Preparation method of rumen bypass dephenolized cottonseed protein
By coating casein and gallnut mixed glue with dephenolized cottonseed protein, combined with UV light and dandelion emulsion processing technology, the problem of rapid degradation of protein feed in the rumen is solved, and the protection and efficient utilization of protein are achieved, which is suitable for high-yield applications. animals, improving the nutritional value and utilization of protein feed.
Patent Information
- Application Number
- CN202410954261.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-10-22
AI Technical Summary
The rapid degradation of existing protein feeds in the rumen leads to ammonia waste and protein shortage problems, especially for high-yielding animals such as beef cattle and high-yielding dairy animals, which cannot meet their protein needs and affect production potential.
A mixed glue solution prepared from casein and gallnut was used for fluidized coating, combined with ultraviolet light irradiation, ultrasonic dispersion of dandelion emulsion and high-temperature spray drying technology to form a double-layer composite material to coat the dephenolized cottonseed protein so that it does not remain in the rumen. Decompose and be digested and utilized in the abomasum.
It realizes the protective treatment of protein feed, delays the degradation rate in the rumen, improves protein utilization, is suitable for high-yielding animals, and the product is harmless, residue-free and has high nutritional value.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of rumen-pass dephenolized cottonseed protein, and particularly relates to a preparation method of rumen-pass dephenolized cottonseed protein. Background Art
[0002] Feed is degraded very quickly in the rumen. For example, the disappearance rate of soybean and peanut meal in the rumen within 24 hours is more than 90%. The rapid degradation of protein feed in the rumen can lead to two problems. First, rumen microorganisms can use the ammonia released by decomposing protein to synthesize bacterial protein. However, when the production of ammonia exceeds the ability of microorganisms to utilize it, part of the ammonia enters the blood and participates in other metabolic pathways to be excreted from the body. This will cause a waste of dietary protein, and the more protein is degraded, the greater the waste. If the degradation rate of protein feed in the rumen is too fast and the amount of ammonia produced is too much, the blood ammonia concentration is too high, and the liver must deaminize and transaminize in a short time, which puts the liver in a state of stress, which can lead to endocrine system disorders and severe cases of ammonia poisoning. Second, because the speed and amount of bacterial protein synthesized by rumen microorganisms in ruminants are limited, it can only meet the protein needs of animals with medium and low production levels, and cannot provide sufficient protein for fast-growing beef cattle, sheep and high-yielding dairy animals, which restricts the production potential of high-yielding animals. Protecting protein feed and reducing its degradation rate in the rumen so that more protein can be digested in the small intestine is the key to improving protein feed utilization. Those skilled in the art are in urgent need of developing a method for preparing rumen-dephenolized cottonseed protein to meet the existing application market and performance requirements. Summary of the invention
[0003] In view of this, the present invention provides rumen-free dephenolized cottonseed protein and a preparation method thereof.
[0004] A method for preparing rumen-pass dephenolized cottonseed protein comprises the following steps: a first step, weighing casein, adding distilled water, preparing a casein solution with a mass fraction of 4% to 8%, adjusting the pH value of the solution to 7 to 9 with edible alkali, continuing to stir for 0.5 to 1 hour until it is completely dissolved, adding 3% to 4% of gallnut powder by mass to the casein solution, and air-drying at room temperature to obtain a casein-galnut mixed glue solution; a second step, taking the casein-galnut mixed glue solution obtained in the first step as a coating liquid, taking the dephenolized cottonseed protein and placing it in a fluidized bed coating machine for coating, and blowing 8 After drying with hot air at 0℃ for 0.5-1h, irradiate with ultraviolet lamp for 10-15s to obtain casein gallnut-coated dephenolized cottonseed protein; the phenolic hydroxyl group of gallnut can cross-link with casein and dephenolized cottonseed protein to a certain extent through hydrogen bonds, hydrophobic bonds and other effects, and ultraviolet lamp irradiation can increase the degree of cross-linking; in the third step, take 4%-5% mass fraction of dandelion latex, pour the oxidized rosin-coated guanidine acetic acid obtained in the previous step into the dandelion latex at a uniform speed, ultrasonically disperse it evenly, and then spray dry it at high temperature to obtain rumen-permeated dephenolized cottonseed protein.
[0005] Furthermore, the second step UV light power is 2000mw / cm 2 , peak wavelength 365nm, power 600W.
[0006] Furthermore, the dandelion latex in the first step is one of rubber grass latex with a solid content of 10% to 15%.
[0007] The latex of rubber grass contains some natural rubber with low polymerization degree, but it is not acid-resistant and quickly decomposes in an acidic environment. At the same time, the casein gallnut inside is also acid-resistant. After dissolving, the dephenolized cottonseed protein is absorbed and utilized.
[0008] Furthermore, the dephenolized cottonseed protein in the second step is first-grade dephenolized cottonseed protein or dephenolized premium-grade cottonseed protein that complies with GH / T1042-2007.
[0009] Furthermore, in the third step, the pressure is 6.5-7.0 bar, the residence time is 1-1.5 s, the inlet temperature is 160-170° C., the material rate is 6-8 mL / min, and the jet gas flow is 1000-1200 L / h.
[0010] Furthermore, in the second step, the inlet air temperature of the coating is 120-130° C., the atomizing gas pressure is 0.12-0.15 MPa, the peristaltic pump speed is 9-10 r / min, and the fan speed is 1000-1200 rpm.
[0011] Dephenolized cottonseed protein is a dephenolized cottonseed protein product made from cottonseed as raw material, which is produced by extracting oil cake under low temperature conditions to remove free cottonpol.
[0012] Gall oil is produced by the gall aphids of the Aphididae family, which feed on the rachis, wings, leaflets or tips of the Rhus chinensis leaves, stimulating the proliferation of plant tissues and forming galls.
[0013] Beneficial effects of the present invention: The present invention firstly uses casein and gallnut to prepare a mixed glue solution, performs fluidized coating, and irradiates with ultraviolet light to obtain coated dephenolized cottonseed protein, thereby forming a double-layer composite material whose wall material is a mixture of casein gallnut and dandelion latex and whose core material is a pure substance of dephenolized cottonseed protein and rumen-passed dephenolized cottonseed protein. By utilizing the difference between the pH value of the rumen and the pH value of the abomasum, the double-layer composite material of the mixture of casein gallnut and dandelion latex does not decompose in a neutral solution but decomposes in an acidic environment, so that it is not degraded in the rumen but is digested and utilized after the abomasum. Its protective film will not decompose in an environment with a pH value of 5 to 7 in the rumen, and the dephenolized cottonseed protein will not dissolve. However, in the acidic environment of the abomasum (pH value of 2 to 3), the protective film is destroyed, and the coated dephenolized cottonseed protein is dissolved. The raw material is a food source, has a dandelion fragrance, is harmless, has no residue, and has a high degree of protection.
[0014] Compared with the prior art, the present invention has the following advantages: the rumen-dephenolized cottonseed protein disclosed in the present invention can be widely used in livestock, poultry and aquaculture. After being applied in dairy farms, it can largely replace soybean meal and sunflower seed meal in dairy cow feed formula to feed high-yielding dairy cows and achieve the effect of increasing milk production. Its amino acid composition is reasonable and its nutritional value is high. DETAILED DESCRIPTION Example 1
[0015] Xinsai Bio-Protein Feed Grade GH / T1042-2007 superior dephenolized cottonseed protein, Nanyang Rongwei Bio-500 mesh gallnut powder; Huoshan Tianan Bio-Taraxacum rubber grass latex with 10% solid content.
[0016] The preparation method of rumen dephenolized cottonseed protein comprises the following steps: the first step is to weigh casein, add distilled water, prepare a casein solution with a mass fraction of 8%, then use edible alkali to adjust the pH value of the solution to 9, continue stirring for 0.5h until it is completely dissolved, then add 3% of gallnut powder by mass to the casein solution, and air-dry at room temperature to obtain a casein-galnut mixed glue solution; the second step is to take the casein-galnut mixed glue solution of the first step as a coating liquid, take the dephenolized cottonseed protein and place it in a fluidized bed coating machine for coating, blow in 80°C hot air to dry for 0.5h, and then irradiate with an ultraviolet lamp for 15s, 2000mw / cm 2, peak wavelength 365nm, power 600W, casein gallnut coated dephenolized cottonseed protein, coating air inlet temperature 130℃, atomizing gas pressure 0.15MPa, peristaltic pump speed 10 / min, fan speed 1200rpm; third step, take 4% to 5% mass fraction of dandelion latex, pour the oxidized rosin coated guanidine acetic acid obtained in the previous step into the dandelion latex at a uniform speed for ultrasonic dispersion, and then spray dry at high temperature in S-300 spray dryer, pressure 7.0 bar, residence time 1.5s, inlet temperature 170℃, material rate 8mL / min, jet air flow 1200L / h, to obtain rumen dephenolized cottonseed protein. The dephenolized cottonseed protein mass content in the rumen dephenolized cottonseed protein is 70%.
[0017] Product: Light yellow powder, no cotton shells and cotton lint, no mildew, insect bites and peculiar smell. Crude protein ≥ 65.0; crude fiber ≤ 6.0; moisture ≤ 8.0; amino acid ratio of crude protein ≥ 90.0; 8h rumen passage rate determined by rumen nylon bag method is 73.8%. Example 2
[0018] Zhongmian Ziguang GH / T1042-20071 grade dephenolized cottonseed protein; Longbo Yukang 800 mesh gallnut powder; Dadukou Mingjia Biological Huainan Keda dandelion rubber grass latex with 15% solid content.
[0019] A method for preparing rumen-pass dephenolized cottonseed protein comprises the following steps: a first step, weighing casein, adding distilled water, preparing a casein solution with a mass fraction of 4%, adjusting the pH value of the solution to 7 with edible alkali, continuing to stir for 0.5h until it is completely dissolved, adding 3% of gallnut powder with a mass fraction to the casein solution, and air-drying at room temperature to obtain a casein-galnut mixed glue solution; a second step, taking the casein-galnut mixed glue solution in the first step as a coating liquid, taking the dephenolized cottonseed protein and placing it in a fluidized bed coating machine for coating, blowing in 80°C hot air to dry for 0.5h, and then irradiating with an ultraviolet lamp for 10s, 2000mw / cm 2 , peak wavelength 365nm, power 600W, casein gallnut coated dephenolized cottonseed protein, coating air inlet temperature 120℃, atomizing gas pressure 0.12MPa, peristaltic pump speed 9r / min, fan speed 1000rpm; third step, take 4% to 5% mass fraction of dandelion latex, pour the oxidized rosin coated guanidinoacetic acid obtained in the previous step into the dandelion latex at a uniform speed for ultrasonic dispersion, and then spray dry at high temperature in S-300 spray dryer, pressure 6.5bar, residence time 1s, inlet temperature 160℃, material rate 6mL / min, jet air flow 1000L / h, to obtain rumen dephenolized cottonseed protein. The dephenolized cottonseed protein mass content in the rumen dephenolized cottonseed protein is 60%.
[0020] Product: Light yellow powder, no cotton shells and cotton lint, no mildew, insect bites and peculiar smell. Crude protein ≥ 65.0; crude fiber ≤ 6.0; moisture ≤ 8.0; amino acid ratio of crude protein ≥ 90.0; 8h rumen passage rate determined by rumen nylon bag method is 67.5%. Example 3
[0021] Changji Taikun Biological GH / T1042-20071 grade dephenolized cottonseed protein; Nanyang Rongwei Biological 1000 mesh gallnut powder, Watsonwei gallnut powder; Huainan Keda dandelion rubber grass latex with 12% solid content.
[0022] The preparation method of rumen dephenolized cottonseed protein comprises the following steps: first, weighing casein, adding distilled water, preparing a casein solution with a mass fraction of 6%, adjusting the pH value of the solution to 8 with edible alkali, continuing to stir for 0.85h until it is completely dissolved, adding 3.5% of gallnut powder by mass to the casein solution, and air-drying at room temperature to obtain a casein-galnut mixed glue liquid; second, taking the casein-galnut mixed glue liquid in the first step as a coating liquid, taking the dephenolized cottonseed protein and placing it in a fluidized bed coating machine for coating, blowing in 80°C hot air to dry for 0.75h, and then irradiating it with a D800 ultraviolet lamp for 12s, with the ultraviolet light power of 2000mw / cm 2 , peak wavelength 365nm, power 600W, casein gallnut coated dephenolized cottonseed protein, coating air inlet temperature 125℃, atomizing gas pressure 0.15MPa, peristaltic pump speed 10r / min, fan speed 1100rpm; third step, take 4% to 5% mass fraction of dandelion latex, pour the oxidized rosin coated guanidine acetic acid obtained in the previous step into the dandelion latex at a uniform speed for ultrasonic dispersion, and then spray dry at high temperature in S-300 spray dryer, pressure 6.8bar, residence time 1.2s, inlet temperature 165℃, material rate 7mL / min, jet air flow 1100L / h, to obtain rumen dephenolized cottonseed protein. The dephenolized cottonseed protein mass content in the rumen dephenolized cottonseed protein is 65%.
[0023] Product: Light yellow powder, no cotton husks and cotton lint, no mildew, insect bites and peculiar smell. Crude protein ≥ 65.0; crude fiber ≤ 6.0; moisture ≤ 8.0; amino acid ratio of crude protein ≥ 90.0; 8h rumen passage rate determined by rumen nylon bag method is 71.2%.
[0024] Note: Crude fiber shall be in accordance with GB / T6434; moisture shall be in accordance with GB / T6435; amino acid shall be in accordance with GB / T18246 and GB / T15399; free cottonpol shall be in accordance with GB / T13086; hygiene indicators shall be in accordance with GB / T13078; Salmonella content shall be in accordance with GB / T13091; mold shall be in accordance with GB / T13092; aflatoxin B1 shall be in accordance with B13078-2017; rumen passage rate was measured by Bengbu Modern Animal Husbandry using 2-year-old healthy fistula cattle, with reference to the dragon bag method of Ørskov et al.
Claims
1. A method for preparing rumen-free dephenolized cottonseed protein, It is characterized in that The following steps are involved: The first step is to weigh casein, add distilled water, prepare a casein solution with a mass fraction of 4% to 8%, then use edible alkali to adjust the pH value of the solution to 7 to 9, continue stirring for 0.5 to 1 hour until it is completely dissolved, then add 3% to 4% of gallnut powder by mass to the casein solution, and air-dry at room temperature to obtain a casein gallnut mixed glue solution; the second step is to take the casein gallnut mixed glue solution in the first step as a coating liquid, take dephenolized cottonseed protein and place it in a fluidized bed coating machine for coating, blow into 80°C hot air to dry for 0.5 to 1 hour, and then irradiate with an ultraviolet lamp for 10 to 15 seconds to obtain casein gallnut coated dephenolized cottonseed protein; the third step is to take 4% to 5% of dandelion latex, uniformly pour the oxidized rosin-coated guanidine acetic acid obtained in the previous step into the dandelion latex solution for ultrasonic dispersion, and then spray dry at high temperature to obtain rumen-dephenolized cottonseed protein.
2. The method for preparing rumen-free dephenolized cottonseed protein according to claim 1, It is characterized in that The first step dandelion latex is one of the rubber grass latex with a solid content of 10% to 15%.
3. The method for preparing rumen-free dephenolized cottonseed protein according to claim 1, It is characterized in that The second-step dephenolized cottonseed protein is first-grade dephenolized cottonseed protein or premium dephenolized cottonseed protein in accordance with GH / T1042-2007.
4. The method for preparing rumen-free dephenolized cottonseed protein according to claim 1, It is characterized in that The pressure in the third step is 6.5-7.0 bar, the residence time is 1-1.5 s, the inlet temperature is 160-170° C., the material rate is 6-8 mL / min, and the jet gas flow is 1000-1200 L / h.
5. The method for preparing rumen-dephenolized cottonseed protein according to claim 1, It is characterized in that In the second step, the inlet air temperature of the coating is 120-130° C., the atomizing gas pressure is 0.12-0.15 MPa, the peristaltic pump speed is 9-10 r / min, and the fan speed is 1000-1200 rpm.
Citation Information
Patent Citations
Preparation method of coated guanidinoacetic acid
CN110663821A
Preparation method of novel rumen bypass glucose oxidase
CN112868912A
Gelatin-Arabic gum / urea resin double-layer wall material DCOIT microcapsule as well as preparation method and application thereof
CN114653315A
Rumen bypass nicotinic acid and preparation method thereof
CN116998612A