A shallow trench isolation structure and a manufacturing method thereof

By introducing air pores into the shallow trench isolation structure and reducing the dielectric constant of the filling medium, the problem of interference between devices in integrated circuits is solved, and the operating speed and isolation performance of the device are improved.

CN110911345BActive Publication Date: 2024-10-15CHANGXIN MEMORY TECH INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN201811087794.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2018-09-18
Publication Date
2024-10-15
Estimated Expiration
2038-09-18

AI Technical Summary

Technical Problem

As the size of integrated circuit devices shrinks, the dielectric constant of the trench filling medium in the shallow trench isolation structure is higher, resulting in a decrease in isolation performance, increased interference between devices, and reduced operating speed.

Method used

The pores are introduced into the shallow trench isolation structure, and the pores can contain air to reduce the dielectric constant of the filling medium. A multi-layer filling dielectric structure is formed through specific process steps to enhance the isolation performance.

Benefits of technology

It effectively reduces the parasitic capacitance at shallow trench isolation, reduces interference between devices, increases device operating speed, and enhances the isolation performance of the trench.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110911345B_ABST
    Figure CN110911345B_ABST
Patent Text Reader

Abstract

The present invention provides a shallow trench isolation structure and a manufacturing method thereof, the manufacturing method comprising the following steps: providing a substrate, forming an isolation trench in the substrate to define a plurality of active areas in the substrate; forming a first filling medium on the sidewall of the isolation trench; forming a sacrificial layer on the sidewall of the first filling medium; forming a second filling medium in the remaining space in the isolation trench; removing the sacrificial layer to obtain a pore between the first filling medium and the second filling medium; forming a third filling medium on the top of the pore to seal the pore. The present invention introduces a pore in the shallow trench isolation structure, the pore may include air, and since the dielectric constant of air is only 1.0, the K value of the filling medium in the isolation trench can be effectively reduced, thereby enhancing the isolation performance of the trench, reducing the parasitic capacitance generated at the shallow trench isolation, reducing mutual interference between devices, and improving the operating speed of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of manufacturing integrated circuits and electronic components, and relates to a shallow trench isolation structure and a manufacturing method thereof. Background Art

[0002] As device size becomes smaller and smaller, the width of STI will also become smaller and smaller. Then, when there are mobile charges in the devices isolated on both sides of STI, parasitic capacitance may be generated. Since the dielectric constant of the trench filling medium in the existing shallow trench isolation structure is relatively high, the isolation performance of the channel is not ideal, which causes mutual interference between devices and reduces the operating speed of the devices.

[0003] Therefore, how to provide a shallow trench isolation structure and a manufacturing method thereof for isolation between units in an integrated circuit to reduce the dielectric constant of the trench filling medium, reduce interference between adjacent devices, and improve the isolation effect has become an important technical problem that needs to be urgently solved by technical personnel in this field. Summary of the invention

[0004] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a shallow trench isolation structure and a manufacturing method thereof, so as to solve the problem in the prior art that as the device size decreases, the shallow trench isolation width decreases accordingly, resulting in a decrease in isolation performance.

[0005] To achieve the above-mentioned object and other related objects, the present invention provides a method for manufacturing a shallow trench isolation structure, comprising the following steps:

[0006] Providing a substrate, forming isolation trenches in the substrate to define a plurality of active regions in the substrate;

[0007] forming a first filling dielectric on the sidewalls of the isolation trench;

[0008] forming a sacrificial layer on the sidewalls of the first filling medium;

[0009] forming a second filling dielectric in the remaining space in the isolation trench;

[0010] removing the sacrificial layer to obtain a pore between the first filling medium and the second filling medium;

[0011] A third filling medium is formed on the top of the pore to seal the pore.

[0012] The present invention also provides another method for manufacturing a shallow trench isolation structure, comprising the following steps:

[0013] Providing a substrate, and forming a first isolation trench in the substrate;

[0014] forming a first filling dielectric in the first isolation trench;

[0015] A word line region is defined on the substrate, and a second isolation trench is formed in the substrate, wherein the second isolation trench intersects the first isolation trench and avoids the word line region, and the first isolation trench and the second isolation trench together define a plurality of active regions in the substrate;

[0016] forming a second filling dielectric on the sidewalls of the second isolation trench;

[0017] forming a sacrificial layer on the sidewall of the second filling medium;

[0018] forming a third filling dielectric in the remaining space in the second isolation trench;

[0019] removing the sacrificial layer to obtain a pore between the second filling medium and the third filling medium;

[0020] A fourth filling medium is formed on the top of the pore to seal the pore.

[0021] Optionally, the second isolation trench is parallel to the word line region.

[0022] Optionally, the pore has a width ranging from 30 angstroms to 200 angstroms, and a height ranging from 500 angstroms to 2800 angstroms.

[0023] Optionally, the pores contain air.

[0024] Optionally, forming a first isolation trench in the substrate comprises the following steps:

[0025] forming a liner layer and a hard mask layer on the substrate in sequence from bottom to top;

[0026] forming a photoresist layer on the hard mask layer, and patterning the photoresist layer;

[0027] The hard mask layer, the liner layer and the substrate are etched using the patterned photoresist layer as a mask to obtain the first isolation trench.

[0028] Optionally, forming a second isolation trench in the substrate comprises the following steps:

[0029] forming a photoresist layer on the substrate and patterning the photoresist layer;

[0030] The first filling medium is etched using the patterned photoresist layer as a mask to obtain the second isolation trench.

[0031] Optionally, a bottom surface of the second isolation trench is flush with a bottom surface of the first isolation trench, or a bottom surface of the second isolation trench is relatively shallower than a bottom surface of the first isolation trench.

[0032] Optionally, forming the second filling dielectric on the sidewall of the second isolation trench comprises the following steps:

[0033] Depositing the second filling dielectric, wherein the second filling dielectric covers the substrate, the sidewalls of the second isolation trench, and the bottom surface of the second isolation trench;

[0034] Anisotropic etching is used to remove the second filling medium outside the second isolation trench and on the bottom surface of the second isolation trench.

[0035] Optionally, forming the sacrificial layer on the sidewall of the second filling medium comprises the following steps:

[0036] Depositing the sacrificial layer, wherein the sacrificial layer covers the substrate, the sidewalls of the second filling medium, and the bottom surface of the second isolation trench;

[0037] Anisotropic etching is used to remove the sacrificial layer outside the second isolation trench and on the bottom surface of the second isolation trench.

[0038] Optionally, the method of removing the sacrificial layer includes any one of plasma etching and wet etching.

[0039] Optionally, a method of forming the fourth filling medium includes chemical vapor deposition.

[0040] The present invention also provides a shallow trench isolation structure, comprising:

[0041] substrate;

[0042] Isolation trenches formed in the substrate to define a plurality of active regions in the substrate;

[0043] A first filling dielectric formed on the sidewalls of the isolation trench;

[0044] A second filling dielectric is formed in the middle of the isolation trench;

[0045] a pore located between the first filling medium and the second filling medium;

[0046] A third filling medium is formed on the top of the pore to seal the pore.

[0047] Optionally, the pore has a width ranging from 30 angstroms to 200 angstroms, and a height ranging from 500 angstroms to 2800 angstroms.

[0048] Optionally, the pores contain air.

[0049] The present invention also provides another shallow trench isolation structure, comprising:

[0050] A substrate having a word line region defined thereon;

[0051] a first isolation trench formed in the substrate;

[0052] a first filling dielectric formed in the first isolation trench;

[0053] a second isolation trench formed in the substrate, the second isolation trench intersecting the first isolation trench and avoiding the word line region, the first isolation trench and the second isolation trench jointly defining a plurality of active regions in the substrate;

[0054] a second filling dielectric formed on a sidewall of the second isolation trench;

[0055] a third filling dielectric formed in the middle of the second isolation trench;

[0056] a pore located between the second filling medium and the third filling medium;

[0057] A fourth filling medium is formed on the top of the pore to seal the pore.

[0058] Optionally, the second isolation trench is parallel to the word line region.

[0059] Optionally, the pore has a width ranging from 30 angstroms to 200 angstroms, and a height ranging from 500 angstroms to 2800 angstroms.

[0060] Optionally, the pores contain air.

[0061] Optionally, a bottom surface of the second isolation trench is flush with a bottom surface of the first isolation trench, or a bottom surface of the second isolation trench is relatively shallower than a bottom surface of the first isolation trench.

[0062] As described above, the shallow trench isolation structure and the manufacturing method thereof of the present invention have the following beneficial effects: the present invention introduces pores in the shallow trench isolation structure, and the pores may include air. Since the dielectric constant of air is only 1.0, the K value of the medium filled in the isolation trench can be effectively reduced, thereby enhancing the isolation performance of the trench, reducing the parasitic capacitance generated at the shallow trench isolation, reducing mutual interference between devices, and improving the operating speed of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0063] Figure 1a The cross-sectional view shows a shallow trench isolation structure in the prior art.

[0064] Figure 1b The diagram shows a planar layout of an active region, an isolation structure and a word line region in a shallow trench isolation structure in the prior art.

[0065] Figure 2a-2g It is a schematic structural diagram showing the steps of the manufacturing method of the shallow trench isolation structure of the present invention in the first embodiment.

[0066] Figure 3a-Figure 3u It is a schematic structural diagram showing the steps of the manufacturing method of the shallow trench isolation structure of the present invention in the second embodiment.

[0067] Figure 4a It is a top view of the shallow trench isolation structure of the present invention in the third embodiment.

[0068] Figure 4b Display as Figure 4a A-A' cross-sectional view.

[0069] Figure 5a Shown is a top view of the shallow trench isolation structure of the present invention in the fourth embodiment.

[0070] Figure 5b Display as Figure 5a B-B' cross-sectional view.

[0071] Figure 5c Display as Figure 5a C-C' cross-section diagram.

[0072] Component number description

[0073] 1 Substrate

[0074] 2 Isolation Structure

[0075] 3 Active region

[0076] 4 Word line area

[0077] 101 Substrate

[0078] 102 Isolation trench

[0079] 103 Active Area

[0080] 104 First filling medium

[0081] 105 Sacrificial Layer

[0082] 106 Second filling medium

[0083] 107 Porosity

[0084] 108 Third filling medium

[0085] 201 Substrate

[0086] 202 cushion layer

[0087] 203 Hard mask layer

[0088] 204 Photoresist layer

[0089] 205 Photoresist layer opening

[0090] 206 first isolation trench

[0091] 207 First filling medium

[0092] 208 photoresist layer

[0093] 209 Photoresist layer opening

[0094] 210 Second isolation trench

[0095] 211 word line area

[0096] 212 Active Area

[0097] 213 Second filling medium

[0098] 214 Sacrificial Layer

[0099] 215 Third filling medium

[0100] 216 Porosity

[0101] 217 Fourth filling medium

[0102] 301 substrate

[0103] 302 Isolation trench

[0104] 303 Active Area

[0105] 304 First filling medium

[0106] 305 Second filling medium

[0107] 306 Porosity

[0108] 307 Third filling medium

[0109] 401 substrate

[0110] 402 word line area

[0111] 403 first isolation trench

[0112] 404 First filling medium

[0113] 405 second isolation trench

[0114] 406 Active Area

[0115] 407 Second filling medium

[0116] 408 Third filling medium

[0117] 409 Porosity

[0118] 410 Fourth filling medium DETAILED DESCRIPTION

[0119] like Figure 1a As shown, it is a cross-sectional view of an existing shallow trench isolation structure, including a substrate 1 and an isolation structure 2 formed in the substrate 1, wherein the isolation structure 2 isolates a plurality of active regions 3 in the substrate 1. Figure 1b As shown, a planar layout of the active area 3, the isolation structure 2 and the word line area 4 in the existing shallow trench isolation structure is shown.

[0120] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0121] See also Figures 2a to 5c It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0122] Embodiment 1

[0123] This embodiment provides a method for manufacturing a shallow trench isolation structure, comprising the following steps:

[0124] First, execute step S101: Figure 2a As shown, a substrate 101 is provided, and isolation trenches 102 are formed in the substrate 101 to define a plurality of active regions 103 in the substrate 101 .

[0125] Specifically, the substrate 101 includes but is not limited to semiconductor substrates such as Si, Ge, SiGe, and III-V compound. The method of forming the isolation trench 102 includes but is not limited to a plasma etching process.

[0126] As an example, Figure 2b A planar layout of the active region 103 and the isolation trench 102 is shown. In other embodiments, the active region and the isolation trench may also adopt other planar layouts as required, and the protection scope of the present invention should not be excessively limited here.

[0127] Then, step S102 is performed: Figure 2c As shown, a first filling dielectric 104 is formed on the sidewalls of the isolation trench 102 .

[0128] Specifically, the first filling medium is deposited by chemical vapor deposition, physical vapor deposition, atomic layer deposition or other deposition methods, and anisotropic etching is used to remove excess first filling medium at the bottom of the isolation trench and outside the trench.

[0129] Then execute step S103: Figure 2d As shown, a sacrificial layer 105 is formed on the sidewall of the first filling medium 104 .

[0130] Specifically, the sacrificial layer is deposited by any one of chemical vapor deposition, physical vapor deposition, and atomic layer deposition or a combination thereof, and plasma anisotropic etching is used to remove the excess sacrificial layer at the bottom of the isolation trench and outside the trench.

[0131] Then execute step S104: Figure 2e As shown, a second filling dielectric 106 is formed in the remaining space in the isolation trench 102 .

[0132] Specifically, the second filling medium is deposited by any one of chemical vapor deposition, physical vapor deposition, and atomic layer deposition or a combination thereof, and excess second filling medium outside the groove is removed by chemical or physical grinding.

[0133] Then execute step S105: Figure 2f As shown, the sacrificial layer 105 is removed to obtain a pore 107 between the first filling medium 104 and the second filling medium 106 .

[0134] Specifically, the sacrificial layer is removed by plasma etching or wet etching.

[0135] Then execute step S106: Figure 2g As shown, a third filling medium 108 is formed on the top of the pore 107 to seal the pore 107 .

[0136] Specifically, the third filling medium 108 is deposited by chemical vapor deposition or other deposition methods, and the third filling medium in the peripheral area of ​​the trench is removed by chemical mechanical polishing.

[0137] The manufacturing method of the shallow trench isolation structure of the present embodiment introduces pores in all shallow trench isolation regions, and the pores may include air. Since the dielectric constant of air is only 1.0, the K value of the medium filled in the isolation trench can be effectively reduced, thereby enhancing the isolation performance of the trench, reducing the parasitic capacitance generated at the shallow trench isolation, reducing mutual interference between devices, and improving the operating speed of the device.

[0138] Embodiment 2

[0139] This embodiment provides another method for manufacturing a shallow trench isolation structure. The difference between this embodiment and the first embodiment is that in the first embodiment, pores are introduced in all shallow trench isolation areas, which is suitable for semiconductor structures in which word lines are located on a substrate, or suitable for semiconductor structures without word lines. In this embodiment, pores are introduced only in part of the shallow trench isolation areas, which is suitable for semiconductor structures using buried word lines. The pores avoid the area where the buried word lines are located, so as to avoid the pores being destroyed when the word line trenches are formed, thereby reducing the isolation effect.

[0140] The manufacturing method of the shallow trench isolation structure of this embodiment comprises the following steps:

[0141] First, execute step S201: Figure 3a-3d As shown, a substrate 201 is provided, and a first isolation trench 206 is formed in the substrate 201 .

[0142] As an example, the following specific processes are included:

[0143] like Figure 3a As shown, a liner layer 202 and a hard mask layer 203 are sequentially formed on the substrate 201 from bottom to top. The substrate 201 can be a semiconductor substrate such as Si, Ge, SiGe, or a III-V compound. The liner layer 202 includes but is not limited to a thermal oxide layer, and its thickness ranges from 5 to 20 angstroms. The thermal oxide layer is formed by a dry oxygen oxidation process, and the oxidation temperature ranges from 800 to 1100°C. The material of the hard mask layer 203 includes but is not limited to silicon nitride, and its thickness ranges from 500 to 1000 angstroms. The formation of the hard mask layer 203 includes but is not limited to chemical vapor deposition, physical vapor deposition, atomic layer deposition and other methods.

[0144] like Figure 3b As shown, a photoresist layer 204 is formed on the hard mask layer by spin coating or other methods, and the photoresist layer 204 is patterned by photolithography processes such as exposure and development to obtain a plurality of photoresist layer openings 205 .

[0145] like Figure 3c As shown, the hard mask layer 203, the liner layer 202 and the substrate 201 are etched downward using the patterned photoresist layer 204 as a mask by a plasma etching process to obtain the first isolation trench 206. The longitudinal section of the first isolation trench includes but is not limited to a rectangle. The depth of the first isolation trench is less than 4000 angstroms. In this embodiment, the depth of the first isolation trench is 3000 angstroms as an example.

[0146] As an example, Figure 3eA planar layout of the first isolation trench 206 in the substrate 201 is shown, wherein a plurality of first isolation trenches spaced from each other are formed. It should be noted that the plurality of first isolation trenches 206 are only a portion of the shallow trench isolation region to be defined, and the overall outline of the active area has not yet been presented. In this embodiment, the plurality of first isolation trenches 206 are parallel to each other. However, it should be noted that in other embodiments, when the defined active area and bit line adopt other layout methods, the layout and extension direction of the first isolation trench can also be adjusted accordingly, and the protection scope of the present invention should not be excessively limited here.

[0147] As an example, Figure 3f Another planar layout of the first isolation trench 206 in the substrate 201 is shown, wherein the first isolation trench 206 corresponds to the entire shallow trench isolation region, and at this time the overall outline of the active area 212 has been presented.

[0148] Then, step S202 is executed: Figure 3g-3h As shown, a first filling dielectric 207 is formed in the first isolation trench 206 .

[0149] As an example, the following specific processes are included:

[0150] like Figure 3g As shown, a first filling dielectric 207 is deposited in the first isolation trench 206 and on the surface of the hard mask layer 203 by chemical vapor deposition, physical vapor deposition, atomic layer deposition or other deposition methods until the first isolation trench 206 is filled. The material of the first filling dielectric 207 includes but is not limited to silicon oxide.

[0151] like Figure 3h As shown, the first filling medium 207 located on the surface of the hard mask layer 203 is removed by chemical mechanical polishing.

[0152] Then execute step S203: Figure 3i-3j As shown, the surface of the hard mask layer 203 on the substrate 201 defines a word line region 211, and a second isolation trench 210 is formed in the substrate 201. The second isolation trench 210 intersects with the first isolation trench 206 and avoids the word line region 211. The first isolation trench 206 and the second isolation trench 210 together define a plurality of active regions 212 in the substrate 201. In this embodiment, the second isolation trench 210 opens from the surface of the hard mask layer 203, penetrates the hard mask layer 203 and the liner layer 202, and extends into the substrate 201.

[0153] As an example, the following process is included:

[0154] like Figure 3i As shown, a photoresist layer 208 is formed on the surface of the hard mask layer 203 above the substrate 201 by spin coating or other methods, and the photoresist layer 208 is patterned by photolithography processes such as exposure and development to obtain a plurality of photoresist layer openings 209 .

[0155] like Figure 3j As shown, the patterned photoresist layer 208 is used as a mask and a plasma etching process is adopted to etch downward the first filling medium 207 to obtain the second isolation trench 210 .

[0156] It should be noted that if the first isolation trench 206 is Figure 3e The planar layout also includes the step of etching the substrate 201 downwards using the patterned photoresist layer 208 as a mask.

[0157] In this embodiment, the bottom surface of the second isolation trench 210 is flush with the bottom surface of the first isolation trench 206 , and the depth of the second isolation trench 210 is 3000 angstroms. In other embodiments, the bottom surface of the second isolation trench 210 may also be relatively shallower than the bottom surface of the first isolation trench 206 .

[0158] As an example, Figure 3k A planar layout of the first isolation trench 206, the second isolation trench 210 and the word line region 211 in the substrate 201 is shown. The second isolation trench 210 avoids the word line region to avoid damaging the pores subsequently formed in the second isolation trench 210 when a buried word line trench is subsequently formed.

[0159] In this embodiment, the second isolation trench 210 is parallel to the word line region 211 and is located between two columns of active regions 212. In other embodiments, the shape and arrangement of the second isolation trench 210 can also be adjusted according to the actual arrangement of active regions and word line layout, as long as the word line region is avoided, and the protection scope of the present invention should not be excessively limited here.

[0160] Then execute step S204: Figure 3l-3m As shown, a second filling dielectric 213 is formed on the sidewalls of the second isolation trench 210 .

[0161] As an example, the following specific processes are included:

[0162] like Figure 3l As shown, the second filling dielectric 213 is deposited, and the second filling dielectric 213 covers the surface of the hard mask layer 203 above the substrate 201, the sidewalls of the second isolation trench 210, and the bottom surface of the second isolation trench 210. The material of the second filling dielectric 213 includes but is not limited to silicon oxide.

[0163] like Figure 3m As shown, anisotropic etching is used to remove the bottom surface of the second isolation trench 210 and the redundant second filling medium 213 outside the second isolation trench 210 .

[0164] Then execute step S205: Figure 3n-Figure 3o As shown, a sacrificial layer 214 is formed on the sidewalls of the second filling medium 213 .

[0165] As an example, the following specific processes are included:

[0166] like Figure 3n As shown, the sacrificial layer 213 is deposited by any one or a combination of chemical vapor deposition, physical vapor deposition, and atomic layer deposition, and the sacrificial layer 213 covers the surface of the hard mask layer 203 above the substrate 201, the sidewalls of the second filling medium 213, and the bottom surface of the second isolation trench 210. The material of the sacrificial layer can be selected from a material that has a high selectivity to the second filling medium 213 or is easy to remove by a wet method. For example, when the second filling medium 213 is silicon oxide, the material of the sacrificial layer can be selected from silicon nitride, borophosphosilicate glass (BPSG), etc.

[0167] like Figure 3o As shown, plasma anisotropic etching is used to remove the bottom surface of the second isolation trench 210 and the redundant sacrificial layer 214 outside the second isolation trench 210 .

[0168] Then execute step S206: Figure 3p-Figure 3q As shown, a third filling dielectric 215 is formed in the remaining space in the second isolation trench 210 .

[0169] As an example, the following specific processes are included:

[0170] like Figure 3p As shown, the third filling medium 215 is deposited by any one or a combination of chemical vapor deposition, physical vapor deposition, and atomic layer deposition. The third filling medium 215 fills the remaining space of the second isolation trench 210 and covers the surface of the hard mask layer 203. The material of the third filling medium 215 includes but is not limited to silicon oxide.

[0171] like Figure 3q As shown, the excess third filling medium 215 on the surface of the hard mask layer 203 is removed by chemical physical grinding.

[0172] Then execute step S207: Figure 3rAs shown, the sacrificial layer 214 is removed to obtain a pore 216 between the second filling medium 213 and the third filling medium 215 .

[0173] Specifically, the sacrificial layer 214 is removed by plasma etching or wet etching.

[0174] Then execute step S201: Figure 3s-Figure 3u As shown, a fourth filling medium 217 is formed on the top of the pore 216 to seal the pore 216 .

[0175] Specifically, the following specific processes are included:

[0176] like Figure 3s As shown, the fourth filling medium 217 is deposited by chemical vapor deposition or other deposition methods. The fourth filling medium 217 quickly seals the pores 216 and covers the surface of the hard mask layer 203 .

[0177] like Figure 3t As shown, a chemical mechanical polishing process is used to remove the redundant fourth filling medium 217 on the surface of the hard mask layer 203 , and the hard mask layer 203 is used as a chemical mechanical polishing stop layer.

[0178] like Figure 3u As shown, the hard mask layer 203 above the substrate 201 is removed by dry etching process, and the liner layer 202 above the substrate 201 is removed by wet cleaning.

[0179] Specifically, after sealing, the width of the pore 216 is in the range of 30 angstroms to 200 angstroms, and the height is in the range of 500 angstroms to 2800 angstroms. The pore may contain air, and may further contain a process gas used when depositing the fourth filling medium 217 .

[0180] The manufacturing method of the shallow trench isolation structure of this embodiment introduces pores in part of the shallow trench isolation area (avoiding the word line area), and the pores may include air. Since the dielectric constant of air is only 1.0, the K value of the medium filled in the isolation trench can be effectively reduced, thereby enhancing the isolation performance of the trench, reducing the parasitic capacitance generated at the shallow trench isolation, reducing mutual interference between devices, and improving the operating speed of the device.

[0181] Embodiment 3

[0182] This embodiment provides a shallow trench isolation structure. Figure 4a and Figure 4b ,in, Figure 4a Shown is a top view of the shallow trench isolation, Figure 4b Display as Figure 4a A-A' cross-sectional view.

[0183] It can be seen that the shallow trench isolation structure includes a substrate 301, an isolation trench 302, a first filling medium 304, a second filling medium 305, a pore 306 and a third filling medium 307, wherein the isolation trench 302 is formed in the substrate 301 to define a plurality of active areas 303 in the substrate 301, the first filling medium 304 is formed on the sidewall of the isolation trench 302, the second filling medium 305 is formed in the middle of the isolation trench 302, the pore 306 is located between the first filling medium 304 and the second filling medium 305, and the third filling medium 307 is formed on the top of the pore 306 to seal the pore 306.

[0184] Specifically, the substrate includes but is not limited to semiconductor substrates such as Si, Ge, SiGe, and III-V compounds. The depth of the isolation trench is less than 4000 angstroms. In this embodiment, the depth of the isolation trench is 3000 angstroms. The materials of the first filling medium, the second filling medium, and the third filling medium include but are not limited to silicon oxide.

[0185] Specifically, after sealing, the width of the pore 306 is in the range of 30 angstroms to 200 angstroms, and the height is in the range of 500 angstroms to 2800 angstroms. The pore may contain air, and may further contain a process gas used when depositing the third filling medium 307 .

[0186] The shallow trench isolation structure of this embodiment introduces pores in all shallow trench isolation areas, and the pores may include air. Since the dielectric constant of air is only 1.0, the K value of the medium filled in the isolation trench can be effectively reduced, thereby enhancing the isolation performance of the trench, reducing the parasitic capacitance generated at the shallow trench isolation, reducing mutual interference between devices, and improving the operating speed of the device.

[0187] Embodiment 4

[0188] Another shallow trench isolation structure is provided in the present embodiment. The difference between the present embodiment and the third embodiment is that in the third embodiment, pores are introduced in all shallow trench isolation areas, which is suitable for semiconductor structures in which word lines are located on substrates, or suitable for semiconductor structures without word lines. In the present embodiment, pores are introduced only in part of the shallow trench isolation areas, which is suitable for semiconductor structures using buried word lines. The pores avoid the area where the buried word lines are located, thereby preventing the word line trenches from destroying the pores and reducing the isolation effect.

[0189] See also Figure 5a-5c ,in, Figure 5a The top view of the shallow trench isolation structure of this embodiment is shown. Figure 5b Display as Figure 5a The B-B' cross-section diagram, Figure 5c Display as Figure 5a C-C' cross-section diagram.

[0190] It can be seen that the shallow trench isolation structure includes a substrate 401, a first isolation trench 403, a first filling medium 404, a second isolation trench 405, a second filling medium 407, a third filling medium 408, a pore 409 and a fourth filling medium 410, wherein the first isolation trench 403 and the second isolation trench 405 are both formed in the substrate 401, and the second isolation trench 405 intersects with the first isolation trench 403, and the first isolation trench 403 and the second isolation trench 405 jointly define a plurality of active areas 406 in the substrate 401.

[0191] Specifically, the substrate includes but is not limited to semiconductor substrates such as Si, Ge, SiGe, and III-V compounds. The depths of the first isolation trench and the second isolation trench are both less than 4000 angstroms. The bottom surface of the second isolation trench can be flush with the bottom surface of the first isolation trench, or can be relatively shallower than the bottom surface of the first isolation trench. In this embodiment, the depths of the first isolation trench and the second isolation trench are both 3000 angstroms. The materials of the first filling medium, the second filling medium, the third filling medium, and the fourth filling medium include but are not limited to silicon oxide.

[0192] Specifically, a word line region 402 is defined on the substrate 401, and the second isolation trench 405 avoids the word line region 402. The first filling medium 404 is formed in the first isolation trench 403, the second filling medium 407 is formed on the sidewall of the second isolation trench 405, the third filling medium 408 is formed in the middle of the second isolation trench 405, the pore 409 is located between the second filling medium 407 and the third filling medium, and the fourth filling medium 410 is formed on the top of the pore 409 to seal the pore 409.

[0193] As an example, the second isolation trench 405 is parallel to the word line region 402. After sealing, the width of the pore 409 ranges from 30 angstroms to 200 angstroms, and the height ranges from 500 angstroms to 2800 angstroms. The pore may contain air, and may further contain a process gas used when depositing the fourth filling dielectric 410.

[0194] The shallow trench isolation structure of this embodiment introduces pores in part of the shallow trench isolation area (avoiding the word line area), and the pores may include air. Since the dielectric constant of air is only 1.0, the K value of the medium filled in the isolation trench can be effectively reduced, thereby enhancing the isolation performance of the trench, reducing the parasitic capacitance generated at the shallow trench isolation, reducing mutual interference between devices, and improving the operating speed of the device.

[0195] In summary, the shallow trench isolation structure and the manufacturing method thereof of the present invention introduce pores in the shallow trench isolation structure, and the pores may include air. Since the dielectric constant of air is only 1.0, the K value of the medium filled in the isolation trench can be effectively reduced, thereby enhancing the isolation performance of the trench, reducing the parasitic capacitance generated at the shallow trench isolation, reducing mutual interference between devices, and improving the operating speed of the device. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.

[0196] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for manufacturing a shallow trench isolation structure, characterized in that: The following steps are involved: Providing a substrate, and forming a first isolation trench in the substrate; forming a first filling dielectric in the first isolation trench; A word line region is defined on the substrate, and a second isolation trench is formed in the substrate, wherein the second isolation trench intersects the first isolation trench and avoids the word line region, and the first isolation trench and the second isolation trench together define a plurality of active regions in the substrate; forming a second filling dielectric on the sidewalls of the second isolation trench; forming a sacrificial layer on the sidewall of the second filling medium; forming a third filling dielectric in the remaining space in the second isolation trench; removing the sacrificial layer to obtain a pore between the second filling medium and the third filling medium; A fourth filling medium is formed on the top of the pore to seal the pore.

2. The method for manufacturing a shallow trench isolation structure according to claim 1, characterized in that: The second isolation trench is parallel to the word line region.

3. The method for manufacturing a shallow trench isolation structure according to claim 1, characterized in that: The width of the pores ranges from 30 angstroms to 200 angstroms, and the height ranges from 500 angstroms to 2800 angstroms, and the pores contain air.

4. The method for manufacturing a shallow trench isolation structure according to claim 1, characterized in that: Forming a first isolation trench in the substrate comprises the following steps: forming a liner layer and a hard mask layer on the substrate in sequence from bottom to top; forming a photoresist layer on the hard mask layer, and patterning the photoresist layer; The hard mask layer, the liner layer and the substrate are etched using the patterned photoresist layer as a mask to obtain the first isolation trench.

5. The method for manufacturing a shallow trench isolation structure according to claim 1, characterized in that: Forming a second isolation trench in the substrate comprises the following steps: forming a photoresist layer on the substrate and patterning the photoresist layer; The first filling medium is etched using the patterned photoresist layer as a mask to obtain the second isolation trench.

6. The method for manufacturing a shallow trench isolation structure according to claim 1, characterized in that: Forming the second filling dielectric on the sidewall of the second isolation trench comprises the following steps: Depositing the second filling dielectric, wherein the second filling dielectric covers the substrate, the sidewalls of the second isolation trench, and the bottom surface of the second isolation trench; Anisotropic etching is used to remove the second filling medium outside the second isolation trench and on the bottom surface of the second isolation trench.

7. The method for manufacturing a shallow trench isolation structure according to claim 1, characterized in that: Forming the sacrificial layer on the sidewall of the second filling medium comprises the following steps: Depositing the sacrificial layer, wherein the sacrificial layer covers the substrate, the sidewalls of the second filling medium, and the bottom surface of the second isolation trench; Anisotropic etching is used to remove the sacrificial layer outside the second isolation trench and on the bottom surface of the second isolation trench.

8. A shallow trench isolation structure, characterized in that: include: A substrate having a word line region defined thereon; a first isolation trench formed in the substrate; a first filling dielectric formed in the first isolation trench; a second isolation trench formed in the substrate, the second isolation trench intersecting the first isolation trench and avoiding the word line region, the first isolation trench and the second isolation trench jointly defining a plurality of active regions in the substrate; a second filling dielectric formed on a sidewall of the second isolation trench; a third filling dielectric formed in the middle of the second isolation trench; a pore located between the second filling medium and the third filling medium; a fourth filling medium formed on the top of the pore to seal the pore; The depths of the first isolation trench and the second isolation trench are both less than 4000 angstroms.

9. The shallow trench isolation structure according to claim 8, characterized in that: The second isolation trench is parallel to the word line region.

10. The shallow trench isolation structure according to claim 8, characterized in that: The width of the pores ranges from 30 angstroms to 200 angstroms, and the height ranges from 500 angstroms to 2800 angstroms, and the pores contain air.

11. The shallow trench isolation structure according to claim 8, characterized in that: The bottom surface of the second isolation trench is flush with the bottom surface of the first isolation trench, or the bottom surface of the second isolation trench is relatively shallower than the bottom surface of the first isolation trench.

Citation Information

Patent Citations

  • Shallow trench isolating structure having an air gap, a cmos image sensor employing the same, and a production method therefor

    CN102138210A

  • Shallow trench isolation structure

    CN208923085U

  • Method of manufacturing trench and trench insemiconductor

    KR1020040055354A

  • Method and structure for relieving transistor performance degradation due to shallow trench isolation induced stress

    US20090206442A1

  • Semiconductor device having a shallow trench isolation structure and methods of forming the same

    US20160148833A1