Doping device of single crystal furnace, single crystal furnace and crystal pulling method of heavily doped silicon single crystal
By designing a doping device in a single crystal furnace, the dopant is directly extended above the funnel and the input amount and rate are controlled, the problem of difficult to control dopant volatility is solved, and the resistivity consistency and finished product of silicon single crystals are improved Rate.
Patent Information
- Application Number
- CN202411038490.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-01
AI Technical Summary
During the drawing process of heavily doped silicon single crystals, the volatility of the dopant is difficult to control, resulting in difficulty in meeting the actual resistivity, and the yield of silicon single crystals is relatively low.
A single crystal furnace doping device is designed, including a fixing mechanism, a storage mechanism, a feeding mechanism and a lifting mechanism. The dopant is directly extended into the funnel in the single crystal furnace through a guide tube, and a vacuum and argon environment are used. Control the dopant input amount and rate to reduce the volatility of the dopant.
It effectively reduces the volatility of the dopant, improves the consistency between the actual resistivity of the crystal rod and the target resistivity, improves the yield of silicon single crystal, reduces the dopant usage, and reduces the cost.
Smart Images

Figure CN118880435A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of single crystal silicon processing, and in particular to a single crystal furnace doping device, a single crystal furnace and a crystal pulling method for heavily doped silicon single crystals. Background Art
[0002] The resistivity of silicon single crystals is closely related to semiconductor devices. At present, with the rise of photovoltaic power generation and new energy electric vehicles, the demand for semiconductor power devices is growing, which has also led to higher and higher requirements for the resistivity characteristics of crystal rods for power devices such as IGBT. In the process of preparing semiconductor materials, the resistivity of silicon single crystals is usually adjusted by doping, that is, by introducing impurities into the silicon material to adjust its electrical properties.
[0003] With the development of "4C industries" such as communications, computers, consumer electronics and automobiles, the application scope of power semiconductor devices is becoming increasingly wide, and has become the foundation of major pillar industries of the national economy. Power semiconductor devices usually work under high current conditions, and the current flows vertically through the device. Therefore, when the device is in the on state, the silicon wafer as the substrate will consume a part of the power. In order to minimize this part of the power, it is necessary to reduce the resistivity of the silicon wafer substrate. Therefore, power devices are usually made of heavily doped single crystal silicon, such as using silicon single crystals pulled by heavily doped red phosphorus to prepare power devices.
[0004] However, currently, when heavily doping silicon single crystals, the dopant is usually placed in a quartz bell jar, which is then hoisted above the melt in the furnace body and then enters the melt through high-temperature gasification. However, during the entire dopant addition process, the dopant is always in a volatilization state, and the volatilization amount is difficult to determine, that is, the actual amount of dopant entering the melt cannot be determined. Especially for dopants such as red phosphorus that have a low sublimation point and are more volatile, their volatilization rate is faster and the volatilization amount is greater. Therefore, in the existing heavily doped silicon single crystal pulling scheme, the actual doping amount is difficult to determine due to the large amount of volatilization of the dopant, which in turn causes the actual resistivity of the crystal rod to often be difficult to meet the target resistivity requirements, and the silicon single crystal yield is low. Summary of the invention
[0005] In view of this, and to address the above shortcomings, it is necessary to propose a single crystal furnace doping device, a single crystal furnace and a crystal pulling method for heavily doped silicon single crystals, so as to reduce the volatilization of dopants during the pulling process of heavily doped silicon single crystals, thereby improving the consistency between the actual resistivity of the crystal rod and the target resistivity, and improving the yield of silicon single crystals.
[0006] In the first aspect, the present invention provides a single crystal furnace doping device, comprising: a fixing mechanism, a material storage mechanism, a feeding mechanism and a lifting mechanism; the feeding mechanism comprises: a feeding control assembly and a material guide pipe, the material storage mechanism is used to hold dopants, and is fixedly connected to the feeding control assembly, and the feeding end of the feeding control assembly is connected to the discharging end of the material storage mechanism; the feeding control assembly is connected to the material guide pipe, and the discharging end of the feeding control assembly is connected to the inlet end of the material guide pipe to control the amount of dopants entering the material guide pipe; the outlet end of the material guide pipe is used to extend into the inlet of the funnel in the single crystal furnace, wherein the outlet end of the funnel is located above the molten soup; the lifting mechanism is movably connected to the feeding mechanism, and is used to drive the feeding mechanism to move up and down, so as to extend the outlet end of the material guide pipe into the inlet of the funnel in the single crystal furnace; one end of the fixing mechanism is rotatably connected above the lifting mechanism, and the other end is rotatably connected to the furnace barrel of the single crystal furnace.
[0007] Preferably, the material storage mechanism includes a closed material storage chamber, the upper end of which is provided with a vacuum interface for evacuating the material storage chamber by a vacuum machine; the lower end of the material storage chamber is provided with an argon interface for introducing argon to provide an argon atmosphere for the material storage chamber and the material guide tube.
[0008] Preferably, a switch valve is provided between the discharge end of the material storage chamber and the feed end of the material feeding control assembly, for controlling the communication between the material feeding control assembly and the material storage chamber.
[0009] Preferably, the feeding control assembly includes: a first motor, a coupling, a first threaded rod and a connecting assembly; the driving end of the first motor is connected to the non-threaded end of the first threaded rod through the coupling; there is a "ㄣ"-shaped cavity inside the connecting assembly, the first threaded rod is arranged in the transverse part of the "ㄣ"-shaped cavity, and the first threaded rod is tightly matched with the inner wall of the "ㄣ"-shaped cavity; the upper end of the "ㄣ"-shaped cavity is connected to the discharge end of the storage mechanism, and the lower end is connected to the inlet end of the guide tube, and both are opposite to the threaded part of the first threaded rod; the first motor is used to drive the first threaded rod to rotate, so as to transport the dopant input from the storage mechanism into the "ㄣ"-shaped cavity and fall into the guide tube.
[0010] Preferably, the lifting mechanism includes: an upper base, a lower base, a second drive motor, a second threaded rod and a slide rail; the lower base is used to be fixedly mounted on the outer surface of the furnace body of the single crystal furnace, and is sealed with the furnace body; both ends of the second threaded rod and the slide rail are respectively fixedly connected to the upper base and the lower base, the slide rail is slidably connected to the feeding mechanism, the second threaded rod is threadedly connected to the feeding mechanism, the second drive motor is fixedly mounted on the lower base, and is drivingly connected to the second threaded rod; the fixing mechanism is fixedly connected to the upper base.
[0011] Preferably, the slide rails include four, and the lifting mechanism also includes two first connecting members and one second connecting member; one end of the two first connecting members are fixedly connected to the material guide tube, and the other ends of the two first connecting members are respectively slidably connected to the two slide rails on both sides of the material guide tube; the second connecting member is provided with two first through holes and one internally threaded through hole, one end of the second connecting member is fixedly connected to the material guide tube, and is respectively slidably connected to the two slide rails away from the material guide tube through the two first through holes, and the second threaded rod is threadedly connected to the internally threaded through hole.
[0012] Preferably, the material guiding tube is a quartz material guiding tube, and a flexible bellows is sleeved on the material guiding tube.
[0013] In a second aspect, the present invention provides a single crystal furnace, comprising a single crystal furnace body and a single crystal furnace doping device as described in the first aspect; A funnel is fixedly mounted on the graphite heat shield inside the single crystal furnace body, the inlet of the funnel is located at the upper end of the graphite heat shield, and the outlet of the funnel is located at the quartz outer flow guide cover above the molten soup, and the quartz outer flow guide cover is provided with a plurality of dopant vapor discharge holes; The fixing mechanism of the single crystal furnace doping device is fixedly installed on the furnace barrel of the single crystal furnace body, and the material guide pipe of the feeding mechanism is inserted into the single crystal furnace from above the furnace body of the single crystal furnace body and fixed on the furnace body through the lower base of the lifting mechanism.
[0014] Preferably, the material guide pipe of the feeding mechanism is inserted into the single crystal furnace from the position of the observation window of the single crystal furnace body.
[0015] In a third aspect, the present invention further provides a method for pulling a heavily doped silicon single crystal, the implementation subject of which is the single crystal furnace as described in the second aspect, and the method for pulling a crystal comprises: Step S1: controlling the lifting mechanism of the single crystal furnace doping device to move the lower end of the material guide pipe into the funnel mouth; Step S2: calculating the doping amount of the dopant of the silicon single crystal to be pulled; Step S3: adding the corresponding dopant into the material storage mechanism according to the calculated doping amount; Step S4: setting the doping rate of the dopant by setting the rotation speed of the first motor; Step S5: starting the crystal pulling procedure of the single crystal furnace; Step S6: At the same time, after the vacuum of the single crystal furnace doping device is extracted, a switch valve is provided between the discharge end of the storage chamber and the feed end of the feeding control component; argon gas is introduced, and the first motor is started to allow the dopant to enter the funnel along the guide pipe, so that it can be output through the funnel and then evaporated into the melt.
[0016] It can be seen from the above technical scheme that in the single crystal furnace doping device, single crystal furnace and crystal pulling method of heavily doped silicon single crystal provided by the present invention, the single crystal furnace doping device and the single crystal furnace body constitute a single crystal furnace, and based on the constituted single crystal furnace, the heavily doped silicon single crystal can be pulled, and the single crystal furnace doping device can include a fixing mechanism, a storage mechanism, a feeding structure and a lifting mechanism, wherein the fixing mechanism can fix the doping device on the single crystal furnace body to ensure the stability of the device. The storage mechanism can be used to hold dopants, the feeding assembly can control the amount of dopants entering the guide tube, and the guide tube can be adjusted by the lifting mechanism to extend above the funnel in the single crystal furnace. In this way, since the guide tube can be adjusted to extend directly into the position of the funnel through the lifting mechanism, the volatilization of the dopant when the dopant is thrown from the top of the furnace body through the quartz bell jar is reduced. Moreover, the present scheme can add dopants to the molten soup at any time or continuously and slowly through the feeding mechanism, thereby further volatilizing a small amount of dopant. It can be seen that the pulling of heavily doped silicon single crystals according to this scheme can greatly reduce the volatilization of dopants and improve the consistency between the actual resistivity of the crystal rod and the target resistivity, that is, the actually pulled crystal rod can meet the expected resistivity requirements, thereby improving the yield of silicon single crystals. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 A schematic structural diagram of a single crystal furnace doping device provided in an embodiment of the present invention.
[0018] Figure 2 A schematic structural diagram of a material storage mechanism provided in an embodiment of the present invention.
[0019] Figure 3 A cross-sectional view of a feeding control assembly provided in an embodiment of the present invention.
[0020] Figure 4 A structural schematic diagram of a lifting mechanism provided by an embodiment of the present invention.
[0021] Figure 5 A partial schematic diagram of a second threaded rod provided in an embodiment of the present invention.
[0022] Figure 6 A schematic structural diagram of a single crystal furnace provided in an embodiment of the present invention.
[0023] Figure 7 A cross-sectional view of a single crystal furnace body provided in an embodiment of the present invention.
[0024] Figure 8 A schematic structural diagram of a dopant vapor exhaust hole provided in an embodiment of the present invention.
[0025] Fig. 9 This is the resistivity distribution diagram of the crystal rod obtained based on the traditional quartz bell solution in Example 1.
[0026] Fig.10 This is the resistivity distribution diagram of the crystal rod obtained based on this scheme in Example 1.
[0027] Fig.11 This is the resistivity distribution diagram of the crystal rod obtained based on the traditional quartz bell jar solution in Example 2.
[0028] Fig.12 This is the resistivity distribution diagram of the crystal rod obtained based on this scheme in Example 2.
[0029] In the figure: a fixing mechanism 10, a material storage mechanism 20, a material storage chamber 21, a vacuum interface 22, an argon interface 23, a switch valve 24, a feeding mechanism 30, a feeding control assembly 31, a first motor 311, a coupling 312, a first threaded rod 313, a connecting assembly 314, a "ㄣ"-shaped cavity 315, a material guide pipe 32, a bellows 33, a lifting mechanism 40, an upper base 41, a lower base 42, a second drive motor 43, a second threaded rod 44, a slide rail 45, a first connecting piece 46, a second connecting piece 47, a single crystal furnace doping device 100, a single crystal furnace body 200, a graphite heat shield 201, a funnel 202, a quartz outer flow guide cover 203, and a dopant vapor discharge hole 204. DETAILED DESCRIPTION
[0030] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for use in the embodiments. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0031] See also Figure 1-5The present invention provides a single crystal furnace doping device 100, comprising: a fixing mechanism 10, a material storage mechanism 20, a feeding mechanism 30 and a lifting mechanism 40; the feeding mechanism 30 comprises: a feeding control component 31 and a material guide pipe 32, the material storage mechanism 20 is used to hold dopants, and is fixedly connected to the feeding control component 31, and the feeding end of the feeding control component 31 is connected to the discharging end of the material storage mechanism 20; the feeding control component 31 is connected to the material guide pipe 32, and the discharging end of the feeding control component 31 is connected to the inlet of the material guide pipe 32. The ends are connected to each other to control the amount of dopant entering the guide tube 32; the outlet end of the guide tube 32 is used to extend into the entrance of the funnel 202 in the single crystal furnace, wherein the outlet end of the funnel 202 is located above the molten soup; the lifting mechanism 40 is movably connected to the feeding mechanism 30, and is used to drive the feeding mechanism 30 to move up and down to extend the outlet end of the guide tube 32 into the entrance of the funnel 202 in the single crystal furnace; one end of the fixing mechanism 10 is rotatably connected to the top of the lifting mechanism 40, and the other end is rotatably connected to the furnace barrel of the single crystal furnace.
[0032] In this embodiment, since the guide tube 32 of the feeding mechanism 30 can be adjusted by the lifting mechanism 40 to directly extend into the position of the funnel 202, the volatilization of the dopant when the dopant is thrown from the top of the furnace body through the quartz bell is reduced. Moreover, the present solution can add the dopant to the melt at any time or continuously and slowly through the feeding mechanism 30, thereby further volatilizing a small amount of dopant. It can be seen that the pulling of heavily doped silicon single crystals according to this solution can greatly reduce the volatilization of dopants and improve the consistency between the actual resistivity of the crystal rod and the target resistivity, that is, the actually pulled crystal rod can meet the requirements of the desired resistivity, thereby improving the yield rate of silicon single crystals. Moreover, since this solution can greatly reduce the volatilization of dopants, when pulling crystal rods with the same target target resistivity, the present solution uses less dopants and has lower costs. When the same mass of dopants is used to pull silicon single crystals, the present solution can make the resistivity of silicon single crystals lower due to less volatilization, thereby further improving the quality of the crystal rods.
[0033] The fixing mechanism 10 may be a rectangular frame, one short side of which is rotatably mounted above the lifting mechanism 40, and the other short side of which is rotatably mounted on the furnace drum of the single crystal furnace body 200. In this way, when the lifting mechanism 40 drives the feeding mechanism 30 to move up and down, the fixing mechanism 10 can rotate with the side connected to the furnace drum as a fulcrum so that the feeding mechanism 30 can extend the guide tube 32 into the funnel 202, or move it out of the funnel 202. Moreover, the entire device needs to be inserted into the single crystal furnace body 200 at an angle, with only a fixed point at the insertion point. By traction and fixing the doping device through the fixing mechanism 10, not only can the doping device be more balanced, but also the lateral force on the fixed point on the single crystal furnace body 200 can be greatly reduced, thereby reducing damage to the doping device or the single crystal furnace body 200 and increasing the service life of the device.
[0034] The storage mechanism 20 may include a closed storage chamber 21, the upper end of which is provided with a vacuum interface 22 for evacuating the storage chamber 21 to a vacuum through a vacuum machine; the lower end of the storage chamber 21 is provided with an argon interface 23 for introducing argon to provide an argon atmosphere in the storage chamber 21 and the guide tube 32. In this way, the storage chamber 21 and the guide tube 32 can have the same atmosphere as that in the single crystal furnace, so that crystal pulling and doping can be achieved at the same time, and it will not cause a significant change in the crystal pulling conditions in the single crystal furnace, affecting the success rate and quality of crystal pulling. In addition, by introducing argon into the guide tube 32, the argon can play a conveying role, smoothly bringing the dopant out of the guide tube 32 and into the funnel 202, and evaporating into the melt after being output from the funnel 202.
[0035] In addition, a switch valve 24 is provided between the discharge end of the storage chamber 21 and the feed end of the feeding control assembly 31, for controlling the communication between the feeding control assembly 31 and the storage chamber 21. In this embodiment, the switch valve 24 can control the communication between the feeding control assembly 31 and the storage chamber 21, so that not only can the release and stop of the dopant in the storage chamber 21 be controlled at any time, but also when the vacuum degree and argon gas environment parameters are adjusted in the single crystal furnace, the switch valve 24 can be closed, and the vacuum degree and argon gas environment parameters inside the device can be adjusted through the vacuum interface 22 and the argon gas interface 23, so as to ensure the consistency of the device and the environmental parameters in the single crystal furnace.
[0036] The storage cavity 21 of the storage mechanism 20 can be provided with cavities of different capacities according to different doping amounts. For example, the storage cavity 21 can be of sizes of Φ86mm*115mm, Φ105mm*150mm, etc. The storage cavity 21 can be made of a transparent material so as to facilitate real-time observation of the dopant residue in the storage cavity 21.
[0037] The feeding mechanism 30 may include a feeding control component 31 and a guide tube 32 for controlling the amount of dopant added, and adding the dopant to the funnel 202 in the single crystal furnace body 200 through the guide tube 32, so that the dopant flows out through the funnel 202 to the top of the melt and evaporates into the melt.
[0038] For the feeding control component 31, it may include: a first motor 311, a coupling 312, a first threaded rod 313 and a connecting component 314; the driving end of the first motor 311 is connected to the non-threaded end of the first threaded rod 313 through the coupling 312; there is a "ㄣ"-shaped cavity 315 inside the connecting component 314, the first threaded rod 313 is arranged in the transverse part of the "ㄣ"-shaped cavity 315, and the first threaded rod 313 is tightly matched with the inner wall of the "ㄣ"-shaped cavity 315; the upper end of the "ㄣ"-shaped cavity 315 is connected to the discharge end of the storage mechanism 20, and the lower end is connected to the inlet end of the guide tube 32, and both are opposite to the threaded part of the first threaded rod 313; the first motor 311 is used to drive the first threaded rod 313 to rotate, so as to transport the dopant input from the storage mechanism 20 into the "ㄣ"-shaped cavity 315 and fall into the guide tube 32.
[0039] In this embodiment, the coupling 312 connects the driving end of the first motor 311 and the first threaded rod 313 together, and the first threaded rod 313 is tightly arranged in the "U"-shaped cavity 315 inside the connecting assembly 314. In this way, when the storage mechanism 20 outputs the dopant into the "U"-shaped cavity 315 through the discharge end, the first motor 311 drives the first threaded rod 313 to rotate, and then the dopant falling into one side of the "U"-shaped cavity 315 is spirally transported to the other side of the "U"-shaped cavity 315, and then flows out from the guide pipe 32 connected to the other side, and is transported along the guide pipe 32 to the funnel 202 in the single crystal furnace.
[0040] Since the inner surface of the U-shaped cavity 315 and the first threaded rod 313 are in direct contact with the dopant, surface treatment is required. For example, a ceramic coating can be sprayed on the inner surface of the U-shaped cavity 315 and the outer surface of the first threaded rod 313 .
[0041] The rotation speed of the first motor 311 is adjustable to ensure that the doping rate of the dopant can be adjusted within the range of 0-100 g / min.
[0042] As for the lifting mechanism 40, it is mainly used to drive the feeding mechanism 30 to move up and down, so that the guide tube 32 can penetrate into the funnel 202 in the single crystal furnace. The lifting mechanism 40 may include: an upper base 41, a lower base 42, a second drive motor 43, a second threaded rod 44 and a slide rail 45; the lower base 42 is used to be fixedly installed on the upper surface of the furnace body of the single crystal furnace, and is sealed with the furnace body; both ends of the second threaded rod 44 and the slide rail 45 are respectively fixedly connected to the upper base 41 and the lower base 42, the slide rail 45 is slidably connected to the feeding mechanism 30, the second threaded rod 44 is threadedly connected to the feeding mechanism 30, the second drive motor 43 is fixedly installed on the lower base 42, and is drivingly connected to the second threaded rod 44; the fixing mechanism 10 is fixedly connected to the upper base 41.
[0043] In this embodiment, the second threaded rod 44 and the feeding mechanism 30 are threadedly connected, and each slide rail 45 is slidably connected to the feeding mechanism 30. In this way, the second threaded rod 44 is driven by the second drive motor 43 to rotate forward and reverse, which can drive the feeding mechanism 30 to move upward and downward, thereby realizing the extension of the guide tube 32 into the funnel 202 and the removal from the funnel 202.
[0044] Specifically, the slide rails 45 may include four, which are distributed in a rectangular shape, two of which are respectively distributed on both sides of the material storage mechanism 20, and the other two are distributed on the side close to the second threaded rod 44. The lifting mechanism 40 also includes two first connecting members 46 and a second connecting member 47; one end of the two first connecting members 46 is fixedly connected to the material guide tube 32, and the other ends of the two first connecting members 46 are respectively slidably connected to the two slide rails 45 on both sides of the material guide tube 32; the second connecting member 47 is provided with two first through holes and an internal threaded through hole, one end of the second connecting member 47 is fixedly connected to the material guide tube 32, and is respectively slidably connected to the two slide rails 45 away from the material guide tube 32 through the two first through holes, and the second threaded rod 44 is threadedly connected to the internal threaded through hole.
[0045] In this embodiment, the material guide tube 32 is a quartz material guide tube 32, and a flexible bellows 33 is sleeved on the material guide tube 32. This not only protects the quartz material guide tube 32, but also allows it to expand or contract with the up and down movement of the feeding mechanism 30, without affecting the movement of the feeding mechanism 30.
[0046] See also Figure 6-8 As shown, the present invention further provides a single crystal furnace, comprising a single crystal furnace body 200 and a single crystal furnace doping device 100 as described in the above embodiments; A funnel 202 is fixedly mounted on the graphite heat shield 201 inside the single crystal furnace body 200. The inlet of the funnel 202 is located at the upper end of the graphite heat shield 201, and the outlet of the funnel 202 is located at the quartz outer flow guide cover 203 above the molten soup. The quartz outer flow guide cover 203 is provided with a plurality of dopant vapor discharge holes 204. The fixing mechanism 10 of the single crystal furnace doping device 100 is fixedly installed on the furnace drum of the single crystal furnace body 200, and the material guide pipe 32 of the feeding mechanism 30 is inserted into the single crystal furnace from above the furnace body of the single crystal furnace body 200, and is fixed on the furnace body through the lower base 42 of the lifting mechanism 40.
[0047] In this embodiment, a quartz funnel 202 is fixedly installed on the graphite heat shield 201 in the single crystal furnace body 200. The inlet of the quartz funnel 202 is located near the upper end of the heat shield, and the outlet is located at the quartz outer flow guide cover 203 above the melt. In this way, when adding dopants to the single crystal furnace body 200 through the single crystal furnace doping device 100, the dopants will be output from the guide tube 32 and enter the quartz funnel 202, and then output from the outlet of the quartz funnel 202. The output dopants evaporate and enter the melt. In order to allow the dopants to evaporate more evenly and quickly into the melt, it is considered to set a plurality of dopant vapor discharge holes 204 on the quartz outer flow guide cover 203, so that the dopants are discharged from the dopant vapor discharge holes 204 after evaporation and evenly enter the melt.
[0048] In addition, the single crystal furnace doping device 100 can be installed at the observation window of the single crystal furnace body 200, that is, the material guide pipe 32 of the feeding mechanism 30 can be inserted into the single crystal furnace from the observation window position of the single crystal furnace body 200, and then fixed at the observation position through the lower base 42. In this way, additional operations such as re-drilling holes on the single crystal furnace body 200 are avoided. Of course, when the lower base 42 is fixed at the observation window position of the single crystal furnace body 200, it should be sealed.
[0049] In addition, the present invention also provides a method for pulling a heavily doped silicon single crystal, the implementation subject of which is a single crystal furnace as described in the above embodiments, and the method for pulling a crystal includes: Step S1: Control the lifting mechanism 40 of the single crystal furnace doping device 100 to move the lower end of the guide tube 32 to the opening of the funnel 202; Step S2: calculating the doping amount of the dopant of the silicon single crystal to be pulled; Step S3: adding the corresponding dopant into the storage mechanism 20 according to the calculated doping amount; Step S4: setting the doping rate of the dopant by setting the rotation speed of the first motor 311; Step S5: starting the crystal pulling procedure of the single crystal furnace; Step S6: At the same time, after the vacuum of the single crystal furnace doping device 100 is extracted, the switch valve 24 is opened between the discharge end of the storage chamber 21 and the feed end of the feeding control component 31; argon gas is introduced, and the first motor 311 is started to allow the dopant to enter the funnel 202 along the guide pipe 32, so that it can be output through the funnel 202 and then evaporated into the melt.
[0050] In this embodiment, when pulling heavily doped silicon single crystals, dopants can be added while pulling single crystal silicon. For example, the rotation speed of the first motor 311 can be calculated according to the total amount of doping, and then the rotation speed of the first motor 311 can be set, so that the dopant is driven by the first motor 311 to add the dopant to the molten soup in the single crystal furnace at a set doping rate. This can not only reduce the volatilization of dopants, but also greatly improve the crystal pulling efficiency compared to the traditional solution that can only add dopants after stopping the machine. In addition, because the present solution allows dopants to be added while pulling the crystal, the resistivity consistency in each region of the pulled crystal rod can be higher and the resistivity uniformity can be stronger.
[0051] In addition, this solution can also achieve the one-time addition of dopants in the traditional solution. For example, when adding dopants before crystal pulling, the speed of the first motor 311 is adjusted to a larger value, and all dopants in the storage mechanism 20 are added to the single crystal furnace at the fastest speed and in the shortest time.
[0052] The following is a further explanation of this scheme in combination with specific experiments: Example 1: For pulling 1450mm heavily phosphorus-doped single crystal silicon, the target resistivity is <0.0013Ω.cm; Traditional quartz bell solution: The amount of dopant phosphorus used is 800-860g, and the resistivity distribution of the crystal rod is as follows: Fig. 9 As shown; In this solution, the amount of dopant phosphorus used is 560-600g, and the resistivity distribution of the crystal rod is as follows: Fig.10 shown.
[0053] By comparing the conventional scheme and the present scheme of Example 1, it can be seen that when pulling heavily phosphorus-doped single crystal silicon with a target resistivity of less than 0.0013Ω.cm at the same time, the conventional scheme needs to use 800-860g of dopant to make the target resistivity of the single crystal silicon meet the requirement of less than 0.0013Ω.cm; while based on the present scheme, only 560-600g of dopant is needed to meet the requirement of target resistivity less than 0.0013Ω.cm. Moreover, the resistivity distribution of the single crystal silicon pulled by the doping device is 0.00128-0.00119Ω.cm, while the resistivity distribution of the single crystal silicon pulled by the conventional scheme is 0.00134-0.00123Ω.cm. Compared with the conventional quartz bell jar scheme, the single crystal silicon pulled by the present scheme has a lower resistivity and a better resistivity distribution uniformity.
[0054] Example 2: For pulling 1800 mm heavily phosphorus-doped single crystal silicon, the total amount of dopant is: 950 g; Traditional quartz bell solution: The actual resistivity distribution of the crystal rod is as follows Fig.11 As shown; This scheme: The actual resistivity distribution of the crystal rod is as follows: Fig.12 As shown; By comparing the conventional solution of Example 2 with the present solution, it can be seen that when 950g of dopant is used to pull 1800mm heavily phosphorus-doped single crystal silicon, the resistivity distribution of the crystal rod obtained by the conventional bell jar doping solution is 0.00155-0.0011Ω.cm, while the resistivity distribution of the crystal rod obtained by the present solution is 0.0013-0.00095Ω.cm. It is obvious that the resistivity of the crystal rod obtained by the conventional bell jar doping method is much greater than the resistivity obtained by the present solution. Therefore, doping and crystal pulling based on the doping device provided by the present solution can greatly reduce the volatilization of the dopant, reduce the amount of dopant used, and can reduce the resistivity of the silicon single crystal and improve the yield of the silicon single crystal.
[0055] In addition, since the method embodiments and system embodiments provided by the present invention are based on the same inventive concept as the device embodiments of this specification, the specific contents can be found in the description of the device embodiments of this specification and will not be repeated here.
[0056] The modules or units in the device of the embodiment of the present invention can be combined, divided and deleted according to actual needs. The above disclosure is only the preferred embodiment of the present invention, and of course it cannot be used to limit the scope of the rights of the present invention. Those skilled in the art can understand that all or part of the processes of the above embodiment are implemented, and the equivalent changes made according to the claims of the present invention still fall within the scope of the invention.
Claims
1. A single crystal furnace doping device, It is characterized in that include: Fixing mechanism, material storage mechanism, material feeding mechanism and lifting mechanism; The feeding mechanism comprises: a feeding control component and a material guide pipe, the material storage mechanism is used to hold dopants, and is fixedly connected to the feeding control component, and the feeding end of the feeding control component is communicated with the discharging end of the material storage mechanism; the feeding control component is connected to the material guide pipe, and the discharging end of the feeding control component is communicated with the inlet end of the material guide pipe to control the amount of dopants entering the material guide pipe; the outlet end of the material guide pipe is used to extend into the inlet of the funnel in the single crystal furnace, wherein the outlet end of the funnel is located above the molten soup; the lifting mechanism is movably connected to the feeding mechanism, and is used to drive the feeding mechanism to move up and down, so as to extend the outlet end of the material guide pipe into the inlet of the funnel in the single crystal furnace; one end of the fixed mechanism is rotatably connected above the lifting mechanism, and the other end is rotatably connected to the furnace barrel of the single crystal furnace.
2. The single crystal furnace doping device according to claim 1, It is characterized in that The material storage mechanism comprises a closed material storage chamber, the upper end of which is provided with a vacuum extraction interface for evacuating the material storage chamber to a vacuum by a vacuum machine; the lower end of the material storage chamber is provided with an argon gas interface for introducing argon gas to provide an argon gas atmosphere in the material storage chamber and the material guide tube.
3. The single crystal furnace doping device according to claim 2, It is characterized in that A switch valve is provided between the discharge end of the material storage cavity and the feed end of the material feeding control component, for controlling the communication between the material feeding control component and the material storage cavity.
4. The single crystal furnace doping device according to claim 1, It is characterized in that The feeding control assembly includes: a first motor, a coupling, a first threaded rod and a connecting assembly; the driving end of the first motor is connected to the non-threaded end of the first threaded rod through the coupling; there is a "ㄣ"-shaped cavity inside the connecting assembly, the first threaded rod is arranged in the transverse part of the "ㄣ"-shaped cavity, and the first threaded rod is tightly matched with the inner wall of the "ㄣ"-shaped cavity; the upper end of the "ㄣ"-shaped cavity is connected to the discharge end of the material storage mechanism, and the lower end is connected to the inlet end of the material guide pipe, and both are opposite to the threaded part of the first threaded rod; the first motor is used to drive the first threaded rod to rotate, so as to transport the dopant input from the material storage mechanism into the "ㄣ"-shaped cavity and fall into the material guide pipe.
5. The single crystal furnace doping device according to claim 1, It is characterized in that The lifting mechanism includes: an upper base, a lower base, a second drive motor, a second threaded rod and a slide rail; the lower base is used to be fixedly installed on the outer surface of the furnace body of the single crystal furnace, and is sealed with the furnace body; both ends of the second threaded rod and the slide rail are respectively fixedly connected to the upper base and the lower base, the slide rail is slidably connected to the feeding mechanism, the second threaded rod is threadedly connected to the feeding mechanism, the second drive motor is fixedly installed on the lower base, and is drivingly connected to the second threaded rod; the fixing mechanism is fixedly connected to the upper base.
6. The single crystal furnace doping device according to claim 5, It is characterized in that The slide rails include four, and the lifting mechanism also includes two first connecting members and one second connecting member; one end of the two first connecting members are fixedly connected to the material guide tube, and the other ends of the two first connecting members are respectively slidably connected to the two slide rails on both sides of the material guide tube; the second connecting member is provided with two first through holes and an internal threaded through hole, one end of the second connecting member is fixedly connected to the material guide tube, and is respectively slidably connected to the two slide rails away from the material guide tube through the two first through holes, and the second threaded rod is threadedly connected to the internal threaded through hole.
7. The single crystal furnace doping device according to claim 6, It is characterized in that The material guiding tube is a quartz material guiding tube, and a flexible corrugated tube is sleeved on the material guiding tube.
8. A single crystal furnace, It is characterized in that It comprises a single crystal furnace body and a single crystal furnace doping device as claimed in claims 1 to 7; A funnel is fixedly mounted on the graphite heat shield inside the single crystal furnace body, the inlet of the funnel is located at the upper end of the graphite heat shield, and the outlet of the funnel is located at the quartz outer flow guide cover above the molten soup, and the quartz outer flow guide cover is provided with a plurality of dopant vapor discharge holes; The fixing mechanism of the single crystal furnace doping device is fixedly installed on the furnace barrel of the single crystal furnace body, and the material guide pipe of the feeding mechanism is inserted into the single crystal furnace from above the furnace body of the single crystal furnace body and fixed on the furnace body through the lower base of the lifting mechanism.
9. The single crystal furnace according to claim 8, It is characterized in that The material guide pipe of the feeding mechanism is inserted into the single crystal furnace from the position of the observation window of the single crystal furnace body.
10. A method for pulling a heavily doped silicon single crystal, It is characterized in that The implementation subject is the single crystal furnace as claimed in claim 8 or 9, and the crystal pulling method comprises: Step S1: controlling the lifting mechanism of the single crystal furnace doping device to move the lower end of the material guide pipe into the funnel mouth; Step S2: calculating the doping amount of the dopant of the silicon single crystal to be pulled; Step S3: adding the corresponding dopant into the material storage mechanism according to the calculated doping amount; Step S4: setting the doping rate of the dopant by setting the rotation speed of the first motor; Step S5: starting the crystal pulling procedure of the single crystal furnace; Step S6: At the same time, after the vacuum of the single crystal furnace doping device is extracted, a switch valve is provided between the discharge end of the storage chamber and the feed end of the feeding control component; argon gas is introduced, and the first motor is started to allow the dopant to enter the funnel along the guide pipe, so that it can be output through the funnel and then evaporated into the melt.
Citation Information
Cited By
Gas phase doping device and doping method for low-resistivity heavily phosphorus-doped silicon single crystal
CN120989733A
Dopant guiding device and single crystal furnace with high doping efficiency
CN121250532A
Dopant flow guide and single crystal furnace with high doping efficiency