Membrane material and display module
By setting a communication structure in the closed gap of the display module, the molding problem caused by deformation of the protective film during the secondary vacuum defoaming process is solved, and the visual effect of the product is improved.
Patent Information
- Application Number
- CN202411147660.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-29
AI Technical Summary
During the secondary vacuum defoaming process of the display module, the protective film is deformed due to inconsistent pressure of the sealed gap, resulting in molding, affecting the visual effect.
A membrane material is designed to connect it with the external environment by setting a communication structure in the closed gap to avoid a closed state and prevent micro-deformation.
It effectively avoids molding on the surface of the display panel and improves the visual effect of the product.
Smart Images

Figure CN119053173A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of electronic equipment, and more specifically, to a film material and a display module. Background Art
[0002] For various modules that need to be attached with protective films, such as display modules, when a closed space is formed in the protective film, if the module needs secondary vacuum degassing, the deformation of the protective film in the closed space may cause mold marks on the module.
[0003] For example, a protective film (SCF Tape) is usually set on the back of a conventional OLED display module as a protective layer, and a graphite layer is added to the protective layer to improve heat distribution and heat dissipation capabilities, and PET is used for edge wrapping to prevent graphite from falling off. However, in this solution, there is a gap between the graphite and PET, which forms a closed state after the copper foil is attached. When secondary vacuum degassing is required, the protective film may be deformed, and the display panel may be slightly deformed, resulting in a visible mold print on the front, affecting the visual effect of the product. Summary of the invention
[0004] The purpose of the present disclosure is to provide a film material and a display module to solve the technical problem in the related art that the film material with a closed gap is deformed during the secondary vacuum degassing process, resulting in mold marks on the surface of the module such as the display panel.
[0005] In order to achieve the above objectives, the present invention adopts the following technical solutions:
[0006] The first aspect of the present disclosure provides a film material, comprising:
[0007] The first film layer;
[0008] a second film layer, disposed on a first side of the first film layer;
[0009] a third film layer, disposed on a first side of the first film layer, and surrounding the second film layer, with a first gap formed between the third film layer and the second film layer;
[0010] a fourth film layer, covering the second film layer, the third film layer and the first gap;
[0011] The film material also includes a first connecting structure, which is formed on at least one of the third film layer and the fourth film layer or at least two of the second film layer, the third film layer and the fourth film layer, and connects the first gap with the external environment.
[0012] Optionally, the third membrane layer includes at least one corner area, and the third membrane layer at at least one corner area includes a third sub-membrane layer and a fourth sub-membrane layer, and the corner area is formed when the third sub-membrane layer and the fourth sub-membrane layer are arranged around the second membrane layer, and a second gap is formed between the third sub-membrane layer and the fourth sub-membrane layer, and the second gap is connected to the first gap and the external environment, and the second gap forms the first connecting structure.
[0013] Optionally, when the third film layer is arranged around the second film layer, four corner regions are formed, at least one corner region has the second gap formed therein, and the second gap is arranged along the direction of the angle bisector of the corner region corresponding to the corner.
[0014] Optionally, the first film layer also includes a first through hole, the second film layer also includes a second through hole, the second through hole's orthographic projection on the first film layer covers the orthographic projection of the first through hole on the first film layer, the third film layer also surrounds the first through hole and a third gap is formed between the outer edge of the third film layer and the inner wall of the second through hole, the second connecting structure is formed on the fourth film layer or on at least two layers of the second film layer, the third film layer and the fourth film layer, and the second connecting structure connects the third gap with the external environment.
[0015] Optionally, the second film layer and / or the third film layer are provided with a first notch on the edge facing the first gap, the first notch is connected to the first gap, and the fourth film layer is provided with a first opening, the orthographic projection of the first opening on the first film layer at least partially overlaps with the orthographic projection of the first notch on the first film layer, and the first opening and the first notch form the first connecting structure.
[0016] Optionally, the film material also includes a fifth film layer, which is arranged on a side of the fourth film layer away from the third film layer, and a second opening is provided on the fifth film layer, and the orthographic projection of the second opening on the first film layer at least partially overlaps with the orthographic projection of the first opening on the first film layer, and the first notch, the first opening and the second opening form the first connecting structure.
[0017] Optionally, a center position of an orthographic projection of the first opening on the first film layer overlaps with a center position of an orthographic projection of the second opening on the first film layer, and the second opening is a linear opening.
[0018] Optionally, the film material also includes a sixth film layer arranged between the first film layer and the third film layer, the sixth film layer covers the first film layer and the second film layer, and a first opening is arranged on the fourth film layer, and the orthographic projection of the first opening on the first film layer and the orthographic projection of the first gap on the first film layer have at least a partial overlapping area, and the first opening forms the first connecting structure.
[0019] Optionally, the first film layer is a substrate layer, the second film layer is a heat dissipation layer, the third film layer is a sealing frame layer, and the fourth film layer is a metal layer.
[0020] A second aspect of the present disclosure provides a display module, comprising a display panel and the above-mentioned film material, wherein the film material is arranged on the backlight side of the display panel.
[0021] The beneficial effects of the present disclosure are as follows:
[0022] The film material of the disclosed embodiment can connect the first gap in a closed state with the external environment by providing a first connecting structure, so that the first gap is no longer in a closed state, thereby avoiding micro-deformation in the secondary vacuum degassing process, and further avoiding the formation of mold prints on the surface of the display panel, thereby improving the visual effect of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The specific implementation methods of the present disclosure are further described in detail below with reference to the accompanying drawings.
[0024] Figure 1 It is a schematic diagram of the planar structure of the protective film in the related art and the film layer structure in the thickness direction of the display device;
[0025] Figure 2 A schematic diagram of producing a mold print for a display device provided with a protective film;
[0026] Figure 3 A schematic plan view of a membrane material provided in an embodiment of the present disclosure;
[0027] Figure 4 A schematic diagram of the film layer structure of the film material provided in an embodiment of the present disclosure along the B1-B2 section line direction;
[0028] Figure 5 A schematic diagram of an embodiment of a first connecting structure provided by the present disclosure;
[0029] Figure 6 A schematic diagram of an embodiment of a first connecting structure provided by the present disclosure;
[0030] Figure 7 A schematic diagram of an embodiment of a first connecting structure provided by the present disclosure;
[0031] Figure 8A schematic diagram of an embodiment of a first connecting structure provided by the present disclosure;
[0032] Fig. 9 A schematic diagram of an embodiment of a first connecting structure provided by the present disclosure;
[0033] Fig.10 A schematic diagram of an embodiment of a first connecting structure provided by the present disclosure;
[0034] Fig.11 A schematic diagram of an embodiment of a first connecting structure provided by the present disclosure. DETAILED DESCRIPTION
[0035] In order to make the purpose, technical solution and advantages of the embodiments of the present disclosure clearer, the technical solution of the embodiments of the present disclosure will be clearly and completely described below in conjunction with the drawings of the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the described embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.
[0036] Unless otherwise defined, the technical terms or scientific terms used in the present disclosure should be understood by people with ordinary skills in the field to which the present disclosure belongs. The "first", "second" and similar words used in the present disclosure do not indicate any order, quantity or importance, but are only used to distinguish different components. Similarly, similar words such as "one", "one" or "the" do not indicate quantity restrictions, but indicate that there is at least one. Similar words such as "include" or "comprise" mean that the elements or objects appearing before the word cover the elements or objects listed after the word and their equivalents, without excluding other elements or objects. Similar words such as "connect" or "connected" are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.
[0037] In the related art, for various modules that need to be attached with a protective film, such as a display module, when a closed space is formed in the protective film, if the module needs to undergo secondary vacuum degassing, deformation of the protective film in the closed space may cause mold marks on the module.
[0038] In the disclosed embodiment, the module is described as a display module as an example. The OLED display module is attached with a protective film on the back of the display panel, and in order to improve the heat distribution and heat dissipation capacity of the protective layer, a graphite layer is also added to the thin film layer. Since graphite has a powder falling problem, it is also necessary to use a PET film to wrap the graphite layer. However, due to current process limitations, a gap is provided between the PET film and the graphite, and the gap forms a closed state after the copper foil is attached. When secondary vacuum degassing is required, the closed gap is inconsistent with the external pressure, which will cause the protective film to deform, and eventually the display panel will be slightly deformed, thereby producing a visible mold print on the front, affecting the user's visual experience. In addition, a fingerprint module hole is usually provided on the display panel. At the position of the fingerprint module hole, the graphite layer has a corresponding opening, and the graphite layer at the opening also needs to be wrapped with a PET film to prevent graphite from falling into the fingerprint module hole. Therefore, at this position, the gap between the graphite layer and the PET film will form a closed state after the copper foil is attached. The closed gap will also cause mold printing during the secondary vacuum degassing, affecting the user's visual experience.
[0039] Please refer to Figure 1 to Figure 2 , Figure 1 Schematic diagram of the planar structure of the protective film in the related art and the film layer structure in the thickness direction of the display device, Figure 2 A schematic diagram of producing a mold print for a display device provided with a protective film, Figure 1 The schematic diagram of the membrane layer in the middle and lower part is a cross-sectional view of the upper plane along the C1-C2 direction, as shown in Figure 1 to Figure 2 As shown, a graphite layer 11 is arranged above the first protective film 10, and the graphite layer 11 is edged by the PET layer 12, and a gap X0 is formed between the graphite layer 11 and the PET layer 12. After the PET layer 12 and the graphite layer 11 are covered by the copper foil 13, the gap X0 forms a closed state. Similarly, the gap between the graphite layer 11 and the PET layer 12 near the fingerprint module hole H0 is recorded as X1, and the gap X1 will also form a closed state after being covered by the copper foil 13. When secondary vacuum degassing is required, the gap X0 and the gap X1 are in a normal pressure state, and the external environment (vacuum environment) is in a low pressure state. The internal and external pressures of the gaps X0 and X1 are inconsistent, which will cause micro-deformation of each film layer at this position, and the display panel 14 and the transparent adhesive layer 15 arranged between the display panel 14 and the cover plate 16 will also be slightly deformed, thereby producing a front visible mold print on one side of the cover plate 16. Among them, the first protective film 10 includes an EMBO adhesive layer 101 and a Foam film layer 102 stacked.
[0040] It is understandable that the technical solution in the embodiments of the present disclosure is not limited to display modules, but can also be applied to all modules with closed gaps and requiring a secondary vacuum degassing process. The following embodiments are described by taking the module as a display module and the film material as a protective film attached to the display module and having a heat dissipation function as an example.
[0041] In order to solve the above technical problems, the present disclosure provides a film material and a display module. Figures 3 to 8 , Figure 3 A schematic plan view of a membrane material provided in an embodiment of the present disclosure, Figure 4 A schematic diagram of the film layer structure of the film material provided in the embodiment of the present disclosure along the B1-B2 section line direction, Figures 5 to 8 Schematic diagram of the structure of each embodiment of the first connecting structure, such as Figures 3 to 8 As shown, the film material 20 includes:
[0042] A first film layer 201;
[0043] A second film layer 202, disposed on a first side of the first film layer 201;
[0044] The third film layer 203 is disposed on the first side of the first film layer 201 and is disposed around the second film layer 202, and a first gap X10 is formed between the third film layer 203 and the second film layer 202;
[0045] A fourth film layer 204, covering the second film layer, the third film layer and the first gap X10;
[0046] The film material 20 also includes a first connecting structure 30, which is formed on at least one layer of the third film layer 203 and the fourth film layer 204 or at least two layers of the second film layer 202, the third film layer 203 and the fourth film layer 204, and the first connecting structure 30 connects the first gap X10 with the external environment.
[0047] In a possible implementation, the film material 20 is applied to a display module, which includes a display panel. The film material 20 may be a film material that is disposed on the backlight side of the display panel 20 and has a heat dissipation function.
[0048] Optionally, the first film layer 201 is a substrate layer, which includes a first sub-film layer 2011 and a second sub-film layer 2022 that are stacked, the first sub-film layer 2011 is arranged on the side of the film material 20 close to the display panel, the second sub-film layer 2022 is arranged on the side of the film material 20 away from the display panel, and the second film layer 202 and the third film layer 203 are arranged on the side of the second sub-film layer 2022 away from the display panel.
[0049] Optionally, the first sub-film layer 2011 is an EMBO adhesive layer, and the second sub-film layer 2012 can be bonded to the display panel through the first sub-film layer 2011. The second sub-film layer 2012 is a foam material layer, i.e., a Foam film layer, which is a film layer made of foam material. The foam material has good compressibility and recovery due to its porous structure, and can provide buffer protection for the display panel.
[0050] Optionally, the second film layer 202 is a heat dissipation layer, and the material of the heat dissipation layer may be graphite. The graphite layer is used to dissipate heat, which has a good heat dissipation effect.
[0051] Optionally, the third film layer 203 is a sealing layer for wrapping the second film layer 202. The third film layer 203 may be made of resin. The resin may be polyester film (full name: polyethylene glycol terephthalate, PET for short) or polyimide resin (Polyimide, PI) etc. according to actual application conditions.
[0052] Optionally, the fourth film layer 204 is a metal layer. Exemplarily, the material of the metal layer is copper foil, that is, the fourth film layer 204 is a copper foil layer, and the copper foil layer can seal the second film layer 202, prevent the graphite of the second film layer 202 from falling off, and enhance the thermal and electrical conductivity of the second film layer 202, thereby achieving a certain degree of electromagnetic shielding.
[0053] Optionally, the first connecting structure 30 is used to connect the first gap X10 with the external environment, so that the first gap X10 is no longer in a closed state. In a specific implementation, the first connecting structure 30 can be any structure such as an exhaust groove, an exhaust port, an exhaust line, etc., and the first connecting structure 30 can be provided on any one or two layers of the third film layer 203 and the fourth film layer 204, or on at least two layers of the second film layer 202, the third film layer 203 and the fourth film layer 204, as long as the first gap X10 can be connected with the external environment.
[0054] Compared with the related art, the film material of the embodiment of the present disclosure can connect the first gap in a closed state with the external environment by setting a first connecting structure, so that the first gap is no longer in a closed state, which can avoid micro-deformation in the secondary vacuum degassing process, and further avoid the formation of mold imprints on the surface of the display panel, thereby improving the visual effect of the product.
[0055] In a possible implementation, the film material further includes a fingerprint module hole H10 , and the fingerprint module hole H10 is formed by through holes formed on each layer of the film material 20 .
[0056] Exemplarily, the first film layer 201 further includes a first through hole 201H, the second film layer 202 further includes a second through hole 202H, the orthographic projection of the second through hole 202H on the first film layer 201 covers the orthographic projection of the first through hole 201H on the first film layer 201, the third film layer 203 also surrounds the first through hole 201H, and a third gap X11 is formed between the outer edge of the third film layer 203 and the inner wall of the second through hole 202H, the second connecting structure is formed on the fourth film layer 204 or at least two layers of the second film layer 202, the third film layer 203 and the fourth film layer 204, and the second connecting structure connects the third gap X11 with the external environment. Optionally, the second through hole 202H is coaxially arranged with the first through hole 201H.
[0057] In the embodiment of the present disclosure, the first gap X10 and the third gap X11 are both formed by the second film layer 202 and the third film layer 203 , and the first connecting structure 30 may be based on the same principle as the second connecting structure.
[0058] The following takes the first connected structure as an example to describe the specific implementation of the first connected structure.
[0059] In a possible implementation, the second film layer and / or the third film layer is provided with a first notch at an edge facing the first gap, and the first notch is connected to the first gap; the fourth film layer is provided with a first opening, and the orthographic projection of the first opening on the first film layer at least partially overlaps with the orthographic projection of the first notch on the first film layer; the first notch and the first opening form the first connecting structure. At this time, the first connecting structure is formed on the second film layer and the fourth film layer, or on the third film layer and the fourth film layer. It can be understood that the film material can also be provided with multiple first connecting structures, some of which are formed on the second film layer and the fourth film layer, and some of which are formed on the third film layer and the fourth film layer.
[0060] The orthographic projections of the first opening and the first notch on the first film layer at least partially overlap, including three schemes: (1) the orthographic projection of the first opening on the first film layer and the orthographic projection of the first notch on the first film layer have a partial overlapping area but do not completely overlap; (2) the orthographic projection of the first opening on the first film layer and the orthographic projection of the first notch on the first film layer completely overlap; (3) the orthographic projection of the first opening on the first film layer covers the orthographic projection of the first notch on the first film layer, or the orthographic projection of the first notch on the first film layer covers the orthographic projection of the first opening on the first film layer.
[0061] For the third solution, on the basis of connecting the first gap with the external environment and solving the problem of mold imprint on the display panel caused by deformation of the film material during the secondary vacuum degassing process, the smaller the size of the first notch and the first opening, the better. Therefore, the third structure is usually not adopted.
[0062] For the second solution, when the orthographic projections of the first opening and the first notch completely overlap, the contact area between the first opening and the first gap is the largest. Since graphite powder is falling off in the second film layer, the probability of graphite powder entering the first notch through the first gap and flowing out of the first opening is also relatively high. In order to reduce the probability of graphite powder flowing out of the first opening, the first opening and the first gap can be staggered, that is, the first solution can be adopted.
[0063] For the first solution, the first opening and the first notch are staggered. At this time, there is a partial overlapping area between the orthographic projections of the first opening and the first notch on the first film layer, and the size of the overlapping area is smaller than the size of the first opening or the first notch. By staggering the first opening, on the one hand, the first gap can be connected to the external environment via the first notch and the first opening, and on the other hand, the probability of graphite powder flowing out of the first opening can be reduced.
[0064] In a possible implementation, the film material 20 also includes a fifth film layer 205, and the fifth film layer 205 is arranged on the side of the fourth film layer 204 away from the third film layer 203, and a second opening is arranged on the fifth film layer 205, and the orthographic projection of the second opening on the first film layer at least partially overlaps with the orthographic projection of the first opening on the first film layer, and the first notch, the first opening and the second opening form the first connecting structure.
[0065] Exemplarily, the fifth film layer 205 is the second protective layer, and the fifth film layer 205 covers the fourth film layer 204. Therefore, when a first opening is opened on the fourth film layer 204, a second opening connected to the first opening also needs to be opened on the fifth film layer 205, so that the first gap X10 can be connected to the external environment via the first notch, the first opening, and the second opening.
[0066] Optionally, the center position of the orthographic projection of the first opening on the first film layer overlaps with the center position of the orthographic projection of the second opening on the first film layer. In this way, the first opening and the second opening can have a larger overlapping area, that is, the connecting channels overlap as much as possible, which can better balance the internal and external pressures on both sides of the first gap X10.
[0067] Optionally, the second opening is a linear opening. The linear opening can also be understood as an exhaust line, and the linear design of the exhaust line helps to reduce the resistance of the gas flowing in the exhaust line, so that the gas can flow more smoothly and quickly in the first exhaust channel, and the opening size of the exhaust line is small, which will not adversely affect the protection function of the fifth film layer 205.
[0068] Exemplarily, the linear openings include multiple linear openings extending along the first direction, such as the orthographic projection of the linear openings on the first film layer is in the shape of "="; or, the linear openings include at least one first linear opening extending along the first direction and at least one second linear opening extending along the second direction, such as the orthographic projection of the linear openings on the first film layer is in the shape of "+", "well", etc.
[0069] Combine the following Figures 5 to 8 A specific example in which the first communication structure is formed by the first notch, the first opening, and the second opening is described.
[0070] For example, Figure 5 As shown, the edge of the second film layer 202 facing the first gap X10 is provided with a first notch 301a, and the fourth film layer 204 is provided with a first opening 302a ( Figure 5 The first film layer 201 is provided with a second opening 303a ( Figure 5 The orthographic projection of the first opening 302a on the first film layer 201 partially overlaps with the orthographic projection of the first notch 301a on the first film layer 201, the orthographic projection of the second opening 303a on the first film layer 201 partially overlaps with the orthographic projection of the first opening 302a on the first film layer 201, and the first notch 301a, the first opening 302a and the second opening 303a form a first connecting structure 30.
[0071] Figure 5 In the illustrated embodiment, the second film layer 202 is grooved in a direction away from the third film layer 203 (i.e., a first notch 301a is provided), and a window design is performed on the fourth film layer 204 at the location of the first notch 301a (i.e., a first opening 302a is provided), so that the first gap X10 is connected to the external environment through the overlapping area of the first notch 301a and the first opening 302a. At the same time, considering that the fifth film layer 205 needs to be carried out together during the secondary vacuum degassing, the fifth film layer 205 is also designed with an exhaust line at the corresponding position of the window of the fourth film layer 204, so as to achieve the effect of balancing the internal and external pressures during degassing.
[0072] For example, Figure 6 As shown, the edge of the third film layer 203 facing the first gap X10 is provided with a first notch 301b, and the fourth film layer 204 is provided with a first opening 302b ( Figure 6The first film layer 201 is provided with a second opening 303b ( Figure 6 The orthographic projection of the first opening 302b on the first film layer 201 partially overlaps with the orthographic projection of the first notch 301b on the first film layer 201, the orthographic projection of the second opening 303b on the first film layer 201 partially overlaps with the orthographic projection of the first opening 302b on the first film layer 201, and the first notch 301b, the first opening 302b and the second opening 303b form a first connecting structure 30.
[0073] in, Figure 5 and Figure 6 In the illustrated embodiment, the second film layer 202 is rectangular, the third film layer 203 is a quadrilateral frame disposed around the second film layer 202 , and the first notch 301 a / 301 b is disposed on a straight edge of the third film layer 203 or the second film layer 202 .
[0074] In other embodiments, the first notch 301 a / 301 b may also be disposed at a corner region of the second film layer 202 or the third film layer 203 .
[0075] For example, Figure 7 As shown, the second film layer 202 is rectangular, a first notch 301c is provided at the corner edge where the vertex of the second film layer 202 is located, and a first opening 302c ( Figure 7 A second opening 303c is provided on the fifth film layer 205 ( Figure 7 “+” shaped exhaust line).
[0076] For example, Figure 8 As shown, the second film layer 202 is rectangular, the third film layer 203 is arranged in a quadrilateral frame, a first notch 301d is arranged at the corner edge of the third film layer 203, and a first opening 302d is arranged on the fourth film layer 204 ( Figure 8 A second opening 303d ( Figure 8 “+” shaped exhaust line).
[0077] It is understandable that when the above Figures 5 to 8 When the scheme of the first connecting structure 30 shown is applied to the third gap X11 formed around the fingerprint module hole H10, the second film layer 202 and the third film layer 203, it can be understood that the second film layer 202 is arranged around the third film layer 203. At this time, the principle of setting the second connecting structure is the same as the scheme recorded in the above embodiments, and will not be repeated here.
[0078] It is understandable that, for the first gap X10 , either one first connecting structure 30 or multiple first connecting structures 30 may be provided on the film material 20 , and the embodiment of the present disclosure does not limit the specific number of the first connecting structures 30 .
[0079] In addition, when the display panel is a curved screen, the four sides of the curved screen are all arc-shaped, and the film material 20 also needs to be adapted to the curved screen. At this time, the film material 20 is also designed to be curved. When the four sides of the film material 20 are all arc-shaped, the four corner areas of the film material 20 are subjected to bidirectional compression when they are attached to the display panel. If the deformation of each film layer of the film material 20 (especially the third film layer 203) is not enough to cover the compression amount, wrinkles may occur.
[0080] In order to alleviate the wrinkling phenomenon of the film material 20 at the corner position, in a possible implementation, the third film layer includes at least one corner area, and the third film layer at at least one corner area includes a third sub-film layer and a fourth sub-film layer, and the third sub-film layer and the fourth sub-film layer are arranged around the second film layer to form the corner area, and a second gap X12 is formed between the third sub-film layer and the fourth sub-film layer, and the second gap X12 is connected to the first gap X10 and the external environment, and the second gap X12 forms the first connecting structure 30. At this time, the first connecting structure 30 is formed in the third film layer 203.
[0081] In the embodiment of the present disclosure, a second gap X12 is set in the corner area of the third film layer 203, and the second gap X12 connects the first gap X10 and the external environment. On the one hand, after the second gap X12 is set, when the film layer is subjected to bidirectional extrusion, the second gap X12 allows air to flow freely, thereby effectively balancing the pressure difference on both sides of the film layer. This balancing effect reduces the deformation and wrinkles of the film layer caused by uneven pressure, and the existence of the second gap X12 provides a certain elastic space for the film layer, so that the film material can have a larger deformation space to adapt to compression during the bonding process, thereby reducing wrinkles caused by excessive compression; in addition, the corner area is an area of stress concentration. By setting the second gap X12, the stress transfer path can be changed, so that the stress distribution is more uniform, reducing the risk of excessive local stress, and thus reducing the generation of wrinkles.
[0082] Optionally, when the third film layer is arranged around the second film layer, four corner regions are formed, at least one corner region has the second gap formed therein, and the second gap is arranged along the direction of the angle bisector of the corner region corresponding to the corner.
[0083] Exemplarily, the second film layer 202 is rectangular, and the third film layer 203 forms four corner regions A when arranged around the second film layer 202, and the third film layer 203 at at least one corner region A includes the third sub-film layer 2031 and the fourth sub-film layer 2032, and a second gap X12 is formed between the third sub-film layer 2031 and the fourth sub-film layer 2032. It can be understood that the second film layer 202 is rectangular, and the corner regions of the second film layer 202 can be either right-angled sides or arc-shaped corners.
[0084] Optionally, the corner angle of the corner area is 90°, and the third sub-membrane layer 2031 and the fourth sub-membrane layer 2032 form the second gap X12 at the 45° corner position. Setting the second gap X12 at the 45° corner position (i.e., equivalent to the angle bisector direction of the corner) is, on the one hand, conducive to maximizing the relief of the wrinkle phenomenon at the corner area, and on the other hand, it can also make the first gap X10 connected to the second gap X12 symmetrically distributed around the second gap X12 at the corner area, which is more conducive to balancing the internal and external pressures.
[0085] like Figure 4 As shown, the second gap X12 is set at the 45° position of the four corners of the third film layer 203, so that the external environment is connected to the first gap X10 through the second gap X12, thereby balancing the pressure; at the same time, because the second gap X12 can alleviate the compression during bonding, the wrinkles on the third film layer 203 can be alleviated, which can be beneficial to the alleviation of wrinkles in the entire corner position.
[0086] In a possible implementation, the orthographic projection of the second gap on the first film layer is curved. Fig. 9 As shown, by setting the second gap X12 to be curved, the difficulty of the graphite powder in the second film layer 202 flowing out of the film material 20 through the first gap X10 and the second gap X12 can be increased, making it more difficult for the graphite powder to flow out of the film material 20.
[0087] It can be understood that, in the case where a first gap X10 and a third gap X11 are formed on the film material 20, the first connecting structure set at the first gap X10 adopts the implementation scheme of the second gap X12, and the second connecting structure set at the third gap X11 can adopt a scheme of setting openings (such as a first notch, a first opening, and a second opening).
[0088] In a possible implementation, the first connection structure is formed on the fourth film layer, that is, only an opening can be provided on the fourth film layer to form the first connection structure. For example, a second opening is provided on the fourth film layer, and the orthographic projection of the second opening on the first film layer and the orthographic projection of the first gap on the first film layer at least partially overlap, and the second opening forms the first connection structure. Similarly, the second connection structure can adopt the same structure as the first connection structure, and in this case, the second connection structure is formed on the fourth film layer.
[0089] like Fig.10 As shown, in this embodiment, a first opening 302e (such as an exhaust line) is directly opened at a position corresponding to the first gap X10 on the fourth film layer 204, and the first gap X10 is connected to the external environment through the first opening 302e. This manufacturing method is simple and has a low cost (the cost of the knife die for cutting through the fourth film layer 204 to form the first opening 302e is low), but it will cause serious appearance problems and reliability (such as copper foil warping, graphite powder exposure, etc.), and the exhaust effect is poor.
[0090] It is understandable that when the film layer 20 further includes the fifth film layer 205 as shown above, the fifth film layer 205 also needs to have a second opening 303e, and the orthographic projection of the second opening 303e on the first film layer 201 at least partially overlaps with the orthographic projection of the first opening 302e on the first film layer 201. In this case, the first connecting structure is formed on the fourth film layer and the fifth film layer. Similarly, the second connecting structure can also be formed on the fourth film layer and the fifth film layer.
[0091] In a possible implementation, the film material also includes a sixth film layer arranged between the first film layer and the third film layer, the sixth film layer covers the first film layer and the second film layer, the fourth film layer is provided with a first opening, the orthographic projection of the first opening on the first film layer and the orthographic projection of the first gap on the first film layer have at least a partial overlapping area, and the first opening forms the first connecting structure.
[0092] Optionally, the film material also includes a fifth film layer, which is arranged on a side of the fourth film layer away from the third film layer, and a second opening is arranged on the fifth film layer, and the orthographic projection of the second opening on the first film layer at least partially overlaps with the orthographic projection of the first opening on the first film layer, and the first opening and the second opening form a first connecting structure.
[0093] Optionally, the sixth film layer is an insulating tape. The thickness of the sixth film layer is relatively thin, and exemplary, the thickness of the sixth film layer is 0.01 mm.
[0094] like Fig.11As shown, in the specific implementation, the second film layer 202 is covered by an insulating tape to prevent the graphite powder from falling off. At the same time, at the first gap X0, the fourth film layer 204 and the fifth film layer 205 are cut through together to cut out a window or exhaust line, wherein a first opening 302f is formed on the fourth film layer 204, and a second opening 303f is formed on the fifth film layer 205, and the first opening 302f and the second opening 303f form an exhaust channel. This solution can prevent graphite powder from falling to the outside, but due to the addition of the sixth film layer 206, the material cost and process cost are increased, and due to the increase in the number of layers, the probability of stratification of the film material during the whole machine is also increased, which is not conducive to improving the competitiveness of the film material.
[0095] It can be understood that multiple first connecting structures and multiple second connecting structures can be set on the membrane material, some of the multiple first connecting structures can adopt the second gap scheme, some can adopt any one or any multiple opening schemes, and some of the multiple second connecting structures can adopt any one or any multiple opening schemes.
[0096] Based on the same inventive concept, a second aspect of the present disclosure provides a module, including a module body and the film material as described above.
[0097] Optionally, the module is a display module, the module body is a display panel, and the film material is arranged on the backlight side of the display panel, and the film material is as described in the above embodiment. That is, the present disclosure also provides a display module, including a display panel and the film material as described above, and the film material is arranged on the backlight side of the display panel. Optionally, on the light-emitting side of the display panel, the display module may also include a stacked optical adhesive (Optically Clear Adhesive, OCA) layer and a cover plate, etc. Exemplarily, the cover plate may be a glass cover plate (CG), etc.
[0098] For example, the film material can be applied to devices with display functions such as mobile phones, computer monitors, tablet computers, televisions, advertising screens, etc., which are not listed here in this disclosure. The beneficial effects of the display device can be found in the detailed discussion in the above method embodiment, which will not be repeated here.
[0099] It is understandable that the display device in the embodiment of the present disclosure may include multiple types, and can be selected and set according to actual needs. For example, the display device may be an organic light-emitting diode (OLED) display, a quantum dot light-emitting diode (QLED) display, or a micro light-emitting diode (Micro LED) display.
[0100] Obviously, the above embodiments of the present disclosure are merely examples for clearly illustrating the present disclosure, and are not limitations on the implementation methods of the present disclosure. For ordinary technicians in this field, other different forms of changes or modifications can be made on the basis of the above description. It is impossible to list all the implementation methods here. All obvious changes or modifications derived from the technical solution of the present disclosure are still within the protection scope of the present disclosure.
Claims
1. A membrane material, characterized in that: include: The first film layer; a second film layer, disposed on a first side of the first film layer; a third film layer, disposed on a first side of the first film layer, and surrounding the second film layer, with a first gap formed between the third film layer and the second film layer; a fourth film layer, covering the second film layer, the third film layer and the first gap; The film material also includes a first connecting structure, which is formed on at least one of the third film layer and the fourth film layer or at least two of the second film layer, the third film layer and the fourth film layer, and connects the first gap with the external environment.
2. The membrane material according to claim 1, characterized in that: The third membrane layer includes at least one corner area, and the third membrane layer at at least one corner area includes a third sub-membrane layer and a fourth sub-membrane layer. The corner area is formed when the third sub-membrane layer and the fourth sub-membrane layer are arranged around the second membrane layer. A second gap is formed between the third sub-membrane layer and the fourth sub-membrane layer. The second gap is connected to the first gap and the external environment, and the second gap forms the first connecting structure.
3. The membrane material according to claim 1, characterized in that: When the third film layer is arranged around the second film layer, four corner regions are formed, at least one corner region has the second gap formed therein, and the second gap is arranged along the direction of the angle bisector of the corner region corresponding to the corner.
4. The membrane material according to claim 1, characterized in that: The first film layer also includes a first through hole, the second film layer also includes a second through hole, the second through hole's orthographic projection on the first film layer covers the orthographic projection of the first through hole on the first film layer, the third film layer also surrounds the first through hole and a third gap is formed between the outer edge of the third film layer and the inner wall of the second through hole, the second connecting structure is formed on the fourth film layer or at least two layers of the second film layer, the third film layer and the fourth film layer, and the second connecting structure connects the third gap with the external environment.
5. The membrane material according to claim 1, characterized in that: The second film layer and / or the third film layer are provided with a first notch at the edge facing the first gap, the first notch is connected with the first gap, the fourth film layer is provided with a first opening, the orthographic projection of the first opening on the first film layer at least partially overlaps with the orthographic projection of the first notch on the first film layer, and the first opening and the first notch form the first connecting structure.
6. The membrane material according to claim 5, characterized in that: The film material also includes a fifth film layer, which is arranged on a side of the fourth film layer away from the third film layer. A second opening is arranged on the fifth film layer, and the orthographic projection of the second opening on the first film layer at least partially overlaps with the orthographic projection of the first opening on the first film layer. The first notch, the first opening and the second opening form the first connecting structure.
7. The membrane material according to claim 6, characterized in that: The center position of the orthographic projection of the first opening on the first film layer overlaps with the center position of the orthographic projection of the second opening on the first film layer, and the second opening is a linear opening.
8. The membrane material according to claim 1, characterized in that: The film material also includes a sixth film layer arranged between the first film layer and the third film layer, the sixth film layer covers the first film layer and the second film layer, and a first opening is arranged on the fourth film layer. The orthographic projection of the first opening on the first film layer and the orthographic projection of the first gap on the first film layer have at least a partial overlapping area, and the first opening forms the first connecting structure.
9. The membrane material according to claim 1, characterized in that: The first film layer is a substrate layer, the second film layer is a heat dissipation layer, the third film layer is a sealing frame layer, and the fourth film layer is a metal layer.
10. A display module, characterized in that: The invention comprises a display panel and the film material according to any one of claims 1 to 9, wherein the film material is arranged on the backlight side of the display panel.