technical field
[0001] The invention relates to a PET material, in particular to a modified flame-retardant PET material, which belongs to the technical field of plastic materials. Background technique
[0002] Polyethylene terephthalate PET is an important engineering plastic, which has excellent physical and mechanical properties in a wide temperature range, and can still maintain excellent electrical insulation properties under high temperature and high frequency. It is used to produce PET sheets are widely used in electronics, food, medicine, office supplies, toys and other industries. However, PET also has many shortcomings, such as: poor impact performance, low tensile and bending strength, slow crystallization, long molding cycle, poor flame retardancy, etc., which limit its application in many aspects, so it is necessary to carry out research on PET materials. Certain modifications are required to obtain PET materials that meet the requirements of various applicatio...
Examples
Embodiment Construction
[0011] The preferred embodiments of the present invention are described in detail below, so that the advantages and features of the present invention can be more easily understood by those skilled in the art, so as to define the protection scope of the present invention more clearly.
[0012] In the modified flame-retardant PET material mentioned in the present invention, the raw materials and percentage content ratio of the PET material are: polyethylene terephthalate 70%-80%, modified montmorillonite 2% -6%, nano-titanium nitride 2%-4%, composite flame retardant 10%-20%.
[0013] To further explain, the raw materials of PET materials and their percentage ratios are: polyethylene terephthalate 76%-78%, modified montmorillonite 4%-5%, nano-titanium nitride 3%-4 %, composite flame retardant 15%-17%; modified montmorillonite is obtained by modifying phosphorus-based montmorillonite with modifier toluene-2,4-diisocyanate, and its average particle size is about 12nm ; The average...