Electroluminescent device, method for forming the same, and display device including the same
By using cluster layer structures of inorganic oxide particles and metal organic compounds in electroluminescent devices, the problems of leakage current and charge carrier balance are solved, and efficient luminescence performance and long life are achieved.
Patent Information
- Application Number
- CN201910192538.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-03-12
- Filing Date
- 2019-03-14
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2039-03-14
AI Technical Summary
The leakage current in existing electroluminescent devices is large, which affects the luminescence efficiency and device performance, and it is difficult to effectively regulate the balance and transmission of electrons and holes.
Using an electron transport layer including inorganic oxide particles and metal organic compounds, by filling the surface of the emission layer with metal organic compounds or their thermal decomposition products, a cluster layer structure is formed to reduce leakage current and optimize the thickness and composition of the electron transport layer to increase the Charge carrier equilibrium.
It significantly reduces leakage current, improves luminous efficiency and device life, improves external quantum efficiency and brightness, improves charge carrier balance, and enhances the overall performance of the device.
Smart Images

Figure CN110277501B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to and the benefit of Korean Patent Application No. 10-2018-0029942 filed on March 14, 2018, in the Korean Intellectual Property Office, and Korean Patent Application No. 10-2019-0028358 filed on March 12, 2019, in the Korean Intellectual Property Office, the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present invention relates to an electroluminescent device, a method for forming the same and a display device comprising the same. Background Art
[0004] Quantum dots are nanocrystalline semiconductor materials with diameters ranging from several to hundreds of nanometers, which exhibit quantum confinement effects. Quantum dots produce stronger light than commonly used phosphors in a narrow wavelength region. When excited electrons transition from the conduction band to the valence band, quantum dots emit light, and the wavelength changes depending on the particle size, even in the same material. Since quantum dots emit shorter wavelength light with smaller particle sizes, they can obtain light in the desired wavelength region by adjusting the size.
[0005] In other words, compared to an organic light emitting diode using an emission layer including phosphorescent and / or phosphor (fluorescent powder) materials, an emission layer including quantum dots and various electronic devices including the emission layer can generally save manufacturing costs, and the desired color can be emitted by changing the size of the quantum dots, without the need to use other organic materials in the emission layer to emit light of other colors.
[0006] The luminous efficiency of the emission layer including quantum dots is determined by the quantum efficiency of the quantum dots, the balance of charge carriers, the light extraction efficiency, the leakage current, etc. That is, in order to improve the luminous efficiency of the emission layer, there are methods such as adjusting excitons to be confined in the emission layer, adjusting holes and electrons to be smoothly transferred to the quantum dots, or preventing leakage current. Summary of the invention
[0007] Provided are an electroluminescent device having improved device characteristics by reducing leakage current and a display apparatus including the same.
[0008] According to an embodiment, an electroluminescent device includes: a first electrode and a second electrode facing each other; an emission layer arranged between the first electrode and the second electrode and including light-emitting particles; an electron transport layer arranged between the first electrode and the emission layer; and a hole transport layer arranged between the second electrode and the emission layer, wherein the electron transport layer includes inorganic oxide particles and a metal organic compound, and the metal organic compound or a thermal decomposition product of the metal organic compound is soluble in a non-polar solvent.
[0009] The metal-organic compound may include Zn, Ti, Sn, W, Ta, Mg, Ga, Na, Cu, Ag, or a combination thereof.
[0010] The metal organic compound may include an oleate-based compound, an amine-based compound, or a combination thereof.
[0011] The non-polar solvent may include at least one of the following: C6 to C20 linear, branched or cyclic aliphatic hydrocarbons, C6 to C20 aromatic hydrocarbons, dichloromethane, ethyl acetate.
[0012] The inorganic oxide particles may be an oxide including at least one of zinc, titanium, zirconium, tin, tungsten, tantalum, magnesium, gallium, sodium, copper, and silver.
[0013] The inorganic oxide particles may be dispersed in a polar solvent.
[0014] The surface of the electron transport layer facing the emission layer may include a first portion in which the inorganic oxide particles are disposed and a second portion in which the metal organic compound or a thermal decomposition product thereof is filled between adjacent inorganic oxide particles.
[0015] The electron transport layer may include: a first layer including inorganic oxide particles; and a second layer including a metal organic compound or a thermal decomposition product thereof.
[0016] The second layer may be disposed between the first layer and the emission layer.
[0017] The first layer may include a cluster layer including the inorganic oxide particles.
[0018] The surface of the first layer facing the second layer may be filled with the metal organic compound or a thermal decomposition product thereof.
[0019] The first layer may include an organic matrix filled in adjacent inorganic oxide particles, and the organic matrix may include an organic material other than the metal organic compound or a thermal decomposition product thereof.
[0020] The average thickness of the second layer may be less than the average thickness of the first layer.
[0021] The inorganic oxide particles may be metal oxide particles, and a metal element included in the metal oxide particles may be the same as a metal element included in the metal organic compound.
[0022] The electron transport layer may have an average thickness of about 20 nm to about 60 nm.
[0023] The luminescent particles may include quantum dots.
[0024] The luminescent particles may have a core-shell structure.
[0025] The luminescent particles may include: Group II-VI compounds excluding Cd, Group III-V compounds, Group IV-VI compounds, Group IV elements or compounds, Group I-III-VI compounds, Group I-II-IV-VI compounds excluding Cd, or combinations thereof.
[0026] Hydrophobic organic ligands may be attached to the surface of the luminescent particles.
[0027] On the other hand, a display device including the electroluminescent device according to the embodiment is provided.
[0028] An electroluminescent device having improved device characteristics by reducing leakage current can be provided.
[0029] In addition, as described above, a display apparatus including an electroluminescent device having improved device characteristics is provided. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 is a schematic cross-sectional view of an electroluminescent device according to an embodiment,
[0031] Figures 2 to 4 are cross-sectional views illustrating various positional relationships between inorganic oxide particles and metal organic compounds or thermal decomposition products thereof in an electron transport layer of an electroluminescent device according to an embodiment,
[0032] Figure 5 A scanning electron microscope (SEM) image showing the surface of the ZnO cluster layer according to Comparative Example 1,
[0033] Figure 6 is a SEM image of the surface of the zinc oleate or thermal decomposition product layer formed on the ZnO cluster layer according to Example 1,
[0034] Figure 7 are voltage-current density curves of the electroluminescent devices according to Example 1 and Comparative Examples 1 to 4,
[0035] Figure 8 is a brightness-external quantum efficiency (EQE) curve of the electroluminescent device according to Example 1 and Comparative Examples 1 to 4,
[0036] Fig. 9 shows the life characteristics of the electroluminescent devices according to Example 1 and Comparative Example 1, and
[0037] Fig.10 The life characteristics of the electroluminescent devices according to Example 2 and Comparative Example 5 are shown. DETAILED DESCRIPTION
[0038] Hereinafter, example embodiments will be described in detail so that those skilled in the art will understand them. However, the present disclosure may be embodied in many different forms and is not to be construed as limited to the example embodiments set forth herein.
[0039] In the accompanying drawings, the thickness of layers, films, panels, regions, etc. is exaggerated for clarity. In the specification, the same reference numerals always represent the same elements. It will be understood that when an element such as a layer, film, region, or substrate is referred to as being "on" another element, it may be directly on the other element or there may be an intermediate element. On the contrary, when an element is referred to as being "directly on" another element, there is no intermediate element.
[0040] As used herein, a "Group" may refer to a Group of the periodic table.
[0041] As used herein, “Group II” may refer to Group IIA and Group IIB, and examples of Group II metals may be Cd, Zn, Hg, and Mg, but are not limited thereto.
[0042] As used herein, examples of “Group II metal excluding Cd” may refer to Group II metals other than Cd, such as Zn, Hg, Mg, and the like.
[0043] As used herein, “Group III” may refer to Group IIIA and Group IIIB, and examples of Group III metals may be Al, In, Ga, and Tl, but are not limited thereto.
[0044] As used herein, "Group IV" may refer to Group IVA and Group IVB, and examples of Group IV metals may be Si, Ge, and Sn, but are not limited thereto. As used herein, the term "metal" may include semimetals such as Si.
[0045] As used herein, “Group I” may refer to Group IA and Group IB, and examples may include Li, Na, K, Rb, and Cs, but are not limited thereto.
[0046] As used herein, “Group V” may refer to Group VA, and examples may include nitrogen, phosphorus, arsenic, antimony, and bismuth, but are not limited thereto.
[0047] As used herein, “Group VI” may refer to Group VIA, and examples may include sulfur, selenium, and tellurium, but are not limited thereto.
[0048] As used herein, "aliphatic" means a saturated or unsaturated straight or branched hydrocarbon group. For example, an aliphatic group may be an alkyl, alkenyl, or alkynyl group.
[0049] As used herein, "amine" has the general formula NRR, wherein each R is independently hydrogen, C1-C30 alkyl, C3-C8 cycloalkyl, C2-C30 alkenyl, C2-C30 alkynyl, or C6-C30 aryl, each of which may be substituted or unsubstituted.
[0050] As used herein, "aromatic" means an organic compound or group that includes at least one unsaturated cyclic group having delocalized π electrons. The term includes both hydrocarbon aromatic compounds and heteroaromatic compounds.
[0051] In an embodiment, for the particle diameters of the particles, although they can be quantified by measurement to show the average size of the group, methods generally used include a mode diameter showing the maximum value of the distribution (mode diameter, modediameter), a median diameter corresponding to the central value of the integrated distribution curve, a variety of average diameters (number average, length average, area average, mass average, volume average, etc.), etc. Unless otherwise specified, the average particle diameter refers to the number average diameter in the present disclosure, and it is obtained by measuring D50 (particles at the position of 50% of the distribution rate).
[0052] In an embodiment, "solubility" refers to the property of a solute being well dissolved in a specific solvent. In an embodiment, when a solute is well dissolved in a non-polar solvent, the corresponding solute may be expressed as having solubility with respect to a non-polar solvent, and when a solute is well dissolved in a polar solvent, the corresponding solute may be expressed as having solubility with respect to a polar solvent.
[0053] Unless otherwise described in the embodiments, the thickness of each constituent element may refer to an “average thickness”.
[0054] The “average thickness” of each constituent element is calculated by extracting arbitrary 5 to 10 points from a scanning electron microscope (SEM) cross-sectional image of each constituent element, measuring the thickness, and calculating the arithmetic mean of the measured thicknesses.
[0055] Figure 1 is a schematic cross-sectional view of an electroluminescent device according to an embodiment, and Figures 2 to 4 are cross-sectional views illustrating various positional relationships between inorganic oxide particles and a metal organic compound or a thermal decomposition product thereof in an electron transport layer of an electroluminescent device according to an embodiment.
[0056] The electroluminescent device 10 according to the embodiment includes: a first electrode 110 and a second electrode 170 facing each other; an emission layer 140 disposed between the first electrode 110 and the second electrode 170 and including light-emitting particles 141; an electron transport layer 120 disposed between the first electrode 110 and the emission layer 140; and a hole transport layer 150 disposed between the second electrode 170 and the emission layer 140, and a hole injection layer 160 disposed between the hole transport layer 150 and the second electrode 170 and which can be omitted in consideration of the relationship between the constituent elements.
[0057] The electroluminescent device 10 may have a stacked structure in which the electron transport layer 120, the emission layer 140, the hole transport layer 150, and the hole injection layer 160 are disposed between the first electrode 110 and the second electrode 170 facing each other.
[0058] The electroluminescent device 10 according to the embodiment provides current to the emission layer 140 through the first electrode 110 and the second electrode 170, and causes electroluminescence of the light emitting particles 141 to generate light. The electroluminescent device 10 can generate light in various wavelength regions according to the material, size or fine structure of the light emitting particles 141 of the emission layer 140.
[0059] In an embodiment, the first electrode 110 and the second electrode 170 may be connected to a driving power source, respectively, and thus may function to allow current to flow to the emission layer 140. One of the first electrode 110 and the second electrode 170 may be an anode, and the other may be a cathode. In an embodiment, the first electrode 110 may be a cathode, and the second electrode 170 may be an anode.
[0060] At least one of the first electrode 110 and the second electrode 170 may include a material having light transmittance (light transmittance) in at least the visible light wavelength region, but is not limited thereto. The first electrode 110 may include a material having light transmittance (light transmittance) in the infrared or ultraviolet (UV) wavelength region. For example, the first electrode 110 may include an optically transparent material. For example, the second electrode 170 may include an optically transparent material. For example, the first electrode 110 and the second electrode 170 may include an optically transparent material.
[0061] In an embodiment, the optically transparent material may include, for example, molybdenum oxide, tungsten oxide, vanadium oxide, rhenium oxide, niobium oxide, tantalum oxide, titanium oxide, zinc oxide, nickel oxide, copper oxide, cobalt oxide, manganese oxide, chromium oxide, indium oxide, tin oxide, indium tin oxide, indium zinc oxide, or a combination thereof, or at least one selected from silver (Ag), aluminum (Al), copper (Cu), gold (Au), and alloys thereof.
[0062] In an embodiment, one of the first electrode 110 and the second electrode 170 may include molybdenum oxide, tungsten oxide, vanadium oxide, rhenium oxide, niobium oxide, tantalum oxide, titanium oxide, zinc oxide, nickel oxide, copper oxide, cobalt oxide, manganese oxide, chromium oxide, indium oxide, tin oxide, indium tin oxide, indium zinc oxide, or a combination thereof, and the other of the first electrode 110 and the second electrode 170 may include at least one of silver (Ag), aluminum (Al), copper (Cu), gold (Au), and alloys thereof. For example, the first electrode 110 may include molybdenum oxide, tungsten oxide, vanadium oxide, rhenium oxide, niobium oxide, tantalum oxide, titanium oxide, zinc oxide, nickel oxide, copper oxide, cobalt oxide, manganese oxide, chromium oxide, indium oxide, tin oxide, indium tin oxide, indium zinc oxide, or a combination thereof, and the second electrode 170 may include at least one of silver (Ag), aluminum (Al), copper (Cu), gold (Au), and alloys thereof.
[0063] However, according to the embodiment, the first electrode 110 and / or the second electrode 170 are not necessarily limited thereto, but may include a material that also has light transmittance (light transmittance) with respect to light in the infrared or ultraviolet (UV) wavelength region, or a semi-transparent material that selectively transmits light in a specific wavelength region and can perform the function of reflecting light in the visible light wavelength region.
[0064] Each of the first electrode 110 and the second electrode 170 may be formed by depositing a material for forming an electrode on the substrate 100 or an organic layer by a method such as sputtering or deposition.
[0065] Meanwhile, in an embodiment, the first electrode 110 may be disposed on the substrate 100, such as Figure 1 As shown in . The substrate 100 may be a transparent insulating substrate or may be made of a ductile material. The substrate 100 may include glass or a polymer material, and the polymer material may have, for example, a glass transition temperature (Tg) greater than or equal to about 150° C. For example, it includes a COC (cyclic olefin copolymer) or COP (cyclic olefin polymer) based material.
[0066] In an implementation, the substrate 100 may support the electron transport layer 120 , the emission layer 140 , the hole transport layer 150 , and the hole injection layer 160 disposed between the first electrode 110 and the second electrode 170 .
[0067] However, the substrate 100 of the electroluminescent device 10 according to the embodiment does not have to be disposed under the first electrode 110 , but may be disposed on the second electrode 170 or may be omitted as needed.
[0068] In an embodiment, the electron transport layer 120 is disposed between the first electrode 110 and the emission layer 140, and transports charges from the first electrode 110 to the emission layer 140. The charges may be electrons.
[0069] In an embodiment, the average thickness of the electron transport layer 120 may vary taking into account the charge carrier balance of the hole transport layer 150, the hole injection layer 160 and / or the emission layer 140 in the device, but may be, for example, greater than or equal to about 20 nm, greater than or equal to about 25 nm, greater than or equal to about 30 nm, greater than or equal to about 35 nm, or greater than or equal to about 40 nm, and, for example, less than or equal to about 100 nm, less than or equal to about 90 nm, less than or equal to about 80 nm, less than or equal to about 70 nm, less than or equal to about 60 nm, less than or equal to about 55 nm, or less than or equal to about 50 nm, for example, from about 20 nm to about 60 nm, from about 30 nm to about 60 nm, or from about 40 nm to about 60 nm.
[0070] When the average thickness of the electron transport layer 120 is less than about 20 nm, voids, cracks, etc. of the electron transport layer 120 may increase and device characteristics may be significantly deteriorated, and it is difficult to satisfy carrier balance with other constituent elements of the electroluminescent device.
[0071] On the other hand, when the average thickness of the electron transport layer 120 is greater than about 100 nm, electrons may be supplied to the emission layer 140 too quickly and / or in large quantities compared to holes, and the electrons may encounter holes at the interface between the emission layer 140 and the hole transport layer 150 to cause interface light emission, or may move to the hole transport layer 150 and / or the hole injection layer 160 to be quenched.
[0072] In an embodiment, the electron transport layer 120 may include the inorganic oxide particles 121. For example, the electron transport layer 120 may include a cluster layer composed of the inorganic oxide particles 121.
[0073] In an embodiment, the inorganic oxide particles 121 may be composed of a material having an electron transport property, and thus it may have an electron transport property. The inorganic oxide particles 121 according to an embodiment may be, for example, an oxide including at least one of zinc, titanium, zirconium, tin, tungsten, tantalum, magnesium, gallium, sodium, copper, and silver, and may include, for example, ZnO, TiO 2 、ZrO 2 SnO 2 , WO 3 、 2 O 3 or a combination thereof, but not limited thereto.
[0074] The inorganic oxide particles 121 according to the embodiment may have dispersibility with respect to a polar solvent. The dispersibility of the inorganic oxide particles 121 may be caused by hydroxyl groups (-OH) on the surface of the inorganic oxide particles 121 at room temperature. For example, ZnO particles may include a large number of hydroxyl groups (-OH) on the surface at room temperature. Therefore, when ZnO particles are introduced into a polar solvent such as water or ethanol at room temperature, the ZnO particles may be controlled to be uniformly dispersed in the polar solvent by simple physical treatment such as stirring without aggregation.
[0075] Therefore, it is easy to form a cluster layer composed of the inorganic oxide particles 121 by applying a dispersion in which the inorganic oxide particles 121 are dispersed in a polar solvent to the first electrode 110 and then drying the dispersion. In addition, the cluster layer formed thereon may have a relatively uniform distribution of the inorganic oxide particles 121 without excessively agglomerating in a specific portion.
[0076] On the other hand, the average particle diameter of the inorganic oxide particles 121 according to an embodiment may be, for example, less than or equal to about 70 nm, less than or equal to about 60 nm, less than or equal to about 50 nm, less than or equal to about 40 nm, less than or equal to about 30 nm, less than or equal to about 20 nm, or less than or equal to about 10 nm, and, for example, greater than or equal to about 1 nm, greater than or equal to about 2 nm, greater than or equal to about 3 nm, greater than or equal to about 4 nm, or greater than or equal to about 5 nm.
[0077] When the average particle diameter of the inorganic oxide particles 121 is within the above range, the cluster layer composed of the inorganic oxide particles 121 may exhibit excellent electron transport properties.
[0078] In an embodiment, the electron transport layer 120 may include a metal organic compound having solubility with respect to a non-polar solvent or a thermal decomposition product thereof.
[0079] The metal organic compound may be a metal salt having an organic group. The metal organic compound has an electron transport property like the inorganic oxide particles 121 , but unlike the inorganic oxide particles 121 , may have solubility with respect to a non-polar solvent.
[0080] In an embodiment, the metal organic compound may have the same or similar level of electron transport properties as compared to the inorganic oxide particles 121. The metal in the metal organic compound may be Zn, Ti, Sn, W, Ta, Mg, Ga, Na, Cu, Ag, or a combination thereof.
[0081] On the other hand, the electron mobility and energy level of the metal organic compound may vary depending on the kind of metal and / or organic compound, but may be the same as or similar to those of the inorganic oxide particles 121 .
[0082] For example, the metal in the metal organic compound may be the same as the metal in the inorganic oxide particles 121. For example, the inorganic oxide particles 121 may be metal oxide particles, and the metal element included in the metal oxide particles and the metal element included in the metal organic compound may be the same as each other. In this case, it is easy to control the energy level and / or electron mobility of the electron transport layer 120 to the same or similar level.
[0083] However, the embodiment is not necessarily limited thereto, and the metal in the inorganic oxide particles 121 and the metal of the metal organic compound may be different from each other in consideration of charge carrier balance between constituent elements of the electroluminescent element 10 .
[0084] In an embodiment, the organic compound in the metal organic compound imparts solubility of the metal organic compound relative to the non-polar solvent. The organic compound may include an oleate (salt, ester) based compound, an amine based compound, or a combination thereof. For example, the organic compound may be an oleate (salt, ester) based compound.
[0085] In addition, examples of non-polar solvents for dissolving metal organic compounds may be at least one selected from the following: C6 to C20 straight, branched or cyclic aliphatic hydrocarbons, C6 to C20 aromatic hydrocarbons, methylene chloride, ethyl acetate. C6 to C20 straight, branched or cyclic aliphatic hydrocarbons may contain one or more unsaturated groups, but are not aromatic. Heteroatoms may or may not be present in the aliphatic or aromatic hydrocarbons, and only exist when the aliphatic or aromatic hydrocarbons are non-polar.
[0086] When the organic compound in the metal organic compound according to the embodiment is selected from the compounds, a solution containing the metal organic compound in a nonpolar solvent is applied to the cluster layer in a simple manner and then dried to form the electron transport layer 120 .
[0087] Specifically, since the cluster layer is prepared using a polar solvent, when a metal organic compound having solubility relative to the polar solvent is used, the cluster layer may be destroyed by the polar solvent. However, since the metal organic compound according to the embodiment uses a non-polar solvent having a chemical property different from that of the inorganic oxide particles 121, even when the metal organic compound is applied to the cluster layer, damage to the surface of the cluster layer can be minimized.
[0088] The thermal decomposition product of the metal organic compound may refer to a product obtained by thermally decomposing a solution including the metal organic compound during coating and drying at a predetermined temperature. The thermal decomposition product of the metal organic compound may include metal, metal oxide, organic compound or a combination thereof.
[0089] Specifically, the thermal decomposition product may include Zn, Ti, Sn, W, Ta, Mg, Ga, Na, Cu, Ag, or a combination thereof, or an oxide thereof, and a carbon compound.
[0090] The carbon compound may be a product or a derivative thereof in which an organic compound in the metal organic compound, particularly an oleate compound, an amine compound and other organic compounds are separated from a metal by thermal decomposition of the metal organic compound. The thermal decomposition product may be chemically bonded to the surface of the inorganic oxide particle 121.
[0091] The carbon compound may have solubility relative to the non-polar solvent.
[0092] When a metal organic compound or a thermal decomposition product thereof is included together with the inorganic oxide particles 121 as in the embodiment, there is a difference in energy level change compared to the case where the inorganic oxide particles 121 are simply doped with a metal.
[0093] Specifically, when Mg is used as the metal in the metal organic compound and ZnO particles are used as the inorganic oxide particles 121, the electron transport layer 12 in which the pure Mg-organic compound or its thermal decomposition product and the ZnO particles are mixed has a slightly lower lowest unoccupied molecular orbital (LUMO) energy level and a highest occupied molecular orbital (HOMO) energy level compared to the electron transport layer including the ZnO particles alone. On the other hand, ZnMgO in which ZnO is doped with Mg may exhibit slightly increased LUMO and HOMO energy levels compared to the electron transport layer including the ZnO particles alone.
[0094] In an embodiment, the amount of the metal organic compound can be changed differently by considering the relationship between the above energy levels and / or electron mobility. The amount of the metal organic compound can be adjusted differently in consideration of, for example, the type of organic compound bonded to the metal, the type of inorganic oxide particles 121, the thickness of the electron transport layer 120, etc.
[0095] refer to Figures 2 to 4 , the electron transport layer 120 in the electroluminescent devices 10, 10' and 10" may include a first layer including a cluster layer composed of inorganic oxide particles 121. In this case, the metal organic compound or its thermal decomposition product may be disposed at various positions between the first layer 124 and the emission layer 140.
[0096] The average thickness of the first layer 124 may vary in consideration of the average particle diameter and material of the inorganic oxide particles 121, the charge carrier balance between the emission layer 140 and / or the hole transport layer 150, the hole injection layer 160, etc. However, it may be, for example, less than or equal to about 60 nm, less than or equal to about 50 nm, less than or equal to about 40 nm, less than or equal to about 35 nm, or less than or equal to about 30 nm, and, for example, greater than or equal to about 20 nm, greater than or equal to about 25 nm, or greater than or equal to about 30 nm.
[0097] When the average thickness of the first layer 124 satisfies the above range, the first layer 124 may exhibit excellent electron transport properties.
[0098] refer to Figure 2 , the metal organic compound or its thermal decomposition product 122 in the electroluminescent device 10 directly contacts the surface of the first layer 124 facing the emission layer 140, and may also fill the empty space on the surface.
[0099] Specifically, regarding the surface of the electron transport layer 120 facing the emission layer 140, the surface may include a first region where inorganic oxide particles 121 exist and a second region where the metal organic compound or its thermal decomposition product 122 filling the empty space between adjacent inorganic oxide particles 121 exists.
[0100] On the surface of the electron transport layer 120 facing the emission layer 140 , the inorganic oxide particles 121 may be mixed with the metal organic compound or a thermal decomposition product thereof 122 .
[0101] Therefore, according to Figure 2 In the electroluminescent device 10, the electron transport layer 120 may be a composite layer including: a first layer 124 including inorganic oxide particles 121 and a layer including a metal organic compound or a thermal decomposition product thereof 122 and filling the empty space on the surface of the first layer 124 facing the emission layer, as described above.
[0102] On the other hand, reference Figure 3 , and according to Figure 2 Unlike the electroluminescent device 10 of the present invention, the electroluminescent device 10' may further include a second layer 126 having a predetermined thickness between the emission layer 140 and the first layer 124, wherein the second layer 126 may include a metal organic compound or a thermal decomposition product thereof. For example, the second layer 126 may be a layer formed of a metal organic compound or a thermal decomposition product thereof.
[0103] Specifically, according to Figure 2Unlike the electroluminescent device 10 of the embodiment of the present invention, the surface of the electron transport layer 120 facing the emission layer 140 may be the surface of the second layer 126, and the inorganic oxide particles 121 may not be exposed to the surface but covered. The surface of the second layer 126 facing the emission layer 140 may be relatively smooth compared to the surface of the first layer 124 contacting the second layer 126. Therefore, the morphology of the electron transport layer 120 contacting the emission layer 140 may be improved.
[0104] for Figure 3 The electroluminescent device 10', with Figure 2 Like the electroluminescent device 10 , the surface of the first layer 124 directly contacts the metal organic compound or its thermal decomposition product, which can fill the empty space on the surface of the first layer 124 .
[0105] As described above, second layer 126 according to an embodiment has a thickness sufficient to cover at least the surface with which first layer 124 contacts without exposing inorganic oxide particles 121 toward emission layer 140. On the other hand, second layer 126 may be formed thicker than required in consideration of interaction with a solution for forming emission layer 140 during formation of emission layer 140 to be described later.
[0106] In an embodiment, taking into account all of the above conditions, the second layer 126 may have an average thickness that is thinner than the average thickness of the first layer 120, for example, an average thickness of greater than or equal to about 2 nm, greater than or equal to about 3 nm, greater than or equal to about 4 nm, greater than or equal to about 5 nm, and greater than or equal to about 10 nm, and for example, less than or equal to about 15 nm, for example, in the range of about 3 nm to about 15 nm, for example, in the range of about 5 nm to about 15 nm, for example, in the range of about 7 nm to about 15 nm, and for example, in the range of about 10 nm to about 15 nm.
[0107] When the second layer 126 has an average thickness of less than about 2 nm, the thickness of the second layer 126 may be reduced by a nonpolar solvent during the formation of the emission layer 140 described later, and the inorganic oxide particles 121 may be exposed. On the other hand, when the second layer 126 has an average thickness of more than about 15 nm, the charge carrier balance of the entire electroluminescent device may be deteriorated.
[0108] In accordance with Figure 2 and 3 In the electroluminescent devices 10 and 10', the empty space on the surface of the first layer 124 may vary depending on the average particle diameter of the inorganic oxide particles 121, the thickness of the first layer 124, etc., but is inevitably formed because the first layer 124 is a cluster layer formed of the inorganic oxide particles 121. The empty space includes gaps, cracks, etc. between the inorganic oxide particles 121.
[0109] The empty space serves as a leakage path of electrons during operation of the device and may not be completely removed even if the first layer 124 is formed by using an inorganic oxide having excellent dispersibility with respect to a polar solvent.
[0110] However, in Figure 2 and 3 In the electroluminescent devices 10 and 10', the empty space of the first layer 124 may not only be filled with the metal organic compound or its thermal decomposition product, but also the surface of the first layer 124 may be covered by the second layer 126, such as Figure 3 The electroluminescent device 10' is shown in FIG.
[0111] In other words, for Figure 2 and 3 In the electroluminescent devices 10 and 10', the leakage path of the electron transport layer can be reduced by filling the space of the first layer 124 with the metal organic compound or its thermal decomposition product.
[0112] However, the embodiment is not necessarily limited thereto. Figure 4 The electroluminescent device 10", and Figure 2 and 3 Different from the cluster layers of the electroluminescent devices 10 and 10', the first layer 124' may include an organic material matrix filled between adjacent inorganic oxide particles 121. Here, the organic material matrix may include an organic material selected from monomers, oligomers and / or polymers, wherein the organic material may be different from a metal organic compound or a thermal decomposition product thereof.
[0113] For example, the organic material matrix may be an adhesive. In other words, the first layer 124' may be a mixed layer of the inorganic oxide particles 121 and an organic material used as an adhesive. The organic material matrix may include a variety of organic materials without particular limitation, as long as they are different from metal organic compounds or their thermal decomposition products and function as a well-known adhesive.
[0114] On the other hand, the second layer 126' may not fill the empty space within the first layer 124' but may cover the first layer 124' so that the surface of the first layer 124' may not be exposed to the emission layer 140. Here, the morphology of the surface of the first layer 124' may be improved by covering the surface of the first layer 124' with the second layer 126', and the leakage current of the electron transport layer may be reduced by the second layer 126'.
[0115] In an embodiment, according to Figure 3 and 4The electroluminescent devices 10' and 10" may have equal or almost similar energy levels between the first layers 124 and 124' and the second layers 126 and 126'. For example, when the same metal is used for the first layers 124 and 124' and the second layers 126 and 126', the LUMO energy levels of the second layers 126 and 126' may be slightly increased compared to the LUMO energy levels of the first layers 124 and 124' by organic compounds or the like.
[0116] However, the LUMO energy level difference between the second layers 126 and 126' and the first layers 124 and 124' can be, for example, less than or equal to about 0.3 eV, less than or equal to about 0.2 eV, and less than or equal to about 0.1 eV, and even designed to be close to 0 eV by changing the kind of organic compound and the kind of metal used for the electron transport layer, as described above.
[0117] On the other hand, the embodiment is not necessarily limited thereto, but the second layers 126 and 126' and the first layers 124 and 124' may be variously adjusted to have a LUMO energy level difference of, for example, greater than about 0.3 eV, for example, greater than or equal to about 0.4 eV, greater than or equal to about 0.5 eV, or, for example, in the range of about 0.3 eV to about 0.7 eV. However, the thickness of the second layers 126 and 126', etc. may be adjusted to minimize the second layers 126 and 126' from acting as an energy barrier.
[0118] On the other hand, between the electron transport layer 120 and the first electrode 110 , an electron injection layer (not shown) for facilitating electron injection and / or a hole blocking layer (not shown) for blocking movement of holes may be further formed.
[0119] The average thickness of each of the electron injection layer and the hole blocking layer may be appropriately selected. For example, the average thickness of each layer may be greater than or equal to about 1 nm and less than or equal to about 500 nm, but is not limited thereto. The electron injection layer may be an organic layer formed by deposition and may be omitted in consideration of the thickness and material of the electron transport layer 120.
[0120] The electron injection layer may include, for example, at least one selected from the group consisting of 1,4,5,8-naphthalene-tetracarboxylic dianhydride (NTCDA), bathocuproin (BCP), tris[3-(3-pyridyl)- yl]borane (3TPYMB), LiF, Alq 3 , Gaq 3 、Inq 3 、Znq 2 、Zn(BTZ) 2 、BeBq 2, ET204 (8-(4-(4,6-di(naphthalene-2-yl)-1,3,5-triazine-2-yl)phenyl)quinolone), 8-hydroxyquinoline lithium (Liq), n-type metal oxides (such as ZnO, HfO 2 etc.), and combinations thereof, but are not limited thereto.
[0121] The hole blocking layer may include, for example, at least one selected from the group consisting of 1,4,5,8-naphthalene-tetracarboxylic dianhydride (NTCDA), bathocuproin (BCP), tris[3-(3-pyridyl)- yl]borane (3TPYMB), LiF, Alq 3 , Gaq 3 、Inq 3 、Znq 2 、Zn(BTZ) 2 、BeBq 2 and combinations thereof, but are not limited thereto. It may be omitted in consideration of the thickness, material, etc. of other constituent elements in the electroluminescent device 10.
[0122] The emission layer 140 may be disposed between the electron transport layer 120 and the hole transport layer 150. The emission layer 140 may contact the electron transport layer 120 and may include at least two light emitting particles.
[0123] The emission layer 140 is a location where electrons and holes are transferred by current supplied from the first electrode 110 and the second electrode 170. The electrons and holes are combined in the emission layer 140 to generate excitons, and the generated excitons transition from an excited state to a ground state to emit light of a wavelength corresponding to the size of the light emitting particle 141.
[0124] On the other hand, the emission layer 140 may emit light in a predetermined wavelength region. The predetermined wavelength region belongs to the visible light region, for example, one of the following: a first wavelength region of about 380 nm to about 488 nm, a second wavelength region of about 490 nm to about 510 nm, a third wavelength region of greater than 510 nm to about 580 nm, a fourth wavelength region of about 582 nm to about 600 nm, and a fifth wavelength region of about 620 nm to about 680 nm.
[0125] In an embodiment, the light emitting particles 141 may include quantum dots. That is, all the light emitting particles 141 may be made of quantum dots. One of the light emitting particles 141 may be formed of quantum dots, and the other may be a different kind of luminescent body from quantum dots, such as a commercially available phosphor (fluorescent powder).
[0126] The quantum dots have a discontinuous energy band gap due to the quantum confinement effect to convert incident light into light having a predetermined wavelength and radiate it. That is, when the light emitting particles 141 are composed of quantum dots, the emission layer 140 can generate light having excellent color reproducibility and color purity.
[0127] In an embodiment, the material of the quantum dot is not particularly limited, and the quantum dot may be known or commercially available. For example, the luminescent particle 141 according to the embodiment may be a quantum dot including a II-VI compound, a III-V compound, a IV-VI compound, a IV element or compound, a I-III-VI compound, a I-II-IV-VI compound not containing Cd, or a combination thereof. That is, the luminescent particle 141 according to the embodiment may be a non-cadmium-based quantum dot. Like this, when the luminescent particle 141 is formed of a non-cadmium-based material, they are non-toxic and therefore non-dangerous and environmentally friendly compared to conventional cadmium-based quantum dots.
[0128] The II-VI group compound may be selected from: a binary compound selected from ZnS, ZnSe, ZnTe, ZnO, HgS, HgSe, HgTe, MgSe, MgS and mixtures thereof; a ternary compound selected from ZnSeS, ZnSeTe, ZnSTe, HgSeS, HgSeTe, HgSTe, HgZnS, HgZnSe, HgZnTe, MgZnSe, MgZnS and mixtures thereof; and a quaternary compound selected from ZnSeSTe, HgZnTeS, HgZnSeS, HgZnSeTe, HgZnSTe and mixtures thereof. The II-VI group compound may further include a group III metal.
[0129] The III-V compound may be selected from: a binary compound selected from GaN, GaP, GaAs, GaSb, AlN, AlP, AlAs, AlSb, InN, InP, InAs, InSb and mixtures thereof; a ternary compound selected from GaNP, GaNAs, GaNSb, GaPAs, GaPSb, AlNP, AlNAs, AlNSb, AlPAs, AlPSb, InNP, InNAs, InNSb, InPAs, InPSb, InZnP and mixtures thereof; and a quaternary compound selected from GaAlNP, GaAlNAs, GaAlNSb, GaAlPAs, GaAlPSb, GaInNP, GaInNAs, GaInNSb, GaInPAs, GaInPSb, InAlNP, InAlNAs, InAlNSb, InAlPAs, InAlPSb and mixtures thereof. The III-V compound may further include a Group II metal (InZnP).
[0130] The IV-VI group compound may be selected from: a binary compound selected from SnS, SnSe, SnTe, PbS, PbSe, PbTe and mixtures thereof; a ternary compound selected from SnSeS, SnSeTe, SnSTe, PbSeS, PbSeTe, PbSTe, SnPbS, SnPbSe, SnPbTe and mixtures thereof; and a quaternary compound selected from SnPbSSe, SnPbSeTe, SnPbSTe and mixtures thereof. Examples of I-III-VI group compounds may be CuInSe 2 、CuInS 2 , CuInGaSe and CuInGaS, but not limited thereto. Examples of I-II-VI-VI group compounds may be CuZnSnSe and CuZnSnS, but not limited thereto. Examples of IV group elements or compounds may be: a simple substance selected from Si, Ge and a mixture thereof; and a binary compound selected from SiC, SiGe and a mixture thereof.
[0131] The binary compound, ternary compound or quaternary compound is present in the particles at a uniform concentration or in partially different concentrations in the same particles, respectively.
[0132] According to an embodiment, the quantum dot may have a core-shell structure including a semiconductor nanocrystal core and another semiconductor nanocrystal shell surrounding the core. The core and the shell may have a concentration gradient, wherein the concentration of the element of the shell decreases toward the core. In addition, the quantum dot may have a semiconductor nanocrystal core and multiple shells surrounding the core. Here, the multilayer shell structure has a structure of two or more shells, and each layer may have a single composition or alloy or may have a concentration gradient.
[0133] In an embodiment, the luminescent particle may have a core-shell structure. When the luminescent particle has a core-shell structure, the material composition of the shell has a larger energy band gap than the core, which can show an effective quantum confinement effect. However, the embodiment is not limited thereto. At the same time, in a multilayer shell, the shell outside the core may have a higher energy band gap than the shell near the core, and the quantum dot may have an ultraviolet (UV) to infrared wavelength range.
[0134] The quantum dots may have a quantum efficiency of greater than or equal to about 10%, for example, greater than or equal to about 20%, greater than or equal to about 30%, greater than or equal to about 40%, greater than or equal to about 50%, greater than or equal to about 60%, greater than or equal to about 70%, greater than or equal to about 90%, or even 100%.
[0135] In a display, quantum dots may have a relatively narrow spectrum to improve color purity or color reproducibility. The quantum dots may have, for example, a half width (FWHM) of a wavelength spectrum of less than or equal to about 45 nm, less than or equal to about 40 nm, or less than or equal to about 30 nm. Within this range, the color purity or color reproducibility of the device may be improved.
[0136] The quantum dots may have a particle diameter (the longest length for non-spherical particles) of about 1 nm to about 100 nm. For example, the quantum dots may have a particle diameter of about 1 nm to about 20 nm, such as about 2 nm (or about 3 nm) to about 15 nm.
[0137] In addition, the shape of the quantum dot can be a common shape in the art, and therefore there may be no particular limitation. For example, the quantum dot may have a spherical, elliptical, tetrahedral, pyramidal, cuboctahedral, cylindrical, polyhedral, multi-armed, or cubic nanoparticle, nanotube, nanowire, nanofiber, nanosheet, or a combination thereof. The quantum dot may have any cross-sectional shape.
[0138] Quantum dots can be commercially available or can be synthesized by any method. For example, quantum dots of several nanometers in size can be synthesized according to a wet chemical process. In a wet chemical process, a precursor reacts in an organic solvent to grow crystalline particles, and an organic solvent or a ligand compound can coordinate the surface of the quantum dots to control the growth of the crystal. Examples of organic solvents and ligand compounds are known. The organic solvent coordinated on the surface of the quantum dots can affect the stability of the device, and therefore the residues that are not coordinated on the surface of the nanocrystal can be removed by pouring it into an excess of a non-solvent and centrifuging the resulting mixture. Examples of non-solvents can be acetone, ethanol, methanol, etc., but are not limited thereto. After removing the residue, the amount of the ligand compound, organic solvent, or a combination thereof coordinated on the surface of the quantum dots can be less than or equal to about 5% weight %, for example, less than or equal to about 30 weight %, less than or equal to about 20 weight %, or less than or equal to about 10 weight %, based on the weight of the quantum dots.
[0139] The hydrophobic organic ligand having a hydrophobic portion may be bound to the surface of the luminescent particle. In an embodiment, the hydrophobic organic ligand may include RCOOH, RNH 2 , R 2 NH, R 3 N, RSH, R 3 PO, R 3 P, ROH, RCOOR', RPO(OH) 2 , R 2POOH (wherein, R and R' are independently C5 to C24 alkyl, C5 to C24 alkenyl, C5 to C20 alicyclic group or C6 to C20 aryl), polymer organic ligand compound, or a combination thereof. For example, the hydrophobic organic ligand may be oleic acid, palmitic acid, myristic acid, stearic acid or a combination thereof. The hydrophobic organic ligand may be an organic ligand having a monofunctional group, and the functional group may be chemically bonded to the surface of the quantum dot.
[0140] When the hydrophobic organic ligand is attached to the surface of the light emitting particle, both the light emitting particle and the light emitting layer according to the embodiment may have hydrophobicity as a whole. If the light emitting layer 140 has hydrophobicity, it may be easily affected by a non-polar solvent.
[0141] The electroluminescent device 10 according to the embodiment may include the above-mentioned metal organic compound or its thermal decomposition product between the cluster layer formed by the inorganic oxide particles 121 and the emission layer 140, as described above, wherein the metal organic compound or its thermal decomposition product may fill the empty space on the surface of the cluster layer and form a layer having a predetermined thickness between the cluster layer and the emission layer 140. Therefore, when the hydrophobic emission layer 140 is formed on the already formed electron transport layer 120, the emission layer may be prevented from being damaged by a non-polar solvent.
[0142] The hole transport layer 150 may be disposed between the emission layer 140 and the second electrode 170 and / or between the hole injection layer 160 and the emission layer 140, or between the emission layer 140 and the second electrode 170 and between the hole injection layer 160 and the emission layer 140. The hole transport layer 150 may provide holes and transport the holes into the emission layer 140. The hole transport layer 150 may be directly formed on the emission layer 140 and may directly contact the emission layer 140.
[0143] In an embodiment, the hole transport layer 150 may be formed of a p-type semiconductor material or a material doped with a p-type dopant. For example, the hole transport layer 150 may include a PEDOT [poly (3,4-ethylenedioxythiophene)] derivative, a PSS [poly (styrene sulfonate)] derivative, a poly-N-vinyl carbazole (PVK) derivative, a bicarbazole derivative, a polyphenylene vinylene derivative, a poly-p-phenylene vinylene (PPV) derivative, a polymethacrylate derivative, a poly (9,9-dioctylfluorene) derivative, a poly (spiro-fluorene) derivative, TCTA (tri (4-carbazole-9-yl) phenyl) amine), TPD (N,N'-diphenyl-N,N'-bis (3-methylphenyl) -(1, 1'-biphenyl)-4,4'-diamine), NPB (N,N'-di(naphthalene-1-yl)-N,N'-diphenylbenzidine), m-MTDATA (tri(N-3-methylphenyl-N-phenylamino)-triphenylamine), TFB (poly[(9,9-dioctylfluorenyl-2,7-diyl-co-(4,4'-(N-4-butylphenyl)diphenylamine]), PFB (poly(9,9-dioctylfluorenyl)-co-N,N-diphenyl-N,N-di-(p-butylphenyl)-1,4-diaminobenzene), poly-TPD, metal oxides such as NiO and MoO 3 , or a combination thereof, but not limited thereto.
[0144] For example, the hole transport layer 150 may include at least one of TCTA and compounds represented by Chemical Formula 1 to Chemical Formula 9, but is not limited thereto.
[0145]
[0146]
[0147]
[0148] The hole transport layer 150 may be formed by a wet coating method such as spin coating, etc. Thus, the hole transport layer 150 may be formed on the emission layer 140 in a simple manner. In addition, when the emission layer 140 has hydrophobicity, a polar solvent may be selected as a solvent for forming the hole transport layer 150, so that damage to the emission layer 140 may be minimized.
[0149] For example, a polymer film such as PPV can be obtained by spin coating a precursor solution including a PPV precursor polymer and a polar solvent (such as water, methanol, ethanol, etc.) on the emission layer 140, and heat treating it, such as in N 2 The curing is performed at a curing temperature of about 250° C. to about 300° C. for 3 hours in an inert gas atmosphere or under vacuum to obtain a hole transport layer 150 composed of a PPV thin film.
[0150] The hole injection layer 160 may be disposed between the hole transport layer 150 and the second electrode 170. The hole injection layer 160 may supply holes to the emission layer 140 together with the hole transport layer 150. However, considering the thickness and material of the hole transport layer 150, the hole injection layer 160 may be omitted.
[0151] On the other hand, the hole injection layer 160 may be formed of a p-type semiconductor material or a material doped with a p-type dopant, like the hole transport layer 150. For example, the hole injection layer 160 may include a PEDOT [poly (3,4-ethylenedioxythiophene)] derivative, a PSS [poly (styrene sulfonate)] derivative, a poly-N-vinyl carbazole (PVK) derivative, a polyphenylene vinylene derivative, a poly-p-phenylene vinylene (PPV) derivative, a polymethacrylate derivative, a poly (9,9-dioctylfluorene) derivative, a poly (spiro-fluorene) derivative, TCTA (tri (4-carbazole-9-yl) phenyl) amine), TPD (N,N'-diphenyl-N,N'-bis (3-methylphenyl) -(1,1'-bis)- ... phenyl)-4,4'-diamine), NPB (N,N'-di(naphthalene-1-yl)-N,N'-diphenylbenzidine), m-MTDATA (tri(N-3-methylphenyl-N-phenylamino)-triphenylamine), TFB (poly[(9,9-dioctylfluorenyl-2,7-diyl-co-(4,4'-(N-4-butylphenyl)diphenylamine]), PFB (poly(9,9-dioctylfluorenyl)-co-N,N-diphenyl-N,N-di-(p-butylphenyl)-1,4-diaminobenzene), poly-TPD, metal oxides such as NiO and MoO 3 , or a combination thereof, but not limited thereto.
[0152] As described above, in the electroluminescent device 10 according to the embodiment, the electron transport layer 120 includes the inorganic oxide particles 121 and the metal organic compound or its thermal decomposition product. Therefore, the electroluminescent device 10 according to the embodiment can minimize the void space between adjacent inorganic oxide particles using the metal organic compound or its thermal decomposition product. As a result, the electroluminescent device 10 according to the embodiment can improve the luminous efficiency of the device by reducing the leakage current.
[0153] Hereinafter, a display device including the electroluminescent device 10 is described.
[0154] A display device according to an embodiment includes a substrate, a driving circuit formed on the substrate, and first, second, and third electroluminescent devices spaced apart from each other at predetermined intervals and disposed on the driving circuit.
[0155] The first to third electroluminescent devices have the same structure as the electroluminescent device 10, but the wavelengths of light emitted from the respective quantum dots may be different from each other.
[0156] In an embodiment, the first electroluminescent device may be a red device emitting red light, the second electroluminescent device may be a green device emitting green light, and the third electroluminescent device may be a blue device emitting blue light. In other words, the first to third electroluminescent devices may be pixels expressing red, green, and blue, respectively, in a display device.
[0157] However, the embodiment is not necessarily limited thereto, but the first to third electroluminescent devices may respectively express one of magenta, yellow, cyan, or may express other colors.
[0158] On the other hand, one of the first to third electroluminescent devices may be the electroluminescent device 10. In this case, the third electroluminescent device expressing blue may desirably be the electroluminescent device 10.
[0159] In a display device according to an embodiment, a hole injection layer, a hole transport layer, an electron transport layer, an electron injection layer, and a hole blocking layer other than the emission layer of each pixel may be integrated (integrated) to form a common (common) layer. However, the embodiment is not limited thereto. The hole injection layer, the hole transport layer, the electron transport layer, the electron injection layer, and the hole blocking layer may be independently formed in each pixel of the display device, or at least one of the hole injection layer, the hole transport layer, the electron transport layer, the electron injection layer, and the hole blocking layer may form a common layer, and the remaining layers may form separate independent layers.
[0160] The substrate may be a transparent insulating substrate or may be made of a ductile material. The substrate may include glass or a polymer material, and the polymer material may be selected from a material having a glass transition temperature (Tg) greater than about 150°C. For example, it includes a material based on COC (cyclic olefin copolymer) or COP (cyclic olefin polymer). All of the first to third electroluminescent devices are formed on the substrate. That is, the substrate of the display device according to the embodiment provides a common layer.
[0161] The driving circuit is disposed on the substrate and is independently connected to each of the first to third electroluminescent devices. The driving circuit may include: at least one line including a scan line, a data line, a driving power line, a common power line, etc., at least two thin film transistors (TFTs) connected to the wires and corresponding to one organic light emitting diode, and at least one capacitor, etc. The driving circuit may have a variety of known structures.
[0162] As described above, the display device according to the embodiment may reduce leakage current and improve device characteristics, and thus may exhibit excellent electroluminescent characteristics.
[0163] Hereinafter, the embodiments are described in more detail with reference to Examples. However, these Examples are exemplary, and the present disclosure is not limited thereto.
[0164] Example 1
[0165] An indium tin oxide (ITO) layer was deposited on a glass substrate, and a ZnO cluster layer having an average thickness of about 30 nm to 35 nm was formed thereon by spin coating a composition for a first electron transport layer prepared by dispersing 3 mmol of ZnO particles having an average particle diameter of 4.5 nm in an ethanol solvent at 4000 rpm for 40 seconds, and then drying the composition at 80° C. for 30 minutes.
[0166] Subsequently, on the ZnO cluster layer, 0.1 mmol of a zinc oleate compound (in which Zn and oleate were included in a molar ratio of 1:1) was dissolved in 1 mL of hexane, and then the solution was spin-coated at 4000 rpm for 40 seconds.
[0167] The spin-coated layer was washed with hexane and dried at 80° C. for 30 minutes to remove the hexane to induce crystallization of the zinc oleate compound and thereby form a layer including the zinc oleate compound or its thermal decomposition product on the ZnO cluster layer. The layer including the zinc oleate compound or its thermal decomposition product covers the upper surface of the ZnO cluster layer and has an average thickness thinner than that of the ZnO cluster layer.
[0168] Subsequently, on the layer including the zinc oleate compound or its thermal decomposition product, a blue emission layer having a thickness of 25 nm was formed by coating a composition for an emission layer, the composition being prepared by dispersing blue quantum dots (ZnSeTe / ZnSe / ZnS core-shell blue quantum dots) to which a hydrophobic organic ligand (oleic acid) is attached and a binder in octane, and then drying the composition at 80° C. The blue quantum dots have a maximum emission wavelength in the range of 440 nm to 460 nm, a half width (FWHM) in the range of 18 nm to 25 nm, and an external quantum efficiency greater than or equal to 85%.
[0169] After forming the blue emission layer, the electron transport layer has an average thickness (the sum of the average thickness of the ZnO cluster layer and the layer including the zinc oleate compound or its thermal decomposition product) in the range of about 35 nm to 45 nm.
[0170] Subsequently, on the blue emission layer, a TCTA layer was formed by coating a composition for a hole transport layer in which TCTA was dissolved in methanol, and then heating the composition.
[0171] Then, by depositing MoO on the TCTA layer 3 Forming MoO as a hole injection layer 3 layer.
[0172] at MoO3 A silver (Ag) layer was deposited on the layer to manufacture the electroluminescent device (ITO / ZnO cluster layer / layer including a zinc oleate compound or a thermal decomposition product thereof / blue emission layer / TCTA / MoO 3 / Ag).
[0173] Example 2
[0174] The electroluminescent device according to Example 2 (ITO / ZnO cluster layer / layer including zinc oleate compound or its thermal decomposition product / red emission layer / chemical formula 1 / MoO 3 / Ag), except that a red emission layer is formed by using red quantum dots (InP) to which a hydrophobic organic ligand (oleic acid) is attached instead of blue quantum dots (ZnSeTe / ZnSe / ZnS) to which a hydrophobic organic ligand (oleic acid) is attached, and a hole transport layer formed by a bicarbazole-based compound represented by Chemical Formula 1 is included instead of the TCTA layer.
[0175] Comparative Example 1
[0176] The electroluminescent device (ITO / ZnO cluster layer / blue emission layer / TCTA / MoO 3 / Ag), except that the blue emission layer is formed directly on the ZnO cluster layer.
[0177] Comparative Example 2
[0178] An electroluminescent device (ITO / ZnO cluster layer / layer including zinc acetate compound or its thermal decomposition product / blue emission layer / TCTA / MoO 3 / Ag), except as follows: a composition for a second electron transport layer was prepared by dissolving 0.1 mmol of a zinc acetate compound (including Zn and acetate in a molar ratio of 1:1) in 1 mL of ethanol, and a layer including the zinc acetate compound or a thermal decomposition product thereof was formed instead of the layer including the zinc oleate compound or a thermal decomposition product thereof.
[0179] Comparative Example 3
[0180] The electroluminescent device (ITO / ZnO cluster layer / ZnCl 2 / Blue emission layer / TCTA / MoO 3 / Ag), except that: ZnCl is formed by using the composition for the second electron transport layer 2The layer comprising the zinc oleate compound or its thermal decomposition product is replaced by the layer comprising the zinc oleate compound or its thermal decomposition product, the composition being prepared by adding 0.1 mmol of ZnCl 2 Prepared by dissolving in 1 mL of acetone and using acetone instead of hexane for washing.
[0181] Comparative Example 4
[0182] An electroluminescent device (ITO / ZnO cluster layer / layer including zinc diethyldithiocarbamate compound or its thermal decomposition product / blue emission layer / TCTA / MoO 3 / Ag), except that: a layer including a zinc diethyldithiocarbamate compound or a thermal decomposition product thereof is formed instead of a layer including a zinc oleate compound or a thermal decomposition product thereof by using a composition for a second electron transport layer, the composition being prepared by dissolving 0.1 mmol of a zinc diethyldithiocarbamate compound (including Zn and diethyldithiocarbamate in a molar ratio of 1:1) in chloroform (CHCl 3 ) and chloroform was used instead of hexane for washing.
[0183] Comparative Example 5
[0184] The electroluminescent device (ITO / ZnO cluster layer / red emission layer / chemical formula 1 / MoO 3 / Ag), except that the red emission layer was formed directly on the ZnO cluster layer.
[0185] Evaluation 1: Surface between the ZnO cluster layer and the surface of the ZnO cluster layer / layer including the zinc oleate compound or the thermal decomposition product Comparison of face images
[0186] Figure 5 and 6 The upper surface of the ZnO cluster layer in Comparative Example 1 and the surface of the layer including the zinc oleate compound or its thermal decomposition product on the ZnO cluster layer in Example 1 are respectively shown.
[0187] Figure 5 A scanning electron microscope (SEM) image showing the surface of the ZnO cluster layer according to Comparative Example 1, and Figure 6 is a SEM image of the surface of the zinc oleate or thermal decomposition product thereof layer formed on the ZnO cluster layer according to Example 1.
[0188] refer to Figure 5, the ZnO cluster layer according to Comparative Example 1 has a first region (relatively bright region) filled with ZnO particles and a second region (black region) not filled with ZnO particles but left as an empty space, as described above. This second region left as an empty space includes voids and / or cracks and can be used as a leakage path during electron transport in the device.
[0189] On the other hand, reference Figure 6 , the layer including the zinc oleate compound or the thermal decomposition product thereof according to Example 1 may be formed to cover the ZnO cluster layer, and partially and / or completely fill the empty space on the surface of the ZnO cluster layer. Therefore, when the layer including the zinc oleate compound or the thermal decomposition product thereof according to the embodiment is directly formed on the ZnO cluster layer, voids and / or cracks in the ZnO cluster layer may be removed or minimized.
[0190] Evaluation 2: Device characteristics of electroluminescent devices of Examples and Comparative Examples
[0191] The relationships between voltage-current density and brightness-external quantum efficiency of the electroluminescent devices according to Example 1 and Comparative Examples 1 to 4 are shown in FIG. Figures 7 to 8 middle.
[0192] Figure 7 : is the voltage-current density curve of the electroluminescent device according to Example 1 and Comparative Examples 1 to 4. Figure 7 In the graph, the change in current density according to voltage is represented by a logarithmic scale.
[0193] refer to Figure 7 The electroluminescent device having the electron transport layer (including the ZnO cluster layer / the layer of the zinc oleate compound or its thermal decomposition product) according to Example 1 shows an increase in current density at a voltage of about 2.5 V or less, as compared with the electroluminescent device according to the comparative example, and in particular, has a stable current density increasing effect as compared with Comparative Example 1, and has an excellent current density increasing effect as compared with Comparative Examples 3 to 4.
[0194] Figure 8 is a graph showing luminance-external quantum efficiency (EQE) of the electroluminescent devices according to Example 1 and Comparative Examples 1 to 4.
[0195] refer to Figure 8, the electroluminescent device of Example 1 exhibited a maximum external quantum efficiency that was 1.8 to 2.5 times higher than that of the comparative example. In addition, when the external quantum efficiency was compared depending on the specific brightness, Example 1 exhibited an external quantum efficiency of about 1.4% at 100 nits, Comparative Example 1 exhibited an external quantum efficiency of about 0.8% at 100 nits, Comparative Examples 2 and 4 exhibited external quantum efficiencies of about 1.0% at 100 nits, respectively, and Comparative Example 3 exhibited an external quantum efficiency of about 0% at 100 nits.
[0196] In addition, for the external quantum efficiency at 500 nits, Example 1 shows approximately 2.4%, Comparative Example 1 shows approximately 1.4%, Comparative Example 2 shows approximately 1.5%, Comparative Example 3 shows 0%, and Comparative Example 4 shows approximately 0.9%, and for the external quantum efficiency at 1000 nits, Example 1 shows approximately 2.3%, Comparative Example 1 shows approximately 1.2%, Comparative Example 2 shows approximately 0.5%, and Comparative Examples 3 and 4 show approximately 0%, respectively.
[0197] On the other hand, as for the maximum brightness of each electroluminescent device, Example 1 showed about 1400 Cd / m 2 , Comparative Example 1 shows about 1200Cd / m 2 , Comparative Example 2 shows about 1000Cd / m 2 , Comparative Example 3 shows about 24Cd / m 2 , and Comparative Example 4 shows about 740Cd / m 2 .
[0198] First, Comparative Example 3 shows a more deteriorated property than the other comparative examples. The reason is that when ZnCl 2 When the metal organic compound is used as the compound for forming the electron transport layer, the ZnCl on the ZnO cluster layer 2 The layer has equal or more voids and / or cracks than the ZnO cluster layer. Therefore, when an inorganic compound such as ZnCl is used instead of a metal organic compound, 2 When the second electron transport layer is formed, device characteristics are more difficult to achieve.
[0199] On the other hand, Comparative Examples 2 to 4 in which a polar solvent was used during the formation of the layer including the metal organic compound or its thermal decomposition product showed an external quantum efficiency and / or maximum brightness comparable to those of Comparative Example 1 having only the ZnO cluster layer (Comparative Example 2), and an external quantum efficiency and / or maximum brightness greatly deteriorated compared to those of Comparative Example 1 (Comparative Examples 3 and 4). Therefore, when a metal organic compound having no solubility with respect to a nonpolar solvent but having solubility with respect to a polar solvent is used, the polar solvent may have an influence on at least the ZnO cluster layer.
[0200] In other words, Comparative Examples 2 to 4 fill the voids and / or cracks of the ZnO cluster layer by using a metal organic compound or its thermal decomposition product similarly to Example 1, but the ZnO cluster layer is damaged by the polar solvent, etc., and therefore, the metal organic compound or its thermal decomposition product has no great effect (Comparative Example 2) and on the contrary exhibits more deteriorated performance (Comparative Examples 3 and 4).
[0201] Therefore, when a layer including a metal organic compound or a thermal decomposition product thereof is formed on a ZnO cluster layer by using a metal organic compound having solubility with respect to a nonpolar solvent according to Example 1, Example 1 exhibits excellent external quantum efficiency at about 100 to 1000 nits compared to the comparative example.
[0202] Evaluation 3: Lifespan characteristics of electroluminescent devices of Examples and Comparative Examples
[0203] The life characteristics of the electroluminescent devices (blue) according to Example 1 and Comparative Example 1 and the life characteristics of the electroluminescent devices (red) according to Example 2 and Comparative Example 5 are shown in FIG. Figures 9 to 10 middle.
[0204] Fig. 9 shows the life characteristics of the electroluminescent devices according to Example 1 and Comparative Example 1, and Fig.10 The life characteristics of the electroluminescent devices according to Example 2 and Comparative Example 5 are shown.
[0205] refer to Fig. 9 and 10 , since Example 1 showed a T50 of about 1.5 hours, and Comparative Example 1 showed a T50 of about 1 hour, Example 1 showed a life improvement effect of about 1.5 times with respect to the blue electroluminescent device. On the other hand, Example 2 showed a T50 of about 67.7 hours, and Comparative Example 5 showed a T50 of about 9.7 hours, and thus the life improvement effect with respect to the red electroluminescent device was about 7 times.
[0206] Therefore, the electroluminescent device according to the embodiment shows excellent life characteristics compared with the comparative example not including the layer of the metal organic compound or its thermal decomposition product. The reason is that the layer of the metal organic compound or its thermal decomposition product allows stable injection of current into the electron transport layer and thus improves the charge carrier balance.
[0207] While the present disclosure has been described in conjunction with what are presently considered to be practical example embodiments, it is to be understood that the invention is not limited to the disclosed embodiments, but is intended to cover various modifications and equivalent arrangements included within the spirit and scope of the appended claims.
[0208] <Reference Numbers>
[0209] 10: Electroluminescent device 100: Substrate
[0210] 110: first electrode 120: electron transport layer
[0211] 121: Inorganic oxide particles 124: First layer
[0212] 126: second layer 140: emission layer
[0213] 141: luminescent particles 150: hole transport layer
[0214] 160: hole injection layer 170: second electrode
Claims
1. Electroluminescent devices, including a first electrode and a second electrode facing each other; an emission layer disposed between the first electrode and the second electrode and comprising light-emitting particles; an electron transport layer disposed between the first electrode and the emission layer; as well as a hole transport layer disposed between the second electrode and the emission layer, wherein the electron transport layer comprises inorganic oxide particles and a metal organic compound, wherein the metal organic compound or a thermal decomposition product of the metal organic compound is soluble in a non-polar solvent, The metal organic compound comprises an oleate-based compound, an amine-based compound or a combination thereof.
2. The electroluminescent device of claim 1, wherein the metal organic compound comprises Zn, Ti, Sn, W, Ta, Mg, Ga, Na, Cu, Ag, or a combination thereof.
3. The electroluminescent device of claim 1, wherein the non-polar solvent comprises at least one of the following: C6 to C20 linear, branched or cyclic aliphatic hydrocarbons, C6 to C20 aromatic hydrocarbons, dichloromethane, ethyl acetate.
4. The electroluminescent device of claim 1, wherein the inorganic oxide particles are oxides comprising at least one of zinc, titanium, zirconium, tin, tungsten, tantalum, magnesium, gallium, sodium, copper, and silver. The electroluminescent device according to claim 1 , wherein the inorganic oxide particles have dispersibility with respect to a polar solvent.
6. The electroluminescent device of claim 1, wherein the surface of the electron transport layer facing the emission layer comprises The inorganic oxide particles are disposed in the first portion, and The metal organic compound or its thermal decomposition product is filled in the second portion between adjacent inorganic oxide particles.
7. The electroluminescent device of claim 1, wherein the electron transport layer comprises a first layer comprising said inorganic oxide particles, and A second layer includes the metal organic compound or a thermal decomposition product thereof.
8. The electroluminescent device of claim 7, wherein the second layer is disposed between the first layer and the emissive layer.
9. The electroluminescent device of claim 7, wherein the first layer comprises a cluster layer comprising the inorganic oxide particles.
10. The electroluminescent device of claim 9, wherein a surface of the first layer facing the second layer comprises the metal organic compound or a thermal decomposition product thereof.
11. The electroluminescent device of claim 7, wherein the first layer comprises an organic matrix filled between adjacent inorganic oxide particles, and the organic matrix comprises an organic material different from the metal organic compound or a thermal decomposition product thereof.
12. The electroluminescent device of claim 7, wherein the average thickness of the second layer is less than the average thickness of the first layer.
13. The electroluminescent device of claim 1, wherein the inorganic oxide particles comprise metal oxide particles, and The metal element included in the metal oxide particles is the same as the metal element included in the metal organic compound.
14. The electroluminescent device of claim 1, wherein the electron transport layer has an average thickness of 20 nm to 60 nm.
15. The electroluminescent device of claim 1, wherein the light-emitting particles comprise quantum dots.
16. The electroluminescent device of claim 1, wherein the light-emitting particle has a core-shell structure.
17. The electroluminescent device of claim 1, wherein the luminescent particles comprise a II-VI compound that does not contain Cd, a III-V compound, a IV-VI compound, a IV element or compound, a I-III-VI compound, a I-II-IV-VI compound that does not contain Cd, or a combination thereof.
18. The electroluminescent device of claim 1, wherein a hydrophobic organic ligand is attached to a surface of the light emitting particle.
19. A display device comprising the electroluminescent device according to any one of claims 1 to 18.
20. A method of forming an electroluminescent device, the method include: providing a first electrode and a second electrode facing each other; An emission layer is provided between the first electrode and the second electrode, wherein the emission layer includes light-emitting particles; An electron transport layer is provided between the first electrode and the emission layer, wherein the electron transport layer comprises inorganic oxide particles and a metal organic compound, wherein the metal organic compound or a thermal decomposition product of the metal organic compound is soluble in a non-polar solvent; and A hole transport layer is provided between the second electrode and the emission layer, The metal organic compound comprises an oleate-based compound, an amine-based compound or a combination thereof.
Citation Information
Patent Citations
Water piping system including slam reduction means
KR1020180029942A
Organic electronic device and method for manufacturing same
CN103548171A
Organic light emitting diode with double-layer electron transport layer and preparation method thereof
CN104064690A
Nanocrystal with quantum well energy level structure and preparation method thereof, and semiconductor device
CN106601886A
Light Emitting Device and Method Of Manufacturing Electron Transport layer
KR1020150120026A