A method and an assembly for producing virgin carbon black from treated recovered pyrolysis materials

The method and assembly for producing virgin carbon black from treated pyrolysis materials address environmental and economic challenges by using waste tire pyrolysis to create high-quality carbon black with enhanced properties, reducing emissions and promoting a circular economy.

WO2026234432A1PCT designated stage Publication Date: 2026-11-12MYNAMPATI HARIKRISHNA MURLIDHAR
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/IB2025/056492
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-08
Filing Date
2025-06-26
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Traditional carbon black production methods are energy-intensive, emit high greenhouse gases, and rely on non-renewable feedstocks, posing environmental and economic challenges, with byproducts contributing to air pollution and resource scarcity.

Method used

A method and assembly for producing virgin carbon black from treated recovered pyrolysis materials, involving oxygen-deficient tire pyrolysis, thermal processing to reduce moisture, mechanical milling for particle size, blending with tire pyrolysis oil, and controlled oxidation in a furnace reactor to activate ash components like zinc and silica.

Benefits of technology

This approach yields high-quality carbon black with enhanced properties, reduces emissions, and promotes a circular economy by utilizing waste materials efficiently, increasing yield and scalability while minimizing environmental impact.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure IB2025056492_12112026_PF_FP_ABST
    Figure IB2025056492_12112026_PF_FP_ABST
Patent Text Reader

Abstract

A method and an assembly for producing virgin carbon black from treated recovered pyrolysis materials is disclosed. The method includes generating the recovered carbon black from the tire pyrolysis in an oxygen-deficient environment, producing the recovered carbon black, gas, and tire pyrolysis oil. The recovered carbon black is then thermally treated using industrial equipment to reduce moisture content below 0.5%, preventing undesirable reactions. Further, the dried recovered carbon black is milled to a target particle size for dispersion or downstream processing. The milled recovered carbon black is blended with tire pyrolysis oil in a predefined ratio using a mechanical mixer to form a homogeneous mixture. This mixture is transferred to a reactor, where virgin carbon black is formed via oxidation of various components, including zinc and silica-based ash. The method enables conversion of waste tire materials into high-value virgin carbon black suitable for industrial applications.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] A METHOD AND AN ASSEMBLY FOR PRODUCING VIRGIN CARBON BLACK FROM TREATED RECOVERED PYROLYSIS MATERIALS

[0002] EARLIEST PRIORITY DATE:

[0003] This Application claims priority from a complete patent application filed in India having Patent Application No. 202521044816, filed on 08th day of May 2025, and titled “A METHOD AND AN ASSEMBLY FOR PRODUCING VIRGIN CARBON BLACK FROM TREATED RECOVERED PYROLYSIS MATERIALS”.

[0004] FIELD OF INVENTION

[0005] Embodiments of the present disclosure relate to the field of chemical manufacturing and petrochemical and more particularly a method and an assembly for producing virgin carbon black from treated recovered pyrolysis materials.

[0006] BACKGROUND

[0007] A carbon black is a fine black powder made from the incomplete combustion of heavy petroleum products including fluid catalytic cracking (FCC) tar, coal tar, and ethylene cracking tar. It is a critical industrial material used primarily as a reinforcing agent in rubber products, especially tires, and as a black pigment in inks, coatings, and plastics. The global demand for carbon black continues to grow due to its indispensable role in the automotive and manufacturing sectors. However, the traditional production of carbon black is energy-intensive and contributes significantly to greenhouse gas emissions and other pollutants, making it a subject of environmental concern.

[0008] Typically, the most prevalent method of producing carbon black is the furnace black process, where hydrocarbons are combusted in a limited oxygen environment,generating soot that is collected and processed. Additionally, the other traditional methods include the channel process, acetylene black process, and thermal black process. Among these, the furnace black method is dominant due to its scalability and cost-effectiveness. These methods typically use fossil fuels as feedstock and operate at very high temperatures, which are energy-intensive and result in the release of large amounts of CO2and particulate matter.

[0009] While the existing production methods are effective in producing high-quality carbon black, they suffer from several environmental and economic drawbacks. The significant drawbacks includes a high energy consumption, significant greenhouse gas emissions, and reliance on non-renewable feedstocks which are an area of major concerns. Additionally, the process generates harmful byproducts including sulphur oxides and nitrogen oxides, contributing to air pollution and environmental degradation. Furthermore, the fluctuations in the price and availability of petroleum-based feedstocks pose economic challenges for manufacturers.

[0010] In response to these challenges, there exists a need to address these challenges and provide a solution which includes the methods adapted to shift toward a sustainable and an eco-friendly production. One promising solution lies in the exploration of alternative, more sustainable raw materials and cleaner energy sources for carbon black production. By shifting away from traditional fossil-based inputs, this approach aims to reduce environmental impact while addressing issues related to resource scarcity and waste generation. Additionally, incorporating circular economy principles including utilizing by-products or renewable materials, can contribute to a more responsible production cycle. Furthermore, ongoing advancements in process optimization and energy efficiency are paving the way for methods that lower emissions and overall energy consumption. These efforts collectively strive to make carbon black production more environmentally sustainable without compromising product quality or industrial performance.Hence, there is a need for an improved a method and an assembly for producing virgin carbon black from treated recovered pyrolysis materials which addresses the aforementioned issue(s).

[0011] OBJECTIVES OF THE INVENTION

[0012] The primary objective of this invention is to provide a method and an assembly for producing virgin-grade carbon black from recovered carbon black and tire pyrolysis oil. The process aims to utilize sustainable feedstock while delivering high-quality carbon black comparable to industrial standards.

[0013] Another objective of the invention is to overcome the quality limitation of the recovered carbon black because of its ash content (zinc & silica). Typically, these ash contents are usually considered as contaminants, but in the illustrated invention these components will undergo oxidation in furnace black reactor resulting to the production of virgin carbon black with unique properties.

[0014] Yet another objective of the invention is to improve the quality of recovered carbon black by reducing its moisture content to below 0.5% and achieving a fine particle size utilizing a bead milling technique. These processes ensure optimal blending and combustion characteristics during the production.

[0015] Yet another objective of the invention is introducing a controlled and efficient blending method, combining the tire pyrolysis oil and the recovered carbon black in a predetermined weight ratio using a mechanical blender and dispersing additive. This homogenized blend is then processed in a furnace black reactor, offering an innovative and environmentally conscious route to virgin carbon black synthesis.BRIEF DESCRIPTION

[0016] In accordance with an embodiment of the present disclosure, a method for producing virgin carbon black from treated recovered pyrolysis materials is disclosed. The method includes generating a recovered carbon black from a tire pyrolysis utilizing a recovery unit, wherein the tire pyrolysis is performed in an oxygen-deficient environment to produce a plurality of substances including at least one of a tire pyrolysis oil, a gas, and the recovered carbon black. Additionally, the method includes heating the recovered carbon black by utilizing at least one of a plurality of industrial thermal processing equipment to minimize its moisture content to less than 0.5% to prevent an undesirable reaction, wherein the industrial thermal processing equipment is adapted to apply a thermal energy to dry a raw material and remove moisture content. Furthermore, the method includes milling the recovered carbon black by utilizing at least one of a mechanical grinding apparatus to achieve a predetermined particle size suitable for at least one of a dispersion and downstream processing. Moreover, the method includes blending the recovered carbon black and the tire pyrolysis oil using a mechanical mixer equipped with a stirrer in a predetermined weight ratio to formulate a blended mixture, wherein the blending is done for a predetermined duration to achieve a blended homogeneous mixture. Moreover, the method includes transferring the blended mixture into a reactor adapted to facilitate a virgin carbon black formation in response to an oxidation of a plurality of components within the blended mixture, wherein the oxidation of plurality of components comprises an ash component of a zinc and silica.

[0017] In accordance with another embodiment of the present disclosure, an assembly for producing virgin carbon black from treated recovered pyrolysis materials is disclosed. The assembly includes a recovery unit adapted to generate a recovered carbon black from a tire pyrolysis, wherein the tire pyrolysis is performed in an oxygen-deficient environment to produce a plurality of substances including at least one of a tire pyrolysis oil, a gas, and the recovered carbon black. Additionally, theassembly includes a plurality of industrial thermal processing equipment adapted to heat the recovered carbon black to minimize its moisture content to less than 0.5% to prevent an undesirable reaction, wherein the industrial thermal processing equipment is adapted to apply a thermal energy to dry a raw material and remove moisture content. Furthermore, the assembly includes a mechanical grinding apparatus operable to mill the recovered carbon black to achieve a predetermined particle size suitable for at least one of a dispersion and downstream processing. Moreover, the assembly includes a mechanical mixer equipped with a stirrer adapted to blend the recovered carbon black and the tire pyrolysis oil in a predetermined weight ratio to formulate a blended mixture, wherein the blend is performed for a predetermined duration to achieve a blended homogeneous mixture. Moreover, the assembly includes a reactor utilized to accommodate the blended mixture and facilitate a virgin carbon black formation in response to an oxidation of a plurality of components within the blended mixture, wherein the oxidation of plurality of components comprises an ash component of a zinc and silica.

[0018] To further clarify the advantages and features of the present disclosure, a more explicit description of the disclosure will follow by reference to specific embodiments thereof, which are illustrated in the appended figures. It is to be appreciated that these figures depict typical embodiments of the disclosure and are therefore not to be considered limiting in scope. The disclosure will be described and explained with additional details with the appended figures.

[0019] BRIEF DESCRIPTION OF THE DRAWINGS

[0020] The disclosure will be described and explained with additional specificity and detail with the accompanying figures in which:FIG. 1 is a flow chart representing the steps involved in a method for producing virgin carbon black from treated recovered pyrolysis materials in accordance with an embodiment of the present disclosure;

[0021] FIG. 2 is a block diagram representation of an assembly for producing virgin carbon black from treated recovered pyrolysis materials with an embodiment of the present disclosure; and

[0022] FIG. 3 is a circular flow diagram of a cyclic process associated with an assembly for producing virgin carbon black from treated recovered pyrolysis materials with an embodiment of the present disclosure.

[0023] Further, those skilled in the art will appreciate that elements in the figures are illustrated for simplicity and may not have necessarily been drawn to scale. Furthermore, in terms of the construction of the device, one or more components of the device may have been represented in the figures by conventional symbols, and the figures may show only those specific details that are pertinent to understanding the embodiments of the present disclosure so as not to obscure the figures with details that will be readily apparent to those skilled in the art having the benefit of the description herein.

[0024] DETAILED DESCRIPTION

[0025] For the purpose of promoting an understanding of the principles of the disclosure, reference will now be made to the embodiment illustrated in the figures and specific language will be used to describe them. It will nevertheless be understood that no limitation of the scope of the disclosure is thereby intended. Such alterations and further modifications in the illustrated system, and such further applications of the principles of the disclosure as would normally occur to those skilled in the art are to be construed as being within the scope of the present disclosure.The terms "comprises", "comprising", or any other variations thereof, are intended to cover a non-exclusive inclusion, such that a process or method that comprises a list of steps does not include only those steps but may include other steps not expressly listed or inherent to such a process or method. Similarly, one or more devices or sub-systems or elements or structures or components preceded by "comprises... a" does not, without more constraints, preclude the existence of other devices, sub-systems, elements, structures, components, additional devices, additional sub-systems, additional elements, additional structures, or additional components. Appearances of the phrase "in an embodiment", "in another embodiment" and similar language throughout this specification may, but not necessarily do, all refer to the same embodiment.

[0026] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this disclosure belongs. The system, methods, and examples provided herein are only illustrative and not intended to be limiting.

[0027] In the following specification and the claims, reference will be made to a number of terms, which shall be defined to have the following meanings. The singular forms “a”, “an”, and “the” include plural references unless the context clearly dictates otherwise.

[0028] In accordance with an embodiment of the present disclosure, a method for producing virgin carbon black from treated recovered pyrolysis materials is disclosed. The method includes generating a recovered carbon black from a tire pyrolysis utilizing a recovery unit, wherein the tire pyrolysis is performed in an oxygen-deficient environment to produce a plurality of substances including at least one of a tire pyrolysis oil, a gas, and the recovered carbon black. Additionally, the method includes heating the recovered carbon black by utilizing at least one of a plurality of industrial thermal processing equipment to minimize its moisture content to less than 0.5% to prevent an undesirable reaction, wherein the industrial thermal processing equipment is adapted to apply a thermal energy to dry a rawmaterial and remove moisture content. Furthermore, the method includes milling the recovered carbon black by utilizing at least one of a mechanical grinding apparatus to achieve a predetermined particle size suitable for at least one of a dispersion and downstream processing. Moreover, the method includes blending the recovered carbon black and the tire pyrolysis oil using a mechanical mixer equipped with a stirrer in a predetermined weight ratio to formulate a blended mixture, wherein the blending is done for a predetermined duration to achieve a blended homogeneous mixture. Moreover, the method includes transferring the blended mixture into a reactor adapted to facilitate a virgin carbon black formation in response to an oxidation of a plurality of components within the blended mixture, wherein the oxidation of plurality of components comprises an ash component of a zinc and silica.

[0029] FIG. 1 is a flow chart representing the steps involved in a method for producing virgin carbon black from treated recovered pyrolysis materials in accordance with an embodiment of the present disclosure. The treated recovered pyrolysis material provides a plurality of substances including the recovered carbon black and the tire pyrolysis oil. Typically, the tire pyrolysis is a process that heats the used tires in the absence of oxygen to break them down into smaller chemical compounds. It produces useful byproducts like oil, gas, carbon black, and scrap steel. This tire pyrolysis helps recycle waste tires and recover energy and materials for industrial reuse. The tire pyrolysis oil is derived from waste tire pyrolysis. The recovered carbon black, derived from tire pyrolysis, typically contains 16–21% ash including zinc and silica and requires a pre-treatment including a plurality of steps through moisture removal and milling. These steps enhance its quality and suitability for industrial reuse in rubber, plastics, and coatings.

[0030] The method (100) includes generating a recovered carbon black from a tire pyrolysis utilizing a recovery unit, wherein the tire pyrolysis is performed in an oxygen-deficient environment to produce a plurality of substances comprising atleast one of a tire pyrolysis oil, a gas, and the recovered carbon black in the step (105).

[0031] The tire pyrolysis is conducted in a sealed, oxygen-deficient reactor where high temperature thermally decompose the tire material. The absence of oxygen prevents combustion, allowing the tires to break down into tire pyrolysis oil, syngas, and a solid carbon-rich residue. These byproducts are then separated and collected for further processing or reuse. Additionally, the recovery unit is adapted to extract recovered carbon black from the solid residue of tire pyrolysis by employing a combination of cooling, cyclone separation, and filtration. This process ensures efficient separation and purification of recovered carbon black for reuse, forming a key component in sustainable tire recycling mechanism.

[0032] The method (100) includes heating the recovered carbon black by utilizing at least one of a plurality of industrial thermal processing equipment to minimize its moisture content to less than 0.5% to prevent an undesirable reaction, wherein the industrial thermal processing equipment is adapted to apply a thermal energy to dry a raw material and remove moisture content in the step (110).

[0033] The recovered carbon black from tire pyrolysis often contains residual moisture, which can cause undesirable reactions during storage or further use. To prevent this, the recovered carbon black is subjected to thermal drying using industrial thermal processing equipment including rotary dryers, fluidized bed dryers, and flash dryers. These equipment’s are designed to apply controlled thermal energy to efficiently evaporate moisture from the material. The process of heating ensures that the moisture content is reduced to below 0.5%, stabilizing the recovered carbon black for safe handling and downstream applications. Additionally, the drying of the raw material associated with the recovered carbon black is essential to enhance the quality, consistency, and performance in industrial reuse including rubber and plastics manufacturing. Typically, it is not desired to have any water content in the raw material as it leads to moisture formation and results in an undesired reaction.The recovered carbon black is hygroscopic by nature and its properties so to minimize the moisture content and keep it below 0.5 percent this heating is done.

[0034] In one embodiment, a controlled heat is applied to minimize the moisture content of the recovered carbon black for improved processing and performance by utilizing a rotatory drum heater pertaining to the plurality of industrial thermal processing equipment. The rotary drum heater applies controlled, uniform heat while continuously tumbling the recovered carbon black to effectively reduce its moisture content. This motion-enhanced heating ensures even drying and prevents clumping, lowering moisture below 0.5% for improved handling and performance. The utilization of the rotary drum heater is adapted with some salient features including its energy efficiency, consistent output quality, and suitability for large-scale industrial drying of fine powders including the recovered carbon black.

[0035] The method (100) includes milling the recovered carbon black by utilizing at least one of a mechanical grinding apparatus to achieve a predetermined particle size suitable for at least one of a dispersion and downstream processing in the step (115). The recovered carbon black is milled using a mechanical grinding apparatus wherein the mechanical grinding apparatus include at least but not limited to one of a jet mill, ball mill, and hammer mill to reduce the recovered carbon black particle’s size to a fine and uniform particle size. A grinding process enhances surface area and consistency, which are critical for effective dispersion in materials like rubber, plastics, and inks. This milling process is essential for upgrading the raw recovered carbon black into a high-quality filler material that meets industrial standards. Additionally, the finely milled recovered carbon black will disperse better in the tire pyrolysis oil or other feedstock such as FCC, EBO etc that is used to produce virgin carbon black.

[0036] In one embodiment, a minimized particle size of the recovered carbon black is obtained utilizing a bead milling machine associated with the mechanical grinding apparatus. The bead milling machine utilizes high-speed rotating beads to grind recovered carbon black into ultra-fine particles through intense shear and impactforces. The bead milling machine is effective for achieving a highly uniform and minimized particle size, ideal for applications requiring superior dispersion. A closed unit prevents contamination and allows precise control over temperature and grinding time. Therefore, utilizing the bead milling machine significantly improves the recovered carbon black performance in high-end applications including coatings, inks, and advanced polymer composites.

[0037] In another embodiment, the reduced particle size of the recovered carbon black is adapted to be less than forty microns to enhance dispersion and performance in downstream applications. The method and the assembly is not limited to forty microns and adapted to be scalable to achieve further reduction much below forty microns, depending on processing requirements. This enables flexibility for use in various high-precision industries requiring fine particulate materials.

[0038] The method (100) includes blending the recovered carbon black and the tire pyrolysis oil using a mechanical mixer equipped with a stirrer in a predetermined weight ratio to formulate a blended mixture, wherein the blending is done for a predetermined duration to achieve a blended homogeneous mixture in the step (120).

[0039] The recovered carbon black and the tire pyrolysis oil are combined in the mechanical mixer equipped with the stirrer, operated at controlled speed and duration. Additionally, in a predetermined weight ratio a blended mixture is prepared for the recovered carbon black and the tire pyrolysis oil to ensure optimal interaction between the solid and liquid components. The mixing process applies continuous shear and agitation to uniformly disperse the recovered carbon black particles within the tire pyrolysis oil. Furthermore, the blending is carried out for a specific time to achieve a homogeneous, stable mixture without phase separation. Moreover, at least a one of dispersing additives can be added at this stage to improve dispersion of the recovered carbon black in the tire pyrolysis oil. This is done toenhance handling, transport, and further processing of the mixture, and enabling use in fuel blends and material formulations.

[0040] In one embodiment, the method (100) utilizes at least one of mechanical mixer including a badge type of dryer. The badge type of dryer includes an agitator, wherein the recovered carbon black and the tyre pyrolysis oil is adapted to put on the agitator. The recovered carbon black and the tyre pyrolysis oil are blended in a predetermined weight ratio for a specific duration utilizing the agitator.

[0041] In one embodiment, the predetermined weight ratio of the blended mixture is 100:75 for the tire pyrolysis oil to the recovered carbon black by weight. The blending is performed in a predetermined weight ratio, illustratively 100:75 for the tire pyrolysis oil to the recovered carbon black ensuring uniform dispersion and stable consistency. However, this ratio is not limited to 100:75 and is variable within a feasible range from 100: 10 to other suitable proportions. The selected ratio can be adjusted based on desired material characteristics and application-specific requirements. In general, it can be illustrated that the predetermined weight ratio for the tire pyrolysis oil to the recovered carbon black can be scaled up and generalized in a M: N weight ratio, wherein M represents the weighted ratio for the tire pyrolysis oil and the N represents the weighted ratio for the recovered carbon black, wherein M and N be the whole number values ranging from 0 to 100.

[0042] In one embodiment, the blended mixture is mixed for the predetermined duration of 30 minutes based on process conditions and desired material properties. The blended mixture is mixed for a predetermined duration and based on the present illustration it is 30 minutes, to achieve uniform dispersion and material consistency. However, this duration is not limited to 30 minutes and may be scaled based on specific process parameters. The mixing duration can vary depending on factors including material viscosity, batch size, and equipment capacity. This flexibility ensures the blend meets the required performance characteristics for downstream applications.In one embodiment, the tire pyrolysis oil is pre-filtered to remove particulate contaminants prior to the blending process. The pre-filtering of the tire pyrolysis oil is essential to remove particulate contaminants that could interfere with the uniform blending of recovered carbon black. This not only improves the stability, consistency, and quality of the final blended mixture but also prevents equipment wear and ensures better performance in downstream applications.

[0043] In one embodiment, a dispersing of the recovered carbon black in the tire pyrolysis oil is obtained utilizing the mechanical mixer (240) adapted with a high-shear blade. The recovered carbon black is dispersed into the tire pyrolysis oil utilizing the mechanical mixer equipped with the high-shear blade. The high-shear blade is designed to generate intense mixing forces, effectively breaking down agglomerates and ensuring fine particle dispersion. It is ideal for creating uniform, stable mixtures in viscous or multi-phase materials like recovered carbon black in pyrolysis oil. Additionally, the high-shear blade generates intense mixing forces that break down particle clusters and promote uniform distribution. This dispersion helps in improving a consistent and homogeneous mixture with improved stability and reduced sedimentation.

[0044] In one embodiment, the blending process is carried out under an inert atmosphere to minimize oxidation. The blending process is carried out under an inert atmosphere including at least one of a nitrogen and argon to minimize exposure to oxygen. This prevents oxidation of the tire pyrolysis oil and recovered carbon black, which could degrade material quality. Additionally, maintaining an inert environment helps preserve the chemical stability and performance of the blend. It is especially critical for ensuring safe processing and extending the shelflife of the final blended mixture.

[0045] In one embodiment, the blending process utilizes at least one a plurality of additive substances comprising sodium lignosulphonate, wherein the plurality of additive substances are adapted to provide a uniform blend and consistency to the blended mixture. These additives act as dispersants or binders, improving the interactionbetween recovered carbon black and tire pyrolysis oil. Additionally, other potential additives include stearic acid, polyethylene glycol, and surfactants like nonylphenol ethoxylate utilized depending on the desired blend properties. The utilization of sodium lignosulphonate is recommended but not limited to a two percent proportion in the blended mixture for optimum results.

[0046] The method (100) includes transferring the blended mixture into a reactor adapted to facilitate a virgin carbon black formation in response to an oxidation of a plurality of components within the blended mixture, wherein the oxidation of plurality of components comprises an ash component of a zinc and silica in the step (125). The blended mixture is transferred into a specialized reactor designed to initiate controlled oxidation of various components, including ash constituents like zinc and silica. The reactor utilized is at least one of a including a furnace black reactor. Within the reactor, an elevated temperature and oxygen exposure trigger chemical reactions that facilitate the formation of virgin carbon black. This process transforms the blended material into a higher-purity carbon product with enhanced functional properties. Significantly, the overall method (100) enables value-added recovery from waste materials by generating a refined carbon black suitable for high-performance applications. The oxidation process in the furnace black reactor activates the ash components including zinc and silica, enhancing the reinforcement properties of the resulting virgin carbon black.

[0047] Additionally, in conventional methods of utilizing recovered carbon black the zinc and silica are usually treated as a contaminant and hinderance for selling the recovered carbon black. In the proposed illustration in the recovered carbon black usually the chemicals utilized are zinc oxide and silica di oxide. In pyrolysis process all these oxygen bonds are removed. Further, during the production of virgin carbon black when the recovered carbon black is mixed with tire pyrolysis oil the resultant blended mixture undergoes a partial combustion process where the zinc and silica get sufficient oxygen to bind up and get convert again to silica di oxide and zinc oxide.In one embodiment, the produced virgin carbon black includes but not limited to at least one of a grade selected from N330, N220, N375, N550, N660, N772 etc. The N330, N220, and N375 are types of virgin carbon black with varying properties and applications in rubber and tire manufacturing industries. The N330 offers good reinforcement, abrasion resistance, and tensile strength. The N220 provides enhanced abrasion resistance, tensile strength, and heat-up / hardness compared to N330, and is conductive. The N375 is a general -purpose grade suitable for various applications where balanced properties are needed.

[0048] In one embodiment, the utilization of tire pyrolysis oil alone presents challenges due to its low specific gravity (0.92), which results in a lower yield and reduced commercial viability. The proposed method (100) by utilizing the blended mixture by blending the recovered carbon black with tire pyrolysis oil to create a high- specific-gravity (1.15) that enhances yield, creates a more viable market for pyrolysi byproducts, and optimizes the activation of zinc and silica during furnace black processing, leading to superior carbon black production for use in rubber formulations. The increase in specific gravity for virgin carbon black indicates higher material density, which can improve reinforcement properties in rubber and polymer applications. Additionally, it helps in reduced increased porosity of the virgin carbon black, leading to better dispersion and consistency in final product formulations.

[0049] In one embodiment, the yield of the produced virgin carbon black is adapted to be increased by at least six percent compared to using the tire pyrolysis oil alone. This enhancement results from the improved composition and reactivity of the blend, leading to more efficient carbon formation.

[0050] In one embodiment, the recovered carbon black, production is scalable and enhanced through diversification of feedstock sources and flexible integration into multiple industrial pathways. The recovered carbon black can be blended with conventional fossil-based feedstocks, offering a direct drop-in solution for existingcarbon black production methods. Additionally, the emergence of bio-based recovered carbon black produced via pyrolysis of bio-waste provides a renewable alternative that can be integrated with bio-based pyrolysis oil, supporting sustainable and circular production models. Furthermore, the recovered carbon black in the existing illustration, derived from end-of-life tire pyrolysis can also be utilized alongside fossil or bio-based feedstocks, further broadening its applicability. These multiple sourcing and blending strategies significantly increase the potential for scaling the recovered carbon black production, making it a viable and flexible component in both conventional and next-generation carbon black manufacturing processes.

[0051] In a non-limiting example, consider a scenario, where a startup company in the city thought of a circular economy and has decided to adopt the disclosed a method and an assembly for producing virgin carbon black from treated recovered pyrolysis materials to create a closed-loop solution for waste tires. The company sources end-of-life tires from across different area and processes them in an oxygen-deficient pyrolysis unit to extract tire pyrolysis oil, gas, and recovered carbon black. This carbon black is then dried in a fluidized bed dryer to reduce its moisture content to below 0.5%, ensuring chemical stability and process efficiency. The dried material is then milled using a bead milling machine to achieve a uniform particle size ideal for use in rubber compounding. After milling, the recovered carbon black is blended with tire pyrolysis oil in a predetermined specific weight ratio using a mechanical mixer, wherein the mechanical mixer is a high-torque industrial mixer, creating a homogeneous mixture over a fixed blending period. This mixture is fed into a specialized oxidation reactor including a furnace black reactor where the controlled oxidation of zinc and silica-based ash components facilitates the formation of high-purity virgin carbon black. The resulting product is then supplied to the tire and rubber manufacturers who prefer sustainable raw materials. By using this method, the startup not only diverts tires from landfills but also offers a lower-emission alternative to traditional carbon black, cutting production emissions and raw material costs, while promoting greener manufacturing across the supply chain.FIG. 2 is a block diagram representation of an assembly for producing virgin carbon black from treated recovered pyrolysis materials with an embodiment of the present disclosure. The assembly (200) includes a recovery unit (210) adapted to generate a recovered carbon black from a tire pyrolysis, wherein the tire pyrolysis is performed in an oxygen-deficient environment to produce a plurality of substances comprising at least one of a tire pyrolysis oil, a gas, and the recovered carbon black. The recovery unit (210) is adapted to utilize a plurality of filters and separators to isolate the solid recovered carbon black from gases and oils. Additionally, the recovery unit (210) includes a cooling mechanism helps condense volatile substances, leaving behind solid carbon black. Furthermore, the recovery unit (210) is coupled with at least one of a cyclone and centrifuges adapted to help condense volatile substances, leaving behind solid recovered carbon black.

[0052] The assembly (200) includes a plurality of industrial thermal processing equipment (220) adapted to heat the recovered carbon black to minimize its moisture content to less than 0.5% to prevent an undesirable reaction, wherein the industrial thermal processing equipment is adapted to apply a thermal energy to dry a raw material and remove moisture content. The plurality of industrial thermal processing equipment (220), adapted to utilize the rotary drum heaters, wherein the rotary drum heaters apply controlled thermal energy to recovered carbon black to effectively reduce moisture content below 0.5%. The rotary drum heater utilizes its rotating cylindrical chamber, heated externally or internally, to ensure uniform heat distribution and continuous material agitation for optimal drying. This assembly (200) prevents undesirable reactions by minimizing residual moisture, leveraging the drum's motion and thermal transfer capabilities for efficient and consistent moisture removal.

[0053] The assembly (200) includes a mechanical grinding apparatus (230) operable to mill the recovered carbon black to achieve a predetermined particle size suitable for at least one of a dispersion and downstream processing. The mechanicalgrinding apparatus (230) is adapted to be utilized as a bead milling machine, wherein the bead milling machine is adapted to mill the recovered carbon black to achieve a fine, uniform particle size for optimal dispersion and downstream processing. The bead milling machine uses a high-speed rotating shaft and grinding media including beads within a sealed chamber to apply shear and impact forces to the material. This enables a continuous, controlled grinding, utilizing media agitation and a chamber pressure to produce particles of precise size and consistency.

[0054] The assembly (200) includes a mechanical mixer (240) equipped with a stirrer adapted to blend the recovered carbon black and the tire pyrolysis oil in a predetermined weight ratio to formulate a blended mixture, wherein the blend is performed for a predetermined duration to achieve a blended homogeneous mixture. The mechanical mixer (240) is coupled as a badge-type dryer adapted to use an integrated stirrer to blend recovered carbon black with tire pyrolysis oil in a specified weight ratio. The badge-type dryer includes a mixing chamber, wherein the mixing chamber is enclosed and ensures a controlled temperature and agitation, promoting uniform distribution of the tire pyrolysis oil over the recovered carbon black particles. Through timed mixing cycles, the stirrer creates a homogeneous blend, leveraging both mechanical shear and thermal conditioning for optimal mixture consistency.

[0055] The assembly (200) includes a reactor (250) utilized to accommodate the blended mixture and facilitate a virgin carbon black formation in response to an oxidation of a plurality of components within the blended mixture, wherein the oxidation of plurality of components comprises an ash component of a zinc and silica. The reactor (250), implemented as a furnace black reactor, is designed to thermally process the blended mixture under high-temperature oxidative conditions to generate virgin carbon black. Inside the reactor, controlled oxidation of components such as zinc and silica-containing ash occurs, initiating chemical reactions that restructure carbon-based compounds. The furnace black reactor features a high-temperature combustion zone, feed injection ports, and cooling sections to manage reaction kinetics and carbon black formation. This assembly (200) allows precise control over temperature, airflow, and residence time, ensuring consistent particle morphology and purity of the produced carbon black.

[0056] FIG. 3 is a circular flow diagram (300) of a cyclic process associated with an assembly for producing virgin carbon black from treated recovered pyrolysis materials with an embodiment of the present disclosure. The virgin carbon black is utilized as a raw material for production of tire and other commercially deemed rubber products (302). Once these tires are utilized to their full scale for commercial and other application (304). once the tires get degraded now the waste management is utilized and the proposed invention and the FIG.3 gives a cyclic picture of the recycling of the degraded tires (306). Now these degraded tires are pyrolyzed in an oxygen deficit environment, once the tires are not pyrolyzed it will be burnt as a fuel and result in a large production of carbon di oxide in the environment (308). Therefore, the tyre pyrolysis not only provides a renewable byproduct but also prevents environmental degradation. The tire pyrolysis gives a plurality of substances including the tire pyrolysis oil and recovered carbon black. The tire pyrolysis oil and recovered carbon black are heated and extracted and then blended to form a mixture (310). Further, in reactor this blended mixture produces a high quality virgin carbon black which can further be utilized as a raw material for manufacturing (312). This solution not only helps in generating a circular economy but also provide a solution in line with the sustainable development goals.

[0057] Various embodiments of the method and the assembly for producing virgin carbon black from treated recovered pyrolysis materials described above enable various advantages. Firstly, one major benefit is its higher yield, achieved through the increased specific gravity (1.15) of the blended mixture, which boosts carbon black yield by at least 6% compared to using the conventional tire pyrolysis oil alone. This improvement translates directly to enhanced economic viability, as it offers tire pyrolysis operations a profitable route to utilize recovered carbon black moreefficiently. The method also creates a viable direct application for the recovered carbon black in furnace black reactors, addressing long-standing market challenges. From an environmental perspective, this proposed method promotes sustainability by providing an alternative to petroleum-derived feedstocks and significantly reducing the carbon emissions traditionally linked with virgin carbon black production. Moreover, the activation of ash components like zinc and silica during the oxidation stage improves the resulting carbon black’s properties, especially for rubber formulations. By using industrial thermal processing equipment, the method ensures the recovered carbon black's moisture content remains below 0.5%, minimizing the risk of unwanted reactions. The milling process further refines particle size for enhanced dispersion and downstream applications. Through controlled blending of recovered carbon black and the tire pyrolysis oil, followed by processing in a specialized furnace black reactor, the method results in a consistent and a high-quality virgin carbon black as a product is achieved. Moreover, the use of existing infrastructure for implementation makes the process highly scalable with minimal capital investment. This innovation not only enhances production efficiency but also supports environmental responsibility and industry growth.

[0058] It will be understood by those skilled in the art that the foregoing general description and the following detailed description are exemplary and explanatory of the disclosure and are not intended to be restrictive thereof. While specific language has been used to describe the disclosure, any limitations arising on account of the same are not intended.

[0059] The figures and the forgoing description give examples of embodiments. Those skilled in the art will appreciate that one or more of the described elements may well be combined into a single functional element. Alternatively, certain elements may be split into multiple functional elements. Elements from one embodiment may be added to another embodiment. For example, the order of processes described herein may be changed and is not limited to the manner described herein. Moreover,the actions of any flow diagram need not be implemented in the order shown; nor do all the acts need to be necessarily performed. Also, those acts that are not dependent on other acts may be performed in parallel with the other acts. The scope of embodiments is by no means limited by these specific examples.

Claims

I CLAIM:

1. A method (100) for producing virgin carbon black from treated recovered pyrolysis materials comprising:characterized in that,generating a recovered carbon black from a tire pyrolysis utilizing a recovery unit, wherein the tire pyrolysis is performed in an oxygen-deficient environment to produce a plurality of substances comprising at least one of a tire pyrolysis oil, a gas, and the recovered carbon black; (105)heating the recovered carbon black by utilizing at least one of a plurality of industrial thermal processing equipment to minimize its moisture content to less than 0.5% to prevent an undesirable reaction, wherein the industrial thermal processing equipment is adapted to apply a thermal energy to dry a raw material and remove moisture content; (110)milling the recovered carbon black by utilizing at least one of a mechanical grinding apparatus to achieve a predetermined particle size suitable for at least one of a dispersion and downstream processing; (115)blending the recovered carbon black and the tire pyrolysis oil using a mechanical mixer equipped with a stirrer in a predetermined weight ratio to formulate a blended mixture, wherein the blending is done for a predetermined duration to achieve a blended homogeneous mixture; (120) andtransferring the blended mixture into a reactor adapted to facilitate a virgin carbon black formation in response to an oxidation of a plurality of components within the blended mixture, wherein the oxidation of plurality of components comprises an ash component of a zinc and silica (125)2. The method (100) as claimed in claim 1, wherein a controlled heat is applied to minimize the moisture content of the recovered carbon black for improved processing and performance by utilizing a rotatory drum heater pertaining to the plurality of industrial thermal processing equipment (220).

3. The method (100) as claimed in claim 1, wherein a minimized particle size of the recovered carbon black is obtained utilizing a bead milling machine associated with the mechanical grinding apparatus (230).

4. The method (100) as claimed in claim 1, wherein the predetermined weight ratio of the blended mixture is 100:75.

5. The method (100) as claimed in claim 1, wherein the blended mixture is mixed for the predetermined duration of 30 minutes based on process conditions and desired material properties.

6. The method (100) as claimed in claim 1, wherein the tire pyrolysis oil is pre-filtered to remove particulate contaminants prior to the blending process.

7. The method (100) as claimed in claim 1, wherein a dispersing of the recovered carbon black in the tire pyrolysis oil is obtained utilizing the mechanical mixer (240) adapted with a high-shear blade.

8. The method (100) as claimed in claim 1, wherein the blending process is carried out under an inert atmosphere to minimize oxidation.

9. The method (100) as claimed in claim 1, wherein the blending process utilizes at least one a plurality of additive substances comprising sodium lignosulphonate, wherein the plurality of additive substances are adapted to provide a uniform blend and consistency to the blended mixture.

10. An assembly (200) for producing virgin carbon black from treated recovered pyrolysis materials comprising:a recovery unit (210) adapted to generate a recovered carbon black from a tire pyrolysis, wherein the tire pyrolysis is performed in an oxygen-deficient environment to produce a plurality of substances comprising at least one of a tire pyrolysis oil, a gas, and the recovered carbon black;a plurality of industrial thermal processing equipment (220) adapted to heat the recovered carbon black to minimize its moisture content to less than 0.5% to prevent an undesirable reaction, wherein the industrial thermal processing equipment is adapted to apply a thermal energy to dry a raw material and remove moisture content;a mechanical grinding apparatus (230) operable to mill the recovered carbon black to achieve a predetermined particle size suitable for at least one of a dispersion and downstream processing;a mechanical mixer (240) equipped with a stirrer adapted to blend the recovered carbon black and the tire pyrolysis oil in a predetermined weight ratio to formulate a blended mixture, wherein the blend is performed for a predetermined duration to achieve a blended homogeneous mixture; anda reactor (250) utilized to accommodate the blended mixture and facilitate a virgin carbon black formation in response to an oxidation of a plurality of components within the blended mixture, wherein the oxidation of plurality of components comprises an ash component of a zinc and silica