Semiconductor structure forming method and semiconductor structure
By forming an interface layer and a high-k dielectric layer in the semiconductor structure, and using a metal gate electrode to replace the dummy gate electrode, the problem of difficulty in forming the conductive layer in HKMG is solved, the component performance and reliability are improved, and the contact resistance is reduced .
Patent Information
- Application Number
- CN201811183706.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-10-11
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2039-03-01
AI Technical Summary
In high-k metal gates (HKMG), as the feature size decreases, there are challenges in forming multiple conductive layers. Especially when the gate length is shortened, existing methods are difficult to effectively improve device performance.
By forming an interface layer and a high-k dielectric layer on the semiconductor layer, creating a dummy gate electrode on it, forming spacers after patterning, and then replacing the dummy gate electrode with a metal gate electrode, adding a silicide layer and contact insertion Plug, using a sharp wave annealing process to expand the processing window and improve component performance.
This increases the processing window for forming multiple conductive layers in HKMG, expanding the contact area between the suicide layer and the source/drain features, improving device performance and reliability, and reducing contact resistance.
Smart Images

Figure CN110610989B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a semiconductor structure forming method and a semiconductor structure. Background Art
[0002] The semiconductor integrated circuit (IC) industry has experienced quite rapid growth. Advances in integrated circuit materials and design techniques have resulted in generations of integrated circuits, each with smaller and more complex circuits than the previous generation. In the course of integrated circuit evolution, functional density (i.e., the number of interconnected elements per unit chip area) has generally increased, while geometry size (i.e., the smallest component (or line) that a process can produce) has shrunk. This shrinking process generally provides the benefits of increased production efficiency and lower associated costs, but also increases the complexity of processing and manufacturing integrated circuits.
[0003] For example, device performance can be improved by replacing a polysilicon gate with a high-k metal gate structure (HKMG). Although existing methods are generally adequate, implementing such methods remains challenging, particularly with respect to forming multiple conductive layers in a HKMG structure as feature dimensions (e.g., gate length) continue to decrease. Summary of the invention
[0004] According to some embodiments of the present disclosure, a method for forming a semiconductor structure includes: providing a semiconductor layer; forming an interface layer above the semiconductor layer; depositing a high-k dielectric layer above the interface layer; forming a dummy gate electrode above the high-k dielectric layer; patterning the dummy gate electrode, the high-k dielectric layer and the interface layer so that the width of the interface layer is greater than the width of the high-k dielectric layer; after patterning, forming spacers along the sidewalls of the dummy gate electrode, the high-k dielectric layer and the interface layer; forming a plurality of source / drain features above the semiconductor layer; replacing the dummy gate electrode with a metal gate electrode to form a high-k metal gate structure; depositing a capping layer above the high-k dielectric layer after depositing the high-k dielectric layer and before forming the dummy gate electrode; performing a spike annealing process on the capping layer in a nitrogen environment; and removing the capping layer before replacing the dummy gate electrode.
[0005] According to some embodiments of the present disclosure, a method for forming a semiconductor structure includes: providing a semiconductor layer; forming an interface layer above the semiconductor layer; depositing a high-k dielectric layer above the interface layer; forming a dummy gate electrode above the high-k dielectric layer; patterning the dummy gate electrode, the high-k dielectric layer and the interface layer so that the width of the interface layer is greater than the width of the high-k dielectric layer; after patterning, forming spacers along the sidewalls of the dummy gate electrode, the high-k dielectric layer and the interface layer; forming a plurality of source / drain features above the semiconductor layer; replacing the dummy gate electrode with a metal gate electrode to form a high-k metal gate structure; depositing a capping layer above the high-k dielectric layer after depositing the high-k dielectric layer and before forming the dummy gate electrode; depositing a silicon-containing capping layer above the capping layer before forming the dummy gate electrode; performing a spike annealing process on the silicon-containing capping layer; and removing the silicon-containing capping layer.
[0006] According to some embodiments of the present disclosure, a semiconductor structure includes a high-k metal gate structure, a gate spacer, a plurality of source / drain features, and a contact plug. The high-k metal gate structure is disposed above a channel region of a semiconductor layer, and the semiconductor layer is disposed above a substrate. The high-k metal gate structure includes an interface layer, a high-k dielectric layer, and an electrode. The interface layer is disposed above the semiconductor layer and has a first length along a first direction. The high-k dielectric layer is disposed above the interface layer and has a second length along the first direction, and the second length is less than the first length. The electrode is disposed above the high-k dielectric layer and has a third length along the first direction, and the second length is greater than the third length. The distance between the outer edge of the electrode and the outer edge of the high-k dielectric layer is less than the distance between the outer edge of the electrode and the outer edge of the interface layer. The gate spacer is disposed along the sidewall of the electrode, and the bottom of the gate spacer contacts the top surface of the high-k dielectric layer. The source / drain features are disposed in the semiconductor layer and are located on opposite sides of the high-k metal gate structure. Contact plugs are disposed over the source / drain features.
[0007] According to some embodiments of the present disclosure, a method for forming a semiconductor structure includes: forming an interface layer above a semiconductor layer; depositing a high-k dielectric layer above the interface layer; forming a dummy gate electrode above the high-k dielectric layer; patterning the dummy gate electrode, the high-k dielectric layer, and the interface layer so that the interface layer extends laterally beyond the outer edge of the high-k dielectric layer, and the high-k dielectric layer extends laterally beyond the outer edge of the dummy gate electrode; forming spacers along the sidewalls of the patterned dummy gate electrode, the high-k dielectric layer, and the interface layer; forming a plurality of source / drain features adjacent to the spacers; and replacing the dummy gate electrode with a metal gate electrode.
[0008] According to some embodiments of the present disclosure, a method for forming a semiconductor structure includes: forming an interface layer above a fin, the fin extending along a first direction; depositing a high-k dielectric layer above the interface layer; depositing a polysilicon layer above the high-k dielectric layer, the polysilicon layer extending along a second direction, the second direction being substantially perpendicular to the first direction; patterning the polysilicon layer, the high-k dielectric layer, and the interface layer so that the interface layer partially extends beyond an outer edge of the high-k dielectric layer in the first direction; forming a gate spacer on a sidewall of the polysilicon layer, wherein the gate spacer is partially formed above a portion of the interface layer extending beyond an outer edge of the high-k dielectric layer; forming a plurality of source / drain features in the fin; forming a silicide layer above the source / drain features, the silicide layer covering a portion of the source / drain features; removing the polysilicon layer to form a trench; and forming a metal gate in the trench.
[0009] According to some embodiments of the present disclosure, a semiconductor structure includes a high-k metal gate structure, a gate spacer, and a plurality of source / drain features. The high-k metal gate structure is disposed above a channel region of a semiconductor layer, and the semiconductor layer is formed above a substrate. The high-k metal gate structure includes an interface layer, a high-k dielectric layer, and a gate electrode. The interface layer is disposed above the semiconductor layer and has a first length along a first direction. The high-k dielectric layer is disposed above the interface layer and has a second length along the first direction, and the second length is less than the first length. The gate electrode is disposed above the high-k dielectric layer and has a third length along the first direction, and the second length is greater than the third length. The outer edges of the interface layer, the high-k dielectric layer, and the gate electrode form a step profile. The gate spacer has a sidewall portion that contacts the sidewall of the gate electrode and a bottom portion that contacts the top of the high-k dielectric layer and the interface layer. The source / drain features are disposed in the semiconductor layer and are adjacent to the high-k metal gate structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] The present disclosure can be best understood when the following detailed description is read in conjunction with the accompanying drawings. It should be emphasized that, in accordance with standard practice in the industry, many features are not drawn to scale and are only used for illustrative purposes. In fact, the size of each feature may be arbitrarily increased or decreased for clarity of description.
[0011] Figure 1A as well as Figure 1B A cross-sectional view of a semiconductor structure in an XZ plane is shown according to one or more embodiments of the present disclosure;
[0012] Figure 1C According to one or more embodiments of the present disclosure, Figure 1A A top view of the semiconductor structure shown in the XY plane;
[0013] Figure 1DAccording to one or more embodiments of the present disclosure, Figure 1C A perspective view of the semiconductor structure shown;
[0014] Figure 1E According to one or more embodiments of the present disclosure, Figure 1A A cross-sectional view of the semiconductor structure shown in the YZ plane;
[0015] Figure 2A as well as Figure 2B A flow chart of a method for forming a semiconductor structure is shown according to one or more embodiments of the present disclosure;
[0016] Figures 3 to 16 According to one or more embodiments of the present disclosure, a semiconductor structure is shown in Figure 2A as well as Figure 2B A cross-sectional view of an intermediate step in a method of forming a semiconductor structure is shown. DETAILED DESCRIPTION
[0017] Many different implementations or embodiments for implementing different features of the present disclosure are provided below. Specific embodiments of components and arrangements are described below to simplify the present disclosure, and these embodiments are of course only examples and are not intended to be limiting. For example, the description below of forming a first feature on or above a second feature may include an implementation in which the first feature is directly in contact with the second feature, and may also include an implementation in which other features are formed between the first feature and the second feature so that the first feature is not in direct contact with the second feature. In addition, the present disclosure may reuse the same component symbols in different embodiments for the purpose of simplicity and clarity, and does not in itself represent the relationship between the various embodiments and / or configurations discussed.
[0018] In addition, the description below about a feature formed on another feature, a feature formed in a manner of being connected and / or coupled to another feature, may include an embodiment in which the above two features are directly contacted, and may also include an embodiment in which other features are formed between the above two features so that the above two features are not directly contacted. In addition, spatially relative terms such as "lower", "upper", "horizontal", "vertical", "above", "above", "below", "below", "up", "down", "top", "bottom" and their derivatives (for example, "horizontally", "downward", "upward", etc.) are used in this disclosure to conveniently express the relationship between one feature and another feature. Spatially relative terms are intended to cover different directions of elements and features. Furthermore, when describing a number or a range of numbers with "about", "approximately" and similar terms, it is intended to cover numbers that fall within a reasonable range that includes the number, such as within + / -10% of the number, or other values understood by those familiar with the art. For example, the term "about 5nm" covers a size range of 4.5nm to 5.5nm.
[0019] The present disclosure relates to semiconductor devices and manufacturing methods, and more particularly to manufacturing high-k metal gates in semiconductor devices.
[0020] As feature sizes continue to decrease, replacing polysilicon gates (or dummy gates) with high-k metal gates (HKMG, where "high-k" refers to dielectric materials with a higher dielectric constant than silicon dioxide) has led to improved device performance. Although methods for implementing HKMG processes are generally adequate, not all aspects are completely satisfactory. For example, there are still challenges in forming multiple conductive layers in HKMG when the gate length is shortened due to the reduction in feature size. In the "later high-k dielectric layer" process, a dummy gate is first formed to reserve a position for the HKMG and then removed after the other components of the device are manufactured, so that the high-k dielectric constant material portion of the HKMG is formed along the sidewalls of the gate trench, reducing the space available for forming the conductive layer. In addition, since the formation of a silicide layer on the source / drain features of the device is generally postponed until after the deposition of the interlayer dielectric layer and the formation of the source / drain contact holes, the size of the silicide layer may be limited. The present disclosure provides a HKMG structure and a method for forming the same, aiming to increase a process window for forming multiple conductive layers in the HKMG and improve device performance by enlarging the contact area between the silicide layer and source / drain features of the device.
[0021] Figure 1A A partial cross-sectional view of a semiconductor device 100 (or device) taken on an XZ plane is shown. Figure 1B To illustrate Figure 1A FIG. 1 is a partial enlarged view of the semiconductor device 100 shown in FIG. Figure 1C A partial top view of a semiconductor device 100 on an XY plane is shown, wherein the semiconductor device 100 includes a fin for forming a fin field effect transistor (FinFET). Figure 1D To illustrate Figure 1C A perspective view of a semiconductor device 100 is shown. Figure 1E FIG. 1 is a partial cross-sectional view of the semiconductor device 100 taken along the YZ plane. Figure 2A as well as Figure 2B A flow chart of an exemplary method 200 for manufacturing the semiconductor device 100 is shown. Figures 3 to 16 To illustrate Figure 1A A cross-sectional view of a semiconductor device 100 in the XZ plane during various steps of fabrication of an embodiment of a method 200 is shown. The semiconductor device 100 may be an intermediate device or a portion thereof fabricated during processing of an integrated circuit, and the semiconductor device 100 may include: static random access memory (SRAM) and / or other logic circuits; passive devices such as resistors, capacitors, and inductors; and active devices such as p-type field effect transistors (PFETs), n-type field effect transistors (NFETs), fin field effect transistors (FinFETs), metal oxide semiconductor field effect transistors (MOSFETs), complementary metal oxide semiconductor (CMOS) transistors, bipolar transistors, high voltage transistors, high frequency transistors, and / or other memory cells. The present disclosure is not limited to any particular number of devices or device regions, or any particular device configuration. For example, the semiconductor device 100 may be a FinFET device having semiconductor fins protruding from a substrate (as shown herein), or alternatively, the semiconductor device 100 may be a planar field effect transistor device.
[0022] Please refer to Figure 1AThe semiconductor device 100 includes a substrate 102, a semiconductor layer 104 (e.g., a semiconductor fin) protruding from the substrate 102, a doped region 108 disposed in the semiconductor layer 104, an isolation structure 106 above the substrate 102 and adjacent to the semiconductor layer 104, a high-k metal gate 120 contacting the semiconductor layer 104 in a channel region, a source / drain feature 110 disposed above the semiconductor layer 104 and located on opposite sides of the high-k metal gate 120, a silicide layer 112 disposed on a surface of the source / drain feature 110, a gate spacer 150 disposed along a sidewall of the high-k metal gate 120, an interlayer dielectric layer 114 disposed above the isolation structure 106 and a plurality of other components of the semiconductor device 100, and a source / drain contact plug 160 (or contact plug) disposed in the interlayer dielectric layer 114 and contacting the source / drain feature 110. In at least one embodiment, the high-k metal gate 120 extends along the Y direction and includes an interface layer 122 disposed above the semiconductor layer 104, a high-k dielectric layer 124 disposed above the interface layer 122, and one or more work function metal layers (e.g., Figure 1A The semiconductor device 100 includes two work function metal layers 142, 144) and a gate electrode 132 of a bulk conductive layer 146. In many embodiments, the semiconductor device 100 includes Figure 1A Each component of semiconductor device 100 is discussed in detail below.
[0023] The substrate 102 may include any suitable semiconductor material, such as silicon; germanium; semiconductor compounds such as silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide and / or indium antimonide; semiconductors such as SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP and / or GaInAsP alloys; other suitable materials or combinations of the above materials.
[0024] The substrate 102 may be a uniform single layer of material, such as a bulk silicon substrate. Alternatively, the substrate 102 may include multiple material layers having similar or different compositions suitable for integrated circuit device manufacturing. For example, the substrate 102 may be a silicon-on-insulator (SOI) substrate having a semiconductor silicon layer formed on a silicon oxide layer.
[0025] Depending on the specific design requirements of the semiconductor device 100, the semiconductor layer 104 can be configured to provide an n-type field effect transistor device or a p-type field effect transistor device. In some embodiments, the semiconductor layer 104 is configured to provide an n-well structure, a p-well structure, or a protrusion structure as shown herein (e.g., an active fin protruding from the substrate 102). The semiconductor layer 104 may include one or more semiconductor materials, such as silicon, germanium, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, indium antimonide, SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, GaInAsPIn, and / or other suitable materials. In some embodiments, the semiconductor layer 104 includes the same material as the substrate 102. In some embodiments, the semiconductor layer 104 includes two different semiconductor material layers stacked alternately, such as alternately stacked silicon layers and SiGe layers. In at least one embodiment, the semiconductor layer 104 includes a doped region 108 (e.g., a lightly doped drain (LDD) region or a source / drain extension region) to improve certain performances of the semiconductor device 100. Depending on the design requirements of the semiconductor device 100, the doped region 108 may be doped with an n-type dopant (e.g., phosphorus or arsenic) or a p-type dopant (e.g., boron or BF2).
[0026] The isolation structure 106 is configured to electrically isolate the semiconductor layer 104 from other active regions, and the isolation structure 106 may include: silicon oxide, silicon nitride, silicon oxynitride, fluoride-doped silicate glass (FSG), low dielectric constant dielectric material, other suitable dielectric materials, or combinations thereof. The isolation structure 106 may be a shallow trench isolation (STI) feature. The isolation structure 106 may further or alternatively include: field oxide, local oxidation of silicon (LOCOS), other suitable structures, or combinations thereof. The isolation structure 106 may be a multi-layer structure, such as a thermal oxide liner layer adjacent to the semiconductor layer 104 and other insulating materials on the liner layer.
[0027] Please refer to Figure 1A as well as Figure 1B. The high-k metal gate 120 contacts the semiconductor layer 104 at a channel region (not shown) between the source / drain features 110. In one embodiment, the high-k metal gate 120 includes a high-k dielectric layer 124 disposed above the semiconductor layer 104 and a gate electrode 132 disposed above the high-k dielectric layer 124, wherein the gate electrode 132 includes a plurality of conductive layers, such as work function metal layers 142, 144 and a bulk conductive layer 146. In one embodiment, the high-k metal gate 120 further includes an interface layer 122 formed between the semiconductor layer 104 and the high-k dielectric layer 124. The high-k metal gate 120 may further include other layers, such as a capping layer, a diffusion layer, a barrier layer, a hard mask layer, other suitable material layers or combinations thereof.
[0028] Please refer to Figure 1B In one embodiment, the interface layer 122 and the high-k dielectric layer 124 are disposed above the semiconductor layer 104, but are not disposed along the sidewalls of the gate spacer 150. On the other hand, the work function metal layer 142 includes a bottom portion disposed above the high-k dielectric layer 124, and a sidewall portion disposed along and directly contacting the gate spacer 150. In one embodiment, the gate electrode 132 is configured to have an inclined sidewall that forms an acute angle 134 (i.e., an angle less than 90 degrees) with a top surface of the high-k dielectric layer 124.
[0029] Please continue to refer to Figure 1B , and refer to Figure 1C as well as Figure 1D The outer edges of the high-k dielectric layer 124 and the interface layer 122 extend beyond the outer edge of the gate electrode 132 (ie, the outer edge of the work function metal layer 142), so that the gate electrode 132 and the high-k dielectric layer 124 form a Figure 1B In other words, the high-k dielectric layer 124 is configured to form a base profile relative to the bottom of the gate electrode 132. In one embodiment, in the X direction, the width 136 of the gate electrode 132 is less than the width 138 of the high-k dielectric layer 124. In addition, in some embodiments, the width of the interface layer 122 is greater than the width 138, however, the present disclosure is also applicable to embodiments in which the width of the interface layer is equal to the width 138.
[0030] The substrate profile formed by the high-k dielectric layer 124 provides many benefits. For example, the portion of the high-k dielectric layer 124 extending beyond the outer edge of the gate electrode 132 increases the width of the high-k metal gate 120 (or the channel region thereunder) in the X direction, thereby forming or expanding the overlap area of the doped region 108 and the high-k metal gate 120. Furthermore, the portion of the high-k dielectric layer 124 extending beyond the outer edge of the gate electrode 132 may generate a fringe electric field under the high-k metal gate 120, which may also improve device performance. Conversely, if the high-k dielectric layer 124 does not extend beyond the outer edge of the gate electrode 132, a portion of the gate spacer 150 formed subsequently may remain under the high-k metal gate 120, resulting in a decrease in device performance due to dielectric breakdown. In many embodiments, the portion of the high-k dielectric layer 124 extending beyond the outer edge of the gate electrode 132 is approximately 5% to 15% of the width 136. If the extension is less than 5%, the expansion of the overlap region cannot significantly improve the device performance. If the extension is greater than 15%, the width of the gate spacer 150 formed subsequently will not be sufficient to cover the extension of the high-k dielectric layer 124, resulting in the loss of the high-k dielectric layer 124 during the subsequent wet etching process.
[0031] In one embodiment, the interface layer 122 includes silicon oxide, silicon oxynitride, other suitable dielectric materials or combinations thereof. The high-k dielectric layer 124 may include one or more high-k dielectric materials (or one or more layers of high-k dielectric materials), such as hafnium silicon oxide (HfSiO), hafnium oxide (HfO2), aluminum oxide (Al2O3), zirconium oxide (ZrO2), lanthanum oxide (La2O3), titanium oxide (TiO2), yttrium oxide (Y2O3), strontium titanate (SrTiO3), other suitable high-k dielectric materials or combinations thereof.
[0032] Depending on whether the semiconductor device 100 is configured as a PFET (p-type field effect transistor) or an NFET (n-type field effect transistor), the work function metal layers 142 and 144 may both be p-type or n-type work function layers. Examples of p-type work function materials include titanium nitride (TiN), tantalum nitride (TaN), ruthenium (Ru), molybdenum (Mo), tungsten (W), platinum (Pt), other suitable p-type work function materials, or combinations thereof. Examples of n-type work function materials include titanium (Ti), aluminum (Al), tantalum carbide (TaC), tantalum carbide (TaCN), tantalum nitride (TaSiN), titanium silicon nitride (TiSiN), other suitable n-type work function materials, or combinations thereof. In some embodiments, the high-k metal gate 120 includes additional work function metal layers. In one embodiment, the threshold voltage of the high-k metal gate 120 is adjusted by including multiple work function metal layers of the same type or opposite types. The bulk conductive layer 146 (or referred to as a filling conductive layer) may include copper (Cu), tungsten (W), cobalt (Co), ruthenium (Ru), aluminum (Al), other suitable conductive materials, or a combination of the above materials.
[0033] The semiconductor device 100 further includes a gate spacer 150 disposed along the sidewall of the gate electrode 132 and disposed above a portion of the high-k dielectric layer 124, a portion of the interface layer 122, and a portion of the semiconductor layer 104. The gate spacer 150 may include one or more layers of dielectric materials, such as silicon oxycarbonitride, silicon nitride, silicon oxynitride, silicon oxide, silicon carbide, other suitable dielectric materials, or combinations thereof. Figure 1B In one embodiment, the gate spacer 150 includes at least three layers of dielectric material (layers 152, 154, 156). The layer 152 may include silicon dioxide (SiO2), silicon oxynitride (SiON), silicon oxycarbonitride (SiOCN), or other suitable materials, and the layer 152 is disposed along the sidewalls of the gate electrode 132, a portion of the high-k dielectric layer 124, a portion of the interface layer 122, and a portion of the semiconductor layer 104. The layer 154 may include silicon oxynitride, silicon oxycarbonitride, or other suitable materials, and the layer 154 is disposed above the layer 152. The layers 154 and 152 may have different materials or different compositions. The layer 156 may include silicon nitride and is disposed on the layer 154. In many embodiments, the layers 152 and 154 are configured to enhance adhesion between the layer 156 and components of the high-k metal gate 120. In many embodiments, the gate spacer 150 includes a dielectric material different from the isolation structure 106 and the interlayer dielectric layer 114. In some embodiments, the bottom of at least one of the layers 152, 154, 156 included in the gate spacer 150 has a step profile similar to the gate electrode 132, the high-k dielectric layer 124, and / or the interface layer 122. Figure 1B For example, a portion of layer 152 contacts work function metal layer 142, a portion of the top surface of high-k dielectric layer 124, and a portion of the top surface of interface layer 122. Layer 154 is configured to have a step profile similar to layer 152.
[0034] Please refer to Figure 1A as well as Figure 1E . The source / drain features 110 (or epitaxial source / drain features) are disposed in the source / drain regions of the semiconductor layer 104, i.e., disposed on opposite sides of the high-k metal gate 120, and the channel region is defined in the semiconductor layer 104 and is located between the source / drain regions and between the doped regions 108. The source / drain features 110 include semiconductor material epitaxially grown in the source / drain regions of the semiconductor layer 104. In many embodiments, the source / drain features 110 are doped with n-type dopants or p-type dopants. In some embodiments where the semiconductor device 100 is configured as an n-type device (e.g., having an n-type channel), the source / drain features 110 include silicon and / or silicon carbon epitaxially grown and doped with phosphorus and / or other n-type dopants (e.g., forming a silicon:phosphorus layer or a silicon:carbon:phosphorus layer). In some embodiments where the semiconductor device 100 is configured as a p-type device (e.g., having a p-type channel), the source / drain features 110 include epitaxially grown silicon germanium doped with boron and / or other p-type dopants (e.g., forming silicon:germanium:boron layers). In some embodiments, the source / drain features 110 include materials and / or dopants that achieve a desired tensile stress and / or compressive stress in the channel region.
[0035] Please refer to Figure 1E , the silicide layer 112 is disposed between the source / drain features 110 and the surface of the interlayer dielectric layer 114. For an embodiment in which the semiconductor device 100 is a FinFET device, the silicide layer 112 surrounds the surface of the source / drain features 110, and the source / drain features 110 are located above the plane of the substrate 102. In many embodiments, since the silicide layer 112 surrounds the source / drain features 110, the bottom of the silicide layer 112 is located below the interface layer 122. In many embodiments, the silicide layer 112 includes: nickel silicide, cobalt silicide, tungsten silicide, tantalum silicide, titanium silicide, platinum silicide, erbium silicide, palladium silicide, other suitable silicides, or combinations of the above materials.
[0036] The interlayer dielectric layer 114 may include one or more dielectric materials, such as silicon oxide, silicon nitride, silicon oxynitride, tetraethyl orthosilicate (TEOS) oxide, undoped silicate glass, doped silicon oxide such as borophosphosilicate glass (BPSG), fused silica glass (FSG), phosphosilicate glass (PSG), borondoped silicon glass (BSG), low-k dielectric materials, and / or other suitable dielectric materials. In one embodiment, the interlayer dielectric layer 114 includes a low-k dielectric material. The interlayer dielectric layer 114 may include a multilayer structure having multiple dielectric materials. In many embodiments, the isolation structure 106, the gate spacer 150, and the interlayer dielectric layer 114 include different dielectric materials.
[0037] Please refer to Figure 1A as well as Figure 1E The contact plug 160 is disposed in the interlayer dielectric layer 114 and is located above the source / drain feature 110, so that the bottom surface of the contact plug 160 electrically and / or physically contacts the silicide layer 112 disposed above the source / drain feature 110. The contact plug 160 is configured to couple the source / drain feature 110 to additional conductive features, such as vias and / or metal lines subsequently formed in the semiconductor device 100. The contact plug 160 includes a conductive material, such as copper (Cu), tungsten (W), cobalt (Co), ruthenium (Ru), aluminum (Al), other suitable conductive materials, or combinations of the above materials. Please refer to Figure 1E The portion of the contact plug 160 that contacts the silicide layer 112 has a width 162 , and the widest portion of the silicide layer 112 has a width 164 . In at least one embodiment, the width 164 is greater than the width 162 .
[0038] Figure 2A as well as Figure 2B According to some embodiments of the present disclosure, a flow chart of a method 200 for forming a semiconductor device 100 is shown. The method 200 is merely an example and is not intended to limit the present disclosure beyond the scope of the claims. Additional operations may be performed before, during, and after the method 200, and some operations described may be replaced, deleted, or moved in other embodiments of the method 200. Figures 3 to 16 , which shows a cross-sectional view of the semiconductor device 100 at an intermediate step of the method 200 (eg Figures 1A to 1C as shown).
[0039] Please refer to Figure 2A as well as Figure 3 The method 200 provides (or is provided) a semiconductor device 100 in operation 202, which has Figure 1A as well as Figure 1B The illustrated substrate 102, a semiconductor layer 104 formed in or protruding from the substrate 102, and an isolation structure 106 formed above the substrate 102. Materials suitable for forming the substrate 102, the semiconductor layer 104, and the isolation structure 106 have been discussed above.
[0040] In one embodiment, the semiconductor layer 104 includes semiconductor fins (eg Figure 1C and Figure 1D), and the method 200 forms fins by epitaxially growing one or more semiconductor layers over the entire area of the substrate 102 and then patterning the semiconductor layers. The semiconductor layer 104 can be patterned in any suitable manner. For example, the semiconductor layer 104 can be patterned using one or more photolithography processes, including double patterning or multi-patterning processes. In general, the double patterning or multi-patterning process combines photolithography with an automatic alignment process so that the resulting pattern has, for example, a smaller pitch than that obtainable using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed over the substrate and patterned using a photolithography process. Spacers are formed next to the patterned sacrificial layer using an automatic alignment process, and then the sacrificial layer is removed. The remaining spacers or mandrels can then be used to pattern the semiconductor layer 104 by etching the initial epitaxial semiconductor layer. The etching process can include: dry etching, wet etching, reactive ion etching (RIE) and / or other suitable processes. The dry etching process can be performed with a fluorine-containing gas (e.g., CF4, SF6, CH2F2, CHF3 and / or C2F6), a chlorine-containing gas (e.g., Cl2, CHCl3, CCl4 and / or BCl3), a bromine-containing gas (e.g., HBr and / or CHBR3), an iodine-containing gas, an oxygen-containing gas (e.g., O2), a nitrogen-containing gas (e.g., N2), helium, argon and / or other suitable gases and / or plasma. The wet etching process can be performed with hydrochloric acid (HCl), potassium hydroxide (KOH), ammonium hydroxide (NH4OH), hydrogen peroxide (H2O2), sulfuric acid (H2SO4), nitric acid (HNO3), hydrofluoric acid (HF), phosphoric acid (H3PO4), ammonium phosphate ((NH4)3PO4), tetramethylammonium hydroxide (TMAH) and / or other suitable etchants. Alternatively or additionally, the wet etching process may use a mixture of solutions, for example: a standard clean 1 (SC1; also known as an ammonia-peroxide mixture (APM)) mixture comprising NH4OH, H2O2 and distilled water (DIW); a standard clean 2 (SC2) mixture comprising HCl, H2O2 and DIW; or a mixture of H2SO4, H2O2 and DIW.
[0041] The isolation structure 106 may be formed by one or more deposition and etching methods. The deposition method may include thermal oxidation, chemical oxidation, and chemical vapor deposition (CVD, such as flow CVD (FCVD)). The etching method may include dry etching and / or wet etching, and a subsequent planarization method, such as chemical-mechanical polishing / planarizing (CMP).
[0042] Please refer to Figure 2A as well as Figure 4 In operation 204, the method 200 forms an interface layer 122 above the semiconductor layer 104. Various materials suitable for forming the interface layer 122 have been previously described with reference to Figure 1A as well as Figure 1B Discussion. In one embodiment, the interface layer 122 is formed by performing a chemical cleaning process on a portion of the semiconductor layer 104 to form the interface layer 122 comprising silicon oxide, silicon oxynitride, other suitable chemical oxides, or a combination of the foregoing materials. In an exemplary embodiment, the chemical cleaning process is performed with a mixture comprising sulfuric acid. In many embodiments, the interface layer 122 is provided to enhance adhesion between the semiconductor layer 104 and a subsequently formed material layer (e.g., a high-k dielectric layer 124). Alternatively, the interface layer 122 can be formed by an oxidation process, such as chemical oxidation, thermal oxidation, other suitable oxidation processes, or a combination of the foregoing processes.
[0043] Please refer to Figure 5 The method 200 then forms a high-k dielectric layer 124 over the interface layer 122 in operation 206. Various materials suitable for forming the high-k dielectric layer 124 have been described above with reference to Figure 1A as well as Figure 1BFor example, the high dielectric constant dielectric layer 124 may be: hafnium oxide (HfO2), hafnium silicon oxide (HfSiO), aluminum oxide (Al2O3), zirconium oxide (ZrO2), lanthanum oxide (La2O3), other suitable high dielectric constant dielectric materials or combinations of the above materials. The high dielectric constant dielectric layer 124 may be deposited by any suitable deposition process, such as: CVD, atomic layer deposition (ALD), physical vapor deposition (PVD), other deposition processes or combinations thereof. The high dielectric constant dielectric layer 124 may be deposited to any suitable thickness, such as about 1 nanometer to about 2 nanometers. A thickness outside the above range may result in a decrease in the reliability and / or performance of the device. For example, if the thickness of the high dielectric constant dielectric layer 124 is too thin (e.g., less than about 1 nanometer), the reliability of the device may be a concern due to phenomena such as time-dependent dielectric breakdown (TDDB). In another example, if the thickness of the high-k dielectric layer 124 is too thick (e.g., greater than about 2 nanometers), device performance may be degraded due to a higher than desired equivalent oxide thickness (EOT). In an exemplary embodiment, the deposition of the high-k dielectric layer 124 is performed at a temperature of about 300 degrees Celsius for about 5 minutes, although the present disclosure is not limited to this set of processing conditions.
[0044] In some embodiments, after depositing the high-k dielectric layer 124, the method 200 optionally performs an annealing process (hereinafter referred to as a "post-deposition annealing" or PDA process) in operation 206. In one embodiment, the PDA process implements a spike annealing process, in which the high-k dielectric layer 124 is annealed in an inert environment (e.g., a nitrogen environment) at a maximum temperature of about 800 degrees Celsius to about 900 degrees Celsius for about 1 second. The PDA process can be adjusted so that the material in the high-k dielectric layer 124 is crystallized before performing subsequent manufacturing steps. In some embodiments, the PDA process is optional, and the high-k dielectric layer 124 is not subjected to the PDA process after formation.
[0045] Please refer to Figure 2A as well as Figure 6In some embodiments, after depositing the high-k dielectric layer 124 (e.g., including a subsequent PDA process), the method 200 forms a capping layer 126 over the high-k dielectric layer 124 in operation 206. In many embodiments, the capping layer 126 is provided to limit excessive regrowth of the interface layer 122 that would result in a thicker EOT. The capping layer 126 may include one or more conductive materials, such as titanium nitride (TiN), titanium silicon nitride (TiSiN), tantalum silicon nitride (TaSiN), tantalum nitride (TaN), tantalum carbide (TaC), tantalum carbonitride (TaCN), other suitable metal materials, or combinations thereof. In one embodiment, the capping layer 126 includes titanium nitride. The capping layer 126 may be formed by any suitable deposition process, such as CVD, ALD, PVD, other suitable processes, or combinations thereof, at a temperature of about 375 degrees Celsius. In some embodiments, the thickness of the capping layer 126 may fall within a range of 1 nm to 2 nm. If the thickness of the capping layer 126 is too thin (e.g., less than about 1 nm), the capping layer 126 may not effectively prevent the regrowth of the interface layer 122, and if the thickness of the capping layer 126 is too thick (e.g., greater than about 2 nm), the number of metal gate conductive layers that can be formed in the subsequent gate replacement process may be limited due to the reduced space in the gate trench. In one embodiment, after depositing the capping layer 126, the method 200 selectively performs an annealing process (hereinafter referred to as a "post-metallization annealing" or PMA process). In one embodiment, the PMA process implements a spike annealing process, in which the capping layer 126 is annealed in an inert environment (e.g., a nitrogen environment) at a maximum temperature of about 800 degrees Celsius to about 900 degrees Celsius for about 1 second. Although similar to the PDA process applied to the high-k dielectric layer 124, the PMA process can be implemented with different annealing conditions according to different design requirements. The PMA process can be tuned to limit the regrowth of the interface layer 122 to improve device reliability. In many embodiments, the formation and annealing of the capping layer 126 can be omitted.
[0046] In one embodiment, the method 200 further forms a second capping layer (not shown) over the capping layer 126 in operation 206. The second capping layer is different from the capping layer 126 in that the second capping layer is a silicon-containing capping layer that can be deposited at about 390 degrees Celsius by a deposition process (e.g., CVD, ALD, PVD, other suitable processes, or combinations thereof) to a thickness of about 2 nanometers to about 6 nanometers. The method 200 then performs an annealing process (hereinafter referred to as "post capping layer annealing" or PCA process). The PCA process can be implemented as a spike annealing at a maximum temperature of about 850 degrees Celsius to about 910 degrees Celsius for about 1 second. After the PCA process, the second capping layer is removed from the semiconductor device 100 by any suitable method, such as a dry etching method or a wet etching method (for example, using a wet etchant such as HF). In many embodiments, the second capping layer is provided to prevent the capping layer 126 from absorbing oxygen and forming excessive oxides that may degrade the performance of the semiconductor device 100. In some embodiments, the formation, annealing, and removal of the second capping layer may be omitted during the implementation of the method 200 .
[0047] Please refer to Figure 2A as well as Figure 7 The method 200 forms a polysilicon layer 128 on the cap layer 126 (or directly on the high-k dielectric layer 124 if the cap layer 126 is omitted) in operation 208. The polysilicon layer 128 may be formed by any deposition process, such as CVD, low pressure chemical vapor deposition (LPCVD), plasma enhanced chemical vapor deposition (PECVD), other suitable deposition processes, or combinations thereof.
[0048] Please refer to Figure 2A , Fig. 8A as well as Figure 8B In operation 210, the method 200 patterns the polysilicon layer 128 (and one or more hard mask layers, such as the hard mask layer 232) to form a dummy gate electrode 130. Specifically, the process and conditions of the method 200 are adjusted so that the length of the dummy gate electrode 130 in the X direction is formed to be smaller than the length of the high-k dielectric layer 124. Fig. 8AAs shown, the method 200 forms a mask element 236 above the polysilicon layer 128 to expose the portion of the polysilicon layer 128 to be removed. The mask element 236 may include a patterned resist layer 234, and may further include other material layers, such as a hard mask layer 232. The method 200 then performs an etching process 302 to remove a portion of the hard mask layer 232, the polysilicon layer 128, the cap layer 126, the high-k dielectric layer 124, and the interface layer 122, so that the dummy gate electrode 130 has a sloped sidewall (i.e., the bottom of the dummy gate electrode 130 is wider than the top of the dummy gate electrode 130). After the etching process 302 is completed, the patterned resist layer 234 is removed from the dummy gate electrode 130 by any suitable method, such as plasma ashing or resist stripping. In this manufacturing step, the hard mask layer 232 remains above the dummy gate electrode 130.
[0049] In this embodiment, the dummy gate electrode 130 is replaced by a gate electrode (see Fig.15 , Fig.16 and related text below), however, the high-k dielectric layer 124 will remain in the final device and be used as a gate dielectric or a portion thereof. Because the high-k dielectric layer 124 is deposited before the dummy gate electrode 130 is deposited, this process is also referred to as a "high-k dielectric layer first" process, which is different from other processes in which the high-k dielectric layer 124 is not formed until after the dummy gate electrode 130 is replaced (referred to as a "high-k dielectric layer later" process). The "high-k dielectric layer first" process allows high-temperature annealing of the high-k dielectric layer 124 to be performed at an earlier stage of manufacturing, and subsequently allows the silicidation process of the source / drain features 110 to be performed before the gate replacement process. In this way, the silicide layer (e.g., silicide layer 112) can completely cover the source / drain features 110, as described in detail below. In addition, since the high-k dielectric layer 124 is formed before replacing the dummy gate electrode 130, more space can be allocated to form additional work function metal layers (e.g., work function metal layers 142, 144) for adjusting the threshold voltage of HKMG. Similarly, the "high-k dielectric layer first formation" process also allows more space to be used for forming a bulk conductive layer (e.g., bulk conductive layer 146), thereby reducing the contact resistance between HKMG and the contact plug (not shown) subsequently formed above HKMG.
[0050] In many embodiments, the etching process 302 includes a two-step etching process. The first step of the etching process 302 can be performed using a dry etchant, and the dry etchant includes: a chlorine-containing gas (such as Cl2), a fluorine-containing gas (such as CF4, CHF3, CH3F or NF3), a bromine-containing gas (such as HBr), an oxygen-containing gas (such as O2), other suitable gases or combinations of the above gases. The first step can be performed at an etching power of about 300 watts to about 1000 watts for about 10 seconds to about 100 seconds. The second step of the etching process 302 can be performed using a dry etchant, and the dry etchant includes: a chlorine-containing gas (such as Cl2), a bromine-containing gas (such as HBr), an oxygen-containing gas (such as O2), other suitable gases or combinations of the above gases.
[0051] Figure 8B for Fig. 8A FIG. 1 is an enlarged view of a portion 140 of a semiconductor device 100. For example, Figure 8B As shown, the etching process 302 can be adjusted to selectively remove a portion of the high-k dielectric layer 124 and the capping layer 126 relative to the interface layer 122. As a result, in at least one embodiment, the outer edge of the interface layer 122 extends beyond the outer edge of the dummy gate electrode 130 by a distance 334, and the outer edge of the capping layer 126 and / or the high-k dielectric layer 124 extends beyond the outer edge of the dummy gate electrode 130 by a distance 336, wherein the distance 334 is greater than the distance 336. In another example, the outer edge of the interface layer 122 is aligned with the outer edge of the high-k dielectric layer 124, i.e., the distance 334 is substantially equal to the distance 336.
[0052] Specifically, during one or both steps of the etching process 302, a polymerized gaseous substance may be deposited on the semiconductor device 100 to control the etching of the polysilicon layer 128 relative to the interface layer 122, the high-k dielectric layer 124, and / or the cap layer 126, resulting in Figure 1A and Figure 1B The substrate profile shown. For example, to form the substrate profile, the polymerized gas material deposited along the sidewalls of the polysilicon layer 128 in the second etching step is less than that in the first etching step (i.e., anisotropic etching of the polysilicon layer 128), and the polysilicon layer 128 can be etched more laterally (i.e., in the X direction) relative to the interface layer 122 and / or the high-k dielectric layer 124. Alternatively or additionally, more polymerized gas material can be deposited in the second etching step to limit the extent of the lateral etching of the interface layer 122 and / or the high-k dielectric layer 124 relative to the polysilicon layer 128, so that a portion of the remaining interface layer 122 and / or the high-k dielectric layer 124 can extend laterally in the X direction beyond the outer edge of the dummy gate electrode 130 (e.g., as shown in FIG. 1 ). Fig. 8A and Figure 8BIn some embodiments, since the bottom of the polysilicon layer 128 near the interface layer 122 and the high-k dielectric layer 124 is etched less than the top, the dummy gate electrode 130 may be configured to have an inclined sidewall, such as Figure 1A and Figure 1B As shown. Examples of polymerizing gaseous substances include: oxygen-containing substances, carbon dioxide-containing substances, nitrogen-containing substances, substances that produce polymer etching byproducts, or combinations thereof. In addition, different etchants or combinations of etchants may be used in addition (or instead of depositing polymer gaseous substances) to achieve selective etching of the polysilicon layer 128, the high-k dielectric layer 124, the interface layer 122, and / or the capping layer 126 to form the substrate profile.
[0053] Please refer to Figure 2A as well as Fig. 9 . In operation 212, the method 200 forms a doped region 108 (e.g., an LDD region or a source / drain extension region) on both sides of the dummy gate electrode 130 and between the source / drain regions of the semiconductor layer 104. For example, the doped region 108 can be formed by using tilted and rotated ion implantation and using the dummy gate electrode 130 as a mask to implant ions into the semiconductor layer 104, and then performing an annealing process to activate the dopant. The doped region 108 may include one or more layers at different depths below the top surface of the semiconductor layer 104. Depending on the desired FET device type, the doped region 108 may be an n-type doped region or a p-type doped region. For example, the doped region 108 includes an n-type dopant for forming an NFET device, whereas the doped region 108 includes a p-type dopant for forming a PFET device. The doped region 108 can be formed to extend laterally below the dummy gate electrode 130 (e.g., Fig. 9 ), or in an alternative embodiment does not extend below the dummy gate electrode 130. In many embodiments, the doped region 108 comprises an extension of the source / drain region of the semiconductor device 100. In some embodiments, the doped region 108 can be formed after forming the gate spacer 150 and before forming the source / drain features 110 in the semiconductor device 100.
[0054] Please refer to Figure 2B , Fig. 10A as well as Fig. 10B In operation 214, the method 200 forms a gate spacer 150 along the sidewalls of the dummy gate electrode 130, the high-k dielectric layer 124, the interface layer 122, and / or the capping layer 126, and the exposed top surface of the high-k dielectric layer 124, the interface layer 122, and / or the capping layer 126. Figure 1A as well as Figure 1BAs shown, the gate spacer 150 may be a multi-layer structure, including layers 152, 154, 156 as discussed above. Each of the layers 152, 154, 156 may be formed by depositing a spacer material covering the isolation structure 106, the semiconductor layer 104, and the dummy gate electrode 130, and then etching the spacer material by an anisotropic etching process to expose the top surface of the isolation structure 106, the dummy gate electrode 130, and the top surface of the semiconductor layer 104. The portion of the spacer material along the sidewalls of the dummy gate electrode 130, the high-k dielectric layer 124, the interface layer 122, and / or the capping layer 126 and located above the exposed portion of the top surface of the high-k dielectric layer 124, the interface layer 122, and / or the capping layer 126 becomes the layer 152, 154, 156 of the gate spacer 150.
[0055] Please refer to Figure 2B as well as Fig.11 The method 200 forms a source / drain feature 110 in the semiconductor device 100 in operation 218. Various materials suitable for forming the source / drain feature 110 have been previously described with reference to Figure 1A as well as Figure 1B Discussion. In one embodiment, method 200 forms a recess (not shown) in a portion of semiconductor layer 104 by an etching process, and epitaxially grows semiconductor material in the recess as source / drain features 110. Prior to epitaxially growing the semiconductor material, a cleaning process may be optionally performed to clean the recess with a hydrofluoric acid (HF) solution or other suitable solution. The semiconductor material may extend upward beyond the top surface of semiconductor layer 104 (e.g., Fig.11) or formed below the top surface of the semiconductor layer 104. The method 200 may form the source / drain features 110 for NFET and PFET devices, respectively. For example, the method 200 may form the source / drain features 110 with n-type doped silicon for NFET devices, or form the source / drain features 110 with p-type doped silicon germanium for PFET devices. The method 200 may implement a CVD deposition technique (e.g., vapor-phase epitaxy (VPE), ultra-high vacuum CVD (UHV-CVD), LPCVD, PECVD, other suitable CVD techniques, or combinations thereof), molecular beam epitaxy, selective epitaxial growth (SEG), other suitable processes, or combinations thereof to form the source / drain features 110. In many embodiments, the source / drain features 110 and the doped region 108 include dopants of similar semiconductor types but different concentrations. For example, source / drain features 110 and doped regions 108 may both include an n-type dopant such as phosphorus, but source / drain features 110 may have a significantly higher dopant concentration than doped regions 108. In many embodiments, source / drain features 110 partially overlap doped regions 108.
[0056] Please refer to Figure 2B as well as Fig.12 The method 200 forms a silicide layer 112 on the surface of the source / drain feature 110 in operation 218. Various materials suitable for forming the silicide layer 112 have been previously described with reference to Figure 1A as well as Figure 1C Discussion. The silicide layer 112 may be formed by a deposition process, such as CVD, ALD, PVD, other suitable processes or combinations thereof. For example, a metal layer (e.g., nickel) may be deposited on the source / drain feature 110, and then the semiconductor device 100 may be annealed to allow the metal layer to react with the semiconductor material of the source / drain feature 110. Thereafter, the unreacted metal layer is removed, leaving the silicide layer 112 on the source / drain feature 110. Specifically, in the present embodiment, the silicide layer 112 surrounds the upper portion of the source / drain feature 110 and matches the shape of the upper portion of the source / drain feature 110 (e.g., a hexagon or a diamond, etc.).
[0057] Generally speaking, the silicide layer (e.g., silicide layer 112) can withstand a processing temperature of up to about 500 degrees Celsius. Therefore, in the "high-k dielectric layer formed last" process, the formation and heat treatment of the high-k dielectric layer (e.g., high-k dielectric layer 124) has the risk of damaging the silicide layer, thereby increasing the contact resistance of the device. Therefore, in the "high-k dielectric layer formed last" process, the formation of the silicide layer is usually postponed until after the dummy gate electrode is replaced with HKMG, after the contact hole is etched in the interlayer dielectric layer above the source / drain features, and before the contact plug is deposited. The above process will limit the contact area between the silicide layer and the source / drain features to the area exposed through the contact hole, thereby limiting the degree of contact resistance reduction provided by the silicide layer. However, in the present disclosure, since the high-k dielectric layer 124 has been formed and heat-treated in an earlier manufacturing step (e.g., operation 206), the silicide layer 112 can be formed on each exposed surface of the source / drain feature 110 before the interlayer dielectric layer 114 is formed, thereby increasing the contact area between the silicide layer 112 and the source / drain feature 110 (i.e., reducing the contact resistance). Please refer back to Figure 1E In one exemplary embodiment, a silicide layer 112 is formed to cover an upper portion of the source / drain features 110 .
[0058] Please refer to Fig.13 . Thereafter, the method 200 forms an interlayer dielectric layer 114 over the source / drain features 110 (including the silicide layer 112), the dummy gate electrode 130, the gate spacer 150, and the isolation structure 106. In some embodiments, the method 200 forms a contact etch-stop layer (CESL, not shown) before forming the interlayer dielectric layer 114. The CESL may include silicon nitride, silicon oxynitride, silicon carbon nitride oxide, other suitable materials, or a combination of the foregoing materials, and the CESL may be formed by CVD, PVD, ALD, other suitable methods, or a combination of the foregoing methods. Various materials suitable for forming the interlayer dielectric layer 114 have been described above with reference to Figure 1A as well as Figure 1B Discussion. The interlayer dielectric layer 114 may be formed by PECVD, FCVD, other suitable methods, or a combination of the above methods. The method 200 then performs one or more CMP processes to planarize the top surface of the semiconductor device 100 and expose the top surface of the dummy gate electrode 130 (as shown in FIG. 10 ).
[0059] Please refer to Figure 2B Fig.14 as well as Fig.15 The method 200 continues in operation 220 by Figure 1A as well as Figure 1B The gate electrode 132 shown replaces the dummy gate electrode 130. Fig.14 , method 200 first removes the dummy gate electrode 130 to form a gate trench 148 and partially exposes the underlying material layer. Removal of the dummy gate electrode 130 includes performing one or more etching processes that are selective to the material contained in the dummy gate electrode 130 (e.g., polysilicon) rather than the gate spacer 150, the capping layer 126 and / or the high-k dielectric layer 124. The etching process may include dry etching, wet etching, RIE and / or other suitable etching methods. In one embodiment, the etching process for removing the dummy gate electrode 130 is implemented with a dry etchant, and the dry etchant includes a fluorine-containing gas (e.g., NF3), a hydrogen-containing gas (e.g., H2), helium, other suitable gases, or a combination of the above gases. The etchant has a relatively high etching selectivity to the dummy gate electrode 130 and does not etch the high-k dielectric layer 124. In many embodiments, such as Fig.14 As shown, the capping layer 126 and the hard mask layer 232 are removed after the dummy gate electrode 130 is removed, thereby exposing the high-k dielectric layer 124 in and outside the gate trench 148 .
[0060] Please refer to Fig.15 Thereafter, the method 200 forms a gate electrode 132 above the high-k dielectric layer 124 in the gate trench 148 to form a high-k metal gate 120. Figure 1A as well as Figure 1B As shown, the gate electrode 132 includes multiple conductive layers, such as work function metal layers 142, 144 and a bulk conductive layer 146. Materials suitable for forming the work function metal layers 142, 144 and the bulk conductive layer 146 have been discussed above. The work function metal layers 142, 144 may be of the same conductivity type (i.e., both are n-type or both are p-type), or of opposite conductivity types (i.e., one is n-type and the other is p-type). The number and type of work function metal layers to be included depends on the desired threshold voltage of the final high dielectric constant metal gate 120. Although not shown in the figure, the gate electrode 132 may further include other material layers, such as: additional work function metal layers, capping layers, barrier layers, diffusion layers, other suitable layers or combinations thereof. The various material layers included in the gate electrode 132 can be deposited by any suitable process, such as: CVD, PVD, ALD, electroplating, chemical plating, other suitable deposition processes or combinations of the above processes. Thereafter, the method 200 performs one or more CMP processes to planarize the top of the semiconductor device 100 , thereby exposing the top surface of the gate electrode 132 , the gate spacer 150 , and / or the top surface of the interlayer dielectric layer 114 .
[0061] In many embodiments, since the high-k dielectric layer 124 is formed prior to forming and removing the dummy gate electrode 130, no high-k material is formed in the gate trench 148, and thus, the process window for forming multiple conductive layers is increased, thereby accommodating more conductive layers in the gate trench 148 compared to embodiments in which the high-k dielectric layer 124 is formed in the gate trench 148 as a partial gate replacement process. Allowing the inclusion of additional work function metal layers provides an opportunity to fine-tune the threshold voltage of the high-k metal gate 120, thereby improving the performance of the semiconductor device 100. In addition, the increased process window allows the bulk conductive layer 146 to be formed with a greater thickness, thereby reducing the contact resistance between the bulk conductive layer 146 and a contact plug (not shown) subsequently formed on the high-k metal gate 120.
[0062] Please refer to Fig.16 In operation 222, the method 200 forms a source / drain contact plug 160 in the interlayer dielectric layer 114 such that the contact plug 160 contacts the silicide layer 112 formed on the source / drain feature 110. Materials suitable for forming the contact plug 160 have been previously described with reference to Figure 1A as well as Figure 1C Discussion. The contact plug 160 may include copper (Cu), cobalt (Co), ruthenium (Ru), tungsten (W), aluminum (Al), other suitable conductive materials, or combinations thereof. The contact plug 160 may be formed by patterning and etching the interlayer dielectric layer 114 to form a contact hole in the interlayer dielectric layer 114 above the source / drain features 110, and then depositing one or more conductive materials in the contact hole, and the conductive material deposition method is, for example, CVD, ALD, PVD, electroplating, chemical plating, other suitable methods, or combinations thereof. One or more CMP processes are then performed to remove excess material from the top surface of the semiconductor device 100 so that the top surfaces of the high-k metal gate 120, the contact plug 160, and the interlayer dielectric layer 114 are coplanar.
[0063] Please refer back Figure 2B Next, the method 200 performs additional processing steps on the semiconductor device 100 in operation 224. For example, the method 200 may form additional vertical interconnect features, such as vias connected to the contact plugs 160 (also known as device-level contacts), or form multi-layer interconnect features, such as metal layers including conductive lines and interlayer dielectric materials formed above the semiconductor device 100.
[0064] Although the embodiments described above show FinFETs, the inventive concepts disclosed herein can be applied to other types of transistors including planar FETs. For example, in a planar FET, the semiconductor layer 104 is part of the substrate 102, and the substrate 102 may be a bulk silicon substrate or an SOI substrate. The disclosed manufacturing method can be similarly applied to these planar FETs to form a high-k dielectric layer before forming a dummy gate electrode, and retain the high-k dielectric layer in the final transistor, as described above with respect to FinFETs.
[0065] Although not intended to be limiting, one or more embodiments of the present disclosure provide a number of benefits to semiconductor devices and methods of forming the same. For example, in contrast to a "high-k dielectric layer formed last" process, forming a high-k dielectric layer prior to the formation and removal of a dummy gate electrode increases the processing window available for forming multiple conductive layers (e.g., work function metal layers 142, 144) during the gate replacement process, providing an opportunity to adjust the threshold voltage of the final high-k metal gate to improve device performance. In addition, because the silicide layer can be formed after the high-k dielectric layer is formed and annealed, thermal damage to the silicide layer caused by processing the high-k dielectric layer can be reduced (or minimized), and the silicide layer can be formed to have a larger surface area than when the silicide layer is formed by a subsequent patterning process, resulting in a reduced contact resistance between the contact plug and the source / drain features.
[0066] According to some embodiments of the present disclosure, a method for forming a semiconductor structure includes: providing a semiconductor layer; forming an interface layer above the semiconductor layer; depositing a high-k dielectric layer above the interface layer; forming a dummy gate electrode above the high-k dielectric layer; patterning the dummy gate electrode, the high-k dielectric layer, and the interface layer so that the width of the dummy gate electrode is smaller than the width of the high-k dielectric layer; after patterning, forming spacers along the sidewalls of the dummy gate electrode, the high-k dielectric layer, and the interface layer; forming a plurality of source / drain features above the semiconductor layer; and replacing the dummy gate electrode with a metal gate electrode to form a high-k metal gate structure.
[0067] In one or more embodiments of the present disclosure, the method for forming a semiconductor structure further includes performing a spike annealing process after depositing the high-k dielectric layer and before forming the dummy gate electrode.
[0068] In one or more embodiments of the present disclosure, the method for forming a semiconductor structure further includes depositing a capping layer on the high-k dielectric layer after depositing the high-k dielectric layer and before forming the dummy gate electrode.
[0069] In one or more embodiments of the present disclosure, after depositing the high-k dielectric layer and before forming the dummy gate electrode, the semiconductor structure forming method further includes: performing a spike annealing process on the capping layer in a nitrogen environment; and removing the capping layer before replacing the dummy gate electrode.
[0070] In one or more embodiments of the present disclosure, before forming the dummy gate electrode, the semiconductor structure forming method further includes: depositing a silicon-containing capping layer on the capping layer; performing a spike annealing process on the silicon-containing capping layer; and removing the silicon-containing capping layer.
[0071] In one or more embodiments of the present disclosure, the patterning step removes a portion of the interface layer, such that the width of the interface layer is greater than the width of the high-k dielectric layer.
[0072] In one or more embodiments of the present disclosure, the method for forming a semiconductor structure further includes forming a silicide layer on the surface of the source / drain features before replacing the dummy gate electrode.
[0073] According to some embodiments of the present disclosure, a method for forming a semiconductor structure includes: forming an interface layer above a fin, the fin extending along a first direction; depositing a high-k dielectric layer above the interface layer; depositing a polysilicon layer above the high-k dielectric layer, the polysilicon layer extending along a second direction, the second direction being substantially perpendicular to the first direction; patterning the polysilicon layer, the high-k dielectric layer, and the interface layer so that the high-k dielectric layer partially extends beyond an outer edge of the polysilicon layer in the first direction; and after patterning, forming a dielectric film along a sidewall of the polysilicon layer. The invention relates to a method for forming a plurality of gate spacers, wherein the gate spacers are partially formed above a portion of the high-k dielectric layer extending beyond an outer edge of the polysilicon layer; forming a plurality of source / drain features in the fin; forming a silicide layer on a surface of the source / drain features; forming an interlayer dielectric layer above the polysilicon layer, the gate spacers, and the silicide layer; removing the polysilicon layer to expose the high-k dielectric layer; forming a metal gate above the high-k dielectric layer; and forming a source / drain contact plug in the interlayer dielectric layer, the source / drain contact plug contacting the silicide layer.
[0074] In one or more embodiments of the present disclosure, the steps of patterning a polysilicon layer, a high-k dielectric layer, and an interface layer include: forming an etching mask over a portion of the polysilicon layer; and performing an etching process to remove the portion of the polysilicon layer that exposes the etching mask, so that the patterned polysilicon layer has an inclined sidewall.
[0075] In one or more embodiments of the present disclosure, the etching process selectively removes a portion of at least one of the interface layer and the high-k dielectric layer.
[0076] In one or more embodiments of the present disclosure, after depositing the high-k dielectric layer and before forming the polysilicon layer, the method for forming a semiconductor structure further includes: annealing the high-k dielectric layer; depositing a titanium-containing capping layer over the high-k dielectric layer; and annealing the titanium-containing capping layer.
[0077] In one or more embodiments of the present disclosure, the step of removing the polysilicon layer selectively does not remove the high-k dielectric layer.
[0078] In one or more embodiments of the present disclosure, the step of removing the polysilicon layer includes performing a dry etching process, wherein the dry etching process is performed using nitrogen trifluoride, hydrogen, helium, or a combination thereof.
[0079] According to some embodiments of the present disclosure, a semiconductor structure includes a high-k metal gate, a plurality of source / drain features, and a contact plug. The high-k metal gate is disposed above a channel region of a semiconductor layer, and the semiconductor layer is disposed above a substrate. The high-k metal includes an interface layer, a high-k dielectric layer, an electrode, and a plurality of gate spacers. The interface layer is disposed above the semiconductor layer and has a first length along a first direction. The high-k dielectric layer is disposed above the interface layer and has a second length along the first direction. The electrode is disposed above the high-k dielectric layer and has a third length along the first direction. Both the first length and the second length are greater than the third length. The gate spacer is disposed along the sidewall of the electrode, and the bottom of the gate spacer contacts the top surface of the high-k dielectric layer. The source / drain features are disposed in the semiconductor layer and are located on opposite sides of the high-k metal gate. The contact plug is disposed above the source / drain features.
[0080] In one or more embodiments of the present disclosure, the gate spacer includes a first silicon oxycarbon nitride layer, a second silicon oxycarbon nitride layer, and a silicon nitride layer. The first silicon oxycarbon nitride layer is disposed along the sidewall of the electrode and is disposed above the top surface of the high-k dielectric layer and the exposed portion of the top surface of the interface layer. The second silicon oxycarbon nitride layer is disposed above the first silicon oxycarbon nitride layer, and the second silicon oxycarbon nitride layer is different from the first silicon oxycarbon nitride layer. The silicon nitride layer is disposed above the second silicon oxycarbon nitride layer.
[0081] In one or more embodiments of the present disclosure, a sidewall of the electrode directly contacts the gate spacer.
[0082] In one or more embodiments of the present disclosure, the semiconductor structure further includes a silicide layer disposed above the source / drain features. The silicide layer covers the source / drain features.
[0083] In one or more embodiments of the present disclosure, the bottom of the silicide layer is lower than the interface layer.
[0084] In one or more embodiments of the present disclosure, the distance from the outer edge of the electrode to the outer edge of the high-k dielectric layer is greater than the distance from the outer edge of the electrode to the outer edge of the interface layer.
[0085] In one or more embodiments of the present disclosure, the distance from the outer edge of the electrode to the outer edge of the high-k dielectric layer is smaller than the distance from the outer edge of the electrode to the outer edge of the interface layer.
[0086] The features of several embodiments are summarized above so that those skilled in the art can better understand the aspects of the present disclosure. Those skilled in the art should understand that the present disclosure can be easily used to design or modify other processes and structures to achieve the same purposes and / or achieve the same advantages as the embodiments described herein. Those skilled in the art should also understand that such equivalent constructions do not depart from the spirit and scope of the present disclosure, and various changes, substitutions and modifications can be made herein without departing from the spirit and scope of the present disclosure.
Claims
1. A method for forming a semiconductor structure, characterized in that: Include: providing a semiconductor layer; forming an interface layer above the semiconductor layer; Depositing a high-k dielectric layer over the interface layer; forming a dummy gate electrode above the high-k dielectric layer; Patterning the dummy gate electrode, the high-k dielectric layer, and the interface layer so that a width of the interface layer is greater than a width of the high-k dielectric layer; After the patterning, forming a spacer along the sidewalls of the dummy gate electrode, the high-k dielectric layer, and the interface layer; forming a plurality of source / drain features over the semiconductor layer; Replacing the dummy gate electrode with a metal gate electrode to form a high dielectric constant metal gate structure; After depositing the high-k dielectric layer and before forming the dummy gate electrode, depositing a capping layer on the high-k dielectric layer; performing a spike annealing process on the capping layer in a nitrogen environment; and The capping layer is removed before replacing the dummy gate electrode.
2. A method for forming a semiconductor structure, characterized in that: Include: providing a semiconductor layer; forming an interface layer above the semiconductor layer; Depositing a high-k dielectric layer over the interface layer; forming a dummy gate electrode above the high-k dielectric layer; Patterning the dummy gate electrode, the high-k dielectric layer, and the interface layer so that a width of the interface layer is greater than a width of the high-k dielectric layer; After the patterning, forming a spacer along the sidewalls of the dummy gate electrode, the high-k dielectric layer, and the interface layer; forming a plurality of source / drain features over the semiconductor layer; Replacing the dummy gate electrode with a metal gate electrode to form a high dielectric constant metal gate structure; After depositing the high-k dielectric layer and before forming the dummy gate electrode, depositing a capping layer on the high-k dielectric layer; Before forming the dummy gate electrode, depositing a silicon-containing capping layer on the capping layer; performing a spike annealing process on the silicon-containing capping layer; and The silicon-containing capping layer is removed.
3. A semiconductor structure, characterized in that: Include: A high dielectric constant metal gate structure is disposed above a channel region of a semiconductor layer, wherein the semiconductor layer is disposed above a substrate, and the high dielectric constant metal gate structure comprises: An interface layer is disposed above the semiconductor layer and has a first length along a first direction; a high-k dielectric layer disposed above the interface layer and having a second length along the first direction, wherein the second length is smaller than the first length; and an electrode disposed above the high-k dielectric layer and having a third length along the first direction, wherein the second length is greater than the third length, wherein a distance between an outer edge of the electrode and an outer edge of the high-k dielectric layer is less than a distance between the outer edge of the electrode and an outer edge of the interface layer; a gate spacer disposed along a sidewall of the electrode, wherein a bottom of the gate spacer contacts a top surface of the high-k dielectric layer; a plurality of source / drain features disposed in the semiconductor layer and located on opposite sides of the high-k metal gate structure; and A contact plug is disposed above the plurality of source / drain features.
4. A method for forming a semiconductor structure, characterized in that: Include: forming an interface layer above a semiconductor layer; Depositing a high-k dielectric layer over the interface layer; forming a dummy gate electrode above the high-k dielectric layer; Patterning the dummy gate electrode, the high-k dielectric layer and the interface layer so that the interface layer extends laterally beyond the outer edge of the high-k dielectric layer and the high-k dielectric layer extends laterally beyond the outer edge of the dummy gate electrode; forming a spacer along the patterned sidewalls of the dummy gate electrode, the high-k dielectric layer, and the interface layer; forming a plurality of source / drain features adjacent to the spacer; as well as The dummy gate electrode is replaced by a metal gate electrode.
5. The method for forming a semiconductor structure according to claim 4, wherein: Further including: After depositing the high-k dielectric layer and before forming the dummy gate electrode, a spike annealing process is performed.
6. The method for forming a semiconductor structure according to claim 4, wherein: Further including: Before replacing the dummy gate electrode, a silicide layer is formed on the plurality of source / drain features, so that the silicide layer covers a portion of the plurality of source / drain features.
7. The method for forming a semiconductor structure according to claim 4, wherein: The step of replacing the dummy gate electrode comprises: removing the dummy gate electrode to form a trench; forming a work function metal layer in the trench so that a sidewall portion of the work function metal layer contacts the spacer and a bottom of the work function metal layer contacts the high-k dielectric layer; and A bulk conductive layer is formed above the work function metal layer.
8. The method for forming a semiconductor structure according to claim 4, wherein: Further including: Before forming the spacer, a plurality of doped regions are formed in the semiconductor layer below the dummy gate electrode.
9. The method for forming a semiconductor structure according to claim 4, wherein: Further including: Before forming the dummy gate electrode, a covering layer is formed on the high-k dielectric layer, wherein the step of replacing the dummy gate electrode includes removing the covering layer.
10. The method for forming a semiconductor structure according to claim 9, wherein: Further including: Before forming the dummy gate electrode, a spike annealing process is performed on the capping layer in a nitrogen environment.
11. A method for forming a semiconductor structure, characterized in that: Include: forming an interface layer above a fin, the fin extending along a first direction; Depositing a high-k dielectric layer over the interface layer; Depositing a polysilicon layer on the high-k dielectric layer, wherein the polysilicon layer extends along a second direction substantially perpendicular to the first direction; Patterning the polysilicon layer, the high-k dielectric layer, and the interface layer so that the interface layer partially extends beyond the outer edge of the high-k dielectric layer in the first direction; forming a gate spacer on the sidewall of the polysilicon layer, wherein the gate spacer is partially formed over a portion of the interface layer extending beyond an outer edge of the high-k dielectric layer; forming a plurality of source / drain features in the fin; forming a silicide layer over the plurality of source / drain features, wherein the silicide layer covers portions of the plurality of source / drain features; removing the polysilicon layer to form a trench; as well as A metal gate is formed in the trench.
12. The method for forming a semiconductor structure according to claim 11, wherein: The steps of patterning the polysilicon layer, the high-k dielectric layer and the interface layer include: forming an etching mask over a portion of the polysilicon layer; and An etching process is performed to remove the portion of the polysilicon layer that exposes the etching mask, so that the patterned polysilicon layer has an inclined sidewall.
13. The method for forming a semiconductor structure according to claim 12, wherein: The etching process selectively removes a portion of the interface layer, the high-k dielectric layer, or both.
14. The method for forming a semiconductor structure according to claim 11, wherein: The method further comprises, after depositing the high-k dielectric layer and before forming the polysilicon layer: annealing the high-k dielectric layer; depositing a titanium-containing capping layer over the annealed high-k dielectric layer; and The titanium-containing capping layer is annealed.
15. The method for forming a semiconductor structure according to claim 14, wherein: The step of removing the polysilicon layer includes removing the titanium-containing capping layer to expose the high-k dielectric layer.
16. The method for forming a semiconductor structure according to claim 11, wherein: Further including: Before removing the polysilicon layer, an interlayer dielectric layer is formed on the silicide layer.
17. A semiconductor structure, characterized in that: Include: A high dielectric constant metal gate structure is disposed above a channel region of a semiconductor layer formed above a substrate, and the high dielectric constant metal gate structure comprises: An interface layer is disposed above the semiconductor layer and has a first length along a first direction; a high-k dielectric layer disposed above the interface layer and having a second length along the first direction, wherein the second length is smaller than the first length; and a gate electrode disposed above the high-k dielectric layer and having a third length along the first direction, wherein the second length is greater than the third length, wherein the interface layer, the high-k dielectric layer and outer edges of the gate electrode form a step profile; a gate spacer having a sidewall portion contacting a sidewall of the gate electrode and a bottom portion contacting a top portion of the high-k dielectric layer and the interface layer; as well as A plurality of source / drain features are disposed in the semiconductor layer and adjacent to the high-k metal gate structure.
18. The semiconductor structure according to claim 17, wherein: Further including: A silicide layer covers the tops of the plurality of source / drain features.
19. The semiconductor structure according to claim 18, wherein: Further including: an interlayer dielectric layer disposed above the silicide layer; and A source / drain contact is formed in the interlayer dielectric layer to contact the silicide layer.
20. The semiconductor structure according to claim 17, wherein: The sidewall portion of the gate spacer is separated from the high-k dielectric layer.
21. The semiconductor structure according to claim 19, wherein: The silicide layer has a first width in a second direction, the second direction is substantially perpendicular to the first direction, the source / drain contact has a second width in the second direction, and the first width is greater than the second width.
22. The semiconductor structure according to claim 17, wherein: The distance between an outer edge of the gate electrode and an outer edge of the high-k dielectric layer is smaller than the distance between the outer edge of the gate electrode and an outer edge of the interface layer.
23. The semiconductor structure according to claim 17, wherein: Each sidewall of the gate electrode forms an acute angle with the high dielectric constant dielectric layer.
Citation Information
Patent Citations
Notched damascene planar poly / metal gate and methods thereof
US20030235943A1
Local charge and work function engineering on mosfet
US20100065925A1