A hot wire support for preparing large-size diamond films by hot wire chemical vapor deposition

By designing a hot wire stent containing a molybdenum block and a high-temperature spring, the problem of hot wire expansion, bending and breakage at high temperatures is solved, and stable and uniform growth of large-area diamond films is achieved, which is suitable for the preparation of large-size diamond films.

CN110938810BActive Publication Date: 2024-10-01HANGZHOU RUIQING ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201911375199.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-12-27
Publication Date
2024-10-01
Estimated Expiration
2039-12-27

AI Technical Summary

Technical Problem

When the existing hot wire chemical vapor deposition method is used to prepare large-area diamond films, the expansion and bending of the hot wire causes uneven temperature fields, making it difficult to prepare large-sized diamond films. In addition, the deformation of the spring at high temperatures causes the hot wire to break or not be fully stretched, resulting in The experiment failed.

Method used

A hot wire holder including an upper molybdenum electrode, a lower molybdenum electrode, a ceramic tube, a molybdenum round rod, a molybdenum block, an insulating baffle, a molybdenum screw and a high-temperature spring is designed. The gravity of the molybdenum block is used to keep the hot wire straight and the high-temperature spring Relieve the stress on the hot wire and ensure that the hot wire does not break at high temperatures.

Benefits of technology

The gravity of the molybdenum block maintains the flat surface of the hot wire, and the high-temperature spring relieves the stress on the hot wire and avoids breakage of the hot wire. It achieves stable and uniform growth of large-area diamond films, prolongs the life of the hot wire, and is suitable for the preparation of large-size diamond films.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110938810B_ABST
    Figure CN110938810B_ABST
Patent Text Reader

Abstract

The present invention relates to a hot wire bracket for preparing large-size diamond films by hot wire chemical vapor deposition. The hot wire bracket comprises an upper molybdenum electrode 1, a lower molybdenum electrode 2, a ceramic tube 3, a hot wire 4, a molybdenum round rod 5, a self-weight molybdenum block 6, an insulating baffle 7, a molybdenum screw 8 and a high-temperature lightweight spring 9. The hot wire is mounted on the bracket and the entire bracket is vertically placed in a vacuum chamber, and then the upper and lower molybdenum electrodes are connected to the copper electrode column 14 behind the insulating baffle. The present invention effectively overcomes the problems of uneven thickness and quality caused by easy brittle fracture and bending deformation of the hot wire when preparing diamond films by hot wire chemical vapor deposition.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of diamond film preparation, and in particular to a hot wire bracket used for preparing large-size diamond films by hot wire chemical vapor deposition. Background Art

[0002] Diamond has the highest hardness among all materials, the highest thermal conductivity at room temperature, extremely low thermal expansion coefficient, high chemical inertness, large bandgap, highest sound propagation rate, and high transparency from far infrared to deep ultraviolet. These excellent properties make diamond have broad application prospects and can be widely used in the fields of automobiles, aerospace, tools, optics, high-temperature electronics, etc. It is a new functional material in the 21st century. The bandgap of diamond is 5.45eV, and it can work at 600℃, while silicon fails at 170℃, so diamond is an ideal material for making high-temperature electronic devices. The optical absorption of diamond is around 0.22μm, which is equivalent to the vacuum ultraviolet band. From this position to the millimeter wave band, there is no absorption peak except for the weak absorption peak (absorption coefficient ~12.3cm-1) caused by double phonon absorption near ~5μm. Therefore, the transmittance and hardness of diamond allow it to be used as an optical device. Depositing a layer of diamond film on the surface of cemented carbide tools not only greatly extends the service life of the tools, but also significantly improves the processing quality. In addition, diamond film electrodes have a wide potential window, small background current, high chemical stability, and can quickly electrochemically oxidize and decompose organic matter in sewage. However, at present, the preparation of diamond film electrodes in my country is still at the small-scale stage in the laboratory, and it is difficult to apply them on a large scale in the fields of automobiles, aerospace, cutting tools, optics, high-temperature electronics, etc., especially in the application of treating industrial wastewater with a volume of tens or hundreds of tons.

[0003] Hot wire chemical vapor deposition is an effective method for preparing large-sized diamond films. However, the use of this method to prepare large-area diamond films requires a reasonable hot wire support. After the horizontally arranged hot wire is powered on and heated, the hot wire will expand, bend, and sag, thereby changing the distance between the hot wire and the substrate, causing an uneven temperature field, and it is difficult to prepare a large-area diamond film. Chinese patent (CN 202643836 U) discloses an invention: the support includes left and right molybdenum electrodes, a grooved pin, a spring frame, etc. Each hot wire is controlled by a spring to achieve straightness. However, the spring is directly connected to the hot wire. Since the temperature of the hot wire is as high as 2000°C or more, the elastic properties of the spring are easily changed at high temperatures, the stress of the spring changes, or loses elasticity, or becomes hard, and the hot wire is easily brittle after heating. Therefore, when preparing diamond films, the stress change of the spring is easy to cause the hot wire to break, or the hot wire is not fully stretched, resulting in experimental failure. Summary of the invention

[0004] The present invention provides a hot wire support for preparing large-sized diamond films by hot wire chemical vapor deposition. The invention overcomes some technical defects in the prior art, improves the stability and uniformity of the hot wire, is suitable for preparing large-area diamond films by hot wire chemical vapor deposition, and has broad application prospects.

[0005] The technical solution of the present invention is as follows:

[0006] A hot wire bracket for preparing large-sized diamond films by hot wire chemical vapor deposition, comprising an upper molybdenum electrode 1, a lower molybdenum electrode 2, a ceramic tube 3, a hot wire 4 of equal length, a molybdenum round rod 5, a molybdenum block 6, an insulating baffle 7, a molybdenum screw 8 and a high-temperature spring 9. The upper molybdenum electrode 1 and the lower molybdenum electrode 2 are connected and fixed by two molybdenum round rods 5; the molybdenum round rod 5 is separated from the upper molybdenum electrode 1 by insulating ceramic, and is directly connected to the lower molybdenum electrode; the upper molybdenum electrode 1 is provided with screw holes arranged at equal intervals between the two molybdenum round rods 5, and the direction of the screw holes is perpendicular to the axial direction of the upper molybdenum electrode 1; the molybdenum block 6 is provided with screw holes corresponding to the threaded holes on one side of the upper electrode 1, and circular holes with the same outer diameter as the molybdenum round rod 5 are provided at both ends, and the opening directions of the circular holes and the screw holes are consistent and perpendicular to the axial direction of the molybdenum block 6; the molybdenum block 6 is sleeved on the molybdenum round rod 5 through the circular hole, and is positioned Between the upper molybdenum electrode 1 and the lower molybdenum electrode 2; the hot wires 4 of equal length are fixed to the screw hole of the molybdenum electrode 1 at one end and the screw hole of the molybdenum block 6 at the other end through the molybdenum screw 8, and are vertically arranged between the upper molybdenum electrode 1 and the molybdenum block 6 at equal intervals, and all the hot wires 4 are on the same plane; the high-temperature spring 9 is sleeved on the molybdenum round rod 5 and arranged between the molybdenum block 6 and the lower molybdenum electrode 2; the ceramic tube 3 is sleeved on the other end of the upper molybdenum electrode 1 and the lower molybdenum electrode 2, and vertically passes through the insulation baffle 7 together with the upper molybdenum electrode 1 and the lower molybdenum electrode 2, and the length is greater than the width of the entire insulation baffle 7. The entire hot wire bracket is vertically arranged in the reaction chamber from the upper molybdenum electrode 1 to the lower molybdenum electrode 2.

[0007] In the above technical solution, the upper molybdenum electrode 1, the lower molybdenum electrode 2 and the molybdenum block 6 are all long strips. The upper molybdenum electrode and the lower molybdenum electrode are provided with threaded holes for connecting copper cables at the bottom of one end passing through the insulating baffle 7; the high-temperature spring 9 is a lightweight spring that can be compressed by the molybdenum block 6; the insulating baffle 7 can be one or more ceramic plates or stainless steel plates. When there are multiple insulating baffles 7, they are separated by a certain interval and fixed in sequence. The molybdenum round rod 5 is vertically connected to the upper molybdenum electrode 1 and the lower molybdenum electrode 2. Graphite powder is used to lubricate the molybdenum round rod 5 and the molybdenum block 6 to ensure that the molybdenum block 6 can not only have good contact with the molybdenum round rod 5, but also can slide smoothly downward along the round rod 5. The diameter of the molybdenum round rod 5 is more than 3mm. The cross-sectional area of ​​the upper molybdenum electrode 1, the lower molybdenum electrode 2 and the molybdenum block 6 is 36mm 2 above.

[0008] The beneficial effects of the present invention are as follows:

[0009] 1. The gravity of the molybdenum block is used to straighten the hot wires when they are deformed by heat, and all the hot wires are always kept in the same plane.

[0010] 2. Because the molybdenum round rod and molybdenum block are at a temperature of more than 3000℃ and are large in size, they do not deform during the heating process, ensuring that the molybdenum block can slide smoothly along the molybdenum round rod and have good contact with the molybdenum round rod.

[0011] 3. Since a high-temperature lightweight spring is placed between the molybdenum block electrode and the lower molybdenum electrode, the high-temperature lightweight spring can relieve the force on the hot wire at high temperatures, which can effectively avoid the hot wire from breaking due to excessive gravity of the molybdenum block at high temperatures, thereby ensuring the life of the hot wire.

[0012] 4. The number of hot wires can be changed to achieve large-area preparation of diamond films. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 This is a front view of the hot wire bracket.

[0014] Figure 2 A three-dimensional diagram of the hot wire bracket.

[0015] Figure 3 This is a partial enlarged view of the bottom of the molybdenum electrode after passing through the insulating baffle.

[0016] Figure 4 Schematic diagram of the hot wire chemical vapor deposition system structure.

[0017] Reference numerals in the figure: 1. upper molybdenum electrode, 2. lower molybdenum electrode, 3. ceramic tube, 4. hot wire, 5. molybdenum round rod, 6. molybdenum block, 7. insulation baffle, 8. molybdenum screw, 9. high temperature spring, 10. power supply, 11. vacuum system, 12. sample stage, 13. vacuum chamber, 14. gas cylinder, 15 copper electrode support. DETAILED DESCRIPTION

[0018] The invention provides a hot wire support for stably preparing diamond films over a large area, which mainly comprises an upper molybdenum electrode, a lower molybdenum electrode, a ceramic tube, a hot wire, a molybdenum round rod, a molybdenum block, an insulating baffle, a molybdenum screw and a high-temperature spring.

[0019] The bracket is first installed outside the reaction chamber, and then the whole is placed in the reaction chamber. First, the upper molybdenum electrode 1 is connected to the two molybdenum round rods 5, separated by insulating ceramics, so that the upper molybdenum electrode 1 and the molybdenum round rods 5 are not conductive; the molybdenum block 6 is sleeved on the molybdenum round rods 5 through the round holes at both ends; then, the high-temperature spring 9 is sleeved on the molybdenum round rods 5 and is located under the molybdenum block 6; another molybdenum round rod 5 is directly connected to the lower molybdenum electrode 2. At this time, the upper molybdenum electrode 1 and the lower molybdenum electrode 2 are fixed through the molybdenum round rod 5. The ends of the hot wires 4 of equal length are fixed to the screw holes of the upper molybdenum electrode through the molybdenum screws 8, and the other ends are also fixed to the screw holes on the molybdenum block 6 opposite to the screw holes of the upper molybdenum electrode 1 through the molybdenum screws 8. Since the distribution rules of the screw holes on the upper molybdenum electrode 1 and the molybdenum block 6 are the same, they are arranged at equal intervals. Therefore, all the hot wires are distributed in parallel with equal intervals. The lengths of all hot wires are set so that the molybdenum block 6 can just compress the high-temperature spring 9. Afterwards, the ceramic tube 3 is sleeved on the upper molybdenum electrode 1 and the lower molybdenum electrode 2, and passes through the heat-insulating baffle 7 together, and the length of the ceramic tube is greater than the width of the entire heat-insulating baffle 7. If the number of the heat-insulating baffles 7 is greater than 1, the baffles are spaced at a certain interval and fixed in sequence.

[0020] After the entire electrode holder is installed, it is placed vertically from top to bottom into the reaction chamber, and the upper molybdenum electrode 1 and the lower molybdenum electrode 2 are connected to the copper electrode support 15. After that, the reaction chamber is closed and the preparation experiment is started. After power is turned on, the hot wire 4 heats up, and the temperature rises above 2000°C. The hot wire becomes soft, but due to the gravity of the molybdenum block 6 pulling it downward, the hot wire is straightened, and the high-temperature spring under the molybdenum block is also slightly compressed. Therefore, the high-temperature spring prevents the molybdenum block 6 from excessively stretching the hot wire 4 and causing it to break. Subsequently, the sample stage is adjusted so that the distance between the sample and the hot wire is 5-10mm. The molybdenum block 6 slides along the molybdenum round rod 5, which ensures the vertical position of the molybdenum block 6 and also ensures that all the hot wires can remain in the same plane. Therefore, even if the diamond film is deposited for a long time, the hot wire 4 can remain in the same plane, and the distance between the sample and the hot wire remains unchanged, so that a large area of ​​uniform growth of diamond film can be achieved.

Claims

1. A hot wire support for preparing large-size diamond films by hot wire chemical vapor deposition, comprising an upper molybdenum electrode (1), a lower molybdenum electrode (2), a ceramic tube (3), a hot wire (4), a molybdenum round rod (5), a self-weight molybdenum block (6), an insulating baffle (7), a molybdenum screw (8) and a high-temperature spring (9), characterized in that The upper molybdenum electrode (1) and the lower molybdenum electrode (2) are connected and fixed via a molybdenum round rod (5); The molybdenum round rod (5) is separated from the upper molybdenum electrode (1) by insulating ceramics and is directly connected to the lower molybdenum electrode (2); Screw holes are arranged at equal intervals on one side of the upper molybdenum electrode (1), and the direction of the screw holes is perpendicular to the axial direction of the upper molybdenum electrode (1); threaded holes corresponding to the screw holes on one side of the upper molybdenum electrode (1) are provided on the self-weight molybdenum block (6), and circular holes with the same outer diameter as the molybdenum round rod (5) are provided at both ends, and the block is sleeved on the molybdenum round rod (5) through the circular holes and is located between the upper molybdenum electrode (1) and the lower molybdenum electrode (2); The high temperature spring (9) is sleeved on the molybdenum round rod and arranged between the self-weight molybdenum block (6) and the lower molybdenum electrode (2); The ceramic tube (3) is sleeved on the other ends of the upper molybdenum electrode (1) and the lower molybdenum electrode (2), and passes through the heat-insulating baffle (7) together with the upper molybdenum electrode (1) and the lower molybdenum electrode (2).

2. A hot wire support for preparing large-size diamond films by hot wire chemical vapor deposition according to claim (1), characterized in that: The high temperature spring is a light spring that can be compressed by the self-weight molybdenum block (6).

3. A hot wire support for preparing large-size diamond films by hot wire chemical vapor deposition according to claim (1), characterized in that: The upper molybdenum electrode (1) and the lower molybdenum electrode (2) passing through the bottom of one end of the heat-insulating baffle (7) are provided with screw holes for connecting copper cables.