Preparation method of FeO under laboratory conditions
By controlling particle size and atmosphere conditions, FeO was prepared by calcining FeC2O4·2H2O, which solved the problem of preparing high-purity FeO in the laboratory, simplified the operation, improved the purity of the product, and promoted the development of metallurgical technology.
Patent Information
- Application Number
- CN202511649026.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-12
- Publication Date
- 2026-01-16
AI Technical Summary
Existing technologies make it difficult to efficiently prepare high-purity FeO under laboratory conditions, and the preparation conditions are harsh or easily generate impurities such as Fe3O4.
FeC2O4·2H2O reagent with a particle size of less than 150 mesh was used, combined with Ar gas and Ar+CO+CO2 mixed gas protection, and the heating rate and temperature were controlled. The calcination was carried out at 810℃ for 30 minutes to ensure the purity of FeO.
This method enables the simple and effective preparation of high-purity FeO, improves the accuracy of experimental research, and promotes the development of metallurgical technology.
Smart Images

Figure CN121342093A_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The present application belongs to the field of metallurgy, and particularly relates to a preparation method of FeO under laboratory conditions. BACKGROUND
[0002] In the steel metallurgy process, FeO plays a very important role in different stages of slag. For example, in the iron-making process of blast furnace, the amount of FeO generated in the furnace charge will affect the composition and fluidity of the initial slag, thus determining the position and shape of the softening zone, and further affecting the permeability of the whole blast furnace; in the steel-making process of converter, the content of FeO in the steel slag directly determines the strength of its oxidizability, which has an important influence on the links of dephosphorization, desulfurization and deoxidization. Therefore, the physicochemical properties of the FeO-containing slag system are the object of attention of metallurgists. Generally, since FeO cannot exist stably at normal temperature, it is often prepared on site for use in the laboratory. In the existing technology, the preparation of FeO can be divided into two categories: (1) reducing trivalent iron oxide (Fe2O3) by controlling a suitable reducing atmosphere, which requires strict control of the temperature and the ratio of the reducing gas. If the control is not good, metallic iron or Fe3O4 is easily generated; (2) decomposing ferrous oxalate (FeC2O4·H2O) by heating under the condition of air isolation. This method is relatively simple, but the preparation conditions are relatively harsh. If air cannot be isolated, high-valence oxides such as Fe3O4 are easily generated, and pure FeO is difficult to obtain. SUMMARY
[0003] The present application provides a preparation method of FeO under laboratory conditions, which can conveniently prepare FeO with high purity under laboratory conditions, provides FeO raw material for the FeO-containing slag system, helps to improve the accuracy of the research on the FeO-containing slag system, and promotes the development of metallurgical technology.
[0004] The technical scheme of the present application is as follows: A preparation method of FeO under laboratory conditions, comprising the following steps: 1) grinding a certain amount of FeC2O4·2H2O reagent to a particle size of less than 150 mesh, laying it on the bottom of a crucible to obtain a material layer with a thickness of not more than 30 mm; 2) determining the composition of the protective gas; calculating the flow rate of the protective gas according to the mass of the FeC2O4·2H2O reagent; 3) calcining the crucible and passing the protective gas, starting from room temperature and heating to 810℃ at a heating rate of 10℃ / min, and keeping the temperature for 30 min; then naturally cooling to room temperature; obtaining the calcined product as FeO.
[0005] Further, in the step 1) of the preparation method of FeO under laboratory conditions, the mass of the FeC2O4·2H2O reagent is 20g-100g.
[0006] Furthermore, in the method for preparing FeO under laboratory conditions, step 2) includes two types of protective gas: Ar gas and Ar+CO+CO2 mixed gas.
[0007] Furthermore, in the method for preparing FeO under laboratory conditions, the formula for calculating the flow rate of the protective gas in step 2) is as follows: Q Ar =1.67×10 -3 m+0.37 (1) Q CO =0.125×Q Ar (2) Q CO2 =0.125×Q Ar (3) In the formula, Q Ar —Ar flow rate, m 3 / h;Q CO —CO flow, m 3 / h;Q CO2 —CO2 flow rate, m 3 / h; m—mass of FeC2O4·2H2O reagent, g; The actual flow rate of the protective gas differs from the calculated result by no more than 5%.
[0008] Furthermore, in the method for preparing FeO under laboratory conditions, in step 3), the protective gas is introduced in the following ways: when the temperature is below 570°C, only Ar gas is introduced for protection; when the temperature is above 570°C, a mixture of Ar, CO, and CO2 gas is introduced for protection.
[0009] The beneficial effects of this invention are as follows: This invention prepares FeO by calcining FeC2O4·2H2O at a certain temperature and in a certain atmosphere, which has the characteristics of short process flow, simple operation and high product purity; it solves the problems of high difficulty and low purity of traditional FeO preparation technology, effectively improves the purity of FeO reagents used in experiments, helps to improve the accuracy of research on FeO-containing slag systems, and promotes the development of metallurgical technology. Attached Figure Description
[0010] Figure 1 A schematic diagram of the temperature rise and atmosphere composition during the roasting process; Figure 2 The image shows the XRD pattern of the calcined product. Detailed Implementation
[0011] A method for preparing FeO under laboratory conditions, comprising the following steps: 1) Grind 50g of FeC2O4·2H2O reagent to a particle size of less than 150 mesh, spread it evenly at the bottom of the crucible, and obtain a material layer with a thickness of no more than 30mm under natural stacking conditions; 2) Determine the composition of the protective gas, including two types: Ar gas and Ar+CO+CO2 mixture; Based on the mass of the FeC2O4·2H2O reagent, calculate the flow rate of the protective gas; the calculation formula is as follows: Q Ar =1.67×10 -3 ×50 + 0.37 = 0.45m 3 / h (1) Q CO =0.125×0.45m 3 / h= 0.057m 3 / h (2) Q CO2 =0.125×0.45m 3 / h= 0.057m 3 / h (3) The actual flow rate of the protective gas should not differ from the calculated result by more than 5%. 3) The crucible is roasted under a protective gas atmosphere. The temperature is increased from room temperature to 810℃ at a rate of 10℃ / min, and held at this temperature for 30 minutes. Then, it is allowed to cool naturally to room temperature. The protective gas is introduced as follows: when the temperature is below 570℃, only Ar gas is introduced for protection; when the temperature is above 570℃, a mixture of Ar, CO, and CO2 gas is introduced for protection. The oxygen potential corresponding to this atmosphere ensures that FeC2O4 is neither oxidized nor reduced during decomposition, allowing Fe to exist only in its divalent form, i.e., FeO. The roasting process is as follows: Figure 1 As shown; the obtained product was subjected to XRD analysis, and the results are as follows. Figure 2 As shown; by Figure 2 It can be seen that, due to the control of the appropriate oxygen potential, FeC2O4·2H2O is neither oxidized nor reduced during the decomposition process, and the calcination product is only FeO, with no other impurities observed.
Claims
1. A method for the preparation of FeO under laboratory conditions, characterized in that, The method comprises the following steps: 1) grinding a certain mass of FeC2O4.2H2O reagent to a particle size of less than 150 mesh, laying on the bottom of a crucible to obtain a material layer with a thickness of not more than 30 mm; 2) determining the composition of the protective gas; according to the mass of the FeC2O4.2H2O reagent, the flow rate of the protective gas is calculated; 3) calcining the crucible and passing the protective gas, starting from room temperature and heating to 810 DEG C at a temperature rising rate of 10 DEG C / min, keeping the temperature for 30 min, and then naturally cooling to room temperature; obtaining the calcined product FeO.
2. The method of claim 1, wherein the FeO is prepared under laboratory conditions, characterized in that, In the step 1), the mass of the FeC2O4.2H2O reagent is 20 g to 100 g.
3. The method of claim 1, wherein the FeO is prepared under laboratory conditions, characterized by, In the step 2), the composition of the protective gas includes Ar gas and Ar+CO+CO2 mixed gas.
4. The method of claim 3, wherein the FeO is prepared under laboratory conditions characterized by, In the step 2), the calculation formula of the flow rate of the protective gas is as follows: Q Ar = 1.67 x 10 -3 m+0.37 (1) Q CO = 0.125 x Q Ar (2) Q CO2 = 0.125 x Q Ar (3) wherein Q Ar — Ar flow rate, m 3 / h; Q CO — CO flow rate, m 3 / h; Q CO2 — CO2flow rate, m 3 / h; m - mass of FeC2O4·2H2O reagent, g; The actual flow rate of the protective gas is not more than 5% different from the calculation result.
5. The method of claim 4, wherein the FeO is prepared under laboratory conditions characterized by, In the step 3), the protective gas is passed in the following way: when the temperature is lower than 570 DEG C, only Ar gas is passed for protection; when the temperature is higher than 570 DEG C, Ar+CO+CO2 mixed gas is passed for protection.