Optical path control element and display device including the same

By using a high cross-linking density photocuring resin and polymer material layer in the optical path control member, the problems of reducing bond strength and deteriorating optical properties caused by additive migration in the light barrier film are solved, and the bond strength and stability of the component are improved ensures the reliability of perspective control.

CN115552328BActive Publication Date: 2024-12-03LG INNOTEK CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202180033669.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-05-11
Filing Date
2021-04-15
Publication Date
2024-12-03
Estimated Expiration
2041-04-15

AI Technical Summary

Technical Problem

The photocuring resin additives in the existing light barrier films migrate over time, resulting in a decrease in bonding strength and deterioration of optical characteristics, affecting the reliability of viewing angle control.

Method used

By improving the structure of the optical path control member, using a photocuring resin with high cross-linking density and reducing the additive content in the partition wall, the polymer material layer is combined to enhance the bonding strength between the adhesive layer and the light conversion part, and preventing additives migrate.

Benefits of technology

The bonding strength and optical characteristics stability of the optical path control member are improved, haze changes and adhesive layer peeling are prevented, and the reliability of viewing angle control is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115552328B_ABST
    Figure CN115552328B_ABST
Patent Text Reader

Abstract

According to the embodiment, the optical path control member includes an adhesive layer arranged between a second electrode and a light conversion portion, wherein the light conversion portion includes a partition wall portion and a receiving portion arranged alternately, and the partition wall portion includes a first region of 30 μm from the upper surface of the partition wall portion to the direction toward the first substrate, a third region of 30 μm from the lower surface of the partition wall portion to the direction toward the second substrate, and a second region arranged between the first region and the third region, and Si in the first region measured by XPS corresponds to less than 2 at%.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiment relates to a light path control member, and to a display device including the light path control member. Background Art

[0002] The light-blocking film blocks the transmission of light from a light source and is attached to the front surface of a display panel (which is a display device for a mobile phone, a laptop computer, a tablet computer, a vehicle navigation device, a vehicle touch screen, etc.), so that the light-blocking film adjusts the viewing angle of light according to the incident angle of light, thereby presenting clear image quality at the viewing angle required by the user when the display transmits the picture.

[0003] In addition, the light blocking film may be used for windows of vehicles, buildings, and the like to partially shield external light, thereby preventing glare or preventing the interior from being visible from the outside.

[0004] That is, the light blocking film can be a light path control member that controls the moving path of light to block light in a specific direction and transmit light in a specific direction. Therefore, the user's viewing angle can be controlled by controlling the transmission angle of light through the light blocking film.

[0005] Meanwhile, such light blocking films may be divided into light blocking films that can always control the viewing angle regardless of the surrounding environment or the user's environment and switchable light blocking films that can allow the user to turn on / off the viewing angle control according to the surrounding environment or the user's environment.

[0006] Such a switchable light blocking film can be realized by filling particles that can move when a voltage is applied and a dispersion liquid for dispersing the particles inside the pattern portion and switching the pattern portion between the light transmitting portion and the light blocking portion by dispersing and aggregating the particles.

[0007] In order to prevent the filler from overflowing, a photocurable resin may be used to manufacture a light conversion portion having a partition wall portion. In this case, the photocurable resin may include an additive for improving the releasability or electrical properties. Such additives may migrate on the surface of the resin, so there is a problem that the optical properties of the resin may deteriorate over time and the bonding strength between the resin and the bonding layer may deteriorate.

[0008] Therefore, there is a need for an optical path control member having a new structure that can solve the above-mentioned problems. Summary of the invention

[0009] Technical issues

[0010] The embodiment relates to a light path control member having improved reliability by improving adhesive characteristics. In addition, the embodiment can provide a light path control member having improved optical characteristics.

[0011] Technical Solution

[0012] According to the embodiment, the optical path control component includes: a first substrate; a first electrode, arranged on the first substrate; a light conversion part, arranged on the first electrode; a second substrate, arranged on the first substrate; the second electrode, arranged below the second substrate; and an adhesive layer, arranged between the light conversion part and the second electrode, wherein the light conversion part includes alternately arranged partition wall parts and receiving parts, the receiving part has a transmittance that changes according to the applied voltage, the adhesive layer includes a first interface between the upper surface of the adhesive layer and the second electrode and a second interface between the lower surface of the adhesive layer and the light conversion part, the partition wall part includes a first region from the upper surface of the partition wall part to 30 μm toward the first substrate, a third region from the lower surface of the partition wall part to 30 μm toward the second substrate, and a second region between the first region and the third region, and the Si content in the first region measured by X-ray photoelectron spectroscopy (XPS) is less than 2 at%. According to an embodiment, the display device includes: a display panel; and a light path control member arranged on the display panel, wherein the light path control member includes: a first substrate; a first electrode arranged on the first substrate; a light conversion part arranged on the first electrode; a second substrate arranged on the first substrate; the second electrode arranged below the second substrate; and an adhesive layer arranged between the light conversion part and the second electrode, wherein the light conversion part includes alternately arranged partition wall parts and receiving parts, the receiving part has a transmittance that changes according to an applied voltage, the adhesive layer includes a first interface between an upper surface of the adhesive layer and the second electrode and a second interface between a lower surface of the adhesive layer and the light conversion part, the partition wall part includes a first region from the upper surface of the partition wall part to 30 μm toward the first substrate, a third region from the lower surface of the partition wall part to 30 μm toward the second substrate, and a second region between the first region and the third region, and the Si content in the first region measured by XPS is less than 2 at%.

[0013] Beneficial Effects

[0014] The light path controlling member according to the embodiment may improve the adhesive strength and adhesive characteristics of the adhesive layer that bonds the first substrate to the second substrate.

[0015] Embodiments can improve the bonding strength between the partition wall portion and the bonding layer by changing the composition of the photocurable resin for accommodating the photoconversion material and preventing the photoconversion material from overflowing. Specifically, embodiments can reduce the content of the additives included to improve the separation characteristics or electrical characteristics of the photocurable resin. Therefore, embodiments can prevent the film between the partition wall portion and the bonding layer from being removed or delaminated according to the migration of the additives included in the resin.

[0016] In addition, the embodiment can prevent the degradation of optical characteristics due to the migration of additives in the photocurable resin to the surface of the photocurable resin over time. That is, the embodiment can prevent the haze from changing over time. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 and Figure 2 is a perspective view of a light path controlling member according to an embodiment.

[0018] Figure 3 and Figure 4 is a perspective view of a first substrate and a first electrode and a perspective view of a second substrate and a second electrode of a light path control member according to an embodiment.

[0019] Figure 5 is along Figure 1 A cross-sectional view taken along line AA'.

[0020] Figure 6 It is a graph showing the XPS measurement results of Comparative Example.

[0021] Figure 7 is a graph showing the results of adhesive strength tests in Comparative Examples and Examples.

[0022] Figures 8 to 11 is along Figure 1 The cross-sectional view taken along the line AA' in FIG. 1 is used to describe the shapes of various receiving portions in the light path control member according to the embodiment.

[0023] Fig.12 is a light path control member according to another embodiment Figure 1 A cross-sectional view taken along line AA'.

[0024] Fig.13 and Fig.14 : is a graph showing adhesive strength test results under various conditions of an example of a light path control member according to another embodiment and a comparative example.

[0025] Figures 15 to 21 It is a diagram for explaining a method of manufacturing a light path control member according to an embodiment.

[0026] Fig. 22 and Fig.23 is a cross-sectional view of a display device to which the light path control member according to the embodiment is applied.

[0027] Figure 24 to Figure 26 FIG. 1 is a diagram for explaining one embodiment of a display device to which the light path control member according to the embodiment is applied. DETAILED DESCRIPTION

[0028] Hereinafter, embodiments of the present invention will be described in detail with reference to the accompanying drawings. However, the spirit and scope of the present invention are not limited to a part of the embodiments described, but can be implemented in various other forms, and within the spirit and scope of the present invention, one or more elements of the embodiments can be selectively combined and replaced.

[0029] In addition, unless otherwise clearly defined and described, the terms (including technical terms and scientific terms) used in the embodiments of the present invention may be interpreted as having the same meaning as that commonly understood by ordinary technicians in the field to which the present invention belongs, and terms (such as terms defined in commonly used dictionaries) may be interpreted as having a meaning consistent with the meaning in the context of the prior art.

[0030] In addition, the terms used in the embodiments of the present invention are used to describe the embodiments and are not intended to limit the present invention. In this specification, unless otherwise specified in the wording, the singular form may also include the plural form, and when described as "A (and) B and at least one (or more) of C", it may include at least one of all combinations that can be combined with A, B and C.

[0031] In addition, when describing the elements of the embodiments of the present invention, terms such as first, second, A, B, (a), and (b) may be used. These terms are only used to distinguish the elements from other elements, and these terms do not limit the essence, order, or sequence of these elements.

[0032] In addition, when an element is described as being “connected” or “coupled” to another element, it may include not only the element being “directly connected” or “coupled” to the other element, but also the element being “connected” or “coupled” via other elements between the element and the other element.

[0033] In addition, when described as being formed or arranged “on” or “under” each element, “on” or “under” may include not only the two elements being directly connected to each other, but also one or more other elements being formed or arranged between the two elements.

[0034] Furthermore, when expressed as “upper” or “lower”, it can include not only an upward direction but also a downward direction based on one element.

[0035] Hereinafter, a light path control member according to an embodiment will be described with reference to the accompanying drawings. The light path control member described below relates to a switchable light path control member driven in various modes according to electrophoretic particles moved by applying a voltage.

[0036] Reference Figures 1 to 4, the light path control member 1000 according to the embodiment may include a first substrate 110 , a second substrate 120 , a first electrode 210 , a second electrode 220 , and a light conversion part 300 .

[0037] The first substrate 110 may support the first electrode 210. The first substrate 110 may be rigid or flexible.

[0038] In addition, the first substrate 110 may be transparent. For example, the first substrate 110 may include a transparent substrate capable of transmitting light.

[0039] The first substrate 110 may include glass, plastic or a flexible polymer film. For example, the flexible polymer film may be made of any one of polyethylene terephthalate (PET), polycarbonate (PC), acrylonitrile-butadiene-styrene copolymer (ABS), polymethyl methacrylate (PMMA), polyethylene naphthalate (PEN), polyether sulfone (PES), cyclic olefin copolymer (COC), triacetyl cellulose (TAC) film, polyvinyl alcohol (PVA) film, polyimide (PI) film and polystyrene (PS), which is just an example, but the embodiment is not limited thereto.

[0040] In addition, the first substrate 110 may be a flexible substrate having a flexible property.

[0041] In addition, the first substrate 110 may be a curved or bent substrate. That is, the light path control member including the first substrate 110 may also be formed to have flexibility, curved properties, or bent properties. Therefore, the light path control member according to the embodiment may be changed to various designs.

[0042] The first substrate 110 may extend in the first direction 1A, the second direction 2A, and the third direction 3A.

[0043] Specifically, the first substrate 110 may include a first direction 1A corresponding to the length direction or the width direction of the first substrate 110, a second direction 2A extending in a direction different from the first direction 1A and corresponding to the length direction or the width direction of the first substrate 110, and a third direction 3A extending in a direction different from the first direction 1A and the second direction 2A and corresponding to the thickness direction of the first substrate 110.

[0044] For example, the first direction 1A may be defined as the length direction of the first substrate 110, the second direction 2A may be defined as the width direction of the first substrate 110 perpendicular to the first direction 1A, and the third direction 3A may be defined as the thickness direction of the first substrate 110. Alternatively, the first direction 1A may be defined as the width direction of the first substrate 110, the second direction 2A may be defined as the length direction of the first substrate 110 perpendicular to the first direction 1A, and the third direction 3A may be defined as the thickness direction of the first substrate 110.

[0045] Hereinafter, for convenience of description, a first direction 1A is described as a length direction of the first substrate 110 , a second direction 2A is described as a width direction of the first substrate 110 , and a third direction 3A is described as a thickness direction of the first substrate 110 .

[0046] The first electrode 210 may be disposed on one surface of the first substrate 110. Specifically, the first electrode 210 may be disposed on an upper surface of the first substrate 110. That is, the first electrode 210 may be disposed between the first substrate 110 and the second substrate 120.

[0047] The first electrode 210 may include a transparent conductive material. For example, the first electrode 210 may include a conductive material having a light transmittance of about 80% or more. As an example, the first electrode 210 may include a metal oxide such as indium tin oxide, indium zinc oxide, copper oxide, tin oxide, zinc oxide, titanium oxide, etc.

[0048] The first electrode 210 may have a thickness of 0.05 μm to 2 μm.

[0049] Alternatively, the first electrode 210 may include various metals for achieving low resistance. For example, the first electrode 210 may include at least one metal selected from the group consisting of chromium (Cr), nickel (Ni), copper (Cu), aluminum (Al), silver (Ag), molybdenum (Mo), gold (Au), titanium (Ti), and alloys thereof.

[0050] Reference Figure 3 , the first electrode 210 may be disposed on the entire surface of one surface of the first substrate 110. Specifically, the first electrode 210 may be disposed as a surface electrode on one surface of the first substrate 110. However, the embodiment is not limited thereto, and the first electrode 210 may be formed of a plurality of pattern electrodes having a uniform pattern such as a grid shape or a stripe shape.

[0051] For example, the first electrode 210 may include a plurality of conductive patterns. Specifically, the first electrode 210 may include a plurality of mesh lines crossing each other and a plurality of mesh openings formed by the mesh lines.

[0052] Therefore, even if the first electrode 210 includes metal, the first electrode 210 cannot be visually recognized from the outside, so that visibility can be improved. In addition, the light transmittance is improved by the opening, so that the brightness of the light path control member according to the embodiment can be improved.

[0053] The second substrate 120 may be disposed on the first substrate 110. Specifically, the second substrate 120 may be disposed on the first electrode 210 on the first substrate 110.

[0054] The second substrate 120 may include a material capable of transmitting light. The second substrate 120 may include a transparent material. The second substrate 120 may include a material that is the same as or similar to the first substrate 110 described above.

[0055] For example, the second substrate 120 may include glass, plastic or a flexible polymer film. For example, the flexible polymer film may be made of any one of polyethylene terephthalate (PET), polycarbonate (PC), acrylonitrile-butadiene-styrene copolymer (ABS), polymethyl methacrylate (PMMA), polyethylene naphthalate (PEN), polyether sulfone (PES), cyclic olefin copolymer (COC), triacetyl cellulose (TAC) film, polyvinyl alcohol (PVA) film, polyimide (PI) film and polystyrene (PS). This is just an example, however, the embodiment is not limited thereto.

[0056] In addition, the second substrate 120 may be a flexible substrate having a flexible property.

[0057] In addition, the second substrate 120 may be a curved or bent substrate. That is, the light path control member including the second substrate 120 may also be formed to have flexibility, curved properties, or bent properties. Therefore, the light path control member according to the embodiment may be changed to various designs.

[0058] The second substrate 120 may also extend in the first direction 1A, the second direction 2A, and the third direction 3A in the same manner as the first substrate 110 described above.

[0059] Specifically, the second substrate 120 may include a first direction 1A corresponding to the length direction or the width direction of the second substrate 120, a second direction 2A extending in a direction different from the first direction 1A and corresponding to the length direction or the width direction of the second substrate 120, and a third direction 3A extending in a direction different from the first direction 1A and the second direction 2A and corresponding to the thickness direction of the second substrate 120.

[0060] For example, the first direction 1A may be defined as the length direction of the second substrate 120 , the second direction 2A may be defined as the width direction of the second substrate 120 perpendicular to the first direction 1A, and the third direction 3A may be defined as the thickness direction of the second substrate 120 .

[0061] Alternatively, the first direction 1A may be defined as a width direction of the second substrate 120 , the second direction 2A may be defined as a length direction of the second substrate 120 perpendicular to the first direction 1A, and the third direction 3A may be defined as a thickness direction of the second substrate 120 .

[0062] Hereinafter, for convenience of description, the first direction 1A is described as the length direction of the second substrate 120 , the second direction 2A is described as the width direction of the second substrate 120 , and the third direction 3A is described as the thickness direction of the second substrate 120 .

[0063] The second electrode 220 may be disposed on one surface of the second substrate 120. Specifically, the second electrode 220 may be disposed on the lower surface of the second substrate 120. That is, the second electrode 220 may be disposed on one surface of the second substrate 120 where the second substrate 120 and the first substrate 110 face each other. That is, the second electrode 220 may be disposed to face the first electrode 210 on the first substrate 110. That is, the second electrode 220 may be disposed between the first electrode 210 and the second substrate 120.

[0064] The second electrode 220 may include a material that is the same as or similar to that of the first electrode 210 described above.

[0065] The second electrode 220 may include a transparent conductive material. For example, the second electrode 220 may include a conductive material having a light transmittance of about 80% or more. As an example, the second electrode 220 may include a metal oxide such as indium tin oxide, indium zinc oxide, copper oxide, tin oxide, zinc oxide, titanium oxide, etc.

[0066] The second electrode 220 may have a thickness of about 0.1 μm to about 0.5 μm.

[0067] Alternatively, the second electrode 220 may include various metals for achieving low resistance. For example, the second electrode 220 may include at least one metal selected from chromium (Cr), nickel (Ni), copper (Cu), aluminum (Al), silver (Ag), molybdenum (Mo), gold (Au), titanium (Ti), and alloys thereof.

[0068] Reference Figure 4 , the second electrode 220 may be disposed on the entire surface of one surface of the second substrate 120. Specifically, the second electrode 220 may be disposed as a surface electrode on one surface of the second substrate 120. However, the embodiment is not limited thereto, and the second electrode 220 may be formed of a plurality of pattern electrodes having a uniform pattern such as a grid shape or a stripe shape.

[0069] For example, the second electrode 220 may include a plurality of conductive patterns. Specifically, the second electrode 220 may include a plurality of grid lines crossing each other and a plurality of grid openings formed by the grid lines.

[0070] Therefore, even if the second electrode 220 includes metal, the second electrode 220 cannot be visually recognized from the outside, so that visibility can be improved. In addition, the light transmittance is improved by the opening, so that the brightness of the light path control member according to the embodiment can be improved.

[0071] The first substrate 110 and the second substrate 120 may have sizes corresponding to each other. The first substrate 110 and the second substrate 120 may have sizes that are the same as or similar to each other.

[0072] Specifically, a first length of the first substrate 110 extending along the first direction 1A may have the same or similar size as a second length L2 of the second substrate 120 extending along the first direction 1A.

[0073] For example, the first length and the second length may have a dimension of 300 mm to 400 mm.

[0074] In addition, a first width of the first substrate 110 extending along the second direction 2A may have the same or similar size as a second width of the second substrate 120 extending along the second direction 2A.

[0075] For example, the first width and the second width may have a size of 150 mm to 200 mm.

[0076] In addition, a first thickness of the first substrate 110 extending along the third direction 3A may have the same or similar size as a second thickness of the second substrate 120 extending along the third direction 3A.

[0077] For example, the first thickness and the second thickness may have a size of 30 μm to 200 μm.

[0078] Reference Figure 1 , the first substrate 110 and the second substrate 120 may be disposed to be misaligned with each other.

[0079] Specifically, the first substrate 110 and the second substrate 120 may be disposed at positions misaligned with each other along the first direction 1A. Specifically, the first substrate 110 and the second substrate 120 may be disposed such that the sides of the substrates are misaligned with each other.

[0080] Therefore, the first substrate 110 may be disposed to protrude in one direction of the first direction 1A, and the second substrate 120 may be disposed to protrude in the other direction of the second direction 2A.

[0081] That is, the first substrate 110 may include a first protrusion protruding in one direction of the first direction 1A, and the second substrate 110 may include a second protrusion protruding in the other direction of the first direction 1A.

[0082] Therefore, the light path control member 1000 may include a region on the first substrate 110 where the first electrode 210 is exposed and a region below the second substrate 120 where the second electrode 220 is exposed.

[0083] That is, the first electrode 210 disposed on the first substrate 110 may be exposed at the first protrusion, and the second electrode 220 disposed under the second substrate 120 may be exposed at the second protrusion.

[0084] The first electrode 210 and the second electrode 220 exposed at the protrusion may be connected to an external printed circuit board through a connection part to be described below.

[0085] Or, refer to Figure 2 , the first substrate 110 and the second substrate 120 may be disposed at positions corresponding to each other. Specifically, the first substrate 110 and the second substrate 120 may be disposed so that respective sides correspond to each other.

[0086] Therefore, the first substrate 110 may be disposed to protrude in one direction in the first direction 1A, and the second substrate 120 may also be disposed to protrude in one direction in the first direction 1A, that is, to protrude in the same direction as the first substrate 110 .

[0087] That is, the first substrate 110 may include a first protrusion protruding in one direction of the first direction 1A, and the second substrate may also include a second protrusion protruding in one direction of the first direction 1A.

[0088] That is, the first protrusion and the second protrusion may protrude in the same direction.

[0089] Therefore, the light path control member 1000 may include a region on the first substrate 110 where the first electrode 210 is exposed and a region below the second substrate 120 where the second electrode 220 is exposed.

[0090] That is, the first electrode 210 disposed on the first substrate 110 may be exposed at the first protrusion, and the second electrode 220 disposed under the second substrate 120 may be exposed at the second protrusion.

[0091] The first electrode 210 and the second electrode 220 exposed at the protrusion may be connected to an external printed circuit board through a connection part to be described below.

[0092] The light conversion part 300 may be disposed between the first substrate 110 and the second substrate 120. Specifically, the light conversion part 300 may be disposed between the first electrode 210 and the second electrode 220.

[0093] An adhesive layer or a buffer layer may be disposed between at least one of the light conversion part 300 and the first substrate 110 or between the light conversion part 300 and the second substrate 120 , and the first substrate 110 , the second substrate 120 , and the light conversion part 300 may be bonded to each other through the adhesive layer and / or the buffer layer.

[0094] The light conversion part 300 may include a plurality of partition wall parts and a plurality of receiving parts. Light conversion particles that move according to an applied voltage may be provided in the receiving parts, and the light transmission characteristics of the light path control member may be changed by the light conversion particles.

[0095] The size of the light conversion part 300 may be smaller than that of at least one of the first substrate 110 and the second substrate 120 .

[0096] Specifically, the length of the light conversion part 300 in the first direction may be smaller than the length of at least one of the first substrate 110 and the second substrate 120 in the first direction.

[0097] In addition, the width of the light conversion part 300 in the second direction may be equal to or smaller than the width of at least one of the first substrate 110 and the second substrate 120 in the second direction.

[0098] In addition, at least one of both ends of the first substrate 110 and the second substrate 120 in the first direction may be disposed outside both ends of the light conversion part 300 in the first direction.

[0099] Therefore, a sealing portion (not shown in the drawings) can be easily provided, and the adhesive property of the sealing portion can be improved.

[0100] Will refer to Figure 5 A light path controlling member according to an embodiment is described.

[0101] The light path control member according to the embodiment may include a light conversion material. For example, the light conversion material 320' may be an EPD ink. In order to accommodate the light conversion material 320' and prevent it from overflowing, a light conversion unit 300 may be used. The light conversion unit 300 may include a receiving unit 320 for accommodating the light conversion material 320' and a partition wall unit 310 for preventing the light conversion material 320' from overflowing.

[0102] The light conversion unit 300 may be formed of a photocurable resin. For example, the light conversion unit 300 may be formed by imprinting a photocurable resin. That is, the partition wall portion 310 and the receiving portion 32 may be formed of a photocurable resin.

[0103] Specifically, the partition wall portion 310 may include a resin material. For example, the partition wall portion 310 may include a photocurable resin material. As an example, the partition wall portion 310 may include a polyurethane resin or the like.

[0104] The photocurable resin may include an oligomer, a monomer, a photopolymerization initiator, and an additive. The photocurable resin may form a photoconversion part through a reaction of a polymer type prepolymer, a multifunctional monomer as a diluent, and a photopolymerization initiator.

[0105] Here, the additive may refer to various materials for improving the release characteristics or electrical characteristics of the photocurable resin. For example, the additive may refer to various materials including a release additive and / or an antistatic agent.

[0106] The additive has the property of migrating to the resin surface over time. Such migration of the additive may cause the problem of degradation of the optical characteristics of the light path control member. In addition, the migration of the additive may deteriorate the bonding strength between the additive and the partition wall portion.

[0107] In the embodiment, in order to reduce the migration of the additive, various factors such as the composition or the constituent material of the photocurable resin constituting the partition wall portion may be changed.

[0108] The photocurable resin may include a polymer main chain having a high crosslinking density. Here, the crosslinking density may be measured using a swelling method.

[0109] As the crosslinking density of the photocurable resin increases, the amount of solvent molecules that can penetrate between the polymers increases. Therefore, the higher the crosslinking density, the lower the swelling rate (swelling %).

[0110] The swelling ratio can be calculated by the following equation.

[0111]

[0112] Here, each function can be referred to as follows.

[0113] Q = swelling ratio

[0114] W s = weight of swollen cross-linked material

[0115] W u = weight of unswollen cross-linked material

[0116] W sol = weight of swelling solvent

[0117] The photocurable resin according to the embodiment may have a swelling rate of 10% or less.

[0118] When the swelling rate of the photocurable resin exceeds 10%, the crosslinking density is relatively low, thereby increasing the amount of solvent molecules that can penetrate between polymers. Therefore, the amount of additives that can penetrate between rubber chains of the photocurable resin can be increased. Therefore, when the swelling rate of the photocurable resin exceeds 10%, the adhesive strength and optical properties may deteriorate.

[0119] That is, in an embodiment, the cross-linking density of the photocurable resin as a material for forming the partition wall portion may be high. Therefore, the amount of additives that penetrate between the chains of the photocurable resin may be small. Therefore, the bonding strength between the adhesive layer and the partition wall portion in the light path control member can be improved. In addition, the embodiment can prevent the degradation of optical properties caused by the additives in the photocurable resin migrating to the surface of the photocurable resin over time. Therefore, the haze of the light path control member can be improved.

[0120] The photocurable resin may include a urethane acrylate polymer. For example, the oligomer may include urethane acrylate.

[0121] The monomer may have five or more branches. In an embodiment, as the number of functional groups of the monomer increases, the crosslinking property may increase, and thus the crosslinking density may increase.

[0122] The monomer may be a multifunctional monomer. The multifunctional monomer may have five or more functional group branches. Here, the number of branches may refer to the number of each branch connected to the main chain being five or more. As an example, the number of branches of the monomer may be five to seven. For example, the monomer may have five to six branches.

[0123] When the number of branches of the monomer is five or more, the chain length of the polymer becomes shorter and shrinks, so the crosslinking density can be increased. Embodiments may include a monomer having five or more branches so that the swelling ratio can have a value of 10% or less.

[0124] When the number of branches of the monomer is less than five, the crosslinking density of the polymer may decrease. Therefore, when the partition wall portion is formed of a material having five branches of a small monomer, there may be a problem that the adhesive property and optical property of the light path control member are deteriorated.

[0125] When the photocurable resin is 100 wt %, the content of the additive may be 0.5 wt % or less. In the embodiment, since the content of the additive in the photocurable resin is 0.5 wt % or less, the migration amount of the additive on the partition wall portion may be reduced.

[0126] When the amount of the additive exceeds 0.5 wt %, there may be a problem that the additive may migrate to the surface of the photocurable resin.

[0127] Here, the additive may include an antistatic agent and a non-reactive release additive in the form of a silicone product.

[0128] For example, the non-reactive release additive may be a silicon-containing material such as PDMS.

[0129] For example, the antistatic agent may be a fluorine-containing material.

[0130] In the embodiment, by measuring the X-ray photoelectron spectroscopy (XPS) from the interface between the upper surface 310T of the partition wall portion and the lower surface 420B of the adhesive layer in the depth direction of the partition wall portion, the content of the additive according to the position of the partition wall portion can be confirmed. By the XPS device, the content of the additive in the inner region of each thickness of the partition wall portion can be confirmed.

[0131] As an example, while the surface of the partition wall portion can be gradually etched by etching from the upper surface of the partition wall portion, the content of the additive in the region located inside the partition wall portion can be confirmed. When the etching time is short, the content of the additive in the first region can be confirmed, and when the etching time is long, the content of the additive in the third region can be confirmed.

[0132] For example, in the embodiment, while etching the upper surface of the partition wall portion, the content of the additive inside the partition wall portion can be confirmed based on the etching time.

[0133] That is, when the etching time of the partition wall portion is zero, the contents of Si and F expressed on the surface of the partition wall portion can be confirmed.

[0134] As an example, when the etching time of the partition wall portion is less than about 300 seconds, the content of the additive contained in the partition wall portion in a region close to the surface of the partition wall portion may be confirmed.

[0135] As an example, when the etching time of the partition wall portion is about 300 seconds to 1000 seconds, the content of the additive contained in the partition wall portion in the middle of the partition wall portion may be confirmed.

[0136] As an example, when the etching time of the partition wall portion exceeds about 1000 seconds, the content of the additive contained in the partition wall portion in the base layer of the first electrode located close to the partition wall portion can be confirmed.

[0137] The partition wall portion 310 can be divided into a first region as a surface portion of the resin, a second region as a middle portion, and a third region as a base layer portion according to the depth. Specifically, the partition wall portion may include a first region P1 from the upper surface 310T of the partition wall portion to 30 μm in the depth direction, a third region P3 from the lower surface of the partition wall portion to 30 μm in the depth direction, and a second region located between the first region and the third region.

[0138] The partition wall portion may include a first region P1 from the upper surface of the partition wall portion to 30 μm toward the first substrate, a third region P3 from the lower surface of the partition wall portion to 30 μm toward the second substrate, and a second region P2 located between the first region and the third region. Therefore, the partition wall portion having various thickness ranges may include the first region, the second region, and the third region. Alternatively, the partition wall portion may include the first region and the third region.

[0139] As an example, the second region P2 may be a region between 30 μm and 60 μm from the upper surface of the partition wall portion in the depth direction. The third region P3 may include a region between 60 μm and 95 μm from the upper surface of the partition wall portion in the depth direction.

[0140] Reference Figure 5 and 6 , the difference in the migration degree of the additives in the comparative examples and the examples will be described in detail.

[0141] Here, at% of Si may indicate the content and migration degree of the non-reactive release additive according to the position, and at% of F may indicate the content and migration degree of the antistatic agent.

[0142] Figure 6 This is a diagram showing XPS results at various depths of the partition wall portion measured in Comparative Example.

[0143] The XPS result is a measurement of the at% content of Si, and the content of Si contained in the additive can be used as an evaluation standard capable of measuring the migration of Si.

[0144] In the XPS measurement results, the x-axis may represent etching time, and the y-axis may represent at% of Si.

[0145] That is, the XPS measurement result can show the content of elements such as Si and F according to the depth of the partition wall portion with the passage of etching time.

[0146] In a comparative example, the content of Si in the first region P1 may be greater than 2 at %.

[0147] In the comparative example, the content of Si and F in the first region may be greater than 2.6 at %.

[0148] In the comparative example, it can be confirmed that the Si content in the first region P1 is significantly higher than the Si content in the second region P2 and the third region P3. That is, in the comparative example, it can be confirmed that the migration amount of the additive between the interface between the adhesive layer and the partition wall portion is large.

[0149] Reference Figure 6 In the comparative example, it can be confirmed that the Si content measured in the first region P1 is higher than the Si content measured in the second region P2 or the third region P3 by 1.5 at % or more.

[0150] According to the surface analysis results of the resin measured in the example, the content of Si measured on the surface of the partition wall portion before etching may be less than 2.0 at%. For example, according to the surface analysis results of the resin measured in the example, the content of Si measured on the surface of the partition wall portion before etching may be 1.5 at% or less.

[0151] For example, according to the surface analysis results of the resin in the example, the content of Si measured on the surface of the partition wall portion before etching may be 1.3 at % to 1.4 at %. As an example, in the example, according to the surface analysis results of the resin, the content of Si measured on the surface of the partition wall portion before etching may be 1.38 at % to 1.40 at %.

[0152] In an example, the content of Si measured by XPS in the first region may be 2 at% or less. For example, in an example, the content of Si measured by XPS in the first region may be 1.5 at% or less. For example, in an example, the content of Si measured by XPS in the first region may be 1 at% or less.

[0153] In the example, it can be confirmed that the content of Si in the first region P1 is at a level similar to the content of Si in the second region P2 and the third region P3. In addition, in the example, it can be confirmed that the content of F in the first region P1 is at a level similar to the content of F in the second region P2 and the third region P3. Specifically, in the example, it can be confirmed that the content of the additive is similar regardless of the depth of the partition wall portion.

[0154] In the example, the content of Si and the content of F may be constant in a region from the upper surface of the partition wall portion to 30 μm in the depth direction. In the example, the content of Si and the content of F may be constant in a region from the upper surface of the partition wall portion to 90 μm in the depth direction. That is, in the example, it can be confirmed that the migration of the additive at the interface between the adhesive layer and the partition wall portion is small.

[0155] In an example, the Si content and the F content measured in the first region may be 1 at% to 3 at%. For example, in an example, the Si content and the F content measured in the first region may be 1 at% to 2 at%. For example, in an example, the Si content and the F content measured in the first region may be 2 at% to 2.6 at%.

[0156] Specifically, in the example, it can be confirmed that the deviation between the Si content in the first region P1 and the Si content in the second region P2 is less than 1.5 at%. For example, in the example, it can be confirmed that the deviation between the Si content in the first region P1 and the Si content in the second region P2 is less than 1.0 at%. For example, in the example, it can be confirmed that the deviation between the Si content in the first region P1 and the Si content in the second region P2 is less than 0.5 at%.

[0157] Specifically, in the example, it can be confirmed that the deviation between the content of Si in the first region P1 and the content of Si in the third region P3 is less than 1.5 at%. For example, in the example, it can be confirmed that the deviation between the content of Si in the first region P1 and the content of Si in the third region P3 is less than 1.0 at%. For example, in the example, it can be confirmed that the deviation between the content of Si in the first region P1 and the content of Si in the third region P3 is less than 0.5 at%.

[0158] In the examples, the results of the Si content and the F content according to the depth of the partition wall portion are shown in Tables 1 and 2.

[0159] The results when the partition wall portion was etched for 60 seconds are shown in Table 1. In this case, when the partition wall portion was etched for 60 seconds, the content of the additive such as Si and F located in the first region can be confirmed.

[0160] In Table 1, it can be confirmed that the sum of the Si content and the F content in the first region at the time of etching for 60 seconds is 2.53 at %.

[0161] [Table 1]

[0162] Element at% Si2P 0.63 P2p 0.33 S2p 0.48 Cls 74.39 In3d 0.11 O1s 22.16 F1s 1.90

[0163] Table 2 shows the results when the partition wall portion was etched for 1202 seconds. In this case, when the partition wall portion was etched for 1202 seconds, the content of additives such as Si and F located in the third region can be confirmed. In Table 2, it can be confirmed that the sum of the content of Si and the content of F in the third region at the time of etching for 1202 seconds is 0.63at%.

[0164] [Table 2]

[0165] Element at% Cls 81.27 O1s 17.83 Si2P 0.22 P2p 0.15 F1s 0.41 S2p 0.13

[0166] Referring to Tables 1 and 2, in the example, it can be confirmed that the difference in Si content between the first region and the third region is 0.41 at%. Thus, it can be confirmed that the difference in Si content between the first region and the second region is also less than 0.5 at%. In addition, in the example, it can be confirmed that the difference in F content between the first region and the third region is less than 1.5 at%. In the example, it can be confirmed that the difference in F content between the first region and the second region is less than 1.5 at%.

[0167] As the crosslinking density increases, the content of the additive that migrates to the surface portion of the resin can be reduced.

[0168] Reference Figure 7 , the bonding strength between the upper surface of the partition wall and the bonding layer will be described in detail.

[0169] Figure 7 The adhesive strength test results in Examples and Comparative Examples are shown.

[0170] In the example, prepare Figure 5 The sample specimen of the same structure was used for the adhesive strength test. A 180 degree peel test of lifting the second substrate 120 as the upper ITO substrate from the sample specimen was performed. The 180 degree peel test is a test to measure how much force is applied to peel off the upper ITO substrate.

[0171] When the upper ITO substrate is lifted in the 180-degree peel test, the peeled interface may be the interface between the adhesive layer 420 and the second electrode 220 or the interface between the adhesive layer 420 and the partition wall portion 310. Specifically, in the 180-degree peel test, when the upper ITO substrate is lifted, an interface with a lower adhesive strength among the first interface between the adhesive layer and the ITO electrode on the adhesive layer and the second interface between the adhesive layer and the resin below the adhesive layer will be peeled.

[0172] In the comparative example and the example, the peeling test of the upper ITO substrate was performed twice respectively.

[0173] First, after manufacturing the sample substrates according to the comparative examples and examples, a 180-degree peel test of lifting the upper ITO substrate was performed at room temperature. Here, the meaning of after manufacturing the sample substrate may refer to immediately after the resin layer (which is the light conversion part located on the lower ITO substrate) is bonded to the upper ITO substrate through the adhesive layer 420. Here, the measured value of the peel test immediately after manufacturing the sample substrate may be a value measured within 30 minutes after manufacturing the sample substrate. In this case, the standard of the value of the upper ITO substrate being peeled off measured at room temperature immediately after manufacturing the sample substrate may refer to the bonding strength between the OCA adhesive layer and ITO (50 μm) being approximately 100 gf / 25 mm.

[0174] In the comparative example, the partition wall portion may be made of a photocurable resin using a polymer having a low crosslinking density. Therefore, in the comparative example, it can be seen that since the first interface between the adhesive layer 420 and the second electrode 220 is peeled off (109.6 gf / 25 mm) immediately after manufacturing the sample substrate, the adhesive strength of the second interface between the adhesive layer 420 and the photoconversion unit 300 is higher, and it can be estimated that the adhesive strength between the adhesive layer 420 and the photoconversion unit 300 has a value greater than 109.6 gf / 25 mm.

[0175] In the example, the partition wall portion can be manufactured using a photocurable resin using a polymer having a high crosslinking density. Therefore, in the example, it can be seen that since the first interface between the adhesive layer 420 and the second electrode 220 is peeled off (197.2 gf / 25 mm) immediately after manufacturing the sample substrate, the adhesive strength of the second interface between the adhesive layer 420 and the photoconversion unit 300 is higher, and it can be estimated that the adhesive strength between the adhesive layer 420 and the photoconversion unit 300 has a value greater than 197.2 gf / 25 mm.

[0176] In the example, the bonding strength of the first interface measured at room temperature immediately after the second electrode is bonded to the photoconversion part through the bonding layer can be 120gf / 25mm or more. For example, in the example, the bonding strength of the first interface measured at room temperature immediately after the second electrode is bonded to the photoconversion part through the bonding layer can be 150gf / 25mm or more. For example, in the example, the bonding strength of the first interface measured at room temperature immediately after the second electrode is bonded to the photoconversion part through the bonding layer can be 190gf / 25mm or more. That is, unlike the comparative example, since the example contains a polymer with a high cross-linking density, the bonding strength at the first interface can be 120gf / 25mm or more.

[0177] In addition, in the example, the bonding strength of the second interface measured at room temperature immediately after the second electrode is bonded to the light conversion unit through the bonding layer may be 120 gf / 25 mm or more. For example, in the example, the bonding strength of the second interface measured at room temperature immediately after the second electrode is bonded to the light conversion unit through the bonding layer may be 150 gf / 25 mm or more. For example, in the example, the bonding strength of the second interface measured at room temperature immediately after the second electrode is bonded to the light conversion unit through the bonding layer may be 190 gf / 25 mm or more.

[0178] Next, after manufacturing the sample substrates according to the comparative example and the example, a 180-degree peel test in which the upper ITO substrate was lifted was performed after 24 hours at 60° C. Here, in the sample substrate, the adhesive strength of the first interface between the adhesive layer and the second electrode can be increased under the condition of 60° C., which is higher than room temperature. Therefore, the peel test was performed after aging under the condition of 60° C.

[0179] In the comparative example, after manufacturing the sample substrate, a 180-degree peel test in which the upper ITO substrate was lifted was performed at 60°C for 24 hours. In this case, in the sample substrate of the comparative example, it can be seen that the bonding strength of the first interface between the bonding layer and the second electrode is higher because the second interface between the bonding layer 420 and the light conversion part 300 is peeled off (6.4 gf / 25 mm). In addition, in the comparative example, the bonding strength of the second interface between the bonding layer 420 and the light conversion part 300 measured immediately after manufacturing the sample substrate is greater than 109.6 gf / 25 mm, but it can be confirmed that the bonding strength of the second interface between the bonding layer 420 and the light conversion part 300 is greatly reduced to 6.4 gf / 25 mm due to the migration of the additive on the surface of the light conversion part (resin) at 60°C for 24 hours.

[0180] In the example, after the sample substrate was manufactured, a 180-degree peeling test was performed after 24 hours at 60° C. in which the upper ITO substrate was lifted. In this case, in the sample substrate of the example, it can be seen that the bonding strength of the first interface between the bonding layer 420 and the second electrode 220 is higher because the second interface between the bonding layer 420 and the light conversion unit 300 is peeled (483 gf / 25 mm).

[0181] In addition, in the example, the bonding strength of the second interface between the adhesive layer 420 and the light conversion part 300 measured immediately after manufacturing the sample substrate is greater than 197.2 gf / 25 mm, and it can be confirmed that due to the reduction in the amount of migration of the additive on the surface of the light conversion part (resin) within 24 hours at 60°C, the bonding strength of the second interface between the adhesive layer 420 and the light conversion part 300 increases to 483 gf / 25 mm, which is higher than that immediately after manufacturing the sample substrate, or maintains the existing bonding strength.

[0182] In an example, after the second electrode is bonded to the photoconversion unit through the adhesive layer, the adhesive strength of the second interface measured at 60°C after 24 hours may be 300 gf / 25 mm or more. For example, in an example, after the second electrode is bonded to the photoconversion unit through the adhesive layer, the adhesive strength of the second interface measured at 60°C after 24 hours may be 300 gf / 25 mm or more.

[0183] In an example, after the second electrode is bonded to the light conversion part through the adhesive layer, the adhesive strength of the second interface measured at 60° C. after 24 hours may be 400 gf / 25 mm or more.

[0184] For example, in the example, after the second electrode is bonded to the photoconversion unit through the adhesive layer, the bonding strength of the second interface measured at 60°C after 24 hours can be 450 gf / 25 mm or more. For example, in the example, after the second electrode is bonded to the photoconversion unit through the adhesive layer, the bonding strength of the second interface measured at 60°C after 24 hours can be 480 gf / 25 mm or more.

[0185] That is, in the example, it is possible to prevent the additive from migrating over time after bonding, thereby preventing the bonding strength between the partition wall portion and the bonding layer from decreasing.

[0186] In the example, through the 180-degree peel test, it can be confirmed that the bonding strength between the light conversion part and the adhesive layer is improved. That is, in the example, it can be seen that the migration of the additive contained in the light conversion part is reduced, so that the bonding strength of the second interface between the light conversion part (which is a resin material) and the adhesive layer is excellent. Therefore, the reliability of the optical path control component according to the example can be improved.

[0187] Details of the light conversion part 300 will be described in detail below.

[0188] Reference Figure 5 , Figures 8 to 11 , the light conversion portion 300 may include a partition wall portion 310 and a receiving portion 320 .

[0189] The partition wall portion 310 may be defined as a partition wall portion that divides the receiving portion. That is, the partition wall portion 310 may transmit light as a barrier region that divides a plurality of receiving portions. In addition, the receiving portion 320 may be defined as a variable region, wherein the receiving portion 320 is switched to a light blocking portion and a light transmitting portion according to an applied voltage.

[0190] The partition wall portions 310 and the receiving portions 320 may be arranged alternately with each other. The partition wall portions 310 and the receiving portions 320 may be arranged to have different widths. For example, the width of the partition wall portions 310 may be greater than the width of the receiving portions 320.

[0191] The partition wall portions 310 and the receiving portions 320 may be arranged alternately with each other. Specifically, the partition wall portions 310 and the receiving portions 320 may be arranged alternately with each other. That is, each partition wall portion 310 may be arranged between mutually adjacent receiving portions 320, and each receiving portion 320 may be arranged between adjacent partition wall portions 310.

[0192] The partition wall portion 310 may include a transparent material. The partition wall portion 310 may include a material that can transmit light.

[0193] The partition wall part 310 may transmit light incident on any one of the first substrate 110 and the second substrate 120 toward the other substrate.

[0194] For example, in Figures 8 to 11 In the embodiment, light may be emitted from the first substrate 110 by a light source disposed below the first substrate 110, and the light may be incident toward the second substrate 120. In this case, the partition wall portion 310 may transmit light, and the transmitted light may move toward the second substrate 120.

[0195] The receiving part 320 may include a dispersion liquid 320a and light conversion particles 320b. Specifically, the receiving part 320 may be filled by injecting the dispersion liquid 320a. A plurality of light conversion particles 320b may be dispersed in the dispersion liquid 320a.

[0196] The dispersion liquid 320a may be a material for dispersing the light conversion particles 320b. The dispersion liquid 320a may include a transparent material. The dispersion liquid 320a may include a non-polar solvent.

[0197] In addition, the dispersion liquid 320a may contain a material capable of transmitting light. For example, the dispersion liquid 320a may contain at least one of a halogen-based oil, a paraffin-based oil, and isopropyl alcohol.

[0198] The light conversion particles 320b may be disposed to be dispersed in the dispersion liquid 320a. Specifically, a plurality of light conversion particles 320b may be disposed to be spaced apart from each other in the dispersion liquid 320a.

[0199] The light conversion particles 320b may include a material capable of absorbing light. That is, the light conversion particles 320b may be light absorbing particles. The light conversion particles 320b may have a color. For example, the light conversion particles 320b may have a color based on black. As an example, the light conversion particles 320b may include carbon black.

[0200] The photoconversion particles 320b may have polarity by charging their surfaces. For example, the surfaces of the photoconversion particles 320b may be negatively (-) charged. Therefore, the photoconversion particles 320b may move toward the first electrode 210 or the second electrode 220 according to the applied voltage.

[0201] The light transmittance of the receiving portion 320 may be changed by the light conversion particles 320b. Specifically, the receiving portion 320 may be switched between a light blocking portion and a light transmitting portion by changing the light transmittance due to the movement of the light conversion particles 320b. That is, the receiving portion 320 may change the transmittance of light passing through the receiving portion 320 by the dispersion and aggregation of the light conversion particles 320b disposed in the dispersion 320a.

[0202] For example, the light path controlling member according to the embodiment may be converted from the first mode to the second mode or from the second mode to the first mode by a voltage applied to the first electrode 210 and the second electrode 220 .

[0203] Specifically, in the light path control member according to the embodiment, the receiving portion 320 becomes a light blocking portion in the first mode, and light at a specific angle can be blocked by the receiving portion 320. That is, the viewing angle of the user viewing from the outside is narrowed, so that the light path control member can be driven in the privacy mode.

[0204] In addition, in the light path control member of the embodiment, the housing portion 320 becomes a light-transmitting portion in the second mode, and in the light path control member according to the embodiment, light can pass through the partition wall portion 310 and the housing portion 320. That is, the viewing angle of the user viewing from the outside can be widened, so that the light path control member can be driven in the open mode.

[0205] The switching from the first mode to the second mode (i.e., the conversion of the receiving portion 320 from the light blocking portion to the light transmitting portion) can be achieved by the movement of the light conversion particles 320b of the receiving portion 320. That is, the light conversion particles 320b can have charges on their surfaces and can move toward the first electrode or the second electrode according to the applied voltage based on the characteristics of the charges. That is, the light conversion particles 320b can be electrophoretic particles.

[0206] Specifically, the receiving portion 320 may be electrically connected to the first electrode 210 and the second electrode 220 .

[0207] In this case, when no voltage is applied to the light path control member from the outside, the light conversion particles 320b of the receiving part 320 are uniformly dispersed in the dispersion 320a, and the receiving part 320 can block light by the light conversion particles. Therefore, in the first mode, the receiving part 320 can be driven as a light blocking part.

[0208] Alternatively, when a voltage is applied to the light path control member from the outside, the light conversion particle 320b can move. For example, the light conversion particle 320b can move toward one end or the other end of the receiving portion 320 by the voltage transmitted via the first electrode 210 and the second electrode 220. That is, the light conversion particle 320b can move from the receiving portion 320 toward the first electrode 210 or the second electrode 220.

[0209] Specifically, when a voltage is applied to the first electrode 210 and / or the second electrode 220, an electric field is formed between the first electrode 210 and the second electrode 220, and the negatively charged photoconversion particles 320b can move toward the positive poles of the first electrode 210 and the second electrode 220 using the dispersion 320a as a medium.

[0210] That is to say, Figure 8 As shown, when a voltage is applied to the first electrode 210 and / or the second electrode 220, the photoconversion particles 320b may move toward the first electrode 210 in the dispersion 320a. That is, the photoconversion particles 320b may move in one direction, and the receiving portion 320 may be driven as a light-transmitting portion.

[0211] Or, if Fig. 9 As shown, when no voltage is applied to the first electrode 210 and / or the second electrode 220 , the light conversion particles 320 b may be uniformly dispersed in the dispersion 320 a to drive the receiving portion 320 as a light blocking portion.

[0212] Therefore, the light path control member according to the embodiment can be driven in two modes according to the user's surrounding environment. That is, when the user needs to transmit light only at a specific viewing angle, the receiving portion is driven as a light blocking portion, or in an environment where the user needs high brightness, a voltage can be applied to drive the receiving portion as a light transmitting portion.

[0213] Therefore, the light path control member according to the embodiment can be implemented in two modes according to the needs of the user, and thus the light path control member can be applied regardless of the environment of the user.

[0214] Meanwhile, the housing portion may be set to a different shape in consideration of driving characteristics and the like.

[0215] Reference Figure 8 and Fig. 9 In a light path control member according to another embodiment, Figure 5 Differently, both ends of the receiving portion 320 may be disposed to be in contact with the buffer layer 410 and the adhesive layer 420 .

[0216] For example, a lower portion of the receiving portion 320 may be disposed in contact with the buffer layer 410 , and an upper portion of the receiving portion 320 may be disposed in contact with the adhesive layer 420 .

[0217] Therefore, the distance between the receiving portion 320 and the first electrode 210 may be reduced, so that the voltage applied from the first electrode 210 may be smoothly transmitted to the receiving portion 320 .

[0218] Therefore, the moving speed of the light conversion particles 320 b in the receiving portion 320 can be increased, thereby improving the driving characteristics of the light path control member.

[0219] In addition, refer to Fig.10 and Fig.11 ,and Figure 8 and Fig. 9 Differently, in the light path control member according to the embodiment, the receiving portion 320 may be provided to have a constant inclination angle θ.

[0220] Specifically, refer to Fig.10 and Fig.11 The receiving portion 320 may be disposed to have an inclination angle θ of greater than 0° to less than 90° relative to the first substrate 110. Specifically, the receiving portion 320 may extend upward while having an inclination angle θ of greater than 0° to less than 90° relative to one surface of the first substrate 110.

[0221] Therefore, when the light path control member is used together with the display panel, the moire caused by the overlapping phenomenon between the pattern of the display panel and the receiving portion 320 of the light path control member can be alleviated, thereby improving the visibility of the user.

[0222] In the following, reference will be made to Figure 12 to Figure 14 Description of a Light Path Control Member According to Another Embodiment In the description of a light path control member according to another embodiment, the same or similar description as that of the above light path control member according to the embodiment will be omitted, and the same reference numerals will be assigned to the same configuration.

[0223] In the light path control member according to another embodiment, a polymer material layer may be provided between the adhesive layer and the electrode to reduce migration of the above-mentioned additives.

[0224] Reference Fig.12 , the light path control member according to another embodiment may include a polymer material layer disposed on the first electrode 210 or the second electrode 220 .

[0225] Reference Fig.12 , the first electrode 210 may be disposed on the first substrate 110 , the buffer layer 410 defined as a first polymer material layer may be disposed on the first electrode 210 , the second electrode 220 may be disposed on the second substrate 120 , and the second polymer material layer 430 may be disposed on the second electrode 220 .

[0226] The first polymer material layer and the second polymer material layer 430 may be the same as or different from each other.

[0227] The first polymer material layer 410 can improve the adhesive property between the first electrode 210 and the light conversion part 300 formed of resin. Specifically, the first polymer material layer 410 is located between the first electrode 210 and the light conversion part 300, thereby reducing the degradation of the adhesive property caused by the difference in surface energy of different materials.

[0228] The second polymer material layer 430 may improve the adhesive strength between the second electrode 220 and the adhesive layer 420. Specifically, the second polymer material layer 430 is located between the second electrode 220 and the adhesive layer 420, thereby reducing the degradation of adhesive characteristics caused by the difference in surface energy of different materials.

[0229] At least one of the first polymer material layer and the second polymer material layer 430 may have a high surface energy on the surface of the transparent electrode film, and may be a material capable of coating a thin film at a high density. For example, at least one of the first polymer material layer and the second polymer material layer 430 may include polyurethane acrylate. Polyurethane acrylate can be coated with a thin film at a high density. Therefore, the release additive can be prevented from migrating to the interface between the polymer and the ceramic and the interface between the polymer and the metal.

[0230] At least one of the first polymer material layer and the second polymer material layer 430 may be a coating obtained by curing polyurethane acrylate at 50° C. to 80° C. for more than 24 hours. In order to prevent the release additive from migrating within the polymer material layer of at least one of the first polymer material layer and the second polymer material layer 430, the coating may be manufactured by curing polyurethane acrylate at 50° C. to 80° C. for more than 24 hours. Therefore, the first polymer material layer may have high adhesive strength to the photoconversion unit 300 (which is a resin layer). That is, as the release additive in the resin layer migrates, the interface separation between the photoconversion unit 300 and the first electrode 210 may be prevented. In addition, the second polymer material layer 430 may have high adhesive strength to the adhesive layer 420. That is, the second polymer material layer 430 may be located between the adhesive layer 420 and the second electrode 220 to prevent the adhesive layer 420 from being peeled off from the second electrode 220 by the release additive.

[0231] The second polymer material layer 430 may be in contact with the second electrode 220. The upper surface of the second polymer material layer 430 may be in direct contact with the second electrode 220. For example, the second polymer material layer 430 may include a third interface between the upper surface of the second polymer material layer 430 and the second electrode 220. The third interface may not include an additive. That is, the third interface between the upper surface of the second polymer material layer 430 and the second electrode 220 may not include a release additive that migrates from the partition wall portion, so that the second polymer material layer 430 and the second electrode 220 may have excellent adhesion properties. For example, the third interface may include an additive in an amount of 0.1% or less. For example, the third interface may include an additive in an amount of 0.05% or less. For example, the third interface may include an additive in an amount of 0.01% or less. Therefore, the adhesive strength of the second polymer material layer 430 and the second electrode 220 at the third interface may be excellent.

[0232] Meanwhile, when the polymer material layer is formed by rapid curing at a high temperature, the density may be reduced. For example, when the polymer material layer is cured at a temperature of 80° C. or more and / or for less than 24 hours, the release additive may pass through the polymer material layer. Therefore, the second polymer material layer may not be able to prevent the peeling between the second electrode and the adhesive layer.

[0233] The first polymer material layer and the second polymer material layer 430 according to the embodiment can be manufactured at the same time, so that the process efficiency can be improved. For example, the first polymer material layer and the second polymer material layer 430 according to the embodiment can contain the same material. Therefore, the first polymer material layer and the second polymer material layer 430 can be formed by completely disposing the polymer material layer on the transparent electrode film at the same time.

[0234] At least one of the first polymer material layer and the second polymer material layer 430 according to the embodiment may be a high-density polymer material layer. For example, at least one of the first polymer material layer and the second polymer material layer 430 may include a polymer material layer having a high cross-linking density. Here, the high density may be determined by the Kel density as the cross-linking density.

[0235] At least one of the first polymer material layer and the second polymer material layer 430 may have a Kel density (Kel fraction) of 90% or more. For example, at least one of the first polymer material layer and the second polymer material layer 430 may have a Kel density of 95% or more. When at least one of the first polymer material layer and the second polymer material layer 430 has a Kel density of 90% or less, it may be difficult to prevent migration of the release additive due to low crosslinking density.

[0236] The first polymer material layer may include a material with a higher density than the material layer used as a normal buffer layer. For example, the first polymer material layer may be a polymer material layer having a higher crosslinking density than the material layer used as a normal buffer layer. Therefore, in addition to improving the bonding strength between the existing heterogeneous interfaces, it may also have the additional effect of preventing the migration of the release additive. Therefore, in an embodiment, the initial bonding strength may be continuously maintained by the first polymer material layer.

[0237] In addition, the second polymer material layer 430 can prevent the problem of the release additive passing through the adhesive layer made of OCA. For example, the second polymer material layer 430 can be located between the adhesive layer and the upper transparent electrode film. That is, in an embodiment, the second polymer material layer 430 can be arranged between the adhesive layer and the upper transparent electrode film without directly adhering the adhesive layer to the upper transparent electrode film. Therefore, the problem of the release additive passing through the adhesive layer and peeling between the adhesive layer and the upper transparent electrode film can be solved. That is, in an embodiment, since the second polymer material layer 430 is provided, the release additive may not be located at the interface between the second polymer material layer 430 and the electrode located on the second polymer material layer 430, so that the bonding strength can be improved.

[0238] Table 1 shows test results of transmittance, surface resistance, and adhesive strength according to the thickness of the polymer material layer. The adhesive strength described in Table 1 may refer to the adhesive strength between the second electrode and the second polymer material layer or the adhesive strength between the first polymer material layer and the partition wall.

[0239] At least one of the first polymer material layer and the second polymer material layer 430 may have a thickness of 300 nm to 1500 nm. For example, at least one of the first polymer material layer and the second polymer material layer 430 may have a thickness of 400 nm to 1000 nm. For example, at least one of the first polymer material layer and the second polymer material layer 430 may have a thickness of 400 nm to 800 nm.

[0240] For example, when the thickness of the second polymer material layer 430 is less than 300 nm, the second polymer material layer 430 cannot prevent the release additive from migrating to the surface of the second electrode 220 , and thus may reduce the adhesive strength between the second electrode 220 and the adhesive layer 420 .

[0241] For example, when the thickness of the second polymer material layer 430 is 1500 nm or more, as the surface resistance increases, the driving characteristics of the light path control member may deteriorate. Specifically, when the thickness of the second polymer material layer 430 exceeds 1500 nm, the surface resistance may exceed 7.5 (×10 10 Ω / □), so the driving characteristics may deteriorate.

[0242] [Table 3]

[0243]

[0244]

[0245] Will refer to Fig.13 and Fig.14 The adhesive strength of an example of a light path control member according to another embodiment and a comparative example are described.

[0246] Fig.13 and Fig.14 is an adhesive strength test result measured by a peeling test in which the second substrate provided with the second electrode is lifted 180 degrees.

[0247] Fig.13 is a graph showing adhesive strength test results under various conditions according to Comparative Examples.

[0248] Reference Fig.13 In the comparative example, the interface between the partition wall portion and the adhesive layer immediately after bonding has an adhesive strength of about 226 gf / 25 mm, but there is a problem that the interface between the adhesive layer and the upper electrode is peeled off over time due to the migration of the release additive in the partition wall portion to the interface between the adhesive layer and the upper electrode. That is, in the comparative example, the adhesive layer and the second electrode may be peeled off over time.

[0249] Fig.14 is a graph showing adhesive strength test results under various conditions according to Examples.

[0250] In this case, the thickness of the primer layer exemplified is 500 nm and polyurethane acrylate is used.

[0251] Reference Fig.14 , in the examples, the interface between the peeled adhesive layer and the partition wall portion in the 180 degree peel test measured immediately after bonding and after a certain time respectively.

[0252] In the example, the adhesive layer includes a first interface located between the upper surface of the adhesive layer and the second polymer material layer and a second interface located between the lower surface of the adhesive layer and the light conversion part, and the bonding strength between the first interface and the second interface measured at room temperature immediately after the polymer material layer is adhered to the light conversion part through the adhesive layer is greater than 300 gf / 25 mm, and after the second polymer material layer is adhered to the light conversion part through the adhesive layer, the bonding strength between the first interface and the second interface measured after 24 hours at 60°C is greater than 300 gf / 25 mm.

[0253] Specifically, in the example, the adhesive layer includes a first interface located between the upper surface of the adhesive layer and the second polymer material layer and a second interface located between the lower surface of the adhesive layer and the light conversion part, and the bonding strength between the first interface and the second interface measured at room temperature immediately after the polymer material layer is adhered to the light conversion part through the adhesive layer is greater than 400 gf / 25 mm, and after the second polymer material layer is adhered to the light conversion part through the adhesive layer, the bonding strength between the first interface and the second interface measured after 24 hours at 60°C is greater than 400 gf / 25 mm.

[0254] In the example, the adhesive layer includes a first interface located between the upper surface of the adhesive layer and the second polymer material layer and a second interface located between the lower surface of the adhesive layer and the light conversion part, and the bonding strength between the first interface and the second interface measured at room temperature immediately after the polymer material layer is adhered to the light conversion part through the adhesive layer is greater than 450gf / 25mm, and after the second polymer material layer is adhered to the light conversion part through the adhesive layer, the bonding strength between the first interface and the second interface measured after 24 hours at 60°C is greater than 450gf / 25mm.

[0255] That is, in the example, since the second interface was peeled off in each test measured immediately after bonding and one day after bonding, it can be seen that the bonding strength immediately after the first interface bonding was above 480 gf / 25 mm, and the bonding strength after 24 hours at 60°C was above 460 gf / 25 mm.

[0256] When the thickness of the polymer material layer having a Kel fraction of 95% or more is 500 nm or more, the initial bonding strength can be maintained by preventing the migration of the release additive. In the example of the figure, since the initial bonding strength between the bonding layer and the partition wall portion is 400 gf / 25 mm or more, the bonding strength of 400 gf / 25 mm or more can be maintained even after a period of time.

[0257] Meanwhile, in the case of a polymer material layer having a Kel fraction of 90% to 95%, a thickness of 800 nm or more may be required.

[0258] In the following, reference will be made to Figures 15 to 21 A method of manufacturing the light path control member according to the embodiment is described.

[0259] Reference Fig.15 , prepare a first substrate 110 and an electrode material for forming a first electrode. Then, the first electrode may be formed by coating or depositing the electrode material on one surface of the first substrate. Specifically, the electrode material may be formed on the entire surface of the first substrate 110. Thus, the first electrode 210 formed as a surface electrode may be formed on the first substrate 110.

[0260] Then, refer to Fig.16 The resin layer 350 may be formed by coating a resin material on the first electrode 210. Specifically, the resin layer 350 may be formed by coating a polyurethane resin or an acrylic resin on the first electrode 210.

[0261] In this case, the buffer layer 410 may be additionally disposed on the first electrode 210 before the resin layer 350 is disposed. Specifically, by disposing the resin layer 350 on the buffer layer 410 after disposing the buffer layer 410 having good adhesive strength to the resin layer 350 on the first electrode 210, the adhesive strength of the resin layer 350 may be improved.

[0262] For example, the buffer layer 410 may include an organic material including an oleophilic group such as —CH—, an alkyl group, etc. having good adhesion to an electrode and a hydrophilic group such as —NH, —OH, —COOH, etc. having good adhesion to the resin layer 410 .

[0263] The resin layer 350 may be disposed on a partial region of the first substrate 110. That is, the resin layer 350 may be disposed in a region smaller than the first substrate 110. Therefore, a region where the resin layer 350 is not disposed and the first electrode 210 is exposed may be formed on the first substrate 110. In addition, when the buffer layer 410 is disposed on the first electrode 210, a region where the buffer layer 410 is exposed may be formed.

[0264] Specifically, the dimension of the third length of the resin layer 350 extending in the first direction can be smaller than the dimension of the first length of the first substrate 110 extending in the first direction, and the dimension of the third width of the resin layer 350 extending in the second direction can be smaller than or equal to the dimension of the first width of the first substrate 110 extending in the second direction.

[0265] That is, the length of the resin layer 350 may be smaller than the length of the first substrate 110 , and the width of the resin layer 350 may be equal to or smaller than the width of the first substrate 110 .

[0266] Then, refer to Fig.17 , the resin layer 350 may be patterned to form a plurality of partition walls 310 and a plurality of receiving portions 320 in the resin layer 350. Specifically, an intaglio portion may be formed in the resin layer 350, thereby forming an intaglio-shaped receiving portion 320 and an embossed-shaped partition wall 310 between the intaglio portions.

[0267] Thus, the light conversion part 300 including the partition wall part 310 and the receiving part 320 may be formed on the first substrate 110 .

[0268] In addition, the buffer layer 410 exposed on the first electrode 210 may be removed to expose the first electrode 210 in the region where the first substrate 110 protrudes.

[0269] Then, refer to Fig.18 , prepare a second electrode and an electrode material for forming the second substrate 120. Then, the second electrode may be formed by coating or depositing the electrode material on one surface of the second substrate.

[0270] Specifically, the electrode material may be formed on the entire surface of the second substrate 120. Therefore, the second electrode 220 formed as a surface electrode may be formed on the second substrate 120.

[0271] The size of the second substrate 120 may be smaller than that of the first substrate 110. In addition, the size of the second substrate 120 may be smaller than that of the resin layer 350.

[0272] Specifically, the second length of the second substrate 120 extending in the first direction may be larger than the third length of the resin layer 350 extending in the first direction, and the second width of the second substrate 120 extending in the second direction may be smaller than the third width of the resin layer 350 extending in the second direction.

[0273] Then, refer to Fig.19 , the adhesive layer 420 may be formed by coating an adhesive material on the second electrode 220. Specifically, a light-transmitting adhesive layer capable of transmitting light may be formed on the second electrode 220. For example, the adhesive layer 420 may include an optically transparent adhesive layer OCA.

[0274] The adhesive layer 420 may be disposed on a partial region of the light conversion part 300. That is, the adhesive layer 420 may be disposed in a region smaller than the area of ​​the light conversion part 300. Therefore, a region where the adhesive layer 410 is not disposed and the light conversion part 300 is exposed may be formed on the light conversion part 300.

[0275] Specifically, a fourth length of the adhesive layer 420 extending in the first direction may be greater than a third length of the light conversion portion 300 extending in the first direction, and a fourth width of the adhesive layer 420 extending in the second direction may be less than a third width of the light conversion portion 300 extending in the second direction.

[0276] Then, refer to Fig. 20 , the first substrate 110 and the second substrate 120 may be bonded. Specifically, the second substrate 120 may be disposed on the light conversion part 300 , and the second substrate 120 and the light conversion part 300 may be bonded by an adhesive layer 420 disposed under the second substrate 120 .

[0277] Therefore, the first substrate 110 , the light conversion part 300 , and the second substrate 120 may be sequentially stacked in the thickness direction of the first substrate 110 , the light conversion part 300 , and the second substrate 120 .

[0278] In this case, since the size of the second substrate 120 is set to be smaller than that of the resin layer 350 , the plurality of partition wall parts 310 and the plurality of receiving parts 320 may be exposed in a region on the light conversion part 300 where the second substrate 120 is not provided.

[0279] Specifically, since the dimension of the second width of the second substrate 120 extending in the second direction is smaller than the dimension of the third width of the resin layer 350 extending in the second direction, a plurality of partition wall portions 310 and a plurality of accommodating portions 320 can be exposed in the end region of at least one of one end and the other end in the width direction facing the resin layer 350.

[0280] Subsequently, the light conversion material 380 may be injected between the partition walls 310, ie, the housing 320. Specifically, the light conversion material in which light absorbing particles such as carbon black are dispersed in an electrolyte solvent including a paraffin solvent or the like may be injected between the partition walls, ie, the housing 320.

[0281] For example, after a dam portion extending in the longitudinal direction of the light conversion unit 300 is provided on the receiving portion and the partition wall portion of the light conversion unit 300 where the second substrate 120 is not provided, the electrolyte solvent can be injected into the receiving portion 320 between the dam portion and the side surface of the light conversion unit 300 by a capillary injection method.

[0282] Then, refer to Fig.21 , one light path control member may be manufactured by cutting the light conversion part 300. Specifically, the light conversion part 300 may be cut along a longitudinal direction of the light conversion part 300.

[0283] That is to say, you can follow Fig.21 The light conversion unit 300, the buffer layer 410 below the light conversion unit 300, the first electrode 210 and the first substrate 110 are cut by the dotted lines shown. A plurality of light path control members A and B can be formed by the cutting process. Fig.23 is a diagram showing one of a plurality of light path control members.

[0284] Specifically, the light conversion part 300 may be cut such that the first substrate 110 , the second substrate 120 , and the side surfaces of the light conversion part 300 in the width direction may be disposed on the same plane.

[0285] Therefore, both ends of the second substrate 120 , the second electrode 220 , or the adhesive layer 420 in the second direction and both ends of the light conversion part 300 in the second direction may be disposed on the same plane.

[0286] That is, both ends of the adhesive layer 420 in the second direction and both ends of the light conversion part 300 in the second direction may be connected to each other.

[0287] Alternatively, depending on errors during the process, both ends of the second substrate 120 , the second electrode 220 , or the adhesive layer 420 in the second direction may be disposed at outer sides than both ends of the light conversion unit 300 in the second direction.

[0288] Subsequently, the buffer layer 410 disposed on the first substrate 110 and / or the adhesive layer 420 disposed under the second substrate 120 may be partially removed to form a connection portion exposing the electrode.

[0289] Specifically, when the buffer layer 410 is provided on the first electrode without the light conversion part 300 provided on the upper surface of the first substrate 110, the first connection part 211 may be formed on the first substrate 110 by removing a portion of the first buffer layer 410 to expose the first electrode 210 or by not providing the buffer layer 410 on the first electrode without the light conversion part 300 provided from the beginning. In addition, when the adhesive layer 420 is provided on the second electrode without the light conversion part 300 provided on the lower surface of the second substrate 120, the second connection part 221 may be formed under the second substrate 120 by removing a portion of the adhesive layer 420 or by not providing the adhesive layer on the second electrode without the light conversion part 300 provided during the bonding process.

[0290] A printed circuit board or a flexible printed circuit board may be connected to the connection portion through an anisotropic conductive film (ACF) or the like, and the printed circuit board may be connected to an external power source to apply a voltage to the light path control member.

[0291] In the following, reference will be made to Figure 22 to Figure 26 A display device to which the light path control member according to the embodiment is applied will be described.

[0292] Reference Fig. 22 and Fig.23 , the light path controlling member 1000 according to the embodiment may be disposed above or below the display panel 2000 .

[0293] The display panel 2000 and the light path control member 1000 may be arranged to be bonded to each other. For example, the display panel 2000 and the light path control member 1000 may be bonded to each other through an adhesive layer 1500. The adhesive layer 1500 may be transparent. For example, the adhesive layer 1500 may include an adhesive or an adhesive layer including an optically transparent adhesive material.

[0294] The adhesive layer 1500 may include a release film. Specifically, when the light path control member and the display panel are bonded, the light path control member and the display panel may be bonded after removing the release film.

[0295] At the same time, refer to Fig. 22 and Fig.23 , one end or one end and the other end of the light path control member may protrude, and the light conversion unit may not be provided at the protruding portion. The protruding area is an electrode connection portion that exposes the first electrode 210 and the second electrode 220, and an external printed circuit board can be connected to the light path control member through the electrode connection portion.

[0296] The display panel 2000 may include a first substrate 2100 and a second substrate 2200. When the display panel 2000 is a liquid crystal display panel, the light path control member may be formed below the liquid crystal panel. That is, when the surface viewed by the user in the liquid crystal panel is defined as the upper part of the liquid crystal panel, the light path control member may be disposed below the liquid crystal panel. The display panel 2000 may be formed in a structure in which a first substrate 2100 including a thin film transistor (TFT) and a pixel electrode and a second substrate 2200 including a color filter layer are combined with each other, with a liquid crystal layer interposed therebetween.

[0297] In addition, the display panel 2000 may be a liquid crystal display panel of a color filter on transistor (COT) structure, in which a thin film transistor, a color filter, and a black electrolyte are formed at the first 'substrate 2100, and a second 'substrate 2200 is bonded to the first 'substrate 2100 with a liquid crystal layer interposed therebetween. That is, a thin film transistor may be formed on the first 'substrate 2100, a protective film may be formed on the thin film transistor, and a color filter layer may be formed on the protective film. In addition, a pixel electrode in contact with the thin film transistor may be formed on the first 'substrate 2100. At this time, in order to increase the aperture ratio and simplify the mask process, the black electrolyte may be omitted, and a common electrode may be formed to serve as a black electrolyte.

[0298] In addition, when the display panel 2000 is a liquid crystal display panel, the display device may further include a backlight unit 3000 that provides light from a rear surface of the display panel 2000 .

[0299] That is to say, Fig. 22 As shown, the light path control member may be disposed below the liquid crystal panel and on the backlight unit 3000 , and the light path control member may be disposed between the backlight unit 3000 and the display panel 2000 .

[0300] Or, if Fig.23As shown, when the display panel 2000 is an organic light emitting diode panel, the light path control member can be formed on the organic light emitting diode panel. That is, when the surface seen by the user in the organic light emitting diode panel is defined as the upper part of the organic light emitting diode panel, the light path control member can be provided on the organic light emitting diode panel. The display panel 2000 may include a self-luminous element that does not require a separate light source. In the display panel 2000, a thin film transistor may be formed on the first substrate 2100, and an organic light emitting element in contact with the thin film transistor may be formed. The organic light emitting element may include an anode, a cathode, and an organic light emitting layer formed between the anode and the cathode. In addition, a second substrate 2200 configured to be used as an encapsulation substrate for encapsulation may be further included on the organic light emitting element.

[0301] That is, light emitted from the display panel 2000 or the backlight unit 3000 may move from the second substrate 120 of the light path control member toward the first substrate 110 .

[0302] In addition, although not shown in the drawings, a polarizing plate may be further provided between the light path control member 1000 and the display panel 2000. The polarizing plate may be a linear polarizing plate or a polarizing plate that prevents external light from being reflected. For example, when the display panel 2000 is a liquid crystal display panel, the polarizing plate may be a linear polarizing plate. In addition, when the display panel 2000 is an organic light emitting display panel, the polarizing plate may be a polarizing plate that prevents external light from being reflected.

[0303] In addition, an additional functional layer 1300, such as an anti-reflection layer, an anti-glare layer, etc., may be further provided on the light path control member 1000. Specifically, the functional layer 1300 may be bonded to one surface of the first substrate 110 of the light path control member. Although not shown in the drawings, the functional layer 1300 may be bonded to the first substrate 110 of the light path control member via an adhesive layer. In addition, a release film for protecting the functional layer may also be provided on the functional layer 1300.

[0304] In addition, a touch panel may be further provided between the display panel and the light path control member.

[0305] Although the light path control member is shown in the drawings as being disposed on the upper portion of the display panel, the embodiments are not limited thereto, and the light path control member may be disposed in various positions, such as a light-adjustable position, i.e., the lower portion of the display panel or between the second substrate and the first substrate of the display panel, etc.

[0306] In addition, the light conversion part of the light path control member according to the embodiment is shown in the drawings in a direction parallel to or perpendicular to the outer surface of the second substrate, but the light conversion part is formed to be inclined at a predetermined angle to the outer surface of the second substrate. Therefore, the ripple phenomenon occurring between the display panel and the light path control member can be reduced.

[0307] Reference Figure 24 to Figure 26 , the light path controlling member according to the embodiment can be applied to various display devices.

[0308] Reference Figure 24 to Figure 26 , the light path control member according to the embodiment can be applied to a display device that displays a picture.

[0309] For example, Fig.24 As shown, when power is applied to the light path control member, the receiving portion functions as a light-transmitting portion, so that the display device can be driven in a public mode, such as Fig.25 As shown, when power is not applied to the light path controlling member, the housing portion functions as a light blocking portion, so that the display device can be driven in the light blocking mode.

[0310] Therefore, the user can easily drive the display device in the privacy mode or the normal mode according to the application of power.

[0311] The light emitted from the backlight unit or the self-luminous element may move from the first substrate to the second substrate. Alternatively, the light emitted from the backlight unit or the self-luminous element may also move from the second substrate to the first substrate.

[0312] In addition, refer to Fig.26 , a display device to which the light path control member according to the embodiment is applied may also be applied inside a vehicle.

[0313] For example, a display device including the light path control member according to the embodiment may display video confirmation information of the vehicle and a moving route of the vehicle. The display device may be provided between a driver seat and a passenger seat of the vehicle.

[0314] In addition, the light path control member according to the embodiment may be applied to a dashboard that displays the speed, engine, warning signal, etc. of a vehicle.

[0315] In addition, the light path controlling member according to the embodiment may be applied to a front glass (FG) or left and right window glasses of a vehicle.

[0316] The features, structures, effects, etc. described in the above embodiments are included in at least one embodiment of the present invention, and are not limited to one embodiment. In addition, those skilled in the art can combine or modify the features, structures, and effects shown in each embodiment for other embodiments. Therefore, it should be understood that such combinations and modifications are included within the scope of the present invention.

[0317] In addition, the above embodiments are mainly described, but these embodiments are only examples, and do not limit the present invention, and those skilled in the art will understand that, without departing from the basic features of the present invention, several changes and applications not proposed above can be made. For example, the various components specifically shown in the embodiments can be modified and implemented. In addition, it should be interpreted that the differences associated with such changes and such applications are included in the scope of the present invention defined in the appended claims.

Claims

1. A light path control component, comprising: a first substrate; A first electrode, disposed on the first substrate; a light conversion unit, disposed on the first electrode and formed of a light-curable resin; a second substrate, disposed on the first substrate; A second electrode is disposed below the second substrate; as well as an adhesive layer disposed between the light conversion unit and the second electrode, Wherein, the light conversion part includes partition walls and receiving parts which are alternately arranged. The receiving portion has a light transmittance that changes according to an applied voltage, The adhesive layer includes a first interface between an upper surface of the adhesive layer and the second electrode and a second interface between a lower surface of the adhesive layer and the light conversion unit. The partition wall portion includes: A first region of 30 μm from the upper surface of the partition wall portion toward the first substrate; A third region of 30 μm from the lower surface of the partition wall portion toward the second substrate; and a second region between the first region and the third region, and The Si content in the first region measured by X-ray photoelectron spectroscopy (XPS) is less than 2 at %.

2. The optical path control member according to claim 1, wherein: The first interface and the second interface have different adhesive strengths from each other, After the second electrode and the light conversion unit are bonded together via the bonding layer, the bonding strength of the second interface measured at 60° C. for 24 hours is 300 gf / 25 mm or more.

3. The light path control member according to claim 1, wherein: The difference between the Si content in the first region measured by XPS and the Si content in the third region measured by XPS is 1 at % or less.

4. The light path control member according to claim 1, wherein: The difference between the Si content in the first region measured by XPS and the Si content in the second region measured by XPS is 1 at % or less.

5. The light path control member according to claim 1, in, The photocurable resin includes oligomers, monomers, photopolymerization initiators and additives.

6. The light path control member according to claim 5, wherein: The swelling rate of the photocurable resin is less than 10%.

7. The light path control member according to claim 5, wherein: The oligomer includes urethane acrylate.

8. The light path control member according to claim 5, wherein: The number of branches of the monomer is five or more.

9. The light path control member according to claim 5, wherein: When the weight of the photocurable resin is 100 wt %, the content of the additive is 0.5 wt % or less.

10. The light path control member according to claim 1, further comprising: a first polymer material layer between the first electrode and the light conversion unit; as well as A second polymer material layer is between the second electrode and the adhesive layer.

11. The light path control member according to claim 10, wherein: The thickness of any one of the first polymer material layer and the second polymer material layer is 300 nm to 1500 nm.

12. The light path control member according to claim 10, wherein: The adhesive layer includes a first interface between the upper surface of the adhesive layer and the second polymer material layer and a second interface between the lower surface of the adhesive layer and the light conversion portion, The bonding strength between the first interface and the second interface is 300 gf / 25 mm or more.

13. The light path control member according to claim 10, wherein: The light conversion unit is formed of a photocurable resin.

14. The light path control member according to claim 13, wherein: The photocurable resin includes oligomers, monomers, photopolymerization initiators and additives.

15. The light path control member according to claim 10, wherein: The first polymer material layer and the second polymer material layer include polyurethane acrylate.

16. The light path control member according to claim 14, wherein: The second polymer material layer includes a third interface between an upper surface of the second polymer material layer and the second electrode, and The third interface does not include the additive.

17. A display device comprising: Display panel; as well as According to the light path control member according to claim 1, the light path control member is arranged on the display panel.