Stainless blasting medium
The use of austenitic chromium-manganese steel in stainless blasting mediums enhances hardness and wear resistance, addressing the degradation issues of existing stainless blasting mediums, resulting in extended lifetime and efficient surface treatment.
Patent Information
- Application Number
- CA3160959
- Authority / Receiving Office
- CA · CA
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-11-20
- Filing Date
- 2020-11-19
- Publication Date
- 2026-11-03
- Estimated Expiration
- 2040-11-19
AI Technical Summary
Existing stainless blasting mediums face challenges in hardness and wear behavior, leading to rapid degradation and reduced lifetime, particularly when used with corrosion-resistant metals or alloys.
A stainless blasting medium comprising austenitic chromium-manganese steel, with a composition ranging from 90 wt.-% to 100 wt.-%, ensuring high hardness, ductility, and resistance to corrosion, thereby preventing deformation into brittle martensite during use.
The blasting medium exhibits improved hardness and wear properties, maintaining ductility and extending its lifetime significantly, requiring less frequent replacement compared to conventional materials.
Abstract
Description
Stainless blasting medium The present invention relates to a stainless blasting medium and the use of the stain- less blasting medium. Stainless blasting mediums are known per se and are used in particular in the field of blasting treatment of workpieces. In particular, stainless blasting mediums are used in the blasting treatment of workpieces made of corrosion-resistant metals or metal al- loys, since otherwise the workpieces may corrode due to residues of the blasting me- dium which may remain on the workpiece after the blasting treatment. Despite this problem, metallic blasting mediums are frequently used because they usually exhibit a better wear behavior compared to mineral blasting mediums, thus making them partic- ularly suitable as reusable blasting mediums. Stainless blasting mediums can still offer potential for improvement. In particular, there may be potential for improvement in the hardness of the blasting medium and in the wear behavior of the blasting medium. It is therefore the object of the present invention to provide an improved stainless blast- ing medium. This object is achieved by stainless blasting mediums as disclosed herein. Preferred embodiments of the invention are provided in the description, in the examples or in the figures, wherein further features described or shown in the description, the examples or the figures may individually or in any combination constitute a subject matter of the invention, if the context does not clearly indicate the contrary.a The invention proposes a stainless blasting medium comprising blasting medium ele- ments containing an austenitic chromium-manganese steel, wherein the blasting me- dium comprises the blasting medium elements containing an austenitic chromium- manganese steel preferably in a range from ≥ 90 wt.-% to ≤ 100 wt.-%, based on the total weight of the stainless blasting medium. In the sense of the present invention, the term "blasting medium" means an auxiliary material which can be used in the blasting technology for surface treatment and which can be directed at high velocity onto a workpiece or a material to be blasted. In the sense of the present invention, the term "stainless" means the property of being substantially inert to reactions with the environment and / or natural atmospheres. In particular, "stainless blasting mediums" are understood to mean blasting mediums that under normal conditions do substantially not react with ambient air and / or atmospheric humidity. In the sense of the present invention, "blasting medium elements" are understood to mean individual elements of the blasting medium such as individual grains, spheres or particles. In the sense of the present invention "chromium-manganese steel" is understood to mean a steel to which chromium and manganese have been added as main alloying elements. In the sense of the present invention steel is a material composed mainly of iron. In the sense of the present invention, "austenitic chromium-manganese steel" is un- derstood to mean a chromium-manganese steel which mainly has an austenitic struc- ture. Due to the austenitic chromium-manganese steel of the stainless blasting medium, it can advantageously be achieved that the blasting medium is particularly resistant to corrosion. In addition, it can be achieved that the blasting medium elements have a sufficiently high hardness in order to achieve particularly good results when using the blasting medium and, at the same time, a sufficient ductility so that the blasting medium has a particularly good lifetime. Without being bound by any theory, it is assumed that the austenitic chromium-manganese steel does not form deformation martensite dur- ing cold forming, as occurs when the blasting medium strikes onto the material to be blasted, which can quickly make known blasting mediums brittle and thus leads to rapid wear. In particular, compared to known blasting mediums made of chromium-nickel steel, an improved hardness and an improved lifetime of the stainless blasting medium can be achieved. In addition, compared to blasting mediums made of chromium-nickel steel, it can be advantageously achieved that the hardness of the blasting medium increases during use due to the very good work-hardening tendency, without reducing the ductil- ity properties. It can be provided that the blasting medium comprises other blasting medium ele- ments, for example metallic or mineral blasting medium elements, in addition to the blasting medium elements containing an austenitic chromium-manganese steel. Preferably, it may be provided that the blasting medium comprises the blasting medium elements containing an austenitic chromium-manganese steel in a range from ≥ 95 wt.- % to ≤ 100 wt.-%, based on the total weight of the stainless blasting medium, particu- larly preferably from <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 98 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 100 wt.-%. Preferably, it may be provided that the blasting medium consists of the blasting medium elements containing an austenitic chromium-manganese steel. Preferably, it may be provided that the blasting medium elements containing the aus- tenitic chromium-manganese steel consist of the austenitic chromium-manganese steel. By means of the stainless blasting medium described above, it can be advantageously achieved that the advantageous properties of the austenitic chromium-manganese steel, in particular its hardness and wear behavior, can be particularly well utilized for the stainless blasting medium. Preferably, it may be provided that the austenitic chromium-manganese steel com- prises <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 10 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 30 wt.-% chromium and <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 6 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 30 wt.-% manganese, wherein the weight percentage is based on the total weight of the austenitic chromium- manganese steel. Preferably, it may be provided that the austenitic chromium-manganese steel com- prises: [Image disponible dans le document PDF, Image available in the PDF document] wherein the weight percentage is based on the total weight of the austenitic chromium- manganese steel, preferably wherein the austenitic chromium-manganese steel com- prises the carbon and the nitrogen together in an amount of <com:Math><semantics>≥0.2<annotation encoding="application / x-tex">\geq 0.2< / annotation>< / semantics>< / com:Math> wt.-% to <com:Math><semantics>≤1.3<annotation encoding="application / x-tex">\leq 1.3< / annotation>< / semantics>< / com:Math> wt.-%. It should be understood that impurities occurring due to melting are included in the composition. Preferably, it can be provided that the austenitic chromium-manganese steel consists of the composition described above. By means of the above-described compositions, it can advantageously be achieved that the blasting medium has a particularly high hardness and that the hardness of the blasting medium is advantageously further increased to a particularly high degree dur- ing use. In addition, it can be achieved that the blasting medium further exhibits a good corrosion resistance. Preferably, it may be provided that the austenitic chromium-manganese steel com- prises <com:Math><semantics>≥15<annotation encoding="application / x-tex">\geq 15< / annotation>< / semantics>< / com:Math> wt.-% to <com:Math><semantics>≤19<annotation encoding="application / x-tex">\leq 19< / annotation>< / semantics>< / com:Math> wt.-% chromium and <com:Math><semantics>≥17<annotation encoding="application / x-tex">\geq 17< / annotation>< / semantics>< / com:Math> wt.-% to <com:Math><semantics>≤21<annotation encoding="application / x-tex">\leq 21< / annotation>< / semantics>< / com:Math> wt.-% manganese, wherein the weight percentage is based on the total weight of the austenitic chromium- manganese steel. Preferably, it may be provided that the austenitic chromium-manganese steel com- prises: <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0.1 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.3 wt.-% carbon, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0.55 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.65 wt.-% nitrogen, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 15 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 19 wt.-% chromium, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 17 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 21 wt.-% manganese, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0.05 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.15 wt.-% molybdenum, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0.7 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 1.1 wt.-% silicon, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.5 wt.-% copper, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.5 wt.-% cobalt, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.1 wt.-% nickel, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.5 wt.-% titanium, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.5 wt.-% vanadium, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.5 wt.-% niobium, and balance iron, wherein the weight percentage is based on the total weight of the austenitic chromium- manganese steel, preferably wherein the austenitic chromium-manganese steel com- prises carbon and nitrogen together in an amount of <com:Math><semantics>≥0.7<annotation encoding="application / x-tex">\geq 0.7< / annotation>< / semantics>< / com:Math> wt.-% to <com:Math><semantics>≤0.9<annotation encoding="application / x-tex">\leq 0.9< / annotation>< / semantics>< / com:Math> wt.-%. It is to be understood that impurities occurring due to melting are included in the com- position. Preferably, it may be provided that the austenitic chromium-manganese steel com- prises: <com:Math><semantics>≥0.15 wt.-% to ≤0.25 wt.-% carbon,<annotation encoding="application / x-tex">\geq 0.15 \text{ wt.-}\% \text{ to } \leq 0.25 \text{ wt.-}\% \text{ carbon},< / annotation>< / semantics>< / com:Math> <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0.55 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.60 wt.-% nitrogen, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 16 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 18 wt.-% chromium, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 18 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 20 wt.-% manganese, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0.05 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.15 wt.-% molybdenum, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0.8 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 1.0 wt.-% silicon, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.2 wt.-% copper, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.2 wt.-% cobalt, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.2 wt.-% nickel, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.2 wt.-% titanium, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.2 wt.-% vanadium, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.2 wt.-% niobium, and balance iron, wherein the weight percentage is based on the total weight of the austenitic chromium- manganese steel, preferably wherein the austenitic chromium-manganese steel com- prises carbon and nitrogen together in an amount of ≥ 0.7 wt.-% to ≤ 0.85 wt.-%. It is to be understood that impurities occurring due to melting are included in the com- position. Preferably, it may be provided that the austenitic chromium-manganese steel consists of the composition described above. Surprisingly, it has been shown that blasting mediums comprising the composition de- scribed above exhibit a particularly long lifetime. Preferably, it may be provided that the austenitic chromium-manganese steel com- prises substantially no martensitic structural constituents due to the primary manufac- turing process or substantially does not form martensitic structural constituents during cold working. Preferably, it may be provided that the austenitic chromium-manganese steel com- prises substantially no martensitic structural constituents due to the primary manufac- turing process and substantially does not form martensitic structural constituents dur- ing cold working. Thus, it can be achieved in an advantageous manner, that the blasting medium does not become softer during use. In addition, it can be advantageously achieved that the blasting medium does not quickly become brittle during use despite increasing hard- ness, while maintaining a constant ductility, resulting in particularly advantageous wear properties. Preferably, it may be provided that the austenitic chromium-manganese steel com- prises ≤ 5 wt.-% of martensitic structural constituents due to the primary manufacturing process and / or forms ≤ 5 wt.-% of martensitic structural constituents during cold work- ing, more preferably <com:Math><semantics>≤1<annotation encoding="application / x-tex">\leq 1< / annotation>< / semantics>< / com:Math> wt.-%, particularly preferably <com:Math><semantics>≤0.1<annotation encoding="application / x-tex">\leq 0.1< / annotation>< / semantics>< / com:Math> wt.-%, wherein the weight percentage is based on the total weight of the austenitic chromium-manganese steel. Preferably, it can be provided that the blasting medium elements are essentially con- cave, preferably elliptical, particularly preferably spherical. In this way it can be advantageously achieved that the blasting medium elements are particularly homogeneously deformed during use and the wear properties are further improved. Preferably, it may be provided that <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 90 wt.-%, more preferably <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 95 wt.-%, in particular ≥ 99 wt.-%, of the blasting medium elements are substantially concave, preferably el- liptical, more preferably spherical, based on the total amount of blasting medium ele- ments. Preferably, it may be provided that the blasting medium has a bulk density measured according to DIN EN ISO 60:2000-01 in a range from <com:Math><semantics>≥3.5<annotation encoding="application / x-tex">\geq 3.5< / annotation>< / semantics>< / com:Math> g / cm<com:Sup>3< / com:Sup> to <com:Math><semantics>≤5<annotation encoding="application / x-tex">\leq 5< / annotation>< / semantics>< / com:Math> g / cm<com:Sup>3< / com:Sup>, prefer- ably from <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 4.1 g / cm<com:Sup>3< / com:Sup> to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 4.6 g / cm<com:Sup>3< / com:Sup>. Preferably, it may be provided that the blasting medium elements each have a shortest and a longest diameter, wherein the blasting medium has a proportion of blasting me- dium elements whose longest diameter is more than twice as large as their shortest diameter, measured according to DIN EN ISO 11125-5:2018-12, of ≤ 15%, preferably of <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 5%. Preferably, it can be provided that the blasting medium elements have an average equivalent diameter D<com:Sub>50< / com:Sub> measured according to DIN 66165-2:2016-08 in a range from ≤ 3 mm to ≥ 0.01 mm, preferably from ≤ 2.5 mm to ≥ 0.05 mm, more preferably from ≤ 1 mm to <com:Math><semantics>≥0.09<annotation encoding="application / x-tex">\ge 0.09< / annotation>< / semantics>< / com:Math> mm. By means of the parameters described above, it can advantageously be achieved that the blasting medium can be used particularly efficiently. Preferably, it can be provided that the blasting medium elements have a first average equivalent diameter D<com:Sub>50< / com:Sub> as virgin grain before use and a second average equivalent diameter D<com:Sub>50< / com:Sub> as an operating mixture after use, measured according to DIN 66165- 2:2016-08, wherein the second average equivalent diameter is smaller than the first average equivalent diameter, preferably at least 5% smaller, particularly preferably at least 10% smaller. In the sense of the present invention, "virgin grain" is understood to mean the blasting medium element before it first impinges onto the material to be blasted. "Blasting me- dium element after a use" is understood in the sense of the present invention to mean a mixture of blasting medium elements which has been used for treating a material to be blasted. In particular, it is to be understood to mean an operating mixture, the weight of which has been completely balanced in total at least once with virgin grain by com- pensating for weight loss caused by use. In this way, it can be advantageously achieved that blasting medium elements change only slightly during use up to material fatigue. Preferably, it can be provided that the blasting medium elements have a hardness as virgin grain before use, measured according to DIN EN ISO 6507-1:2018, in a range of ≥ 200 HV 0.1 to ≤ 400 HV 0.1, preferably from ≥ 280 HV 0.1 to ≤ 360 HV 0.1. In this way it can advantageously be achieved that the blasting medium has a sufficient hardness for a wide range of applications and, at the same time, has a sufficient duc- tility for particularly advantageous wear properties. Preferably, it can be provided that the blasting medium elements have a first hardness as virgin grain before use and a second hardness as an operating mixture after use, measured according to DIN EN ISO 6507-1:2018, wherein the second hardness is greater than the first hardness, preferably at least 60% greater, particularly preferably at least 65% greater. In this way, it can be advantageously achieved that an even improved hardness is set for an operating mixture. Preferably, it can be provided that the blasting medium in use has a lifetime, measured at an average equivalent diameter D<com:Sub>50< / com:Sub> measured according to DIN 66165-2:2016-08 in a range of ≤ 0.3 mm to ≥ 0.01 mm by means of a lifetime test according to SAE J445- Aug2013, 5.3 "100% Replacement Method A" up to an accumulated loss of 100%, of <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 25,000 cycles, preferably of <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 28,000 cycles, particularly preferably of <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 35,000 cy- cles. In this way it can advantageously be achieved that the blasting medium is particularly efficient and is required to be replaced less frequently compared to known stainless blasting mediums. Preferably, it can be provided that the blasting medium in use has an Almen intensity at the saturation point, measured at an average equivalent diameter D<com:Sub>50< / com:Sub> measured according to DIN 66165-2:2016-08 in a range of <com:Math><semantics>≤0.3<annotation encoding="application / x-tex">\leq 0.3< / annotation>< / semantics>< / com:Math> mm to <com:Math><semantics>≥0.01<annotation encoding="application / x-tex">\geq 0.01< / annotation>< / semantics>< / com:Math> mm by means of an Almen strip N according to SAE J445-Aug2013 5.4 "Transmitted Energy Arc Height Test", of ≥ 0.20 mm. In the sense of the present invention, the saturation point is to be understood as the earliest point of a measurement curve of the arc height of an Almen strip against the blasting time at which a doubling of the blasting time causes at most a ten percent increase in the arc height. Advantageously, it can be achieved that the blasting medium has an improved energy transfer when the blasting medium impinges onto the surface to be treated compared to known blasting mediums with lower Almen intensity at the saturation point. Thus, advantageously, a more efficient blasting medium treatment can be achieved. The invention further proposes the use of a stainless blasting medium as described above, for blasting treatment of surfaces, preferably metallic and non-metallic surfaces, such as workpieces, in particular stainless workpieces. Further advantages and advantageous embodiments of the blasting medium according to the invention are illustrated by the examples and figures and explained in the follow- ing description. It should be noted that the examples and figures are descriptive only and are not intended to limit the invention in any way. Example A A stainless blasting medium according to the invention comprising blasting medium elements consisting of austenitic chromium-manganese steel has been provided, com- prising: 0.2 wt.-% carbon, 0.57 wt.-% nitrogen, 17 wt.-% chromium, 19.1 wt.-% manganese, 0.1 wt.-% molybdenum, 0.9 wt.-% silicon, <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.1 wt.-% copper, <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.1 wt.-% cobalt, <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.1 wt.-% nickel, <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.1 wt.-% titanium, ≤ 0.1 wt.-% vanadium, ≤ 0.1 wt.-% niobium, and balance iron, based on the total weight of the austenitic chromium-manganese steel. The austenitic chromium-manganese steel included essentially no martensitic struc- tural constituents. The blasting medium elements were spherical with a content of non- spherical particles of less than 15%. The blasting medium elements had an average equivalent diameter D<com:Sub>50< / com:Sub> measured according to DIN 66165-2:2016-08 in a range of ≤ 0.3 mm to ≥ 0.01 mm and a hardness measured according to DIN EN ISO 6507- 1:2018, of 324 ± 14 HV 0.1. The lifetime was investigated by use of a Shot Testing Machine (hereinafter referred to as tester) in accordance with SAE J445 Aug2013. For this purpose, the tester was first calibrated with a calibration blasting medium. For the lifetime test, 100 g of the blasting medium according to the invention from Example A were introduced into the tester. For the measurement, the sample was shot onto the target for 500 cycles each at a shaft speed of 7800 / min and a drum speed of 25 / min. After 500 cycles, the entire sample was sieved through a 50 µm sieve and the residue was weighed. From this, the loss was calculated and plotted against the number of cycles. The residue was filled up to 100 g with virgin grain of the blasting medium of the invention from Example A and placed in the tester again. The procedure was repeated until the loss reached 100 g in total. The number of cycles required for this quantifies the lifetime of the blast- ing medium. For the blasting medium according to the invention of Example A, the lifetime up to an accumulated loss of 100%, was ≥ 36,000 cycles. The blasting medium obtained after the lifetime test corresponds to an operating mix- ture. The average equivalent diameter D<com:Sub>50< / com:Sub> of the operating mixture measured accord- ing to DIN 66165-2:2016-08 remained in the range of <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 0.3 mm to <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 0.01 mm, wherein an overall broader distribution compared to the virgin grain was observed. The operat- ing mixture had a hardness measured according to DIN EN ISO 6507-1:2018 of 575 ± 14 HV 0.1, which was more than 65% harder than the virgin grain. The Almen intensity at the saturation point was also examined by use of a Shot Testing Machine according to SAE J445 Aug2013. For this purpose, the sample was shot at a shaft speed of 7800 / min and a drum speed of 25 / min onto an Almen strip N, thickness 0.79 mm. After every 10 cycles, the arc height of the Almen strip was measured with an Almen dial gauge and plotted against the cycles (Fig. 4). An examination of the curve of the arc height showed that at 40 cycles the saturation point was reached, i.e. the earliest point at which a doubling of the blasting time (number of cycles) caused at most a ten percent increase in the arc height. Thus, an Almen intensity 0.20 mm was obtained at the saturation point for the blasting medium according to example A. Comparative example B A stainless blasting medium comprising blasting medium elements consisting of chro- mium-nickel steel has been provided, comprising: 0.2 wt.-% carbon, <com:Math><semantics>≥<annotation encoding="application / x-tex">\geq< / annotation>< / semantics>< / com:Math> 18 wt.-% to <com:Math><semantics>≤<annotation encoding="application / x-tex">\leq< / annotation>< / semantics>< / com:Math> 19 wt.-% chromium, 8 wt.-% nickel, ≤ 2 wt.-% manganese, ≤ 3 wt.-% silicon, and balance iron, based on the total weight of the chromium-nickel steel. Compared to the blasting medium of Example A according to the invention, the blasting medium of the Comparative Example B with a comparable equivalent diameter D<com:Sub>50< / com:Sub> in a range from ≤ 0.3 mm to ≥ 0.01 mm, measured according to DIN 66165-2:2016-08 had a lower hardness, namely 301 ± 11 HV 0.1, measured according to DIN EN ISO 6507-1:2018. For the Comparative Example, a lifetime up to an accumulated loss of 100% of only < 23,500 cycles was obtained. The average equivalent diameter D<com:Sub>50< / com:Sub> of the operating mixture of Comparative Example B measured according to DIN 66165-2:2016-08 hardly changed compared to the virgin grain. Moreover, the operating mixture had a hardness measured according to DIN EN ISO 6507-1:2018 of only 512 ± 22 HV 0.1 and was thus significantly lower than that of the blasting medium of Example A accord- ing to the invention. In terms of the Almen intensity, an Almen intensity at the saturation point after 40 cycles of only 0.19 mm was obtained for the Comparative Example. In the drawings: Fig. 1 is a diagram of the sieve analysis of virgin grain and operating mixture of the blasting medium according to the invention according to Example A and the blasting medium made of chromium-nickel steel according to Comparative Ex- ample B; Fig. 2 is a diagram of the hardness analysis of virgin grain and operating mixture of the blasting medium according to the invention according to Example A and the blasting medium made of chromium-nickel steel according to Comparative Example B; Fig. 3 is a diagram of the lifetime test of the blasting medium according to the inven- tion according to Example A and the blasting medium made of chromium- nickel steel according to Comparative Example B; and Fig. 4 is a diagram of the Almen intensity of the blasting medium according to the invention according to Example A and the blasting medium made of chromium- nickel steel according to Comparative Example B. Fig. 1 shows the diagram of the sieve analysis of virgin grain and operating mixture of the blasting medium according to the invention according to Example A (CrMn austen- ite) and the blasting medium made of chromium-nickel steel according to Comparative Example B (CrNi austenite). Both blasting mediums have almost identical equivalent diameters as virgin grain. Compared to the operating mixture of Comparative Example B, the operating mixture of the blasting medium according to the invention comprises more components with a smaller equivalent diameter. Fig. 2 shows the diagram of the hardness analysis of virgin grain and operating mixture of the blasting medium according to the invention according to Example A and the blasting medium made of chromium-nickel steel according to Comparative Example B. Both virgin grain and operating mixture of the blasting medium according to the inven- tion of Example A are respectively advantageously harder than virgin grain or operating mixture of the blasting medium of Comparative Example B. In addition, the hardness increases between virgin grain and operating mixture for the blasting medium accord- ing to the invention more than for the Comparative Example. Fig. 3 shows the diagram of the lifetime test of the blasting medium according to the invention according to Example A and the blasting medium made of chromium-nickel steel according to Comparative Example B. The loss plotted against the number of cycles of the blasting medium according to the invention is much flatter compared to the loss of the Comparative Example, resulting advantageously in an longer lifetime. Fig. 4 shows the diagram of the Almen intensity test of the blasting medium according to the invention according to Example A and the blasting medium made of chromium- nickel steel according to Comparative Example B. After 40 cycles, both blasting medi- ums exhibit a saturation point at which a doubling of the number of cycles results in at most a ten percent increase in the deflection (arc height) of the Almen strip. Here, the blasting medium according to Example A exhibits an overall greater Almen intensity, from which, due to the comparability of the test conditions, a comparatively improved energy transfer during blasting can be concluded compared to Comparative Example B.
Claims
1. Stainless blasting medium consisting of blasting medium elements consisting of an austenitic chromium-manganese steel.
2. Stainless blasting medium according to claim 1, wherein the austenitic chro- mium-manganese steel consists of [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] [Image disponible dans le document PDF, Image available in the PDF document] balance iron, wherein the weight percentage is based on the total weight of the aus- tenitic chromium-manganese steel.
3. Stainless blasting medium according to claim 2, wherein the austenitic chro- mium-manganese steel comprises carbon and nitrogen together in an amount from ≥ 0.2 \geq 0.2 wt.-% to ≤ 1.3 \leq 1.3 wt.-%.
4. Stainless blasting medium according to any one of claims 1 to 3, wherein the austenitic chromium-manganese steel consists of ≥ 0.1 wt.- % to ≤ 0.3 wt.- % carbon, \geq 0.1 \text{ wt.-}\% \text{ to } \leq 0.3 \text{ wt.-}\% \text{ carbon,} ≥ 0.55 wt.- % to ≤ 0.65 wt.- % nitrogen, \geq 0.55 \text{ wt.-}\% \text{ to } \leq 0.65 \text{ wt.-}\% \text{ nitrogen,} ≥ \geq 15 wt.-% to ≤ \leq 19 wt.-% chromium, ≥ \geq 17 wt.-% to ≤ \leq 21 wt.-% manganese, ≥ \geq 0.05 wt.-% to ≤ \leq 0.15 wt.-% molybdenum, ≥ 0.7 \geq 0.7 wt.-% to ≤ 1.1 \leq 1.1 wt.-% silicon, ≥ 0 \geq 0 wt.-% to ≤ 0.5 \leq 0.5 wt.-% copper, ≥ \geq 0 wt.-% to ≤ \leq 0.5 wt.-% cobalt, ≥ 0 \geq 0 wt.-% to ≤ 0.1 \leq 0.1 wt.-% nickel, ≥ 0 \geq 0 wt.-% to ≤ 0.5 \leq 0.5 wt.-% titanium, ≥ 0 \geq 0 wt.-% to ≤ 0.5 \leq 0.5 wt.-% vanadium, ≥ 0 \geq 0 wt.-% to ≤ 0.5 \leq 0.5 wt.-% niobium, and balance iron, wherein the weight percentage is based on the total weight of the chro- mium-manganese steel.
5. Stainless blasting medium according to claim 4, wherein the austenitic chro- mium-manganese steel comprises carbon and nitrogen together in an amount from ≥ 0.7 \geq 0.7 wt.-% to ≤ 0.9 \leq 0.9 wt.-%.
6. Stainless blasting medium according to any one of the preceding claims 1 to 5, wherein the austenitic chromium-manganese steel comprises substantially no martensitic structural constituents due to the primary manufacturing process or does not form martensitic structural constituents during cold working. 7 Stainless blasting medium according to any one of the preceding claims 1 to 6, wherein the blasting medium elements are elliptical.
8. Stainless blasting medium according to claim 7, wherein the blasting medium elements are spherical.
9. Stainless blasting medium according to any one of the preceding claims 1 to 8, wherein the blasting medium has a bulk density measured according to DIN EN ISO 60:2000-01 in a range from ≥ \geq 3.5 g / cm 3 to ≤ \leq 5 g / cm 3 .
10. Stainless blasting medium according to claim 9, wherein the bulk density meas- ured according to DIN EN ISO 60:2000-01 is in a range from ≥ \geq 4.1 g / cm 3 to ≤ \leq11. Stainless blasting medium according to any one of the preceding claims 1 to 10, wherein the blasting medium elements respectively have a shortest and a long- est diameter, wherein the blasting medium has a proportion of blasting medium elements whose longest diameter is more than twice as large as their shortest diameter, measured according to DIN EN ISO 11125-5:2018-12, of ≤ 15%.
12. Stainless blasting medium according to claim 11, wherein the proportion of blasting medium elements whose longest diameter is more than twice as large as their shortest diameter is ≤ 5 % \leq 5\% .
13. Stainless blasting medium according to any one of the preceding claims 1 to 12, wherein the blasting medium elements have an average equivalent diameter D 50 measured according to DIN 66165-2:2016-08 in a range from ≤ 3 mm to ≥14. Stainless blasting medium according to claim 13, wherein the average equiva- lent diameter D 50 D_{50} is from ≤ 2.5 \leq 2.5 mm to ≥ 0.05 \geq 0.05 mm.
15. Stainless blasting medium according to claim 14, wherein the average equiva- lent diameter D 50 D_{50} is from ≤ 1 \leq 1 mm to ≥ 0.09 \geq 0.09 mm.
16. Stainless blasting medium according to any one of the preceding claims 1 to 15, wherein the blasting medium elements have a first average equivalent diameter D 50 as virgin grain before use and have a second average equivalent diameter D 50 as operating mixture after use, measured according to DIN 66165-2:2016- 08, wherein the second average equivalent diameter is smaller, than the first average equivalent diameter.
17. Stainless blasting medium according to claim 16, wherein the second average equivalent diameter is smaller by at least 5%, than the first average equivalent diamenter.
18. Stainless blasting medium according to claim 17, wherein the second average equivalent diameter is smaller by at least 10%, than the first average equivalent diameter.
19. Stainless blasting medium according to any one of the preceding claims 1 to 18, wherein the blasting medium elements have a hardness as virgin grain before use, measured according to DIN EN ISO 6507-1:2018, in a range from ≥ 200 HV 0.1 to ≤ 400 HV 0.1 . 0.1 \text{ to} \le 400 \text{ HV } 0.1.
20. Stainless blasting medium according to claim 19, wherein the hardness as virgin grain before use is from ≥ \geq 280 HV 0.1 to ≤ \leq 360 HV 0.1.
21. Stainless blasting medium according to any one of the preceding claims 1 to 20, wherein the blasting medium elements have a first hardness as virgin grain be- fore use and a second hardness as operating mixture after use, measured ac- cording to DIN EN ISO 6507-1:2018 -, wherein the second hardness is greater than the first hardness.
22. Stainless blasting medium according to claim 21, wherein the second hardness is greater than the first hardness by at least 60% greater.
23. Stainless blasting medium according to claim 22, wherein the second hardness is greater than the first hardness by at least 65%.
24. Stainless blasting medium according to any one of the preceding claims 1 to 23, wherein the blasting medium in use has a lifetime, measured at an average equivalent diameter D 50 , measured according to DIN 66165-2:2016-08, in a range from ≤ 0.3 mm to ≥ 0.01 mm by means of a lifetime test according to SAE J 445 5.3 up to an accumulated loss of 100%, of ≥ 25,000 cycles.
25. Stainless blasting medium according to claim 24, wherein the lifetime is of ≥ 28,000 cycles.
26. Stainless blasting medium according to claim 25, wherein the lifetime is of ≥ 35,000 cycles.
27. Use of a stainless blasting medium according to any one of the preceding claims 1 to 26, for the blasting treatment of surfaces.
28. Use according to claim 27, wherein the surface is metallic and non-metallic sur- faces.
29. Use according to claim 27, wherein the surface is of a workpiece.
30. Use according to claim 29, wherein the workpiece is a stainless workpiece.