Optical member and display including the same
By adopting a laminated structure with low refractive index in liquid crystal displays, the light transmission efficiency and overall performance of the display are improved, and the cost of wavelength conversion films in the prior art is solved.
Patent Information
- Application Number
- CN201910207726.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-06-08
- Filing Date
- 2019-03-19
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2039-03-19
AI Technical Summary
The wavelength conversion film in existing liquid crystal displays is susceptible to moisture, resulting in high cost and complex assembly, and difficult to improve light transmission efficiency.
A laminated structure with a low refractive index is adopted, including a light guide plate, a low refractive layer, a wavelength conversion layer and a low refractive cover layer. By adjusting the laminated structure and thickness, the light transmittance is improved, the use of a barrier film is reduced, and the manufacturing cost is reduced.
It improves light transmission efficiency, reduces the thickness and manufacturing cost of the display, simplifies the assembly process, and avoids the deterioration of wavelength conversion particles under the influence of moisture.
Smart Images

Figure CN110579832B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to and the benefit of Korean Patent Application No. 10-2018-0066151, filed on Jun. 8, 2018, which is hereby incorporated by reference herein for all purposes as if fully set forth herein. Technical Field
[0003] Exemplary embodiments of the present invention relate generally to optical components, and more particularly to displays including the same. Background Art
[0004] Liquid crystal displays generally receive light from a backlight assembly and display images. Some backlight assemblies include a light source and a light guide plate. The light guide plate can receive light from the light source and guide the light to the display panel. In some products, the light source provides white light, and the white light is filtered through a color filter of the display panel to achieve color.
[0005] Recently, research has been conducted on the application of wavelength conversion films to improve image quality, such as color reproducibility of liquid crystal displays. Typically, a blue light source is used as a light source, and a wavelength conversion film is provided on a light guide plate to convert the blue light into white light. The wavelength conversion film typically includes wavelength conversion particles. Since the wavelength conversion particles are typically susceptible to moisture, they are protected with a barrier film. However, the barrier film is expensive and may increase the overall thickness of the device. In addition, since the wavelength conversion film should be laminated on the light guide plate, a complicated assembly process may be required.
[0006] The above information disclosed in this Background section is only for understanding the background of the present inventive concept and therefore it may contain information that does not constitute prior art. Summary of the invention
[0007] An optical member having a laminated structure and a display device including the same according to an exemplary embodiment of the present invention can provide improved light transmission efficiency.
[0008] Additional features of the inventive concept will be set forth in the description which follows, and in part will be apparent from the description, or may be learned by practice of the inventive concept.
[0009] An optical member according to an exemplary embodiment includes a light guide plate; a low refractive layer disposed on the light guide plate and having a refractive index smaller than that of the light guide plate; a low refractive bottom layer disposed between the low refractive layer and the light guide plate and having a thickness smaller than that of the low refractive layer; and a wavelength conversion layer disposed on the low refractive layer.
[0010] An optical member according to another exemplary embodiment includes a light guide plate; a low refractive layer disposed on the light guide plate and having a refractive index smaller than that of the light guide plate; a wavelength conversion layer disposed on the low refractive layer; and a low refractive cover layer disposed between the low refractive layer and the wavelength conversion layer and having a thickness smaller than that of the low refractive layer.
[0011] According to another exemplary embodiment, an optical component includes a light guide plate; a low-refractive layer disposed on the light guide plate and having a refractive index less than that of the light guide plate; a wavelength conversion layer disposed on the low-refractive layer; a low-refractive bottom layer disposed between the low-refractive layer and the light guide plate; and a low-refractive covering layer disposed between the low-refractive layer and the wavelength conversion layer.
[0012] A display according to yet another example includes an optical component, a light source, and a display panel, wherein the optical component includes a light guide plate; a low-refractive layer, which is disposed on the light guide plate and has a refractive index less than that of the light guide plate; a low-refractive bottom layer, which is disposed between the low-refractive layer and the light guide plate; and a wavelength conversion layer, which is disposed on the low-refractive layer, the light source is disposed on at least one side of the light guide plate, and the display panel is disposed on the optical component.
[0013] A display according to another exemplary embodiment includes an optical member, a light source, and a display panel, wherein the optical member includes a light guide plate; a low-refractive layer, which is disposed on the light guide plate and has a refractive index less than the refractive index of the light guide plate; a wavelength conversion layer, which is disposed on the low-refractive layer; and a low-refractive covering layer, which is disposed between the low-refractive layer and the wavelength conversion layer, the light source is disposed on at least one side of the light guide plate, and the display panel is disposed on the optical member.
[0014] It is to be understood that both the foregoing general description and the following detailed description are exemplary and explanatory and are intended to provide further explanation of the invention as claimed. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] The accompanying drawings, which are included to provide a further understanding of the invention and are incorporated in and constitute a part of this specification, illustrate exemplary embodiments of the invention and together with the description serve to explain the inventive concept.
[0016] Figure 1 is a perspective view of an optical member and a light source according to an exemplary embodiment.
[0017] Figure 2 is along Figure 1 A cross-sectional view taken along line II-II'.
[0018] Figure 3 and Figure 4 is a cross-sectional view of a low-refractive layer according to an exemplary embodiment.
[0019] Figure 5A is a table showing a wavelength conversion underlayer according to an exemplary embodiment, and Figure 5B The transmittance is shown relative to the silicon nitride (SiN x ) is a graph showing the change in thickness.
[0020] Fig. 6A , Figure 6B , Figure 6C and Fig.6D is shown for Figure 5A Table of laminate structures and thicknesses that ensure maximum transmittance for each case.
[0021] Figure 7 , Figure 8 , Fig. 9 , Fig.10 , Fig.11 , Fig.12 , Fig.13 and Fig.14 is a cross-sectional view of a wavelength conversion bottom layer according to an exemplary embodiment.
[0022] Fig.15A is a table showing wavelength conversion cover layers according to exemplary embodiments, and Fig. 15B The transmittance is shown relative to the silicon nitride (SiN) on the wavelength conversion layer. x ) is a graph showing the change in thickness.
[0023] Fig.16A , Fig. 16B and Fig. 16C It is used for Fig.15A Table of laminate structures and thicknesses that ensure maximum transmittance for each case.
[0024] Fig.17 , Fig.18 , Fig.19 and Fig. 20 is a cross-sectional view of a wavelength conversion cover layer according to an exemplary embodiment.
[0025] Fig.21 , Fig. 22 and Fig.23 is a cross-sectional view of an optical member according to an exemplary embodiment.
[0026] Fig.24 is a cross-sectional view of a display according to an exemplary embodiment.
[0027] Fig.25 is a cross-sectional view of a display according to an exemplary embodiment. DETAILED DESCRIPTION
[0028] In the following description, for the purpose of explanation, many specific details are set forth in order to provide a thorough understanding of various exemplary embodiments or embodiments of the present invention. As used herein, "embodiment" and "implementation" are interchangeable words, which are non-limiting examples of devices or methods using one or more inventive concepts disclosed herein. However, it is apparent that various exemplary embodiments can be practiced without these specific details or using one or more equivalent arrangements. In other cases, well-known structures and devices are shown in block diagram form to avoid unnecessary obscurity of various exemplary embodiments. In addition, various exemplary embodiments may be different, but do not have to be exclusive. For example, without departing from the present invention, the specific shape, configuration and characteristics of the exemplary embodiment may be used or implemented in another exemplary embodiment.
[0029] Unless otherwise specified, the exemplary embodiments shown should be understood as providing exemplary features of different details of some ways in which the inventive concept can be implemented in practice. Therefore, unless otherwise specified, the features, components, modules, layers, films, panels, regions and / or aspects, etc. (hereinafter individually or collectively referred to as "elements") of various embodiments can be combined, separated, interchanged and / or rearranged without departing from the inventive concept.
[0030] Cross-hatching and / or shading are generally provided in the drawings to clarify the boundaries between adjacent elements. Therefore, unless otherwise stated, the presence or absence of cross-hatching or shading will not convey or indicate any preference or requirement for the specific material, material properties, size, ratio, commonality between the illustrated elements and / or any other characteristics, attributes, properties, etc. of the elements. In addition, in the drawings, the size and relative size of the elements may be magnified for the purpose of clarity and / or description. When the exemplary embodiments can be implemented differently, the specific processing order can be performed differently from the described order. For example, two consecutively described processes can be performed substantially simultaneously or in an order opposite to the described order. Moreover, the same reference numerals represent the same elements.
[0031] When an element such as a layer is referred to as being "on", "connected to" or "coupled to" another element or layer, it may be directly on, directly connected to or coupled to another element or layer, or there may be an intermediate element or layer. However, when an element or layer is referred to as being "directly on", "directly connected to" or "directly coupled to" another element or layer, there are no intermediate elements or layers. For this purpose, the term "connected" may refer to physical, electrical and / or fluid connections, with or without intermediate elements. In addition, the D1 axis, the D2 axis, and the D3 axis are not limited to the three axes of a rectangular coordinate system (e.g., an x-axis, a y-axis, and a z-axis), and may be interpreted in a broader sense. For example, the D1 axis, the D2 axis, and the D3 axis may be perpendicular to each other, or may represent different directions that are not perpendicular to each other. For the purpose of this disclosure, "at least one of X, Y, and Z" and "at least one selected from the group consisting of X, Y, and Z" may be interpreted as only X, only Y, only Z, or any combination of two or more of X, Y, and Z, such as, for example, XYZ, XYY, YZ, and ZZ. As used herein, the term "and / or" includes any and all combinations of one or more of the associated listed items.
[0032] Although the terms "first", "second", etc. may be used herein to describe various types of elements, these elements should not be limited by these terms. These terms are used to distinguish one element from another element. Therefore, without departing from the teachings of the present disclosure, the first element discussed below may be referred to as the second element.
[0033] Spatially relative terms, such as "below," "beneath," "below," "lower," "above," "above," "higher," "side" (e.g., "sidewall"), and the like, may be used herein for descriptive purposes, and thereby describe the relationship of one element to other element(s) shown in the drawings. Spatially relative terms are intended to encompass different orientations of the device in use, operation, and / or manufacture, in addition to the orientation depicted in the drawings. For example, if the device in the figure is flipped, elements described as being "below" or "below" other elements or features will be oriented "above" the other elements or features. Thus, the exemplary term "below" can include both orientations of above and below. Furthermore, the device may be oriented in other ways (e.g., rotated 90 degrees or in other orientations), and therefore, the spatially relative descriptors used herein are interpreted accordingly.
[0034] The terms used herein are for the purpose of describing specific embodiments, and are not intended to limit. As used herein, the singular forms "one", "an" and "the" are also intended to include plural forms, unless the context clearly states otherwise. In addition, when used in this specification, the terms "include", "comprise", "contain", and / or "have" specify the presence of the features, integers, steps, operations, elements, parts and / or its groups, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or its groups. It should also be noted that, as used herein, the terms "substantially", "about" and other similar terms are used as approximations rather than degree terms, and are therefore used to consider the inherent deviations in the values measured, calculated and / or provided that will be recognized by those of ordinary skill in the art.
[0035] Various exemplary embodiments are described herein with reference to cross-sectional views and / or exploded views, which are schematic diagrams of idealized exemplary embodiments and / or intermediate structures. Therefore, variations in the illustrated shapes due to, for example, manufacturing techniques and / or tolerances can be expected. Therefore, the exemplary embodiments disclosed herein should not necessarily be interpreted as limited to the specific illustrated regional shapes, but rather include shape deviations caused by, for example, manufacturing. In this way, the regions shown in the drawings may be schematic in nature, and the shapes of these regions may not reflect the actual shapes of the regions of the device, and are therefore not necessarily intended to be limiting.
[0036] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as those commonly understood by those skilled in the art to which the present disclosure belongs. Terms such as those defined in commonly used dictionaries should be interpreted as having a meaning consistent with their meaning in the context of the relevant art, and should not be interpreted in an idealized or overly formal sense unless explicitly defined as such herein.
[0037] Figure 1 is a perspective view of an optical member 100 and a light source 400 according to an exemplary embodiment. Figure 2 is along Figure 1 A cross-sectional view taken along line II-II'.
[0038] refer to Figure 1 and Figure 2 The optical member 100 may include a light guide plate 10, a wavelength conversion bottom layer 70 disposed on the light guide plate 10, a wavelength conversion layer 50 disposed on the wavelength conversion bottom layer 70, and a wavelength conversion cover layer 60 disposed on the wavelength conversion layer 50. The wavelength conversion bottom layer 70 may include a low-refractive bottom layer 20, a low-refractive layer 30 disposed on the low-refractive bottom layer 20, and a low-refractive cover layer 40 disposed on the low-refractive layer 30.
[0039] The light guide plate 10 may guide a light path. The light guide plate 10 may generally have a substantially polygonal column shape. The planar shape of the light guide plate 10 may be substantially rectangular, but the inventive concept is not limited thereto. In an exemplary embodiment, the light guide plate 10 may have a substantially hexagonal column shape having a rectangular planar shape, and may include an upper surface 10a, a lower surface 10b, and four side surfaces 10S1, 10S2, 10S3, and 10S4. Hereinafter, the four side surfaces of the light guide plate 10 will be respectively indicated as 10S1, 10S2, 10S3, and 10S4, and one of the four side surfaces will generally be indicated as 10S.
[0040] In an exemplary embodiment, each of the upper surface 10a and the lower surface 10b of the light guide plate 10 may be disposed on a corresponding plane. More specifically, the plane on which the upper surface 10a is disposed may be substantially parallel to the plane on which the lower surface 10b is disposed, so that the total thickness of the light guide plate 10 is uniform. However, the upper surface 10a or the lower surface 10b may be formed by a plurality of planes, or the plane on which the upper surface 10a is disposed may intersect the plane on which the lower surface 10b is disposed. For example, the light guide plate 10 may be thinned from one side surface (e.g., a light incident surface) toward another side surface (e.g., an opposite surface) facing the one side surface, such as a wedge-shaped light guide plate. Alternatively, the lower surface 10b may be inclined upward from one side surface (e.g., a light incident surface) toward another side surface (e.g., an opposite surface) facing the one side surface until a predetermined distance, so that the light guide plate 10 is thinned until the predetermined distance, and then has a substantially uniform thickness beyond the predetermined distance.
[0041] In the optical member 100 according to the exemplary embodiment, the light source 400 may be disposed adjacent to at least one side surface 10S of the light guide plate 10. Figure 1 , a plurality of light emitting diode (LED) light sources 410 are mounted on a printed circuit board 420 and disposed adjacent to the side surface 10S1 of the light guide plate 10. However, the inventive concept is not limited thereto, and for example, the LED light source 410 may be disposed adjacent to the side surfaces 10S1 and 10S3 along two long sides, or may be disposed adjacent to the side surface 10S2 or 10S4 along one short side, or disposed adjacent to the side surfaces 10S2 and 10S4 at two short sides. Figure 1 As shown, a side surface 10S1 of the light guide plate 10 adjacent to the light source 400 may be a light incident surface to which light of the light source 400 is directly incident, and a side surface 10S3 at another long side facing the side surface 10S1 may be an opposing surface.
[0042] The light guide plate 10 may include an inorganic material. For example, the light guide plate 10 may be made of glass.
[0043] The optical interface may be formed at the surface where the layers 20, 30, 40, 50 and 60 of the optical member 100 meet each other. The optical member 100 may include a plurality of optical interfaces 30a, 30b, 50a and 50b. Each optical interface 30a, 30b, 50a and 50b may be substantially parallel to the upper surface 10a of the light guide plate 10.
[0044] The wavelength conversion bottom layer 70 is disposed on the upper surface 10a of the light guide plate 10. The wavelength conversion bottom layer 70 may include a low-refractive layer 30, a low-refractive bottom layer 20, and a low-refractive cover layer 40. The wavelength conversion bottom layer 70 may be directly formed on the upper surface 10a of the light guide plate 10 to contact the upper surface 10a of the light guide plate 10. The wavelength conversion bottom layer 70 is interposed between the light guide plate 10 and the wavelength conversion layer 50 to facilitate total reflection of the optical member 100.
[0045] More specifically, in order for the light guide plate 10 to effectively guide light from the light incident surface 10S1 to the opposite surface 10S3, effective total internal reflection should occur in the light guide plate 10. One condition under which total internal reflection can occur in the light guide plate 10 is that the refractive index of the light guide plate 10 is greater than the refractive index of the medium forming an optical interface with the light guide plate 10. When the refractive index of the medium forming an optical interface with the light guide plate 10 is low, the critical angle of total reflection is smaller, resulting in more total internal reflection.
[0046] For example, when the light guide plate 10 is made of glass having a refractive index of about 1.5, sufficient total reflection may occur on the lower surface 10b of the light guide plate 10 because the lower surface 10b is exposed to an air layer having a refractive index of about 1 and thus forms an optical interface with the air layer.
[0047] On the other hand, since other optical functional layers are integrally laminated on the upper surface 10a of the light guide plate 10, it may be difficult to achieve sufficient total reflection on the upper surface 10a compared to the lower surface 10b. For example, if a material layer having a refractive index of 1.5 or greater is laminated on the upper surface 10a of the light guide plate 10, total reflection will not occur on the upper surface 10a of the light guide plate 10. In addition, if a material layer having a refractive index of, for example, about 1.49 (which is slightly smaller than the refractive index of the light guide plate 10) is laminated on the upper surface 10a of the light guide plate 10, although total internal reflection can occur on the upper surface 10a of the light guide plate 10, sufficient total reflection may not occur due to the increased critical angle. The wavelength conversion layer 50 laminated on the upper surface 10a of the light guide plate 10 typically has a refractive index of about 1.5. If the wavelength conversion layer 50 is directly laminated on the upper surface 10 a of the light guide plate 10 , it may be difficult to have sufficient total reflection on the upper surface 10 a of the light guide plate 10 .
[0048] The low refractive layer 30 inserted between the light guide plate 10 and the wavelength conversion layer 50 to form an interface with the upper surface 10a of the light guide plate 10 has a refractive index lower than that of the light guide plate 10, so total reflection can occur on the upper surface 10a of the light guide plate 10. In addition, the low refractive layer 30 has a refractive index smaller than that of the wavelength conversion layer 50, which is a material layer provided on the low refractive layer 30, so that more total reflection can occur than when the wavelength conversion layer 50 is directly provided on the upper surface 10a of the light guide plate 10.
[0049] When the low-refractive bottom layer 20 is disposed on the light guide plate 10, total reflection may also occur at the interface between the light guide plate 10 and the low-refractive bottom layer 20 due to the difference in refractive index between the light guide plate 10 and the low-refractive bottom layer 20. However, light incident on the interface at an angle less than the critical angle of total reflection may travel toward the low-refractive bottom layer 20. Then, the light may be reflected or refracted again at the interface between the low-refractive bottom layer 20 and the low-refractive layer 30. When the refractive index of the low-refractive layer 30 is less than the refractive index of the low-refractive bottom layer 20, total reflection may also occur at the interface. When the optical member 100 includes the low-refractive bottom layer 20, the low-refractive bottom layer 20 is inserted between the light guide plate 10 and the low-refractive layer 30. However, the difference in refractive index between the light guide plate 10 and the low-refractive layer 30 ultimately determines the critical angle of total reflection. Since the difference in refractive index increases as the refractive index of the low-refractive layer 30 becomes smaller, the critical angle of total reflection may become smaller, resulting in more total reflection.
[0050] The wavelength conversion bottom layer 70 inserted between the light guide plate 10 and the wavelength conversion layer 50 to form an interface with the upper surface 10a of the light guide plate 10 may include a low refractive layer 30. The low refractive layer 30 has a refractive index less than that of the light guide plate 10, so that total reflection can occur on the lower surface 30b of the low refractive layer 30. In addition, the low refractive layer 30 has a refractive index less than that of the wavelength conversion layer 50, which is a material layer disposed on the low refractive layer 30, so that more total reflection can occur than when the wavelength conversion layer 50 is directly disposed on the upper surface 10a of the light guide plate 10.
[0051] The difference between the refractive index of the light guide plate 10 and the refractive index of the low refractive layer 30 may be 0.2 or more. When the refractive index of the low refractive layer 30 is 0.2 or more less than the refractive index of the light guide plate 10, sufficient total reflection may occur on the lower surface 30b of the low refractive layer 30. There is no upper limit to the difference between the refractive index of the light guide plate 10 and the refractive index of the low refractive layer 30. However, considering the typical material of the light guide plate 10 and the typical refractive index of the low refractive layer 30, the difference between the refractive index of the light guide plate 10 and the refractive index of the low refractive layer 30 may be 1 or less. The refractive index of the low refractive layer 30 may be in the range of 1.2 to 1.4. Generally, as the refractive index of the solid medium becomes close to 1, the manufacturing cost increases exponentially. When the refractive index of the low refractive layer 30 is 1.2 or more, the excessive increase of the manufacturing cost may be prevented. In addition, the low refractive layer 30 having a refractive index of 1.4 or less is advantageous in fully reducing the critical angle of total reflection of the upper surface 10a of the light guide plate 10. In an exemplary embodiment, the low-refractive layer 30 having a refractive index of about 1.25 may be applied.
[0052] In order to have the above-mentioned low refractive index, the low refractive layer 30 may include a void. The void may be made of a vacuum, or may be filled with an air layer, a gas, etc. The space of the void may be defined by particles or a matrix, which will be referred to below. Figure 3 and Figure 4 Describe in more detail.
[0053] Figure 3 and Figure 4 is a cross-sectional view of a low-refractive layer according to an exemplary embodiment.
[0054] In an exemplary embodiment, the low-refractive layer 30 may include a plurality of particles PT, a matrix MX surrounding the particles PT and formed as a single sheet, and a plurality of voids VD, such as Figure 3 The particles PT may be fillers for adjusting the refractive index and mechanical strength of the low-refractive layer 30 .
[0055] The particles PT may be dispersed in the matrix MX of the low-refractive layer 30, and the voids VD may be formed in the opening portion of the matrix MX. For example, after the particles PT and the matrix MX are mixed in a solvent, and when the mixture is dried and / or cured, the solvent may be evaporated. At this time, the voids VD may be formed between portions of the matrix MX.
[0056] In an exemplary embodiment, the low-refractive layer 30 may include a matrix MX and voids VD without particles, such as Figure 4 For example, the low-refractive layer 30 may include a matrix MX (such as foamed resin) formed as a single sheet, and a plurality of voids VD provided in the matrix MX.
[0057] When the low-refractive layer 30 includes the void VD, as Figure 3and Figure 4 As shown, the total refractive index of the low-refractive layer 30 may have a value between the refractive index of the particles PT / matrix MX and the refractive index of the voids VD. When the voids VD are filled with a vacuum having a refractive index of 1, or an air layer or gas having a refractive index of about 1, even if a material having a refractive index of 1.4 or more is used as the particles PT / matrix MX, the total refractive index of the low-refractive layer 30 may have a value of 1.4 or less, for example, about 1.25. In an exemplary embodiment, the particles PT may be made of an inorganic material (e.g., SiO 2 , Fe 2 O 3 MgF 2 ), and the matrix MX may be made of an organic material (eg, polysiloxane). However, the inventive concept is not limited thereto, and other organic materials or inorganic materials may be used.
[0058] Return to reference Figure 1 and Figure 2 , the low refractive layer 30 may have a thickness of 0.4 μm to 2 μm. When the thickness of the low refractive layer 30 is 0.4 μm or more (which is the visible light wavelength range), the low refractive layer 30 may form an effective optical interface. Therefore, total reflection according to Snell's law may occur well on the lower surface 30b of the low refractive layer 30. Too thick a low refractive layer 30 may be detrimental to the thinning of the optical member 100, increase material costs, and destroy the luminescence of the optical member 100. Therefore, the low refractive layer 30 may be formed to have a thickness of 2 μm or less. In an exemplary embodiment, the thickness of the low refractive layer 30 may be about 1 μm.
[0059] The low-refractive base layer 20 may be disposed between the light guide plate 10 and the low-refractive layer 30. The low-refractive base layer 20 may be directly formed on the upper surface 10a of the light guide plate 10 to contact the upper surface 10a of the light guide plate 10. In addition, the low-refractive base layer 20 may contact the lower surface 30b of the low-refractive layer 30. The low-refractive base layer 20 may be inserted between the light guide plate 10 and the low-refractive layer 30. The refractive index of the low-refractive base layer 20 may be greater than the refractive index of the low-refractive layer 30. The low-refractive base layer 20 may have a single-layer structure and include any one of a low-refractive material and a high-refractive material. Alternatively, the low-refractive base layer 20 may have a multilayer structure in which low-refractive materials and high-refractive materials are alternately laminated. The refractive index of the low-refractive material may be 1.3 to 1.7. The refractive index of the high-refractive material may be 1.5 to 2.2. In an exemplary embodiment, the low-refractive material may be silicon oxide (SiO x ), and the high refractive material may be silicon nitride (SiN x ). However, the low-refractive material and the high-refractive material may be various other materials satisfying the above-mentioned refractive index.
[0060] Since the influence of constructive interference or destructive interference of light varies according to the laminating material and lamination thickness of the low-refractive bottom layer 20, the light transmittance can be changed. That is, the light transmittance can be adjusted by controlling the laminating material and lamination thickness of the low-refractive bottom layer 20. In addition, when the low-refractive bottom layer 20 includes an inorganic layer, the inorganic layer can be used as a protective layer to prevent moisture / oxygen from penetrating into the low-refractive layer 30.
[0061] The low refractive cover layer 40 may be disposed between the low refractive layer 30 and the wavelength conversion layer 50. The low refractive cover layer 40 may be directly formed on the upper surface of the low refractive layer 30 to contact the upper surface of the low refractive layer 30. In addition, the low refractive cover layer 40 may contact the lower surface of the wavelength conversion layer 50. The low refractive cover layer 40 may be inserted between the low refractive layer 30 and the wavelength conversion layer 50. The refractive index of the low refractive cover layer 40 may be greater than the refractive index of the low refractive layer 30. The low refractive cover layer 40 helps to cause total reflection from the upper surface of the low refractive layer 30 toward the wavelength conversion layer 50. The low refractive cover layer 40 may have a single-layer structure including any one of a low refractive material and a high refractive material. Alternatively, the low refractive cover layer 40 may have a multilayer structure in which the low refractive material and the high refractive material are alternately laminated. As in the low refractive bottom layer 20, the refractive index of the low refractive material may be 1.2 to 1.7. The refractive index of the high refractive material may be 1.5 to 2.2. In an exemplary embodiment, the low refractive material may be silicon oxide (SiO x ), and the high refractive material may be silicon nitride (SiN x ). However, the low-refractive material and the high-refractive material may include various other materials satisfying the above-mentioned refractive index.
[0062] Since the influence of constructive interference or destructive interference of light changes according to the laminating material and lamination thickness of the low-refractive cover layer 40, the light transmittance can be changed. That is, the light transmittance can be adjusted by controlling the laminating material and lamination thickness of the low-refractive cover layer 40. In addition, the low-refractive cover layer 40 can improve the optical efficiency of the optical member 100. When the light transmitted through the low-refractive layer 30 enters the wavelength conversion layer 50 and encounters the dispersed scattering particles, the light is scattered as its wavelength changes. Here, part of the scattered light can be returned toward the light guide plate 10. If the low-refractive cover layer 40 has a refractive index higher than the refractive index of the low-refractive layer 30, the light can be totally reflected at the interface between the low-refractive cover layer 40 and the low-refractive layer 30, and can be reflected back upward, thereby improving the optical efficiency of the display, such as brightness.
[0063] The low-refractive covering layer 40 can completely overlap with the low-refractive layer 30 to prevent moisture and / or oxygen from penetrating into the low-refractive layer 30. That is, the low-refractive covering layer 40 can prevent deformation of the low-refractive layer 30 and ensure structural stability by increasing hardness. In addition, the low-refractive covering layer 40 including an inorganic layer can prevent moisture and / or oxygen from penetrating into the wavelength conversion layer 50 disposed on the low-refractive covering layer 40 and the low-refractive layer 30 disposed below the low-refractive covering layer 40.
[0064] The wavelength conversion bottom layer 70 may be formed by methods such as deposition and coating. The wavelength conversion bottom layer 70 may be formed on the light guide plate 10 in the order of the low-refractive bottom layer 20, the low-refractive layer 30, and the low-refractive cover layer 40. In an exemplary embodiment, the low-refractive bottom layer 20 and the low-refractive cover layer 40 may be formed by an inorganic layer including an inorganic material using a chemical vapor deposition method. The low-refractive layer 30 may be formed by an organic layer including an organic material using a coating method. Examples of coating methods include slit coating, spin coating, roll coating, spray coating, and inkjet. However, the inventive concept is not limited to a specific coating method, and various other lamination methods may be applied.
[0065] The wavelength conversion layer 50 is disposed on the wavelength conversion bottom layer 70. In an exemplary embodiment, when the wavelength conversion bottom layer 70 includes the low-refractive cover layer 40, the wavelength conversion layer 50 may be disposed on the upper surface of the low-refractive cover layer 40. In an exemplary embodiment, when the wavelength conversion bottom layer 70 does not include the low-refractive cover layer 40, the wavelength conversion layer 50 may be disposed on the upper surface of the low-refractive layer 30. The wavelength conversion layer 50 may include an adhesive layer and wavelength conversion particles dispersed in the adhesive layer. In addition to the wavelength conversion particles, the wavelength conversion layer 50 may further include scattering particles dispersed in the adhesive layer.
[0066] The adhesive layer is a medium into which the wavelength conversion particles are dispersed, and may be made of various resin compositions generally referred to as adhesives. However, the present inventive concept is not limited thereto, and any medium into which the wavelength conversion particles and / or scattering particles may be dispersed may be referred to as an adhesive layer, regardless of its name, other functions attached, constituent materials, etc.
[0067] Wavelength conversion particles are particles that convert the wavelength of incident light. For example, the wavelength conversion particles can be quantum dots, fluorescent materials, or phosphorescent materials. Specifically, quantum dots, which are examples of wavelength conversion particles, are materials with a crystal structure of a few nanometers in size. Quantum dots are composed of hundreds to thousands of atoms and exhibit a quantum confinement effect in which the energy band gap increases due to the small size of the quantum dots. When light with a wavelength higher in energy than the band gap is incident on the quantum dots, the quantum dots become excited by absorbing the light and drop to the ground state while emitting light of a specific wavelength. The emitted light of a specific wavelength has a value corresponding to the band gap. By controlling the size and composition of the quantum dots, the luminescence characteristics of the quantum dots from the quantum confinement effect can be adjusted.
[0068] The quantum dots may include at least one of a II-VI compound, a II-V compound, a III-VI compound, a III-V compound, a IV-VI compound, a I-III-VI compound, a II-IV-VI compound, and a II-IV-V compound.
[0069] The quantum dot may include a core and a shell covering the core. The core may be, for example, but is not limited to, CdS, CdSe, CdTe, ZnS, ZnSe, ZnTe, GaN, GaP, GaAs, GaSb, AlN, AlP, AlAs, AlSb, InP, InAs, InSb, SiC, Ca, Se, In, P, Fe, Pt, Ni, Co, Al, Ag, Au, Cu, FePt, Fe 2 O 3 , Fe 3 O 4 The shell may include, but is not limited to, for example, at least one of ZnS, ZnSe, ZnTe, CdS, CdSe, CdTe, HgS, HgSe, HgTe, AlN, AlP, AlAs, AlSb, GaN, GaP, GaAs, GaSb, GaSe, InN, InP, InAs, InSb, TlN, TlP, TlAs, TlSb, PbS, PbSe, and PbTe.
[0070] The wavelength conversion particles may include a plurality of wavelength conversion particles that convert incident light into light of different wavelengths. For example, the wavelength conversion particles may include a first wavelength conversion particle that converts incident light of a specific wavelength into light of a first wavelength and emits light of the first wavelength, and a second wavelength conversion particle that converts incident light of a specific wavelength into light of a second wavelength and emits light of the second wavelength. In an exemplary embodiment, the light emitted from the light source 400 and then incident on the wavelength conversion particles may be light of a blue wavelength, the first wavelength may be a green wavelength, and the second wavelength may be a red wavelength. For example, the blue wavelength may be a wavelength having a peak value of 420nm to 470nm, the green wavelength may be a wavelength having a peak value of 520nm to 570nm, and the red wavelength may be a wavelength having a peak value of 620nm to 670nm. However, the inventive concept is not limited thereto, and all wavelength ranges that can be identified as blue, green, and red may be used.
[0071] In the above exemplary embodiment, when the blue light incident on the wavelength conversion layer 50 passes through the wavelength conversion layer 50, a portion of the blue light can be incident on the first wavelength conversion particles to be converted into a green wavelength and emitted as light of a green wavelength, another portion of the blue light can be incident on the second wavelength conversion particles to be converted into a red wavelength and emitted as light of a red wavelength, and the remaining portion of the blue light can be emitted because it does not enter the first wavelength conversion particles and the second wavelength conversion particles. Therefore, the light that has passed through the wavelength conversion layer 50 includes all blue wavelengths of light, green wavelengths of light, and red wavelengths of light. If the ratio of the emitted light of different wavelengths is appropriately adjusted, white light or other colors of emitted light can be displayed. The light converted by the wavelength conversion layer 50 is concentrated in a narrow specific wavelength range and has a sharp spectrum with a narrow half-width. Therefore, when a color filter is used to filter the light of this spectrum to achieve color, color reproducibility can be improved.
[0072] Unlike the above exemplary embodiment, incident light may be light having a short wavelength, such as ultraviolet light, and three types of wavelength conversion particles for converting the incident light into blue, green, and red wavelengths may be disposed in the wavelength conversion layer 50 to emit white light.
[0073] The wavelength conversion layer 50 may also include scattering particles. The scattering particles may be non-quantum dot particles that do not have a wavelength conversion function. The scattering particles may scatter incident light so that more incident light enters the wavelength conversion particles. In addition, the scattering particles may uniformly control the output angle of light of each wavelength. Specifically, when a portion of the incident light entering the wavelength conversion particles is emitted after its wavelength is converted by the wavelength conversion particles, the emission direction of the portion of the incident light has a random scattering characteristic. If there are no scattering particles in the wavelength conversion layer 50, the green wavelength and the red wavelength emitted after colliding with the wavelength conversion particles may have a scattered luminescence characteristic, but the blue wavelength emitted without colliding with the wavelength conversion particles may not have a scattered luminescence characteristic. Therefore, the emission amount of the blue / green / red wavelengths may vary according to the output angle. The scattering particles may even provide a scattered luminescence characteristic to the blue wavelength emitted without colliding with the wavelength conversion particles, thereby controlling the output angle of light of each wavelength to be similar. The scattering particles may be made of TiO 2 or SiO 2 Made.
[0074] The wavelength conversion layer 50 may be thicker than the low refractive layer 30. The thickness of the wavelength conversion layer 50 may be about 10 μm to 50 μm. In an exemplary embodiment, the thickness of the wavelength conversion layer 50 may be about 10 μm.
[0075] The wavelength conversion layer 50 may be formed by a method such as coating. For example, the wavelength conversion layer 50 may be formed by slit coating a wavelength conversion composition on the light guide plate 10 having the wavelength conversion bottom layer 70, and drying and curing the wavelength conversion composition. However, the present inventive concept is not limited to a specific method of forming the wavelength conversion layer 50, and various other lamination methods may be applied.
[0076] The wavelength conversion cover layer 60 may be disposed on the wavelength conversion layer 50. The wavelength conversion cover layer 60 may be a passivation layer that prevents moisture and / or oxygen (hereinafter, referred to as "moisture / oxygen") from penetrating. The wavelength conversion cover layer 60 may include a plurality of laminated layers. Each laminated layer may include an inorganic layer or an organic layer. The wavelength conversion cover layer 60 may include at least one inorganic layer. That is, the wavelength conversion cover layer 60 may include a single inorganic layer, a plurality of inorganic layers, or laminated organic and inorganic layers.
[0077] Each laminated layer may include a high refractive material, a low refractive material and / or a transparent organic material. The wavelength conversion cover layer 60 may have a single layer structure including a low refractive material, a high refractive material or a transparent organic material, or may have a multilayer structure in which materials with different refractive indices are laminated. In an exemplary embodiment, the high refractive material and the low refractive material may be silicon nitride, aluminum nitride, zirconium nitride, titanium nitride, hafnium nitride, tantalum nitride, silicon oxide, aluminum oxide, titanium oxide, tin oxide, cerium oxide or silicon oxynitride. In an exemplary embodiment, the high refractive material may be silicon nitride (SiN x ), and the low refractive material may be silicon oxide (SiO x ). The transparent organic material may be silicone resin, acrylic resin or epoxy resin.
[0078] The wavelength conversion cover layer 60 may completely overlap the wavelength conversion layer 50 and cover the upper surface of the wavelength conversion layer 50. In an exemplary embodiment, the wavelength conversion cover layer 60 may cover only the upper surface of the wavelength conversion layer 50. However, in an exemplary embodiment, the wavelength conversion cover layer 60 may further extend outward so as to cover the side surfaces of the wavelength conversion layer 50 and the side surfaces of the wavelength conversion bottom layer 70.
[0079] The thickness of the wavelength conversion cover layer 60 may be 0.1 μm to 5 μm. In an exemplary embodiment, when the wavelength conversion cover layer 60 does not include an organic layer, the thickness of the wavelength conversion cover layer 60 may be 0.15 μm to 0.5 μm. In an exemplary embodiment, when the wavelength conversion cover layer 60 includes an organic layer, the thickness of the wavelength conversion cover layer 60 may be 1 μm to 5 μm. The thickness of the wavelength conversion cover layer 60 may be less than the thickness of the wavelength conversion layer 50. If the thickness of the wavelength conversion cover layer 60 is 0.1 μm or more, the wavelength conversion cover layer 60 may apply a significant moisture / oxygen permeation prevention function. The wavelength conversion cover layer 60 having a thickness of 2 μm or less is advantageous in terms of thinning and transmittance. However, the inventive concept is not limited to a specific thickness of the wavelength conversion cover layer 60, and the wavelength conversion cover layer 60 may have various thicknesses. The refractive index and thickness of the laminate of the wavelength conversion cover layer 60 may affect the amount of light extracted through the upper surface, i.e., the transmittance. This will be described in detail later.
[0080] The wavelength conversion cover layer 60 may be formed by a method such as coating and deposition. For example, an inorganic layer including an inorganic material may be formed on the light guide plate 10 by using a chemical vapor deposition method, and the wavelength conversion base layer 70 and the wavelength conversion layer 50 may be sequentially formed on the light guide plate 10. An organic layer including an organic material may be formed on the light guide plate 10 by a coating method. However, the inventive concept is not limited to a specific method of forming the wavelength conversion cover layer 60, and various other lamination methods may be applied.
[0081] As described above, the optical member 100 can perform both the light guiding function and the wavelength conversion function. The optical member 100 may include a wavelength conversion bottom layer 70 and a wavelength conversion cover layer 60. The wavelength conversion bottom layer 70 may include a low refractive layer 30, a low refractive bottom layer 20, and a low refractive cover layer 40. The low refractive bottom layer 20 and the low refractive cover layer 40 may include a material having a refractive index higher than that of the low refractive layer 30. Since the low refractive bottom layer 20 and the low refractive cover layer 40 change the effect of constructive interference or destructive interference of light incident on the optical member 100, they can improve the light transmittance. The wavelength conversion cover layer 60 may include a layer made of at least one of a high refractive material and a low refractive material. In addition, the wavelength conversion cover layer 60 may be a multilayer further including a transparent organic material. The wavelength conversion cover layer 60 completely covers the wavelength conversion layer 50 to prevent the penetration of moisture / oxygen. In addition, the wavelength conversion cover layer 60 allows the light transmitted through the wavelength conversion layer 50 to be effectively output to the outside of the optical member 100, thereby improving the optical efficiency.
[0082] In addition, the wavelength conversion cover layer 60 provided on the wavelength conversion layer 50 of the optical member 100 can reduce manufacturing costs and thickness compared to a wavelength conversion film provided as a separate film. For example, the wavelength conversion film includes a barrier film attached to the upper and lower surfaces of the wavelength conversion layer 50. The barrier film is not only expensive but also has a thickness of 100 μm or more. Therefore, the total thickness of the wavelength conversion film may be about 270 μm. On the other hand, the total thickness of the optical member 100 except the light guide plate 10 according to the exemplary embodiment may be maintained at about 12 μm to 13 μm. Therefore, the thickness of the display using the optical member 100 can be reduced. In addition, since the expensive barrier film can be omitted from the optical member 100, the manufacturing cost can be controlled to a level lower than when the wavelength conversion film is used.
[0083] The lamination structure and thickness of the wavelength conversion bottom layer 70 for obtaining the maximum light transmittance will now be described. When light passes through a medium having different refractive indices, reflection and refraction of light occur at a point where the medium having different refractive indices meets. If the refractive index and thickness of the medium can be identified, the transmittance of the lamination structure can be obtained using the Fresnel equation related to the reflection and refraction of light. That is, a simulation for obtaining transmittance according to the lamination structure and thickness of the wavelength conversion bottom layer 70 can be performed.
[0084] Figure 5A is a table showing a wavelength conversion underlayer according to an exemplary embodiment. Figure 5B The transmittance is shown relative to the silicon nitride (SiN x ) is a graph showing the change in thickness. FIG. 6A to FIG. 6D It is shown in Figure 5AThe wavelength converting underlayer in each lamination case ensures maximum transmittance in the form of lamination structure and thickness.
[0085] Figure 5A is a table showing conditions for performing simulation. Figure 5A In the description, the case where each of the low refractive primer layer and the low refractive cover layer has two layers will be described as an example. When the low refractive primer layer and the low refractive cover layer are omitted or only one of them is provided, the omitted one or more layers will be represented as having a thickness of 0 μm.
[0086] refer to Figure 2 and Figure 5A , the wavelength conversion bottom layer 70 is laminated on the light guide plate 10 in the order of the low refractive bottom layer 20, the low refractive layer 30 and the low refractive cover layer 40. The wavelength conversion bottom layer 70 may be inserted between the light guide plate 10 and the wavelength conversion layer 50. The low refractive bottom layer 20 and the low refractive cover layer 40 may each include two layers or less.
[0087] Under the simulation conditions, the thickness of each layer is selected within the range of 0 μm to 0.2 μm. As described above, a thickness of 0 μm means that the corresponding layer is not included. Under the simulation conditions, the thickness of the low-refractive layer 30 is set to 1 μm. The layers included in the low-refractive bottom layer 20 and the low-refractive cover layer 40 may be made of a high-refractive material and a low-refractive material. In an exemplary embodiment, the high-refractive material may be silicon nitride (SiN x ), and the low refractive material may be silicon oxide (SiO x The high refractive material will be described below as silicon nitride (SiN x ), and the low refractive material will be described below as silicon oxide (SiO x ). The layers including the high refractive material and the layers including the low refractive material may be alternately laminated. The refractive indexes of the high refractive material and the low refractive material may be greater than the refractive index of the low refractive layer 30. The conditions for obtaining the light transmittance of the wavelength conversion bottom layer 70 may be divided into four conditions according to the laminated structure.
[0088] refer to Figure 5A The wavelength conversion bottom layer of Case 1 includes a low-refractive bottom layer 20 laminated on the light guide plate in the order of a high-refractive material and a low-refractive material, and a low-refractive covering layer 40 laminated on the low-refractive layer in the order of a high-refractive material and a low-refractive material.
[0089] The wavelength conversion bottom layer of Case 2 includes a low refractive bottom layer 20 laminated on the light guide plate in the order of a low refractive material and a high refractive material, and a low refractive cover layer 40 laminated on the low refractive layer in the order of a high refractive material and a low refractive material.
[0090] The wavelength conversion bottom layer of Case 3 includes a low refractive bottom layer 20 laminated on the light guide plate in the order of a high refractive material and a low refractive material, and a low refractive cover layer 40 laminated on the low refractive layer in the order of a low refractive material and a high refractive material.
[0091] The wavelength conversion bottom layer of Case 4 includes a low-refractive bottom layer 20 laminated on the light guide plate in the order of low-refractive material and high-refractive material, and a low-refractive cover layer 40 laminated on the low-refractive layer in the order of low-refractive material and high-refractive material.
[0092] Figure 5B is a diagram showing the silicon nitride (SiN) low refractive underlayer provided on the light guide plate in case 1. x ) is a graph showing the change in transmittance under each lamination condition of thickness. Figure 5B is an example of simulation results, and the transmittance of the wavelength conversion bottom layer of the laminated structure with other cases can also be Figure 5B Here, the transmittance represents the ratio of the blue light transmitted through the lower wavelength conversion bottom layer to the blue light incident from the light source. Figure 5B In the graph, silicon nitride (SiN x ) refers to a high refractive material, and silicon oxide (SiO x ) means a low refractive material.
[0093] refer to Figure 2 and Figure 5B , executed on it Figure 5B The wavelength conversion bottom layer 70 of the simulation has the structure of the above-mentioned case 1. The wavelength conversion bottom layer 70 of case 1 includes silicon nitride (SiN x ) and silicon oxide (SiO x ) in the order of laminating a low-refractive bottom layer 20, and a silicon nitride (SiN x ) and silicon oxide (SiO x ) are sequentially laminated to form a low-refractive covering layer 40. The silicon nitride (SiN x ) corresponds to Figure 5B The X-axis of the graph corresponds to silicon nitride (SiN x ) thickness. That is, in this graph, the silicon nitride (SiN x ) has a variable thickness, and the silicon oxide (SiO x ) thickness and the silicon nitride (SiN x ) and silicon oxide (SiO x ) has a specified value. Figure 5B Three graphs G1, G2 and G3 are shown, which show that when the silicon oxide (SiOx ) thicknesses of 0.06 μm, 0.08 μm, and 0.2 μm, respectively, compared to the transmittance of the silicon nitride (SiN x Here, the silicon nitride (SiN x ) and silicon oxide (SiO x ) are all 0 μm, indicating that the wavelength conversion bottom layer 70 does not include the low-refractive covering layer 40 .
[0094] G1 is a graph showing that when the silicon oxide (SiO x G2 is a graph showing the change in transmittance when the thickness of the low refractive underlayer 20 is 0.06 μm. x G3 is a graph showing the change in transmittance when the thickness of the low refractive underlayer 20 is 0.08 μm. x ) is 0.2 μm. x ) thickness is about 0.1 μm, G1 has the maximum transmittance. x ) thickness is about 0.02 μm or about 0.14 μm, G2 has the maximum transmittance. x ) thickness is about 0.1 μm, G3 has the maximum transmittance. That is, when the lamination structure (such as lamination order and lamination thickness) is changed, the transmittance also changes. Therefore, the maximum transmittance under each lamination condition can be identified, and therefore, each lamination condition with the maximum transmittance can be determined.
[0095] FIG. 6A to FIG. 6D : is a table showing the lamination structure and thickness that ensure the maximum blue light transmittance in each lamination case of the wavelength conversion bottom layer. FIG. 6A to FIG. 6D In , three result values with high transmittance are shown for each lamination case. 1.5T glass means that the light guide plate has a thickness of 1.5 mm. The result values are the results of simulations performed with a low refractive layer of 1 μm and a wavelength conversion layer of 10 μm. FIG. 6A to FIG. 6D Silicon oxide (SiO x ) is an example of a low refractive material, and silicon nitride (SiN x ) are examples of highly refractive materials.
[0096] refer to Figure 2 and Fig. 6A , the result of case 1 is 3 according to Figure 5B The result value of G1 described in the above is shown in Figure 3. The result 3 of Case 1 shows that the low-refractive bottom layer 20 and the silicon nitride (SiNx ) and silicon oxide (SiO x ) is the transmittance of the wavelength conversion bottom layer 70 of the low-refractive cover layer 40 of 0 μm, and in the low-refractive bottom layer 20, the silicon nitride (SiN x ) and 0.06μm silicon oxide (SiO x ) are sequentially laminated on the light guide plate, that is, the low refractive cover layer 40 is not included. The wavelength conversion bottom layer 70 of result 3 has a blue light transmittance of 81.3%. If the maximum blue light transmittance in each case is obtained like this, all four cases can have a maximum transmittance of about 81.4%. Now, reference will be made to Figures 7 to 14 A laminate structure of a wavelength conversion bottom layer according to various exemplary embodiments is described in detail.
[0097] Figures 7 to 14 2 are cross-sectional views of wavelength conversion bottom layers 71 to 78 according to an exemplary embodiment. Figures 7 to 14 The wavelength conversion substrates 71 to 78 may each include a low-refractive layer 30, and may also include a low-refractive layer 20 (see Figure 2 ) and a low-refractive coating 40 (see Figure 2 ). In some exemplary embodiments, the wavelength conversion bottom layer does not include a low-refractive bottom layer or a low-refractive cover layer. However, in order to effectively cause total reflection and improve light transmittance, the wavelength conversion bottom layers 71 to 78 may each include a low-refractive bottom layer 20 (see Figure 2 ) and a low-refractive coating 40 (see Figure 2 ) at least one of the following. The low refractive index bottom layer 20 (see Figure 2 ) and a low-refractive coating 40 (see Figure 2 ) may have a single-layer structure or a multi-layer structure in which a high-refractive material and a low-refractive material are alternately laminated. Silicon nitride (SiN x ) will be described below as an example of a high refractive material, and silicon oxide (SiO x ) will be described below as an example of a low refractive material. However, the inventive concept is not limited to the above examples.
[0098] exist Figure 7 In the embodiment, the low-refractive base layer 21 and the low-refractive cover layer 41 of the wavelength conversion base layer 71 have a single-layer structure. Figure 7 The wavelength conversion bottom layer 71 corresponds to Figure 6B The result of case 2 in the structure of 2. That is, in Figure 7 In the wavelength conversion bottom layer 71, the low-refractive bottom layer 21 is a single layer made of a high-refractive material, and the low-refractive cover layer 41 is a single layer made of a low-refractive material. In an exemplary embodiment, the low-refractive bottom layer 21 is made of silicon nitride (SiNx ) and has a thickness of 0.06 μm. The low-refractive cover layer 41 is made of silicon oxide (SiO x ) and has a thickness of 0.1 μm. The wavelength conversion underlayer 71 according to the illustrated exemplary embodiment has a blue light transmittance of 81.3%.
[0099] exist Figure 8 , the low-refractive base layers 22a and 22b of the wavelength conversion base layer 72 include alternately laminated materials having different refractive indices, and the low-refractive cover layer 42 is a single-layer structure. Figure 8 The wavelength conversion bottom layer 72 corresponds to Fig. 6A The structure of result 1 and result 2 in case 1. That is, in Figure 8 In the wavelength conversion bottom layer 72, the low-refractive bottom layers 22a and 22b may be a multilayer including a first low-refractive bottom layer 22a and a second low-refractive bottom layer 22b having different refractive indices, and the low-refractive cover layer 42 may be a single layer of a low-refractive material. The refractive index of the first low-refractive bottom layer 22a may be greater than the refractive index of the second low-refractive bottom layer 22b. The second low-refractive bottom layer 22b may include the same material as the low-refractive cover layer 42. In an exemplary embodiment, the first low-refractive bottom layer 22a is made of silicon nitride (SiN x ) and has a thickness of 0.02 μm. The second low-refractive bottom layer 22b is made of silicon oxide (SiO x ) and has a thickness of 0.06 μm. The low-refractive cover layer 42 is made of silicon oxide (SiO x ) and has a thickness of 0.04 μm, silicon oxide (SiO x ) is a low refractive material. Therefore, the blue light transmittance of the wavelength conversion bottom layer 72 is 81.4%. The wavelength conversion bottom layer 72 according to the exemplary embodiment is the same as the wavelength conversion bottom layer 72 of the exemplary embodiment described above in terms of the laminated material, but the thickness of each layer is different. The thickness of the first low refractive bottom layer 22a is 0.02μm. The thickness of the second low refractive bottom layer 22b is 0.08μm. The thickness of the low refractive cover layer 42 is 0.14μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 72 is 81.4%.
[0100] exist Fig. 9 In the embodiment, the low-refractive base layers 23a and 23b of the wavelength conversion base layer 73 include alternately laminated materials having different refractive indices, and the low-refractive cover layer 43 has a single-layer structure. Fig. 9 The wavelength conversion bottom layer 73 corresponds to Figure 6B The structure of result 1 and result 3 in case 2. That is, in Fig. 9In the wavelength conversion bottom layer 73, the low-refractive bottom layers 23a and 23b may be a multilayer including a first low-refractive bottom layer 23a and a second low-refractive bottom layer 23b having different refractive indices, and the low-refractive cover layer 43 may be a single layer of a low-refractive material. Fig. 9 The wavelength conversion bottom layer 73 may include Figure 8 However, in Fig. 9 In the exemplary embodiment shown, the refractive index of the first low-refractive bottom layer 23a may be less than the refractive index of the second low-refractive bottom layer 23b. In addition, the first low-refractive bottom layer 23a may include the same material as the low-refractive cover layer 43. In the exemplary embodiment, the first low-refractive bottom layer 23a is made of silicon oxide (SiO x ) and has a thickness of 0.06 μm. The second low-refractive bottom layer 23b is made of silicon nitride (SiN x ) and has a thickness of 0.08 μm. The low-refractive cover layer 43 is made of silicon oxide (SiO x ) and has a thickness of 0.02 μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 73 is 81.4%. The wavelength conversion bottom layer 73 according to the exemplary embodiment is the same as the wavelength conversion bottom layer 73 of the exemplary embodiment described above in terms of the laminated material, but the thickness of each layer is different. The thickness of the first low-refractive bottom layer 23a is 0.04 μm. The thickness of the second low-refractive bottom layer 23b is 0.08 μm. The thickness of the low-refractive covering layer 43 is 0.02 μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 73 is 81.3%.
[0101] exist Fig.10 , the wavelength conversion bottom layer 74 does not include a low-refractive bottom layer, and the low-refractive cover layers 44a and 44b have a multi-layer structure. Fig.10 The wavelength conversion substrate 74 corresponds to Fig.6D The result of case 4 in 3 is the structure. That is, in Fig.10 In the wavelength conversion bottom layer 74, no low-refractive bottom layer is provided, that is, the low-refractive bottom layer has a thickness of 0 μm, and the low-refractive cover layers 44a and 44b may be a multilayer including a first low-refractive cover layer 44a and a second low-refractive cover layer 44b having different refractive indices. The refractive index of the first low-refractive cover layer 44a may be smaller than the refractive index of the second low-refractive cover layer 44b. In an exemplary embodiment, the first low-refractive cover layer 44a is made of silicon oxide (SiO x ) and has a thickness of 0.06 μm. The second low-refractive cover layer 44b is made of silicon nitride (SiN x ) and has a thickness of 0.1 μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 74 is 81.3%.
[0102] exist Fig.11, the low-refractive base layer 25 of the wavelength conversion base layer 75 is a single-layer structure, and the low-refractive cover layers 45a and 45b are a multi-layer structure in which materials having different refractive indices are alternately laminated. Fig.11 The wavelength conversion substrate 75 is Figure 6C The result of case 3 in 1 corresponds to the structure. That is, in Fig.11 In the wavelength conversion bottom layer 75 of the embodiment, the low-refractive bottom layer 25 may have a single-layer structure including a high-refractive material, and the low-refractive cover layers 45a and 45b may be a multilayer including a first low-refractive cover layer 45a and a second low-refractive cover layer 45b having different refractive indices. The refractive index of the first low-refractive cover layer 45a may be smaller than the refractive index of the second low-refractive cover layer 45b. The low-refractive bottom layer 25 may be made of the same material as the second low-refractive cover layer 45b. In an exemplary embodiment, the low-refractive bottom layer 25 is made of silicon nitride (SiN x ) and has a thickness of 0.02 μm. The first low-refractive cover layer 45a is made of silicon oxide (SiO x ) and has a thickness of 0.06 μm. The second low-refractive cover layer 45b is made of silicon nitride (SiN x ) and has a thickness of 0.04 μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 75 is 81.4%.
[0103] exist Fig.12 , the low-refractive base layer 26 of the wavelength conversion base layer 76 has a single-layer structure, and the low-refractive cover layers 46a and 46b have a multi-layer structure in which materials having different refractive indices are alternately laminated. Fig.12 The wavelength conversion substrate 76 corresponds to Fig.6D The structure of result 1 and result 2 in case 4. That is, in Fig.12 In the wavelength conversion bottom layer 76, the low-refractive bottom layer 26 may have a single-layer structure including a high-refractive material, and the low-refractive cover layers 46a and 46b may be a multilayer including a first low-refractive cover layer 46a and a second low-refractive cover layer 46b having different refractive indices. The refractive index of the first low-refractive cover layer 46a may be less than the refractive index of the second low-refractive cover layer 46b. Fig.12 The wavelength conversion bottom layer 76 may include Fig.11 However, in Fig.12 In the exemplary embodiment, the low-refractive bottom layer 26 may be made of a low-refractive material. In addition, the low-refractive bottom layer 26 may be made of the same material as the first low-refractive cover layer 46a. In the exemplary embodiment, the low-refractive bottom layer 26 is made of silicon oxide (SiO x ) and has a thickness of 0.06 μm. The first low-refractive cover layer 46a is made of silicon oxide (SiO x) and has a thickness of 0.08 μm. The second low-refractive cover layer 46 b is made of silicon nitride (SiN x ) and has a thickness of 0.02 μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 76 is 81.4%. The wavelength conversion bottom layer 76 according to the exemplary embodiment is the same as the wavelength conversion bottom layer 76 of the exemplary embodiment described above in terms of the laminated material, but the thickness of each layer is different. The thickness of the low-refractive bottom layer 26 is 0.04 μm. The thickness of the first low-refractive covering layer 46a is 0.08 μm. The thickness of the second low-refractive covering layer 46b is 0.02 μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 76 is 81.3%.
[0104] exist Fig.13 , the low-refractive base layers 27a and 27b and the low-refractive cover layers 47a and 47b of the wavelength conversion base layer 77 have a multi-layer structure in which materials having different refractive indices are alternately laminated. Fig.13 The wavelength conversion substrate 77 corresponds to Figure 6C The structure of result 2 and result 3 in case 3. That is, in Fig.13 In the wavelength conversion bottom layer 77, the low-refractive bottom layers 27a and 27b may be a multilayer including a first low-refractive bottom layer 27a and a second low-refractive bottom layer 27b having different refractive indices, and the low-refractive cover layers 47a and 47b may be a multilayer including a first low-refractive cover layer 47a and a second low-refractive cover layer 47b having different refractive indices. The refractive index of the first low-refractive bottom layer 27a may be greater than the refractive index of the second low-refractive bottom layer 27b. The refractive index of the first low-refractive cover layer 47a may be less than the refractive index of the second low-refractive cover layer 47b. In addition, the first low-refractive bottom layer 27a may be made of the same material as the second low-refractive cover layer 47b, and the second low-refractive bottom layer 27b may be made of the same material as the first low-refractive cover layer 47a. In an exemplary embodiment, the first low-refractive bottom layer 27a is made of silicon nitride (SiN x ) and has a thickness of 0.02 μm. The second low-refractive bottom layer 27b is made of silicon oxide (SiO x ) and has a thickness of 0.02 μm. The first low-refractive cover layer 47a is made of silicon oxide (SiO x ) and has a thickness of 0.04 μm. The second low-refractive cover layer 47b is made of silicon nitride (SiN x) and has a thickness of 0.06μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 77 is 81.4%. The wavelength conversion bottom layer 77 according to the embodiment is the same as the wavelength conversion bottom layer 77 of the exemplary embodiment described above in terms of the laminated material, but the thickness of each layer is different. The thickness of the first low-refractive bottom layer 27a is 0.02μm. The thickness of the second low-refractive covering layer 47b is 0.04μm. The thickness of the first low-refractive covering layer 47a is 0.02μm. The thickness of the second low-refractive covering layer 47b is 0.08μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 77 is 81.4%.
[0105] exist Fig.14 In, with Fig.10 In contrast, the wavelength conversion substrate 78 does not include a low-refractive cover layer, and the low-refractive substrates 28a and 28b have a multi-layer structure. Fig.14 The wavelength conversion substrate 78 corresponds to Fig. 6A The result of case 1 in 3 is the structure. That is, in Fig.14 In the wavelength conversion bottom layer 78, no low-refractive covering layer is provided, that is, the low-refractive covering layer has a thickness of 0 μm, and the low-refractive bottom layers 28a and 28b may be a multilayer including a first low-refractive bottom layer 28a and a second low-refractive bottom layer 28b having different refractive indices. The refractive index of the first low-refractive bottom layer 28a may be greater than the refractive index of the second low-refractive bottom layer 28b. In an exemplary embodiment, the first low-refractive bottom layer 28a is made of silicon nitride (SiN x ) and has a thickness of 0.1 μm. The second low-refractive bottom layer 28b is made of silicon oxide (SiO x ) and has a thickness of 0.06 μm. Therefore, the blue light transmittance of the wavelength conversion bottom layer 78 is 81.3%.
[0106] Fig.15A is a table showing the lamination of wavelength conversion cover layers, and Fig. 15B The transmittance is shown relative to the silicon nitride (SiN) on the wavelength conversion layer. x ) is a graph showing the change in thickness.
[0107] refer to Figure 2 and Fig.15A , which shows the conditions for performing the simulation. The wavelength conversion cover layer 60 may be disposed on the wavelength conversion layer 50. The wavelength conversion cover layer 60 may include a high refractive material, a low refractive material, and a transparent organic material. In an exemplary embodiment, the high refractive material may be silicon nitride (SiN x ), and the low refractive material may be silicon oxide (SiO x The high refractive material will be described below as silicon nitride (SiN x), and the low refractive material will be described below as silicon oxide (SiO x ). Fig.15A OC refers to transparent organic material. The transparent organic material may be silicone, acrylic or epoxy. Each layer including a high refractive material or a low refractive material may have a thickness of 0 to 0.2 μm. The layer including the transparent organic material may have a thickness of 0 to 5 μm. A thickness of 0 μm means that the corresponding layer is not included. According to the laminated structure including the layers of high refractive material, low refractive material and transparent organic material, a total of six conditions may exist. Hereinafter, three conditions showing a fairly high light transmittance will be described below.
[0108] The wavelength conversion cover layer 60 of Case 1 may have a structure in which layers including a high refractive material, a low refractive material, and a transparent organic material are sequentially laminated on the wavelength conversion layer 50 in this order.
[0109] The wavelength conversion cover layer 60 of Case 2 may have a structure in which layers including a high refractive material, a transparent organic material, and a low refractive material are sequentially laminated on the wavelength conversion layer 50 in this order.
[0110] The wavelength conversion cover layer 60 of Case 3 may include a structure in which layers including a transparent organic material, a high refractive material, and a low refractive material are sequentially laminated on the wavelength conversion layer 50 in this order.
[0111] Fig. 15B It is shown in Fig.15A The transmittance in case 2 is relatively higher than that of the silicon nitride (SiN x ) is a graph showing the change in thickness. Fig. 15B is an example of a simulation result, and the transmittance of the wavelength conversion cover layer 60 having a laminated structure of other cases may also be different from Fig. 15B Here, the transmittance represents the ratio of the white light transmitted through the lower wavelength conversion cover layer 60 to the white light incident through the wavelength conversion layer 50. Fig. 15B In the graph, silicon nitride (SiN x ) refers to a high refractive material, and silicon oxide (SiO x ) means a low refractive material.
[0112] refer to Fig. 15B It can be seen that the transmittance of the wavelength conversion cover layer 60 increases with the silicon nitride (SiN x ) thickness. Due to the influence of constructive interference or destructive interference of light, the x ) thickness, so the light transmittance also changes. x) thickness increases, the value of the maximum light transmittance tends to decrease due to the material's absorption of light. x ) is about 0.1 μm, the wavelength conversion cover layer 60 according to Case 2 has the maximum transmittance. Fig.15A Cases 1 to 3 shown change the lamination structure (eg, the lamination sequence and lamination thickness of the wavelength conversion cover layer 60 ) to obtain the maximum transmittance under each lamination condition.
[0113] FIG. 16A to FIG. 16C is a table showing the lamination structure and thickness for ensuring the maximum transmittance in each lamination case of the wavelength conversion cover layer. FIG. 16A to FIG. 16C In , three result values with high transmittance are shown for each lamination case. FIG. 16A to FIG. 16C Silicon nitride (SiN x ) is an example of a high refractive material, and silicon oxide (SiO x ) is an example of a low refractive material. OC refers to a transparent organic material. If the maximum light transmittance in each case is obtained, the wavelength conversion cover layer 60 may have a maximum light transmittance of 87.5% to 88.2%. Now, reference will be made to Figures 17 to 20 The laminated structure of the wavelength conversion cover layer 60 according to various exemplary embodiments is described in detail.
[0114] Figures 17 to 20 2 are cross-sectional views of wavelength conversion cover layers 61 to 64 according to an exemplary embodiment. Figures 17 to 20 5 shows that the elements of the wavelength conversion cover layer can be arranged differently. In order to effectively transmit light and prevent moisture / oxygen from penetrating into the wavelength conversion layer 50, the wavelength conversion cover layers 61 to 64 can each have a multilayer structure in which layers including at least two of a high refractive material, a low refractive material, and a transparent organic material are laminated.
[0115] exist Fig.17 In the embodiment, the wavelength conversion cover layers 61a and 61b are disposed on the wavelength conversion layer 50, and have a multi-layer structure including a first wavelength conversion cover layer 61a and a second wavelength conversion cover layer 61b. Fig.17 The wavelength conversion cover layers 61a and 61b correspond to Fig.16A The structure of result 1 to result 3 in case 1. That is, Fig.17 The wavelength conversion cover layers 61a and 61b may not include a high refractive material and may be a multilayer including a first wavelength conversion cover layer 61a and a second wavelength conversion cover layer 61b having different refractive indices. The refractive index of the first wavelength conversion cover layer 61a may be greater than the refractive index of the second wavelength conversion cover layer 61b. In an exemplary embodiment, the first wavelength conversion cover layer 61a is made of silicon oxide (SiOx ) and has a thickness of 0.1 μm. The second wavelength conversion cover layer 61b is made of a transparent organic material and has a thickness of 2 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 61a and 61b is 87.9%. The wavelength conversion cover layers 61a and 61b according to the exemplary embodiment are the same as the wavelength conversion cover layers 61a and 61b of the exemplary embodiment described above in terms of laminated materials, but the thickness of each layer is different. The thickness of the first wavelength conversion cover layer 61a is 0.1 μm. The thickness of the second wavelength conversion cover layer 61b is 3.5 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 61a and 61b is 87.7%. The wavelength conversion cover layers 61a and 61b according to the exemplary embodiment are the same as the wavelength conversion cover layers 61a and 61b of the exemplary embodiment described above in terms of laminated materials, but the thickness of each layer is different. The thickness of the first wavelength conversion cover layer 61a is 0.1 μm. The thickness of the second wavelength conversion cover layer 61b is 4.5 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 61 a and 61 b is 87.5%.
[0116] exist Fig.18 , the wavelength conversion cover layers 62a and 62b are disposed on the wavelength conversion layer 50, and have a multi-layer structure including a first wavelength conversion cover layer 62a and a second wavelength conversion cover layer 62b. Fig.18 The wavelength conversion covering layers 62a and 62b are with Fig. 16B The structure of results 1 to 3 in case 2 corresponds to that of the previous case. That is, Fig.18 The wavelength conversion cover layers 62a and 62b may not include a transparent organic material, and may be a multilayer including a first wavelength conversion cover layer 62a and a second wavelength conversion cover layer 62b having different refractive indices. The refractive index of the first wavelength conversion cover layer 62a may be greater than the refractive index of the second wavelength conversion cover layer 62b. In an exemplary embodiment, the first wavelength conversion cover layer 62a is made of silicon nitride (SiN x ) and has a thickness of 0.1 μm. The second wavelength conversion cover layer 62b is made of silicon oxide (SiO x) and has a thickness of 0.05 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 62a and 62b is 88.2%. The wavelength conversion cover layers 62a and 62b according to the exemplary embodiment are the same as the wavelength conversion cover layers 62a and 62b of the exemplary embodiment described above in terms of laminated materials, but the thickness of each layer is different. The thickness of the first wavelength conversion cover layer 62a is 0.1 μm. The thickness of the second wavelength conversion cover layer 62b is 0.2 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 62a and 62b is 87.9%. The wavelength conversion cover layers 62a and 62b according to the exemplary embodiment are the same as the wavelength conversion cover layers 62a and 62b of the exemplary embodiment described above in terms of laminated materials, but the thickness of each layer is different. The thickness of the first wavelength conversion cover layer 62a is 0.1 μm. The thickness of the second wavelength conversion cover layer 62b is 0.35 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 62a and 62b is 87.7%.
[0117] exist Fig.19 , the wavelength conversion cover layers 63a and 63b are disposed on the wavelength conversion layer 50, and have a multilayer structure including a first wavelength conversion cover layer 63a and a second wavelength conversion cover layer 63b. Fig.19 The wavelength conversion covering layers 63a and 63b correspond to Fig. 16C The result of case 3 in the structure of 1. That is, Fig.19 The wavelength conversion cover layers 63a and 63b may not include a low refractive material and may be a multilayer including a first wavelength conversion cover layer 63a and a second wavelength conversion cover layer 63b having different refractive indices. The refractive index of the first wavelength conversion cover layer 63a may be less than the refractive index of the second wavelength conversion cover layer 63b. In an exemplary embodiment, the first wavelength conversion cover layer 63a is made of a transparent organic material and has a thickness of 1 μm. The second wavelength conversion cover layer 63b is made of silicon nitride (SiN x ) and has a thickness of 0.05 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 63a and 63b is 88.2%.
[0118] exist Fig. 20 , the wavelength conversion cover layers 64a, 64b, and 64c are disposed on the wavelength conversion layer 50, and have a multilayer structure including a first wavelength conversion cover layer 64a, a second wavelength conversion cover layer 64b, and a third wavelength conversion cover layer 64c. Fig. 20 The wavelength conversion covering layers 64a, 64b and 64c correspond to Fig. 16C The structure of result 2 and result 3 in case 3. That is, Fig. 20The wavelength conversion cover layers 64a, 64b, and 64c may be a multilayer including a first wavelength conversion cover layer 64a, a second wavelength conversion cover layer 64b, and a third wavelength conversion cover layer 64c having different refractive indices. The refractive index of the first wavelength conversion cover layer 64a may be the smallest, and the refractive index of the second wavelength conversion cover layer 64b may be the largest. The refractive index of the third wavelength conversion cover layer 64c may be greater than the refractive index of the first wavelength conversion cover layer 64a and less than the refractive index of the second wavelength conversion cover layer 64b. In an exemplary embodiment, the first wavelength conversion cover layer 64a is made of a transparent organic material and has a thickness of 1 μm. The second wavelength conversion cover layer 64b is made of silicon nitride (SiN x ) and has a thickness of 0.05 μm. The third wavelength conversion cover layer 64c is made of silicon oxide (SiO x ) and has a thickness of 0.05 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 64a, 64b and 64c is 88.2%. The wavelength conversion cover layers 64a, 64b and 64c according to the exemplary embodiment are the same as the wavelength conversion cover layers 64a, 64b and 64c of the exemplary embodiment described above in terms of laminated materials, but the thickness of each layer is different. The thickness of the first wavelength conversion cover layer 64a is 1 μm. The thickness of the second wavelength conversion cover layer 64b is 0.05 μm. The thickness of the third wavelength conversion cover layer 64c is 0.3 μm. Therefore, the white light transmittance of the wavelength conversion cover layers 64a, 64b and 64c is 88.2%.
[0119] Figure 21 to Figure 23 101 to 103 are cross-sectional views of optical members 101 to 103 according to example embodiments. Figure 21 to Figure 23 The optical member 101 shows that the wavelength conversion bottom layer 70 and the wavelength conversion cover layer 60 described above can be combined in various ways. Figures 7 to 14 The structures of the eight wavelength conversion substrates 71 to 78 described above and the Fig.17 and Fig. 20 The structures of the four wavelength conversion cover layers 61 to 64 described above can be combined according to an exemplary embodiment to produce 32 optical components (101, 102, 103). However, the laminated structure of the optical components is not limited to the above example, and various other laminated structures can be applied. In the optical component according to the exemplary embodiment, the above reference Figures 7 to 14 The wavelength conversion bottom layers 71 to 78 described above can be divided into a wavelength conversion bottom layer 74 that does not include the low-refractive bottom layer 20, a wavelength conversion bottom layer 78 that does not include the low-refractive cover layer 40, and wavelength conversion bottom layers 71, 72, 73, 75, 76, and 77 that include both the low-refractive bottom layer and the low-refractive cover layer. The wavelength conversion cover layer 60 can be the wavelength conversion bottom layer 74 of the above reference. Fig.17 and Fig. 20Any of the four wavelength conversion cover layers 61 to 64 described.
[0120] The final light transmittance of optical member 100 may be obtained by multiplying the blue light transmittance of wavelength conversion underlayer 70 by the white light transmittance of wavelength conversion cover layer 60 .
[0121] refer to Fig.21 According to the exemplary embodiment, the optical member 101 may include a wavelength conversion bottom layer 70 and a wavelength conversion cover layer 60a. The wavelength conversion bottom layer 70 may include a low-refractive layer 30 and a low-refractive cover layer 40a, but may not include a low-refractive bottom layer. The wavelength conversion bottom layer 70 may be Fig.10 That is, the wavelength conversion bottom layer 70 may be a wavelength conversion bottom layer that does not include a low refractive bottom layer and includes a low refractive cover layer 40a having a multi-layer structure. The wavelength conversion cover layer 60a may have a multi-layer structure in which layers including inorganic or organic materials are laminated.
[0122] refer to Fig. 22 According to an exemplary embodiment, the optical member 102 may include a wavelength conversion bottom layer 70 and a wavelength conversion cover layer 60b. The wavelength conversion bottom layer 70 may include a low-refractive bottom layer 20b and a low-refractive layer 30, but may not include a low-refractive cover layer. The wavelength conversion bottom layer 70 may be Fig.14 That is, the wavelength conversion bottom layer 70 may be a wavelength conversion bottom layer that does not include a low-refractive cover layer and includes a low-refractive bottom layer 20b having a multi-layer structure. The wavelength conversion cover layer 60b may have a multi-layer structure in which layers including inorganic materials or organic materials are laminated.
[0123] refer to Fig.23 According to the exemplary embodiment, the optical member 103 may include a wavelength conversion bottom layer 70 and a wavelength conversion cover layer 60c. The wavelength conversion bottom layer 70 may include a low-refractive bottom layer 20c, a low-refractive layer 30, and a low-refractive cover layer 40c. The wavelength conversion bottom layer 70 may be the above reference Figures 7 to 14 The wavelength conversion substrates 71 to 78 described herein are Fig.10 and Fig.14 Any one of the wavelength conversion bottom layers 71, 72, 73, 75, 76, and 77 according to the exemplary embodiment other than the wavelength conversion bottom layers 74 and 78 of the present invention. That is, the wavelength conversion bottom layer 70 may include a low-refractive bottom layer 20c having a single-layer structure or a multi-layer structure, and a low-refractive cover layer 40c having a single-layer structure or a multi-layer structure. The wavelength conversion cover layer 60c may be a multi-layer structure in which layers including inorganic materials or organic materials are laminated.
[0124] Fig.24is a cross-sectional view of a display 1000 according to an exemplary embodiment.
[0125] refer to Fig.24 The display 1000 includes a light source 400 , an optical member 100 disposed on a light emitting path of the light source 400 , and a display panel 300 disposed above the optical member 100 .
[0126] All of the optical members according to the above-described exemplary embodiments may be used as the optical member 100. Fig.24 , the display 1000 will be described as including Figure 2 The optical member 100 is taken as an example.
[0127] The light source 400 is disposed on a side of the optical member 100. The light source 400 may be disposed adjacent to the light incident surface 10S1 of the light guide plate 10 of the optical member 100. The light source 400 may include a plurality of point light sources or line light sources. The point light sources may be LED light sources 410. The LED light source 410 may be mounted on a printed circuit board 420. The LED light source 410 may emit light of a blue wavelength.
[0128] like Fig.24 As shown, the LED light source 410 may be a top-emitting LED that emits light through its top surface. In this case, the printed circuit board 420 may be disposed on the side wall 520 of the housing 500.
[0129] The blue wavelength light emitted from the LED light source 410 is incident on the light guide plate 10 of the optical member 100. The light guide plate 10 of the optical member 100 guides the light and outputs the light through the upper surface 10a or the lower surface 10b. The wavelength conversion layer 50 of the optical member 100 converts a portion of the blue wavelength light incident from the light guide plate 10 into other wavelengths, such as green wavelength and red wavelength light. The green wavelength light and the red wavelength light are emitted upward toward the display panel 300 together with the unconverted blue wavelength light.
[0130] The diffusion pattern 80 may be disposed on the lower surface 10b of the light guide plate 10. The diffusion pattern 80 changes the angle of light propagating in the light guide plate 10 through total reflection and outputs the light having the changed angle to the outside of the light guide plate 10.
[0131] In an exemplary embodiment, the scattering pattern 80 may be provided as a separate layer or a separate pattern. For example, a pattern layer including a protruding pattern and / or a groove pattern may be formed on the lower surface 10 b of the light guide plate 10, or a printed pattern may be formed on the lower surface 10 b of the light guide plate 10 to serve as the scattering pattern 80.
[0132] In an exemplary embodiment, the diffusion pattern 80 may be formed by the surface shape of the light guide plate 10 itself. For example, a groove may be formed on the lower surface 10 b of the light guide plate 10 to serve as the diffusion pattern 80 .
[0133] The arrangement density of the scattering pattern 80 may be different depending on the region. For example, in a region adjacent to the light incident surface 10S1 provided with a relatively large amount of light, the arrangement density of the scattering pattern 80 may be low, and in a region adjacent to the opposite surface 10S3 provided with a relatively small amount of light, the arrangement density of the scattering pattern 80 may be high.
[0134] The display 1000 may further include a reflective member 90 disposed below the optical member 100. The reflective member 90 may include a reflective film or a reflective coating. The reflective member 90 reflects light output from the lower surface 10b of the light guide plate 10 of the optical member 100 back into the light guide plate 10.
[0135] The display panel 300 is disposed above the optical member 100. The display panel 300 receives light from the optical member 100 and displays a screen. Examples of such a light-receiving display panel that receives light and displays a screen include a liquid crystal display panel and an electrophoretic panel. Hereinafter, the display panel 300 will be described as including a liquid crystal display panel, but the inventive concept is not limited thereto, and various other light-receiving display panels may be applied as the display panel 300.
[0136] The display panel 300 may include a first substrate 310, a second substrate 320 facing the first substrate 310, and a liquid crystal layer disposed between the first substrate 310 and the second substrate 320. The first substrate 310 and the second substrate 320 overlap each other. In an exemplary embodiment, any one of the first substrate 310 and the second substrate 320 may be larger than the other substrate and protrude more outward than the other substrate. Fig.24 It is shown that the second substrate 320 disposed on the first substrate 310 is larger and protrudes on the side where the light source 400 is disposed. The protruding area of the second substrate 320 can provide a space for mounting a driving chip or an external circuit board. Unlike the above example, the size of the first substrate 310 disposed below the second substrate 320 can be larger than the second substrate 320 and can protrude outward. The overlapping area of the first substrate 310 and the second substrate 320 except for the protruding area in the display panel 300 can be substantially aligned with the side surface 10S of the light guide plate 10 of the optical member 100.
[0137] The optical member 100 may be coupled to the display panel 300 through an inter-module coupling member 610. The inter-module coupling member 610 may be shaped like a quadrangular frame in a plan view. The inter-module coupling member 610 may be located at edge portions of the display panel 300 and the optical member 100.
[0138] In an exemplary embodiment, the lower surface of the inter-module coupling member 610 is disposed on the upper surface of the wavelength conversion cover layer 60 of the optical member 100. The lower surface of the inter-module coupling member 610 may be disposed on the wavelength conversion cover layer 60 to overlap only the upper surface of the wavelength conversion layer 50 and not overlap the side surface of the wavelength conversion layer 50.
[0139] The inter-module coupling member 610 may include a polymer resin or an adhesive or a tape.
[0140] In an exemplary embodiment, the inter-module coupling member 610 may also perform a light transmission blocking function. For example, the inter-module coupling member 610 may include a light absorbing material such as a black pigment or dye, or may include a reflective material to perform a light transmission blocking function.
[0141] The display 1000 may further include a housing 500. The housing 500 has an open surface and includes a bottom surface 510 and a side wall 520 connected to the bottom surface 510. The light source 400, the optical member 100 and the display panel 300 attached to each other, and the reflective member 90 may be accommodated in a space defined by the bottom surface 510 and the side wall 520. The light source 400, the reflective member 90, and the optical member 100 and the display panel 300 attached to each other are disposed on the bottom surface 510 of the housing 500. The height of the side wall 520 of the housing 500 may be substantially the same as the height of the optical member 100 and the display panel 300 attached to each other inside the housing 500. The display panel 300 may be disposed adjacent to the upper end of each side wall 520 of the housing 500, and may be coupled to the upper end of each side wall 520 of the housing 500 by a housing coupling member 620. The housing coupling member 620 may be shaped like a quadrilateral frame in a plan view. The housing coupling member 620 may include a polymer resin or an adhesive or a tape.
[0142] The display 1000 may further include at least one optical film 200. One or more optical films 200 may be accommodated in a space surrounded by the inter-module coupling member 610 between the optical member 100 and the display panel 300. The side surfaces of the one or more optical films 200 may contact and be attached to the inner side surface of the inter-module coupling member 610. Although Fig.24 It is shown that there is a gap between the optical film 200 and the optical member 100 , and there is a gap between the optical film 200 and the display panel 300 , but the gap is not necessary and may be omitted.
[0143] The optical film 200 may be a prism film, a diffusion film, a microlens film, a lenticular film, a polarizing film, a reflective polarizing film, or a delay film. The display 1000 may include a plurality of optical films 200 of the same type or different types. When a plurality of optical films 200 are applied, the optical films 200 may be placed to overlap each other, and the side surfaces of the optical films 200 may contact and be attached to the inner side surfaces of the inter-module coupling member 610. The optical films 200 may be separated from each other, and an air layer may be provided between the optical films 200.
[0144] In accordance with Fig.24 In the display 1000 of the exemplary embodiment of the present invention, the optical member 100 and the display panel 300 and further the optical film 200 are integrated with each other by the inter-module coupling member 610, and the display panel 300 and the housing 500 are coupled to each other by the housing coupling member 620. Therefore, even if the mold frame is omitted, various members can be stably coupled, thereby reducing the weight of the display 1000. In addition, since the light guide plate 10 and the wavelength conversion layer 50 are integrated with each other, the thickness of the display 1000 can be reduced. In addition, since the side surface of the display panel 300 is coupled to the side wall 520 of the housing 500 by the housing coupling member 620, the frame space on the side of the display screen can be eliminated or minimized.
[0145] Fig.25 is a cross-sectional view of a display 1001 according to an exemplary embodiment.
[0146] refer to Fig.25 The display 1001 includes a light source 400, an optical member 100_1 disposed on an emission path of the light source 400, and a display panel 300 disposed above the optical member 100_1. Fig.24 The display is 1000 different, in Fig.25 The display 1001 shown in FIG. 1 includes an optical member 100_1 in which a wavelength conversion cover layer 60_1 covers the upper surface and side surfaces of a wavelength conversion layer 50_1 and the side surfaces of a wavelength conversion bottom layer 70_1.
[0147] The wavelength conversion layer 50_1 (particularly the wavelength conversion particles included in the wavelength conversion layer 50_1) is susceptible to moisture / oxygen. In the case of a wavelength conversion film, a barrier film is laminated on the upper and lower surfaces of the wavelength conversion layer to prevent moisture / oxygen from penetrating into the wavelength conversion layer. However, in the exemplary embodiment shown, since the wavelength conversion layer 50_1 is directly provided without a barrier film, a sealing structure for protecting the wavelength conversion layer 50_1 is required. The sealing structure can be implemented by the wavelength conversion cover layer 60_1 and the light guide plate 10_1.
[0148] The inlets and outlets through which moisture can penetrate into the wavelength conversion layer 50_1 are the upper surface, side surface and lower surface of the wavelength conversion layer 50_1. As described above, since the upper surface and side surface of the wavelength conversion layer 50_1 are covered and protected by the wavelength conversion cover layer 60_1, the penetration of moisture / oxygen can be prevented or at least reduced.
[0149] On the other hand, the lower surface of the wavelength conversion layer 50_1 is in contact with the upper surface of the wavelength conversion bottom layer 70_1. If the wavelength conversion bottom layer 70_1 includes a void VD or is made of an organic material, the movement of moisture in the wavelength conversion bottom layer 70_1 is possible. Therefore, moisture / oxygen may be introduced into the lower surface of the wavelength conversion layer 50_1 through the wavelength conversion bottom layer 70_1. However, since the wavelength conversion bottom layer 70_1 according to the exemplary embodiment also has a sealing structure, moisture / oxygen may be blocked from penetrating through the lower surface of the wavelength conversion layer 50_1 at the source.
[0150] Specifically, since the side surface of the wavelength conversion bottom layer 70_1 is covered and protected by the wavelength conversion cover layer 60_1, the penetration of moisture / oxygen through the side surface of the wavelength conversion bottom layer 70_1 can be blocked / reduced. Even if the wavelength conversion bottom layer 70_1 is more protruding than the wavelength conversion layer 50_1 so that a part of the upper surface is exposed, since the exposed part is covered and protected by the wavelength conversion cover layer 60_1, the penetration of moisture / oxygen through the exposed part can be blocked / reduced. The lower surface of the wavelength conversion bottom layer 70_1 is in contact with the light guide plate 10_1. When the light guide plate 10_1 is made of an inorganic material such as glass, it can block / reduced the penetration of moisture / oxygen like the wavelength conversion cover layer 60_1. That is, since the laminated surface of the wavelength conversion bottom layer 70_1 and the wavelength conversion layer 50_1 is surrounded and sealed by the wavelength conversion cover layer 60_1 and the light guide plate 10_1, even if a moisture / oxygen movement path is formed inside the wavelength conversion bottom layer 70_1, the penetration of moisture / oxygen can be blocked / reduced by the above-mentioned sealing structure. Thus, degradation of the wavelength converting particles due to moisture / oxygen may be prevented or at least mitigated.
[0151] The optical member according to the exemplary embodiment can simultaneously perform light guiding functions and wavelength conversion functions while improving light transmission efficiency through materials having a laminated structure with different refractive indices. The optical member according to the exemplary embodiment is relatively thin and can improve optical characteristics of a display by maximizing light transmission efficiency.
[0152] Although certain exemplary embodiments and implementations have been described herein, other implementations and modifications will be apparent from this description. Therefore, the inventive concept is not limited to these implementations, but to the broader scope of the appended claims and various obvious modifications and equivalent arrangements that will be apparent to those of ordinary skill in the art.
Claims
1. An optical component having a plurality of include: Light guide plate; A low-refractive bottom layer, which is arranged on the light guide plate; a low-refractive layer disposed on the low-refractive base layer and having a refractive index less than that of the light guide plate; and a wavelength conversion layer, which is disposed on the low refractive layer, wherein the low-refractive bottom layer has a thickness smaller than that of the low-refractive layer, wherein the low refractive layer comprises voids, The low-refractive bottom layer comprises a first low-refractive bottom layer arranged on the light guide plate and a second low-refractive bottom layer arranged on the first low-refractive bottom layer, and The refractive index of the low-refractive bottom layer is greater than the refractive index of the low-refractive layer.
2. The optical component according to claim 1, in: The lower surface of the low-refractive bottom layer contacts the upper surface of the light guide plate; and An upper surface of the low-refractive base layer contacts a lower surface of the low-refractive layer. 3 . The optical member according to claim 2 , wherein the low-refractive base layer comprises a low-refractive material having a refractive index of 1.3 to 1.7 and a high-refractive material having a refractive index of 1.5 to 2.
2. 4 . The optical member according to claim 3 , wherein one of the first low-refractive primer layer and the second low-refractive primer layer includes the low-refractive material, and the other of the first low-refractive primer layer and the second low-refractive primer layer includes the high-refractive material. 5 . The optical member according to claim 4 , wherein each of the first low-refractive primer layer and the second low-refractive primer layer has a thickness of 0.2 μm or less. The optical member according to claim 4 , wherein the low-refractive material comprises silicon oxide, and the high-refractive material comprises silicon nitride. 7 . The optical member according to claim 1 , wherein a difference in refractive index between the light guide plate and the low-refractive layer is 0.2 or more. The optical member according to claim 7 , wherein the refractive index of the low-refractive layer is 1.2 to 1.
3. 9 . The optical member according to claim 8 , wherein the low refractive layer has a thickness of 0.8 μm to 1.2 μm. 10 . The optical member of claim 1 , further comprising a wavelength conversion cover layer disposed on the wavelength conversion layer. The optical member according to claim 10 , wherein a lower surface of the wavelength conversion cover layer is parallel to an upper surface of the light guide plate. 12 . The optical component of claim 11 , wherein the wavelength conversion capping layer comprises at least one of silicon oxide and silicon nitride.
13. The optical component of claim 12, wherein the wavelength conversion cover layer include: a first wavelength conversion cover layer disposed on the wavelength conversion layer; and A second wavelength conversion cover layer is disposed on the first wavelength conversion cover layer. 14 . The optical member of claim 13 , wherein one of the first wavelength conversion cover layer and the second wavelength conversion cover layer comprises a transparent organic material, and the other of the first wavelength conversion cover layer and the second wavelength conversion cover layer comprises at least one of silicon oxide and silicon nitride.
15. The optical component according to claim 14, in: The first wavelength conversion capping layer comprises silicon oxide; and The second wavelength conversion cover layer includes a transparent organic material. 16 . The optical member of claim 13 , wherein one of the first wavelength conversion cover layer and the second wavelength conversion cover layer comprises silicon oxide, and the other of the first wavelength conversion cover layer and the second wavelength conversion cover layer comprises silicon nitride. 17 . The optical component of claim 13 , wherein the wavelength conversion cover layer further comprises a third wavelength conversion cover layer disposed on the second wavelength conversion cover layer.
18. The optical component of claim 17, wherein the first wavelength converting cover layer comprises a transparent organic material. 19 . The optical component of claim 18 , wherein one of the second wavelength conversion cover layer and the third wavelength conversion cover layer comprises silicon oxide, and the other of the second wavelength conversion cover layer and the third wavelength conversion cover layer comprises silicon nitride.
20. The optical member of claim 1, wherein the light guide plate comprises glass. The optical member according to claim 20 , wherein an upper surface of the light guide plate is parallel to a lower surface of the low-refractive layer.
22. An optical component, wherein include: Light guide plate; A low-refractive bottom layer, which is arranged on the light guide plate; a low-refractive layer disposed on the low-refractive base layer and having a refractive index less than that of the light guide plate; a low-refractive covering layer, which is disposed on the low-refractive layer; and a wavelength conversion layer, which is arranged on the low-refractive cover layer, wherein the low refractive layer comprises voids, The low-refractive bottom layer comprises a first low-refractive bottom layer arranged on the light guide plate and a second low-refractive bottom layer arranged on the first low-refractive bottom layer, and The refractive index of the low-refractive bottom layer is greater than the refractive index of the low-refractive layer.
23. The optical component according to claim 22, in: The low-refractive bottom layer includes silicon oxide and silicon nitride. 24 . The optical member according to claim 23 , wherein each of the first low-refractive primer layer and the second low-refractive primer layer has a thickness of 0.2 μm or less.
25. The optical component according to claim 22, in: The low-refractive cover layer includes at least one of silicon oxide and silicon nitride; and The refractive index of the low-refractive cover layer is greater than the refractive index of the low-refractive layer.
26. The optical component according to claim 25, wherein the low refractive cover layer include: a first low-refractive covering layer disposed on the low-refractive layer; and A second low-refractive covering layer is disposed on the first low-refractive covering layer. 27 . The optical member according to claim 26 , wherein each of the first low-refractive cover layer and the second low-refractive cover layer has a thickness of 0.2 μm or less.
28. The optical component of claim 22, further comprising a wavelength conversion cover layer disposed on the wavelength conversion layer, The wavelength conversion cover layer includes at least one of silicon oxide and silicon nitride.
29. The optical component of claim 28, wherein the wavelength conversion cover layer include: a first wavelength conversion cover layer disposed on the wavelength conversion layer; and A second wavelength conversion cover layer is disposed on the first wavelength conversion cover layer.
30. The optical member of claim 29, wherein one of the first wavelength conversion cover layer and the second wavelength conversion cover layer comprises a transparent organic material and the other of the first wavelength conversion cover layer and the second wavelength conversion cover layer comprises at least one of silicon oxide and silicon nitride.
31. The optical component according to claim 30, in: The first wavelength conversion capping layer comprises silicon oxide; and The second wavelength conversion cover layer includes a transparent organic material.
32. The optical component of claim 29, wherein the wavelength conversion cover further comprises a third wavelength conversion cover disposed on the second wavelength conversion cover.
33. A display, include: An optical member, which includes a light guide plate in sequence in the traveling direction of light; A low-refractive bottom layer, which is arranged on the light guide plate; a low-refractive layer disposed on the low-refractive base layer and having a refractive index less than that of the light guide plate; and a wavelength conversion layer disposed on the low refractive layer; a light source for emitting the light, which is disposed on at least one side of the light guide plate; and A display panel is disposed on the optical member, wherein the low refractive layer comprises voids, The low-refractive bottom layer comprises a first low-refractive bottom layer arranged on the light guide plate and a second low-refractive bottom layer arranged on the first low-refractive bottom layer, and The refractive index of the low-refractive bottom layer is greater than the refractive index of the low-refractive layer.
34. The display according to claim 33, in: The low-refractive bottom layer includes silicon oxide and silicon nitride.
35. The display of claim 33, further comprising a wavelength converting cover layer disposed on the wavelength converting layer, The wavelength conversion cover layer includes at least one of silicon oxide and silicon nitride.
36. The display according to claim 35, in: The wavelength conversion cover layer comprises: a first wavelength conversion cover layer disposed on the wavelength conversion layer; and A second wavelength conversion cover layer is disposed on the first wavelength conversion cover layer.
37. The display of claim 36, wherein the wavelength converting cover layer further comprises a third wavelength converting cover layer disposed on the second wavelength converting cover layer.
38. The display of claim 33, wherein the optical member further comprises a low-refractive cover layer disposed between the low-refractive layer and the wavelength conversion layer.
39. The display according to claim 38, in: The low-refractive cover layer includes at least one of silicon oxide and silicon nitride; and The refractive index of the low-refractive covering layer is greater than the refractive index of the low-refractive layer.
40. The display of claim 39, further comprising a wavelength converting cover layer disposed on the wavelength converting layer, The wavelength conversion cover layer includes at least one of silicon oxide and silicon nitride.