Methods of shielding system-in-package components from electromagnetic interference
By using a single lamination process and a self-supporting EMI shielding film in system-level packaging, the problem in the existing technology that EMI shielding is difficult to apply uniformly in high aspect ratio trenches is solved, achieving high-quality shielding and cost reduction, and improving Improved design flexibility and performance of electronic devices.
Patent Information
- Application Number
- CN201980011103.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-02-01
- Filing Date
- 2019-02-01
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2039-02-01
AI Technical Summary
Existing EMI shielding methods are difficult to apply uniformly in high aspect ratio trenches in system-level packaging, resulting in some areas not being fully shielded, and the process is complex and time-consuming, limiting the size reduction and cost control of electronic devices.
A self-supporting EMI shielding film is used in a system-level package using a single lamination process, vacuum laminated on the insulation layer and in the trench to form a continuous shielding layer, using a self-supporting preform to flow and cure at 20-250°C , fills the trench and covers the outer surface of the insulation layer to achieve high-quality shielding.
The production process is simplified, costs are reduced, high-quality shielding within high-aspect ratio trenches is achieved, electromagnetic interference is reduced, and the design and performance of electronic devices are optimized.
Smart Images

Figure CN111684590B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates generally to electromagnetic interference (EMI) shielding of electronic packages, and more particularly to EMI shielding films and methods of applying EMI shielding films to segmented system-in-package (SIP) electronic packages. Background Art
[0002] There is a continuing demand for electronic devices, especially mobile computing devices such as smart phones and tablets, with increased functionality and reduced size. However, such devices often include circuits that require electromagnetic shielding. For example, some devices include radio frequency transceiver circuits that are susceptible to radio frequency interference. Clock signals are another example of a source of radio frequency interference. For the purposes of this article, the term "electromagnetic interference" (EMI) is intended to include broadband waveform signals, including radio frequency (RF) signals, and other frequency signals emitted from components in electronic devices or from other sources.
[0003] Electromagnetic shielding is often used to reduce EMI to the operation of components within electronic devices. Currently, EMI shielding can be formed by a metal shield or conductive paste between circuits. The conductive properties of the shield or conductive paste are used to mitigate electromagnetic signal transmission in order to minimize electromagnetic interference to the operation of electronic components. However, conventional EMI shielding solutions have limitations on the reduction of package size, and therefore limit the ability of electronic device designers to reduce form factor size in response to user preferences.
[0004] A particularly beneficial application of EMI shielding is between segmented components or groups of components in a system-in-package. Components and groups of components may be segmented in a SIP for a variety of reasons, and may be placed on a substrate accordingly as predefined functional "modules," wherein the segmented portions of the SIP perform specific functions of the system. The segmented portions of the SIP are typically physically separated by gaps or grooves formed in a dielectric overmolding. The segmented portions of the SIP may be ideally shielded from EMI generated by different portions of the SIP. Therefore, EMI shielding is typically provided around each segmented portion and throughout the SIP, including within the segmented grooves.
[0005] While striving to reduce the overall system size, designers have sought to reduce the groove width. However, with typical groove widths currently in the range of 10-100 μm, it may be difficult to cover the groove surface with EMI shielding material. Conventional methods of EMI shielding are to coat the EMI material in the groove and around the outer surface of the overmolded dielectric, combined with printing a conductive paste and sputtering, plating or spraying the metal around the outer surface of the overmolded dielectric material. An exemplary conventional process includes jet printing a curable liquid fill material into the groove, then curing the material and cleaning the outer surface of the overmolded dielectric to then receive the deposited metal layer as a conformal coating around the outer surface of the overmolded dielectric. This method is complex and expensive due to the two-step process used to produce the EMI shielding, and is time consuming due to the slow jet filling process and metal deposition process.
[0006] Another conventional method includes printing a liquid paste material into the trench and around the outer surface of the dielectric layer. However, applicants have found that EMI shielding paste is difficult to apply uniformly along the trench surface, especially for very high aspect ratio (high depth, small width) trench designs. As a result, it is difficult to avoid areas in the trench that are not adequately shielded.
[0007] It is therefore an object of the present invention to provide an EMI shielding application method that eliminates multiple steps in conventional methods, thereby accelerating production throughput and reducing costs associated with the controlled environment of metal vapor deposition.
[0008] Another object of the present invention is to provide an EMI shielding application method that facilitates high quality and thorough coating of EMI shielding material on the surface of a SIP, including within high aspect ratio grooves that separate portions of the SIP. Summary of the invention
[0009] By means of the present invention, an EMI shielding film can be applied to a system-in-package (SIP) assembly in a single lamination process. A conductive film suitable for EMI shielding is vacuum laminated on an insulating layer and substantially fills a groove formed in the insulating layer to produce a continuous EMI shield both above the package and between segmented portions of the package. The SIP assembly includes a substrate; a plurality of component modules mounted on the substrate, wherein each component module includes one or more components; an insulator covering the components on the substrate; and grooves formed in the insulator and located between adjacent component modules. The maximum width of the groove is 10-100 μm.
[0010] In some embodiments, a self-supporting shielding preform is provided, which has a tensile modulus of less than 1 GPa at an operating temperature of 20-250° C. The self-supporting preform can be heated to a flowable state and vacuum laminated on the outer surface of the insulator and in the grooves to form a coating that can substantially fill the grooves and cover the outer surface of the insulator. The coating can then be cured to a tensile modulus of at least 50 MPa.
[0011] In some embodiments, a method for forming a SIP component includes: providing a substrate having a conductive ground plane spaced apart from an active surface of the substrate; and a conductive trace extending from the ground plane to the active surface. A plurality of component modules are mounted on the active surface of the substrate to form an assembly surface of the substrate, wherein each component module includes one or more components. The mounted component modules can then be encapsulated in an insulating layer extending between the assembly surface and the outer surface. Grooves are formed between adjacent component modules and through the dielectric layer to the traces, the maximum width of the grooves being 10-100 μm. A self-supporting preformed shielding film is then vacuum laminated on the outer surface of the dielectric layer and in the grooves to form a coating that substantially fills the grooves and covers the outer surface of the dielectric layer. The self-supporting preformed shielding film exhibits a tensile modulus of less than 1 GPa at an operating temperature of 20-250°C. The shielding film may also exhibit a volume resistivity of less than 0.1 Ω*cm.
[0012] The coating can be pressed onto the outer surface of the dielectric layer and / or into one or more grooves with a force of at least 50 psi. Pressing can be performed before, simultaneously with, or after any curing step required for the coating. If desired, the coating can be cured to a tensile modulus of at least 50 MPa.
[0013] A plurality of SIP devices may be singulated from an assembly by cutting through the substrate and dielectric layers. One or more such singulated SIP devices may be mounted on a carrier for use in an electronic device, such as a mobile device. One or more components of the SIP device may include at least one processor, and the SIP device includes at least one of the grooves that divide at least two component modules. The coating that substantially fills the groove preferably reduces and / or reflects electromagnetic interference by at least 10 db. A mobile device including the SIP device may include a receiver for receiving wireless data and a transmitter for transmitting wireless data. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 is a schematic diagram of a portable electronic device including a system-in-package assembly.
[0015] Figure 2 yes Figure 1 Schematic end view of the system-in-package assembly shown.
[0016] Figure 3 is a cross-sectional view of a system-level package assembly.
[0017] Figure 4 is a cross-sectional view of a system-in-package assembly having a trench formed in a dielectric layer.
[0018] Figure 5 is a diagram of an EMI shielding film and a system-in-package assembly.
[0019] Figure 6 is a cross-sectional view of an EMI shielding film laminated to a system-in-package assembly.
[0020] Fig. 6A is a cross-sectional view of an EMI shielding film laminated to a system-in-package assembly.
[0021] Fig. 7A is a cross-sectional view of an EMI shielding film and a deflated pressure bladder placed at a system-level package assembly.
[0022] Figure 7B is a cross-sectional view of an EMI shielding film laminated and pressed at a system-level package assembly by an inflated pressure bladder.
[0023] Figure 7C is a cross-sectional view of an EMI shielding film laminated and pressed at a system-level package assembly.
[0024] Figure 8 is a flow chart for forming a system-in-package assembly with an EMI shielding film.
[0025] Fig. 9 It is a cross-sectional view of a component array mounted on a substrate and divided into a plurality of component modules.
[0026] Fig.10 It is laminated with EMI shielding film Fig. 9 A cross-sectional view of the array shown in .
[0027] Fig.11 is from Fig.10 A cross-sectional view of a plurality of system-in-package devices singulated in an array is shown.
[0028] Fig.12 It is a cross-sectional view of a component mounted on a substrate and divided into a plurality of component modules.
[0029] Fig.13 It is installed on the carrier Fig.12 Cross-sectional view of a subarray device.
[0030] Fig.14 yes Fig.13 A cross-sectional view of multiple sub-array devices with EMI shielding films laminated thereon is shown.
[0031] Fig.15 is a cross-sectional view of a singulated system package device.
[0032] Fig.16 is a schematic diagram of a mobile device including the system-in-package device of the present invention. DETAILED DESCRIPTION
[0033] The above-listed objects and advantages and other objects, features and advancements given by the present invention will now be presented with respect to the detailed embodiments described with reference to the accompanying drawings, which are intended to represent various possible configurations of the present invention. It is believed that other embodiments and aspects of the present invention are within the grasp of ordinary technicians in the field.
[0034] Unless apparent or otherwise indicated, directional statements such as "upper," "lower," "inner," "outer," "top," "bottom," "vertical," "horizontal," "upward," "downward," "above," "below," etc. are intended to be relative to the orientation of the specific embodiments of the invention as shown in the figures. Additionally, given reference numerals in the figures indicate the same or similar structures when they appear in different figures, and similar reference numerals identify similar structural elements and / or features of the invention.
[0035] Embodiments of the present disclosure describe electromagnetic interference (EMI) shielding methods and configurations. The shielding structure of the present invention mitigates EMI in electrical, mechanical and other components and subsystems in electronic devices including system-in-package (SIP) assemblies. A single package represented by a SIP may include multiple components mounted on a substrate. An exemplary arrangement includes both passive and active components mounted on a printed circuit board (PCB), which is formed of conventional PCB materials such as epoxy resin filled with glass fiber. It should be understood that SIP assemblies can be used in electronic devices, such as portable electronic devices, including cellular phones, tablets, computers, watches, etc.
[0036] Figure 1 An exemplary portable electronic device, such as a mobile device 10, is shown having a housing 12 and a SIP assembly 14 without any overmolded dielectric. The SIP assembly 14 includes a substrate 16 (such as a PCB) and a plurality of components 20-28 mounted on the substrate 16. The components 20-28 may include active components such as processors, integrated circuits, wireless transceivers, receivers, and transmitters, as well as passive components such as resistors and capacitors. Figure 1As shown, the plurality of components 20-28 can be theoretically divided into at least component modules 30-32, which are shown by dashed lines 33, 34. Components 20-28 can be grouped into different modules based on their functionality, wherein components 20-22 are included in component module 30, components 25-28 are included in component module 31, and components 23, 24 are included in component module 32. It may be preferred to shield the components of one module from the components of another module, without which harmful EMI may affect the performance of the corresponding components. For example, the wireless communication integrated circuit 22 may be located in the component module 30 to shield it from signals emitted by, for example, the component 25 in the component module 31.
[0037] Figure 2 1 is a schematic end view of the SIP assembly 14. Schematic components 20a, 20b are mounted on the substrate 16 and are encapsulated in a dielectric layer 18 formed of an overmolded dielectric material. A plurality of component modules 30-32 on the substrate 16 form an assembly surface 35 of the substrate 16. The assembly surface 35 extends along the surface of the substrate 16 and around the components of the component modules 30-32. The insulation layer 18 can encapsulate the assembly surface 35, wherein the insulation layer 18 extends between the assembly surface 35 and the outer surface 19.
[0038] Insulation layer 18 may be formed from a variety of materials, such as epoxy, or generally thermosetting materials, thermoplastic materials, or other materials that may be used to electrically insulate assembly surface 35. In some embodiments, insulation layer 18 may be formed from a material that is both electrically insulating and thermally conductive to facilitate heat transfer away from components 20-28. In some embodiments, insulation layer 18 may be referred to as a dielectric or dielectric layer.
[0039] Substrate 16 may be a printed circuit board (PCB) of an electrically insulating material such as an epoxy laminate. For example, substrate 16 may include an electrically insulating layer of materials such as polytetrafluoroethylene, phenolic cotton paper materials such as flame retardant 4 (FR-4), FR-1, cotton paper and epoxy materials such as CEM-1 or CEM-3, or woven glass materials laminated together using epoxy resin materials. Interconnect structures such as traces, trenches, and through-holes may be formed through the electrically insulating layer to allow electrical signals of components 20-22 to pass through substrate 16.
[0040] Substrate 16 may include metal traces 40 electrically connected to ground plane 42. Metal traces 40 and ground plane 42 may preferably be formed of conductive materials and may protect substrate 16 from damage during the cutting process, including the formation of trenches, as described in more detail below. In some embodiments, metal traces 40 may reflect incident laser energy used to cut / ablate portions of insulating layer 18 to form trenches.
[0041] A cutting device, such as a laser, can form one or more grooves 44 in the insulating layer 18. The grooves 44 divide the component modules 30-32, and the grooves 44 are generally used as areas for depositing EMI shielding material to shield EMI from one component module to an adjacent component module. Figure 4 As shown, grooves 44 can be formed between adjacent component modules 30, 31 and through insulating layer 18 to traces 40. In embodiments where grooves 44 are formed with a laser cutting tool, traces 40 can reflect laser energy to effectively prevent laser cutting / ablation from penetrating into SIP 14. Trace 40 also serves as a conductive contact point of assembly surface 35 exposed to groove 44. Therefore, EMI shielded at groove 44 can be conducted to ground plane 42 through trace 40. Groove 44 can have a maximum width dimension "w" of 10-100 μm.
[0042] As described above, it is known to deposit a thin conductive shielding layer in the groove to shield EMI between component modules. Such conventional shielding layers are usually deposited by chemical vapor deposition, physical vapor deposition or electrochemical plating techniques and are formed of a conductive metal such as copper or aluminum. Conventional EMI shielding methods then apply a separate EMI shielding layer to the outer surface of the insulating layer to cover the upper and side surfaces of the insulating layer. This separate shielding layer works together with the above-mentioned groove shielding layer to achieve a thin "shielding cover" extending into the groove between the component modules.
[0043] exist Figure 5 In the embodiment shown in Figure 7, the EMI shielding material is provided in a self-supporting film preform 50, which can be laminated on the SIP 14 in a single lamination process to coat the grooves 44 and cover at least the outer surface 19 of the insulating layer 18. The EMI shielding film preform 50 can also be laminated to cover the side edges 17 of the substrate 16 and electrically contact the conductive plane 42 at one or more side edges 17 of the substrate 16. The lamination of the EMI shielding film preform 50 can be performed in a single lamination process to provide EMI shielding both in the grooves 44 and around the outer surface of the SIP 14. By applying the EMI shielding layer both in the grooves 44 and around the outer surface 19 with a single self-supporting film, the processing throughput of the EMI shielded SIP unit can be greatly accelerated.
[0044] EMI Shielding Materials
[0045] The EMI shielding film preform 50 is preferably a conductive self-supporting body that is effective in reducing and / or reflecting electromagnetic radiation of at least certain frequencies. EMI shielding can include one or more of reflection and absorption of incident energy, and it is expected that the shielding films of the present invention can have one or both of these properties. The EMI shielding materials useful in the present invention can exhibit a relative humidity of less than 0.1 Ω*cm, preferably about 2.0 x 10 -6 to 0.1Ω*cm, and can be about 5.0x 10 -6 Up to 1.0x 10 -2 Volume resistivity in Ω*cm. "Effective EMI shielding" is intended to mean 1-200dB / 5μm at 10MHz to 10GHz.
[0046] One aspect of the EMI shielding film preform 50 is that it exhibits sufficient flexibility / elongation to be formed around the SIP 14 and into the narrow groove 44 in a single lamination process. In order to maintain the compactness of the board employing the SIP, it is desirable that the groove 44 is as narrow as possible, with a maximum width dimension "w" of 1-100 μm. Applicants have found that it is difficult to successfully apply conventional conductive pastes to both substantially fill the groove 44 and cover the outer surface 19 of the insulating layer 18. Therefore, the EMI shielding film preform 50 can be a flexible but self-supporting film. For this purpose, the term "self-supporting film" refers to a film having a thickness of less than 0.5 mm and capable of maintaining its three-dimensional configuration at 20°C without the need for a support to maintain the configuration. The term "support to maintain the configuration" is intended to mean a structure in contact with the film that resists an applied force to maintain the initial configuration of the film defined in the absence of such applied force.
[0047] As described above, the EMI shielding film preform 50 is preferably a self-supporting film having a thickness "t" of 1-500 μm, preferably 5-200 μm, and more preferably 5-80 μm. The film thickness can be substantially uniform. The film preform 50 can also preferably be flexible, with an elongation of at least 2% at 20°C, preferably at least 3%, and more preferably at least 5%. The elongation of the film can be measured using a stress-strain test method on an Instron 5566 using a 50N load cell at a load speed of 25 mm / min. The size of the film tested is 5 mm x 10 mm x 0.3 mm thick. The EMI shielding film preform 50 can be substantially non-sticky at 20°C.
[0048] The EMI shielding film preform 50 can be formed by a polymer matrix and a filler dispersed in the polymer matrix. Exemplary conductive fillers include metals in particle form such as copper, aluminum, silver, gold, metal alloys (such as nickel-iron alloys) and other conductive materials. Exemplary magnetic interference absorbing fillers include iron, nickel and nickel-iron alloys. In one embodiment, the polymer matrix of the EMI shielding film preform 50 may include a thermoplastic or thermosetting resin, including, for example, epoxy resins, polyurethane resins and polyacrylate resins.
[0049] In some embodiments, the EMI shielding film preform 50 may include multiple layers, including multiple layers with different EMI shielding properties. The various layers of the multilayer preform 50 may be polymer-based or non-polymer-based, including one or more metal foil layers. The different layers of the multilayer film used as the preform 50 can absorb and / or reflect electromagnetic radiation of different frequency ranges or electromagnetic radiation of overlapping frequency ranges. In some embodiments, the layers of the multilayer film or preform 50 may have different or overlapping physical properties, such as elongation, tensile modulus, volume resistivity, thermal conductivity, glass transition temperature, etc. In some embodiments, the EMI shielding film preform 50 can be thermally conductive, at least along the thickness direction with at least 0.5W / m*K, more preferably at least about 1.0W / m*K thermal conductivity.
[0050] In some embodiments, the EMI shielding film preform 50 can be considered a conductive adhesive.
[0051] The EMI shielding material can be curable, wherein the self-supporting EMI shielding film preform 50 can be in a pre-cured state for lamination at SIP 14. The pre-cured film preform 50 can exhibit a tensile modulus of less than 1 GPa at an operating temperature of 20-250°C, but maintain sufficient structural properties to be self-supporting at 20°C. In some embodiments, the laminated preform 50 can be cured at an elevated temperature, such as at a temperature greater than 60°C for at least ten minutes, preferably at a temperature of at least 100°C for at least twenty minutes. The EMI shielding film preform 50 can also or alternatively be cured by other curing mechanisms (including radiation and addition of catalysts). The cured laminate from the preform 50 can exhibit a tensile modulus greater than 50 MPa, greater than 250 MPa, or greater than 1 GPa at 20°C. In other embodiments, the self-supporting EMI shielding film preform 50 can be uncurable or in a cured state, and no significant further crosslinking is required or utilized during or after lamination at SIP 14. In either case, EMI shielding film preform 50 is preferably a self-supporting body that can be applied to SIP 14 and laminated into a coating within grooves 44 and around outer surface 19 .
[0052] Lamination process
[0053] The EMI shielding film preform 50 can be secured to the SIP 14 in a single lamination process. In one embodiment, the EMI shielding film preform 50 can be vacuum laminated on the outer surface 19 of the insulating layer 18, and optionally further laminated on the side surface 17 of the substrate 16. The vacuum lamination preferably forms a coating in the grooves 44 and covers the outer surface 19 of the insulating layer 18, and optionally covers the side surface 17 of the substrate 16. Figure 6 One preferred arrangement of a vacuum laminated EMI shielding film preform 50 on a SIP 14 is shown in FIG.
[0054] In some embodiments, laminating preform 50 to SIP 14 may substantially fill trench 44 and cover outer surface 19 of insulating layer 18. To "substantially fill" trench 44, the EMI shielding material eliminates or nearly eliminates all void space in insulating layer 18 defined by trench 44. However, in other embodiments, laminating preform 50 to SIP 14 forms a coating in trench 44, such as Fig. 6A Preferably, such coating encapsulates the respective components 20a, 20b by forming a continuous EMI shield between the conductive points of the metal traces 40 and the ground plane 42 and around the respective component modules 30-32. The thickness of the laminate coating may be about 1-500 μm, preferably about 5-200 μm, and more preferably about 5-80 μm.
[0055] An exemplary process for applying the EMI shielding film preform 50 includes heating the preform 50 to a flowable state. For the purposes of this article, the term "flowable state" means a tensile modulus of less than 1 GPa. In some embodiments, the EMI shielding film preform 50 can be heated to at least 50°C to achieve a flowable state, preferably between 50 and 175°C. In other embodiments, before lamination or simultaneously with lamination, the EMI shielding film preform 50 does not need to be heated to above room temperature (or 20°C) so that the self-supporting preform 50 is in a sufficiently flowable state at room temperature or 20°C for vacuum lamination.
[0056] The heated or unheated EMI shielding film preform 50 can be vacuum laminated on the SIP 14, including the outer surface 19 of the insulating layer 18, and in the grooves 44 to form a coating in the grooves 44 and cover the outer surface 19 of the insulating layer 18. The EMI shielding film preform 50 can also be laminated on the outer surface of the insulating layer 18, the side surface 17 of the substrate 16, and in the grooves 44 to form a coating that substantially fills the grooves 44 and covers the outer surface 19 of the insulating layer 18 and the side surface 17 of the substrate 16. The EMI shielding film preform 50 can be laminated to establish electrical contact with one or both of the ground plane 42 and the metal trace 40. The EMI shielding film preform 50 can also be laminated to establish electrical contact with one or more conductive areas of the SIP 14.
[0057] The EMI shielding film preform 50 can be applied to the SIP 14 by a vacuum lamination process, which includes placing the preform 50 at the outer surface 19 of the insulating layer 18, and placing the assembly in the lamination chamber of the vacuum laminator, and then setting the temperature to 0-200°C, preferably 20-175°C, more preferably 25-75°C, and reducing the pressure to less than 500mmHg, preferably less than 250mmHg, more preferably 100-200mmHg. In some embodiments, such temperature and pressure conditions are maintained for 1-10 minutes. When a reduced pressure is applied below the film preform in the void area of the SIP 14, a force can be applied to the upper surface of the film to press the film against the outer surface 19 of the insulating layer 18 and in the groove 44. A pressure of at least 50psi, preferably 0.1-1.0MPa, can be applied by inflating an inflatable bladder against the preform 50, while applying a reduced pressure in the void area of the SIP 14. Figure 7A-7B The inflatable bladder 92 is shown inflating and applying force to the film preform 50 during the lamination process. The pressure and reduced pressure act to laminate the preform 50 onto the outer surface 19 of the insulating layer 18 and into the grooves 44.
[0058] The coating formed by laminating the preform 50 to the SIP 14 may be pressed against the outer surface 19 of the insulating layer 18 with a force of at least 50 psi. Figure 7C , and represented by force arrow "F". Pressure "F" can be applied by a pressure mechanism to further press the EMI shielding film preform 50 onto the outer surface 19 of the insulating layer 18 and into the groove 44. The pressure "F" can be provided by an inflatable bladder 92 or a press anvil (not shown) of a vacuum laminator.
[0059] like Figures 7A-7CAs shown in , the coating formed from the laminated EMI shielding film preform 50 can be cured in situ before, simultaneously with, after, or in the absence of a pressing operation. In some embodiments, the coating can be cured to have a tensile modulus of at least 1 GPa at 20°C.
[0060] Figure 8 A flow chart for forming a SIP assembly with an EMI shielding film is shown. The process includes providing a substrate or PCB in step 72. As shown in step 74, the components are mounted on the surface of the substrate. An insulating layer is formed in step 76 using a desired process. For example, the insulating layer can be molded and then transferred to the assembly surface of the substrate, or the insulating layer can be molded in situ at the assembly surface of the substrate. As known in the art, the insulating layer can be injection molded, sintered, matrix molded, compression molded, extruded, etc. In order to form the insulating layer in situ, the dielectric material can be molded in situ or deposited by a deposition process.
[0061] The component modules may be delineated by cutting or ablating trenches / channels in the insulating layer along the delineation boundaries in step 78. Suitable cutting tools for producing the delineation trenches / channels include laser cutting tools, sawing tools or machining tools.
[0062] Then, an EMI shielding film is laminated over the insulating layer and within the grooves / channels in step 80. The laminated EMI shielding layer coats the grooves / channels and establishes electrical contact with the metal traces and ground planes to form an EMI shield around the corresponding component module. The EMI shielding layer is formed from an EMI shielding film preform, which can be a self-supporting film with physical properties that facilitate the desired lamination over the insulating layer and within the grooves / channels.
[0063] Batch Processing
[0064] In some embodiments, multiple SIP devices may be EMI shielded simultaneously in a batch process prior to singulation. Fig. 9 1 shows an array 110 of components mounted on a substrate and divided into a plurality of component modules. An EMI shielding film 150 may be laminated to the array 110, such as by vacuum lamination, to coat the grooves 144 and cover the outer surface 119 of the dielectric array 118. As described above with respect to the SIP 14, the lamination of the EMI shielding film 150 on the array 110 may be performed in a single lamination process. After the lamination process, including any pressing and / or curing of the EMI shielding film 150, a plurality of SIP devices 114 may be singulated from the array 110 by cutting through the array 110 and the EMI shielding film 150 at cut lines 111. In this manner, a plurality of SIP devices 114 may be produced in a single batch process, including in a single EMI shielding film lamination process.
[0065] exist Figure 12-15 2 shows an alternative batch process in which an array 210 is formed by mounting a plurality of components on a substrate 216 (such as a PCB) having a ground plane 242 and a plurality of conductive traces 240 conductively connected to the ground plane 242 and extending to an upper surface of the substrate 216, the upper surface of the substrate 216 forming a portion of the assembly surface 235. The components may be packaged in a dielectric array 218. The array 210 may be cut along cut lines 211 using various cutting tools to initially separate the array into sub-array devices 282, which may be mounted to a carrier 284 using an adhesive 286, such as Fig.13 The sub-array devices 282 may be placed at the carrier 284 at a sufficient spacing "S" to allow the EMI shielding film 250 to be formed on each opposing surface of the adjacent sub-array devices 282 while being located at the carrier 284. The EMI shielding film 250 is applied to the carrier 284 by a lamination process such as a vacuum lamination process. Fig.13 The arrangement shown is to encapsulate the exposed surfaces of the sub-array device 282, including the exposed surfaces within the trench 244, and in some embodiments substantially fill the trench 244. Fig.14 The sub-array device 282 can then be singulated into a plurality of EMI shielding SIPs by cutting through the EMI shielding film 250 at cut lines 292 and removing the sub-array device 282 from engagement with the carrier 284. A plurality of singulated SIP devices 295 are shown in FIG. Fig.15 The mobile device 300 including the SIP device of the present invention is Fig.16 The SIP device 302 is mounted on a housing 301 and includes at least a processor 304. Other relevant components of the mobile device 300 include a receiver 306 for receiving wireless data and a transmitter 308 for transmitting wireless data.
[0066] In some embodiments, SIP device 302 may also include storage device 310 and a plurality of passive components schematically represented as elements 312. It should be understood that mobile device 300 may include several other components and elements to make mobile device 300 fully operational, but such components and elements are not shown for simplicity.
[0067] The invention has been described herein in considerable detail in order to comply with patent statutes and to provide those skilled in the art with the information necessary to apply the new principles and to construct and use the embodiments of the invention as desired. However, it should be understood that the invention can be specifically implemented by different means and that various modifications can be made without departing from the scope of the invention itself.
Claims
1. A method for shielding a system-in-package component from electromagnetic interference, wherein the system-in-package component comprises a substrate; a plurality of component modules mounted on the substrate, wherein each of the component modules comprises one or more components; an insulator covering the components on the substrate; and a groove formed in an insulator and located between adjacent component modules, wherein the maximum width of the groove is 10-100 μm, the method comprising: Providing a self-supporting EMI shielding film preform having a tensile modulus of less than 1 GPa at 20-250°C; vacuum laminating the self-supporting EMI shielding film preform onto the outer surface of the insulator and in the grooves to form a coating in the grooves and covering the outer surface of the insulator; and The coating is cured to a tensile modulus of at least 50 MPa.
2. The method for shielding a system-in-package assembly of claim 1, comprising compressing the coating onto the insulator prior to curing.
3. The method for shielding a system-in-package assembly of claim 2, comprising pressing the coating onto the outer surface of the insulator with a force of at least 50 psi prior to curing.
4. The method for shielding a system-in-package assembly of claim 1, wherein the preform comprises a conductive particle filler dispersed in a polymer resin matrix.
5. The method for shielding a system-in-package assembly of claim 1, comprising heating the preform to at least 50°C prior to vacuum lamination. 6 . The method for shielding a system-in-package assembly according to claim 1 , comprising evacuating the groove to vacuum laminate the heated preform on the outer surface of the insulator and in the groove. 7 . The method for shielding a system-in-package assembly of claim 1 , wherein curing the coating comprises heating the coating to at least 60° C. for at least ten minutes.
8. The method for shielding a system-in-package assembly of claim 7, wherein the cured coating exhibits a tensile modulus of at least 1 GPa at 20°C.
9. The method for shielding a system-in-package assembly of claim 1, wherein the coating substantially fills the trench.
10. A method for forming a system-in-package assembly, comprising: providing a substrate having a conductive ground plane spaced apart from an active surface of the substrate; and a conductive trace extending from the ground plane to the active surface; mounting a plurality of component modules on the active surface of the substrate to form an assembly surface of the substrate, wherein each component module includes one or more components; encapsulating the assembly surface of the substrate in a dielectric layer, wherein the dielectric layer extends between the assembly surface and an external surface; forming trenches between adjacent component modules and through the dielectric layer to reach the traces, wherein the maximum width of the trenches is 10-100 μm; A self-supporting EMI shielding film preform is vacuum laminated on the outer surface of the dielectric layer and in the groove to form a coating in the groove, the coating contacting the traces and covering the outer surface of the dielectric layer, and the self-supporting EMI shielding film preform has a tensile modulus of less than 1 GPa at 20-250°C.
11. The method for forming a system-in-package assembly of claim 10, comprising curing the coating to a tensile modulus of at least 50 MPa.
12. The method for forming a system-in-package assembly of claim 10, comprising pressing the coating onto the outer surface of the dielectric layer with a force of at least 50 psi.
13. The method for forming a system-in-package assembly of claim 12, comprising singulating a plurality of system-in-package devices by cutting through the substrate and the dielectric layer. 14 . The method for forming a system-in-package assembly of claim 13 , comprising forming a plurality of trenches in the dielectric layer, wherein each trench divides a first group of one or more component modules from a second group of one or more modules.
15. The method for forming a system-in-package assembly of claim 10, wherein the coating substantially fills the trench.
16. The method for forming a system-in-package assembly of claim 10, wherein the coating contacts the conductive ground plane.
17. A mobile device comprising: shell; a receiver for receiving wireless data; a transmitter for transmitting wireless data; and A system-in-package component, the system-in-package component comprising: substrate; a plurality of component modules mounted on the substrate, wherein each component module includes one or more components; an insulator covering the components on the substrate, and A groove formed in the insulator and located between adjacent component modules, wherein the maximum width of the groove is 10-100 μm, a coating in the groove covering the outer surface of the insulator and having a tensile modulus of at least 50 MPa, wherein the system-in-package assembly is mounted on the housing, wherein one or more components of the system-in-package assembly include at least one processor, and wherein the system-in-package assembly comprises at least one of the grooves dividing at least two component modules, Wherein the coating substantially filling the trench reduces electromagnetic interference by at least 10 db.