Methods of using composition

A film-forming composition with specific enhancer and pH levels addresses damage and irritation issues in headdress fibers by forming a surface film, improving dyeability and durability.

JP2024172436AInactive Publication Date: 2024-12-12KAO CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023090154
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-31
Publication Date
2024-12-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing hair treatment compositions for fibers used in headdress products, such as regenerated collagen fibers, cause damage due to repeated washing and may lead to skin coloring and scalp irritation, while conventional hair dyes enhance penetration but are not suitable for these fibers.

Method used

A composition containing a film-forming agent and a penetration enhancer with a content of 24% by mass or less and a pH of 10 or less, providing a tensile modulus of 0.4 GPa or more, is used for treating fibers, forming a film on the surface rather than penetrating into the fibers, thereby improving dyeability and reducing damage.

Benefits of technology

The method enhances dyeability of fibers, prevents damage from repeated washing, and reduces the risk of skin coloring and scalp irritation, achieving an ideal finish.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024172436000001
    Figure 2024172436000001
  • Figure 2024172436000002
    Figure 2024172436000002
  • Figure 2024172436000003
    Figure 2024172436000003
Patent Text Reader

Abstract

To provide a method for using a composition for treating fibers for head accessories, which, when used in the dyeing process of fibers for head accessories that meet certain requirements, provides good dyeability to the fibers, suppresses damage to the fibers caused by repeated washing after the dyeing process, and further, achieves an ideal finish while reducing the risk of skin coloring and scalp irritation.SOLUTION: Provided is a method for using a composition which contains a film-forming agent (A), has a penetration enhancer (B) content of 24 mass% or less, and has a pH of 10 or less, and is used in treating fibers for head accessories having a tensile modulus in water of 0.4 GPa or more.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to methods of using the compositions. [Background technology]

[0002] Head accessories such as wigs and hair extensions are made from fibers extracted from natural plants and animals, such as human hair and animal hair, as well as synthetic fibers and artificially produced regenerated collagen fibers.

[0003] Incidentally, many hair cosmetics, including hair dyes, contain a penetration enhancer for the purpose of promoting the penetration of ingredients acting on hair (see, for example, Patent Document 1). However, there is a concern that the fibers may be damaged if the hair treatment composition described in Patent Document 1 or the like is used to treat fibers for head ornament products other than human hair, such as regenerated collagen fibers, and then washed repeatedly. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2002-97122 A Summary of the Invention [Problem to be solved by the invention]

[0005] The present invention relates to a method for using a composition for treating fibers for head accessories, which, when used in the dyeing treatment of fibers for head accessories that meet certain requirements, provides good dyeability to the fibers, suppresses damage to the fibers caused by repeated washing after the dyeing treatment, and further relates to a method that can achieve both an ideal finish and a reduced risk of skin coloration and scalp irritation. [Means for solving the problem]

[0006] The inventor has discovered that the above problem can be solved by using a composition which contains a film-forming agent and has a penetration enhancer content and pH below specified values ​​to treat a specified fiber for head ornament products. That is, the present invention relates to the following. [1] A method for using a composition, comprising: using the composition, which contains a film-forming agent (A), has a penetration enhancer (B) content of 24 mass% or less, and has a pH of 10 or less, for treating fibers for head accessories having a tensile modulus in water of 0.4 GPa or more. [2] A method for dyeing fibers for head accessories, comprising a step of applying a composition containing a film-forming agent (A), a penetration enhancer (B) content of 24 mass% or less, and a pH of 10 or less to fibers for head accessories having a tensile modulus in water of 0.4 GPa or more. Effect of the Invention

[0007] According to the present invention, there is provided a method for using a composition for treating fibers for head ornament products, which, when used in the dyeing treatment of fibers for head ornament products that meet certain requirements, provides good dyeability for the fibers and suppresses damage to the fibers due to repeated washing after the dyeing treatment, and further provides a method which makes it possible to achieve both an ideal finish and a reduced risk of skin coloration and scalp irritation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] [Definition] "Polymer," as used herein, means a compound corresponding to the repeating of one or more units (which units are derived from compounds known as monomers) that are repeated at least twice, and preferably at least three times. "Headwearing products" as used herein means, for example, hair wigs, hairpieces, weaving, hair extensions, braided hair, hair accessories, doll hair, and the like. "Headwear fiber" as used herein means a fiber used in the headwear, excluding human hair. "Hydrophobic", as used herein, means that a substance has a solubility in water of less than 1% by weight at 25°C. "Film-forming," as used herein, means leaving a solid film on the substrate to which it is applied. "Volatile" as used herein means having a boiling point of 260° C. or less at normal pressure.

[0009] In this specification, "good dyeability of the fiber" means that the color change of the fiber for head accessories after treatment with a composition containing a dyeing component is large, and "suppression of damage to the fiber due to repeated washing" means that the fiber for head accessories after treatment with the composition can be combed easily after washing two or more times. The dyeability of the fiber and the suppression of fiber damage due to repeated washing can be specifically evaluated by the method described in the Examples.

[0010] [Method of using the composition] The method for using the composition of the present invention is a method for using a composition which contains a film-forming agent (A), has a content of a penetration enhancer (B) of 24 mass% or less, and has a pH of 10 or less, for treating fibers for head accessories having a tensile modulus in water of 0.4 GPa or more. In the following description, the method for using the composition of the present invention may be simply referred to as the "method of the present invention." The method of the present invention, when a specified composition is used in the dyeing process of fibers for head accessories that satisfy specified requirements, is a method that provides good dyeability to the fibers, suppresses damage to the fibers due to repeated washing after the dyeing process, and further makes it possible to achieve both an ideal finish and a reduced risk of skin coloration and scalp irritation.

[0011] The reason why the method of the present invention exhibits the above-mentioned effects is not clear, but is presumed to be as follows. Conventional hair cosmetics, which are mainly applied to human hair, contain a penetration enhancer to enhance the penetration of functional ingredients into the inside of the hair. For example, in hair dyes, the dyeing properties are improved by penetrating the dyeing ingredients into the inside of the hair. In addition, in hair dyes, an alkali agent is usually blended from the viewpoint of improving the dyeing properties. On the other hand, fibers for head accessories such as regenerated collagen fibers have different properties from human hair, and applying hair cosmetics containing a large amount of penetration enhancers can cause damage such as a decrease in feel. In addition, when it comes to hair dyes, it is unclear what effect a highly alkaline hair cosmetic with a pH of over 10 has on fibers for head accessories and on their dyeability. The composition used in the present invention is different from the hair dye which uses a penetration enhancer to penetrate the dyeing component into the fiber to enhance the dyeability, and contains a film-forming agent and a dyeing component, and is capable of dyeing the fiber by forming a film containing the dyeing component on the fiber surface. Therefore, in the composition, the content of the penetration enhancer can be reduced, and further, even if the pH value is below a predetermined value, the dyeability of the fiber can be enhanced, and it is considered that the fiber damage caused by repeated washing after the dyeing process can also be suppressed. Furthermore, the fibers for head accessories to be treated in the method of the present invention have a tensile modulus in water of a predetermined value or more, which is believed to increase the resistance of the fibers to treatment with the composition, thereby reducing damage to the fibers caused by repeated washing after dyeing. The mechanism of action of the present invention is not limited to the above.

[0012] The composition of the present invention contains a film-forming agent (A), has a content of a penetration enhancer (B) of 24 mass % or less, and has a pH of 10 or less. Each component contained in the composition will be described below.

[0013] <Film-forming agent (A)> The film-forming agent (A) (hereinafter also referred to as "component (A)") may be one or more selected from the group consisting of silicone-based polymers, anionic vinyl polymers, cationic vinyl polymers, amphoteric vinyl polymers, nonionic vinyl polymers, urethane-based polymers, highly polymerized polyethylene glycols, and polysaccharide-based polymers.

[0014] [Silicone-based polymer] Silicone-based polymers include film-forming polymers having a silicone backbone. Examples of such polymers include siloxysilicic acids such as trimethylsiloxysilicate, phenylpropyldimethylsiloxysilicate, fluorine-modified alkyldimethylsiloxysilicate, and crosspolymers of these siloxysilicates crosslinked with dimethiconol or the like; polysilsesquioxanes such as polymethylsilsesquioxane, polypropylsilsesquioxane, polyphenylsilsesquioxane, polymethylphenylsilsesquioxane, and fluorine-modified alkyldimethylpolysilsesquioxane; poly(N-acylalkyleneimine)-modified organopolysiloxanes such as poly(N-formylethyleneimine)organopolysiloxane, poly(N-acetylethyleneimine)organopolysiloxane, and poly(N-propionylethyleneimine)organopolysiloxane (INCI name: Polysilicone-9); organopolysiloxane graft polymers described in International Publication No. 2014 / 002707, such as Polysilicone-28; Silsoft Spread TT (manufactured by Momentive Performance Materials); polysilicone-6; acrylates / dimethicone copolymers such as KP-545 and KP-549 (both manufactured by Shin-Etsu Chemical Co., Ltd.); and acrylates / polytrimethylsiloxy methacrylate copolymers such as DOWSIL FA 4001 CM Silicone Acrylate, DOWSIL FA 4002 ID Silicone Acrylate, DOWSIL FA 4003 DM Silicone Acrylate, and DOWSIL FA 4004 ID Silicone Acrylate (all manufactured by Dow-Toray Co., Ltd.).

[0015] [Anionic vinyl polymer] The anionic vinyl polymer is an anionic vinyl polymer that does not have a silicone skeleton, and examples thereof include the following. <Anionic vinyl polymer containing a structural unit derived from any one of crotonic acid, maleic acid, maleic acid monoester, and itaconic acid> There are no particular limitations on the copolymer as long as it contains a structural unit derived from any one of crotonic acid, maleic acid, maleic acid monoester, and itaconic acid. Examples of copolymers with one or more of vinyl ethers, vinyl esters, and vinyl alcohols include methyl vinyl ether / alkyl maleate copolymers (GANTREZ ES-225, ES-425, and SP-215 (all manufactured by ISP)), vinyl acetate / crotonic acid copolymers (Resin 28-1310 (manufactured by Nouryon), etc.), vinyl acetate / crotonic acid / vinyl neodecanoate copolymers (Resin 28-2930 (manufactured by Nouryon), etc.), vinyl acetate / crotonic acid / vinyl propionate copolymers (Rubyset CAP (manufactured by BASF), etc.), and vinyl alcohol / itaconic acid copolymers (KM-118 (manufactured by Kuraray Co., Ltd.), etc.).

[0016] <Anionic vinyl polymer containing a structural unit derived from (meth)acrylic acid> There is no particular limitation as long as the vinyl polymer contains a structural unit derived from (meth)acrylic acid. Examples of copolymers with one or more of (meth)acrylic acid alkyl esters or N-alkyl (meth)acrylamides include acrylic acid / ethyl acrylate / Nt-butylacrylamide copolymers (Ultrahold 8, Ultrahold Strong (both manufactured by BASF), etc.), octyl acrylamide / acrylic acid copolymers (Amphomer HC (manufactured by Nouryon), etc.), acrylate / methacrylate / acrylic acid / meth Examples of such copolymers include acrylic acid copolymers (Amafold DR25 (manufactured by Union Carbide Corporation)), acrylates / diacetone acrylamide copolymers (Pluscise L-9540B (the copolymer neutralized with 2-amino-2-methyl-1-propyl alcohol) (manufactured by GOO Chemical Industry Co., Ltd.)), and acrylates / C1-18 alkyl acrylates / C1-8 alkyl acrylamide copolymers (Pluscise L-9909B (the copolymer neutralized with 2-amino-2-methyl-1-propyl alcohol) (manufactured by GOO Chemical Industry Co., Ltd.)). In this specification, "(meth)acrylic" includes both acrylic and methacrylic.

[0017] [Cationic vinyl polymer] Examples of the cationic vinyl polymer include cationic vinyl polymers that do not have a silicone skeleton, such as vinylpyrrolidone / dimethylaminoethyl methacrylate copolymer diethyl sulfate (HC Polymer 1S (M), HC Polymer 2 (both manufactured by Osaka Organic Chemical Industry Co., Ltd.), Gafcoat 755N (manufactured by ISP Co., Ltd.)), vinylpyrrolidone / dimethylaminopropyl methacrylamide / lauryldimethylaminopropyl methacrylamide copolymer (Stylese W-20 (manufactured by ISP Co., Ltd.)), vinylpyrrolidone / N,N-dimethylaminoethyl methacrylate / alkyl acrylate / tripropylene glycol diacrylate copolymer (Coscut GA467, Coscut GA468 (both manufactured by Osaka Organic Chemical Industry Co., Ltd.)). Examples of such copolymers include polydimethylmethylene piperidinium chloride (Mercury 100 (manufactured by Lubrizol Corporation)), dimethyldiallylammonium chloride / acrylamide copolymer (Mercury 550 (manufactured by Lubrizol Corporation)), trimethylammoniopropylacrylamide chloride / dimethylacrylamide copolymer, alkylacrylamide / acrylate / alkylaminoalkylacrylamide / polyethylene glycol methacrylate copolymer (see JP-A-2-180911), and t-butylacrylamide / dimethylacrylamide / dimethylaminopropylacrylamide / methoxypolyethylene glycol (PEG400) methacrylate copolymer (see JP-A-8-291206).

[0018] [Amphophilic vinyl polymer] Examples of the amphoteric vinyl polymer include amphoteric vinyl polymers that do not have a silicone skeleton, such as octylamide acrylate / hydroxypropyl acrylate / butylaminoethyl methacrylate copolymers (AMPHOMER SH30, AMPHOMER LV-71, AMPHOMER 28-4910 (all manufactured by Nouryon)), methacryloyloxyethyl carboxybetaine / alkyl methacrylate copolymer (Yukaformer R205, Yukaformer 301, Yukaformer SM, Yukaformer M-75, Yukaformer 104D (all manufactured by Mitsubishi Chemical Corporation), RAM Resin-1000, RAM Resin-2000, RAM Resin-3000, RAM Resin-4000 (all manufactured by Osaka Organic Chemical Industry Co., Ltd.)), dimethyldiallylammonium chloride / acrylic acid copolymer (Marcoat 280, Marcoat 295 (all manufactured by Lubrizol)), dimethyldiallylammonium chloride / acrylamide / acrylic acid copolymer (Marcoat Plus 3330, Marcoat Plus 3331 (all manufactured by Lubrizol)).

[0019] [Nonionic vinyl polymer] Examples of the nonionic vinyl polymer include polyvinyl alcohol, polyvinylpyrrolidone (Ruviscol K17, Ruviscol K30, Ruviscol K90 (all manufactured by BASF), PVP K (manufactured by ISP)), vinylpyrrolidone / vinyl acetate copolymer (PVP / VA S-630, PVP / VA E-735, PVP / VA E-335 (all manufactured by ISP), Ruviscol VA73W, Ruviscol 37E (all manufactured by BASF), PVA-6450 (manufactured by Osaka Organic Chemical Industry Co., Ltd.)), vinylpyrrolidone / methacrylamide / vinylimidazole copolymer (Ruvisset Clear (manufactured by BASF)), polyvinyl caprolactam (Ruviscol Plus (manufactured by BASF)), and the like.

[0020] [Urethane-based polymer] Examples of urethane-based polymers include Yodozole PUD (manufactured by Nouryon), Rubyset PUR (manufactured by BASF), and polymers described in JP-A-2006-213706, and examples of acrylic-urethane-based polymers include DynamX (manufactured by Nouryon).

[0021] [Highly polymerized polyethylene glycol] Highly polymerized polyethylene glycol is an ethylene oxide polymer having an average molecular weight of 10,000 to 4,000,000, and examples of commercially available products include Polyox™ WSR205 and Polyox™ WSR301 (both manufactured by Dow Chemical Company).

[0022] [Polysaccharide-based polymers] Examples of polysaccharide polymers include gum arabic, glucan, succinoglycan, carrageenan, karaya gum, tragacanth gum, guar gum, locust bean gum, galactomannan gum, xanthan gum, starch, carob gum, quince seed, casein, dextrin, gelatin, sodium pectinate, sodium alginate, methylcellulose, ethylcellulose, carboxymethylcellulose, hydroxyethylcellulose, hydroxypropylcellulose, crystalline cellulose, O-[2-hydroxy-3-(trimethylammonio)propyl]hydroxyethylcellulose chloride, O-[2-hydroxy-3-(trimethylammonio)propyl]guar gum chloride, O-[2-hydroxy-3-(trimethylammonio)propyl]locust bean gum chloride, and hydroxypropyltrimonium starch chloride.

[0023] From the viewpoints of being able to form a hydrophobic film, improving dyeability of the fiber, suppressing fiber damage caused by repeated washing after treatment, and improving washability, stain resistance, and sebum resistance, it is preferable that component (A) contains a silicone-based polymer. The content of the silicone-based polymer in component (A) is preferably 50% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, still more preferably 90% by mass or more, still more preferably 95% by mass or more, and still more preferably 98% by mass or more, and 100% by mass or less.

[0024] More specifically, component (A) preferably contains a silicone-based polymer, and more preferably contains one or more selected from the group consisting of siloxysilicates, poly(N-acylalkyleneimine)-modified organopolysiloxane, (acrylates / dimethicone) copolymer, and (acrylates / polytrimethylsiloxy methacrylate) copolymer. More preferably, component (A) comprises one or more selected from the group consisting of trimethylsiloxysilicate, (acrylates / dimethicone) copolymer, (acrylates / polytrimethylsiloxy methacrylate) copolymer, and poly(N-propionylethyleneimine)organopolysiloxane [polysilicone-9], even more preferably it comprises trimethylsiloxysilicate, and one or more selected from the group consisting of (acrylates / dimethicone) copolymer and (acrylates / polytrimethylsiloxy methacrylate) copolymer, even more preferably it comprises trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer.

[0025] When component (A) contains trimethylsiloxysilicate and one or more selected from the group consisting of (acrylates / dimethicone) copolymer and (acrylates / polytrimethylsiloxy methacrylate) copolymer, the total content of trimethylsiloxysilicate, (acrylates / dimethicone) copolymer and (acrylates / polytrimethylsiloxy methacrylate) copolymer in component (A) is preferably 50% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, still more preferably 90% by mass or more, still more preferably 95% by mass or more, still more preferably 98% by mass or more, and 100% by mass or less.

[0026] When component (A) contains trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer, the total content of trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer in component (A) is preferably 50 mass% or more, more preferably 70 mass% or more, even more preferably 80 mass% or more, still more preferably 90 mass% or more, still more preferably 95 mass% or more, and even more preferably 98 mass% or more, and is 100 mass% or less.

[0027] When component (A) contains trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer, the mass ratio of trimethylsiloxysilicate to (acrylates / polytrimethylsiloxy methacrylate) copolymer [trimethylsiloxysilicate / (acrylates / polytrimethylsiloxy methacrylate) copolymer] is, from the standpoints of film-formability, fiber dyeability, feel, and washing resistance, and of stain resistance and sebum resistance, preferably 0.2 or more, more preferably 0.5 or more, even more preferably 0.8 or more, still more preferably 1.0 or more, still more preferably 1.1 or more, and is preferably 10 or less, more preferably 5.0 or less.

[0028] When component (A) contains a poly(N-acylalkyleneimine)-modified organopolysiloxane, the content of the poly(N-acylalkyleneimine)-modified organopolysiloxane in component (A) is preferably 50 mass% or more, more preferably 70 mass% or more, even more preferably 80 mass% or more, still more preferably 90 mass% or more, still more preferably 95 mass% or more, and even more preferably 98 mass% or more, and is 100 mass% or less.

[0029] The content of component (A) in the composition is preferably 0.5% by mass or more, more preferably 1% by mass or more, even more preferably 2% by mass or more, even more preferably 3% by mass or more, even more preferably 5% by mass or more, even more preferably 10% by mass or more, even more preferably 15% by mass or more, from the viewpoint of improving film-forming properties and dyeability of fibers, washing resistance, stain resistance, and sebum resistance, and is preferably 30% by mass or less, more preferably 25% by mass or less, from the viewpoint of suppressing deterioration of handling properties and feel. The content of component (A) in the composition is preferably 0.5% by mass or more and 30% by mass or less, more preferably 1% by mass or more and 30% by mass or less, even more preferably 2% by mass or more and 30% by mass or less, even more preferably 3% by mass or more and 25% by mass or less, even more preferably 5% by mass or more and 25% by mass or less, even more preferably 10% by mass or more and 25% by mass or less, even more preferably 15% by mass or more and 25% by mass or less.

[0030] <Penetration enhancer (B)> In the present specification, examples of the penetration enhancer (B) include one or more selected from the group consisting of alkylene carbonates such as propylene carbonate; aromatic ring-containing alcohols such as benzyl alcohol, cinnamyl alcohol, phenethyl alcohol, p-anisyl alcohol, p-methylbenzyl alcohol, phenoxyethanol, 2-benzyloxyethanol, γ-phenylpropyl alcohol, cinnamic alcohol, p-methylbenzyl alcohol, α,α-dimethylphenethyl alcohol, and α-phenylethanol; and lactones such as γ-valerolactone and γ-caprolactone. Among these, a representative penetration enhancer (B) is one or more selected from the group consisting of alkylene carbonate and aromatic ring-containing alcohol, preferably one or more selected from the group consisting of propylene carbonate and benzyl alcohol.

[0031] The content of component (B) in the composition is 24% by mass or less, from the viewpoint of suppressing fiber damage due to repeated washing after treatment, preferably 20% by mass or less, more preferably 15% by mass or less, even more preferably 10% by mass or less, even more preferably 8% by mass or less, even more preferably 7% by mass or less, even more preferably 5% by mass or less, even more preferably 3% by mass or less, even more preferably 2% by mass or less, even more preferably 1% by mass or less, even more preferably 0.5% by mass or less, even more preferably 0.1% by mass or less, even more preferably 0.01% by mass or less, and even more preferably 0% by mass.

[0032] <Component (C): High molecular weight organopolysiloxane> The composition preferably contains a high molecular weight organopolysiloxane as component (C) from the standpoints of improving the dyeability of the fiber, suppressing fiber damage due to repeated washing after treatment, and improving washability, stain resistance, and sebum resistance. The degree of polymerization of component (C) is preferably 650 or more, more preferably 800 or more, more preferably 1,200 or more, even more preferably 1,400 or more, even more preferably 1,900 or more, and even more preferably 2,200 or more from the viewpoint of improving the dyeability of the fiber and suppressing fiber damage due to repeated washing after treatment, and from the viewpoint of availability, it is preferably 20,000 or less, more preferably 10,000 or less, even more preferably 4,500 or less, even more preferably 4,000 or less, and even more preferably 3,900 or less. And, the degree of polymerization of component (C) is preferably 650 or more, more preferably 650 or more and 20,000 or less, even more preferably 800 or more and 10,000 or less, even more preferably 1,200 or more and 4,500 or less, even more preferably 1,400 or more and 4,000 or less, even more preferably 1,900 or more and 4,000 or less, and even more preferably 2,200 or more and 3,900 or less.

[0033] More specifically, component (C) is preferably an organopolysiloxane represented by the following general formula (1). [ka] (In the formula, R 11 each independently represents a hydrocarbon group having 1 to 6 carbon atoms; R 12 R each independently represents a hydroxy group, an alkoxy group having 1 to 6 carbon atoms, or a hydrocarbon group having 1 to 6 carbon atoms. 13 represents a hydrocarbon group having 1 to 6 carbon atoms, or a group containing a primary to tertiary amino group. m represents the degree of polymerization and is a number of 650 or more. m R 13 may be the same or different.)

[0034] In general formula (1), R 11 The hydrocarbon group in may be either an aliphatic group or an aromatic group, and examples thereof include an alkyl group, an alkenyl group, a phenyl group, etc. The alkyl group and the alkenyl group may be either a straight chain or a branched chain. Among the above, R 11is preferably an alkyl group or a phenyl group having 1 to 6 carbon atoms, more preferably an alkyl group or a phenyl group having 1 to 3 carbon atoms, even more preferably a methyl group or a phenyl group, and still more preferably a methyl group.

[0035] In general formula (1), R 12 each independently represents a hydroxy group, an alkoxy group having 1 to 6 carbon atoms, or a hydrocarbon group having 1 to 6 carbon atoms. R 12 Examples of the alkoxy group in include a methoxy group, an ethoxy group, a propoxy group, and a butoxy group. R 12 The hydrocarbon group in R 11 and is preferably an alkyl group or a phenyl group having 1 to 6 carbon atoms, more preferably an alkyl group or a phenyl group having 1 to 3 carbon atoms, even more preferably a methyl group or a phenyl group, and still more preferably a methyl group. R 12 From the viewpoint of improving the dyeability of the fiber and suppressing fiber damage, is preferably a hydroxy group, an alkyl group having 1 to 6 carbon atoms, or a phenyl group, more preferably a hydroxy group, an alkyl group having 1 to 3 carbon atoms, or a phenyl group, even more preferably a hydroxy group, a methyl group, or a phenyl group, and still more preferably a methyl group.

[0036] In general formula (1), R 13 represents a hydrocarbon group having 1 to 6 carbon atoms, or a group containing a primary to tertiary amino group. R 13 The hydrocarbon group in R 11 and is preferably an alkyl group or a phenyl group having 1 to 6 carbon atoms, more preferably an alkyl group or a phenyl group having 1 to 3 carbon atoms, even more preferably a methyl group or a phenyl group, and still more preferably a methyl group. R 13 The primary to tertiary amino group-containing groups (hereinafter simply referred to as "amino group-containing groups") in 14 )2, -NR 14(CH2) p N(R 14 )2, or -NR 14 (CH2) p N(R 15 )CO-R 16 In this case, R 14 R represents a hydrogen atom or a monovalent hydrocarbon group having 1 to 4 carbon atoms, and is preferably a hydrogen atom, a methyl group, or an ethyl group. 15 R represents a monovalent hydrocarbon group having 1 to 4 carbon atoms, and is preferably a methyl group or an ethyl group. 16 represents a monovalent hydrocarbon group having a carbon number of 1 to 4. p represents a number of 2 to 6, preferably 2 to 4. R 13 Preferred amino group-containing groups in are -(CH2)3-NH2, -(CH2)3-N(CH3)2, -(CH2)3-NH-(CH2)2-NH2, or -(CH2)2-NH-(CH2)2-N(CH3)2, and more preferably -(CH2)3-NH2.

[0037] R 13 is preferably a hydrocarbon group having 1 to 6 carbon atoms, more preferably an alkyl group or a phenyl group having 1 to 6 carbon atoms, even more preferably an alkyl group or a phenyl group having 1 to 3 carbon atoms, still more preferably a methyl group or a phenyl group, and even more preferably a methyl group.

[0038] In general formula (1), m represents the degree of polymerization and is a number of at least 650. From the viewpoints of improving the dyeability of the fiber, suppressing fiber damage due to repeated washing after treatment, and improving washability, stain resistance, and sebum resistance, m is preferably at least 800, more preferably at least 1,200, even more preferably at least 1,400, still more preferably at least 1,900, and still more preferably at least 2,200, and from the viewpoint of availability, m is preferably at most 20,000, more preferably at most 10,000, even more preferably at most 4,500, still more preferably at most 4,000, and still more preferably at most 3,900. In general formula (1), m is 650 or more, preferably 650 or more and 20,000 or less, more preferably 800 or more and 10,000 or less, even more preferably 1,200 or more and 4,500 or less, still more preferably 1,400 or more and 4,000 or less, still more preferably 1,900 or more and 4,000 or less, and still more preferably 2,200 or more and 3,900 or less.

[0039] The viscosity of component (C) is preferably 5,000 mm from the viewpoints of improving the dyeability of the fiber, suppressing fiber damage caused by repeated washing after treatment, and improving washability, stain resistance, and sebum resistance. 2 / s or more, preferably 10,000 mm 2 / s or more, and more preferably 50,000 mm 2 / s or more, and even more preferably 100,000 mm 2 / s or more, and even more preferably 450,000 mm 2 / s or more, and even more preferably 1 million mm 2 From the viewpoint of availability, it is preferably 140 million mm 2 / s or less, preferably 50 million mm 2 / s or less, and more preferably 40 million mm 2 The viscosity of component (C) is preferably 5,000 mm 2 / s or more 140 million mm 2 / s or less, preferably 10,000 mm 2 / s or more 140 million mm 2 / s or less, and more preferably 10,000 mm 2 / s or more 140 million mm2 / s or less, and even more preferably 50,000 mm 2 / s or more 140 million mm 2 / s or less, and even more preferably 100,000 mm 2 / s or more 50 million mm 2 / s or less, and even more preferably 450,000 mm 2 / s or more 40 million mm 2 / s or less, and even more preferably 1 million mm 2 / s or more 40 million mm 2 / s or less.

[0040] The above viscosity is a value measured at 25°C based on JIS Z8803:2011 "Method for measuring viscosity of liquids." For example, it can be measured using an appropriate viscometer selected from a capillary viscometer, a falling ball viscometer, a rotational viscometer, and a vibration viscometer. If the viscosity exceeds the normal measurement range of the viscometer, it can be determined from a diluted solution of component (C) by the following method. A toluene solution of component (C) with a concentration of 1 g / 100 mL is prepared, and the specific viscosity ηsp (25°C) is calculated using the following formula (1). Next, the intrinsic viscosity [η] is calculated by substituting this into the Huggins relational equation shown in the following formula (2). Furthermore, [η] is substituted into the A. Kolorlov equation shown in the following formula (3) to calculate the molecular weight M. Finally, the viscosity η of component (C) can be calculated by substituting M into the AJ Barry equation shown in the following formula (4) (for example, see 4.2, Performance Test Results of Silicone Oil KF-96, Shin-Etsu Chemical Co., Ltd.). ηsp=(η / η0)-1 (1) (Here, η0 is the viscosity of toluene, and η is the viscosity of the solution) ηsp=〔η〕+K'〔η〕 2 (2) (However, K': Huggins constant is as described in Nakamuta, J. Chem. Soc., 77588

[1956] .) [η] = 0.215 × 10 -4 M 0.65 (3) logη=1.00+0.0123M 0.5 (4)

[0041] The commercially available dimethylpolysiloxane used as component (C) is KF-96H-10,000cs (viscosity 10,000mm). 2 / s), KF-96H-12,500 cs (viscosity 12,500 mm 2 / s), KF-96H-30,000 cs (viscosity 30,000 mm 2 / s), KF-96H-50,000 cs (viscosity 50,000 mm 2 / s), KF-96H-60,000 cs (viscosity 60,000 mm 2 / s), KF-96H-100,000 cs (viscosity 100,000 mm 2 / s), KF-96H-300,000 cs (viscosity 300,000 mm 2 / s), KF-96H-500,000 cs (viscosity 500,000 mm 2 / s), KF-96H-1 million cs (viscosity 1 million mm 2 / s), X-21-5686 (viscosity 3 million mm 2 / s, 30% by mass-isododecane solution), X-25-9074 (viscosity 30 million mm 2 / s, 30 mass%-isododecane solution) (all manufactured by Shin-Etsu Chemical Co., Ltd.), TSF451-100MA (viscosity 1 million mm 2 / s), TSE200A, Silsoft B3020 (viscosity 20 million mm 2 / s, 20% by mass-isododecane solution) (all manufactured by Momentive Performance Materials, Inc.). Commercially available aminopropylmethylpolysiloxanes for use as component (C) include KF-8017 (10% by mass low-viscosity dimethylpolysiloxane solution), KF-8018 (10% by mass cyclopentasiloxane solution), and KF-8020 (20% by mass low-viscosity dimethylpolysiloxane solution) (all manufactured by Shin-Etsu Chemical Co., Ltd.). Commercially available dimethiconol products used as component (C) include X-21-5613 (20% by mass low-viscosity dimethylpolysiloxane solution), X-21-5666 (30% by mass cyclopentasiloxane solution), X-21-5847, and X-21-5849 (all manufactured by Shin-Etsu Chemical Co., Ltd.).

[0042] From the viewpoints of improving the dyeability of the fiber, suppressing fiber damage due to repeated washing after treatment, and improving washability, stain resistance, and sebum resistance, component (C) is preferably one or more members selected from the group consisting of dimethylpolysiloxane, methylphenylpolysiloxane, aminopropylmethylpolysiloxane, and dimethiconol, each of which has a degree of polymerization in the above-mentioned range, and more preferably dimethylpolysiloxane, each of which has a degree of polymerization in the above-mentioned range.

[0043] When the composition contains component (C), the content of component (C) in the composition is preferably 0.01% by mass or more, more preferably 0.02% by mass or more, even more preferably 0.05% by mass or more, still more preferably 0.1% by mass or more, still more preferably 0.2% by mass or more, still more preferably 0.5% by mass or more, and still more preferably 1.0% by mass or more, from the viewpoint of improving the dyeability, washing resistance, stain resistance, and sebum resistance of the fiber. Also, from the viewpoint of suppressing stickiness and imparting a good feel, it is preferably 10% by mass or less, more preferably 8.0% by mass or less, still more preferably 5.0% by mass or less, still more preferably 4.0% by mass or less, and still more preferably 3.5% by mass or less. The content of component (C) in the composition is preferably 0.01 mass% or more and 10 mass% or less, more preferably 0.02 mass% or more and 8.0 mass% or less, even more preferably 0.05 mass% or more and 5.0 mass% or less, still more preferably 0.1 mass% or more and 4.0 mass% or less, still more preferably 0.2 mass% or more and 4.0 mass% or less, still more preferably 0.5 mass% or more and 3.5 mass% or less, and still more preferably 1.0 mass% or more and 3.5 mass% or less.

[0044] <Component (D): Organopolysiloxane having a cationic group other than the components (A) and (C)> The composition may contain, as component (D), an organopolysiloxane having a cationic group other than components (A) and (C). The cationic group contained in component (D) refers to a cationic group or a group that can be ionized to become a cationic group. Specific examples include a primary amino group, a secondary amino group, a tertiary amino group, and a quaternary ammonium group. The cationic group contained in component (D) is preferably at least one selected from the group consisting of a primary amino group, a secondary amino group, and a tertiary amino group.

[0045] From the viewpoints of improving the dyeability of the fiber, suppressing fiber damage due to repeated washing after treatment, and improving washability, stain resistance, and sebum resistance, component (D) is preferably one or more selected from the group consisting of amino-modified silicones and amino polyether-modified silicones.

[0046] The amino-modified silicone is a silicone such as dimethylpolysiloxane (dimethicone) or methylphenylpolysiloxane that has an amino group in the main chain or side chain and does not have a polyether group. Specific examples of amino-modified silicones include one or more selected from the group consisting of aminoethylaminopropyl dimethicone [amodimethicone], aminopropyl dimethicone, bis(aminopropyl) dimethicone, and bis(cetearyl) amodimethicone. Commercially available amino-modified silicones include Silicone SF 8457 C (manufactured by Dow Toray Co., Ltd.), etc. Also usable is DOWSIL CF 1046 (manufactured by Dow Toray Co., Ltd.), which is a mixture of amino-modified silicone and dimethylpolysiloxane.

[0047] The aminopolyether modified silicone is a silicone having an amino group and a polyether group in the main chain or side chain, such as dimethylpolysiloxane (dimethicone) or methylphenylpolysiloxane. From the viewpoints of improving dyeability of the fiber, suppressing fiber damage due to repeated washing after treatment, improving washability, stain resistance, and sebum resistance, and also from the viewpoint of availability, the polyether group is preferably a polyoxyalkylene group, more preferably one or more types selected from the group consisting of a polyoxyethylene group and a polyoxypropylene group, and even more preferably a polyoxyethylene group. The average oxyalkylene number in the polyoxyalkylene group is, from the viewpoints of improving the dyeability of the fiber, suppressing fiber damage due to repeated washing after treatment, and improving washability, stain resistance, and sebum resistance, preferably 3 or more, more preferably 5 or more, even more preferably 10 or more, and is preferably 60 or less, more preferably 40 or less, even more preferably 30 or less, and still more preferably 20 or less.

[0048] Specific examples of amino polyether modified silicones include methoxy PEG / PPG-7 / 3 aminopropyl dimethicone, (bisisobutyl PEG-15 / amodimethicone) copolymer, (bisisobutyl PEG-14 / amodimethicone) copolymer, (bisisobutyl PEG / PPG-20 / 35 / amodimethicone) copolymer, PEG-40 / PPG-8 methylaminopropyl / hydroxypropyl dimethicone copolymer, and the like.

[0049] Commercially available amino polyether modified silicones include ABIL Soft AF100 (methoxy PEG / PPG-7 / 3 aminopropyl dimethicone) (manufactured by Evonik), DOWSIL SS-3588 Fluid (80% by mass ethanol solution of (bisisobutyl PEG-15 / amodimethicone) copolymer), DOWSIL SILSTYLE 104 ((bisisobutyl PEG-14 / amodimethicone) copolymer), DOWSIL SILSTYLE 201 ((bisisobutyl PEG-14 / amodimethicone) copolymer), DOWSIL SILSTYLE 401 ((bisisobutyl PEG / PPG-20 / 35 / amodimethicone) copolymer) (all manufactured by Dow Toray Co., Ltd.), Silsoft A+ (PEG-40 / PPG-8 Methylaminopropyl / hydroxypropyl dimethicone copolymer (manufactured by Momentive Performance Materials), etc.

[0050] Component (D) may be one or more of the above. Among the above, from the viewpoints of improving dyeability of fibers, suppressing fiber damage caused by repeated washing after treatment, and improving washability, stain resistance, and sebum resistance, component (D) is preferably an aminopolyether-modified silicone, more preferably an aminopolyether-modified silicone having a polyoxyethylene group, even more preferably one or more selected from the group consisting of (bisisobutyl PEG-15 / amodimethicone) copolymer and (bisisobutyl PEG-14 / amodimethicone) copolymer, and even more preferably (bisisobutyl PEG-15 / amodimethicone) copolymer.

[0051] When the composition contains component (D), the content of component (D) in the composition is preferably 0.01% by mass or more, more preferably 0.02% by mass or more, even more preferably 0.05% by mass or more, still more preferably 0.1% by mass or more, and even more preferably 0.2% by mass or more from the viewpoints of improving the dyeability of the fiber, suppressing fiber damage due to repeated washing after treatment, improving washability, stain resistance, and sebum resistance. Also, from the viewpoint of suppressing stickiness and imparting a good feel, the content is preferably 8.0% by mass or less, more preferably 5.0% by mass or less, even more preferably 3.0% by mass or less, and even more preferably 2.5% by mass or less. The content of component (D) in the composition is preferably 0.01 mass% or more and 8.0 mass% or less, more preferably 0.02 mass% or more and 5.0 mass% or less, even more preferably 0.05 mass% or more and 3.0 mass% or less, still more preferably 0.1 mass% or more and 3.0 mass% or less, and even more preferably 0.2 mass% or more and 2.5 mass% or less.

[0052] From the viewpoints of improving dyeability of the fiber, suppressing fiber damage due to repeated washing after treatment, and improving wash resistance, stain resistance, and sebum resistance, the composition is preferably the following composition (I) or (II). (I) A composition comprising a film-forming agent (A), a penetration enhancer (B) content of 24% by mass or less, and a pH of 10 or less, A composition wherein said component (A) comprises trimethylsiloxysilicate. (II) A composition comprising a film-forming agent (A), a penetration enhancer (B) content of 24% by mass or less, and a pH of 10 or less, A composition, wherein component (A) comprises a poly(N-acylalkyleneimine)-modified organopolysiloxane.

[0053] The composition (I) further preferably contains one or more selected from the group consisting of the following components, more preferably two or more, even more preferably three or more, and still more preferably all of the following components. Component (A) is an acrylates / dimethicone copolymer. Component (A) is an acrylates / polytrimethylsiloxy methacrylate copolymer. Component (C), a high molecular weight organopolysiloxane Component (D) is an organopolysiloxane having a cationic group other than components (A) and (C).

[0054] Component (A) in composition (I) contains trimethylsiloxysilicate, preferably contains trimethylsiloxysilicate and one or more selected from the group consisting of (acrylates / dimethicone) copolymer and (acrylates / polytrimethylsiloxy methacrylate) copolymer, more preferably contains trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer.

[0055] When component (A) in composition (I) contains trimethylsiloxysilicate and one or more selected from the group consisting of (acrylates / dimethicone) copolymer and (acrylates / polytrimethylsiloxy methacrylate) copolymer, the total content of trimethylsiloxysilicate, (acrylates / dimethicone) copolymer and (acrylates / polytrimethylsiloxy methacrylate) copolymer in component (A) is preferably 50% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, still more preferably 90% by mass or more, still more preferably 95% by mass or more, still more preferably 98% by mass or more, and is 100% by mass or less.

[0056] When component (A) in composition (I) contains trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer, the total content of trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer in component (A) is preferably 50 mass% or more, more preferably 70 mass% or more, even more preferably 80 mass% or more, still more preferably 90 mass% or more, still more preferably 95 mass% or more, and even more preferably 98 mass% or more, and is 100 mass% or less.

[0057] When component (A) in composition (I) contains trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer, the mass ratio of trimethylsiloxysilicate to (acrylates / polytrimethylsiloxy methacrylate) copolymer [trimethylsiloxysilicate / (acrylates / polytrimethylsiloxy methacrylate) copolymer] is, from the viewpoints of improving film-forming properties, fiber dyeability, feel, and washing resistance, and of improving stain resistance and sebum resistance, preferably 0.2 or more, more preferably 0.5 or more, even more preferably 0.8 or more, still more preferably 1.0 or more, still more preferably 1.1 or more, and is preferably 10 or less, more preferably 5.0 or less.

[0058] The poly(N-acylalkyleneimine)-modified organopolysiloxane in the component (A) of the composition (II) is preferably one or more selected from the group consisting of poly(N-formylethyleneimine)organopolysiloxane, poly(N-acetylethyleneimine)organopolysiloxane, and poly(N-propionylethyleneimine)organopolysiloxane [polysilicone-9], and more preferably poly(N-propionylethyleneimine)organopolysiloxane [polysilicone-9].

[0059] In the composition (II), the content of the poly(N-acylalkyleneimine)-modified organopolysiloxane in the component (A) is preferably 50 mass% or more, more preferably 70 mass% or more, even more preferably 80 mass% or more, still more preferably 90 mass% or more, still more preferably 95 mass% or more, and still more preferably 98 mass% or more, and is 100 mass% or less.

[0060] In the composition (I), the component (C) is preferably a dimethylpolysiloxane having a degree of polymerization of 650 or more, more preferably from 650 to 20,000, even more preferably from 800 to 10,000, still more preferably from 1,200 to 4,500, still more preferably from 1,400 to 4,000, still more preferably from 1,900 to 4,000, and still more preferably from 2,200 to 3,900. In the composition (I), the component (D) is preferably an aminopolyether-modified silicone, more preferably an aminopolyether-modified silicone having a polyoxyethylene group, even more preferably one or more selected from the group consisting of (bisisobutyl PEG-15 / amodimethicone) copolymer and (bisisobutyl PEG-14 / amodimethicone) copolymer, and even more preferably a (bisisobutyl PEG-15 / amodimethicone) copolymer.

[0061] Regarding the composition (I) and the composition (II), the preferred embodiments of each component other than those mentioned above are the same as those described above.

[0062] <Pigments> When the composition is a dye composition, it is preferred that the composition further contains a pigment. Examples of pigments include pearl pigments (interference pearl pigments, colored pearl pigments), organic pigments, inorganic pigments, and metal powder pigments.

[0063] The interference pearl pigment has a core particle and a coating layer formed on the surface of the core particle. The material of the core particle constituting the interference pearl pigment includes mica, sericite, talc, kaolin, smectite clay minerals, bismuth oxychloride, synthetic mica, synthetic sericite, plate-like silica, plate-like alumina, etc. The coating layer constituting the interference pearl pigment is a layer that acts as a reflective interference layer. The coating layer is a layer made of a thin film mainly composed of colorless metal oxide such as titanium dioxide, zinc oxide, aluminum oxide, or colorless metal such as titanium, zirconium, zinc, tin, silicon, aluminum, and may be a single layer structure or a multilayer structure. Commercially available interference pearl pigments include Timiron Super Blue, Timiron Super Gold, Timiron Super Green, and Timiron Super Red (all manufactured by Merck).

[0064] Examples of colored pearl pigments include iron oxide-coated mica, iron oxide-coated titanium mica, black iron oxide-coated mica, black iron oxide-coated titanium mica, yellow iron oxide-coated mica, iron oxide-black iron oxide-coated titanium mica, iron oxide-Prussian blue-coated titanium mica, iron oxide-coated bismuth oxychloride, iron oxide-coated bismuth oxychloride mica, etc. Examples of commercially available colored pearl pigments include Timica Golden Bronze, Cloisonne Super Green (both manufactured by BASF), COLORONA BORDEAUX, COLORONA LIGHT BLUE, COLORONA Blackstar BLUE, COLORONA FINE GOLD MP-20, COLORONA PRECIOUS GOLD, COLORONA RED BROWN, COLORONA DARK BLUE, etc.

[0065] Examples of organic pigments include Red No. 201, Red No. 202, Red No. 203, Red No. 204, Red No. 205, Red No. 206, Red No. 207, Red No. 208, Red No. 219, Red No. 220, Red No. 221, Red No. 226, Red No. 228, Red No. 404, Red No. 405, Orange No. 203, Orange No. 204, Orange No. 401, Yellow No. 205, Yellow No. 401, Blue No. 404, and the like.

[0066] Among the inorganic pigments, inorganic black pigments include carbon black, black iron oxide, and black titanium oxide; inorganic red pigments include iron oxide (red iron oxide), iron hydroxide, and iron titanate; inorganic brown pigments include γ-iron oxide, etc.; inorganic yellow pigments include yellow iron oxide and yellow ochre; inorganic blue pigments include ultramarine and Prussian blue; inorganic purple pigments include manganese violet and cobalt violet; inorganic green pigments include chromium oxide, chromium hydroxide, and cobalt titanate; and inorganic white pigments include titanium oxide, zinc oxide, cerium oxide, and barium sulfate.

[0067] Examples of the metal powder pigment include gold powder, silver powder, copper powder, aluminum powder, and brass powder. The pigments may be used alone or in combination of two or more of the above.

[0068] When the composition contains a pigment, the content of the pigment in the composition is preferably 0.01% by mass or more, more preferably 0.1% by mass or more, even more preferably 0.5% by mass or more, and even more preferably 1.0% by mass or more from the viewpoint of improving the dyeability of the fiber, and is preferably 30% by mass or less, more preferably 20% by mass or less, even more preferably 15% by mass or less, and even more preferably 10% by mass or less from the viewpoint of dispersibility in the composition and economic efficiency. The content of the pigment in the composition is preferably 0.01% by mass or more and 30% by mass or less, more preferably 0.1% by mass or more and 20% by mass or less, even more preferably 0.5% by mass or more and 15% by mass or less, and even more preferably 1.0% by mass or more and 10% by mass or less.

[0069] <Volatile solvent> From the viewpoint of dispersing or dissolving the components (A) to (D) and the pigment, the composition preferably further contains a volatile solvent. Note that the volatile solvent defined in the present invention does not include water.

[0070] Examples of the volatile solvent include alcohol-based solvents, ether-based solvents, ketone-based solvents, ester-based solvents, hydrocarbon-based solvents, and silicone-based solvents, each of which has the volatility defined above. Examples of the alcohol solvent include ethanol, 1-propanol, 2-propanol, 1-butanol, and 2-butanol. Examples of the ether solvent include diethyl ether and tetrahydrofuran, and examples of the ketone solvent include acetone and methyl ethyl ketone. Examples of the ester solvent include methyl acetate, ethyl acetate, butyl acetate, and isobutyl acetate. Examples of the hydrocarbon solvent include light liquid isoparaffin (mainly composed of isoparaffin having 8 to 16 carbon atoms), pentane, isopentane, hexane, isohexane, heptane, isoheptane, decane, isodecane, dodecane, isododecane, tridecane, isotridecane, tetradecane, and isotetradecane. In addition, silicone-based solvents with a viscosity of 10 mm at 25°C are 2 Dimethylpolysiloxanes with a viscosity of 20 mm / s or less, alkyl trimethicones such as methyl trimethicone, and 2 As the volatile solvent, one or more of these can be used.

[0071] From the viewpoint of dispersing or dissolving the components (A) to (D) and the pigment, the volatile solvent is preferably at least one selected from the group consisting of alcohol-based solvents, hydrocarbon-based solvents, and silicone-based solvents, and more preferably ethanol, 1-propanol, 2-propanol, 1-butanol, 2-butanol, pentane, isopentane, hexane, isohexane, heptane, isoheptane, decane, isodecane, dodecane, isododecane, tridecane, isotridecane, tetradecane, isotetradecane, light liquid isoparaffin, and a viscosity at 25° C. of 10 mm 2 Dimethylpolysiloxane, methyltrimethicone, and a viscosity of 20mm at 25°C or less 2 More preferably, the solvent is ethanol, isodecane, isododecane, isotetradecane, or light liquid isoparaffin; the viscosity at 25° C. is 5 mm2 More preferably, it is one or more selected from the group consisting of dimethylpolysiloxane having a molecular weight of 1 / s or less, and methyltrimethicone, and even more preferably, it is one or more selected from the group consisting of ethanol, isodecane, isododecane, isotetradecane, and light liquid isoparaffin, and even more preferably, it is isododecane.

[0072] When the composition contains a volatile solvent, the content of the volatile solvent in the composition is preferably 1% by mass or more, more preferably 5% by mass or more, even more preferably 10% by mass or more, even more preferably 20% by mass or more, even more preferably 30% by mass or more, and even more preferably 40% by mass or more from the viewpoint of dispersing or dissolving the components (A) to (D) and the pigment, and is preferably 98% by mass or less, more preferably 95% by mass or less, even more preferably 90% by mass or less, and even more preferably 80% by mass or less from the viewpoint of adjusting the viscosity to be easily applied to the fiber for head ornament products. The content of the volatile solvent in the composition is preferably 1% by mass or more and 98% by mass or less, more preferably 5% by mass or more and 95% by mass or less, even more preferably 10% by mass or more and 90% by mass or less, even more preferably 20% by mass or more and 80% by mass or less, even more preferably 30% by mass or more and 80% by mass or less, and even more preferably 40% by mass or more and 80% by mass or less. The content of the volatile solvent in the composition may be the balance of components (A) to (D) and the pigment.

[0073] <Water> The water content in the composition is preferably small from the viewpoint of improving the dispersibility of components (A) to (D) and the pigment, and from the viewpoint of improving the drying speed, and is preferably less than 10 mass%, more preferably less than 8 mass%, even more preferably less than 6 mass%, still more preferably less than 5 mass%, still more preferably less than 3 mass%, and even more preferably less than 1 mass%. In this specification, the term "substantially free" means that it is not added intentionally, and does not exclude the inclusion of a trace amount as an impurity.

[0074] <Solid oil> The composition preferably contains a small amount of solid oil from the viewpoint of improving film-forming properties, improving dyeability of fibers, and suppressing fiber damage caused by repeated washing after treatment. The solid oil is an oil agent that is solid at 25°C, and examples of the solid oil include paraffin wax such as solid paraffin, polyolefin wax such as polyethylene wax, and beeswax. The content of the solid oil in the composition is preferably less than 50% by mass, more preferably less than 20% by mass, even more preferably less than 10% by mass, still more preferably less than 5% by mass, and even more preferably less than 1% by mass.

[0075] <Volatile cyclic silicone> From the viewpoint of improving drying speed, the composition preferably has a low content of volatile cyclic silicone such as decamethylcyclopentasiloxane.This is because volatile cyclic silicone has a slower volatilization time than other volatile solvents, and tends to take a long time to dry after being applied to an object.The content of volatile cyclic silicone in the composition is preferably less than 5% by mass, more preferably less than 2% by mass, even more preferably less than 1% by mass, even more preferably less than 0.5% by mass, even more preferably less than 0.1% by mass, and even more preferably 0% by mass.

[0076] <Silicone surfactant> The composition preferably contains a small amount of silicone surfactant from the viewpoint of improving film-forming property, improving dyeability of fibers, and suppressing fiber damage caused by repeated washing after treatment.The silicone surfactant means a surfactant having a silicone structure, typically a polysiloxane structure, and may have a hydrophilic group, a hydrophilic polymer chain, etc., on a side chain, an end, etc.The content of the silicone surfactant in the composition is preferably less than 5% by mass, more preferably less than 2% by mass, even more preferably less than 1% by mass, even more preferably less than 0.5% by mass, and even more preferably less than 0.1% by mass.

[0077] <Oil gelling agent> From the viewpoints of improving film-forming properties, improving dyeability of fibers, and suppressing fiber damage due to repeated washing after treatment, the composition preferably contains a small amount of oil gelling agents such as fatty acid dextrin, hydrophobic silica, lipophilic clay minerals, etc. The content of the oil gelling agent in the composition is preferably less than 5% by mass, more preferably less than 2% by mass, even more preferably less than 1% by mass, still more preferably less than 0.5% by mass, and even more preferably less than 0.1% by mass.

[0078] <Non-volatile liquid oil> From the viewpoints of improving film-forming properties, improving dyeability of fibers, and suppressing fiber damage due to repeated washing after treatment, the composition preferably contains a small amount of non-volatile liquid oil. The content of non-volatile liquid oil in the composition is preferably less than 50% by mass, more preferably less than 40% by mass, even more preferably less than 30% by mass, still more preferably less than 20% by mass, still more preferably less than 10% by mass, still more preferably less than 5% by mass, still more preferably less than 2% by mass, still more preferably less than 1% by mass, still more preferably less than 0.5% by mass, and still more preferably less than 0.1% by mass.

[0079] <Polyhydric alcohol> From the viewpoint of improving film-forming properties, improving dyeability of fibers, and suppressing fiber damage caused by repeated washing after treatment, the composition preferably contains a small amount of polyhydric alcohol. Examples of the polyhydric alcohol include propylene glycol and glycerin. The content of the polyhydric alcohol in the composition is preferably less than 5% by mass, more preferably less than 2% by mass, even more preferably less than 1% by mass, still more preferably less than 0.5% by mass, and even more preferably less than 0.1% by mass.

[0080] <Other ingredients> In addition to the above-mentioned components, the composition may contain antioxidants, fragrances, preservatives, thickeners, pH adjusters, and the like.

[0081] <ph> The pH of the composition is 10 or less, preferably 9.5 or less, more preferably 9.0 or less, more preferably 8.5 or less, even more preferably 8.0 or less, and even more preferably 7.5 or less, from the viewpoint of suppressing fiber damage and skin irritation caused by repeated washing after treatment. Also, from the viewpoint of improving the dyeability of the fiber and suppressing fiber damage and skin irritation, it is preferably 3.0 or more, more preferably 4.0 or more, more preferably 5.0 or more, even more preferably 5.5 or more, and even more preferably 6.0 or more. The pH of the composition is 10 or less, preferably 3.0 or more and 10 or less, more preferably 4.0 or more and 9.5 or less, even more preferably 5.0 or more and 9.0 or less, even more preferably 5.0 or more and 8.5 or less, even more preferably 5.5 or more and 8.0 or less, and even more preferably 6.0 or more and 7.5 or less. The above pH can be measured at 30° C. by the method described in the Examples.

[0082] <Dosage form, etc.> The formulation of the composition is not particularly limited, and can be in the form of liquid, paste, cream, gel, foam, spray, wax, etc., depending on the product form. The composition may be in the form of an emulsion type composition such as a water-in-oil type composition, or in the form of a non-emulsion type composition. From the viewpoints of improving film-forming properties, improving fiber dyeability, and suppressing fiber damage, however, a non-emulsion type composition is preferable.

[0083] Examples of the product form of the composition include a cleaning composition, a conditioning composition, a treatment composition (including leave-in type), a styling composition, a dye composition, a permanent composition, etc. Among these, from the viewpoint of the effectiveness of the effects of the present invention, the dye composition is preferred.

[0084] From the viewpoint of the effect of the invention that the composition has good dyeability to fibers and can suppress damage to the fibers due to repeated washing after treatment, it is preferable that the composition is a leave-on composition that is applied to fibers for head ornament products and then dried without being washed off. For example, when the composition is a dye composition, the dye composition is preferably a dye composition that is applied to fibers for head ornament products to form a colored film and then dried without being washed off.

[0085] The method for preparing the composition is not particularly limited. For example, the composition can be prepared by mixing the components (A) and (B) and other components used as necessary, and stirring the mixture using a known stirring device.

[0086] <Fiber for headdress products> As used herein, headwear fibers exclude human hair. The fibers for head ornament products to be treated with the composition may be either naturally derived or synthetic, but naturally derived fibers are preferred. Naturally derived fibers refer to fibers collected from natural animals and plants, or fibers artificially manufactured using collagen, casein, soybeans, peanuts, corn, silk waste, silk protein (e.g., silk fibroin), and other proteins, polysaccharides, and other polymers or oligomers as raw materials. Among these, fibers artificially manufactured using animal hair, or proteins derived from keratin, collagen, casein, soybeans, peanuts, corn, silk waste, silk protein (e.g., silk fibroin), and other polymers or oligomers as raw materials are preferred, and regenerated protein fibers made from proteins derived from keratin, collagen, casein, soybean protein, peanut protein, corn protein, silk protein (e.g., silk fibroin), and other proteins are more preferred, and regenerated protein fibers such as regenerated collagen fibers made from collagen, and regenerated silk fibers made from silk fibroin are even more preferred, with regenerated collagen fibers being even more preferred. Regenerated collagen fibers can be produced by known techniques. The composition of regenerated collagen fibers does not need to be 100% collagen, and may contain natural polymers, synthetic polymers, additives, etc. for quality improvement. Furthermore, regenerated collagen fibers may be post-processed or post-treated. Filaments are preferred as the form of regenerated collagen fibers. Filaments are generally taken out from bobbins or boxes. In addition, filaments coming out of the drying process in the manufacturing process of regenerated collagen fibers can be used directly.

[0087] The synthetic fiber may be a fiber containing a synthetic resin as a main component. From the viewpoint of ease of production of the synthetic fiber and of obtaining a texture similar to that of human hair, the synthetic resin is preferably a thermoplastic resin, more preferably one or more selected from the group consisting of polyester resin, polyamide resin, polyimide resin, polyamideimide resin, vinyl chloride resin, polycarbonate resin, polyphenylene sulfide resin, and modacrylic resin (a copolymer of acrylonitrile and vinyl chloride). The term "main component" as used herein means a component whose content in the synthetic fiber is preferably 50% by mass or more, more preferably 60% by mass or more, even more preferably 70% by mass or more, even more preferably 80% by mass or more, and even more preferably 90% by mass or more, but not more than 100% by mass. In addition to the above synthetic resins, the synthetic fibers may further contain various additives such as flame retardants, flame retardant assistants, light or heat stabilizers, fluorescent agents, antioxidants, antistatic agents, and ultraviolet absorbing agents, as long as the effects of the present invention are not impaired.

[0088] The tensile modulus in water of the fiber for head ornament products to be treated with the composition is 0.4 GPa or more, preferably 0.5 GPa or more, more preferably 0.6 GPa or more, and even more preferably 0.7 GPa or more, from the viewpoint of suppressing fiber damage due to repeated washing after treatment. The upper limit is not particularly limited, but from the viewpoint of use in head ornament products, it is usually 10 GPa or less, preferably 5.0 GPa or less, more preferably 3.0 GPa or less, even more preferably 2.0 GPa or less, and even more preferably 1.0 GPa or less. The tensile modulus of the fiber for head accessories in water can be measured in water at 20° C., specifically, by the method described in the Examples.

[0089] In the method of the present invention, from the viewpoint of quickly forming a film, in the treatment of the fiber for head accessories, the composition is preferably applied to the fiber for head accessories and then dried. From the viewpoint of uniform application, the composition is preferably temporarily dissolved or dispersed before use and then applied to the surface of the fiber for head ornament products. As a means for temporarily dissolving or dispersing, any of thermodynamic means such as heating, physical means such as mechanically applying shear stress, and chemical means such as adding a compatible solvent can be used. From the viewpoint of user convenience, it is preferable to dissolve or disperse the composition uniformly by physical means such as stirring or shaking.

[0090] In the treatment of the fiber for head ornament products, the fiber for head ornament products to which the composition is applied may be in a dry or wet state, but from the viewpoint of ease of film formation, it is preferable to apply the composition to the fiber for head ornament products in a dry state. Methods for applying the composition include casting, spraying, coating, immersion, etc., and from the viewpoint of ease of treatment, spraying, coating, or immersion are preferable, and coating is more preferable.

[0091] In the treatment of the fiber for head ornament products, the amount of the composition applied to the fiber for head ornament products is not particularly limited, but from the viewpoint of improving film formability and dyeability of the fiber, the mass ratio of the composition to the fiber for head ornament products (composition / fiber for head ornament products) is preferably 0.005 or more, more preferably 0.01 or more, and even more preferably 0.05 or more, and from the viewpoint of suppressing fiber damage due to repeated washing after treatment and improving drying speed, it is preferably 10 or less, more preferably 5 or less, even more preferably 3 or less, still more preferably 2 or less, and even more preferably 1 or less. The amount of the composition applied to the fiber for head ornament products is preferably 0.005 or more and 10 or less, more preferably 0.005 or more and 5 or less, even more preferably 0.01 or more and 3 or less, still more preferably 0.01 or more and 2 or less, and even more preferably 0.05 or more and 1 or less.

[0092] It is preferable that the fiber for head accessories after the composition is applied is dried without rinsing with water. The fiber for head accessories after the composition is applied may be dried naturally or with a device such as a hood, a hair dryer, or a straightening iron. When using the device, from the viewpoint of suppressing thermal damage to the fiber for head accessories, it is preferable to dry the fiber at a temperature of 40° C. or more and 220° C. or less. More preferable is drying with a hood or a hair dryer, and the drying temperature is preferably 40° C. or more and 110° C. or less, more preferably 50° C. or more and 90° C. or less. The drying time is not particularly limited as long as a film is substantially formed on the surface of the fiber for head ornament products, and may be adjusted appropriately. For example, the drying time may be within the range of 10 seconds to 120 minutes.

[0093] The treatment of the fiber for headwear products may include a step of applying the composition to the fiber for headwear products in a state where it is worn on the head, or may include a step of applying the composition to the fiber for headwear products in a state where it is not worn on the head. The method of applying the composition to the fibers for head accessories in a state where the fibers are worn on the head is advantageous in that the fibers can be treated to approach an ideal finish, whereas the method of applying the composition to the fibers for head accessories not worn on the head is advantageous in that the composition (particularly the dye composition) can be prevented from adhering to parts other than the fibers, such as the hair and scalp.

[0094] In the method of the present invention, in order to achieve an ideal finish, the step of applying the composition to the fiber for a head accessory may be repeated two or more times. The number of repetitions is not particularly limited, but is preferably 10 times or less, more preferably 5 times or less, from the viewpoint of reducing the burden on the practitioner.

[0095] Specific examples of the method for treating fibers for head accessories using the composition of the present invention include the following methods. (1) A method comprising the steps of: attaching a fiber for head accessories to the head; and applying the composition to the fiber for head accessories in the state that the fiber is attached to the head. The step of applying the composition to the fiber for head accessories may be performed two or more times while the fiber for head accessories is attached to the head, while checking the finished state. (2) A method comprising a step of applying the composition to a fiber for a head accessory product not worn on the head. The method may further comprise, after the step, a step of wearing the fiber for a head accessory product on the head (checking the finished state), a step of removing the fiber for a head accessory product from the head, and a step of applying the composition to the fiber for a head accessory product not worn on the head. The cycle of the steps of wearing the fiber for a head accessory product on the head, removing the fiber for a head accessory product from the head, and applying the composition to the fiber for a head accessory product not worn on the head may be performed two or more times. From the viewpoint of reducing the risk of skin coloring and scalp irritation, the treatment of the fiber for head decoration products is preferably the above-mentioned (2), i.e., a method including a step of applying the composition to the fiber for head decoration products in a state where the fiber is not worn on the head. From the viewpoint of achieving both an ideal finish and reducing the risk of skin coloring and scalp irritation, the treatment of the fiber for head decoration products is more preferably a method including a step of applying the composition to the fiber for head decoration products in a state where the fiber for head decoration products is not worn on the head, and after the step, a cycle of a step of wearing the fiber for head decoration products on the head, a step of removing the fiber for head decoration products from the head, and a step of applying the composition to the fiber for head decoration products in a state where the fiber for head decoration products is not worn on the head is performed once or more and nine times or less, preferably once or more and four times or less.

[0096] The treatment is preferably a dyeing treatment of fibers for head accessories. When the composition is used in the dyeing treatment of the fibers, the dyeability of the fibers is good, damage to the fibers caused by repeated washing after the dyeing treatment can be suppressed, and further, it is possible to achieve both an ideal finish and a reduced risk of skin coloration and scalp irritation.

[0097] [Dyeing method for fibers for headwear products] The present invention further provides a method for dyeing fibers for head accessories, comprising a step of applying a composition containing a film-forming agent (A), having a content of a penetration enhancer (B) of 24 mass% or less, and having a pH of 10 or less, to fibers for head accessories having a tensile modulus in water of 0.4 GPa or more. The composition used in the dyeing method is preferably a dye composition further containing a pigment. The step of applying the composition to fibers for head accessories can be carried out in the same manner as described above. According to the method for dyeing fibers for head accessories of the present invention, the dyeability of the fibers is good, and damage to the fibers caused by repeated washing after the dyeing process can be suppressed. Furthermore, it is possible to achieve both an ideal finish and a reduced risk of skin coloration and scalp irritation.

[0098] With respect to the above-mentioned embodiments, the present invention discloses the following. <1> A method for using a composition comprising a film-forming agent (A), a penetration enhancer (B) content of 24 mass% or less, and a pH of 10 or less, in the treatment of fibers for head accessories having a tensile modulus in water of 0.4 GPa or more. <2> The component (A) contains at least one selected from the group consisting of silicone-based polymers, anionic vinyl polymers, cationic vinyl polymers, amphoteric vinyl polymers, nonionic vinyl polymers, urethane-based polymers, highly polymerized polyethylene glycols, and polysaccharide-based polymers. <1> How to use: <3> The component (A) preferably contains a silicone-based polymer, and more preferably contains one or more selected from the group consisting of siloxysilicates, poly(N-acylalkyleneimine)-modified organopolysiloxane, (acrylates / dimethicone) copolymer, and (acrylates / polytrimethylsiloxy methacrylate) copolymer. More preferably, component (A) comprises one or more selected from the group consisting of trimethylsiloxysilicate, (acrylates / dimethicone) copolymer, (acrylates / polytrimethylsiloxy methacrylate) copolymer, and poly(N-propionylethyleneimine)organopolysiloxane [polysilicone-9], even more preferably, component (A) comprises one or more selected from the group consisting of trimethylsiloxysilicate, (acrylates / dimethicone) copolymer, and (acrylates / polytrimethylsiloxy methacrylate) copolymer, even more preferably, component (A) comprises trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer. <1> or <2> How to use: <4> The content of the component (A) in the composition is preferably 0.5% by mass or more and 30% by mass or less, more preferably 1% by mass or more and 30% by mass or less, even more preferably 2% by mass or more and 30% by mass or less, still more preferably 3% by mass or more and 25% by mass or less, still more preferably 5% by mass or more and 25% by mass or less, still more preferably 10% by mass or more and 25% by mass or less, and still more preferably 15% by mass or more and 25% by mass or less. <1> ~ <3> Use one of the following methods. <5> The penetration enhancer (B) is at least one selected from the group consisting of propylene carbonate, aromatic ring-containing alcohols, and lactones, more preferably at least one selected from the group consisting of alkylene carbonate and aromatic ring-containing alcohols, and even more preferably at least one selected from the group consisting of propylene carbonate and benzyl alcohol. <1> ~ <4> Use one of the following methods. <6> The content of the component (B) in the composition is preferably 20% by mass or less, more preferably 15% by mass or less, even more preferably 10% by mass or less, still more preferably 8% by mass or less, still more preferably 7% by mass or less, still more preferably 5% by mass or less, still more preferably 3% by mass or less, still more preferably 2% by mass or less, still more preferably 1% by mass or less, still more preferably 0.5% by mass or less, still more preferably 0.1% by mass or less, still more preferably 0.01% by mass or less, and still more preferably 0% by mass. <1> ~ <5> Use one of the following methods. <7> The composition further comprises a high molecular weight organopolysiloxane as component (C). <1> ~ <6> Use one of the following methods. <8> The degree of polymerization of the component (C) is preferably 650 or more, more preferably 650 or more and 20,000 or less, even more preferably 800 or more and 10,000 or less, still more preferably 1,200 or more and 4,500 or less, still more preferably 1,400 or more and 4,000 or less, still more preferably 1,900 or more and 4,000 or less, and still more preferably 2,200 or more and 3,900 or less. <7> How to use <9> The component (C) is an organopolysiloxane represented by the following general formula (1): <7> or <8> How to use: [ka] (In the formula, R 11 each independently represents a hydrocarbon group having 1 to 6 carbon atoms; R 12 R each independently represents a hydroxy group, an alkoxy group having 1 to 6 carbon atoms, or a hydrocarbon group having 1 to 6 carbon atoms. 13 represents a hydrocarbon group having 1 to 6 carbon atoms, or a group containing a primary to tertiary amino group. m represents the degree of polymerization and is a number of 650 or more. m R 13 may be the same or different.) <10> The viscosity of the component (C) is preferably 5,000 mm 2 / s or more 140 million mm 2 / s or less, preferably 10,000 mm 2 / s or more 140 million mm 2 / s or less, and more preferably 10,000 mm 2 / s or more 140 million mm 2 / s or less, and even more preferably 50,000 mm 2 / s or more 140 million mm 2 / s or less, and even more preferably 100,000 mm 2 / s or more 50 million mm 2 / s or less, and even more preferably 450,000 mm 2 / s or more 40 million mm 2 / s or less, and even more preferably 1 million mm 2 / s or more 40 million mm 2 / s or less, <7> ~ <9> Use one of the following methods.

[0099] <11> The component (C) contains one or more selected from the group consisting of dimethylpolysiloxane, methylphenylpolysiloxane, aminopropylmethylpolysiloxane, and dimethiconol, and more preferably contains dimethylpolysiloxane. <7> ~ <10> Use one of the following methods. <12> The content of component (C) in the composition is preferably 0.01% by mass or more and 10% by mass or less, more preferably 0.02% by mass or more and 8.0% by mass or less, even more preferably 0.05% by mass or more and 5.0% by mass or less, still more preferably 0.1% by mass or more and 4.0% by mass or less, still more preferably 0.2% by mass or more and 4.0% by mass or less, still more preferably 0.5% by mass or more and 3.5% by mass or less, and still more preferably 1.0% by mass or more and 3.5% by mass or less. <7> ~ <11> Use one of the following methods. <13> The composition further contains, as component (D), an organopolysiloxane having a cationic group other than components (A) and (C). <1> ~ <12> Use one of the following methods. <14> The component (D) is at least one selected from the group consisting of amino-modified silicones and aminopolyether-modified silicones, preferably aminopolyether-modified silicones, more preferably aminopolyether-modified silicones having polyoxyethylene groups, even more preferably at least one selected from the group consisting of (bisisobutyl PEG-15 / amodimethicone) copolymers and (bisisobutyl PEG-14 / amodimethicone) copolymers, and even more preferably (bisisobutyl PEG-15 / amodimethicone) copolymers. <13> How to use: <15> The content of the component (D) in the composition is preferably 0.01% by mass or more and 8.0% by mass or less, more preferably 0.02% by mass or more and 5.0% by mass or less, even more preferably 0.05% by mass or more and 3.0% by mass or less, still more preferably 0.1% by mass or more and 3.0% by mass or less, and still more preferably 0.2% by mass or more and 2.5% by mass or less. <13> or <14> How to use: <16> The composition is the following composition (I) or (II): <1> ~ <15> Use one of the following methods. (I) A composition comprising a film-forming agent (A), a penetration enhancer (B) content of 24% by mass or less, and a pH of 10 or less, A composition wherein said component (A) comprises trimethylsiloxysilicate. (II) A composition comprising a film-forming agent (A), a penetration enhancer (B) content of 24% by mass or less, and a pH of 10 or less, A composition, wherein component (A) comprises a poly(N-acylalkyleneimine)-modified organopolysiloxane. <17> The composition (I) further preferably contains one or more selected from the group consisting of the following components, more preferably two or more selected from the group consisting of the following components, and even more preferably all of the following components: <16> How to use: Component (A) is an acrylates / dimethicone copolymer. Component (A) is an acrylates / polytrimethylsiloxy methacrylate copolymer. Component (C), a high molecular weight organopolysiloxane Component (D) is an organopolysiloxane having a cationic group other than components (A) and (C). <18> The component (A) in the composition (I) preferably contains trimethylsiloxysilicate and one or more selected from the group consisting of (acrylates / dimethicone) copolymer and (acrylates / polytrimethylsiloxy methacrylate) copolymer, and more preferably contains trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer. <17> How to use: <19> The total content of trimethylsiloxysilicate, (acrylates / dimethicone) copolymer, and (acrylates / polytrimethylsiloxy methacrylate) copolymer in the component (A) is preferably 50% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, still more preferably 90% by mass or more, still more preferably 95% by mass or more, and still more preferably 98% by mass or more, and is 100% by mass or less. <18> How to use: <20> The total content of trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer in the component (A) is preferably 50% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, still more preferably 90% by mass or more, still more preferably 95% by mass or more, still more preferably 98% by mass or more, and 100% by mass or less. <18> or <19> How to use:

[0100] <21> When the component (A) in the composition (I) contains trimethylsiloxysilicate and (acrylates / polytrimethylsiloxy methacrylate) copolymer, the mass ratio of trimethylsiloxysilicate to (acrylates / polytrimethylsiloxy methacrylate) copolymer [trimethylsiloxysilicate / (acrylates / polytrimethylsiloxy methacrylate) copolymer] is preferably 0.2 or more, more preferably 0.5 or more, even more preferably 0.8 or more, still more preferably 1.0 or more, still more preferably 1.1 or more, and is preferably 10 or less, more preferably 5.0 or less. <17> ~ <20> Use one of the following methods. <22> The poly(N-acylalkyleneimine)-modified organopolysiloxane in the component (A) of the composition (II) is preferably at least one selected from the group consisting of poly(N-formylethyleneimine)organopolysiloxane, poly(N-acetylethyleneimine)organopolysiloxane, and poly(N-propionylethyleneimine)organopolysiloxane [polysilicone-9], and more preferably poly(N-propionylethyleneimine)organopolysiloxane [polysilicone-9]. <16> ~ <21> Use one of the following methods. <23> In the composition (II), the content of the poly(N-acylalkyleneimine)-modified organopolysiloxane in the component (A) is preferably 50% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, still more preferably 90% by mass or more, still more preferably 95% by mass or more, still more preferably 98% by mass or more, and 100% by mass or less. <16> ~ <22> Use one of the following methods. <24> In the composition (I), the component (C) is preferably a dimethylpolysiloxane having a degree of polymerization of 650 or more, more preferably 650 or more and 20,000 or less, even more preferably 800 or more and 10,000 or less, still more preferably 1,200 or more and 4,500 or less, still more preferably 1,400 or more and 4,000 or less, still more preferably 1,900 or more and 4,000 or less, and still more preferably 2,200 or more and 3,900 or less. <17> ~ <23> Use one of the following methods. <25> In the composition (I), the component (D) preferably contains an aminopolyether-modified silicone, more preferably an aminopolyether-modified silicone having a polyoxyethylene group, further preferably contains one or more selected from the group consisting of (bisisobutyl PEG-15 / amodimethicone) copolymer and (bisisobutyl PEG-14 / amodimethicone) copolymer, and even more preferably contains (bisisobutyl PEG-15 / amodimethicone) copolymer. <17> ~ <24> Use one of the following methods. <26> The composition further comprises a pigment. <1> ~ <25> Use one of the following methods. <27> The content of the pigment in the composition is preferably 0.01% by mass or more and 30% by mass or less, more preferably 0.1% by mass or more and 20% by mass or less, even more preferably 0.5% by mass or more and 15% by mass or less, and still more preferably 1.0% by mass or more and 10% by mass or less. <26> How to use: <28> The composition further comprises a volatile solvent. <1> ~ <27> Use one of the following methods. <29> The volatile solvent is at least one selected from the group consisting of alcohol-based solvents, ether-based solvents, ketone-based solvents, ester-based solvents, hydrocarbon-based solvents, and silicone-based solvents, preferably at least one selected from the group consisting of alcohol-based solvents, hydrocarbon-based solvents, and silicone-based solvents, and more preferably ethanol, 1-propanol, 2-propanol, 1-butanol, 2-butanol, pentane, isopentane, hexane, isohexane, heptane, isoheptane, decane, isodecane, dodecane, isododecane, tridecane, isotridecane, tetradecane, isotetradecane, light liquid isoparaffin, a viscosity at 25° C. of 10 mm 2 Dimethylpolysiloxane, methyltrimethicone, and a viscosity of 20mm at 25°C or less 2 More preferably, the solvent is ethanol, isodecane, isododecane, isotetradecane, or light liquid isoparaffin; the viscosity at 25° C. is 5 mm 2 / s or less, and methyl trimethicone, and more preferably one or more selected from the group consisting of ethanol, isodecane, isododecane, isotetradecane, and light liquid isoparaffin, and even more preferably isododecane. <28> How to use: <30> The content of the volatile solvent in the composition is preferably 1% by mass or more and 98% by mass or less, more preferably 5% by mass or more and 95% by mass or less, even more preferably 10% by mass or more and 90% by mass or less, still more preferably 20% by mass or more and 80% by mass or less, still more preferably 30% by mass or more and 80% by mass or less, and still more preferably 40% by mass or more and 80% by mass or less. <28> or <29> How to use: <31> The water content in the composition is preferably less than 10% by mass, more preferably less than 8% by mass, even more preferably less than 6% by mass, even more preferably less than 5% by mass, even more preferably less than 3% by mass, and even more preferably less than 1% by mass. <1> ~ <30> Use one of the following methods. <32> The pH of the composition is preferably 3.0 to 10, more preferably 4.0 to 9.5, even more preferably 5.0 to 9.0, even more preferably 5.0 to 8.5, even more preferably 5.5 to 8.0, and even more preferably 6.0 to 7.5. <1> ~ <31> Use one of the following methods. <33> The composition is in the form of a liquid, paste, cream, gel, foam, spray, or wax; <1> ~ <32> Use one of the following methods. <34> The product form of the composition is a cleaning composition, a conditioning composition, a treatment composition (including a leave-in type), a styling composition, a dye composition, or a permanent composition, and is preferably a dye composition. <1> ~ <33> Use one of the following methods. <35> The composition is a leave-on type composition that is applied to a fiber for a headwear product and then dried without being washed off. <1> ~ <34> Use one of the following methods. <36> The fiber for headwear products is preferably a naturally derived fiber, more preferably a regenerated protein fiber, and even more preferably a regenerated collagen fiber. <1> ~ <35> Use one of the following methods. <37> The tensile modulus of the fiber for head accessories in water is preferably 0.5 GPa or more, more preferably 0.6 GPa or more, even more preferably 0.7 GPa or more, and is 10 GPa or less, preferably 5.0 GPa or less, more preferably 3.0 GPa or less, even more preferably 2.0 GPa or less, and even more preferably 1.0 GPa or less. <1> ~ <36> Use one of the following methods. <38> applying the composition to the headwear fabric and then drying; <1> ~ <37> Use one of the following methods. <39> The amount of the composition applied to the fiber for head decoration products is preferably 0.005 or more and 10 or less, more preferably 0.005 or more and 5 or less, even more preferably 0.01 or more and 3 or less, still more preferably 0.01 or more and 2 or less, and even more preferably 0.05 or more and 1 or less, as a mass ratio of the composition to the fiber for head decoration products (composition / fiber for head decoration products). <1> ~ <38> Use one of the following methods. <40> After applying the composition, the headwear fabric is dried without rinsing with water. <38> or <39> How to use:

[0101] <41> The treatment includes applying the composition to the headwear fabric in a state where the headwear fabric is worn on the head. <1> ~ <40> Use one of the following methods. <42> The treatment includes applying the composition to the headwear fabric when not being worn on the head. <1> ~ <40> Use one of the following methods. <43> The step of applying the composition to the headwear fiber is repeated at least two times, preferably at most ten times, more preferably at most five times. <41> or <42> How to use: <44> The treatment of the fiber for headwear products is the following method (1) or (2), preferably method (2): <1> ~ <43> Use one of the following methods. (1) A method comprising the steps of: wearing a fiber for head accessories on the head; and applying the composition to the fiber for head accessories while it is being worn on the head, in that order. (2) A method comprising a step of applying the composition to a headwear fabric that is not worn on the head. <45> In the method (1), the step of applying the composition to the fiber for head accessories is carried out two or more times while the fiber for head accessories is worn on the head while checking the finished state. <44> How to use: <46> The method of (2) further includes, after the step, a step of wearing the fiber for head accessories on a head, a step of removing the fiber for head accessories from the head, and a step of applying the composition to the fiber for head accessories in a state where the fiber is not worn on the head. <44> How to use: <47> In the method (2) above, a cycle of a step of attaching the fiber for head accessories to a head, a step of removing the fiber for head accessories from the head, and a step of applying the composition to the fiber for head accessories not attached to the head is performed 1 to 9 times, preferably 1 to 4 times. <46> How to use: <48> The treatment is a dyeing treatment of the fiber for headwear products. <1> ~ <47> Use one of the following methods. <49> The composition contains 8.0% by mass of trimethylsiloxysilicate, dimethylpolysiloxane (viscosity at 25°C of 20 million mm 2 / s) 4.0 mass%, and a composition other than the composition consisting of isododecane, <1> ~ <48> Use one of the following methods. <50> A method for dyeing fibers for head accessories, comprising a step of applying a composition containing a film-forming agent (A), a penetration enhancer (B) content of 24 mass% or less, and a pH of 10 or less, to fibers for head accessories having a tensile modulus in water of 0.4 GPa or more. <51> Use of a composition containing a film-forming agent (A), with a penetration enhancer (B) content of 24 mass% or less and a pH of 10 or less, as a treatment agent for fibers for head accessories having a tensile modulus in water of 0.4 GPa or more. <52> A treatment composition for fibers for headwear products, comprising a film-forming agent (A), a penetration enhancer (B) content of 24 mass% or less, a pH of 10 or less, and a tensile modulus in water of 0.4 GPa or more. <53> The composition contains 8.0% by mass of trimethylsiloxysilicate, dimethylpolysiloxane (viscosity at 25°C of 20 million mm 2 A composition excluding a composition consisting of 4.0% by mass of / s) and isododecane, a dyeing method of <50>, a use of <51>, or a treatment composition of <52>.

Examples

[0102] Hereinafter, the present invention will be described with reference to examples, but the present invention is not limited to the scope of the examples. In these examples, various measurements and evaluations were performed by the following methods.

[0103] <pH Measurement> Using a pH meter (F-72, manufactured by Horiba, Ltd.), the pH of the composition at 30 °C was measured.

[0104] <Tensile Elastic Modulus of Fibers for Headgear Products in Water> Ten fibers were cut from the base of the headgear product. A total of 10 fiber pieces, each 3 cm long, were collected from near the middle of the base and the tip of each fiber. These fiber pieces were set in an automatic fiber tensile tester ("MTT690" manufactured by DIA-STRON limited). After leaving the fiber pieces immersed in water at 20 °C for 30 minutes, automatic measurement was started, and the load and strain amount when the fiber pieces were stretched and broken while immersed in water were measured. The tensile elastic modulus of the fiber pieces in water was calculated from the slope of the stress-strain straight line after converting the load into stress based on the following formula. Stress σ (GPa) = Load (N) / Cross-sectional area of fiber (mm 2 ) / 1000 Cross-sectional area of fiber (mm 2 ) was measured and calculated using a laser diameter measuring device ("FDAS770" manufactured by DIA-STRON limited) for the fiber diameter of the dried fiber standing still in an environment of 20 °C and 65% RH.

[0105] <Preparation of Fiber Bundle for Evaluation> Using the fibers for headgear products used in each example, a fiber bundle with a length of 10 cm and a mass of 2 g was prepared. After washing the fiber bundle with a plane shampoo having the following composition, it was rinsed with warm water at 40 °C and dried thoroughly to obtain a fiber bundle for evaluation.

[0106] (Plain Shampoo Composition) Ingredient (mass%) Sodium polyoxyethylene (2) lauryl ether sulfate (*1) 15.5 Lauric acid diethanolamide (*2) 1.5 EDTA tetrasodium salt 0.3 Sodium benzoate 1.43 Purified water Remaining amount Total 100.0 *1: 57.4% by weight of Emeral 227 (manufactured by Kao Corporation, active ingredient 27% by weight) *2: Aminone L-02 (Kao Corporation)

[0107] Example 1 (Treatment and evaluation of fibers for headwear products) The fiber bundles for evaluation were prepared using regenerated collagen fibers having the tensile modulus shown in the table as fibers for head ornament products. The components shown in Table 1 were blended in the blending ratios shown in the table and mixed until uniform to prepare a composition (stain composition). After the fiber bundle for evaluation was placed on the head of the subject, 0.4 g of the composition was applied. Then, hot air was applied from a position 18 cm away from the fiber bundle for 30 seconds using a dryer. Further, the fiber bundle was dried by applying hot air from the dryer while combing for 30 seconds, and fiber treatment was performed. After the treatment, the fiber bundle was removed from the head and evaluated by the following methods. The results are shown in Table 1.

[0108] <Stainability> The dyeability of the treated fibers was evaluated by five expert panelists according to the following criteria. The results are shown in Table 1. A: Good dyeability. B: Dyeability is slightly insufficient. C: Insufficient staining.

[0109] <Combing of fibers after three washes after treatment> After the treatment, the fibers were washed and dried three times, and then the combability of the fibers was evaluated by five expert panelists using a ring comb according to the following criteria. The results are shown in Table 1. All of the fibers before treatment were rated "A" for combability. A: Easy to comb. B: Slightly difficult to comb. C: Combing is difficult.

[0110] <Ideal Finish> Regarding the ideal finish, which is influenced by the color balance between the treated fibers and the natural hair (head hair), five expert panelists conducted a sensory evaluation according to the following criteria. The results are shown in Table 1. A: The color balance is good and the finish is ideal. B: The color balance is slightly off, falling short of the ideal finish. C: The color balance is poor and the result is not ideal.

[0111] <Reduced risk of skin coloration and scalp irritation> Regarding coloring and irritation to the scalp, a sensory evaluation was performed by five expert panelists according to the following criteria. The results are shown in Table 1. A: There is no skin staining and no scalp irritation. B: There is some skin discoloration or some scalp irritation. C: Skin staining and scalp irritation.

[0112] <Achieving the ideal finish while reducing the risk of skin coloration and scalp irritation> A sensory evaluation was conducted by five expert panelists using the following criteria to determine whether the ideal finish could be achieved while reducing the risk of skin coloration and scalp irritation. The results are shown in Table 1. A: The color balance is good and the finish is ideal, and it does not stain the skin or irritate the scalp. B: The color balance is good and the finish is ideal, but there is some skin coloring or some scalp irritation. Or, the color balance is slightly poor and the finish is slightly short of the ideal, but there is no skin coloring and no scalp irritation. C: The color balance is poor, the finish is not ideal, there is skin coloring, and scalp irritation is felt.

[0113] Comparative Example 1 Except for using regenerated collagen fibers having the tensile modulus shown in the table as the fibers for the head ornament product, the fibers were treated and evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0114] Example 2 After preparing the composition in the same manner as in Example 1, 0.4 g of the composition was applied to the subject's head without placing the fiber bundle for evaluation on the subject's head, and then hot air was blown from a dryer at a position 18 cm away from the fiber bundle for 30 seconds. The fiber bundle was then dried by blowing hot air from the dryer while combing for 30 seconds, thereby carrying out fiber treatment. The treated fiber bundle was evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0115] Example 3 After the fiber treatment was performed in the same manner as in Example 2, the treated fiber bundle was attached to the subject's head to check the dyed state, and then the fiber bundle was removed from the subject's head. 0.4 g of the composition was applied to the fiber bundle again in the same manner as above, and then hot air was applied to the fiber bundle from a position 18 cm away from the fiber bundle for 30 seconds using a dryer. The fiber bundle was attached to the subject's head again to check the dyed state. The treated fiber bundle was evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0116] [Table 1]

[0117] The ingredients shown in the table are as follows. Note that the blending amounts (mass%) shown in the table are all the amounts of active ingredients. *1: X-21-5595, manufactured by Shin-Etsu Chemical Co., Ltd., a solution of trimethylsiloxysilicate (60% by mass) in isododecane *2: DOWSIL FA 4004 ID Silicone Acrylate, manufactured by Dow Toray Co., Ltd., (acrylates / polytrimethylsiloxy methacrylate) copolymer (40% by mass) solution in isododecane *3: Silsoft B3020, Momentive Performance Materials, dimethylpolysiloxane, viscosity at 25°C: 20 million mm 2 / s(degree of polymerization 3,546) *4: DOWSIL SS-3588 Fluid, manufactured by Dow Toray Co., Ltd., ethanol solution of (bisisobutyl PEG-15 / amodimethicone) copolymer (80% by mass) *5: Marukasol R, Maruzen Petrochemical Co., Ltd., Isododecane

[0118] With regard to the degree of polymerization (P) of the above component *3, the molecular weight (M) is calculated from the viscosity (η) using the above formula (4), and the degree of polymerization (P) can be calculated from the following formula (5) since the molecular weight of the base unit of dimethylpolysiloxane is 74. P=M / 74 (5)

[0119] From Table 1, it can be seen that when the method of the present invention is used, the treated fibers for head ornament products have good dyeability, and damage to the fibers due to repeated washing after the treatment is also suppressed. Table 1 also shows the evaluation results for three items: (1) ideal finish, (2) reduced risk of skin coloring and scalp irritation, and (3) achieving both an ideal finish and reduced risk of skin coloring and scalp irritation. In Example 1, the composition is applied to fibers for a head accessory product worn on the head, and since it is easy to approach the ideal finish, (1) ideal finish is rated "A." On the other hand, since the composition is applied to fibers for a head accessory product worn on the head, (2) reduced risk of skin coloring and scalp irritation is rated "B." In Example 2, the composition was applied to fibers for head accessories that were not being worn on the head, so (1) the ideal finish was rated a "B"; however, the risk of skin coloring and scalp irritation was low, so (2) the reduction in the risk of skin coloring and scalp irritation was rated an "A." In Example 3, the composition was applied to the fiber for a head accessory product that was not attached to the head, then the fiber was attached to the head once to check the finish, and then the treated head accessory was removed from the head and the composition was applied again. Therefore, it is easy to achieve an ideal finish and the risk of skin coloration and scalp irritation is reduced, so (1) to (3) are all rated "A". [Industrial Applicability]

[0120] According to the present invention, there is provided a method for using a composition for treating fibers for head ornament products, which, when used in the dyeing treatment of fibers for head ornament products that meet certain requirements, provides good dyeability for the fibers and suppresses damage to the fibers due to repeated washing after the dyeing treatment, and further provides a method which makes it possible to achieve both an ideal finish and a reduced risk of skin coloration and scalp irritation.< / ph>

Claims

1. A method for using a composition comprising a film-forming agent (A), a penetration enhancer (B) content of 24 mass% or less, and a pH of 10 or less, for treating fibers for head accessories having a tensile modulus in water of 0.4 GPa or more.

2. The method of claim 1 , wherein the treatment comprises applying the composition to the headwear fabric while it is worn on the head.

3. The method of claim 1 , wherein the treatment comprises applying the composition to the headwear fabric when not worn on the head.

4. The method according to claim 2 or 3, wherein the step of applying the composition to the headwear fiber is repeated two or more times.

5. The method according to any one of claims 1 to 4, wherein the film-forming agent (A) comprises a silicone-based polymer.

6. The method according to any one of claims 1 to 5, wherein the penetration enhancer (B) is at least one member selected from the group consisting of alkylene carbonates, aromatic ring-containing alcohols, and lactones.

7. The method for use according to any one of claims 2 to 6, wherein the fiber for headwear after application of the composition is dried without rinsing with water.

8. The use according to any one of claims 1 to 7, wherein the composition further comprises a pigment.

9. The method according to any one of claims 1 to 8, wherein the treatment is a dyeing treatment of the fiber for head accessories.

10. A method for dyeing fibers for head accessories, comprising a step of applying a composition containing a film-forming agent (A), a penetration enhancer (B) content of 24 mass% or less, and a pH of 10 or less to fibers for head accessories having a tensile modulus in water of 0.4 GPa or more.

Citation Information

Patent Citations

  • Hair cosmetic

    JP2002097122A