] An opening H is provided in the widthwise central portion of the battledore 112a, penetrating the entire anode foil 101 in the thickness direction. The opening H is formed by penetrating needle-shaped members 8 through multiple points in the battledore 112a when the battledore 112a is crimped to position Pa on the anode foil 101 (see arrows D). As a result, burrs B of the battledore 112a are formed on the opposite surface of the anode foil 101 due to the penetration of the needle-shaped members 8. The burrs B are pushed outward from the opening H so as to sandwich the anode foil 101 between the battledore 112a and the battledore 112a.
[0047] In this way, battledore portion 112a is crimped and connected to anode foil 101 by burrs B at the end of the battledore portion that penetrates anode foil 101. Similarly, the other battledore portion 112b is crimped and connected to cathode foil 102 by burrs at the end of the battledore portion that penetrates cathode foil 102.
[0048] The battledore portion 112a is covered with the insulating sheet 5a, and the burr B is covered with the insulating sheet 5b. The insulating sheet 5a overlaps the separator 103, and the insulating sheet 5b overlaps the separator 104. This improves the tensile strength of the separators 103 and 104. Therefore, for example, the risk that the corner E1 of the plate surface of the battledore portion 112a will damage the separator 103 is reduced, and the risk that the tip E2 of the burr B will damage the separator 104 is reduced.
[0049] In this example, the insulating sheet 5a covers the battledore portion 112a via the separator 103, and the insulating sheet 5b directly covers the burr B, but this is not limiting. Even if the insulating sheet 5a directly covers the battledore portion 112a and the insulating sheet 5b covers the burr B via the separator 104, the tensile strength of the separators 103 and 104 is similarly improved. However, from the perspective of preventing the burr B from breaking through the separators 103 and 104, it is preferable that the insulating sheets 5a and 5b directly abut the burr B.
[0050] 5a and 5b are front views of the outer surfaces 101a and 102a of the anode foil 101 and the cathode foil 102, respectively, unfolded in the winding direction. Figures 5a and 5b show the anode foil 101 and the cathode foil 102, respectively, when the battledore portions 112a and 112b are viewed along the arrows V1a and V1b in Figure 3. The battledore portion 112a is connected to the outer surface 101a of the anode foil 101, and the battledore portion 112b is connected to the outer surface 102a of the cathode foil 102.
[0051] 6a and 6b are front views of the inner surfaces 101b and 102b of the anode foil 101 and the cathode foil 102, respectively, unfolded in the winding direction. Figures 6a and 6b show the anode foil 101 and the cathode foil 102, respectively, when the burrs B on the backsides of the battledore portions 112a and 112b are viewed along the arrows V2a and V2b in Figure 3. The burr B of the battledore portion 112a is provided on the inner surface 101b of the anode foil 101, and the burr B of the battledore portion 112b is provided on the inner surface 102b of the cathode foil 102.
[0052] 5a, 5b, 6a, and 6b mainly show the overlapping areas of anode foil 101 and cathode foil 102 with one insulating sheet 5a, and the other insulating sheet 5b is omitted. 5a, 5b, 6a, and 6b also show anode foil 101 and cathode foil 102 with the insulating sheets 5a aligned in the winding direction (horizontal direction on the page).
[0053] Insulating sheets 5a and 5b are provided for each separator 103 and 104. The length Lb of insulating sheets 5a and 5b in the winding direction is set so that, when wound, they overlap the area between position Pa of anode foil 101 and position Pb of cathode foil 102. Therefore, insulating sheet 5a faces positions Pa and Pb on separator 103, respectively, and can cover burrs B of battledore portion 112a and battledore portion 112b. Insulating sheet 5b faces positions Pa and Pb on separator 104, respectively, and can cover burrs B of battledore portion 112b and battledore portion 112a.
[0054] Therefore, insulating sheets 5a, 5b suppress damage to separators 103, 104 caused by shuttlecock portions 112a, 112b and their burrs B, and also ensure length Lb spanning positions Pa, Pb where shuttlecock portions 112a, 112b are provided. Therefore, insulating sheets 5a, 5b have a larger contact area with separators 103, 104 than if they were individually disposed at position Pa of anode foil 101 and position Pb of cathode foil 102, and are therefore less likely to become misaligned when wound in the manufacturing process of aluminum electrolytic capacitor 1.
[0055] 7a and 7b are front views of the outer surfaces of anode foil 101 and cathode foil 102, respectively, when insulating sheets 6a, 6b, 7a, and 7b are individually arranged at position Pa of anode foil 101 and position Pb of cathode foil 102. In Figures 7a and 7b, components common to Figures 5a and 5b are denoted by the same reference numerals, and descriptions thereof will be omitted.
[0056] The insulating sheets 6a, 6b, 7a, and 7b are made of the same insulating material as the insulating sheets 5a and 5b. The insulating sheet 6a covers the battledore portion 112a on the separator 103, and the insulating sheet 6b covers a burr (not shown) on the back side of the battledore portion 112a on the separator 104. The insulating sheet 7a covers the battledore portion 112b on the separator 104, and the insulating sheet 7b covers a burr (not shown) on the back side of the battledore portion 112b on the separator 103.
[0057] The insulating sheet 6a covers only one battledore 112a on the anode foil 101, and does not cover the other battledore 112b on the cathode foil 102. Therefore, the insulating sheet 6a only has a length Lb in the winding direction that faces only the area near position Pa of the anode foil 101. Similarly, the insulating sheet 7a covers only one battledore 112b on the cathode foil 102, and does not cover the other battledore 112a on the anode foil 101. Therefore, the insulating sheet 6b only has a length Lb in the winding direction that faces only the area near position Pb of the cathode foil 102. Similarly, the insulating sheets 6b and 7b also only have a length Lb that faces only the areas near positions Pa and Pb.
[0058] As such, the length Lb of the insulating sheets 6a, 6b, 7a, and 7b is shorter than the length Lb of the insulating sheets 5a and 5b in the embodiment, so the contact area with the separators 103 and 104 is small, and they are prone to misalignment when wound during the manufacturing process of the aluminum electrolytic capacitor 1.
[0059] In contrast, the insulating sheets 5a and 5b of the embodiment each have a length Lb that allows them to face both positions Pa and Pb in the wound body 100, thereby not only improving the tensile strength of the separators 103 and 104 but also suppressing misalignment. Therefore, damage to the separators 103 and 104 is suppressed, and deterioration in the quality of the electrolytic capacitor element 10 is suppressed.
[0060] It is preferable that the length Lb of the insulating sheets 5a, 5b in the winding direction be three times or more the distance La between the battledores 112a, 112b, because this significantly reduces short-circuit defects compared to the case where individual insulating sheets 6a, 6b are provided as shown in Figures 7a and 7b. Also, it is preferable that the length Lb of the insulating sheets 5a, 5b in the winding direction be ten times or less the distance La between the battledores 112a, 112b, because this allows the diameter of the wound body 100 to be kept to an appropriate size, making it easy to house the electrolytic capacitor element 10 in the case 11 and seal it with the sealing body 12.
[0061] In this embodiment, the battledores 112a and 112b are disposed on the outer surfaces 101a and 102a of the anode foil 101 and the cathode foil 102, respectively, but are not limited to this and may be disposed on the inner surfaces 101b and 102b. Therefore, the insulating sheets 5a and 5b can cover any two of the battledore 112a and the burrs B on its back side, and the battledore 112b and the burrs B on its back side. For example, the insulating sheet 5a may cover the battledore 112b and the burrs B on its back side, and the insulating sheet 5b may cover the battledore 112a and the burrs B on its back side.
[0062] The insulating sheets 5 a, 5 b may have the same length or different lengths. For example, by making the insulating sheet 5 b on one separator 104 about 1.1 times longer than the insulating sheet 5 a on the other separator 103, it is possible to improve the winding accuracy of the wound body 100.
[0063] (Method for Manufacturing Aluminum Electrolytic Capacitor) Next, a method for manufacturing the aluminum electrolytic capacitor 1 will be described.
[0064] 8 is a flowchart showing an example of a manufacturing process for the aluminum electrolytic capacitor 1. In manufacturing the aluminum electrolytic capacitor 1, anode foil 101, cathode foil 102, separators 103 and 104, insulating sheets 5a and 5b, and the like are prepared.
[0065] For example, the thickness of the anode foil 101 is 5 to 200 μm, and the thickness of the separator is 1 to 100 μm. The thickness of the insulating sheets 5a and 5b is 30 μm. Pits are formed on the surfaces of the anode foil 101 and the cathode foil 102 by etching. The anode foil 101 is subjected to a chemical conversion treatment, and a dielectric layer of an oxide film is formed on the etched surface.
[0066] First, the lead electrode 19a is crimped to the anode foil 101 at position Pa, and the lead electrode 19b is crimped to the cathode foil 102 at position Pb (step St1). Next, the anode foil 101, separator 103, cathode foil 102, and separator 104 are stacked in this order, wound, and the outer surfaces are secured with a winding tape to produce the wound body 100 (step St2). The anode foil 101 and cathode foil 102 are wound with the separators 103 and 104 interposed between them, and the separators 103 and 104 are wound on opposite sides of the anode foil 101 and cathode foil 102. This produces the electrolytic capacitor element 10 before it is immersed in the conductive polymer solution and the electrolyte solution.
[0067] In the process of producing wound body 100, insulating sheet 5a is wound around wound body 100 so as to face positions Pa and Pb on separator 103, and insulating sheet 5b is wound around wound body 100 so as to face positions Pa and Pb on separator 104. Insulating sheet 5b is disposed on the opposite side of insulating sheet 5a with anode foil 101 and cathode foil 102 sandwiched therebetween.
[0068] 9 is a diagram showing an example of a schematic configuration of a winding device 9 that produces a wound body 100. The winding device 9 has a reel 101R around which an anode foil 101 is wound, a reel 102R around which a cathode foil 102 is wound, a reel 103R around which a separator 103 is wound, a reel 104R around which a separator 104 is wound, a reel 5aR around which an insulating sheet 5a is wound, and a reel 5bR around which an insulating sheet 5b is wound.
[0069] The anode foil 101, the cathode foil 102, and the separators 103, 104 are pulled out in the pulling directions D1 to D4 via rollers 93, 95, 92, and 94, respectively. The anode foil 101, the cathode foil 102, and the separators 103, 104 are superimposed by passing through a clamp roller 96 on the downstream side, and are then spirally wound around the circumferential surface of the winding core Ax, as shown in FIG. 3 . A cutter 97 is disposed on the upstream side of the winding core Ax. After a predetermined length of the anode foil 101, the cathode foil 102, and the separators 103, 104 has been wound, the cutter 97 moves in a direction D5 approximately perpendicular to the winding direction to cut the anode foil 101, the cathode foil 102, and the separators 103, 104.
[0070] Insulating sheet 5a is unwound from reel 5aR and superimposed on separator 103 by clamp roller 90 located upstream of roller 92. Insulating sheet 5b is unwound from reel 5bR and superimposed on separator 104 by clamp roller 91 located upstream of roller 94. Reel 5aR feeds insulating sheet 5a so that insulating sheet 5a is superimposed only on a predetermined area of anode foil 101, and reel 5aL feeds insulating sheet 5b so that insulating sheet 5b is superimposed only on a predetermined area of cathode foil 102.
[0071] Fig. 10 is a diagram showing another example of the schematic configuration of the winding device 9 that produces the wound body 100. In Fig. 10, the same components as those in Fig. 9 are denoted by the same reference numerals, and the description thereof will be omitted.
[0072] The winding device 9 has laminating devices 98 and 99 for the insulating sheets 5a and 5b. The laminating device 98 is located upstream of the roller 92 and affixes the insulating sheet 5a to the anode foil 101. The laminating device 99 is located upstream of the roller 94 and affixes the insulating sheet 5b to the cathode foil 102. An acrylic adhesive, for example, is applied in advance to the laminating surfaces of the insulating sheets 5a and 5b. By affixing the insulating sheets 5a and 5b to the anode foil 101 and the cathode foil 102 in this manner, misalignment of the insulating sheets 5a and 5b is more effectively suppressed.
[0073] Referring again to FIG. 8 , the wound body 100 is immersed in, for example, an ammonium phosphate aqueous solution, and a predetermined voltage is applied to the anode foil 101 while the wound body 100 is subjected to a chemical conversion treatment again, thereby repairing the oxide film and forming a dielectric layer on the surface of the cut end of the anode foil 101 (step St3).
[0074] Next, in a reduced pressure atmosphere, the wound body 100 is immersed in a dispersion liquid of a conductive polymer to impregnate the dispersion liquid into the wound body 100 (step St4). Note that instead of the dispersion liquid of a conductive polymer, the wound body 100 may be immersed in a solution containing a conductive polymer.
[0075] Next, the wound body 100 is dried (step St5). At this time, the water content of the conductive polymer solution impregnated in the separators 103 and 104 in the wound body 100 evaporates, forming a conductive polymer layer.
[0076] Next, electrolytic capacitor element 10 is impregnated with an electrolyte in a reduced pressure atmosphere (step St6). Next, electrolytic capacitor element 10 is housed in case 11 and sealed with sealing member 12 (step St7). At this time, extraction electrodes 19a, 19b extending from electrolytic capacitor element 10 are inserted into through-holes 120 in sealing member 12. Thereafter, an aging treatment may be performed while applying a rated voltage to aluminum electrolytic capacitor 1. The manufacturing process for aluminum electrolytic capacitor 1 is performed in this manner.
[0077] Following the above manufacturing process, 10,000 units of each of Samples 1 to 4 of the aluminum electrolytic capacitor 1 were produced. Furthermore, for the evaluation of Samples 1 to 4, Sample 5 was produced as a comparison. Unlike Samples 1 to 4, Sample 5 has a total of four insulating sheets 6a, 6b, 7a, and 7b, which individually cover the battledore portion 112a and the burr B on its back side, and the battledore portion 112b and the burr B on its back side, similar to the configuration shown in Figures 7a and 7b. In contrast, Samples 1 to 4 have a total of two insulating sheets: insulating sheet 5a, which covers the battledore portions 112a and 112b, and insulating sheet 5b, which covers the burr B on the back side of the battledore portions 112a and 112b.
[0078] The diameter of the case 11 of Samples No. 1 to 5 was 18 mm, and the height of Samples No. 1 to 5 was 40 mm. The thickness of the anode foil 101 was 120 μm, the thickness of the separators 103 and 104 was 30 μm, and the thickness of the insulating sheets 5 a, 5 b, 6 a, and 6 b was 40 μm.
[0079]
[0080] Table 1 shows various parameters and evaluation results for Samples No. 1 to 5. Samples No. 1 to 4 each used two insulating sheets 5a and 5b. The length Lb of the insulating sheets 5a and 5b of Sample No. 1 was 20.0 mm, the length Lb of the insulating sheets 5a and 5b of Sample No. 2 was 24.0 mm, the length Lb of the insulating sheets 5a and 5b of Sample No. 3 was 80.0 mm, and the length Lb of c of Sample No. 4 was 88.0 mm.
[0081] Sample No. 5 used four insulating sheets 6a, 6b, 7a, and 7b. The length Lb of the insulating sheets 6a, 6b, 7a, and 7b of Sample No. 5 was 10.0 mm. Samples 1 to 5 had a distance La between the lead electrodes 19a and 19b (inter-electrode distance) of 8.0 mm.
[0082] The ratio (Lb / La) of the length Lb of the insulating sheets 5a, 5b, 6a, and 6b to the inter-terminal distance La was calculated from the above values. Lb / La for Sample No. 1 was 2.5, Lb / La for Sample No. 2 was 3.0, Lb / La for Sample No. 3 was 10.0, Lb / La for Sample No. 4 was 11.0, and Lb / La for Sample No. 5 was 1.25.
[0083] Samples No. 1 to 5 were evaluated by measuring the short-circuit defect rate (defect rate) (%) and the diameter (element diameter) (mm) of the wound body 100. The defect rate was measured using a short-circuit detection mechanism of an aging machine, and the element diameter was measured using a vernier caliper.
[0084] The defective rate for sample No. 1 was 2.15% (%), the defective rate for sample No. 2 was 1.54% (%), the defective rate for sample No. 3 was 0.42% (%), and the defective rate for sample No. 4 was 0.37% (%). The defective rate for sample No. 5 was 3.61% (%). Sample No. 5 had insulating sheets 6a, 6b, 7a, and 7b individually provided on battledore portions 112a and 112b and their burrs B, and because the length Lb was the shortest, the insulating sheets 6a, 6b, 7a, and 7b were easily misaligned, resulting in the highest defective rate.
[0085] The improvement rate (%) indicates the ratio of the defect rate of Samples No. 1 to 4 to the defect rate of Sample No. 5. Sample No. 1 had the shortest length Lb of the insulating sheets 5a, 5b among Samples No. 1 to 4, and therefore had the lowest improvement rate of 40%. Sample No. 4 had the longest length Lb of the insulating sheets 5a, 5b among Samples No. 1 to 4, and therefore had the highest improvement rate of 90%. Sample No. 2 had an improvement rate of 57%, and Sample No. 3 had an improvement rate of 88%.
[0086] As described above, the longer the length Lb of the insulating sheets 5a and 5b, the more effectively the positional misalignment is suppressed. However, the larger the diameter (element diameter) of the wound body 100, the more difficult it becomes to house the electrolytic capacitor element 10 in the case 11 and seal it with the sealing body 12. The element diameter of Sample No. 5 was 15.70 mm. Since the length Lb of the insulating sheets 5a and 5b of Sample No. 1 was the shortest among Samples Nos. 1 to 4, the element diameter was the smallest at 15.68 mm. Since the length Lb of the insulating sheets 5a and 5b of Sample No. 4 was the longest among Samples Nos. 1 to 4, the element diameter was the largest at 16.01 mm. Furthermore, the element diameter of Sample No. 2 was 15.70 mm, and the element diameter of Sample No. 3 was 15.97 mm.
[0087] The diameter increase rate (%) indicates the ratio of the element diameter of Samples Nos. 1 to 4 to the element diameter of Sample No. 5. From the above element diameter measurement results, the diameter increase rate of Sample No. 1 was −0.1(%), the diameter increase rate of Sample No. 2 was 0(%), the diameter increase rate of Sample No. 3 was +1.7(%), and the diameter increase rate of Sample No. 4 was +2.0(%).
[0088] Samples No. 1 to No. 4 were judged based on the evaluation results of the improvement rate and diameter increase rate. The judgment was "Good" (Excellent) when the two conditions of improvement rate > 50 (%) and diameter increase rate < 2.0 (%) were met, and "Good" (△) when only one of the two conditions was met. According to the above criteria, Samples No. 1 and No. 4 were judged as "Good", and Samples No. 2 and No. 3 were judged as "Good".
[0089] From the above, it is preferable that Lb / La is 3.0 or more from the viewpoint of the defect rate, and it is preferable that Lb / La is 10.0 or less from the viewpoint of the element diameter.
[0090] Although the embodiments of the present invention have been described in detail above, the present invention is not limited to such specific embodiments, and various modifications and changes are possible within the scope of the gist of the present invention as described in the claims.
Claims
1. An electrolytic capacitor element comprising: a wound body in which an anode foil and a cathode foil are wound with a first separator and a second separator on opposite sides of each other; an anode connection terminal connected to a first position of the anode foil; a cathode connection terminal connected to a second position of the cathode foil; a first insulating material wound within the winding body so as to face the first position and the second position on the first separator; and a second insulating material wound within the winding body so as to face the first position and the second position on the second separator, and positioned on the opposite side of the first insulating material with the anode foil and cathode foil in between.
2. The electrolytic capacitor element according to claim 1, characterized in that the length in the winding direction of at least one of the first insulating material and the second insulating material is three times or more the distance between the anode connection terminal and the cathode connection terminal.
3. The electrolytic capacitor element described in claim 1, characterized in that the length in the winding direction of at least one of the first insulating material and the second insulating material is 10 times or less the distance between the anode connection terminal and the cathode connection terminal.
4. The electrolytic capacitor element according to any one of claims 1 to 3, characterized in that at least one of the first insulating material and the second insulating material contains fibers.
5. An electrolytic capacitor element as described in any one of claims 1 to 3, characterized in that the anode connection terminal and the cathode connection terminal have burrs at the ends where they penetrate the anode foil and the cathode foil, and are crimp-connected to the anode foil and the cathode foil by the burrs, and at least one of the first insulating material and the second insulating material covers the burrs of at least one of the anode foil and the cathode foil.
6. The electrolytic capacitor element according to any one of claims 1 to 3, wherein the first insulating material is attached to the first separator.
7. The electrolytic capacitor element according to any one of claims 1 to 3, wherein the second insulating material is attached to the second separator.
8. A method for manufacturing an electrolytic capacitor element, comprising: a step of connecting an anode connection terminal to a first position of an anode foil and connecting a cathode connection terminal to a second position of a cathode foil; and a step of generating a wound body by winding the anode foil and the cathode foil with a first separator and a second separator on opposite sides thereof, wherein in the step of generating the wound body, a first insulating material is wound within the wound body so as to face the first position and the second position on the first separator, and a second insulating material is wound within the wound body on the opposite side to the first insulating material, sandwiching the anode foil and the cathode foil, so as to face the first position and the second position on the second separator.
Citation Information
Patent Citations
Electrolytic capacitor element structure
JP1983018337U
Electrolytic capacitor
JP2000150307A
Electrolytic capacitor, and method of manufacturing the same
JP2010074083A
Electronic component and manufacturing method of the same
JP2012169575A
Electronic component
JP2018206846A