AI Technical Summary
Existing methods for recycling polyester fibers struggle to produce high-quality fibers with mechanical properties and color tone comparable to virgin materials, while also facing issues of fiber fluff and process inefficiencies, especially in mass production and long-term production stability.
The use of a polyester resin composed mainly of recovered polyester with polymethaxylylene adipamide (MXD6) and controlled inorganic impurities, along with specific processing conditions, to create recycled polyester fibers that maintain mechanical properties and color tone, suitable for sportswear and sewing threads, without requiring special equipment or high costs.
The solution enables the production of recycled polyester fibers with improved mechanical properties and color tone comparable to virgin materials, suitable for sportswear and sewing threads, while ensuring low fiber fluff and efficient mass production with reduced chemical cleaning time and improved process passability.
Abstract
Description
Recycled polyester fiber The present invention relates to recycled polyester fibers. Specifically, it can be applied not only to knitted fabrics that make up sportswear but also to sewing threads used for sewing, and relates to recycled polyester fibers that can be developed for sportswear that requires a color tone comparable to virgin raw materials. Polyester is used in various applications such as clothing, materials, and medical due to its useful functionality such as mechanical properties, heat resistance, and moldability. Among them, polyethylene terephthalate is excellent in terms of versatility and practicality and is preferably used. These polyester products are discarded after use. However, when incinerated, high heat is generated during combustion, and in a normal incinerator, the furnace is easily damaged, and a special incinerator with excellent high-temperature durability is required. Also, when discarded without incineration, since it is difficult to decompose by decay, it remains as waste semi-permanently, and problems such as animals accidentally eating it and dying occur, so improvement is required in terms of environmental protection. In view of such a situation, from the aspects of resource reuse and sustainable environmental protection, in order to recover and reuse discarded polymer products, mainly polyethylene terephthalate, which has a large usage amount and is expected to increase in the future, recycling attempts have been actively carried out in recent years, such as remelting and pelletizing molded products including used edible liquid bottles (PET bottles) and then making them into fibers, films, and molded products again. However, the recycled polyester recovered contains polymers of various forms and various degrees of polymerization, such as containers, clothing polyester, industrial waste polyester, or defective products or waste polyester generated in various processes for manufacturing fibers, films, and other molded products. Since these mixed polymers are melt-mixed, the resulting recycled polyester has the problem of being prone to dullness and coloring. In addition, when the obtained recycled polyester, for example, the recycled polyester formed into pellets is spun and fiberized, impurities such as additives and foreign matters contained in the polyester, and further metals and glass that are mixed in without being separated during recovery cause the filter on the back of the nozzle to become clogged quickly during melt spinning, the back pressure rises rapidly, and long-term operation becomes difficult. On the other hand, if the pore size of the filter is increased to ensure long-term operability, yarn breakage frequently occurs in the spinning or drawing process, and the operability deteriorates. Therefore, it has been difficult to obtain recycled polyester fibers with excellent mechanical properties and processability from the recovered polyester. In response to the above problems, improving the quality of the polyester to be recycled and improving the processes of the recycling process are considered the simplest and most effective means that also contribute to quality improvement, color tone improvement, and further improvement of processability, and several proposals have been made so far. Regarding quality improvement, for example, an invention related to a modified polyester resin in which a polyethylene terephthalate resin is reacted with one or more polymers selected from the group consisting of polymers having an amide bond, polymers having a urethane bond, polymers having a urea bond, and polymers having a π bond and a terminal amine in the main chain, and the residual elongation rate represented by the ratio of the elongation after crystallization to the elongation before crystallization of the polyester resin is 50% or more has been proposed (see Patent Document 1). It is described that a modified polyester resin and a polyester resin molded product capable of maintaining the extensibility without a significant decrease in elongation even after crystallization can be obtained. Regarding color tone improvement, it is mainly a polyester filament obtained by spinning and drawing using recovered polyester as a starting material, containing at most 5% by weight of organic and / or inorganic impurities, and in addition to a specific elongation and the difference between the maximum and minimum values of the number average molecular weight, the stress at 10% elongation is 3.0 to 3.9 g / d, and an invention related to a recovered polyester filament in which the standard deviation at that time is defined has been proposed (see Patent Document 2). It is described that a polyester fiber product for clothing exhibiting a natural unevenness similar to natural fibers can be obtained. In addition, regarding quality and color tone improvement, there is an invention related to a recycled polyester using polyester A for reproduction with a b value in the color tone of 4 to 15 and polyester B for reproduction with a b value in the color tone of less than 4 as raw materials, wherein the weight ratio of polyester A to polyester B is 20 / 80 to 70 / 30, the content of sulfur-containing sodium aluminosilicate is 30 to 200 ppm, the limiting viscosity is 0.5 or more, and the b value in the color tone is 3 or less (see Patent Document 3). It is described that a recycled polyester with little viscosity reduction and good color tone can be obtained despite using waste-recovered polyester as a raw material. Japanese Patent Application Laid-Open No. 2011-246665, Japanese Patent Application Laid-Open No. 2000-212832, Japanese Patent Application Laid-Open No. 2000-63557 As described above, various proposals have been made in the prior art. In the proposal of Patent Document 1, although there is a description of polymetaxylylene adipamide (MXD6) as in the present invention, it is only cited as an example of a polymer. That is, as can be seen from the description of a polyester resin modified by reacting with various polymers, the invention described in Patent Document 1 aims to lower the crystallinity and obtain stretchability by copolymerizing the polymer, and does not have a fiber design like the present invention that suppresses the loss of toughness when made into a fiber product by adding a specific polyamide resin as an additive. Also, as a spun processed product, although there are descriptions of fibers and clothes, there is no description in the examples, and there is no suggestion that it is a technology for obtaining high-quality fiber products. The proposal of Patent Document 2 defines the amount of foreign matter as in the present invention, but its purpose is to exhibit a natural unevenness similar to natural fibers due to foreign matter. From the fact that the stress at 10% elongation described in Claim 1 is 3.0 to 3.9 g / d, it could never be applied to a sewing thread that requires high mechanical properties for sewing fiber products. In addition, the proposal in Patent Document 3 defines the b value in the color tone as in the present invention, focuses on suppressing the decrease in viscosity to suppress the deterioration in quality, and aims to reinforce the resin by adding 30 to 200 ppm of sulfur-containing sodium aluminosilicate. At first glance, it may be considered possible to obtain a fiber product that combines high quality and good color tone as in the present invention. However, sulfur-containing sodium aluminosilicate is a particle, and in applications that require stretching and thinning like fiber products, the additive becomes a stretching inhibitor particle rather than playing a role in resin reinforcement, greatly impairing the expression of mechanical properties and resulting in the problem that high-quality fiber products cannot be obtained. As described above, in the conventional technology, when the recycled polyester is fiberized, it has not been possible to simultaneously satisfy mass production that exhibits excellent mechanical properties, has a color tone comparable to that of virgin raw materials, is low-cost, and maintains a state with few fiber flyings during long-term production. An object of the present invention is to solve the problems of the above-described conventional technology, and it can be applied not only to knit fabrics constituting sportswear but also to sewing threads used for sewing, and can be developed for sports uniforms that require a color tone comparable to that of virgin raw materials. Moreover, the present invention provides a recycled polyester fiber that can be mass-produced at low cost while maintaining a state with few fiber flyings during long-term production without requiring special devices and equipment. The present invention aims to achieve the above problems, and includes a polyester resin mainly composed of recycled polyester and poly(m-xylylene adipamide) (MXD6). The content of the poly(m-xylylene adipamide) (MXD6) is 0.01 to 1% by weight when the total weight of the recycled polyester fiber is 100% by weight, and the L value is 70 to 100 and the b value is -5 to 5. It is a recycled polyester fiber characterized by this. In the recycled polyester fiber of the present invention, the polyester resin contains inorganic impurities (excluding titanium compounds and dyes and pigments for coloring) in an amount of 0.1 to 5% by weight in terms of ash content when the total weight of the polyester resin is 100% by weight, the recycled polyester fiber of the present invention has a functional group that can be dyed with a cationic dye, and the recycled polyester is derived from a beverage bottle, which are respectively preferable conditions. According to the present invention, it is possible to apply not only to the knitted fabric constituting sportswear but also to the sewing thread used for sewing, and a recycled polyester fiber capable of being developed into a sports uniform that requires a virgin raw material-like color tone can be obtained. Further, the knitted fabric and the sewing thread for sewing can be composed of the recycled polyester fiber of the present invention, and a product made of 100% recycled polyester fiber can be obtained. Furthermore, according to the present invention, the recycled polyester fiber can be mass-produced at low cost while maintaining a state with few fiber fuzzes during long-term production. The recycled polyester fiber of the present invention will be specifically described. The recycled polyester fiber of the present invention contains a polyester resin mainly composed of recycled polyester and polymetaxylylene adipamide (MXD6), and the content of the polymetaxylylene adipamide (MXD6) is 0.01 to 1% by weight when the total weight of the recycled polyester fiber is 100% by weight, and is characterized in that the L value is 70 to 100 and the b value is -5 to 5. As the recycled polyester for forming the recycled polyester fiber of the present invention (hereinafter, may be simply referred to as "fiber"), containers and clothing polyesters recycled for the purpose of resource recycling, industrial waste polyesters, or defective products or waste polyesters generated in various processes for manufacturing fibers, films and other molded products are used. Among them, when a PET bottle, which is a polyester container, particularly a beverage PET bottle, is used as the recycled polyester, compared with the resin for general clothing fibers, the degree of polymerization is high, and when regenerated into fibers, even if it is heated and melted, mechanical properties such as fiber strength required for clothing fibers are likely to be stable, which is preferable. In addition, companies handling products made from recycled raw materials such as the recycled polyester fibers of the present invention are, in principle, certified with the GRS (Global Recycle Standard). With this GRS, since the details of the recycled raw materials being used are disclosed in a list, it is possible to distinguish between the recycled polyester and virgin raw material polyester from the information in said list. Moreover, the recycled polyester forming the recycled polyester fibers can employ any recycling method such as material recycling (mechanical recycling, feedstock recycling) within a range that does not inhibit the effects of the present invention. However, since the heat history during remelting is relatively short and it is possible to suppress dullness and coloring due to heat, it is preferable to use a mechanical recycling method among material recycling methods. The polyester resin having the recycled polyester as a main component (hereinafter, may be simply referred to as "polyester resin" or "resin") preferably contains inorganic compounds other than titanium compounds and dyestuffs for coloring purposes (in this specification, also referred to as "inorganic impurities (excluding titanium compounds and dyestuffs for coloring purposes)" or "inorganic impurities") in an ash content of 0.1 to 5% by weight, more preferably 0.1 to 3% by weight, based on 100% by weight of the total weight of the resin. By setting the inorganic impurities within such a range, it is possible to shorten the chemical cleaning time in the cleaning step in the recycling process (raw material acceptance, sorting, pulverization (flaking), flake cleaning, pelletization) of the recycled polyester, and while removing foreign matter of coarse particles, it is possible to suppress polymer yellowing due to long-term treatment with chemicals, so that a color tone suitable for sports uniforms is easily obtained. Note that the ash content of the inorganic impurities (excluding titanium compounds and dyestuffs for coloring purposes) in the polyester resin can be determined by the method described later. In addition, within a range that does not inhibit the effects of the present invention, separately from the inorganic impurities, a titanium compound can be further contained as a matting agent. In this case, titanium oxide is preferable considering both cost and matting effect. The greatest feature and important requirement of the present invention is that the recycled polyester fiber of the present invention contains 0.01 to 1% by weight of polymetaxylylene adipamide (MXD6) based on 100% by weight of the total weight of the fiber, and 0.01 to 0.8% by weight is suitable for the manifestation of mechanical properties during fibrillation. Although the exact reason is not yet clear at present, it is considered as follows. When polymetaxylylene adipamide (MXD6) in the recycled polyester fiber is contained within the above range, thermal decomposition does not occur even when the recovered polyester is melted due to the high heat resistance peculiar to polymetaxylylene adipamide (MXD6). Also, since MXD6 has properties similar to those of polyester resin (specific gravity 1.21 g / cm 3 , melting point 237 °C, etc.), it can be uniformly distributed in the polymer and create free volume while forming a stacking structure with the polyester resin. It is considered that this improves the fluidity of the polyester resin and suppresses the inhibition of drawability by foreign substances, thereby exhibiting high mechanical properties. Hitherto, in order to enhance the mechanical properties of recycled polyester fibers, for example, strength, attention has been paid to foreign substances as in Patent Document 2, and efforts have been simply focused on reducing the amount of foreign substances. However, in order to reduce the amount of foreign substances, it is necessary to perform chemical cleaning for an extremely long time until fine particles are removed in the cleaning process in the recycling process, and polymer decomposition occurs in parallel with the removal of foreign substances, resulting in deterioration of color tone such as dullness and coloring. On the other hand, the present inventors focused on the properties of the molecular chains in order to simultaneously satisfy the improvement of contradictory mechanical properties and color tone in recycled polyester fibers, and as a result of analysis, it was clarified that particles derived from foreign substances inhibit the continuity of the molecular chains and also inhibit the orientation of the molecular chains in the drawing process, which is the main cause of the decrease in strength. That is, it was concluded that ensuring the continuity of the molecular chains and the orientation during drawing is effective for improving the mechanical properties. The present invention has found a method to simultaneously achieve color tone improvement while satisfying the improvement of mechanical properties through intensive study based on this analysis. In addition, when the content of polymetaxylylene adipamide (MXD6) is less than 0.01% by weight based on 100% by weight of the total weight of the recycled polyester fiber, the stacking structure with the polyester resin is not sufficiently formed, the free volume is small, and the mechanical properties are deteriorated. On the other hand, when it exceeds 1% by weight, a stacking structure is formed between polymetaxylylene adipamide (MXD6) molecules, resulting in a decrease in free volume and deterioration of mechanical properties. The number average molecular weight of the polymetaxylylene adipamide (MXD6) used in the present invention is preferably from 10,000 to 50,000, more preferably 15,000 or more, still more preferably 20,000 or more. Also, more preferably 45,000 or less, still more preferably 40,000 or less. When the number average molecular weight satisfies the range of 10,000 to 50,000, uniform compatibility is easily obtained during melt kneading with the polyester resin, and the fiber formability is good. The number average molecular weight of the polymetaxylylene adipamide (MXD6) is calculated from the following formula. Number average molecular weight = 2 × 1,000,000 / ([COOH] + [NH 2 ) In addition, the polymetaxylylene adipamide (MXD6) used in the present invention can be used as a copolymerization component with diamine components, dicarboxylic acid components, lactams such as ε-caprolactam and laurolactam, and aliphatic aminocarboxylic acids such as aminocaproic acid and aminoundecanoic acid, as long as the effects of the present invention are not impaired. In the recycled polyester fiber of the present invention, in order to obtain excellent mechanical properties as a sewing thread for sewing, the degree of polymerization of the polyester resin mainly composed of the recycled polyester is preferably high. At a temperature of 25 ° C., the relative viscosity ηr of an 8 wt / vol% orthochlorophenol solution is measured using an Ostwald viscometer, and the intrinsic viscosity (IV) obtained is preferably from 0.55 to 1.10. In addition, the recycled polyester fiber of the present invention preferably has a functional group that can be dyed with a cationic dye. That is, it is preferable that the polyester resin mainly composed of the recycled polyester has a functional group that can be dyed with a cationic dye. Specifically, the polymer constituting the polyester resin may have the functional group (feedstock recycling method), or the functional group may be added by kneading another component having the functional group into the polyester resin (mechanical recycling method). Examples of the functional group include a sulfonic acid group, a carboxylic acid group, and a phosphoric acid group. Known techniques can be adopted for imparting the functional group. In the mechanical recycling method, for example, it is preferable to add a sodium naphthalene sulfonate formalin condensate when melting the recycled polyester. In the feedstock recycling method, for example, after depolymerizing the recycled polyester with ethylene glycol, it is a preferable embodiment to copolymerize and repolymerize an isophthalic acid component containing a metal sulfonate group. By imparting such functionality, it is possible to obtain a cation-dyeable recycled polyester fiber having excellent high color development when dyed with a cationic dye in a recycled polyester fiber having a color tone close to that of a virgin raw material as in the present invention. The total fineness of the recycled polyester fiber of the present invention is preferably 50 to 4,000 dtex, more preferably 50 to 2,000 dtex. When the total fineness satisfies the range of 50 to 4,000 dtex, it is possible to obtain uniform cooling properties in the cooling process after spinning in long-term production while maintaining the productivity per unit time, so that mass production can be carried out with few flyings. The total fineness of the fiber refers to the value measured by the measurement method described later. The recycled polyester fiber of the present invention needs to have an L value in the range of 70 to 100. When the L value satisfies 70 to 100, a whiteness suitable for sports uniforms is exhibited. When the L value is less than 70, the color tone becomes dark and it cannot be said to be a color tone like that of a virgin raw material. Since the L value exceeding 100 exceeds the upper limit value of the measuring instrument, it is theoretically impossible to satisfy. In addition, the recycled polyester fiber of the present invention must have a b value in the range of -5 to 5, preferably -5 to 4, and particularly preferably -5 to 3. When the b value satisfies -5 to 5, a color tone like that of virgin raw materials is exhibited. When the b value is less than -5, the blue tint becomes stronger and the expressiveness of warm colors during dyeing deteriorates. When the b value exceeds 5, the yellowness is strong and it is unsuitable for sportswear. The L value and b value refer to the values measured by the measurement methods described below. The recycled polyester fiber of the present invention preferably has a breaking strength in the range of 2.0 to 9.0 cN / dtex, more preferably 3.5 cN / dtex or more, and still more preferably 8.5 cN / dtex or less. When the breaking strength satisfies the range of 2.0 to 9.0 cN / dtex, it is applicable not only to the knitted fabric constituting sportswear but also to the sewing thread used for sewing, and a product using 100% recycled polyester fiber can be obtained. The breaking strength of the fiber is synonymous with the linear strength and refers to the value measured by the measurement method of the linear strength described below. In addition, the recycled polyester fiber of the present invention preferably has a shrinkage rate in dry heat at a temperature of 150°C of 1 to 15%, more preferably 2% or more, and still more preferably 12% or less. Setting the shrinkage rate due to dry heat at 150°C within the above range is suitable because it leads to good processability during processing into fiber products and maintenance / improvement of the dimensional stability of the products. The shrinkage rate of the fiber refers to the value measured by the measurement method described below. Next, the manufacturing method of the recycled polyester fiber of the present invention will be described. The manufacturing method preferably employs polyethylene terephthalate melt spinning that can obtain recycled polyester pellets by applying a known recycling process of recycled polyester and enables mass production while maintaining a state with less hairiness at low cost and in long-term production. Next, an example will be described. The recycled polyester suitably used in the present invention is derived from beverage bottles. That is, it is polyester recycled from beverage PET bottles. As the polyester recycled from beverage PET bottles, those in the form of flakes (sheet-like) are preferred, and flakes obtained by sorting, crushing, chemically washing, rinsing, dehydrating, and drying the recycled used PET bottles can be suitably used. Next, using the obtained flakes as raw materials, recycled polyester fibers are produced through a solid-phase polymerization process, a pelletizing process, and a fiber spinning process as required. The details of each process will be described below. The recovered shape of the PET bottle can be any shape such as bale shape or bottle shape. If transportation efficiency is prioritized, the bale shape is preferred, and if high quality is prioritized, the bottle shape is suitable. The recovered used PET bottles are sorted in the sorting process using known sorting techniques such as optical sorting machines and manual sorting, separated from other resin bottles, colored bottles, etc., and the caps and labels are also sorted together. In the sorting process, it is preferable to wash the sorted PET bottles once with water or warm water while still in the bottle shape to remove the surface dirt of the PET bottles, but it may be determined whether it is necessary to carry out according to the dirt condition of the recovered PET bottles. Next, after removing metals such as aluminum with a metal detector, it is crushed into flakes of the target size in the crushing process. In the crushing, known crushing techniques can be used, but wet crushing using water is preferred to suppress the frictional heat during crushing. Next, in the washing process, the flakes obtained by crushing the PET bottles are washed using an aqueous solution of an alkali metal hydroxide as chemical washing. As the aqueous solution of the alkali metal hydroxide used in this washing process, an aqueous solution of potassium hydroxide and an aqueous solution of sodium hydroxide are preferred. In such a washing process, preliminary washing may be carried out before washing with the aqueous solution of the alkali metal hydroxide. The concentration of the aqueous solution of the alkali metal hydroxide used in the washing process depends on conditions such as washing time, temperature, and agitation. Usually, it is 0.5 to 10% by weight, preferably 1 to 5% by weight. Also, the washing time of the washing process in which the flakes formed by crushing the PET bottle come into contact with the aqueous solution of the alkali metal hydroxide is usually 5 to 120 minutes, preferably 10 to 60 minutes, more preferably about 20 to 40 minutes. Such a washing process is preferably carried out with agitation. In such a washing process, at least a part of the surface of the flakes formed by crushing the PET bottle is hydrolyzed by the aqueous solution of the alkali metal hydroxide. As a result, impurities adhering to or impregnated in the surface of the flakes, non-volatile substances such as salts impregnated in the surface, and fine solid foreign matters biting into the surface, which cannot be removed by water washing or surfactant washing, can be highly washed and removed. Such a washing process is desirably carried out under conditions where 0.1 to 5% by weight, preferably 0.5 to 3% by weight, of the flakes to be washed is hydrolyzed. By controlling the conditions of the washing process in this way, while removing foreign matter of coarse particles, yellowing of the polymer due to long-term treatment with chemicals can be suppressed, so that a color tone such as that of the present invention suitable for sports uniforms can be easily obtained. Also, in the washing process, it is desirable to perform rinsing, dehydration, and drying following the washing with the aqueous solution of the alkali metal hydroxide. The flakes washed in this way can be subjected to a solid-phase polymerization process as needed. In the solid-phase polymerization process, the flakes washed in the washing process can be continuously solid-phase polymerized by contacting them with an inert gas at 180 to 230°C, preferably 190 to 230°C. As the inert gas, any gas having no reactivity can be used under the conditions of contacting with the washed flakes. Specifically, nitrogen gas, noble gases, etc. can be mentioned. Among these, using nitrogen gas is particularly preferable in consideration of the production cost. By subjecting to the solid-phase polymerization process, the degree of polymerization of the resin can be improved, adjusted to an appropriate degree of polymerization for fiber production, and a part of the volatile components contained as impurities in the flakes can be removed. Next, the flakes obtained in the above process are subjected to a pelletizing process. The pelletizing process can be carried out by melting and granulating the flakes using an extruder having a devolatilization means and a filtration means. As a means of incorporating poly(m-xylylene adipamide) (MXD6) in an amount of 0.01 to 1% by weight when the total weight of the fiber is 100% by weight as in the present invention, it is preferable to add it either in the pelletizing process or in the fiber spinning process. However, in the fiber spinning process, since it is necessary to supply it to a blending device while contacting with an inert gas, the process becomes complicated. Therefore, it is desirable to add it in the pelletizing process. The addition in the pelletizing process is carried out by melt-kneading poly(m-xylylene adipamide) (MXD6) weighed so as to be 0.01 to 1% by weight when the total weight of the flakes and the fiber is 100% by weight in the melting zone of the extruder, usually at 260 to 300 °C, preferably 265 to 280 °C. The extruder used in the pelletizing process preferably has at least one vacuum vent in the melting zone of the resin as a devolatilization means. The devolatilization of volatile substances in the molten resin is preferably carried out under a reduced pressure of usually 70 kPa or less, preferably 65 kPa or less, in a molten state by the vacuum vent. Volatile impurities in the resin can be strictly removed by such devolatilization in the molten state in the pelletizing process. Further, the extruder preferably has a filter capable of filtering and removing solid foreign matters having a particle size of 25 μm or more, preferably 15 μm or more, more preferably 10 μm or more in the molten resin as a filtration means. In the pelletizing process, it is desirable that solid foreign matters having a particle size of 25 μm or more, preferably 15 μm or more, more preferably 10 μm or more in the molten resin are filtered and removed from the resin. Although solid foreign matters in the resin are also removed in the above-described washing process, they can be removed more strictly by such filtration and removal. The molten resin from which volatile impurities and solid foreign matters have been sufficiently removed in this way can be granulated by extrusion molding into pellets of a desired shape and size by an extruder according to a conventional method to form pellets. Note that, as long as the extruder used in the pelletizing process is within the range where the pellets can be obtained, known extruders such as a single-screw extruder or a twin-screw extruder can be employed. The pellets obtained in the above process are subjected to a fiber spinning process. The polyester pellets obtained above are temporarily stored in a spinning hopper and supplied to a single-screw extruder type melt spinning apparatus for melt spinning. This molten polymer is metered by a gear pump to match the final fineness of the multifilament, then filtered by a metal nonwoven fabric filter in a spin pack, and extruded from a die. The fibers thus extruded are cooled and solidified by a cooling device and then produced by a direct spinning and drawing method of hot drawing. Details of each process of fiber spinning will be described below. The intrinsic viscosity (IV) of the polyester resin mainly composed of the recovered polyester used in the present invention is preferably in a specific range from the viewpoint of controlling the breaking strength and elongation of the raw yarn. In the case of the pellets described above, the intrinsic viscosity is preferably in the range of 0.60 to 1.2. The recycled polyester fiber of the present invention can be obtained by melting and kneading the polyester pellets filled in a hopper with a single-screw extruder in an inert gas nitrogen atmosphere, metering this molten polymer with a metering pump to match the final fineness of the multifilament, then introducing it into a spin pack and filtering it with a metal nonwoven fabric filter in the spin pack, and discharging it from a die. In addition to the above single-screw extruder, as long as the polyester fiber of the present invention can be obtained, it can be melt-kneaded with a twin-screw extruder, a pressure melter, a roll, a Banbury mixer, a kneader, etc. When adding the above-mentioned additives, etc., a method of directly mixing with an extruder or a method of preparing polyester pellets containing the additives, etc. at a high concentration in advance and blending the pellets before melting can be adopted. The melt spinning temperature can be appropriately changed according to the inherent viscosity, polymer type, etc., but it is preferably in the range of 270 to 330 °C. When such a temperature range is satisfied, sufficient fluidity can be obtained during polymer melting, quality variations can be reduced, and problems such as polymer decomposition do not occur, so it is suitable for the recycled polyester fiber of the present invention. Immediately below the spinneret, with the upper end being 0 to 15 cm from the spinneret surface, in accordance with the target mechanical properties of the raw yarn, the range from its upper end to 5 to 60 cm is surrounded by a heating cylinder and / or a heat-insulating cylinder, and after passing the spun yarn through an atmosphere heated to a temperature of 250 to 350 °C, it is preferably cooled and solidified with cooling air at a temperature of 10 to 80 °C, more preferably 15 to 50 °C. When such a range is satisfied, not only can cooling be achieved with a normal device without the need for a large cooling device, but also the single fibers during spinning are sufficiently and uniformly cooled, so the Uster yarn irregularity of the yarn becomes smaller, leading to stability in quality and grade, which is therefore preferable. Regarding the heating cylinder and / or the heat-insulating cylinder, there is no particular problem even if they are unused as long as the recycled polyester fiber as described in the present invention can be obtained. Such an air-cooling device can be of the horizontal blowing type (uniflow type) or the annular blowing type can also be used. Also, when a high cooling effect is required, such as for monofilaments, cooling methods such as water cooling or mist can be adopted. By undergoing such a temperature history, fibers having mechanical properties such as linear tensile strength suitable for sewing threads used in sewing can be produced with good quality. The cooled and solidified undrawn yarn is then applied with an oil agent by an oiling device. The oil agent can be either water-based or non-water-based. It is a preferred embodiment to use an oil agent composition mainly composed of a lubricant and containing components such as a surfactant, an antistatic agent, and an extreme pressure agent component, excluding components active to the polyester resin. For example, a non-water-based oil agent in which an alkyl ether ester is used as the lubricant component, an alkylene oxide adduct of a higher alcohol is used as the surfactant component, and an organic phosphate salt is used as the extreme pressure agent component and diluted with mineral oil is a more preferred embodiment. The undrawn yarn strip applied with the oil agent is wound around a take-up roll and taken up. The surface speed of the take-up roll, i.e., the take-up speed, is preferably 300 m / min or more, more preferably 500 m / min or more. When such a range is satisfied, the production efficiency is good and industrially stable, and polyester fibers such as those of the present invention can be produced. Also, since the cooling of the single fiber proceeds sufficiently, the Uster yarn stain of the yarn strip becomes small, and it is suitable because the deterioration of quality and grade can be suppressed. The undrawn yarn strip taken up at the above take-up speed may be subjected to normal heat drawing, and the draw ratio can be varied depending on the birefringence and drawing temperature of the undrawn yarn. However, after being wound up once, or without being wound up once, it is preferably heat-drawn continuously at a draw ratio of 1 to 6 times, more preferably 1.5 to 5.5 times. When the draw ratio is within such a range, stable yarn production is possible, and the resulting fibers have not only suitable strength and elastic modulus for not only knitted fabrics constituting sportswear but also sewing threads used for sewing, but also the frequency of single filament breakage of the fiber itself is reduced. Therefore, it is suitable for improving the yield in the weaving process and enabling the resulting final product to exhibit excellent performance. For example, as the drawing method, similar to the take-up roll (1GR), a Nelson type roll with two rolls as one unit is arranged side by side with the feed roll (2GR), the first draw roll (3GR), the heat set roll (4GR), and the relaxation roll (5GR), and the yarn strip is sequentially wound and heat-treated under the above conditions. At this time, the number of rolls and the heat treatment temperature on the rolls are not particularly limited. Normally, a prestretch treatment is performed between 1GR and 2GR to converge the yarn strip. The prestretch treatment in the present invention is different from the above-mentioned drawing, and aims to improve the convergence of the yarn strip and compensate for the insufficient yarn production tension due to the yarn strip shaking accompanying shrinkage during heat treatment, and is within a range that does not affect the strength and elongation characteristics of the polyester fibers of the present invention. The prestretch ratio is preferably in the range of 1 to 8% when the total draw ratio is 100%. 1GR is preferably heated to a temperature of 50 to 90°C to preheat the drawn yarn strip and send it to the next drawing step. The stretching is preferably a multi-stage stretching between 2GR and 4GR. The temperature of 2GR is 70 to 120°C, and then, when the overall stretching ratio is 100% at 3GR (100 to 140°C), it is preferable to perform thermal stretching of the yarn in the range of 60 to 80%. When the overall stretching ratio is 100% at 4GR, it is preferable to perform heat treatment while stretching the yarn in the range of 12 to 39%. In order to impart thermal dimensional stability that can be used for sewing threads used for sewing and the like to the yarn stretched as described above, it is effective to set the surface temperature (heat treatment temperature) of 4GR to 180 to 250°C, particularly 200 to 240°C. After the above-mentioned stretching, relaxation heat treatment is performed between 4GR and 5GR. In the case of the regenerated polyester fiber of the present invention, the relaxation rate is relatively high, and specifically, it is preferably set to about 0.5 to 10%. In the relaxation treatment, not only the strain generated by thermal stretching is removed, but also the orientation in the amorphous region is relaxed, the heat shrinkage rate is lowered, and the thermal dimensional stability can be improved. It is preferable to use an unheated roll or a roll overheated to 150°C or lower for RR (Relax Roll). By performing relaxation heat treatment under these conditions, it is easy to obtain a fiber that satisfies the heat shrinkage stress suitable for sewing thread applications used for sewing, has excellent heat resistance, and has thermal dimensional stability. In addition, in order to converge the yarn and reduce the generation of fluff to obtain high-quality polyester fibers, it is preferable to spray a high-pressure fluid onto the fiber yarn between 2GR and 3GR, between 3GR and 4GR, and between 4GR and 5GR to impart entanglement to the fiber yarn and perform stretching while converging the yarn. The fluid pressure can be changed according to the total fineness of the yarn, the single fiber fineness, the stretching speed, etc., but it is preferably set in the range of 0.3 to 0.8 MPa. It is preferable to impart entanglement as uniformly as possible and as much as possible in the fiber longitudinal direction. By imparting entanglement, the unwindability of the yarn from the wound product and the processability of the yarn are improved, and troubles in the high-order processing process can be avoided. Also, the raw yarn obtained in the above process may be drawn and false-twisted as necessary. False-twisting is a processing method in which false twist is applied while stretching a multi-filament partially oriented drawn yarn. The yarn is twisted while being heated, and untwisted after passing through a false-twist disk to obtain a bulky texture. Thereafter, interlacing is imparted using an air nozzle, an oiling agent is applied, and it is wound around a paper tube to form a package. When stretching and false-twisting a partially oriented undrawn yarn, the regenerated polyester fiber of the present invention preferably heats the yarn at a non-contact heater temperature of 200 to 350°C, sets the draw ratio to 1.2 to 2.5 times, and sets the running speed ratio of the surface of the friction disk to the yarn speed in the range of 1.3 to 2.5. The false-twisted regenerated polyester fiber is preferably wound up with a known package such as a cone shape using a winding machine. In this way, the regenerated polyester fiber of the present invention is obtained. Next, the present invention will be specifically described in Examples. The definitions of the characteristics used in the specification and examples and the measurement and calculation methods of each physical property are as follows. (1) [Total fineness]: Based on JIS L1013 (2010) 8.3.1 Positive quantity fineness a) Method A, using a measuring instrument manufactured by Nakayama Electric Industry Co., Ltd., an initial load of display fineness × 0.45 mN / dtex was applied and measured at a predetermined yarn length of 100 m to obtain the total fineness. (2) [Linear strength (breaking strength) and elongation]: The linear strength and elongation were measured under the constant elongation conditions shown during the standard test of JIS L-1013 (2010) 8.5.1 using "Tensilon" (TENSILON) UCT-100 manufactured by Orientec Co., Ltd. in a temperature-controlled chamber at a temperature of 20°C and a humidity of 65%. At this time, the gripping interval was 250 mm, the tensile speed was 300 mm / min, and the number of test times was 10 times. The breaking elongation was obtained from the elongation at the point indicating the maximum strength in the load-elongation curve. The strength was calculated by dividing the point indicating the maximum strength in the above load-elongation curve by the total fineness. (3) [Dry heat shrinkage rate]: The dry heat shrinkage rate was measured according to JIS L-1013 (2010) 8.18.2 Dry heat shrinkage rate a) Creep shrinkage rate (Method A), with the specified load at the time of sample collection being 5 mN / tex × the indicated fineness and the specified load at the time of creep length measurement being 200 mN / tex × the indicated fineness, and the treatment temperature being 150°C. (4) [Intrinsic viscosity]: For the intrinsic viscosity, 8.0 g of the sample was added to 100 mL of orthochlorophenol, and the relative viscosity ηr of the solution heated and dissolved at 160°C for 10 minutes was measured at 25°C using an Ostwald viscometer, and calculated according to the following approximate formula. Intrinsic viscosity = 0.0242ηr + 0.2634 (5) [L value and b value]: A colorimetric sample was prepared by winding the obtained fiber around a plate to form three layers so that the filament pitch was 0.7 cm and the width was 6.5 cm, and measured using a Konica Minolta color difference meter CR-410. The L value represents the lightness (brightness) of the color, ranging from 0 to 100 (0 is black and 100 is white), and the larger the number, the brighter the color. The b value represents the yellow-blue hue (the plus side is yellowish and the minus side is bluish). (6) [Ash content]: The measurement of the ash content was carried out according to the following method. Approximately 5 g of polyester resin in a state where the moisture was removed by drying at 105°C for 30 minutes was placed in a crucible, and the crucible was weighed (initial weight). Then, it was fired in an electric furnace set at 800°C for 2 hours. After firing, it was cooled in a desiccator and then weighed again, and the ash content of the entire inorganic impurities was calculated by comparing with the initial weight. Next, after drying at 105°C for 1 hour, 10 ml of sulfuric acid and 6 ml of perchloric acid were added to 1 g of the sample for wet decomposition. After decomposition, water was added to the solution and 5 ml of 3 wt% hydrogen peroxide solution to make a 100 ml diluted aqueous solution. Then, titanate (IV) was reacted in 3 wt% hydrogen peroxide solution to form a yellow peroxotitanium (IV) complex, and the absorbance at 420 nm was measured using an absorptiometer (manufactured by Hitachi, Ltd., U-3900H) to colorimetrically determine the amount of titanium compound. By subtracting the amount of titanium compound from the ash content of the entire inorganic impurities, the ash content of the inorganic impurities (excluding titanium compounds and dyes and pigments for coloring purposes) was determined. In addition, since the dye-pigment for coloring purposes loses weight during firing, the ash content can be quantified by this measurement method. (7) [Process Passability]: After the start of production, without replacing the guides and rolls, for the recycled polyester fibers obtained 24 hours and 240 hours after continuous spinning, while unwinding at a speed of 500 m / min, the hairiness (single filament breakage) contained in the yarn was detected with a light-sensing hairiness detector manufactured by Ohiro Co., Ltd., and evaluated according to the following criteria based on the number of hairiness per 100,000 m of yarn length. ◎ (Excellent): 0 - 1 (pieces / 100,000 m) ○ (Good): 2 - 5 (pieces / 100,000 m) △ (Poor): 6 - 50 (pieces / 100,000 m) × (Very Poor): 51 (pieces / 100,000 m) or more [Production Example 1] The used PET bottles in the form of bales, which were won at auction by the Japan Container and Packaging Recycling Association, a public interest incorporated foundation, were sorted (removed) from other resin bottles, colored bottles, caps, and labels using an optical sorter (manufactured by Nippon Seam Co., Ltd.) and manual sorting, and then the PET bottles were washed with warm water at 40°C in their bottle shape. Next, after detecting and removing metals including non-ferrous metals with a metal detector (manufactured by Nippon Metal Detector Co., Ltd.), they were wet-ground into flakes of 2 - 15 mm, and the flakes were continuously washed in a stirring bath with a 3 wt% aqueous sodium hydroxide solution for 30 minutes. After washing, rinsing, dehydration, and drying were performed to obtain washed PET bottle flakes. Then, solid-phase polymerization was carried out at 220°C under nitrogen gas using VACUREMA 1109T manufactured by EREMA. After that, when the total weight of the solid-phase polymerized flakes and the fibers was set to 100 wt%, Mitsubishi Gas Chemical's (S6007) polymetaxylylene adipamide (MXD6) was weighed to be 0.4 wt% and melt-kneaded at 275°C in an extruder. The melt resin was passed through a filter capable of filtering and removing solid foreign matters with a particle size of 15 μm or more in the melt resin, and extruded in a strand shape into cold water from a 20-hole die and cut to obtain a pelletized polyester resin composition. Next, the polyester resin composition pellets obtained above were dried and crystallized at a temperature of 125°C for 6 hours under vacuum to obtain recycled polyester pellets having an intrinsic viscosity of 0.80. [Production Example 2] In the content described in Production Example 1, except that the flaky material after wet grinding was washed in a stirring bath with an 8 wt% aqueous sodium hydroxide solution for 20 minutes, and Mitsubishi Gas Chemical Co., Ltd. (S6007) polymetaxylylene adipamide (MXD6) was melt-kneaded at 275°C so as to be 0.08 wt% when the total weight of the flakes and fibers after solid-phase polymerization was 100 wt%, recycled polyester pellets were obtained by the same method as in Production Example 1. [Production Example 3] In the content described in Production Example 1, except that Mitsubishi Gas Chemical Co., Ltd. (S6007) polymetaxylylene adipamide (MXD6) was melt-kneaded at 275°C so as to be 0.95 wt% when the total weight of the flakes and fibers after solid-phase polymerization was 100 wt%, and the molten resin was passed through a filter capable of filtering and removing solid foreign matters having a particle size of 10 μm or more, recycled polyester pellets were obtained by the same method as in Production Example 1. [Production Example 4] In the content described in Production Example 1, except that when melt-kneading the flakes after solid-phase polymerization and Mitsubishi Gas Chemical Co., Ltd. (S6007) polymetaxylylene adipamide (MXD6), sodium naphthalene sulfonate formalin condensate was added so as to be 1.20 wt% when the total weight of the fibers was 100 wt%, recycled polyester pellets were obtained by the same method as in Production Example 1. [Production Example 5] In the content described in Production Example 1, except that only the flakes after solid-phase polymerization were melt-kneaded without adding polymetaxylylene adipamide (MXD6), recycled polyester pellets were obtained by the same method as in Production Example 1. [Production Example 6] In the content described in Production Example 1, except that the flaky material after wet grinding was not washed with an aqueous solution of an alkali metal hydroxide and only the flakes after solid-phase polymerization without addition of polymetaxylylene adipamide (MXD6) were melt-kneaded, recycled polyester pellets were obtained by the same method as in Production Example 1. [Production Example 7] In the content described in Production Example 1, except that the flaky material after wet grinding was washed with an aqueous solution of sodium hydroxide having a concentration of 10% by weight for 150 minutes in a stirring bath and only the flakes after solid-phase polymerization without addition of polymetaxylylene adipamide (MXD6) were melt-kneaded, recycled polyester pellets were obtained by the same method as in Production Example 1. [Production Example 8] In the content described in Production Example 1, except that the flaky material after wet grinding was washed with an aqueous solution of sodium hydroxide having a concentration of 10% by weight for 150 minutes in a stirring bath and polymetaxylylene adipamide (MXD6) manufactured by Mitsubishi Gas Chemical Co., Ltd. (S6007) weighed so as to be 1.10% when the total weight of the flakes and fibers after solid-phase polymerization was 100% by weight was melt-kneaded at 275°C, recycled polyester pellets were obtained by the same method as in Production Example 1. [Production Example 9] In the content described in Production Example 1, except that the flaky material after wet grinding was washed with an aqueous solution of sodium hydroxide having a concentration of 10% by weight for 150 minutes in a stirring bath and polymetaxylylene adipamide (MXD6) manufactured by Mitsubishi Gas Chemical Co., Ltd. (S6007) weighed so as to be 1.10% when the total weight of the flakes and fibers after solid-phase polymerization was 100% by weight was melt-kneaded at 275°C and sodium naphthalenesulfonate formalin condensate weighed so as to be 1.20% when the total weight of the fibers was 100% by weight was added, recycled polyester pellets were obtained by the same method as in Production Example 1. [Example 1] The recycled polyester pellets obtained by the method of Production Example 1 were continuously supplied to and melted in a single-screw extruder-type extruder at a temperature of 295°C. The obtained molten polymer was kneaded with an eight-stage static mixer through a pipe at a temperature of 295°C, adjusted by a metering pump to a discharge rate of 50 g / min, then led to a spinning pack at a temperature of 295°C, passed through a filter with a 15-micron cut in the pack, and then spun from a die having 72 round single holes with a pore diameter of 0.6 mmφ and a pore length of 0.78 mm. The spun yarn was passed through a heating cylinder with a length of 70 mm provided below the die and an ambient temperature of 285°C, and then solidified by blowing cold air at a temperature of 40°C at a speed of 30 m / min using an annular chimney. Next, an oil agent (manufactured by Sanyo Chemical Industries, Ltd.: Sun Oil F) was applied to the cooled yarn by an oil agent roll, the obtained yarn was subjected to a GR (unheated) with a surface speed of 3,500 m / min, and wound up with a winder at 3,500 m / min to obtain a partially oriented yarn of recycled polyester of 135 dtex - 72 filaments. Next, the obtained partially oriented yarn of recycled polyester was subjected to a draw texturing process using a disk false twister at a non-contact heater temperature of 350°C, a draw speed of 750 m / min, a DY ratio of 1.7, and a draw ratio of 1.65 times to obtain recycled polyester fibers of 83 dtex - 72 filaments. The results are shown in Table 1. [Example 2] The recycled polyester pellets obtained by the method of Production Example 2 were spun in the same manner as in Example 1, except that they were adjusted by a metering pump to a discharge rate of 167 g / min and a die having 48 round single holes with a pore diameter of 0.6 mmφ and a pore length of 0.78 mm was used. The spun yarn was passed through a heating cylinder with a length of 200 mm provided below the die and an ambient temperature of 320°C, and then solidified by blowing cold air at a temperature of 20°C at a speed of 30 m / min using a uniflow chimney. Next, an oil agent (manufactured by Sanyo Chemical Industries, Ltd.: Sun Oil F) was applied to the cooled yarn by an oil agent roll, the obtained yarn was subjected to a GR (unheated) with a surface speed of 1,000 m / min, and wound up with a winder at 1,000 m / min to obtain an undrawn yarn of recycled polyester of 1,670 dtex - 48 filaments. Next, the obtained undrawn recycled polyester yarn was continuously fed to 1GR (90°C) at a speed of 74 m / min, 2GR (110°C) at a speed of 300 m / min, 3GR (225°C) at a speed of 430 m / min, and 4GR (unheated) at a speed of 400 m / min using a multi-stage drawing machine, drawn, and wound with a winder to obtain recycled polyester fibers of 278 dtex - 48 filaments. The results are shown in Table 1. [Example 3] The recycled polyester pellets obtained by the method of Production Example 3 were adjusted by a metering pump to have a discharge rate of 500 g / min, and a die having 144 round single holes with a hole diameter of 0.6 mmφ and a hole length of 0.78 mm was used. Except for a 10-micron cut filter in the pack, spinning was performed in the same manner as in Example 2. The spun yarn was passed through a heating cylinder with a length of 350 mm provided under the die and an ambient temperature of 285°C, and then solidified by blowing cold air at a temperature of 40°C at a speed of 30 m / min using an annular chimney. Next, an oil agent (Sun Oil F manufactured by Sanyo Chemical Industries, Ltd.) was applied to the cooled yarn by an oil agent roll, and the obtained yarn was taken up at 1GR (70°C) having a surface speed of 500 m / min and continuously fed to a drawing process. Without winding the yarn that had passed through 1GR once, drawing was performed by continuously feeding it to 2GR (115°C) at a speed of 530 m / min, 3GR (110°C) at a speed of 1,900 m / min, 4GR (230°C) at a speed of 3030 m / min, and 5GR (unheated) at a speed of 3,000 m / min. An interlacing treatment device was installed between 2GR - 3GR, 4GR - 5GR, and 5GR - the winder, and interlacing treatment was performed by injecting high-pressure fluid at settings of 0.4, 0.1, and 0.5 MPa, respectively, and wound with a winder to obtain recycled polyester fibers of 1,670 dtex - 144 filaments. The results are shown in Table 1. [Example 4] The recycled polyester pellets obtained by the method of Production Example 4 were used, the discharge rate was adjusted to 60 g / min by a metering pump, and a partially oriented yarn of recycled polyester with a fineness of 125 dtex - 72 filaments was obtained. Except that the stretching false twisting process was carried out at a non-contact heater temperature of 300 °C, a DY ratio of 1.6, and a draw ratio of 1.56 times, recycled polyester fibers with a fineness of 75 dtex - 72 filaments were obtained in the same manner as in Example 1. The results are shown in Table 1. Using the recycled polyester fibers obtained in Examples 1 to 4, the results of measuring the intrinsic viscosity (IV), total fineness, linear strength (breaking strength), elongation, dry heat shrinkage rate, L value, b value, and ash content, as well as the results of evaluating the process passability of the recycled polyester fibers obtained in Examples 1 to 4, are shown in Table 1. [Comparative Examples 1 and 2] The same procedure as in Example 2 was carried out except that the recycled polyester pellets obtained by the methods of Production Examples 5 and 6 were used. However, for Comparative Examples 1 and 2, since the yarn-making property deteriorated and recycled polyester fibers could not be obtained, the raw yarn evaluation was not performed. [Comparative Example 3] Recycled polyester fibers with a fineness of 83 dtex - 72 filaments were obtained in the same manner as in Example 1 except that the recycled polyester pellets obtained by the method of Production Example 7 were used. The results are shown in Table 1. [Comparative Example 4] Recycled polyester fibers with a fineness of 278 dtex - 48 filaments were obtained in the same manner as in Example 1 except that the recycled polyester pellets obtained by the method of Production Example 8 were used. The results are shown in Table 1. [Comparative Example 5] Recycled polyester fibers with a fineness of 278 dtex - 48 filaments were obtained in the same manner as in Example 2 except that the recycled polyester pellets obtained by the method of Production Example 8 were used. The results are shown in Table 1. [Comparative Example 6] Recycled polyester fibers with a fineness of 75 dtex - 72 filaments were obtained in the same manner as in Example 4 except that the recycled polyester pellets obtained by the method of Production Example 9 were used. As is clear from the results in Table 1, in Comparative Examples 1 and 2, although it is possible to achieve L values and b values like those of the present invention, the processability was low and the stretchability was insufficient due to impurities in the recycled polyester resin, and polyester fibers could not be obtained. Further, as in Comparative Examples 3 to 5, in order to obtain stretchability, the flaky material after wet grinding was washed with an aqueous solution of an alkali metal hydroxide for a long time, so that the processability was improved, but the b value increased and recycled polyester fibers comparable to virgin raw materials like those of the present invention could not be obtained. On the other hand, the recycled polyester fiber of the present invention not only has excellent processability, but also has high mechanical properties and achieves a color tone comparable to that of virgin raw materials. Therefore, it can be applied not only to knit fabrics constituting sportswear but also to sewing threads used for sewing, and can be effectively used for sports uniforms. Although the present invention has been described in detail and with reference to specific embodiments, it will be apparent to those skilled in the art that various changes and modifications can be made without departing from the spirit and scope of the present invention. This application is based on a Japanese patent application filed on August 30, 2016 (Japanese Patent Application No. 2016-167741), the content of which is incorporated herein by reference.
Claims
1. A recycled polyester fiber comprising a polyester resin mainly composed of the recycled polyester and poly(m-xylylene adipamide) (MXD6), wherein the content of the poly(m-xylylene adipamide) (MXD6) is 0.01 to 1% by weight based on 100% by weight of the total weight of the recycled polyester fiber, and the L value is 70 to 100 and the b value is -5 to 5.
2. The recycled polyester fiber according to claim 1, wherein the polyester resin contains inorganic impurities (excluding titanium compounds and dyes and pigments for coloring) in an amount of 0.1 to 5% by weight in terms of ash content based on 100% by weight of the total weight of the polyester resin.
3. The recycled polyester fiber according to claim 1 or 2, which has a functional group capable of being dyed with a cationic dye.
4. The recycled polyester fiber according to any one of claims 1 to 3, wherein the recycled polyester is derived from beverage bottles.