A three-dimensional flexible organic field-effect transistor
By adopting vertical channel structure and multi-layer superposition technology in organic field effect transistors, the problem of difficult channel length reduction in planar structures is solved, the output current and integration are improved, and the field effect transistor with flexible three-dimensional structure is realized, supporting Application of high-integration circuits.
Patent Information
- Application Number
- CN201610031166.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2016-01-14
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2036-01-14
AI Technical Summary
Due to the limitations of lithography technology, the channel length of the existing organic field effect transistors is difficult to reduce, resulting in low output current, high operating voltage and low operating frequency, which cannot meet the needs of large-scale and high-integrated circuits.
A flexible organic three-dimensional structure field effect transistor with vertical channel structure is used to prepare an organic semiconductor layer through evaporation technology to form a vertical channel with good film uniformity and small thickness, combined with a grid-shaped metal gold electrode extension layer and a multi-layer superposition structure. Implement the expansion of three-dimensional circuits.
It significantly improves the source and drain current, achieves effective reduction of channel length, enhances carrier mobility, supports multi-layer device superposition and inter-layer connection, and improves integration and circuit performance.
Smart Images

Figure CN105470389B_ABST
Abstract
Description
[Technical field]
[0001] The invention belongs to the field of organic semiconductor devices, and in particular relates to a flexible organic field effect transistor with a three-dimensional structure. [Background technology]
[0002] With the deepening of the study of traditional OFETs, the research on the application of functionalization, integration, solution, etc. has made great progress and has become a frontier hotspot in the current research of organic electronics / molecular electronics. Compared with inorganic materials, organic materials have many inherent advantages in low-cost, large-area, flexible circuits. For example, its film-forming process is simple, the material type is wide, it is compatible with flexible substrates, it is small in size and light, and it is low in cost. It is easy to use spin coating and dip coating technology to prepare various flexible devices and circuits on a large area. In addition, for organic semiconductor materials, people can easily achieve the regulation of device performance by changing the molecular structure, so that organic semiconductor materials can be designed according to the application requirements of the device. The large-scale industrial production in the fields of low-cost, large-area flexible display, flexible sensors, etc. has a very broad prospect. The main applications are: flexible display driver, electronic newspaper, human body sensor, active matrix circuit, low-cost fully printed flexible RFID tag, commercial flexible RFID tag, etc.
[0003] Traditional organic field effect transistors mainly include two structures: top gate and bottom gate. The top gate includes two types: bottom contact type and top contact type, and the bottom gate includes two types: bottom contact type and top contact type. Due to the characteristics of OTFT organic materials themselves, organic field effect transistors generally adopt a bottom gate structure. The so-called top contact means that the source and drain electrodes are at the top and the gate is at the bottom, while the bottom contact means that the source and drain electrodes are at the bottom and the gate is at the top. The main feature of the top-contact OTFT is that the source and drain electrodes are far away from the substrate, and the organic semiconductor layer and the insulating layer are directly connected. During the manufacturing process, the insulating layer can be modified to change the film structure and morphology of the semiconductor, thereby improving the carrier mobility of the device. At the same time, the area of the semiconductor layer affected by the gate electric field in this structure is larger than that of the device structure with the source and drain at the bottom, so it has a higher carrier mobility; the main feature of the bottom-contact OTFT is that the organic semiconductor layer is evaporated on the source and drain electrodes, and the device structure with the source and drain electrodes at the bottom can use the photolithography method to prepare the gate and source and drain electrodes at one time, which can simplify the process preparation. Moreover, for organic sensors, the semiconductor layer needs to be exposed to the test environment without covering. At this time, the device structure with the source and drain electrodes at the bottom has a relatively large advantage.
[0004] However, the existing planar structure of organic field effect transistors has performance limitations due to many reasons. For example, it is very difficult to further reduce the channel length due to the limitation of photolithography technology. In addition, the organic field effect transistor itself has the characteristics of low mobility, resulting in low output current, high operating voltage and low operating frequency. There are two main ways to increase the output current at the device level, namely increasing the mobility and reducing the channel width. In terms of channel length, since the field effect of the planar structure is limited in reducing the channel length, we use organic field effect transistors prepared with vertical channels. The channel length of the field effect transistor with this structure is determined by the thickness of the organic semiconductor layer, and the organic semiconductor layer is prepared by evaporation technology. The film formed in this way has good uniformity and the minimum thickness can reach several nanometers. Due to the significant reduction in channel length, the source-drain current can be significantly improved. This channel length is difficult to achieve in field effect transistors with horizontal channels. In large-scale, high-integration circuits, single-layer devices cannot meet the required requirements. Since the thickness of organic devices is very thin, multi-layer devices are usually stacked in actual circuit applications to save space and improve integration. Another important feature of vertical channel organic field effect transistors is that they can be used as connecting devices between layers, expanding the two-dimensional circuit to a three-dimensional spatial structure. In summary, vertical channel field effect transistors are indispensable in future organic integrated circuits, and the present invention is of great significance to the true realization of organic field effect transistor circuits. [Summary of the invention]
[0005] The purpose of the present invention is to provide a flexible organic three-dimensional structure field effect transistor.
[0006] The present invention provides a flexible organic three-dimensional structure field effect transistor, the structure of which is as follows Figure 1 As shown, it includes a first source electrode (101), a second source electrode (102), a first drain electrode (201), a second drain electrode (202), an electrode extension layer (203), a first organic semiconductor layer (301), a second organic semiconductor layer (302), a first insulating layer (401), a second insulating layer (402), a gate electrode (5), and a flexible substrate (6);
[0007] Wherein: the flexible substrate, the gate electrode, and the second insulating layer are stacked in sequence, the electrode extension layer and the second drain electrode are respectively located on both sides of the second insulating layer, and the electrode extension layer and the second drain electrode are connected; the second organic semiconductor layer and the second source electrode are respectively located on the second drain electrode, and the width of the second organic semiconductor layer and the second source electrode is the same as that of the second drain electrode; the first insulating layer covers the electrode extension layer, the second organic semiconductor layer, and the second source electrode; the first organic semiconductor layer is located on the first insulating layer, and the first source electrode and the first drain electrode are respectively located on both sides of the first organic semiconductor layer. The second source electrode is a grid-shaped metal gold, and the material constituting the electrode extension layer is metal gold. The material constituting the first source electrode, the first drain electrode, and the second drain electrode is metal aluminum, the material constituting the first organic semiconductor layer and the second organic semiconductor layer is one or more of copper phthalocyanine, pentacene, and P3HT, the material constituting the first insulating layer and the second insulating layer is PVA, the material constituting the gate electrode is ITO, and the material constituting the flexible substrate is polyethylene terephthalate (PET) or polyimide (PI); the overall area of the first organic semiconductor layer, the first source electrode, and the first drain electrode is less than or equal to the second source electrode.
[0008] The method for preparing the above-mentioned flexible organic three-dimensional structure field effect transistor provided by the present invention comprises the following steps:
[0009] (1) The flexible substrate was ultrasonically cleaned in ethanol, acetone, and deionized water solution for 10 min in sequence, and then dried with nitrogen gas;
[0010] (2) preparing a second insulating layer on the flexible substrate by spin coating, wherein a 20 wt% PVA aqueous solution was spin coated at a rotation speed of 4000 rpm, the spin-coated PVA was irradiated with 365 nm wavelength (8 W) ultraviolet light for 10 min, and placed in a vacuum drying oven at 200° C. for cross-linking for 2 hours, and then annealed at 60° C. for 30 min;
[0011] (3) preparing a second source electrode and an electrode extension layer on the second insulating layer, preparing a grid-shaped sacrificial layer on the second insulating layer by using a photolithography process, and then preparing a layer of metal gold by vacuum thermal evaporation, controlling the evaporation rate and time so that the thickness of the evaporated metal gold is less than the thickness of the grid-shaped sacrificial layer, and forming a grid-shaped metal gold by releasing the sacrificial layer; the electrode extension layer is prepared by vacuum thermal evaporation through a mask;
[0012] (4) On the prepared second source electrode and electrode extension layer, a second organic semiconductor layer was prepared by vacuum thermal evaporation through a mask, with a vacuum degree of 10 -6 Below Pascal;
[0013] (5) preparing a second drain electrode on the prepared second organic semiconductor layer by vacuum thermal evaporation through a mask;
[0014] (6) preparing a first insulating layer on the prepared second drain electrode by spin coating at a rotation speed of 4000 rpm, and annealing the spin-coated PVA in a vacuum drying oven at 150° C. for two hours;
[0015] (7) On the prepared first insulating layer, a first organic semiconductor layer is prepared by vacuum thermal evaporation through a mask plate, and the vacuum degree is 10 -6 Below Pascal;
[0016] (8) forming a first source electrode and a first drain electrode on the prepared first organic semiconductor layer by vacuum thermal evaporation through a mask;
[0017] Technical analysis of the present invention:
[0018] In terms of channel length, since the planar field effect transistor is limited in reducing the channel length, we use vertical channels to prepare organic field effect transistors. The channel length of the field effect transistor with this structure is determined by the thickness of the organic semiconductor layer, and the organic semiconductor layer is prepared by evaporation technology. The film formed in this way has good uniformity and the minimum thickness can reach several nanometers. Due to the significant reduction in channel length, the source-drain current can be significantly improved; at the same time, the three-dimensional organic field effect transistor can interconnect the upper and lower layers and use the same gate electrode for control. In practical applications, it can control two different layers of devices, which has important application significance.
Brief Description of the Drawings
[0019] Figure 1 A schematic structural diagram of a three-dimensional flexible organic field effect transistor provided by the present invention.
[0020] In the figure, 101 is the first source electrode, 102 is the second source electrode, 201 is the first drain electrode, 202 is the second drain electrode, 203 is the electrode extension layer, 301 is the first organic semiconductor layer, 302 is the second organic semiconductor layer, 401 is the first insulating layer, 402 is the second insulating layer, 5 is the gate electrode, and 6 is the flexible substrate.
[0021] Figure 2 The present invention discloses a three-dimensional flexible organic field effect transistor, in which the working principle of the vertical channel portion composed of a second drain electrode (202), a second organic semiconductor layer (302), a second source electrode (102), a second insulating layer (402) and a gate electrode (5) is disclosed.
[0022] In the figure, 202 is a second drain electrode, 302 is a second organic semiconductor layer, 102 is a second source electrode, 402 is a second insulating layer, and 5 is a gate electrode. [Specific implementation method]
[0023] The present invention will be further described below in conjunction with specific examples.
[0024] like Figure 2 As shown in the figure, the working principle of the vertical channel organic field effect transistor is that since the selected organic semiconductor material is P-type and the drain-source voltage is negative, when no gate voltage is applied, there are only a small number of hole carriers in the organic semiconductor. When the source-drain voltage increases, the output current is extremely small due to the extremely small number of carriers. When a negative gate voltage is applied, the source and the gate form a capacitor structure, and the mesh structure adopted by the source can allow part of the accumulated hole charges to exist in the organic semiconductor layer, resulting in an increase in the number of carriers in the organic semiconductor layer and an increase in the output current.
[0025] In this embodiment, a three-dimensional flexible organic field effect transistor is prepared according to the following steps:
[0026] 1) The flexible substrate was placed in ethanol, acetone, and deionized water solution for ultrasonic cleaning for 10 minutes, and then dried with nitrogen gas;
[0027] 2) A second insulating layer was prepared on the flexible substrate by spin coating. A 20 wt% PVA aqueous solution was spin coated at a speed of 4000 rpm. The spin-coated PVA was irradiated with 365 nm (8 W) UV light for 10 min, placed in a vacuum drying oven at 200° C. for cross-linking for 2 hours, and then annealed at 60° C. for 30 min.
[0028] 3) preparing a second source electrode and an electrode extension layer on the second insulating layer, preparing a grid-shaped sacrificial layer on the second insulating layer by using a photolithography process, and then preparing a layer of metal gold by vacuum thermal evaporation, controlling the evaporation rate and time so that the thickness of the evaporated metal gold is less than the thickness of the grid-shaped sacrificial layer, and forming a grid-shaped metal gold by releasing the sacrificial layer; the electrode extension layer is prepared by vacuum thermal evaporation through a mask;
[0029] 4) On the prepared second source electrode and electrode extension layer, a second organic semiconductor layer is prepared by vacuum thermal evaporation through a mask, with a vacuum degree of 10 -6 Below Pascal;
[0030] 5) preparing a second drain electrode on the prepared second organic semiconductor layer by vacuum thermal evaporation through a mask;
[0031] 6) A first insulating layer is prepared on the prepared second drain electrode by spin coating, wherein a 20 wt% PVA aqueous solution is spin coated at a rotation speed of 4000 rpm, and the spin-coated PVA is annealed in a vacuum drying oven at 150° C. for two hours;
[0032] 7) On the prepared first insulating layer, a first organic semiconductor layer is prepared by vacuum thermal evaporation through a mask, with a vacuum degree of 10 -6 Below Pascal;
[0033] 8) On the prepared first organic semiconductor layer, a first source electrode and a first drain electrode are prepared by vacuum thermal evaporation through a mask.
Claims
1. A three-dimensional flexible organic field effect transistor, characterized in that: It comprises a first source electrode (101), a second source electrode (102), a first drain electrode (201), a second drain electrode (202), an electrode extension layer (203), a first organic semiconductor layer (301), a second organic semiconductor layer (302), a first insulating layer (401), a second insulating layer (402), a gate electrode (5), and a flexible substrate (6); Wherein: the flexible substrate, the gate electrode, and the second insulating layer are stacked in sequence, the electrode extension layer and the second source electrode are respectively located on both sides of the second insulating layer, and the electrode extension layer and the second source electrode are connected; the second organic semiconductor layer and the second drain electrode are sequentially located above the second source electrode, and the width of the second organic semiconductor layer and the second drain electrode is the same as that of the second source electrode; the first insulating layer covers the electrode extension layer, the second organic semiconductor layer, and the second drain electrode; the first organic semiconductor layer is located above the first insulating layer, and the first source electrode and the first drain electrode are respectively located on both sides of the first organic semiconductor layer; The second source electrode is a grid-shaped metal gold; The material of the electrode extension layer is metal gold; The three-dimensional flexible organic field effect transistor interconnects the upper and lower layers and is controlled by the same gate electrode.
2. The three-dimensional flexible organic field effect transistor according to claim 1, characterized in that: The material of the first source electrode, the first drain electrode and the second drain electrode is metal aluminum.
3. The three-dimensional flexible organic field effect transistor according to claim 1, characterized in that: The materials of the first organic semiconductor layer and the second organic semiconductor layer are copper phthalocyanine, pentacene, One or more of P3HT.
4. The three-dimensional flexible organic field effect transistor according to claim 1, characterized in that: The material of the first insulating layer and the second insulating layer is PVA.
5. The three-dimensional flexible organic field effect transistor according to claim 1, characterized in that: The material of the gate electrode is ITO.
6. The three-dimensional flexible organic field effect transistor according to claim 1, characterized in that: The material of the flexible substrate is polyethylene terephthalate (PET) or polyimide (PI).
7. The three-dimensional flexible organic field effect transistor according to claim 1, characterized in that: The overall area of the first organic semiconductor layer, the first source electrode and the first drain electrode is smaller than or equal to the second source electrode.
8. A method for manufacturing a flexible organic field effect transistor with a three-dimensional structure as claimed in claim 1, characterized in that: The steps include: (1) The flexible substrate was ultrasonically cleaned in ethanol, acetone, and deionized water solution for 10 min in sequence, and then dried with nitrogen gas; (2) A second insulating layer was prepared on the flexible substrate by spin coating at a rotation speed of 4000 rpm. The spin-coated PVA was irradiated with 365 nm (8 W) UV light for 10 min, placed in a vacuum drying oven at 200 ° C for cross-linking for 2 hours, and then annealed at 60 ° C for 30 min: (3) preparing a second source electrode and an electrode extension layer on the second insulating layer, preparing a grid-shaped sacrificial layer on the second insulating layer by using a photolithography process, and then preparing a layer of metal gold by vacuum thermal evaporation, controlling the evaporation rate and time so that the thickness of the evaporated metal gold is less than the thickness of the grid-shaped sacrificial layer, and forming a grid-shaped metal gold by releasing the sacrificial layer; the electrode extension layer is prepared by vacuum thermal evaporation through a mask; (4) on the prepared second source electrode and electrode extension layer, a second organic semiconductor layer is prepared by vacuum thermal evaporation through a mask, with a vacuum degree of less than 10-6 Pascal; (5) preparing a second drain electrode on the prepared second organic semiconductor layer by vacuum thermal evaporation through a mask; (6) preparing a first insulating layer on the prepared second drain electrode by spin coating at a rotation speed of 4000 rpm, and annealing the spin-coated PVA in a vacuum drying oven at 150° C. for two hours; (7) preparing a first organic semiconductor layer on the prepared first insulating layer by vacuum thermal evaporation through a mask, with a vacuum degree of less than 10-6 Pascal; (8) On the prepared first organic semiconductor layer, a first source electrode and a first drain electrode are prepared by vacuum thermal evaporation through a mask.