SYSTEMS AND METHODS FOR CLOSED-LOOP RECYCLING OF A LIQUID COMPONENT FROM A LEACHING MIXTURE WHEN RECYCLING LEAD FROM LEAD-ACID BATTERIES

MX438984BActive Publication Date: 2026-10-05CLARIOS GERMANY GMBH & CO KG +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
MX2022008768
Authority / Receiving Office
MX · MX
Patent Type
Patents
Current Assignee / Owner
Priority Date
2014-09-26
Filing Date
2016-12-16
Publication Date
2026-10-05
Estimated Expiration
2035-06-08
Patent Text Reader

Abstract

This description generally refers to systems and methods for purifying and recycling the lead content of lead-acid batteries. A system (40) includes a reactor (56) that receives and mixes a lead-bearing material (54), a carboxylate source (58), and a recycled liquid component (60) to form a leaching mixture (62), wherein a phase-separating device (64) isolates a lead salt precipitate (66) from a liquid component (68) of the leaching mixture (62). The system further includes a closed-loop liquid recycling system coupled to the phase-separating device and the reactor, wherein the closed-loop liquid recycling system receives the liquid component isolated by the phase-separating device and recycles a substantial portion of the received liquid component back into the reactor as the recycled liquid component.The closed-loop recycling system optionally comprises a purification device (76), specially configured to remove sulfates from the liquid component without substantially removing the dissolved lead salt.
Need to check novelty before this filing date? Find Prior Art

Description

SYSTEMS AND METHODS FOR CLOSED-LOOP RECYCLING OF A LIQUID COMPONENT FROM A LEACHING MIXTURE WHEN RECYCLING LEAD FROM LEAD-ACID BATTERIES DESCRIPTION OF THE INVENTION This description generally refers to systems and methods for recycling lead-acid batteries and more specifically, refers to purifying and recycling the lead content of lead-acid batteries. The lead present in a lead-acid battery can take several forms. For example, a lead-acid battery may include grids containing lead alloys and lead oxide (PbO, PbO2), battery paste containing metallic lead sponge, lead oxide, red lead, and / or lead sulfate, and posts and / or interconnects containing metallic lead, lead alloys, and possibly lead-free alloys. While it may be desirable to attempt to recover lead from spent or retired lead-acid battery waste, this material can include a variety of lead compounds (lead alloys, oxides, sulfates, and carbonates) and a range of physical and / or chemical impurities.Existing methods for purifying lead typically rely almost entirely on multi-stage pyrometallurgical smelting, in which some of the compounds are burned to produce volatile gases. Some of these gases must be purified (e.g., captured and removed from the exhaust stream) to prevent their release, in accordance with environmental regulations. The remaining impurities are then removed from the metallic lead in several refining operations. Because these operations often require specialized equipment and certain consumables (e.g., solutions or other refining agents), this refining process generally adds cost and complexity to the lead recovery process. This description relates to systems and methods by which lead can be extracted, purified, and used in the construction of new lead-acid batteries. In one embodiment, a system includes a reactor that receives and mixes lead-bearing waste material, a carboxylate source, and a recycled liquid component to form a leaching mixture that produces a lead salt precipitate. The system also includes a phase separation device coupled to the reactor, wherein the phase separation device isolates the lead salt precipitate from a liquid component of the leaching mixture.The system also includes a closed-loop liquid recycling system coupled to the phase separation device and the reactor, wherein the closed-loop liquid recycling system receives the liquid component isolated by the phase separation device and recycles a substantial portion of the received liquid component back into the reactor as the recycled liquid component. οα / οηη / ζζηζ / Ε / γ οο / οηη / ζζηζ / Ε / γ In another embodiment, a method involves forming a leaching mixture that includes a lead-bearing material, a carboxylate source, and a recycled liquid component, wherein the leaching mixture generates a lead salt precipitate as the carboxylate source reacts with the lead-bearing material. The method also includes isolating a liquid component from the lead salt precipitate of the leaching mixture. The method further includes recycling at least a portion of the isolated liquid component back into the leaching mixture as the recycled liquid component. In another embodiment, a system includes a closed-loop liquid recycling system coupled to a leaching vessel containing a leaching mixture. The liquid recycling system receives a liquid component from the leaching mixture, purifies the received liquid component to generate a purified liquid component with a lower sulfate content than the received liquid component, and supplies the purified liquid component to the leaching vessel as part of the leaching mixture. BRIEF DESCRIPTION OF THE DRAWINGS FIGURE 1 is a flow diagram illustrating one modality of a process by which lead can be extracted, purified, and used in the construction of new lead-acid batteries; and FIGURE 2 is a schematic diagram of an οα / οηη / ζζηζ / E / γ modality of a system to perform the process of FIGURE 1. One or more specific modes will be described below. In an effort to provide a concise description of these modes, not all features of an actual implementation are described in the specification. It should be appreciated that in the development of any actual implementation, as in any engineering or design project, numerous implementation-specific decisions must be made to achieve the developers' specific goals, such as compliance with system-related and business-related constraints, which may vary from one implementation to another. Furthermore, it should be appreciated that such a development effort may be complex and time-consuming, but it can nonetheless be a routine task of design, fabrication, and manufacturing for those of ordinary experience who benefit from this description. When elements from several modalities of this description are presented, the articles one, an, and the are intended to signify that one or more of the elements exist. The terms comprising, including, and having are intended to be inclusive and mean that additional elements may exist beyond those listed. Furthermore, references to a modality or a modality in this description are not intended to be interpreted as excluding the existence of additional modalities that also incorporate the described characteristics. As used herein, the description of a particular component formed from or including a particular element called by name (e.g., lead) should be interpreted to encompass all forms of lead (e.g., metallic lead, lead compounds, or mixtures thereof). For distinction, as used herein, the description of a metallic form of an element may be indicated by the chemical formula (e.g., Pb(O)) or by using the terms elemental, metallic, or free (e.g., elemental lead, metallic lead, or free lead). As used herein, lead powder may be used to indicate a mixture of metallic lead (e.g., Pb(O)) and lead oxide (e.g., PbO) in various ratios as described.As used herein, the term substantially free may be used to indicate that the identified component is not present at all or is present only in a trace amount (e.g., less than 0.1%, less than 0.01%, or less than 0.001%). As used herein, a Group X element or compound may refer to any chemical substance (e.g., element or compound) that includes an element from the identified column of the periodic table. For example, a Group 14 element or compound may include any of the Group 14 elements (e.g., carbon, silicon, tin, etc.) as well as any compounds that include Group 14 elements (e.g., carbonates, silicates, stannates, etc.). As used herein, a carboxylate source is any molecule or polymer that includes at least one carboxylate or carboxylic acid portion or functionality.Accordingly, a non-limited list of exemplary carboxylate sources includes: citric acid, acetic acid, formic acid, citrate, acetate, formate, dilactate, oxalate, tartarate, or any combination thereof. The term citrate herein refers to citric acid, or a citrate salt of a Group 1 or Group 2 metal, or ammonium citrate. The term acetate herein refers to acetic acid, or acetate salts of a Group 1 or Group 2 metal, or ammonium acetate. New lead-acid battery herein refers to a newly manufactured lead-acid battery, while the term spent lead-acid battery indicates a battery at the end of its service life. As used herein, peroxide refers to hydrogen peroxide and / or any organic peroxide (e.g., peracetic acid).The term hydroxide herein refers to a Group 1 or Group 2 metal hydroxide, ammonium hydroxide, or ammonia gas introduced into the reaction mixture to form ammonium hydroxide in situ, or combinations thereof. As mentioned above, existing methods typically rely heavily on pyrometallurgical smelting or combustion to recover and purify lead from spent lead-acid batteries. For such methods, the lead-bearing material from the spent lead-acid batteries, which may include a quantity of lead compounds and a quantity of impurities, can be heated so that at least a portion of the impurities can be burned or volatilized and released as byproducts. Additionally, after the pyrometallurgical smelting or combustion of the lead-bearing material, such methods may involve subsequent refining stages to remove byproducts or other impurities to produce purified lead.Since the atmospheric release of some of these combustion byproducts (e.g., SO2, soot) may be restricted by local environmental regulations, the present embodiments are aimed at enabling solution-based removal of various impurities from recovered lead, thereby avoiding or reducing the formation of such combustion byproducts and / or the cost associated with removing them from the exhaust stream. Additionally, the present embodiments address limitations of other waste lead purification techniques, enabling a robust method for purifying and recycling recovered lead on an industrial scale.Furthermore, as described in detail below, these embodiments enable the closed-loop recycling of the liquid component of the leaching solution used during the lead recovery and purification process. This improves lead recovery and avoids the potentially costly disposal of this liquid component. Consequently, these embodiments provide a lead recovery and purification technique that is robust to a wide variety of impurities, enhances lead recovery, and minimizes the production of byproducts that can be expensive to purify and dispose of properly. Figure 1 is a flow diagram illustrating one embodiment of process 10 by which lead can be extracted, purified, and used from spent lead-acid batteries in the construction of new lead-acid batteries. It can be seen that process 10 in Figure 1 is provided only as an example, and in other embodiments, process 10 may include additional purification steps (e.g., additional hydrometallurgical purification steps, additional phase-, size-, or density-based separation steps, additional pH adjustment steps) in accordance with the present description. As illustrated in Figure 1, process 10 begins with the processing (block 12) of spent lead-acid batteries to generate a lead-bearing material.For example, in one embodiment, one or more lead-acid batteries can be fed through a hammer mill or other suitable device capable of crushing, pulverizing, grinding, or otherwise phase-breaking down the entire spent lead-acid battery. The battery components... Spent lead-acid batteries may include, for example, metal posts, metal connectors, metal grids, carbon black, glass, a plastic or metal casing, plastic separators, plastic fibers, lignosulfonates or other organic extenders, battery paste (for example, including various lead oxides, lead carbonates, lead sulfates), sulfuric acid, and other components (for example, non-lead metal components such as brass terminals). The lead present in a spent lead-acid battery may have several different forms, including, for example, PbO2, PbO, PbSO4, PbCO3, and Pb(O). After substantial pulverization, the resulting battery waste, in certain embodiments, can be passed through one or more preliminary purification stages in which certain components (e.g., shredded plastic components) can be removed from the remaining lead-bearing mixture, for example, using a separation device (e.g., a settling tank or cyclone separator) that takes advantage of the lower density of these plastic components. For example, in certain embodiments, screening can be applied as a separation stage to separate the bulk metal particle fractions from other portions of the battery waste. Furthermore, in certain embodiments, some or all of the residual sulfuric acid trapped in the lead-bearing material can be recycled for reuse or neutralized and crystallized as solid sulfate for disposal or resale.In certain forms, the pretreatment of lead-bearing material may include a complete or partial desulfurization stage in which the sulfate content of the lead-bearing material can be reduced by chemical means, for example, by treatment with a hydroxide (e.g., sodium hydroxide) or carbonate (e.g., soda ash). Each of these actions or stages can generally be represented by block 12. Method 10, as illustrated, continues with the formation (block 14) of a leaching mixture that includes the lead-bearing material generated in block 12 (which may include all battery residue, or a separate fraction thereof, as discussed above), a carboxylate source, and a recycled liquid component. The recycled liquid component is, or may be, formed from an aqueous solution isolated during a later step (block 18) of Method 10, as discussed in further detail below. In block 14, the recycled liquid component may be partially or fully saturated with a dissolved lead salt (e.g., lead citrate, lead acetate, and / or other lead salts) and may optionally provide a means for leaching the lead-bearing material.In certain embodiments, the carboxylate source may be metal citrate (e.g., sodium citrate), citric acid, metal acetate (e.g., sodium acetate), acetic acid, a combination thereof, or any other suitable carboxylate source that can promote the formation of lead salts in the leaching mixture. In certain embodiments, water and / or peroxide may also be added to the leaching mixture to promote the dissolution of solid lead and the formation of lead salts (e.g., lead citrate, lead acetate) in the leaching mixture. In certain embodiments, sodium hydroxide or sodium carbonate may be added to the mixture, or sodium citrate may be used as at least a portion of the carboxylate source, to promote the formation of sodium sulfate from any lead sulfate that may be present in the leaching mixture. In certain configurations, block 14 can be carried out in a reactor, such as a leaching tank, at low (acidic) pH (e.g., pH between 1 and 7) and slightly elevated temperatures (e.g., approximately 30 °C or higher). It can be seen that this leaching mixture may include both insoluble and soluble residues from spent and decomposed batteries. Additionally, the carboxylate source reacts with one or more forms of lead in the leaching mixture (e.g., metallic lead, lead sulfate, lead carbonate, and lead oxide), with or without the assistance of a peroxide, to produce one or more lead salts. Since these lead salts may have limited solubility at low pH levels, a lead salt precipitate (e.g., a lead citrate precipitate) may be generated (block 16). QQ / onn / zznz / E / Y in the leaching mixture as a result. Furthermore, as discussed below, the lead salt dissolved in the recycled liquid component can visualize the lead salt generated to precipitate within the leaching mixture. Subsequently, the lead salt precipitate can be isolated (block 18) from the liquid component of the leaching mixture, for example, by filtration. After separation from the liquid component of the leaching mixture, the lead salt precipitate can be washed with water, and the filtrate and wash water may retain all or most of the remaining impurities from the lead salt precipitate. For example, in certain embodiments, the isolated lead salt precipitate may include little or no residual sulfate (e.g., sodium sulfate and / or lead sulfate), such as less than 5% sulfates, less than 4% sulfates, less than 3% sulfates, less than 2% sulfates, less than 1% sulfates, less than 0.5% sulfates, less than 0.3% sulfates, or less than 0.1% sulfates. Recycling of the liquid component (and the wash water) is discussed in further detail below. Next, in process 10 illustrated, the lead salt precipitate can be treated (block 20) ​​to produce lead powder. For example, in certain embodiments, the treatment in block 20 may involve treating the isolated lead salt precipitate with the base (e.g., hydroxide, 25–50 wt% sodium hydroxide solution) to produce QQ / onn / zznz / E / Y The lead powder product, in certain embodiments, the treatment of block 20 may involve a calcination treatment carried out using a belt dryer, a spray calciner, a stirred crucible reactor, a rotary kiln, or another suitable calciner or furnace. For embodiments using a calcination treatment, the lead salt precipitate may be heated to a temperature lower than 450°C (e.g., between approximately 275°C and approximately 400°C, to approximately 330°C). In certain modalities, this heating can occur in the presence of a gas stream (e.g., air, oxygen-rich air, oxygen-reduced air, air / inert gas mixtures, water vapor) so that the organic portion of the carboxylate source is burned, resulting in a mixture of free lead (i.e., Pb(0)) and lead oxide (i.e., PbO), commonly referred to as lead powder.Since the carboxylate source structure includes a substantial amount of oxygen, in certain processes calcination can occur while burning an oxygen-reducing agent (e.g., methane, coke, propane, natural gas, etc.) to limit the amount of oxygen present during the calcination process and thus control the chemistry of the lead powder product. For such processes, examples of process controls that can affect the resulting lead powder include the calcination temperature, time, droplet size (e.g., for spray calcination), lead salt particle size, the amount of residual water remaining in the lead salt, the rate at which the lead salt is heated to the calcination temperature, and / or the oxygen content in the gas stream. Process 10, as illustrated, continues with the lead powder produced from the treatment of block 20 being formed (block 22) into an active lead powder material for use in new lead-acid batteries. For example, the lead powder can be mixed with water and sulfuric acid to form a battery paste that can be applied to a plurality of lead grids to serve as the active material of a new lead-acid battery. Accordingly, a new lead-acid battery can be constructed (block 24) using the lead powder battery paste formed in block 22. The active lead powder material formed by the present process can enable the production of new lead-acid batteries that have good to excellent electrical performance. The lead powder formed in block 20 can also be used to manufacture tribasic lead sulfate (3BS), tetrabasic lead sulfate (4BS), and red lead (lead(II,IV) oxide, PbsCu).In the case of 3BS and 4BS, the materials can be produced by mixing the lead powder formed in block 20 with water and sulfuric acid using a mixer. In the case of red lead, the material can be formed by further treating (e.g., calcination and oxidation) the lead powder formed in block 20. All these materials are useful in the construction of new lead-acid batteries, or for other suitable technical purposes. Furthermore, it can be seen that while the liquid component isolated from the leaching mixture, as well as any wash water, contains certain contaminants (e.g., sulfates or salts of elements other than lead) that are desirably separated from the lead salt precipitate in Block 18, this isolated liquid component also includes a substantial amount of dissolved lead salt. That is, although the solubility of the lead salt in the leaching mixture from Block 16 may be low (e.g., due to the pH of the leaching mixture and / or the amount of lead salt present in the leaching mixture), a certain amount of lead salts (e.g., lead citrate, lead acetate) will remain dissolved in the liquid component after the lead salt precipitate is isolated in Block 18.In fact, in certain forms, this isolated liquid component may be partially or fully saturated with lead salts (e.g., at least 5% saturated, at least 10% saturated, or at least 15% saturated with lead salts, up to 100% saturated with lead salts) and may also include other impurities (e.g., lead sulfate, sodium sulfate, or other salts of elements other than lead). As such, if the liquid component were discarded, a substantial amount of purification (e.g., lead removal, sulfate removal, etc.) would likely be required, and a substantial amount of lead would also be lost.By recycling the isolated liquid component back into the leaching mixture in Block 14 in a closed-loop manner, the aforementioned high concentration of dissolved lead salts (e.g., lead citrate, lead acetate) in this recycled liquid component causes the additional lead salts generated in Block 16 to precipitate, rather than remain dissolved in the leaching mixture. Therefore, in addition to avoiding costly purification and disposal steps, the recycling of the liquid component from the leaching mixture described herein increases the yield of the lead salt precipitate isolated in Block 18 and the overall efficiency of Method 10. With the above in mind, Method 10, illustrated in Figure 1, includes steps in which the liquid component isolated in Block 18 can be recycled back into the leaching mixture of Block 14, limiting waste production and improving lead recovery. As illustrated in Figure 1, the liquid component isolated in Block 18, which may or may not include water from one or more washes, can be purified (Block 26) to remove one or more impurities from the liquid component before it is recycled (Block 28) into the mixture of Block 14. For example, in certain embodiments, it may be desirable to remove or reduce the sulfate content (e.g., sodium sulfate, lead sulfate, salts of elements other than lead, etc.) in the liquid component before it is recycled back into the leaching mixture of Block 14.By way of a specific example, in certain embodiments, the purification of block 26 may include chemical purification (e.g., forming insoluble calcium sulfate from other sulfates using calcium hydroxide), physical purification (e.g., reverse osmosis or nanofiltration), and / or ion exchange resins. It can be seen that, in certain embodiments, the purification described for block 26 preferentially removes one or more impurities from the liquid component without substantially altering the amount of lead salt (e.g., lead citrate, lead acetate) dissolved in the liquid component. Furthermore, in certain embodiments, the liquid component isolated in block 18 does not undergo the purification described for block 26 and, instead, may be recycled directly (block 28) into the leaching mixture of block 14. Figure 2 illustrates one embodiment of a system 40 configured to perform the process illustrated in Figure 1 in what may be termed a continuous manner. In certain embodiments, part or all of the illustrated system 40 may be implemented as a multi-stage reactor system, or a series of individual reactors and devices, to enable the continuous processing of spent lead-acid batteries into lead powder particles. In addition to these devices, stages, and / or reactors (illustrated as rectangles) in the system 40, Figure 2 also illustrates the various inputs and outputs (illustrated as non-rectangular parallelograms) for each device in the system 40. The illustrated system 40 in Figure 2 has a control system 42 that includes a controller 44 (e.g., a programmable logic controller (PLC)).The controller 44 includes a memory 46 and a processor 48 that enable the controller 44 to store and execute instructions (e.g., applications, modules, apps, firmware) to control the operation of the system 40 using field devices 49. For example, the field devices 49 can include any number of sensing devices (e.g., temperature sensors, pressure sensors, flow rate sensors, oxygen sensors, particle size sensors, rotation speed sensors, pH sensors) that are distributed throughout the system 40 and communicatively coupled to the controller 44 (e.g., via a wired and wireless communication channel) to enable the controller 44 to determine the operating parameters of the system 40.In addition, the field devices 49 may include any number of control devices (e.g., actuators, valves, motors, screws, heating elements, compressors) configured to receive control signals from the controller 44 and modulate the operation or state of the system 40 accordingly. With the above in mind, the illustrated system 40 includes a lead-acid battery processing system 52 that receives spent lead-acid batteries 50 and generates a lead-bearing material 54. As such, the lead-acid battery processing system 52 performs the actions described by block 12 of process 10 illustrated in FIGURE 1. As mentioned above, this lead-acid battery processing system 52 may include a hammer mill or other suitable device capable of receiving all the lead-acid batteries (e.g., via a feed channel) and grinding the lead-acid batteries into particulate battery waste. Additionally, as mentioned above, the lead-acid battery processing system 52 may include certain preliminary purification features to remove one or more components from the particulate battery waste.For example, in certain embodiments, the lead-acid battery processing system 52 may include a cyclone separation device that receives particulate battery waste from the hammer mill and can separate lower-density battery waste (e.g., plastic components from the lead-acid battery housing) from the higher-density lead-bearing material 54, which can then be advanced to the next device (e.g., the leaching vessel 56) in the illustrated system 40. Also, as mentioned above, screening can be applied to bulk particle fractions separated from other fractions of the battery waste. The system 40 illustrated in FIGURE 2 includes a leaching vessel 56 configured to perform the acts described in blocks 14 and 16 of process 10 illustrated in FIGURE 1. The leaching vessel 56 may be a reactor or a stage of a multi-stage reactor (e.g., a leaching tank or reactor) that receives lead-bearing material 54 from the lead-acid battery processing system 52 and adds a carboxylate source 58 (e.g., citric acid, sodium citrate, acetic acid, sodium acetate, or a combination thereof) and a purified, recycled liquid component 60 (e.g., a solution that is at least partially saturated with lead salts) to form a leaching mixture 62.In certain embodiments, the leaching vessel 56 may also add a peroxide, a hydroxide, acetic acid, and / or sodium carbonate to the leaching mixture 62 to promote the formation of lead salt from the lead-bearing material. In certain embodiments, the leaching vessel 56 may also be capable of providing temperature control (e.g., heating and / or cooling between approximately 30°C and 100°C) and agitation (e.g., mixing and / or stirring) of the mixture to facilitate the formation of the lead salt precipitate in the leaching mixture 62. Therefore, the leaching vessel 56 can produce (e.g., store, contain, or produce) the leaching mixture 62, which includes the lead salt precipitate formed and the remainder of the lead-bearing material.This leaching mixture 62 can be subsequently advanced to the next device (e.g., phase separation device 64) in the illustrated system 40. The system 40 illustrated in FIGURE 2 includes a phase separation device 64 configured to perform the actions described in block 18 of process 10 illustrated in FIGURE 1. In certain embodiments, the phase separation device 64 may include a filter press, clarifier, cyclone separator, settling tank, belt dryer, or any other device capable of separating components of the leaching mixture 62 based on oil phase, density, and / or size. As such, the phase separation device 64 receives the leaching mixture 62 and separates the solid lead salt precipitate 66 from the liquid component 68. Subsequently, the isolated lead salt precipitate 66 may proceed to the next device (e.g., lead salt precipitate treatment device 70) in the illustrated system 40 and eventually provide the lead dust particles 74, as discussed below. For the illustrated modality, the liquid component 68, isolated by the phase separation device 64, which includes dissolved lead salt as well as dissolved impurities (e.g., lead sulfate, sodium sulfate, salts of elements other than lead), is subsequently supplied to the purification device 76 of the closed-loop liquid recycling system 77. The purification device 76 is configured to perform the actions described in block 26 of process 10 illustrated in FIGURE 1.By way of specific example, in certain embodiments, the purification device 76 may include a reactor that adds calcium hydroxide to the liquid component 68, and a phase separation device (e.g., a filter press, clarifier, or settling tank) that removes the resulting insoluble calcium sulfate from the liquid component 68 to produce (e.g., store, contain, or produce) the purified liquid component 60. In other embodiments, the purification device 76 may include a nanofiltration device and / or one or more ion-exchange resins to facilitate the removal of one or more impurities (e.g., sulfates) from the liquid component 68 to produce (e.g., store, contain, or produce) the purified liquid component 60 that has substantially fewer sulfates.Subsequently, the purified liquid component 60, even if at least partially (e.g., at least 10%) saturated with lead salts, can be recycled into the leaching mixture 62 within the leaching vessel οο / οηη / ζζηζ / E / γ. It can also be seen that, in other embodiments, the closed-loop liquid recycling system 77 may not include the purification device 76 (or may omit the purification device 76), and the liquid component 68, isolated by the phase-separation device 64, can be recycled directly once again into the leaching mixture 62 within the leaching vessel 56 without purification. It can be seen that the closed-loop recycling of the liquid component, as currently illustrated, reduces or eliminates additional purification and disposal steps while increasing the lead recovery from system 40. The system 40 illustrated in FIGURE 2 includes a lead salt precipitate treatment device 70 configured to perform the actions described in block 20 of process 10 illustrated in FIGURE 1. In certain embodiments, the lead salt precipitate treatment device 70 may include a reactor that mixes the isolated lead salt precipitate 66 with the base 86 (e.g., a hydroxide, 25-50 wt. sodium hydroxide solution) to produce the lead powder product 74. In certain embodiments, the lead salt precipitate treatment device 70 may be a calciner (e.g., a belt dryer, a batch calciner, a kiln, a spray calciner, a rotary kiln calciner, a spray pyrolysis reactor, or another suitable calcination device).As such, the lead salt precipitate treatment device οο / οηη / ζζηζ / E / γ receives the lead salt precipitate 66 isolated by the phase separation device 64 and reacts the lead salt precipitate 66 with a gas stream (e.g. air, oxygen-enriched air, oxygen-reduced air, nitrogen / air mixtures, water vapor) or base 72 (e.g. hydroxide) to form the lead powder particles 74. For example, in certain embodiments, the lead salt precipitate treatment device 70 can calcine the lead salt precipitate 66 in a mixture of air and an oxygen-reducing agent (e.g., carbon-based materials such as methane, coke, propane, natural gas, etc.) to provide a low-oxygen environment for calcining the lead salt precipitate 66 into the desired lead powder product 74.The 74 lead powder particles can be subsequently used to form an active lead powder material for the construction of new lead-acid batteries (for example, as discussed in blocks 22 and 24 of process 10 in FIGURE 1). As mentioned above with respect to process 10, the lead powder produced by the illustrated system 40 enables the production of new lead-acid batteries that have good to excellent electrical performance. One or more of the described methods, alone or in combination, can provide one or more useful technical effects in the recovery of lead from spent lead-acid batteries. The methods of the present process enable the industrial-scale extraction and purification of lead from spent lead-acid batteries. Furthermore, these methods allow for the removal of various impurities (e.g., insoluble impurities, sulfates, alloy metals) from the recovered lead, thereby avoiding or reducing the formation of certain undesirable combustion byproducts and the associated costs of removing these byproducts from the exhaust stream. Consequently, these methods enable continuous lead purification techniques that are robust to a wide variety of impurities and provide improved control over the purification process parameters.Furthermore, the present methods allow for the recycling of the liquid component of the leaching mixture during the lead recovery and purification process, which improves lead recovery and avoids potentially costly waste disposal. The technical effects and technical problems described in the specification are illustrative and not limiting. It should be noted that the methods described in the specification may have other technical effects and may resolve other technical problems. Although only certain features and embodiments of the invention have been illustrated and described, many modifications and changes may be introduced to those skilled in the art (e.g., variations in sizes, dimensions, structures, shapes, and proportions of the various elements, parameter values ​​(e.g., temperatures, pressures, etc.), assembly arrangements, use of materials, colors, orientations) without materially departing from the novel teachings and advantages of the subject matter described in the claims. The order or sequence of any process or steps of the method may be varied or resequenced according to alternative embodiments. It shall therefore be understood that the appended claims are intended to cover all modifications and changes that fall within the true spirit of the description.Furthermore, in an effort to provide a concise description of exemplary embodiments, not all features of an actual implementation may have been described (i.e., those not related to the best currently contemplated way of carrying out the invention, or those not related to enabling the claimed invention). It should be appreciated that in the development of any actual implementation, as in any engineering or design project, numerous implementation-specific decisions may be made. Such a development effort may be complex or time-consuming; however, it may be a routine task of design, fabrication, and manufacturing for those of ordinary experience who benefit from this description without undue experimentation.

Claims

CLAIMS 1. A system, characterized in that it comprises: a reactor that receives and mixes lead-bearing material, a carboxylate source, and a recycled liquid component to form a leaching mixture that produces a lead carboxylate precipitate; a phase separation device coupled to the reactor, wherein the phase separation device isolates the lead carboxylate precipitate from a liquid component of the leaching mixture; and a closed-loop liquid recycling system coupled to the phase separation device and the reactor, wherein the closed-loop liquid recycling system receives the liquid component isolated by the phase separation device and recycles a substantial portion of the received liquid component back to the reactor as the recycled liquid component.

2. The system according to claim 1, characterized in that the closed-loop liquid recycling system comprises a purification device that removes at least one impurity from the received liquid component before recycling.

3. The system according to claim 2, characterized in that the at least one impurity comprises dissolved sulfates 28.

4. The system according to claim 2, characterized in that the at least one impurity comprises one or more elements other than lead.

5. The system according to claim 4, characterized in that one or more elements comprise sodium, barium, calcium, antimony, arsenic, tin or combinations thereof.

6. The system according to claim 2, characterized in that the purification device comprises: another reactor that mixes calcium hydroxide with the received liquid component; and another phase separation device that subsequently removes a resulting calcium sulfate precipitate from the received liquid component before recycling.

7. The system according to claim 2, characterized in that the purification device comprises a nanofilter or ion exchange resin.

8. The system according to claim 2, characterized in that the dissolved lead carboxylate content of the liquid component is substantially the same before and after the purification device removes at least one impurity.

9. The system according to claim 1, characterized in that the carboxylate source comprises citric acid, a salt of citric acid, acetic acid, a salt of acetic acid or a combination thereof.

10. The system according to claim 1, characterized in that the recycled liquid component is a less saturated solution of 10% in dissolved lead carboxylate.

11. The system according to claim 1, characterized in that the closed-loop liquid recycling system receives wastewater together with the liquid component from the phase separation device and recycles the wastewater together with the liquid component.

12. The system according to claim 1, characterized in that the phase separation device comprises a belt dryer, a filter press, a clarifier, or a cyclone separator.

13. The system according to claim 1, characterized in that it comprises a lead-acid battery processing device configured to receive at least one lead-acid battery and grind the at least one lead-acid battery into the lead-bearing material.

14. The system according to claim 1, characterized in that it comprises a lead carboxylate precipitate treatment device configured to receive the lead carboxyate precipitate isolated by the phase separation device and treat the lead carboxyate precipitate to form lead oxide.

15. The system according to claim 14, characterized in that the lead carboxylate precipitate treatment device comprises a belt dryer, a spray calciner, a stirred crucible reactor, and a rotary kiln calciner.

16. A system, characterized in that it comprises: a closed-loop liquid recycling system coupled to the leaching vessel containing a leaching mixture, wherein the closed-loop liquid recycling system receives a liquid component from the leaching mixture, purifies the received liquid component to generate a purified liquid component having a lower sulfate content than the received liquid component, and supplies the purified liquid component to the leaching vessel as part of the leaching mixture.

17. The system according to claim 16, characterized in that it comprises a phase separation device coupled to the leaching vessel and the closed-loop liquid recycling system, wherein the phase separation device receives the leaching mixture, including the liquid component, from the leaching vessel, isolates a lead carboxylate precipitate from the liquid component of the leaching mixture, and supplies the liquid component to the closed-loop liquid recycling system.

18. The system according to claim 16, characterized in that it comprises the leaching vessel which, during operation, receives and mixes a lead-bearing material, a carboxylate source, and the purified liquid component to form the leaching mixture.

19. The system according to claim 16, characterized in that the purified liquid component includes substantially the same amount of dissolved lead carboxylate as the received liquid component.

20. The system according to claim 16, characterized in that the leaching mixture comprises: water, a lead-bearing material, a carboxylate source, dissolved lead carboxylate, and a lead carboxylate precipitate.

21. The system according to claim 20, characterized in that the carboxylate source comprises citric acid, a metal citrate salt, acetic acid, a metal acetate salt, or a combination thereof.

22. The system according to claim 20, characterized in that the leaching mixture comprises a peroxide.

23. The system according to claim 20, characterized in that the leaching mixture comprises acetic acid acetate or a metal acetate.