Substrate assembly and method of manufacturing the same, package substrate, package structure, and electronic device
By fabricating annular holes on a glass substrate and then fabricating a buffer layer within those holes, and using a second glass substrate to support the glass pillars, the problem of uneven buffer layer thickness was solved, thus improving the buffering effect and fabrication efficiency.
Patent Information
- Application Number
- CN202610419227.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-03-31
- Publication Date
- 2026-06-23
AI Technical Summary
When filling the TGV hole with a conductive structure, stress mismatch between the buffer layer and the glass causes the glass to crack, and the inconsistent thickness of the buffer layer affects the buffering effect.
An annular hole is prepared on the first glass substrate, and a buffer layer is prepared inside the annular hole. A glass pillar is supported by a second glass substrate. After the second glass substrate is removed, a through hole is formed to prevent the glass pillar from being misaligned or falling off, and to ensure the uniformity of the buffer layer thickness.
The buffering effect of the buffer layer is improved, the risk of cracking of the glass substrate is reduced, the preparation efficiency is increased, and the preparation difficulty is reduced.
Smart Images

Figure CN122270159A_ABST
Abstract
Description
Technical Field
[0001] This application belongs to the field of packaging technology, and more specifically, relates to a substrate assembly and its preparation method, a packaging substrate, a packaging structure, and an electronic device. Background Technology
[0002] With the rapid development of high-performance chips and their packaging technologies, glass substrates are gradually replacing organic substrates due to their superior physical, chemical, and electrical properties.
[0003] Through-Glass Vias (TGVs) are a core component of chip substrates. After TGV vias are formed, conductive structures need to be filled inside. Stress mismatch between the conductive structure and the glass can cause the glass to crack. Therefore, a buffer layer needs to be added between the conductive structure and the glass within the via. Specifically, the TGV via is filled with a buffer layer, then a hole is drilled in the buffer layer, and finally the conductive structure is filled. It is difficult to keep the hole in the buffer layer concentric with the TGV via, resulting in inconsistent thickness of the buffer layer around the TGV via, leading to poor buffering performance. Summary of the Invention
[0004] The purpose of this application is to provide a substrate assembly and its preparation method, a packaged substrate, a packaged structure, and an electronic device to improve the buffering effect of the buffer layer.
[0005] To achieve the above objectives, the technical solution adopted in this application is as follows: In a first aspect, a method for fabricating a substrate assembly is provided, the method comprising: A glass substrate is provided, the glass substrate comprising a first glass substrate and a second glass substrate stacked together; An annular hole is formed in a first glass substrate, the annular hole penetrates the first glass substrate, a glass pillar is formed in the first glass substrate located on the inner periphery of the annular hole, and a second glass substrate covers the glass pillar. A first buffer layer is prepared within the annular hole; Remove the second glass substrate; Remove the glass column to form the first through hole.
[0006] Through the above technical solution, the preparation method provided in this application can form an annular hole on the first glass substrate, and then prepare an annular first buffer layer in the annular hole. During this process, the second glass substrate can support the glass pillar to prevent the glass pillar from being misaligned or falling off. After the first buffer layer is prepared, the second glass substrate can be removed first, and then the glass pillar can be removed. After removing the second glass substrate, it is convenient to remove the glass pillar. After removing the glass pillar, the location of the glass pillar naturally forms the first through hole. This eliminates the need for secondary drilling and helps to improve the uniformity of the thickness of the first buffer layer in the circumferential direction of the first through hole, thereby improving the buffering effect of the first buffer layer.
[0007] In some embodiments, after providing the glass substrate and before fabricating the first buffer layer within the annular hole, the fabrication method provided in this application further includes: Ventilation holes are prepared in the second glass substrate, and the ventilation holes are connected to the annular holes.
[0008] Through the above technical solution, the preparation method provided in this application prepares a vent hole on the second glass substrate and makes the vent hole connected with the annular hole. In this way, when the first buffer layer is prepared in the annular hole, the air in the annular hole can be discharged from the vent hole, which helps to reduce the air pressure in the annular hole, thereby facilitating the entry of the material for preparing the first buffer layer into the annular hole, and thus making it easier to prepare the first buffer layer.
[0009] Optionally, the surface of the second glass substrate facing away from the first glass substrate includes a venting region, and venting holes are formed in the second glass substrate, including: The second glass substrate is modified in the ventilated area to form a second modified structure; The second modified structure is removed to form pores.
[0010] Through the above technical solution, the preparation method provided in this application can form a weakened second modified structure, which is easy to remove, thereby facilitating the formation of pores.
[0011] Optionally, multiple vent holes are provided, spaced apart circumferentially along the annular hole. This facilitates the timely discharge of gas from the annular hole, allowing the material for the first buffer layer to enter the annular hole uniformly, thereby improving the uniformity of the first buffer layer.
[0012] Optionally, the orthographic projection of the vent hole on the surface of the first glass substrate facing away from the second glass substrate does not overlap with the orthographic projection of the glass pillar on the same surface. This increases the connection area between the glass pillar and the sacrificial layer, thereby increasing the strength of the connection and facilitating the removal of the glass pillar when the sacrificial layer is removed.
[0013] Optionally, the orthographic projection of the vent hole on the surface of the first glass substrate facing away from the second glass substrate is located within the orthographic projection of the annular hole on the surface of the first glass substrate facing away from the second glass substrate, which facilitates the timely discharge of gas from the annular hole.
[0014] In some embodiments, the surface of the first glass substrate facing away from the second glass substrate includes an annular region, and an annular hole is formed in the first glass substrate, including: The first glass substrate is modified in the annular region to form an annular first modified structure; The first modified structure is removed to form an annular hole.
[0015] Through the above technical solution, the preparation method provided in this application can form a weakened first modified structure, which is easy to remove, thereby facilitating the formation of annular pores.
[0016] Optionally, the first glass substrate is modified in the annular region by laser irradiation of the first glass substrate in the annular region, thereby forming a weakened first modified structure.
[0017] Optionally, removing the first modified structure to form an annular hole includes etching the first glass substrate.
[0018] Optionally, the annular region includes multiple sub-regions. After modifying the glass substrate in the annular region and before removing the first modified structure to form the annular hole, the preparation method includes: The glass substrate is modified again in the sub-region.
[0019] Through the above technical solution, after the formation of the first modified structure and before its removal, the preparation method provided in this application can further modify and weaken the first modified structure in a sub-region of the annular region, making it easier to remove the first modified structure.
[0020] Optionally, the sub-region is a circular region, and multiple sub-regions are spaced apart along the circumference of the annular region. This facilitates the weakening of the first modified structure, thereby making it easier to form annular holes.
[0021] In some embodiments, after preparing the first buffer layer within the annular hole and before removing the glass column, the preparation method provided in this application further includes: Weakening holes are prepared on the glass column, and the weakening holes penetrate the glass column.
[0022] This allows the glass column to be weakened through the weakening holes, making it easier to remove.
[0023] Optionally, the surface of the glass pillar facing away from the first glass substrate includes at least one weakening region, and a weakening hole is formed on the glass pillar, including: The glass column is modified in the weakened region to form a third modified structure.
[0024] The third modified structure is removed to form a weakened pore.
[0025] In some embodiments, after the first buffer layer is formed within the annular hole and before the second glass substrate is removed, the preparation method provided in this application further includes: A second buffer layer is prepared on the surface of the first glass substrate facing away from the second glass substrate; A second through-hole is prepared on the second buffer layer, and the second through-hole exposes at least the glass column.
[0026] Through the above technical solution, the preparation method provided in this application can prepare a second buffer layer on the surface of the first glass substrate away from the second glass substrate. This can reduce the stress when the first glass substrate is connected to other components. Furthermore, a second through hole is prepared on the second buffer layer so that the second through hole exposes at least the glass pillar. This allows the glass pillar to be disconnected from the second buffer layer, making it easier to remove the glass pillar.
[0027] Optionally, the second through-hole exposes at least a portion of the first buffer layer, which facilitates the fabrication of conductive connections within the first through-hole in subsequent processes.
[0028] In some embodiments, the first glass substrate and the second glass substrate are integrally connected, or the first glass substrate and the second glass substrate are bonded together.
[0029] Through the above technical solution, the first glass substrate and the second glass substrate are integrally connected, which facilitates the provision of the glass substrate. Furthermore, the first glass substrate and the second glass substrate are bonded together, which facilitates the removal of the second glass substrate.
[0030] Secondly, this application provides a substrate assembly, which is manufactured by the preparation method of any of the above embodiments. The substrate assembly provided by this application has the same or similar technical effects as the preparation methods of any of the above embodiments, and will not be described again here.
[0031] Thirdly, this application provides a packaging substrate, which includes a substrate, a conductive connection portion, a first circuit layer and a second circuit layer. The substrate includes at least one substrate assembly as described in the above embodiments. The conductive connection portion is disposed in a first through hole and includes a first connection end and a second connection end along the thickness direction of the glass substrate. The first circuit layer is disposed on one side of the substrate in the thickness direction and is connected to the first connection end of the conductive connection portion. The second circuit layer is disposed on the side of the substrate away from the first circuit layer and is connected to the second connection end of the conductive connection portion.
[0032] The packaging substrate provided in this application has the same or similar technical effects as the substrate assembly of the above embodiments, and will not be described again here.
[0033] Fourthly, this application provides a packaging structure, which includes a packaging substrate and a chip as described in the above embodiments, wherein the chip is packaged on the packaging substrate and is electrically connected to the packaging substrate.
[0034] The packaging structure provided in this application has the same or similar technical effects as the packaging substrate of the above embodiments, and will not be described again here.
[0035] Fifthly, this application provides an electronic device that includes the packaging structure and circuit board of the above embodiments, wherein the circuit board is electrically connected to the packaging structure.
[0036] The electronic device provided in this application has the same or similar technical effects as the packaging structure of the above-described embodiments, and will not be described again here.
[0037] The above description is only an overview of the technical solution of this application. In order to better understand the technical means of this application and to implement it in accordance with the contents of the specification, and to make the above and other objects, features and advantages of this application more obvious and understandable, the following are specific embodiments of this application. Attached Figure Description
[0038] To more clearly illustrate the technical solutions in the embodiments of this application, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0039] Figure 1 This is a schematic diagram of the structure of the electronic device provided in the embodiments of this application; Figure 2 This is one of the cross-sectional structural schematic diagrams of the packaging substrate provided in the embodiments of this application; Figure 3 This is a second cross-sectional view of the packaging substrate provided in the embodiments of this application; Figure 4 for Figure 2 One of the magnified views of a section at point A in the middle; Figure 5 for Figure 2 Second magnified view of a portion of point A in the middle; Figure 6 for Figure 2 One of the magnified views of a section at point B in the middle; Figure 7 for Figure 2 Second magnified view of a section at point B; Figure 8 This is one of the structural schematic diagrams of the packaging substrate provided in the embodiments of this application during the fabrication process; Figure 9 for Figure 8 One of the C-direction views; Figure 10 for Figure 8 The second view from direction C; Figure 11 for Figure 10 A magnified view of a portion of point D; Figure 12 This is the second schematic diagram of the structure of the packaging substrate provided in the embodiments of this application during the manufacturing process; Figure 13 for Figure 12 E-direction view; Figure 14 for Figure 13 One of the magnified views of a section at point F in the middle; Figure 15 for Figure 13 Second magnified view of a section at point F; Figure 16 for Figure 13 The third magnified view of the central F section; Figure 17 for Figure 13 Part 4 of the enlarged view at point F in the middle; Figure 18 for Figure 13 Fifth magnified view of a section at point F; Figure 19 This is the third schematic diagram of the structure of the packaging substrate provided in the embodiments of this application during the manufacturing process; Figure 20 This is the fourth schematic diagram of the structure of the packaging substrate provided in the embodiments of this application during the manufacturing process; Figure 21 Fifth schematic diagram of the structure of the packaging substrate provided in the embodiments of this application during the manufacturing process; Figure 22 This is the sixth schematic diagram of the structure of the packaging substrate provided in the embodiments of this application during the manufacturing process; Figure 23 This is the seventh schematic diagram of the structure of the packaging substrate provided in the embodiments of this application during the manufacturing process; Figure 24 This is the eighth schematic diagram of the structure of the packaging substrate provided in the embodiments of this application during the manufacturing process; Figure 25 This is the ninth schematic diagram of the structure of the packaging substrate provided in the embodiments of this application during the manufacturing process; Figure 26 This is the tenth schematic diagram of the structure of the packaging substrate provided in the embodiment of this application during the manufacturing process; Figure 27 This is eleventh of the structural schematic diagrams of the packaging substrate provided in the embodiments of this application during the manufacturing process.
[0040] The following are the labeling elements in the figure: Electronic device 1000; Packaging structure 1100; Packaging substrate 1101; Chip 1102; Circuit board 1200; Substrate assembly 100; First glass substrate 10; First surface 1001; Second surface 1002; Mounting hole 1003; Annular region 101; Sub-region 1011; Annular hole 102; First through hole 103; First modified structure 11; Substructure 111; Glass pillar 12; Third modified structure 121; Weakening hole 1211; Second glass substrate 10a; Second modified structure 10a1; Vent hole 10a11; First buffer layer 20; Second buffer layer 30; Second through hole 301; Conductive connection portion 200; first connection end 201; second connection end 202; first conductive connection sub-port 210; second conductive connection sub-port 220; Seed layer 300; First seed layer 310; Second seed layer 320; Third buffer layer 400; Third through hole 401; First circuit layer 500; first dielectric layer 510; first conductive line 520; first solder mask layer 530; first opening 531; first surface treatment layer 540; first conductive connection bump 550; Second circuit layer 600; second dielectric layer 610; second conductive line 620; second solder resist layer 630; second opening 631; second surface treatment layer 640; second conductive connection bump 650. Detailed Implementation
[0041] To make the technical problems, technical solutions, and beneficial effects to be solved by this application clearer, the following detailed description is provided in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and are not intended to limit the scope of this application.
[0042] It should be noted that when a component is referred to as being "fixed to" or "set on" another component, it can be directly on or indirectly on that other component. When a component is referred to as being "connected to" another component, it can be directly connected to or indirectly connected to that other component.
[0043] It should be understood that the terms "length", "width", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application.
[0044] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this application, "multiple" means two or more, unless otherwise explicitly specified.
[0045] This application provides an electronic device 1000, which can be, for example, a mobile phone, tablet computer, personal digital assistant (PDA), television, smart wearable products (e.g., smartwatches, smart bracelets), virtual reality (VR) terminal devices, augmented reality (AR) terminal devices, rechargeable small household appliances (e.g., soymilk makers, robot vacuum cleaners), drones, radar, aerospace equipment, in-vehicle equipment, vehicles, and other different types of user equipment or terminal devices; the electronic device 1000 can also be a network device such as a base station. This application does not impose any special limitations on the specific form of the electronic device 1000.
[0046] Please see Figure 1 The electronic device 1000 includes a circuit board 1200 and a package structure 1100, with the circuit board 1200 and the package structure 1100 being electrically connected.
[0047] For example, the package structure 1100 is disposed on the circuit board 1200.
[0048] For example, the circuit board 1200 may be a printed circuit board (PCB), a flexible printed circuit (FPC), or a rigid-flex circuit board 1200.
[0049] For example, electronic device 1000 may include an integrated circuit disposed on circuit board 1200.
[0050] For example, the package structure 1100 is integrated into the integrated circuit.
[0051] Please continue reading. Figure 1 The packaging structure 1100 includes a packaging substrate 1101 and a chip 1102. The chip 1102 is packaged on the packaging substrate 1101 and is electrically connected to the packaging substrate 1101. The packaging substrate 1101 provides support for the chip 1102. For example, the chip 1102 can be integrated into an integrated circuit.
[0052] For example, the chip 1102 provided in this application embodiment can be a logic chip 1102, which can implement functions such as "AND", "OR", and "NOT". Alternatively, the chip 1102 can be a memory chip 1102, which can realize data storage. This application embodiment does not limit the specific type of chip 1102. For example, the chip 1102 can also be a power integrated circuit (PIC) or other types of integrated circuits, or it can also be a circuit module, etc.
[0053] Exemplary, the packaging structure 1100 provided in this application embodiment may further include DC... Electrical components such as DC / DC converters, voltage regulator modules (VRMs), and integrated voltage regulators (IVRs) can be mounted on and electrically connected to the packaging substrate 1101.
[0054] For example, the chip 1102 provided in this application embodiment can be a surface acoustic wave device (SAW device). A surface acoustic wave device is a type of microelectronic component that utilizes the physical properties of surface acoustic waves (SAW) propagating on the surface of piezoelectric materials to achieve the conversion and processing of "electrical signal-acoustic signal-electrical signal". It is widely used in communication, sensing, radio frequency (RF) circuits and other fields.
[0055] Specifically, surface acoustic wave (SAW) devices include signal processing SAW devices (SAW filters, SAW resonators, SAW delay lines, etc.) and sensing SAW devices (temperature sensors, pressure sensors, gas sensors, etc.).
[0056] Taking filters as an example, filters are generally located at the front end of the RF module and belong to the signal processing chip 1102.
[0057] For example, the chip 1102 provided in this application embodiment can adapt to the high requirements of AI chip 1102 for computing power and bandwidth, thereby shortening the signal transmission path and reducing power consumption.
[0058] For example, the chip 1102 provided in this application embodiment can be integrated into a large-scale antenna array to meet the data rate requirements of over GHz in GHz scenarios.
[0059] With the rapid development of high-performance chips 1102 and their packaging technologies, first glass substrates 10, with their superior physical, chemical, and electrical properties, are gradually replacing organic substrates. During the packaging process, first glass substrates 10 can withstand higher temperatures better than organic substrates, and their coefficient of thermal expansion is similar to that of silicon, thus reducing stress warping problems caused by thermal mismatch. The electrical insulation and thermal stability of first glass substrates 10 provide mechanical support and electrical insulation for microelectromechanical systems (MHS), reducing parasitic capacitance and improving device performance, making them applicable to products such as miniature mass spectrometers and inertial sensors. Furthermore, the high flatness and low roughness of the glass surface allow for denser wiring, and the extremely low dielectric constant and dielectric loss of the glass material improve signal transmission speed and signal integrity. Simultaneously, the excellent chemical stability of the glass material effectively resists environmental corrosion such as moisture and acids / alkalis.
[0060] Through-Glass Vias (TGVs) are a core component of the 1102 chip substrate. After TGV vias are formed, conductive structures need to be filled inside. Stress mismatch between the conductive structure and the glass can cause glass cracking, necessitating the addition of a buffer layer between the conductive structure and the glass. The specific process involves filling the TGV via with a buffer layer, then drilling holes in the buffer layer, and finally filling with the conductive structure. However, it's difficult to keep the holes in the buffer layer concentric with the TGV vias, resulting in inconsistent buffer layer thickness around the TGV vias and poor buffering performance.
[0061] To address the aforementioned technical problems, embodiments of this application provide a substrate assembly 100 and its preparation method, a packaged substrate 1101, a packaged structure 1100, and an electronic device 1000, to improve the buffering effect of the buffer layer.
[0062] The purpose of this application is to provide a substrate assembly 100 and its preparation method, a packaged substrate 1101, a packaged structure 1100, and an electronic device 1000 to improve the buffering effect of the buffer layer.
[0063] Please refer to the following: Figure 2 and Figure 3 The packaging substrate 1101 provided in this application embodiment includes at least one substrate assembly 100. The substrate assembly 100 includes a first glass substrate 10. The first glass substrate 10 is provided with a mounting hole 1003, which penetrates the first glass substrate 10.
[0064] It is understandable that the number of substrate components 100 can be 1, 2, 3, etc.
[0065] For example, please refer to Figure 2 The packaging substrate 1101 provided in this application embodiment includes a substrate assembly 100.
[0066] For example, please refer to Figure 3 The packaging substrate 1101 provided in this application embodiment includes two substrate assemblies 100.
[0067] The packaging substrate 1101 provided in this embodiment further includes a conductive connection portion 200, which is disposed within the first through-hole 103. The conductive connection portion 200 includes a first connection end 201 and a second connection end 202 along the thickness direction Z of the laminated structure. The conductive connection portion 200 can be made of a conductive metal such as copper. In this way, the conductive connection portion 200 can be connected to other components through the first connection end 201 and the second connection end 202.
[0068] The packaging substrate 1101 provided in this embodiment further includes a first circuit layer 500. The first circuit layer 500 is disposed on one side of the substrate assembly 100 in the thickness direction Z, and the first circuit layer 500 is connected to the first connection end 201 of the conductive connection portion 200. In this way, the first circuit layer 500 can be connected to the conductive connection portion 200, so that the first circuit layer 500 can transmit electrical signals.
[0069] The packaging substrate 1101 provided in this embodiment further includes a second circuit layer 600. The second circuit layer 600 is disposed on the side of the substrate assembly 100 opposite to the first circuit layer 500, and the second circuit layer 600 is connected to the second connection terminal 202 of the conductive connection portion 200. In this way, the second circuit layer 600 can be connected to the conductive connection portion 200, so that the second circuit layer 600 can transmit electrical signals.
[0070] Please continue reading. Figure 2 and Figure 3 The substrate assembly 100 further includes a first buffer layer 20, which is disposed within the mounting hole 1003. The first buffer layer 20 has a first through hole 103 extending through it, and a conductive connection portion 200 is disposed within the first through hole 103. In this way, the first buffer layer 20 can absorb the stress between the first glass substrate 10 and the conductive connection portion 200, thus reducing the stress on the first glass substrate 10 and making it less prone to breakage, thereby reducing the manufacturing difficulty.
[0071] Optionally, the material of the first buffer layer 20 includes organic materials. In this way, the first buffer layer 20 has a good buffering effect.
[0072] Optionally, the material of the first buffer layer 20 includes Ajinomoto Build-up Film (ABF).
[0073] Please see Figure 2 , Figure 4 and Figure 5 Optionally, the substrate assembly 100 provided in this application embodiment further includes a second buffer layer 30. The first glass substrate 10 includes a first surface 1001 and a second surface 1002 that are opposite each other along the thickness direction Z. The second buffer layer 30 is disposed on the second surface 1002. The second buffer layer 30 is provided with a second through hole 301 that communicates with the first through hole 103. The second circuit layer 600 is disposed on the side of the second buffer layer 30 that is away from the first circuit layer 500. The second connection end 202 of the conductive connection portion 200 passes through the second through hole 301 and is connected to the second circuit layer 600.
[0074] Please see Figure 4 Optionally, the second buffer layer 30 covers the first buffer layer 20.
[0075] Please see Figure 5 Optionally, the second through-hole 301 exposes the first buffer layer 20.
[0076] Optionally, the material of the second buffer layer 30 includes organic materials. In this way, the second buffer layer 30 has a good buffering effect.
[0077] Optionally, the material of the second buffer layer 30 includes Ajinomoto Build-up Film (ABF).
[0078] Please see Figure 2 , Figure 6 and Figure 7 Optionally, the packaging substrate 1101 provided in this application embodiment further includes a third buffer layer 400. The third buffer layer 400 is disposed on the first surface 1001. The third buffer layer 400 is provided with a third through hole 401 communicating with the first through hole 103. The first circuit layer 500 is disposed on the side of the third buffer layer 400 away from the first circuit layer 500. The first connection end 201 of the conductive connection portion 200 passes through the third through hole 401 and is connected to the first circuit layer 500.
[0079] Please see Figure 6 Optionally, the third buffer layer 400 covers the first buffer layer 20.
[0080] Please see Figure 7 Optionally, the third through-hole 401 exposes the first buffer layer 20.
[0081] Optionally, the material of the third buffer layer 400 may include organic materials. In this way, the third buffer layer 400 has a good buffering effect.
[0082] Optionally, the material of the third buffer layer 400 includes Ajinomoto Build-up Film (ABF).
[0083] Please continue reading. Figure 2 and Figure 3 The packaging substrate 1101 provided in this application embodiment also includes a seed layer 300, which is disposed on the outer periphery of the conductive connection portion 200, thus facilitating the fabrication of the conductive connection portion 200.
[0084] Optionally, please refer to Figure 3 The conductive connection portion 200 includes a first conductive connection sub-portion 210 and a second conductive connection sub-portion 220. The seed layer 300 includes a first seed layer 310 and a second seed layer 320. The first seed layer 310 is provided on the outer periphery of the first conductive connection sub-portion 210, which facilitates the processing of the first conductive connection sub-portion 210. The second seed layer 320 is provided on the outer periphery of the second conductive connection sub-portion 220, which facilitates the processing of the second conductive connection sub-portion 220.
[0085] Please continue reading. Figure 2 , Figure 6 and Figure 7 Optionally, the first circuit layer 500 includes a first dielectric layer 510 and a first conductive line 520 alternately stacked in sequence. The first conductive line 520 can be connected to the conductive connection portion 200. The first dielectric layer 510 is located between two adjacent first conductive lines 520 and can separate two adjacent first conductive lines 520. The material of the first conductive line 520 can be copper, aluminum, nickel, gold, etc.
[0086] Optionally, the first circuit layer 500 further includes a first solder mask layer 530 covering the outermost first conductive line 520. The first solder mask layer 530 may have a first opening 531, exposing the outermost first conductive line 520. The first opening 531 is filled with a first surface treatment layer 540, and the surface of the first surface treatment layer 540 is provided with first conductive connection bumps 550, which facilitates the connection of the first circuit layer 500 to other components through the first conductive connection bumps 550.
[0087] Please continue reading. Figure 2 , Figure 4 and Figure 5 Optionally, the second circuit layer 600 includes a second dielectric layer 610 and a second conductive line 620 alternately stacked in sequence. The second conductive line 620 can be connected to the conductive connection portion 200. The second dielectric layer 610 is located between two adjacent second conductive lines 620 and can separate two adjacent second conductive lines 620. The material of the second conductive line 620 can be copper, aluminum, nickel, gold, etc.
[0088] Optionally, the second circuit layer 600 further includes a second solder mask layer 630 covering the outermost second conductive line 620. The second solder mask layer 630 may have a second opening 631, which exposes the outermost second conductive line 620. The second opening 631 is filled with a second surface treatment layer 640, and the surface of the second surface treatment layer 640 is provided with second conductive connection bumps 650, which facilitates the connection of the second circuit layer 600 to other components through the second conductive connection bumps 650.
[0089] It is understandable that the materials for the first conductive line 520 and the second conductive line 620 can be selected according to specific product requirements.
[0090] The following is based on Figures 8 to 27 The preparation method of the substrate assembly 100 provided in the embodiments of this application will be described.
[0091] The method for fabricating the substrate assembly 100 provided in this application includes: S100, please refer to Figure 8 A glass substrate is provided, the glass substrate including a first glass substrate 10 and a second glass substrate 10a stacked thereon; S200, please refer to Figure 12 The first glass substrate 10 has an annular hole 102 that penetrates the first glass substrate 10. The first glass substrate 10 forms a glass pillar 12 located on the inner periphery of the annular hole 102. The second glass substrate 10a covers the glass pillar 12. S400, a first buffer layer 20 is prepared within the annular hole 102; S800, remove the second glass substrate 10a; S900, remove the glass column 12 to form the first through hole 103.
[0092] Through the above technical solution, the preparation method provided in this application embodiment can form an annular hole 102 on the first glass substrate 10, and then prepare an annular first buffer layer 20 in the annular hole 102. During this process, the second glass substrate 10a supports the glass pillar 12 to prevent the glass pillar 12 from being misaligned or falling off. After the first buffer layer 20 is prepared, the second glass substrate 10a can be removed first, and then the glass pillar 12 can be removed. After removing the second glass substrate 10a, it is convenient to remove the glass pillar 12. After removing the glass pillar 12, the position of the glass pillar 12 naturally forms the first through hole 103. This eliminates the need for secondary drilling and helps to improve the uniformity of the thickness of the first buffer layer 20 in the circumferential direction of the first through hole 103, thereby improving the buffering effect of the first buffer layer 20.
[0093] The annular hole 102 can be prepared by processes such as etching.
[0094] In some embodiments, the first glass substrate 10 and the second glass substrate 10a are integrally connected, which facilitates the provision of the glass substrate. The second glass substrate 10a can be removed by methods such as grinding or wet etching.
[0095] In other embodiments, the first glass substrate 10 and the second glass substrate 10a are bonded together, which facilitates the removal of the second glass substrate 10a. The second glass substrate 10a can be removed by unbonding the first glass substrate 10 and the second glass substrate 10a.
[0096] Please see Figure 8 , Figure 9 , Figure 10 and Figure 11 In some embodiments, the surface of the first glass substrate 10 facing away from the second glass substrate 10a (second surface 1002) includes an annular region 101. In step S200, the annular hole 102 is formed in the first glass substrate 10, including: S210, the first glass substrate 10 is modified in the annular region 101 to form an annular first modified structure 11; S230, the first modified structure 11 is removed to form an annular hole 102.
[0097] Through the above technical solution, the preparation method provided in this application embodiment can form a weakened first modified structure 11, which is convenient to remove the first modified structure 11, thereby facilitating the formation of annular holes 102.
[0098] Optionally, modifying the first glass substrate 10 in the annular region 101 includes: irradiating the first glass substrate 10 in the annular region 101 with a laser, thereby forming a weakened first modified structure 11. That is, the preparation method provided in the embodiments of this application can use laser irradiation to weaken the first glass substrate 10 in the annular region 101 to form the first modified structure 11.
[0099] Optionally, removing the first modified structure 11 to form the annular hole 102 includes etching the first glass substrate 10, for example, by using wet etching to remove the first modified structure 11. That is, the preparation method provided in this application embodiment can use an etching process to remove the first modified structure 11.
[0100] Optionally, the annular region 101 includes multiple sub-regions 1011. After the annular region 101 modifies the first glass substrate 10, and before removing the first modified structure 11 to form the annular hole 102, that is, after step S210 and before step S230, step S200 prepares the annular hole 102 in the first glass substrate 10, including: S220, the first glass substrate 10 is modified again in sub-region 1011.
[0101] Through the above technical solution, after the formation of the first modified structure 11 and before its removal, the preparation method provided in this application embodiment can further modify and weaken the first modified structure 11 in the sub-region 1011 of the annular region 101, making it easier to remove the first modified structure 11.
[0102] Optionally, the sub-region 1011 is a circular region, and multiple sub-regions 1011 are arranged at circumferential intervals along the annular region 101, which facilitates the weakening of the first modified structure 11.
[0103] It is understandable that the first modified structure 11 in subregion 1011 is a substructure 111 that has been modified and weakened twice. This can further weaken the first modified structure 11 and make it easier to remove the first modified structure 11.
[0104] Please see Figure 12 , Figure 13 , Figure 14 , Figure 15 , Figure 16 , Figure 17 and Figure 18 In some embodiments, after providing the glass substrate and before preparing the first buffer layer 20 within the annular hole 102, i.e., after step S100 and before step S400, the preparation method provided in this application embodiment further includes: S300, a vent hole 10a11 is prepared in the second glass substrate 10a. The vent hole 10a11 penetrates the second glass substrate 10a and is connected to the annular hole 102.
[0105] Step S300 can be performed before or after step S200.
[0106] Through the above technical solution, the preparation method provided in this application provides a vent hole 10a11 on the second glass substrate 10a and makes the vent hole 10a11 communicate with the annular hole 102. In this way, when the first buffer layer 20 is prepared in the annular hole 102, the air in the annular hole 102 can be discharged from the vent hole 10a11, which helps to reduce the air pressure in the annular hole 102, thereby facilitating the entry of the material for preparing the first buffer layer 20 into the annular hole 102, and thus making it easier to prepare the first buffer layer 20.
[0107] Optionally, please refer to Figure 8 and Figure 12 The surface of the second glass substrate 10a facing away from the first glass substrate 10 includes a breathable area. Step S300 involves preparing breathable holes 10a11 on the second glass substrate 10a, including: The second glass substrate 10a is modified in the ventilated area to form a second modified structure 10a1; The second modified structure 10a1 is removed to form a vent 10a11.
[0108] Through the above technical solution, the preparation method provided in this application can form a weakened second modified structure 10a1, which is easy to remove, thereby facilitating the formation of pores 10a11.
[0109] Please see Figure 13 , Figure 14 , Figure 15 , Figure 16 , Figure 17 and Figure 18 Optionally, there are multiple vent holes 10a11, which are spaced apart circumferentially along the annular hole 102. This facilitates the timely discharge of gas from the annular hole 102 through the multiple vent holes 10a11, thereby promoting the uniform entry of the material for preparing the first buffer layer 20 into the annular hole 102 and improving the uniformity of the first buffer layer 20.
[0110] The number of vents connected by a single annular hole can be 1, 2, 3, 4, 5, 6, etc.
[0111] Optionally, the orthographic projection of the vent 10a11 on the surface of the first glass substrate 10 opposite to the second glass substrate 10a (second surface 102) does not overlap with the orthographic projection of the glass pillar 12 on the surface of the first glass substrate 10 opposite to the second glass substrate 10a (second surface 102). This helps to increase the connection area between the glass pillar 12 and the second glass substrate 10a, thereby increasing the firmness of the connection between the glass pillar 12 and the second glass substrate 10a, and thus facilitating the removal of the glass pillar 12 when the second glass substrate 10a is removed.
[0112] Optionally, the orthographic projection of the vent hole 10a11 on the surface of the first glass substrate 10 opposite to the second glass substrate 10a (second surface 102) is located within the orthographic projection of the annular hole 102 on the surface of the first glass substrate 10 opposite to the second glass substrate 10a (second surface 102), which facilitates the timely discharge of gas from the annular hole 102.
[0113] Please see Figure 19 , Figure 20 and Figure 21 After the first buffer layer 20 is prepared in the annular hole 102 and before the glass column 12 is removed, that is, after step S400 and before step S900, the preparation method provided in this application further includes: S500, a weakening hole 1211 is prepared on the glass column 12, and the weakening hole 1211 penetrates the glass column 12. In this way, the glass column 12 can be weakened through the weakening hole 1211, making it easier to remove the glass column 12.
[0114] Optionally, the surface of the glass pillar 12 facing away from the first glass substrate 10 includes at least one weakened region. Step S500 involves forming a weakened hole 1211 on the glass pillar 12, including: S510, the glass column 12 is modified in the weakened region to form a third modified structure 121.
[0115] S520, the third modified structure 121 is removed to form a weakened pore 1211.
[0116] The weakening hole 1211 can be a round hole, an arc-shaped hole, etc.
[0117] Please see Figure 22 and Figure 23 In some embodiments, after the first buffer layer 20 is prepared in the annular hole 102 and before the second glass substrate 10a and glass pillar 12 are removed, that is, after step S400 and before step S800, the preparation method provided in this application embodiment further includes: S600, a second buffer layer 30 is prepared on the surface of the first glass substrate 10 facing away from the second glass substrate 10a (second surface 102); S700, a second through hole 301 is prepared on the second buffer layer 30, the second through hole 301 exposing at least the glass column 12.
[0118] Through the above technical solution, the preparation method provided in this application embodiment can prepare a second buffer layer 30 on the second surface 1002, which can reduce the stress when the first glass substrate 10 is connected to other components, and prepare a second through hole 301 on the second buffer layer 30, so that the second through hole 301 exposes at least the glass pillar 12, so that the glass pillar 12 is not connected to the second buffer layer 30, which facilitates the removal of the glass pillar 12.
[0119] Optionally, the second through-hole 301 exposes at least a portion of the first buffer layer 20, which facilitates the fabrication of the conductive connection portion 200 within the first through-hole 103 in subsequent processes.
[0120] Please see Figure 23 and Figure 24 In step S800, the second glass substrate 10a is removed by laser peeling. The second glass substrate 10a is connected to the glass pillar 12. When the second glass substrate 10a is removed, the glass pillar 12 can be taken out, thereby forming the first through hole 103.
[0121] Please see Figure 25The preparation method provided in this application embodiment further includes: In step S1000, a third buffer layer 400 is prepared on the surface of the first glass substrate 10 that is opposite to the second surface 1002 (first surface 1001), and a third through hole 401 is prepared, so that the substrate assembly 100 can play a buffering role when connected with other components.
[0122] Please see Figure 26 and Figure 27 The preparation method provided in this application embodiment further includes: Step S1100: A seed layer 300 is prepared in the first through hole 103. The seed layer 300 has a ring structure. In step S1200, a conductive connection portion 200 is prepared in the first through hole 103. The conductive connection portion 200 is located on the inner peripheral side of the seed layer 300.
[0123] In this way, the preparation method provided in this application first prepares the seed layer 300 and then prepares the conductive connection part 200, which facilitates the preparation of the conductive connection part 200.
[0124] The substrate assembly 100 provided in this application embodiment is manufactured by the preparation method of any of the above embodiments. The substrate assembly 100 has the same or similar technical effects as the preparation method of any of the above embodiments, which will not be repeated here.
[0125] The packaging substrate 1101 provided in this application embodiment includes a substrate, a conductive connection portion 200, a first circuit layer 500, and a second circuit layer 600. The substrate includes at least one substrate assembly 100 as described in the above embodiment. The conductive connection portion 200 is disposed in a first through hole 103, and the conductive connection portion 200 includes a first connection end 201 and a second connection end 202 along the thickness direction of the first glass substrate 10. The first circuit layer 500 is disposed on one side of the substrate in the thickness direction and is connected to the first connection end 201 of the conductive connection portion 200. The second circuit layer 600 is disposed on the side of the substrate away from the first circuit layer 500 and is connected to the second connection end 202 of the conductive connection portion 200.
[0126] The packaging substrate 1101 provided in this application embodiment has the same or similar technical effects as the substrate assembly 100 in the above embodiment, and will not be described again here.
[0127] The packaging structure 1100 provided in this application includes the packaging substrate 1101 and chip 1102 of the above embodiments. The chip 1102 is packaged on the packaging substrate 1101 and is electrically connected to the packaging substrate 1101.
[0128] The packaging structure 1100 provided in this application embodiment has the same or similar technical effects as the packaging substrate 1101 in the above embodiment, and will not be described again here.
[0129] The electronic device 1000 provided in this application includes the packaging structure 1100 and circuit board 1200 of the above embodiments, and the circuit board 1200 is electrically connected to the packaging structure 1100.
[0130] The electronic device 1000 provided in this application embodiment has the same or similar technical effects as the packaging structure 1100 in the above embodiment, and will not be described again here.
[0131] The above are merely specific embodiments of this application and are not intended to limit this application. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this application should be included within the protection scope of this application.
Claims
1. A method for preparing a substrate assembly, characterized in that, include: A glass substrate is provided, the glass substrate comprising a first glass substrate and a second glass substrate stacked together; An annular hole is formed in the first glass substrate, the annular hole penetrates the first glass substrate, a glass pillar is formed in the first glass substrate located on the inner periphery of the annular hole, and the second glass substrate covers the glass pillar; A first buffer layer is prepared within the annular hole; Remove the second glass substrate; Remove the glass column to form a first through hole.
2. The preparation method according to claim 1, characterized in that, After providing the glass substrate and before preparing the first buffer layer within the annular hole, the preparation method further includes: A vent hole is formed in the second glass substrate, and the vent hole is connected to the annular hole; Preferably, the surface of the second glass substrate facing away from the first glass substrate includes a breathable region, and the breathable holes are formed in the second glass substrate, including: The second glass substrate is modified in the ventilated area to form a second modified structure; The second modified structure is removed to form the air pores; Preferably, there are multiple vent holes, and the multiple vent holes are arranged at intervals along the circumference of the annular hole; Preferably, the orthographic projection of the vent hole on the surface of the first glass substrate opposite to the second glass substrate does not overlap with the orthographic projection of the glass column on the surface of the first glass substrate opposite to the second glass substrate. Preferably, the orthographic projection of the vent hole on the surface of the first glass substrate facing away from the second glass substrate is located within the orthographic projection of the annular hole on the surface of the first glass substrate facing away from the second glass substrate.
3. The preparation method according to claim 1, characterized in that, The surface of the first glass substrate facing away from the second glass substrate includes an annular region, and the process of forming an annular hole in the first glass substrate includes: The first glass substrate is modified in the annular region to form an annular first modified structure; The first modified structure is removed to form the annular hole; Preferably, modifying the first glass substrate in the annular region includes: irradiating the first glass substrate with a laser in the annular region; Preferably, removing the first modified structure to form an annular hole includes: etching the first glass substrate; Preferably, the annular region comprises multiple sub-regions, and after modifying the glass substrate in the annular region, before removing the first modified structure to form the annular hole, the preparation method includes: The glass substrate is further modified in the sub-region; Preferably, the sub-region is a circular region, and multiple sub-regions are arranged at circumferential intervals along the annular region.
4. The preparation method according to claim 1, characterized in that, After preparing the first buffer layer within the annular hole and before removing the glass column, the preparation method further includes: A weakening hole is prepared on the glass column, and the weakening hole penetrates the glass column; Preferably, the surface of the glass pillar facing away from the first glass substrate includes at least one weakened region, and the process of forming a weakening hole on the glass pillar includes: The glass column is modified in the weakened region to form a third modified structure; The weakened pore is formed by removing the third modified structure.
5. The preparation method according to claim 1, characterized in that, After the first buffer layer is formed within the annular hole and before the second glass substrate is removed, the preparation method further includes: A second buffer layer is prepared on the surface of the first glass substrate facing away from the second glass substrate; A second through-hole is formed on the second buffer layer, the second through-hole exposing at least the glass column; Preferably, the second through-hole exposes at least a portion of the first buffer layer.
6. The preparation method according to claim 1, characterized in that, The first glass substrate and the second glass substrate are integrally connected, or the first glass substrate and the second glass substrate are bonded together.
7. A substrate assembly, characterized in that, It is prepared by the preparation method according to any one of claims 1 to 6.
8. A packaging substrate, characterized in that, include: A substrate, comprising at least one substrate assembly as described in claim 7; A conductive connection portion is disposed within the first through hole, including a first connection end and a second connection end along the thickness direction of the glass substrate; A first circuit layer is disposed on one side of the substrate in the thickness direction and is connected to the first connection end of the conductive connection portion; The second circuit layer is disposed on the side of the substrate opposite to the first circuit layer and is connected to the second connection end of the conductive connection portion.
9. A packaging structure, characterized in that, include: The packaging substrate as described in claim 8; The chip is packaged on the packaging substrate and is electrically connected to the packaging substrate.
10. An electronic device, characterized in that, include: The packaging structure as described in claim 9; The circuit board is electrically connected to the package structure.