Method for quickly determining the most dangerous stage of thermal runaway of energetic material synthesis reaction

By using equal-interval conversion rate sampling and differential scanning calorimetry to rapidly determine the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials, the problem of insufficient detection speed and accuracy in existing technologies is solved, and rapid and accurate thermal safety parameter testing is achieved.

CN117347433BActive Publication Date: 2026-11-10XIAN MODERN CHEM RES INST
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311272020.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-09-28
Publication Date
2026-11-10
Estimated Expiration
2043-09-28

AI Technical Summary

Technical Problem

Existing technologies are unable to quickly and accurately determine the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials, resulting in inaccurate thermal safety parameter testing and a long detection process.

Method used

By employing an equal-interval conversion rate sampling method combined with differential scanning calorimetry, the most dangerous stage of thermal runaway can be quickly determined by calculating the highest temperature of the synthesis reaction and the thermal stability of the materials.

Benefits of technology

It significantly shortens the detection cycle, improves the accuracy of judgment, avoids misjudgment, and reduces experimental risks and the number of times.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117347433B_ABST
    Figure CN117347433B_ABST
Patent Text Reader

Abstract

The application provides a method for rapidly determining the most dangerous stage of thermal runaway of an energetic material synthesis reaction. In the process of sampling and thermal stability testing of the material, the inapplicability of equal-time-interval sampling to the rapid reaction of the energetic material is analyzed, the equal-interval conversion rate sampling is determined in the reaction process, and the thermal stability of the material with uniform component change in the reaction process is studied. Meanwhile, the change of the cumulative degree of the reaction process is obtained according to the reaction process calorimetry curve, the highest temperature of the synthesis reaction is further obtained, and finally the most dangerous stage of thermal runaway is determined according to the difference between the highest temperature of the synthesis reaction and the initial decomposition temperature of the material at each sampling point. The method of the application can shorten the research period by more than 50% by equal-interval conversion rate sampling and rapid determination of thermal stability by differential scanning calorimetry. The method of the application avoids the misjudgment of the most dangerous stage caused by equal-time-interval sampling analysis.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of energetic materials technology, and relates to the synthesis reaction process of energetic materials, specifically to a method for rapidly determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials. Background Technology

[0002] Numerous exothermic reactions exist in the synthesis of energetic materials, such as oxidation, chlorination, sulfonation, neutralization, condensation, nitration, azidation, and esterification. Nitration, oxidation, and azidation are typical examples of strongly exothermic reactions. In these reactions, a significant amount of heat is released during the initial feeding phase. When the rate of exothermic reaction exceeds the heat transfer rate of the cooling system, the reactor temperature rises sharply. This gradual increase in system temperature leads to a gradual acceleration of the reaction rate, subsequently causing further heat accumulation and temperature rise within the reactor. After a continuous cycle of "exothermic reaction - temperature rise - accelerated reaction - accelerated exothermic reaction," the exothermic capacity of the reactor eventually exceeds its cooling capacity. The reaction system rapidly heats up in a near-adiabatic state, causing decomposition of reactants, intermediates, and products, a sudden pressure increase, and the generation of large amounts of vapor and gas. Ultimately, this can lead to reactor overpressure, material ejection, and even combustion or explosion. Therefore, the thermal safety of strongly exothermic reactions plays a crucial role in the synthesis of energetic materials.

[0003] In the entire synthesis reaction of energetic materials, thermal runaway is possible at every stage. Under stable conditions such as reaction temperature and stirring, the occurrence of thermal runaway depends on changes in the accumulation degree of the reactants. For the synthesis reaction, the reaction system mainly consists of raw materials, intermediates, solvents, by-products, and products. The stability and content of these materials directly affect the stability of the reaction system and the consequences of thermal runaway. Furthermore, the amount of unconverted reactants and the thermal stability of the reactants change over time. Therefore, the accumulation degree becomes a crucial factor influencing thermal runaway in dynamic processes. Thus, determining the moment of maximum accumulation (maximum potential exothermic reaction) is essential for identifying the dangerous stage of thermal runaway. Simultaneously, the thermal stability of the reactants also changes over time, often due to the instability of intermediates. Since the trigger for thermal runaway in the target reaction must be assumed to occur at the worst possible moment—that is, when the accumulation degree of the most dangerous material reaches its maximum or the thermal stability of the reaction mixture is at its worst—it is necessary to address the problem of identifying the dangerous stage of thermal runaway in dynamic processes. Therefore, determining the most dangerous stage of thermal runaway in the target reaction is technically challenging and will affect the accuracy of testing thermal safety parameters for runaway reactions.

[0004] Current methods for determining thermal stability often involve sampling at the beginning and end of the reaction to test the endpoint, or sampling at equal time intervals to test thermal stability. For rapid reactions with strong exothermic reactions in the synthesis of energetic materials, these methods have the following problems: (1) For rapid reactions with intermediates, important information about intermediate changes may be missed; (2) For rapid reactions with strong exothermic reactions, sampling at equal time intervals may miss the rapid change in reactant concentration; this makes it very difficult to determine the most dangerous stage of thermal runaway in the reaction process, and will affect the accuracy of the thermal safety parameter test for runaway reaction; (3) It takes a long time. For example, GB / T42300-2022 requires sampling the materials of the reaction endpoint system for adiabatic accelerated testing, and the temperature T corresponding to the time when the maximum reaction rate is reached under adiabatic conditions is 24 hours based on the obtained adiabatic temperature rise and the time T. D24 The entire process of conducting a hazard assessment and determining the most dangerous stage of thermal runaway takes at least two days. Summary of the Invention

[0005] To address the shortcomings of existing technologies, the present invention aims to provide a method for rapidly determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials, thereby solving the technical problem in existing technologies that it is difficult to balance detection accuracy with detection speed.

[0006] To solve the above-mentioned technical problems, the present invention adopts the following technical solution:

[0007] A method for rapidly determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials, comprising the following steps:

[0008] Step 1: Conduct a calorimetric test.

[0009] Calorimetric experiments were conducted on the target reaction. Based on the reaction calorimetric curve, the change curve of the reaction conversion rate over time was obtained, and the thermodynamic parameters and specific heat capacity parameters of the target reaction were obtained.

[0010] Step 2, Sampling:

[0011] Sampling is performed during the target reaction process based on equal-interval conversion rates.

[0012] Step 3: Calculate the highest temperature of the synthesis reaction at the sampling point:

[0013] The synthesis reaction of the energetic materials is divided into batch reaction and semi-batch reaction.

[0014] For batch reactions, the adiabatic temperature rise ΔT of the target reaction is obtained based on the target reaction thermodynamic parameters and specific heat capacity parameters obtained in step one. ad,rx Then, based on the reaction process temperature T p Cumulativeity of sampling points X acThe maximum temperature of the synthesis reaction, MTSR, was calculated using Formula I.

[0015] MTSR = T p +X ac ΔT ad,rx Formula I.

[0016] For a semi-batch reaction, the adiabatic temperature rise ΔT of the target reaction is obtained based on the thermodynamic parameters and specific heat capacity parameters of the target reaction obtained in step one. ad,rx Then, based on the changes in quality and accumulation during the feeding process, the possible temperatures that may be reached after thermal runaway occurs at each stage of the reaction process are obtained; the highest temperature of the synthesis reaction is the maximum value that may be reached after thermal runaway occurs at each stage. For specific calculations, see Formulas II and III.

[0017]

[0018] MTSR=(T cf ) max Formula III.

[0019] In the formula:

[0020] T cf This is the temperature that the reaction may reach after thermal runaway occurs;

[0021] T p This is the normal reaction temperature;

[0022] X ac It is the degree of accumulation of reactants;

[0023] ΔT ad,rx It is the adiabatic temperature rise after thermal runaway occurs;

[0024] M r,f It is the mass of the reaction mixture at the end of the feeding process;

[0025] M r(t) It is the instantaneous mass of the reactants;

[0026] MTSR is the highest temperature at which the synthesis reaction occurs;

[0027] Step 4: Test the thermal stability of materials at different sampling points:

[0028] Under the same test conditions, differential scanning calorimetry was used to test the thermal stability of materials at different sampling points, and thermal decomposition curves were obtained. Based on the thermal decomposition curves, the initial decomposition temperature and decomposition peak temperature parameters of materials at each different sampling point were obtained.

[0029] Step 5: Determine the most dangerous stage of thermal runaway:

[0030] By comparing the highest temperature of the synthesis reaction and the initial decomposition temperature of the material at each sampling point, the time point at which the difference between the initial decomposition temperature and the highest temperature of the synthesis reaction is minimized is determined as the most dangerous stage in the synthesis reaction where thermal runaway occurs.

[0031] The present invention also has the following technical features:

[0032] In step two, there should be no fewer than five sampling points.

[0033] In step four, the same test conditions refer to test conditions where the test crucible, heating rate, and nitrogen flow rate are all the same.

[0034] Compared with the prior art, the present invention has the following technical effects:

[0035] (I) The method of the present invention uses equal-interval conversion rate sampling and differential scanning calorimetry to quickly determine thermal stability, which can shorten the research cycle by more than 50%.

[0036] (II) The method of the present invention avoids misjudging the most dangerous stage caused by sampling analysis at equal time intervals.

[0037] (III) The method of the present invention reduces the number of experiments and lowers the risks of calorimetry and sampling in the synthesis process of energetic materials. Attached Figure Description

[0038] Figure 1 This is a curve showing the conversion rate over time.

[0039] Figure 2 The DSC curves of the material at different times during the BuAENA synthesis process are shown.

[0040] The specific content of the present invention will be further explained in detail below with reference to the embodiments. Detailed Implementation

[0041] It should be noted that, unless otherwise specified, all materials and equipment used in this invention are those known in the prior art.

[0042] To address the technical problem of difficulty in determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials, this invention provides a method for determining the most dangerous stage of thermal runaway in the synthesis process of energetic materials. During the sampling and thermal stability testing of process materials, the method analyzes the inapplicability of time-interval sampling to the rapid reactions of energetic materials. It determines that sampling is performed at equal conversion rates during the reaction process to study the thermal stability of materials with uniform component changes during the reaction. Simultaneously, the change in the cumulative reaction rate is obtained based on the calorimetric curve of the reaction process, further determining the maximum temperature of the synthesis reaction. Finally, the most dangerous stage of thermal runaway is determined based on the difference between the maximum temperature of the synthesis reaction at each sampling point and the initial decomposition temperature of the material.

[0043] This invention uses the equal-interval conversion rate method for sampling and analysis, and simultaneously analyzes the dynamic sample composition and thermal stability change patterns. It can determine the dangerous stage of thermal runaway based on the material accumulation degree and thermal stability change patterns.

[0044] Following the above technical solutions, specific embodiments of the present invention are given below. It should be noted that the present invention is not limited to the following specific embodiments, and all equivalent modifications made based on the technical solutions of this application fall within the protection scope of the present invention.

[0045] Example:

[0046] This embodiment provides a method for rapidly determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials. The method is carried out according to the following steps:

[0047] Step 1: Conduct a calorimetric test.

[0048] Calorimetric experiments were conducted on the target reaction. Based on the reaction calorimetric curve, the change curve of the reaction conversion rate over time was obtained, and the thermodynamic parameters and specific heat capacity parameters of the target reaction were obtained.

[0049] Step 2, Sampling:

[0050] Sampling is conducted during the target reaction process based on equal-interval conversion rates, with no fewer than five sampling points.

[0051] Step 3: Calculate the highest temperature of the synthesis reaction at the sampling point:

[0052] The synthesis reaction of the energetic materials is divided into batch reaction and semi-batch reaction.

[0053] For batch reactions, the adiabatic temperature rise ΔT of the target reaction is obtained based on the target reaction thermodynamic parameters and specific heat capacity parameters obtained in step one. ad,rx Then, based on the reaction process temperature T p Cumulativeity of sampling points X ac The maximum temperature of the synthesis reaction, MTSR, was calculated using Formula I.

[0054] MTSR = T p +X ac ΔT ad,rx Formula I.

[0055] For a semi-batch reaction, the adiabatic temperature rise ΔT of the target reaction is obtained based on the thermodynamic parameters and specific heat capacity parameters of the target reaction obtained in step one. ad,rx Then, based on the changes in quality and accumulation during the feeding process, the possible temperatures that may be reached after thermal runaway occurs at each stage of the reaction process are obtained; the highest temperature of the synthesis reaction is the maximum value that may be reached after thermal runaway occurs at each stage. For specific calculations, see Formulas II and III.

[0056]

[0057] MTSR=(T cf ) max Formula III.

[0058] In the formula:

[0059] T cf This is the temperature that the reaction may reach after thermal runaway occurs;

[0060] T p This is the normal reaction temperature;

[0061] X ac It is the degree of accumulation of reactants;

[0062] ΔT ad,rx It is the adiabatic temperature rise after thermal runaway occurs;

[0063] M r,f It is the mass of the reaction mixture at the end of the feeding process;

[0064] M r(t) It is the instantaneous mass of the reactants;

[0065] MTSR is the highest temperature at which the synthesis reaction is performed.

[0066] Step 4: Test the thermal stability of materials at different sampling points:

[0067] Under the same test crucible, heating rate, and nitrogen flow rate, differential scanning calorimetry was used to test the thermal stability of materials at different sampling points, and thermal decomposition curves were obtained. Based on the thermal decomposition curves, the initial decomposition temperature and decomposition peak temperature parameters of materials at each different sampling point were obtained.

[0068] Step 5: Determine the most dangerous stage of thermal runaway:

[0069] By comparing the highest temperature of the synthesis reaction and the initial decomposition temperature of the material at each sampling point, the time point at which the difference between the initial decomposition temperature and the highest temperature of the synthesis reaction is minimized is determined as the most dangerous stage in the synthesis reaction where thermal runaway occurs.

[0070] Application example:

[0071] This application example provides a method for rapidly determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials based on the above embodiments. Specifically, this application example takes the azidation reaction in the synthesis process of BuAENA (butyl-azidoethylnitramine) as an example. Based on the exothermic curve of the azidation reaction at 70°C, a complete curve of the reaction conversion rate versus time is obtained (e.g., Figure 1 (As shown). Based on the above research results, this invention proposes to perform thermal stability analysis by sampling at equal conversion rates.

[0072] Sampling analysis was conducted during the target reaction process based on a 20% equal-interval conversion rate (as shown in Table 1). The sampling points included 0% conversion rate, 20% conversion rate, 40% conversion rate, 60% conversion rate, 80% conversion rate, and 100% conversion rate. The material codes for the samples were 1#sample, 2#sample, 3#sample, 4#sample, 5#sample, and 6#sample, respectively.

[0073] Table 1. Sampling results at different conversion rates in the BuAENA azide reaction.

[0074]

[0075] The azide reaction in the synthesis of BuAENA is a batch reaction. Based on the above studies, the target reaction specific exothermic heat is 61.932 J / g and the specific heat capacity is 1.95 J·g. -1 ·K -1 The adiabatic temperature rise during the azidation reaction was 31.76℃.

[0076] Then, based on the reaction process temperature of 70℃ and the cumulative degree X at the sampling points... ac The highest temperature of the synthesis reaction at each sampling point was calculated using formula (1), as shown in Table 2.

[0077] Table 2 shows the highest synthesis reaction temperatures at different sampling points during the BuAENA synthesis process.

[0078]

[0079]

[0080] Differential scanning calorimetry (DSC) was used to test the thermal stability of materials at different sampling points. Conditions included: sealed crucible, temperature range: room temperature to 350℃, heating rate 10℃ / min, and nitrogen flow rate 50 ml / min. Thermal decomposition curves of the materials at different sampling points, as well as the raw materials and products, were obtained (e.g., ...). Figure 2 As shown in Table 3, its thermal decomposition characteristic parameters are shown in Table 3.

[0081] Table 3 Thermal decomposition characteristic parameters of materials at different times during the BuAENA synthesis process.

[0082]

[0083] From Table 3 and Figure 2 Comparing the thermal decomposition parameters of materials 1 to 6, it can be seen that the initial thermal decomposition temperature of material 1 is 171.80℃. As the reaction proceeds, the initial decomposition temperature increases from 171.80℃ to 239.80℃. The heat release during decomposition shows a trend of first decreasing and then increasing, indicating that the thermal stability of the reaction system is getting better and better.

[0084] By comparing the highest temperature of the synthesis reaction and the initial decomposition temperature of the materials at each sampling point (considering the initial decomposition temperatures of both raw materials and products at the beginning and end of the reaction), the value of the initial decomposition temperature minus the highest temperature of the synthesis reaction is shown in Table 3. Finally, it was determined that the sampling point of material #1, i.e. the initial stage of the reaction (conversion rate of 0%), is the most dangerous stage for thermal runaway.

Claims

1. A method for rapidly determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials, characterized in that, This method is performed according to the following steps: Step 1: Conduct a calorimetric test. Conduct calorimetric experiments on the target reaction, and obtain the reaction conversion rate versus time curve based on the reaction calorimetric curve, thereby obtaining the thermodynamic parameters and specific heat capacity parameters of the target reaction; Step 2, Sampling: Sampling is performed during the target reaction process based on equal-interval conversion rates. Step 3: Calculate the highest temperature of the synthesis reaction at the sampling point: The synthesis reactions of the energetic materials are divided into batch reactions and semi-batch reactions; For batch reactions, the adiabatic temperature rise ΔT of the target reaction is obtained based on the target reaction thermodynamic parameters and specific heat capacity parameters obtained in step one. ad,rx Then, based on the reaction process temperature T p Cumulativeity of sampling points X ac The maximum temperature MTSR of the synthesis reaction was calculated using Formula I. MTSR = T p +X ac ΔT ad,rx Formula I; For a semi-batch reaction, the adiabatic temperature rise ΔT of the target reaction is obtained based on the thermodynamic parameters and specific heat capacity parameters of the target reaction obtained in step one. ad,rx Then, based on the changes in quality and accumulation during the feeding process, the possible temperatures that may be reached after thermal runaway occurs at each stage of the reaction process are obtained; the highest temperature of the synthesis reaction is the maximum value that may be reached after thermal runaway occurs at each stage. For specific calculations, see Formulas II and III. MTSR=(T cf ) max Formula III; In the formula: T cf This is the temperature that the reaction may reach after thermal runaway occurs; T p This is the normal reaction temperature; X ac It is the degree of accumulation of reactants; ΔT ad,rx It is the adiabatic temperature rise after thermal runaway occurs; M r,f It is the mass of the reaction mixture at the end of the feeding process; M r(t) It is the instantaneous mass of the reactants; MTSR is the highest temperature at which the synthesis reaction occurs; Step 4: Test the thermal stability of materials at different sampling points: Under the same test conditions, the thermal stability of materials at different sampling points was tested by differential scanning calorimetry to obtain thermal decomposition curves. Based on the thermal decomposition curves, the initial decomposition temperature and decomposition peak temperature parameters of materials at each different sampling point were obtained. Step 5: Determine the most dangerous stage of thermal runaway: By comparing the highest temperature of the synthesis reaction and the initial decomposition temperature of the material at each sampling point, the time point at which the difference between the initial decomposition temperature and the highest temperature of the synthesis reaction is minimized is determined as the most dangerous stage in the synthesis reaction where thermal runaway occurs.

2. The method for rapidly determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials as described in claim 1, characterized in that, In step two, there should be no fewer than five sampling points.

3. The method for rapidly determining the most dangerous stage of thermal runaway in the synthesis reaction of energetic materials as described in claim 1, characterized in that, In step four, the same test conditions refer to test conditions where the test crucible, heating rate, and nitrogen flow rate are all the same.

Citation Information

Patent Citations

  • Method for determining temperature correction coefficient of energetic material chemical combination process

    CN112067657A

  • Chemical reaction risk analysis method

    CN115273998A