A multilayered coating

The multilayered diamond coating with a doped base layer, intermediate and top layers, and microchannels addresses adhesion and durability issues, enhancing wear resistance and thermal management while enabling real-time wear detection, thus improving the performance and lifespan of mechanical systems.

WO2026234410A1PCT designated stage Publication Date: 2026-11-12MEHTA MITUL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/IB2025/054673
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-05
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Diamond coatings face limitations in complex mechanical systems due to high internal stress, poor adhesion to substrates, tendency to fracture, and high cost, especially in environments with high stress, high speed, high pressure, or corrosion.

Method used

A multilayered coating comprising a base layer of doped diamond crystals for electrical conductivity, an intermediate layer of microcrystalline and nanocrystalline diamonds for thermal conductivity and mechanical strength, and a top layer of nanocrystalline diamonds for wear resistance, with optional microchannels for heat dissipation, and a sensing circuit for wear monitoring.

Benefits of technology

Enhances tribological performance, improves durability and thermal management, extends operational lifespan, and provides real-time wear detection, offering up to 40% improved wear resistance and 25% enhanced thermal management compared to conventional coatings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure IB2025054673_12112026_PF_FP_ABST
    Figure IB2025054673_12112026_PF_FP_ABST
Patent Text Reader

Abstract

A multilayered coating for a substrate is disclosed Said multilayered coating comprises a base layer including doped diamond crystals. The base layer is electrically conductive and is configured to indicate detectable change in electrical 5 conductivity upon wearing of one or more layers of the multilayered coating. An intermediate layer is disposed on the base layer. The intermediate layer includes microcrystalline and nanocrystalline diamonds. A top layer including nanocrystalline diamonds is disposed on the intermediate layer.
Need to check novelty before this filing date? Find Prior Art

Description

A MULTILAYERED COATINGTechnical Field

[0001] The present disclosure relates to a multilayered coating for a substrate. More specifically, the present disclosure relates to a multilayered coating comprising a plurality of layers of diamond and a method for obtaining the multilayered coating.Background

[0002] Diamond coatings offer exceptional hardness (up to 70-100 GPa), thermal conductivity (up to 2200 W / mK), and wear resistance, and therefore find a variety of applications, including biomedical devices and cutting tools. However, their application in complex mechanical systems, such as those exposed to high stress, high speed, high pressure or corrosive environment (for example, screw compressors) has been limited by factors such as high internal stress, poor or limited adhesion to substrates like titanium alloys and steels, tendency to fracture or flake off under high cyclic fatigue, and the potential for high cost and complex deposition processes.Summary

[0003] In an aspect, the present disclosure relates to a multilayered coating for a substrate. The multilayered coating comprises a base layer including doped diamond crystals. The base layer is electrically conductive and is configured to indicate detectable change in electrical conductivity upon wearing of one or more layers of the multilayered coating. An intermediate layer is disposed on the base layer. The intermediate layer includes microcrystalline and nanocrystalline diamonds. A top layer including nanocrystalline diamonds is disposed on the intermediate layer.

[0004] In another aspect, a coated article is described. Said coated article comprises a substrate and a multilayered coating covering at least a portion of atleast one surface of the substrate. The multilayered coating comprises a base layer including doped diamond crystals. The base layer is electrically conductive and is configured to indicate detectable change in electrical conductivity upon wearing of one or more layers of the multilayered coating. An intermediate layer is disposed on the base layer. The intermediate layer includes microcrystalline and nanocrystalline diamonds. A top layer including nanocrystalline diamonds is disposed on the intermediate layer.

[0005] In yet another aspect, the disclosure is directed towards a system comprising the aforesaid coated article and a sensing circuit. The coated article is connected to the sensing circuit at the base layer of the multilayered coating and the sensing circuit is configured to detect wear of the multilayered coating by detecting any difference in the electrical conductivity thereof.

[0006] In yet another aspect, the disclosure is directed towards a method for producing a multilayered coating on a substrate. Said method comprises in step (a), preparing the substrate for deposition of diamonds thereon. In step (b), a base layer comprising doped diamond crystals is deposited on at least a portion of at least one surface of the substrate using a diamond deposition technique. In step (c), one or more deposition process parameters of the diamond deposition technique are varied to deposit an intermediate layer on the base layer. The intermediate layer includes microcrystalline and nanocrystalline diamonds. In step (d), the one or more deposition process parameters of the diamond deposition technique are further varied to deposit a top layer on the intermediate layer. The top layer includes nanocrystalline diamonds. The method further comprises monitoring the diamond deposition in real time using a monitoring system to detect any deviation in the growth of one or more of the base layer, the intermediate layer and the top layer of the multilayered coating. If a deviation is detected, an automatic feedback is generated for adjusting the one or more deposition process parameters based on the automatic feedback from the monitoring system.Brief Description of the Drawings

[0007] The accompanying figures, where the same reference numerals refer to identical or functionally similar elements throughout the separate views, together with the detailed description below, are incorporated into and form part of the specification. They serve to further illustrate embodiments of concepts that include the claimed invention and explain the various principles and advantages of those embodiments.

[0008] FIG. 1 illustrates the trans-sectional view of the multilayered coating provided on a cylindrical substrate, in accordance with some embodiments of the present disclosure;

[0009] FIGs. 2 and 3 illustrate the multilayered coating of FIG. 1 having different microchannel geometries, in accordance with some embodiments of the present disclosure;

[0010] FIGs. 4 and 5 illustrate the multilayered coating having different microchannel geometries, provided on a flat substrate, in accordance with some embodiments of the present disclosure; and

[0011] FIG. 6 provides a schematic representation of a system comprising a coated article and a sensing circuit, in accordance with an embodiment of the present disclosure.

[0012] Skilled artisans will appreciate that the elements in the figures are illustrated for simplicity and clarity and have not necessarily been drawn to scale. For example, the dimensions of some of the elements in the figures may be exaggerated relative to other elements to help to improve understanding of the embodiments.Detailed Description

[0013] Reference will now be made in detail to specific embodiments or features, examples of which are illustrated in the accompanying drawings. Wherever possible, the same reference numbers will be used throughout the drawings to refer to the same or the like parts.

[0014] Referring to Fig. 1, an exemplary multilayered coating 100 is illustrated. This multilayered coating 100 is configured to be applied on a substrate 110, which finds application in high-stress, high-speed, high-pressure, abrasive, and / or corrosive environments, including compressors, turbines, generators, semiconductor heat sinks, medical implants, cutting tools, aerospace components, marine equipment, optical instruments, fuel cells, high-performance sporting goods and the like. In these environments, the multilayered coating 100 is configured to provide one or more of enhanced tribological performance (low friction), improved coating durability, in-situ wear monitoring, optimized heat transfer, and resistance to wear, corrosion, and contamination. In some embodiments, the multilayered coating 100 may also be provided to protect the substrate 110 from a variety of external forces and environmental conditions.

[0015] With continued reference to Fig. 1, the multilayered coating 100 includes a base layer 102, an intermediate layer 104 disposed on the base layer 102, and a top layer 106 disposed on the intermediate layer 104. The multilayered coating 100 is configured to adhere to the substrate 110 at the base layer 102 and cover at least a portion of at least one surface of the substrate 110.

[0016] The base layer 102 comprises doped diamond crystals. In an embodiment, the base layer 102 is configured to provide electrical conductivity to the multilayered coating 100 and provide a mechanism for monitoring wearing of the multilayered coating. In an embodiment, the base layer 102 comprises of diamond crystals doped with a dopant selected from the group consisting of boron, nitrogen, and phosphorus. Doping with boron, nitrogen, and phosphorus fine tunes electricalconductivity of diamond. This allows the base layer 102 to be configured to detect wear changes through variations in electrical resistance to current flow upon wear or formation of small cracks in the multilayered coating 100. In some embodiments, the dopant is boron. In an embodiment, the base layer 102 has a doping concentration ranging from 1019atoms / cm3to 1021atoms / cm3. The doping concentration may be varied depending on the electrical conductivity requirements for wear sensing, while maintaining the mechanical properties of the base layer 102. In some embodiments, the base layer 102 has the doping concentration ranging from 1 * IO20to 5 * IO20atoms / cm3, providing optimized electrical conductivity for wear sensing while maintaining the mechanical integrity and durability of the multilayered coating 100.

[0017] In an embodiment, the base layer 102 has a thickness ranging from 1 to 10 pm. In some embodiments, the base layer 102 has the thickness ranging from 2 to 5 pm. In some embodiments, the base layer 102 includes a varying cross-sectional area across its expanse, allowing for localized optimization of conductivity, mechanical strength, and wear resistance based on application requirements. In an embodiment, the base layer 102 includes doped diamond crystals having a grain size ranging from 500 nm to 10 pm. In some embodiments, the base layer 102 includes doped diamond crystals having the grain size ranging from 1 to 5 pm.

[0018] The intermediate layer 104 comprising of microcrystalline and nanocrystalline diamonds is provided on the base layer 102. In an embodiment, the intermediate layer 104 is configured to provide high thermal conductivity and mechanical strength to the multilayered coating 100. In an embodiment, the intermediate layer 104 comprises microcrystalline diamonds having a grain size ranging from 100 to 500 nm. In an embodiment, the intermediate layer 104 comprises of nanocrystalline diamonds having a grain size ranging from 50 to 100 nm. In an embodiment, the intermediate layer 104 is characterized by a gradient transition from microcrystalline diamonds to nanocrystalline diamonds. In anotherembodiment, the intermediate layer 104 comprises of a plurality of discrete sublayers of microcrystalline and nanocrystalline diamonds of predetermined grain size. Each of these distinct sub-layers is configured to provide specific stress and / or thermal management properties. In an embodiment, the plurality of discrete sublayers exhibits a progressive decrease in diamond grain size, wherein each successive sub-layer features diamonds with a smaller grain size than the preceding sub-layer. In yet another embodiment, the intermediate layer 104 comprises alternating sub-layers of microcrystalline and nanocrystalline diamonds, wherein each sub-layer is optimized to provide specific mechanical, thermal, and / or wearresistance properties. In an embodiment, the diamonds forming the intermediate layer 104 are substantially free of any impurity.

[0019] In an embodiment, the intermediate layer 104 has a thickness ranging from 5 to 50 pm. In some embodiments, the thickness of the intermediate layer 104 ranges between 10 to 30 pm. The thickness of the intermediate layer 104 is optimized based on specific stress concentration and thermal management requirements. In some embodiments, the intermediate layer 104 includes a varying cross-sectional area across its expanse to optimize stress distribution, thermal conductivity, and adhesion to complex substrate geometries.

[0020] In an embodiment, the intermediate layer 104 has a hardness of at least 90 GPa. In some embodiments, the intermediate layer 104 has the hardness of 100 to 110 GPa. In an embodiment, the intermediate layer 104 has a thermal conductivity of at least 2000 W / mK at 25°C. In some embodiments, the intermediate layer 104 has the thermal conductivity of 2200 to 2400 W / mK at 25°C, optimizing heat dissipation for high-performance applications.

[0021] The top layer 106 including nanocrystalline diamonds is provided on the intermediate layer 104. In an embodiment, the top layer 106 comprises of nanocrystalline diamonds having a grain size ranging from 2 to 100 nm. In some embodiments, the top layer 106 comprises nanocrystalline diamonds having thegrain size of 3 to 10 nm, providing superior wear resistance and a low coefficient of friction. In an embodiment, the top layer 106 has a coefficient of friction less than 0.1. In some embodiments, the top layer 106 has the coefficient of friction of 0.03 to 0.07, minimizing energy losses and wear in high-speed, high-stress environments. In some embodiments, the top layer 106 is configured to reduce the friction and enhance the wear resistance, thereby improving the efficiency of the substrate 110 and the machinery in which the substrate 110 is employed.

[0022] In an embodiment, the top layer 106 has a thickness ranging from 1 to 10 pm. In some embodiments, the top layer 106 has the thickness of 2 to 5 pm. The thickness of the top layer 106 is dependent on specific frictional requirements, allowing for tailored tribological performance. In some embodiments, the top layer 106 includes a varying cross-sectional area across its expanse to optimize tribological performance, ensuring reduced friction in high-contact zones and enhanced wear resistance in high-stress regions.

[0023] In an embodiment, the multilayered coating 100 further comprises one or more additional layers positioned between the base layer 102 and the intermediate layer 104 and / or the intermediate layer 104 and the top layer 106. These additional layers are formed of materials including but not limited to tungsten carbide (WC), silicon carbide (SiC), boron nitride (BN), aluminum nitride (AIN), diamond-like carbon (DLC), titanium nitride (TiN), graphene -based coatings, and nanocomposite oxides (e.g., ZrCh, TiCh), which provide one or more of enhanced stress management, adhesion, wear resistance, tribological performance, and tailored functional properties to the multilayered coating 100.

[0024] In an embodiment, the multilayered coating 100 includes a continuous gradient transition from the base layer 102 to the intermediate layer 104 followed by the top layer 106. The continuous gradient transition minimizes stress concentration, strengthens interlayer adhesion, and / or significantly enhances coating durability in dynamic environments.

[0025] In an embodiment, the multilayered coating 100 includes one or more microchannels 108 extending from the top layer 106 to at least a part of the intermediate layer 104. The one or more microchannels 108 have a width ranging from 10 to 500 pm and a depth ranging from 5 to 60 pm. The microchannels 108 allow for heat dissipation directly at the source, maintaining optimal performance even in extreme temperatures (e.g., -40°C to 150°C). In contrast to the prior known coatings requiring external cooling systems, the multilayered coating 100, including the one or more microchannels 108, provides for heat management at the source of heat generation, thereby minimizing thermal gradients in the multilayered coating 100 and reducing the overall complexity of the article and system in which the multilayered coating 100 is employed.

[0026] In an embodiment, the one or more microchannels 108 are left open to ambient air. In another embodiment, the one or more microchannels 108 are configured to receive and / or circulate a working fluid selected from the group consisting of a cooling fluid, a lubricant and a multifunctional fluid that provides both cooling and lubrication. In some embodiments, the one or more microchannels 108 are flooded with the cooling fluid to assist in heat dissipation. In some other embodiments, one or more microchannels 108 are intermittently supplied with the lubricant to reduce friction on the surface of the multilayered coating 100. Any known cooling fluid, a lubricant and a multifunctional fluid may be used. In some embodiments, the cooling fluid includes compressed air, water-glycol, and synthetic heat-transfer oil.

[0027] In an embodiment, the one or more microchannels 108 included in the multilayered coating 100 have linear and / or non-linear (or irregular) geometry. FIGs. 3 and 5 show exemplary microchannels 108 having a linear geometry. FIGs.2 and 4 show exemplary microchannels 108 having a non-linear geometry. In some embodiments, the microchannels 108 include different geometries including but not limited to grid microchannels, sinusoidal microchannels, sinusoidal grid microchannels, hierarchical microchannels, and / or tapered sinusoidalmicrochannels. Optionally or additionally, the one or more microchannels 108 include an irregular cross- section across their depth from the top layer 106 to the intermediate layer 104. In some embodiments, the one or more microchannels 108 included in the multilayered coating 100 have distinct depth and width (as shown in Figs. 2, 4 and 5). In alternate embodiments, the one or more microchannels 108 included in the multilayered coating 100 have the same depth and width (as shown in Fig. 3). In some embodiments, the microchannels 108 are asymmetrical. In some embodiments, the microchannels 108 include one or more ridges, and / or one or more grooves formed therein to increase the surface area of the microchannels 108, thereby enhancing the multilayered coating 100’s thermal management, wear resistance, and mechanical durability. The inclusion of the one or more microchannels 108 with variable geometries, depths, and widths optimizes heat dissipation, lubrication distribution, and structural integrity, making them highly effective for high-performance applications such as compressors, turbines, industrial cutting tools, and high-speed machinery. The microchannels 108 define corresponding openings (not shown) at the top layer 106 of the multilayered coating 100. In an embodiment, the openings of the one or more microchannels 108 are configured to have surface having a profile / geometry which allows minimizing stress concentration and inhibiting crack initiation in the top layer 106. In some embodiments, the surface of the openings of the one or microchannels 108 has a radius of > 5 pm. In other embodiments, the surface of the openings of the one or microchannels 108 has a sinusoidal shape to minimize stress concentration and inhibit crack initiation. The aforesaid features of the one or more microchannels 108 define the geometry of the one or more microchannels 108 and allows for tailoring the properties of the multilayered coating 100 as per the requirements, enabling the substrate 110 to function in an optimal condition. For example, the aforesaid geometry of the microchannels 108 results in an increase in an outer surface area of the multilayered coating 100, thereby allowing relatively more heat dissipation from the substrate 110 in turn keeping the substrate 110 in an optimal working temperature. In an embodiment, the microchannels 108 cover approximately 30% to 50% of the surface area of the multilayered coating 100 toensure efficient heat dissipation and thermal management. In an embodiment, to ensure adequate load-bearing capacity of the multilayered coating 100, a land area comprising at least 30% of the surface area of the multilayered coating 100 is maintained between adjacent microchannels 108. In an embodiment, the microchannels 108 are arranged concentrically, parallelly, or randomly.

[0028] In an embodiment, the multilayered coating 100 includes a uniform cross-sectional area across its expanse. In an alternate embodiment, the multilayered coating 100 has a varying cross-sectional area across its expanse, depending on the heat dissipating requirements of the substrate 110. The heat dissipating requirements include, but are not limited to, the rate at which heat must be removed from the substrate 110, as well as the total amount of heat that needs to be dissipated from the substrate 110 to achieve its optimal operational temperature. In some embodiments, the width and / or depth of the multilayered coating 100 is relatively more in certain regions, which may enable excess heat to be absorbed or extracted thereto, e.g., from hotspots defined by the substrate 110 or from locations of the substrate 110 which may produce relatively excessive heat (e.g., leading edges, tips, or shaft sections of a rotor).

[0029] Referring to FIGs. 1 through 5, exemplary coated articles are described. The coated article comprises a substrate 110 and a multilayered coating 100 covering at least a portion of at least one surface of the substrate. The substrate 110 is composed of, including but not limited to, one or more metals or alloys thereof, ceramics, ceramic composites, polymers (for e.g., polyetheretherketone (PEEK) , and polytetrafluoroethylene (PTFE)), carbon-based materials (for e.g., graphite, and carbon fiber composites), semiconductor materials (for e.g., silicon, and silicon carbide), optical materials (e.g., quartz and sapphire), and refractory materials (for e.g., tungsten, molybdenum, and zirconia-based composites), as well as any other analogous material currently known or developed in the future. Metal substrates include, but are not limited to, iron, iron-based alloys (e.g., stainless steels), nickel-based alloys, cobalt-based alloys and the like. The substrate 110 canvary in size and geometry, ranging from small cylindrical components (e.g., 5 cm in diameter) to large industrial rotors (e.g., up to 1 meter in diameter). Non-limiting exemplary substrates include a rotor for a compressor, a turbine blade, screws of extruder, bearings, compressors, pumps, pipes, tubing, molding dies, valves, walls of reactor vessels, heat exchangers, cutting tools, camshafts, crankshafts, seals, nozzles, pistons, or sliding contacts, or any component of an industrial machinery that is subject to high wear and stress.

[0030] The multilayered coating 100 covers at least a portion of at least one surface of the substrate 110. In an embodiment, the multilayered coating covers at least 50% of at least one surface of the substrate, depending on heat dissipation, wear resistance, and tribological performance requirements. In some embodiments, the multilayered coating completely covers exposed surface of the substrate.

[0031] With continued reference to FIGs. 1 to 5, a method for producing the multilayered coating 100 on the substrate 110 is described. Said method comprises in step (a), preparing the substrate 110 for deposition of diamond thereon. In an embodiment, the preparation of the substrate 110 for the deposition of diamond thereon includes cleaning the surface of the substrate for ensuring optimal adhesion of the multilayered coating 100 to the substrate 110. Exemplary cleaning methods include but are not limited to mechanical polishing, chemical etching, and plasma cleaning. In an embodiment, the preparation of the substrate 110 for the deposition of diamond thereon includes modifying the substrate 110 (such as Fe-based alloys) through alloying elements (such as aluminium, chromium, and silicon) to improve the quality of diamond deposited on them.

[0032] In step (b), the base layer 102 comprising of the doped diamond crystals is deposited on at least a portion of at least one surface of the substrate 110 using a diamond deposition technique. In operation, step (b) begins with providing on substrate 110 a seed layer of diamond inside a reactor used for carrying out the diamond deposition. The diamond deposition technique includes, but is not limitedto, Chemical Vapor Deposition (CVD) technique, High Pressure High Temperature (HPHT) technique, Plasma- Assisted Chemical Vapor Deposition (PACVD), Microwave Plasma Chemical Vapor Deposition (MPCVD), Hot Filament Chemical Vapor Deposition (HFCVD), Pulsed Laser Deposition (PLD), Atomic Layer Deposition (ALD), Ion Beam Deposition, Sputtering, combinations thereof, and any other process of synthesizing diamonds currently known or developed in the future.

[0033] In an embodiment, CVD process is used for diamond deposition. In this process, the substrate 110 is cleaned and pre-treated to ensure a clean surface for the deposition of a nucleation layer. Next, the nucleation layer is deposited on the substrate 110 to promote the controlled formation of subsequent layers by providing nucleation sites. Once the required density of nucleation sites is achieved, the formation of the base layer 102 is initiated. In some embodiments, to initiate the formation of the base layer 102 including doped diamond crystals, a feed gas comprising one or more carbon containing gases (e.g., methane (CH4)) diluted in a high concentration of the hydrogen (H2) gas, and a dopant-containing gas including boron (e.g., diborane (B2H6)), nitrogen (N2), or phosphorus molecules, is fed to a CVD reactor. The in situ doping results in a uniform distribution of dopants throughout the diamond crystals deposited on the substrate 110 as well as allows for precise control over the doping concentration and distribution within the growing diamond, all within the CVD reactor without needing additional postdeposition steps.

[0034] Following the introduction of the feed gas into the CVD reactor, it undergoes ionization and dissociation via micro wave plasma (PECVD) or hot filament activation. This process creates a reactive environment conducive to diamond growth on the substrate 110. The temperature and pressure inside the reactor and the ratio of the dopant-containing gases to the one or more carbon containing gases in the feed gas are maintained at predetermined values such that the obtained base layer 102 has the dopants in the range of 1019atoms / cm3to 1021atoms / cm3. In an exemplary embodiment, to obtain the base layer 102 with a doping concentration of ~5 x 1O20atoms / cm3, the CVD reactor was maintained at 750°C, 50 Torr, and 3 kW microwave power. To this CVD reactor, a gas mixture comprising H2 (1000 seem) as the carrier gas, CH4 (30 seem, ~3% of total flow) as the carbon precursor and B2H6 (200 ppm relative to CH4) for boron doping, was fed. The deposition was carried out for about 6 hours to achieve a thickness of 5 pm. In some embodiments, additional elements and / or compounds, including but not limited to titanium, chromium, or other metal carbides / nitrides are added to the feed gas to enhance adhesion between the base layer 102 and the substrate 110.

[0035] In another embodiment, a hybrid of HPHT and CVD process is employed for diamond deposition. In some embodiments, a diamond seed is initially grown using the HPHT method followed by placing this seed in a CVD reactor wherein the CVD process is carried out using feed gas comprising of dopant containing gas to grow the base layer 102 including doped diamond crystals.

[0036] After the formation of the base layer 102, in step (c), one or more deposition process parameters of the diamond deposition technique used to form the base layer 102 are varied to deposit the intermediate layer 104 on the base layer 102. The intermediate layer 104 comprises of microcrystalline and nanocrystalline diamonds. The deposition process parameters, which are varied include, but are not limited to, composition of feed gas, gas flow rate, reactor pressure, reactor temperature, deposition rate, microwave power, substrate bias voltage, plasma density, dopant concentration, and ion bombardment energy. In an embodiment, in both the CVD process and hybrid of HPHT and CVD process described earlier, once the base layer 102 is formed, the feed gas devoid of the dopant containing gas is fed to the reactor to initiate the formation of the intermediate layer 104, using the CVD process. In another embodiment, the feed gas devoid of dopant and reduced concentration of CH4 composition in H2 (e.g., CH* concentration of 3% during base layer formation reduced to 1%), is used to decrease carbon availability and facilitate the transition to a finer grain size of the intermediate layer 104.

[0037] In an embodiment, the intermediate layer 104 including a gradient transition from microcrystalline diamonds to nanocrystalline diamonds is formed. To cause the transition from microcrystalline diamonds to nanocrystalline diamonds, growth conditions are adjusted to promote the formation of significantly smaller diamond grains. In some embodiments, to cause the transition from microcrystalline diamonds to nanocrystalline diamonds, the composition of the feed gas is modified by increasing the concentration of the carbon precursor (for e.g. methane) relative to hydrogen, leading to a change in a plasma environment and nucleation process, resulting in the growth of nanocrystalline diamonds instead of microcrystalline diamonds. For example, the composition of feed gas is varied by increasing CFU concentration (e.g., from 2 to 10% relative to H2) to cause the transition from microcrystalline diamonds to nanocrystalline diamonds. In other embodiments, the transition from microcrystalline diamonds to nanocrystalline diamonds in the intermediate layer 104 is achieved by increasing the reactor pressure (e.g., by deposition of microcrystalline diamonds at 50 Torr and then increasing the pressure to 80 Torr) to favor nanocrystalline diamond growth by altering ion transportation and nucleation density, thereby controlling grain size. In still other embodiments, to cause the transition from microcrystalline diamonds to nanocrystalline diamonds, the substrate temperature is lowered (e.g., from 850°C to about 650°C). In yet other embodiments, Argon (Ar) is introduced in the feed gas to enhance grain refinement as well as tune the morphology of the nanocrystalline diamonds. In yet other additional embodiments, microwave power is decreased (e.g., from 4 kW to 2 kW) to cause the transition from microcrystalline diamonds to nanocrystalline diamonds. In yet other additional embodiments, the plasma power is increased (e.g., by starting with 2 kW microwave power and then increasing to 3.5 kW) during transition to enhance nucleation rate. Higher plasma density favors the formation of nanocrystalline structures. In yet other additional embodiments, the substrate bias voltage is tuned (e.g., by applying a bias voltage of -50V initially, and then increasing to -100V during transition) to increase ion bombardment, causing a refinement of grain size and improvement of adhesion. One or more of the aforementioned embodiments are combined to facilitate thetransition from microcrystalline to nanocrystalline diamond, while also enabling precise control over diamond morphology.

[0038] In step (d), the one or more deposition process parameters of the diamond deposition technique are further varied to deposit the top layer 106 including nanocrystalline diamonds on the intermediate layer 104. The deposition process parameters which are varied include, but are not limited to, composition of feed gas, gas flow rate, reactor pressure, reactor temperature, deposition rate, microwave power, substrate bias voltage, plasma density, nucleation rate control, and dopant concentration. In some embodiments, the nanocrystalline diamonds are formed over the intermediate layer 104 by varying the composition of the feed gas, for example, to contain 5% - 10% methane (CH4) in hydrogen (H2). In other embodiments, to cause the formation of the top layer 106, reactor pressure was reduced (e.g., from 50 Torr to 25 Torr). In still other embodiments, argon (500 - 1000 seem) was introduced in feed gas. In still another embodiments, microwave power was finetuned (e.g., from 4 kW to 2 kW). In yet other embodiments, substrate temperature was lowered (e.g., from 750°C to 650°C). In some embodiments, a substrate bias voltage of -100V to -150V is applied to enhance nucleation and ensure nanocrystalline grain formation. One or more of the aforementioned embodiments can be combined to facilitate the formation of the top layer 106, while also controlling the morphology of the nanocrystalline diamonds therein.

[0039] In an embodiment, the diamond deposition in each layer is accompanied with real-time monitoring and automatic feedback control for adjusting the deposition process parameters dynamically based on the feedback from the monitoring systems. The real-time monitoring involves tracking, for example, coating thickness, doping concentration, and uniformity of layers during diamond growth. In some exemplary embodiments, the real-time monitoring is carried out using systems, including, but not limited to optical emission spectroscopy, mass spectrometry and laser interferometry. After detecting a defect or an anomaly, the automatic feedback control system re-adjusts one or more deposition processparameters as per the requirement. In some embodiments, an in situ doping control system is employed to monitor and control doping in real-time. The in situ doping control system comprises of optical emission spectrometer to determine the doping concentration, and a feedback control mechanism to dynamically adjust the dopant concentration and other process parameters to optimize doping levels.

[0040] In an embodiment, the method further includes the formation of one or more microchannels 108. In an embodiment, the microchannels 108 are formed by using laser ablation process. The laser ablation process may be performed in a single step or in multiple steps, depending on the desired depth and geometry of the microchannels 108. The laser ablation process includes scanning the laser beam across the surface of the multilayered coating 100 in a predetermined pattern, to form the one or more microchannels 108 having desired depth and geometries. In some embodiments, the method includes the formation of the microchannels 108 by using pulsed laser ablation using femtosecond or nanosecond lasers. The pulsed laser ablation using femtosecond or nanosecond lasers offer high precision and flexibility in forming microchannel geometries on the multilayered coating 100. By precisely controlling the laser parameters, including, but not limited to, the wavelength, and pulse duration, the surface quality of the microchannels 108 may be optimized. Femtosecond lasers provide ultra-short pulse widths, which minimize thermal damage to the surrounding material of the microchannels 108 and thereby enable high-precision micromachining. The ultra-short pulses allow for the formation of the microchannels 108 with smooth surfaces and well-defined edges, reducing the need for post-processing steps. Nanosecond lasers are also commonly used for laser micromachining of diamond substrates.

[0041] In another embodiment, the method includes the formation of the microchannels 108 by using plasma etching techniques such as Reactive Ion Etching (RIE), Deep Reactive Ion Etching (DRIE), Oxygen Plasma Etching or a combination thereof. Plasma etching provides a non-contact, high-precision method for microchannel formation, offering reduced thermal damage and enhancedcontrol over etching depth and geometry. In an embodiment, one or more plasmabased etching techniques are used in combination with one or more laser ablation processes to achieve optimized structures of microchannel 108.

[0042] In yet another embodiment, the one or more microchannels 108 are formed in situ during the deposition of the intermediate layer 104 and the top layer 106 using a masking template. Specifically, after the deposition of the base layer 102, the masking template (composed of a material such as graphite or silicon) having a structural configuration that corresponds to the desired microchannel geometry, is positioned on the base layer 102. Subsequently, the intermediate layer 104 and the top layer 106 are grown on the exposed surface of the masking template, effectively interrupting the diamond growth on the area occupied by the masking template. Upon completion of the top layer 106 formation, the masking template is then sacrificially removed (for e.g., by heating at high temperature ~ 450-550°C), resulting in the formation of the one or more microchannels 108. In an exemplary embodiment, a graphite-based masking template is used for forming one or more microchannels 108. After CVD growth of the intermediate layer 104 and the top layer 106, the coated article is heated in a muffle furnace at 500°C for 2 hours in flowing air, oxidizing the graphite template to CO / CO2 and leaving clean microchannels without requiring additional machining, while maintaining the stability of the multilayered coating 100.

[0043] Optionally and additionally, after the formation of the multilayered coating 100, the method includes one or more post-growth processing steps, including, but not limited to, annealing, surface polishing, laser micromachining, and one or more additional coating (for example, Diamond-Like Carbon (DLC), Titanium Nitride (TiN), Boron Nitride (BN), Silicon Carbide (SiC), or Alumina (AI2O3)) to enhance specific properties like hardness or corrosion resistance of the multilayered coating 100. In an embodiment, any excess or undesired growth of diamond on the multilayered coating 100 is removed using known techniques such as laser cutting or etching process.

[0044] In an embodiment, following the completion of the multilayered coating 100, a series of quality checks are performed to ensure the multilayered coating 100 meets the required specifications. These checks include one or more of adhesion testing, surface roughness measurement, and thermal conductivity assessments to validate the coating's performance in terms of wear resistance, thermal management, and overall durability.

[0045] The method for producing the multilayered coating 100 on the substrate 110 is carried out in any reactor known for carrying out the diamond deposition using CVD process, HPHT process, Plasma-Enhanced CVD (PECVD), Microwave Plasma CVD (MPCVD), Hot Filament CVD (HFCVD), Pulsed Easer Deposition (PED), Atomic Layer Deposition (ALD), Ion Beam-Assisted Deposition (IBAD), or combinations thereof. Optionally and additionally, said reactors include a substrate holder that is connected to a motion mechanism, providing rotational, linear, or both types of motion. This enables precise control over the substrate's position and orientation, facilitating uniform deposition of the multilayered coating 100 on the substrate 110. As a result, consistent coating properties are achieved across various substrate sizes and geometries.

[0046] In an embodiment, the method provides a coating growth rate of up to 100 pm / hour allowing for efficient production of both large industrial units and compact portable systems. The method parameters are configured to be varied to customize the coating properties for specific operational requirements.

[0047] Referring to FIG. 6, an exemplary system 120 is described. The system 120 comprises a coated article including the substrate 110 coated with the multilayered coating 100, and a sensing circuit 122. The coated article is connected to the sensing circuit 122 at the base layer 102 of the multilayered coating 100. In such configuration, the sensing circuit 122 is configured to detect wear of the multilayered coating 100 by detecting any difference in electrical conductivity of the base layer 102. In an example, the sensing circuit 122 includes a sensing unit122' electrically connected in a closed loop with the base layer 102 of the multilayered coating 100. In some embodiments, the sensing unit 122' comprises one or more power sources which provides electrical signal across the base layer 102 to monitor wear progression by detecting variations in the electrical conductivity of the base layer 102. The sensing unit 122' of the sensing circuit 122 includes one or more of a battery or external power supply, capacitors, resistors, conductivity sensors, a signal processing circuit including an Analog-to-Digital Converter (ADC) and a microcontroller, etc (not shown). In operation, the sensing unit 122' is activated to continuously provide the electrical signal across the base layer 102 to measure electrical values, such as conductivity, resistance, and / or capacitance value(s) across the base layer 102. As the multilayered coating 100 including the top layer 106, the intermediate layer 104 and the base layer 102 degrade due to wear, the sensing circuit 122 is configured to detect change (or difference) in the electrical values across the base layer 102. The sensing unit 122' based on the change in the electrical values, detects the variations in charge storage capacity and / or changes in resistance due to material depletion. The sensing unit 122' is configured to process these fluctuations and, upon detecting deviations beyond predefined thresholds, triggers an alert signal, which is transmitted to an external monitoring system (not shown). In an embodiment, the base layer 102 is configured to generate a binary signal, indicating either an "on" or "off" state. In this embodiment, the base layer 102 functions as a threshold sensor such that electrical continuity within this layer (or a significant change in its resistance) is designed to occur only upon the breaching of the overlying intermediate layer 104 and top layer 106. Consequently, the "off" state serves as an unambiguous indicator that the multilayered coating remains in its intended operational condition. Conversely, the transition to an "on" state provides a clear and direct signal signifying the substrate's end of life, thus offering a reliable and readily interpretable indication that the multilayered coating 100 has been breached. In an embodiment, the sensing unit 122' is configured to distinguish between different wear stages — minor, moderate, and severe — thus, ensuring real-time wear detection of the multilayered coating and predictive maintenance of the coated article. In anembodiment, the sensing circuit 122 is configured to detect wear of the multilayered coating 100 by detecting variations in electrical conductivity as small as 5%, corresponding to approximately 1-2 pm of wear. In some embodiments, wear as small as 1 pm can be detected using the disclosed multilayered coating 100. The sensing unit 122' provides a wear management system for the coated article, assisting in assessing and managing the wear of the multilayered coating 100.Industrial Applicability

[0048] The multilayered coating 100 is particularly suited for application on wear-prone components of industrial machinery, operating in extreme environments characterized by high stress, speed, pressure, abrasion and / or corrosion. In an embodiment, the multilayered coating 100 is employed on rotating components, such as blades or rotors, used in rotary machines, including steam turbines, compressor pumps, drilling system and the like. In addition to the applications mentioned above, the multilayered coating 100 finds application in machinery used in various other industries, including, but not limited to, aerospace, automotive, heavy machinery, medical devices, and food processing.

[0049] The thermal conductivity and heat dissipation properties of the multilayered coating 100 enhances the thermal management of components of industrial machinery to which it is applied, which is crucial for their performance, safety, and longevity. Efficient thermal management can lead to a significant increase in the energy storage capacity per unit weight and volume. The thermal properties of diamond and the efficient heat dissipation provided by the microchannels allow for a broader operating temperature range, making the substrate suitable for extreme environments. The advanced thermal management and mechanical stability offered by the multilayered coating 100 significantly reduces the risk of thermal runaway, overheating, and mechanical failures, enhancing the overall safety of the substrate. The multilayered coating 100 provides up to 40% improved wear resistance and up to 25% enhanced thermal management compared to conventional coatings.

[0050] The multilayered coating 100 in combination with sensing unit 122' provides a wear management system for the coated article. This finds application in assessment and management of any wear in the multilayered coating 100. Realtime data from the wear management system can be fed into adaptive control algorithms, allowing for dynamic adjustment of operational parameters to optimize performance and extend the life of the substrate to which the multilayered coating 100 is applied. In contrast to the prior art coatings, the multilayered coating 100 improves the operational lifespan of the substrate 110 by at least 30%.

[0051] In an exemplary embodiment, the multilayered coating 100 is used for coating the rotor of a compressor. The base layer 102 is formed of boron-doped diamonds (BDD) having a doping concentration of 5 * IO20atoms / cm3. The base layer 102 has the thickness of 2 - 5 pm. The intermediate layer 104 comprises diamonds having the average grain size of 100 - 500 nm, providing a transition from microcrystalline to nanocrystalline structures. The intermediate layer 104 has the thickness of 10 - 30 pm. The top layer 106 comprises nanocrystalline diamonds having an average grain size of 3 - 10 nm, ensuring ultra-low friction and high wear resistance. The top layer 106 has the thickness of 2 - 5 pm. The multilayered coating 100 has various microchannels 108 having the width ranging from 10 - 500 pm and the depth ranging from 5 to 60 pm, enabling efficient heat dissipation and fluid transport in high-stress operating environments.

[0052] In an exemplary embodiment, the performance of an oil-free compressor without any coating, an oil-free compressor coated with standard DLC coating, and an oil-free compressor coated with the exemplary multilayered coating 100 were compared. The standard DLC coating used in the comparative analysis is a hydrogenated amorphous carbon (a-C:H) coating, commonly employed in tribological applications for its low friction and wear resistance. The composition of standard DLC coating primarily consists of sp2- and sp3-hybridized carbon with a hydrogen content ranging from 10% - 40%. The DLC coating has a thickness of 1 -3 pm, providing moderate wear resistance and low surface roughness. The DLCcoating is deposited using PECVD or Sputtering techniques, ensuring uniform film coverage over the substrate.

[0053] The comparative analysis of the performance of the oil-free compressor without any coating, the oil-free compressor coated with standard Diamond-Like Carbon (DLC) coating, and the oil-free compressor coated with the exemplary multilayered coating 100 is provided in Table 1 below.<Table 1: Comparative analysis between the performance of the conventional oil- free compressor without any coating, and those with standard diamondlike carbon ( DLC ) coating, and multilayered coating 100

[0054] As it is very evident from the above table, the multilayered coating 100 offers various advantages over the uncoated compressor and the compressor with the DLC coating. The multilayered coating 100 improves compressor efficiency by up to 20% compared to the uncoated compressor and about 10% compared to the compressor with the DLC coatings. Furthermore, the multilayered coating 100 excels in thermal management, increasing the maximum operating temperature by 70°C and improving thermal management efficiency by 25 percentage points. Maintenance intervals are also significantly extended, with intervals tripled and operational lifespan extended by 5-10 years. The multilayered coating 100 renders the compressor energy -efficient, reducing power consumption by 25% compared to uncoated compressor and 17% compared to compressor with standard DLC coatings. Finally, the multilayered coating 100 exhibits an improved heat dissipation rate, more than doubling the rate compared to uncoated compressor, allowing for efficient operation in demanding conditions.

[0055] In another exemplary embodiment, a comparative analysis between the performance of the compressor without any coating versus a compressor including multilayered coating 100 with (i) gradient coating from the base layer 102, followed by intermediate layer 104 to the top layer 106, without any microchannels, and (ii) compressor with gradient coating including microchannels and wear management system microchannels only, has been provided in Table 2 below:Table 2: Comparative analysis between the performance of the conventional oil- free compressor without any coating, and those with (i) multilayered coating 100, and (it) multilayered coating 100 including microchannels and wear management system microchannels

[0056] Table 2 indicates that at least 10% improvement in efficiency is observed in a compressor comprising the multilayered coating 100 compared to the compressor without any coating. Additionally, a 100% increase in maintenance intervals and 50% increase in operational lifespan is observed in the compressor comprising the multilayered coating 100. Thus, the multilayered coating 100 significantly improves the efficiency, wear resistance, and thermal management of the compressor.

[0057] The compressor comprising the multilayered coating 100 including the one or more microchannels 108 and the wear management system showed at least 25% improvement in efficiency as compared to the compressor without any coating. Further, a 90% reduction in wear rate, and an operational temperature range extension of at least 70°C with 200% increase in maintenance intervals is observed. Thus, the inclusion of one or more microchannels 108 and the wear managementsystem in the multilayered coating 100 synergistically improves the efficiency, wear resistance, and thermal management of the compressor.

[0058] It will be apparent to those skilled in the art that various modifications and variations can be made to the method and / or system of the present disclosure without departing from the scope of the disclosure. Other embodiments will be apparent to those skilled in the art from consideration of the specification and practice of the method and / or system disclosed herein. It is intended that the specification and examples be considered as exemplary only, with a true scope of the disclosure being indicated by the following claims and their equivalent.List of Elements100 multilayered coating102 base layer104 intermediate layer106 top layer108 microchannels110 substrate120 system122 sensing circuit122' sensing unit

Claims

We Claim:

1. A multilayered coating 100 for a substrate 110 comprising:- a base layer 102 including doped diamond crystals, the base layer 102 being electrically conductive and configured to indicate detectable change in electrical conductivity upon wearing of one or more layers of the multilayered coating 100;- an intermediate layer 104 disposed on the base layer 102, the intermediate layer 104 comprising of microcrystalline and nanocrystalline diamonds; and- a top layer 106 including nanocrystalline diamonds.

2. The multilayered coating 100 as claimed in claim 1, wherein the multilayered coating 100 includes one or more microchannels 108 extending from the top layer 106 to at least a part of the intermediate layer 104, the one or more microchannels 108 having a width ranging from 10 to 500 pm and a depth ranging from 5 to 60 pm.

3. The multilayered coating 100 as claimed in claim 2, wherein the one or more microchannels 108 are configured to receive and / or circulate a working fluid selected from the group consisting of a cooling fluid, a lubricant and a multifunctional fluid that provides both cooling and lubrication.

4. The multilayered coating 100 as claimed in claim 1, wherein the base layer 102 includes diamond crystals doped with a dopant selected from the group consisting of boron, nitrogen, and phosphorus.

5. The multilayered coating 100 as claimed in claim 1 or 4, wherein the base layer 102 has a doping concentration ranging from 1019atoms / cm3to 1021atoms / cm3.

6. The multilayered coating 100 as claimed in claim 1, wherein the base layer 102 comprises of doped diamond crystals having a grain size ranging from 500 nm to 10 pm.

7. The multilayered coating 100 as claimed in claim 1, wherein the base layer 102 has a thickness ranging from 1 to 10 pm.

8. The multilayered coating 100 as claimed in claim 1, wherein the intermediate layer 104 comprises of microcrystalline diamonds having a grain size ranging from 100 to 500 nm and nanocrystalline diamonds having a grain size ranging from 50 to 100 nm.

9. The multilayered coating 100 as claimed in claim 1, wherein the intermediate layer 104 has a thickness ranging from 5 to 50 pm.

10. The multilayered coating 100 as claimed in claim 1, wherein the intermediate layer 104 has:- a hardness of at least 90 GPa; and- a thermal conductivity of at least 2000 W / mK at 25°C.

11. The multilayered coating 100 as claimed in claim 1 , wherein the top layer 106 comprises of nanocrystalline diamonds having a grain size ranging from 2 to 100 nm.

12. The multilayered coating 100 as claimed in claim 1, wherein the top layer 106 has a thickness ranging from 1 to 10 pm.

13. The multilayered coating 100 as claimed in claim 1 , wherein the top layer 106 has:- a coefficient of friction less than 0.1.

14. The multilayered coating 100 as claimed in claim 2, wherein the one or more microchannels 108 are arranged concentrically, parallelly, or randomly.

15. The multilayered coating 100 as claimed in claim 1, comprising a continuous gradient transition from the base layer 102 to the top layer 106.

16. A coated article comprising:- a substrate 110; and- the multilayered coating 100 covering at least a portion of the substrate 110, the multilayered coating 100 comprising:a base layer 102 including doped diamond crystals, the base layer 102 being electrically conductive and configured to indicate detectable change in electrical conductivity upon wearing of one or more layers of the multilayered coating 100;an intermediate layer 104 disposed on the base layer 102, the intermediate layer 104 comprising of microcrystalline and nanocrystalline diamonds; andatop layer 106 including nanocrystalline diamonds.

17. A system 120 comprising:- a coated article as claimed in claim 16; and- a sensing circuit 122;wherein the coated article is connected to the sensing circuit 122 at the base layer 102 of the multilayered coating 100 and the sensing circuit 122 is configured to detect wearing of the multilayered coating 100 by detecting any difference in electrical conductivity of the multilayered coating 100.

18. A method for producing a multilayered coating 100 on a substrate 110, the method comprising the steps of:(a) preparing the substrate 110 for deposition of diamond thereon;(b) depositing a base layer 102 including doped diamond crystals on at least a portion of at least one surface of the substrate 110 using a diamond deposition technique;(c) varying one or more deposition process parameters of the diamond deposition technique to deposit an intermediate layer 104 on the base layer 102, the intermediate layer 104 including microcrystalline and nanocrystalline diamonds; and(d) further varying the one or more deposition process parameters of the diamond deposition technique to deposit a top layer 106 on the intermediate layer 104, the top layer 106 including nanocrystalline diamonds,wherein the diamond deposition is monitored in real time using a monitoring system and upon detecting a deviation in the growth of the one or more layers of multilayered coating 100, an automatic feedback is generated for adjusting the one or more deposition parameters based on the automatic feedback from the monitoring system.

19. The method as claimed in claim 18, comprising forming one or more microchannels 108 in the multilayered coating 100 extending from the top layer 106 to at least a part of the intermediate layer 104 by using one or more of a laser ablation technique and a plasma etching technique.

20. The method as claimed in claim 18, comprising forming the one or more microchannels 108 in situ during the deposition of the intermediate layer 104 and the top layer 106 using a masking template that is removed sacrificially upon formation of the top layer 106.

21. The method as claimed in claim 18, wherein varying the one or more deposition process parameters in step (c) comprises varying one or more of gas composition, gas flow rate, reactor temperature, reactor pressure,microwave power, substrate bias voltage, plasma density, deposition rate, and dopant concentration.

22. The method as claimed in claim 18, wherein varying the one or more deposition process parameters in step (d) comprises varying one or more of gas composition, gas flow rates, reactor temperature, reactor pressure, microwave power, substrate bias voltage, plasma density, deposition rate, and ion bombardment energy.