Method for manufacturing laminated core
By placing the stacked body on the support part, the protrusions of the stacked rivet parts are not in contact, which solves the problem of unstable stacked rivet parts affecting the processing quality, and achieves stable processing after the stacked rivet parts are interlocked.
Patent Information
- Application Number
- CN201980017756.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-03-07
- Filing Date
- 2019-03-05
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2039-03-05
AI Technical Summary
The bulges of the stacked rivets of the laminated iron core are unstable, which affects the quality of subsequent processing. Especially when the size of the laminated body increases and the demand for interlocking force increases, the bulges of the stacked rivets may cause the laminated body to be unstable and affect the processing quality. .
By placing the laminated body on the support part so that the protrusions of the stacked rivets are not in contact with the support surface, and performing subsequent processing in this state, the stability of the laminated body during processing is ensured.
This achieves stable subsequent processing after the stacked rivets are interlocked, improves the processing quality and stability of the laminated iron core, and avoids instability problems caused by bulging of the stacked rivets.
Smart Images

Figure CN111837320B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a method for manufacturing a laminated core. Background Art
[0002] The laminated core generally includes a laminated body in which a plurality of punched parts obtained by punching a metal plate (eg, an electromagnetic steel plate) into a predetermined shape are stacked. The plurality of punched parts are interlocked with each other by stack rivets (eg, see Patent Document 1).
[0003] Reference List
[0004] Patent Literature
[0005] [Patent Document 1] JP2016-146739A Summary of the invention
[0006] Technical issues
[0007] The stacking rivet includes: a recess formed on the front surface side of the punched component; and a protrusion formed on the back surface side of the punched component. The recess of the stacking rivet of one punched component cooperates with the protrusion of the stacking rivet of another punched component. Therefore, the protrusion of the stacking rivet formed on the punched component forming the bottom layer of the stacked body may protrude further outward than the lower end surface of the stacked body (see Patent Document 1). Figure 6 ).
[0008] In a metal plate blanking device, since the metal plate is usually processed by a punch that descends from above, the stacked body is discharged from the blanking device in a state where the protrusion of the stack rivet protrudes downward. However, since the height of the protrusion of the stack rivet is not constant, the stacked body may be in an unstable state. If subsequent processing is performed on the stacked body in this state, the quality of the processing may be affected.
[0009] In particular, in recent years, with the development of hybrid vehicles (HV) and electric vehicles (EV), the demand for using larger motors in vehicles has increased. As the size of the laminated core increases, the protrusion of the stacking rivet may be set larger to increase the interlocking force between multiple blanked parts. In this case, the protrusion of the stacking rivet is more likely to protrude from the lower end surface of the laminate.
[0010] Thus, the present disclosure describes a method for manufacturing a laminated core in which subsequent processing can be advantageously performed after the laminates are interlocked by stack rivets.
[0011] Problem Solution
[0012] According to an exemplary aspect of the present disclosure, a method for manufacturing a laminated iron core by stacking a plurality of punched parts to form a laminated body, the laminated body comprising a pair of first end faces and a second end face, and the plurality of punched parts being interlocked in a stacking direction of the laminated body by a stacking rivet, the manufacturing method comprising: forming the laminated body so that a protrusion of the stacking rivet protrudes downward from a first end face in a downward state; placing the laminated body on a support portion so that the protrusion does not contact a support surface of the support portion; and processing the laminated body in a state where the laminated body is placed on the support portion.
[0013] Advantageous Effects of the Invention
[0014] According to the manufacturing method of the laminated core disclosed in the present invention, subsequent processing can be advantageously performed after the laminated bodies are interlocked by the stack rivets. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a perspective view showing an example of a rotor laminated core.
[0016] Figure 2 It is along Figure 1 A cross-sectional view taken along line II-II in FIG.
[0017] Figure 3 1 is a schematic diagram showing an example of a manufacturing apparatus for a rotor laminated core.
[0018] Figure 4A is a schematic cross-sectional view for illustrating a process of forming a through hole, and Figure 4B is a schematic cross-sectional view for illustrating a process of forming a stack rivet.
[0019] Figure 5 It is a cross-sectional view schematically showing a mechanism for laminating the blanked parts and a mechanism for discharging the stacked body from a die, and is used to show a state where the blanked parts are blanked out from the electromagnetic steel sheet by a punch.
[0020] Figure 6 It is a cross-sectional view for illustrating a state in which a permanent magnet is attached to a magnet insertion hole of a rotor laminated core by a magnet attaching device.
[0021] Figure 7 It is a flowchart for showing an example of a method for manufacturing a rotor laminated core.
[0022] Figure 8 FIG. 1 is a schematic diagram partially showing another example of the manufacturing apparatus for the rotor laminated core.
[0023] FIG. 9 is a schematic diagram for illustrating a state of measuring a projection or a recess of a stack rivet.
[0024] Fig.10is a partial cross-sectional view showing another example of the rotor laminated core.
[0025] Reference Mark List
[0026] 1... rotor laminated core, 10... laminated body, 11... temporary laminated body (laminated body), 18... rivet portion, 20... rivet piece, 22... through hole, 20a... recess, 20b... protrusion, 100... manufacturing device of rotor laminated core, 130... punching device, 200... pressing device, 300... inversion device, 400... laminated thickness measuring device, 401... clamping part (support part), 401a... opening part, 500... magnet attaching device, 510... lower die (support part), 600... rivet piece measuring device, 601... support part, 602... sensor, Ctr... controller (control unit), L1... load (first load), L3... load (second load), S1... upper end face (second end face), S2... lower end face (first end face), W, W1, W2... punched parts. DETAILED DESCRIPTION
[0027] Hereinafter, an example of an embodiment according to the present disclosure will be described in detail with reference to the accompanying drawings. In the following description, the same elements having the same functions will be denoted by the same reference numerals, and their respective descriptions will be omitted.
[0028] [Laminated rotor core]
[0029] First, refer to Figure 1 and 2 The configuration of the rotor laminated core 1 (laminated core) is described. The rotor laminated core 1 is a part of the rotor. The rotor is formed by attaching an end plate (not shown) and a shaft to the rotor laminated core 1. The rotor is combined with a stator to form a motor. The rotor laminated core 1 in this embodiment is used for an interior permanent magnet (IPM) motor.
[0030] like Figure 1 As shown, the rotor laminated core 1 includes: a laminated body 10 ; a plurality of permanent magnets 12 ; and a plurality of cured resins 14 .
[0031] like Figure 1 As shown, the stack 10 has a cylindrical shape. An axial hole 10a that passes through the stack 10 is provided in the central portion of the stack 10. The axial hole 10a extends along the central axis Ax. That is, the axial hole 10a extends in the stacking direction of the stack 10 (hereinafter referred to as the "stacking direction"). The stacking direction is also the extending direction of the central axis Ax. In the present embodiment, since the stack 10 rotates around the central axis Ax, the central axis Ax is also the rotation axis. The shaft is inserted into the axial hole 10a.
[0032] A plurality of magnetic insertion holes 16 are formed in the laminate 10. Figure 1 As shown, the magnetic insertion holes 16 are arranged at predetermined intervals along the outer peripheral edge of the laminated body 10. Figure 2 As shown, the magnetic insertion hole 16 penetrates the laminated body 10 in a manner extending along the central axis Ax. That is, the magnetic insertion hole 16 extends in the lamination direction.
[0033] In the present embodiment, the shape of the magnetic socket 16 is a long hole extending along the outer periphery of the laminate 10. In the present embodiment, the number of the magnetic sockets 16 is six. The magnetic sockets 16 are arranged on the same circumference when viewed from above. The position, shape and number of the magnetic sockets 16 can be changed according to the purpose of the motor, the required performance, etc.
[0034] The laminated body 10 is formed by laminating a plurality of punched parts W. The punched parts W are plate-shaped bodies formed by punching an electromagnetic steel sheet ES described later into a predetermined shape, and have a shape corresponding to the laminated body 10. Figure 2 As shown, in this specification, the punched parts W constituting the portion other than the bottom layer of the stacked body 10 are referred to as "punched parts W1", and the punched parts W constituting the bottom layer of the stacked body 10 are referred to as "punched parts W2".
[0035] The surface of the punched member W1 constituting the uppermost layer of the stack 10 constitutes the upper end surface S1 (second end surface) of the stack 10. The surface of the punched member W2 constituting the lowermost layer of the stack 10 constitutes the lower end surface S2 (first end surface) of the stack 10.
[0036] The laminate 10 can be formed by so-called roll lamination. The term "roll lamination" means laminating a plurality of punched parts W with the punched parts W being relatively staggered at an angle. Roll lamination is mainly performed to eliminate the plate thickness deviation of the punched parts W. The angle of roll lamination can be set to any size.
[0037] like Figure 1 and 2 As shown, the blanked parts W adjacent to each other in the stacking direction can be interlocked by the overlap rivet portion 18. Specifically, as Figure 2 As shown, the overlap rivet portion 18 includes an overlap rivet 20 formed on the punched part W1 and a through hole 22 formed on the punched part W2 .
[0038] Each stack rivet 20 includes: a recess 20a formed on the front surface side of the punched part W1; and a protrusion 20b formed on the back surface side of the punched part W1. The stack rivet 20 as a whole has, for example, a mountain shape. The stack rivet 20 having such a shape is also called a "V-shaped stack rivet".
[0039] The recess 20a of one blanked part W1 is fitted to the projection 20b of the blanked part W1 adjacent to the front surface side of the one blanked part W1. The projection 20b of one blanked part W1 is bonded to the recess 20a of the blanked part W1 adjacent to the back surface side of the one blanked part W1.
[0040] The through hole 22 is a long hole having a shape corresponding to the outer shape of the stack rivet 20. When the stack rivet 20 is a V-shaped stack rivet, the through hole 22 has a rectangular shape. The protrusion 20b of the punched part W1 adjacent to the punched part W2 fits into the through hole 22. When the stack 10 is continuously manufactured, the through hole 22 has a function of preventing the punched part W formed later from interlocking with the previously manufactured stack 10 due to the stack rivet 20 (protrusion 20b).
[0041] like Figure 2 As shown, the tip end portion of the protrusion 20b of the stack rivet 20 protrudes outward from the through hole 22. That is, in a state where the lower end surface S2 of the stacked body 10 faces downward, the tip end portion of the protrusion 20b of the stack rivet 20 protrudes downward from the lower end surface S2.
[0042] like Figure 1 and 2 As shown, one permanent magnet 12 is inserted into each magnetic insertion hole 16. The shape of the permanent magnet 12 is not particularly limited, and in the present embodiment, the permanent magnet 12 has a rectangular parallelepiped shape. The type of the permanent magnet 12 can be determined according to the purpose of the motor, the required performance, etc., and can be, for example, a sintered magnet or a bonded magnet.
[0043] The cured resin 14 is obtained by curing the molten resin material (molten resin) filled in the magnetic socket 16. For example, the molten resin is filled after the permanent magnet 12 is inserted into the magnetic socket 16. The cured resin 14 has the function of fixing the permanent magnet 12 in the magnetic socket 16 and the function of combining the adjacent punched parts W in the stacking direction (up and down direction). Examples of resin materials constituting the cured resin 14 include thermosetting resins, thermoplastic resins, and the like. Specific examples of thermosetting resins include resin compositions, which include epoxy resins, curing initiators, and additives. Examples of additives include fillers, flame retardants, pressure reducing agents, and the like.
[0044] [Manufacturing device for rotor laminated core]
[0045] Next, refer to Figures 3 to 6 A manufacturing apparatus 100 for the rotor laminated core 1 will be described.
[0046] like Figure 3As shown, the manufacturing device 100 is a device for manufacturing the rotor laminated core 1 from the electromagnetic steel sheet ES (sheet to be processed) as a strip metal plate. The manufacturing device 100 includes an uncoiler 110, a feeding device 120, a punching device 130, a pressing device 200, an inverting device 300, a stacking thickness measuring device 400, a magnet attaching device 500 and a controller Ctr (control unit).
[0047] The uncoiler 110 rotatably holds the coil 111 in a state where the coil 111 is mounted. The coil 111 is obtained by winding the strip-shaped electromagnetic steel sheet ES into a coil shape. The feeding device 120 includes a pair of rollers 121, 122 that sandwich the electromagnetic steel sheet ES from the upper and lower sides. The pair of rollers 121, 122 rotates and stops based on a command signal from the controller Ctr, and intermittently and sequentially feeds the electromagnetic steel sheet ES to the punching device 130.
[0048] The punching device 130 operates based on the command signal from the controller Ctr. The punching device 130 has the following functions: a function of sequentially punching the electromagnetic steel sheet ES intermittently fed by the feeding device 120 using a plurality of punches to form a punched part W; and a function of sequentially stacking the punched parts W obtained by punching to manufacture a temporary laminated body 11. In the present specification, in the same manner as the laminated body 10, the temporary laminated body 11 is in a state where a plurality of punched parts W are stacked and interlocked with each other by the rivet portion 18. However, the punched parts W are not in close contact with each other, and there is a certain degree of gap between the punched parts W.
[0049] like Figure 3 As shown, the blanking device 130 includes a base 131, a lower die 132, a punching plate 133, a demolding machine 134, an upper die 135, a top plate 136, a press machine 137 (driving unit) and a plurality of punches.
[0050] The base 131 is installed on the floor surface, and supports a lower die 132 placed on the base 131. The lower die 132 holds a punch plate 133 placed on the lower die 132. The lower die 132 is provided at a predetermined position with a discharge hole through which a material punched out from the electromagnetic steel sheet ES (e.g., a punched part W and scrap) is discharged.
[0051] The punching plate 133 has a function of forming a blanked part W together with a plurality of punches. The punching plate 133 is provided with dies at positions corresponding to the respective punches. Each die is provided with a die hole through which a corresponding punch can be inserted.
[0052] The demolding machine 134 has a function of clamping the electromagnetic steel sheet ES with the punch plate 133 when the electromagnetic steel sheet ES is punched by each punch, and a function of removing the electromagnetic steel sheet ES clamped by each punch from each punch. The upper die 135 is located above the demolding machine 134. The base end of each punch is fixed to the upper die 135. Therefore, the upper die 135 holds each punch.
[0053] The top plate 136 holds the upper die 135 from the upper side of the upper die 135. The press 137 is located above the top plate 136. The piston of the press 137 is connected to the top plate 136 and operates based on a command signal from the controller Ctr. When the press 137 operates, the piston is extended and retracted, and the demolding machine 134, the upper die 135, the top plate 136 and the respective punches move up and down as a whole.
[0054] Here, a plurality of punches and a plurality of dies included in the punching device 130 will be described in detail. For example, as shown in FIGS. 4 and 5 , the punching device 130 includes punch parts P10, P20, and P30.
[0055] The punch portion P10 has a function of forming a through hole 22 in the electromagnetic steel sheet ES used as the part W2 to be punched. Figure 4A As shown, the punch part P10 is formed by combining the die D1 and the punch P1. A die hole D1a is formed in the die D1.
[0056] The punch P1 has a shape corresponding to the die hole D1a and can be inserted into and removed from the die hole D1a through the through hole 134a of the stripper 134.
[0057] The punch portion P20 has a function of forming a rivet 20 on the electromagnetic steel sheet ES used as the blanking part W1. Figure 4B As shown, the punch part P20 is formed by combining the die D2 and the punch P2. The die hole D2a is formed in the die D2. The size of the die hole D2a may be the same as that of the die hole D1a.
[0058] The punch P2 has a shape corresponding to the die hole D2a. The punch P2 can be inserted into and removed from the die hole D2a through the through hole 134b of the demolding machine 134. The outer shape of the punch P2 is set to be slightly smaller than the outer shape of the die hole D2a. The gap CL between the die hole D2a and the punch P2 can be set to various sizes corresponding to the matching force generated between the stack rivet 20 and the through hole 22.
[0059] The tip of the punch P2 has a mountain shape as a whole. Therefore, a concavo-convex portion having a shape corresponding to the tip of the punch P2 is formed on the electromagnetic steel sheet ES processed by the punch P2.
[0060] The punch portion P30 has the function of punching the electromagnetic steel sheet ES to form a punched component W. Figure 5As shown in FIG. 1 , the punch portion P30 is formed by combining the die D3 and the punch P3. The die hole D3a is formed in the die D3. The die hole D3a has a shape corresponding to the outer shape of the part W to be punched.
[0061] The punch P3 has a shape corresponding to the die hole D3a. The punch P3 can be inserted into and removed from the die hole D3a through the through hole 134c of the demolding machine 134. A plurality of pressing protrusions P3a are provided on the end surface of the punch P3. The pressing protrusions P3a protrude downward from the end surface. The plurality of pressing protrusions P3a are respectively located at positions corresponding to the plurality of stacked rivets 20 formed on the electromagnetic steel sheet ES using the punch P2.
[0062] The column 132b, the stand 132c and the push rod 132d are arranged in the space 132a below the mold D3. The column 132b can move in the up and down directions through the hole 132e set in the stand 132c based on the command signal from the controller Ctr. Specifically, the column 132b moves downward intermittently each time the punched parts W are stacked on the column 132b. When a predetermined number of punched parts W are stacked on the column 132b, the temporary stack 11 is formed, and the column 132b moves to a position where the front surface of the column 132b is flush with the front surface of the stand 132c.
[0063] The push rod 132d can move in the horizontal direction on the front surface of the platform 132c based on the command signal from the controller Ctr. When the column 132b moves to the position where the front surface of the column 132b is flush with the front surface of the platform 132c, the push rod 132d transfers the temporary stack 11 from the column 132b to the platform 132c. At this time, the temporary stack 11 is in a state (upright state) where the lower end surface S2 faces downward and the protrusion 20b protrudes downward from the lower end surface S2. The temporary stack 11 transferred to the platform 132c is transported to the subsequent pressing device 200 by the conveyor Cv. The temporary stack 11 can be manually transported in a state placed in a container.
[0064] Reference Figure 3 The pressing device 200 operates based on the command signal from the controller Ctr. The pressing device 200 has a function of applying a predetermined load L1 (first load) to the temporary stack 11 from the stacking direction to form a stack 10 in which the gap between the punched parts W is smaller than the gap in the temporary stack 11.
[0065] The load L1 applied to the temporary laminate 11 can have various sizes depending on the size of the layer and body 10, and can be, for example, about 0.1 ton to 50 tons, about 0.5 ton to 30 tons or about 1 ton to 10 tons. When the load L1 is equal to or greater than 0.1 ton, it is less likely that rebound will occur. On the other hand, when a load greater than necessary is applied to the temporary laminate 11, the laminate 10 formed may be deformed. When the load L1 is equal to or less than 50 tons, it is less likely that such a deformation of the laminate 10 will occur.
[0066] The pressing device 200 includes a pair of clamping parts 201, 202 and a lifting mechanism 203. The pair of clamping parts 201, 202 are rectangular flat plates. The pair of clamping parts 201, 202 are arranged in the up-down direction. A plurality of guide shafts (not shown) extending upward may be provided on the upper surface of the clamping part 201 located at the lower side. Each guide shaft is positioned at each corner of the clamping part 201. A through hole (not shown) through which the corresponding guide shaft can be inserted may be provided in each corner of the clamping part 202 located at the upper side.
[0067] The lifting mechanism 203 is connected to the clamping member 202. The lifting mechanism 203 operates based on the command signal from the controller Ctr, and reciprocates the clamping member 202 in the up and down directions. That is, the lifting mechanism 203 is configured so that the clamping members 201, 202 can approach and separate from each other by moving the clamping member 202 up and down along the guide shaft. The lifting mechanism 203 is not particularly limited as long as the clamping member 202 moves up and down, and may be, for example, an actuator, a cylinder, or the like.
[0068] In this embodiment, the temporary stack 11 in an upright state is clamped by the clamping members 201, 202. That is, the lower end surface S2 of the temporary stack 11 faces the clamping member 201. The protrusion 20b protruding from the lower end surface S2 of the temporary stack 11 abuts against the upper surface of the clamping member 201. The upper end surface S1 of the temporary stack 11 faces and abuts against the clamping member 202.
[0069] The inverting device 300 operates based on a command signal from the controller Ctr. The inverting device 300 has a function of inverting the posture of the stacked body 10 conveyed from the pressing device 200 in an upright state.
[0070] The inverting device 300 includes a pair of clamping members 301, 302, a lifting mechanism 303 and an inverting mechanism 304. The pair of clamping members 301, 302 are rectangular flat plates. The pair of clamping members 301, 302 are arranged in the up-down direction.
[0071] The lifting mechanism 303 is connected to the clamping members 301, 302. The lifting mechanism 303 operates based on the command signal from the controller Ctr, and causes the clamping member 302 to reciprocate in the up and down directions. That is, the lifting mechanism 303 is configured so that the clamping members 301, 302 can be approached and separated from each other by moving the clamping member 302 up and down. The lifting mechanism 303 is not particularly limited as long as the clamping member 302 moves up and down, and may be, for example, an actuator, a cylinder, or the like.
[0072] The inverting mechanism 304 operates based on the command signal from the controller Ctr, and rotates the clamping members 301, 302 and the lifting mechanism 303 as a whole by 180° around the axis extending along the horizontal plane. That is, when the stacked body 10 is clamped by the clamping members 301, 302 in an upright state, the inverting mechanism 304 rotates the clamping members 301, 302 and the lifting mechanism 303 by 180°, so that the stacked body 10 is in a state where the lower end surface S2 faces upward and the protrusion 20b protrudes upward from the lower end surface S2 (inverted state).
[0073] The stacking thickness measuring device 400 operates based on a command signal from the controller Ctr. The stacking thickness measuring device 400 has a function of measuring the stacking thickness (the height of the stacking body 10 in the stacking direction) of the stacking body 10. The stacking thickness measuring device 400 measures the stacking thickness of the stacking body 10 in a state where a predetermined load L2 is applied to the stacking body 10 from the stacking direction.
[0074] The load L2 applied to the stacked body 10 is set to be equal to or less than the load L1. The load L2 may have various sizes depending on the size of the stacked body 10, and may be set such that, for example, the thickness T of the stacked body 10 after pressing is equal to or more than 99.9% of the thickness T0 of the stacked body 10 before pressing and is less than the thickness T0 (0.999T0≦T <T0)。
[0075] The stacking thickness measuring device 400 includes a pair of clamping parts 401, 402, a lifting mechanism 403 and a distance sensor 404. The pair of clamping parts 401, 402 are rectangular flat plates. The pair of clamping parts 401, 402 are arranged in the up-down direction. A plurality of guide shafts (not shown) extending upward may be provided on the upper surface of the clamping part 401 located on the lower side. Each guide shaft is positioned on each corner of the clamping part 401. A through hole (not shown) through which the corresponding guide shaft can be inserted may be provided in each corner of the clamping part 402 located on the upper side.
[0076] The lifting mechanism 403 is connected to the clamping member 402. The lifting mechanism 403 operates based on the command signal from the controller Ctr, and reciprocates the clamping member 402 in the up and down directions. That is, the lifting mechanism 403 is configured so that the clamping members 401, 402 can be approached and separated from each other by moving the clamping member 402 up and down. The lifting mechanism 403 is not particularly limited as long as the clamping member 402 moves up and down, and may be, for example, an actuator, a cylinder, or the like.
[0077] In the present embodiment, the stacked body 10 in an inverted state is clamped by the clamping members 401, 402. That is, the upper end surface S1 of the stacked body 10 faces and abuts against the upper surface of the clamping member 401. Therefore, the upper surface of the clamping member 401 serves as a supporting surface for supporting the stacked body 10. The lower end surface S2 of the stacked body 10 faces the lower surface of the clamping member 402. The protrusion 20b protruding from the lower end surface S2 of the stacked body 10 abuts against the lower surface of the clamping member 402.
[0078] The distance sensor 404 is, for example, provided on the clamping member 402. The distance sensor 404 is configured to measure the distance between the clamping member 401 and the clamping member 402 when the clamping members 401 and 402 clamp the stacked body 10. That is, the distance sensor 404 indirectly measures the stacking thickness of the stacked body 10. The data of the stacking thickness of the stacked body 10 measured by the distance sensor 404 is transmitted to the controller Ctr.
[0079] The magnet attachment device 500 operates based on a command signal from the controller Ctr. The magnet attachment device 500 has: a function of inserting the permanent magnets 12 into each magnetic insertion hole 16; and a function of filling the magnetic insertion hole 16 through which the permanent magnets 12 are inserted with molten resin. The magnet attachment device 500 includes a lower mold 510 (supporting portion), an upper mold 520, and a plurality of plungers 530, such as Figure 6 Shown in detail.
[0080] The lower mold 510 includes a base member 511 and an insertion column 512 disposed on the base member 511. The base member 511 is a plate-like member in a rectangular shape. The base member 511 is configured so that the stacked body 10 can be placed thereon. The insertion column 512 is located at a substantially central portion of the base member 511 and protrudes upward from the upper surface of the base member 511. The insertion column 512 has a columnar shape and has an outer shape corresponding to the shaft hole 10a of the stacked body 10.
[0081] The upper mold 520 is configured to be able to clamp the stack 10 in the stacking direction (the height direction of the stack 10) together with the lower mold 510. When the upper mold 520 and the lower mold 510 clamp the stack 10 together, a predetermined load L3 (second load) is applied to the stack 10 from the stacking direction. The load L3 applied to the stack 10 is set to be equal to or less than the load L1. Depending on the size of the stack 10, the load L3 may have various sizes, and may be, for example, about 0.1 tons to 10 tons.
[0082] The upper mold 520 includes a base member 521 and a built-in heat source 522. The base member 521 is a plate-like member in a rectangular shape. The base member 521 includes a through hole 521a, a plurality of receiving holes 521b, and a plurality of recessed portions 521c. The through hole 521a is located in a substantially central portion of the base member 521. The through hole 521a has a shape (substantially circular) corresponding to the insertion column 512, and the insertion column 512 can be inserted through the through hole 521a.
[0083] A plurality of receiving holes 521b penetrate the base member 521 and are arranged at predetermined intervals along the periphery of the through hole 521a. Each receiving hole 521b is located at a position corresponding to each magnetic insertion hole 16 of the stacked body 10 when the lower mold 510 and the upper mold 520 clamp the stacked body 10. Each receiving hole 521b has a columnar shape and has a function of accommodating at least one resin particle P therein. Each of the plurality of recessed portions 521c is capable of accommodating a protrusion 20b protruding from the lower end surface S2 of the stacked body 10.
[0084] In the present embodiment, the stacked body 10 in an inverted state is clamped by the lower mold 510 (base member 511) and the upper mold 520 (base member 521). That is, the upper end surface S1 of the stacked body 10 faces and abuts against the upper surface of the base member 511. Therefore, the upper surface of the base member 511 serves as a supporting surface for supporting the stacked body 10. The lower end surface S2 of the stacked body 10 faces and abuts against the lower surface of the base member 521. The protrusion 20b protruding upward from the lower end surface S2 of the stacked body 10 is accommodated in the corresponding recessed portion 521c.
[0085] The built-in heat source 522 is, for example, a heater built into the base member 521. When the built-in heat source 522 operates, the base member 521 is heated, the laminated body 10 in contact with the base member 521 is heated, and the resin particles P accommodated in the accommodation hole 521b are heated. As a result, the resin particles P melt and change into molten resin.
[0086] A plurality of plungers 530 are located above the upper mold 520. Each plunger 530 is configured to be insertable into and removable from a corresponding accommodation hole 521b by a driving source (not shown).
[0087] The controller Ctr generates command signals for operating the feeding device 120, the punching device 130, the pressing device 200, the inverting device 300, the stacking thickness measuring device 400 and the magnet attaching device 500 based on, for example, a program recorded in a recording medium (not shown) or an operation input by an operator, and sends the command signals to these devices respectively.
[0088] The controller Ctr has a function of determining whether the data of the stacking thickness measured by the stacking thickness measuring device 400 is within the standard. The stacked body 10 whose stacking thickness is within the standard is determined by the controller Ctr as a non-defective product and is conveyed to the magnet attaching device 500. On the other hand, the stacked body 10 whose stacking thickness is outside the standard is determined by the controller Ctr as a defective product and is excluded from the manufacturing line.
[0089] [Manufacturing method of rotor laminated core]
[0090] Next, refer to Figures 3 to 7 A method of manufacturing the rotor laminated core 1 is described.
[0091] First, the electromagnetic steel sheets ES are sequentially punched out by the punching device 130, and the punched parts W obtained are stacked to form a temporary stack 11 (see FIG. Figure 7 Specifically, as shown in FIG. 4 , the electromagnetic steel sheet ES is fed to the punching device 130 by the feeding device 120, and the processing target portion of the electromagnetic steel sheet ES reaches the predetermined punch, a through hole consistent with the shaft hole 10a is formed (so-called inner shape punching), a through hole consistent with each magnetic socket 16 is formed, a stacked rivet 20 or a through hole 22 is formed, and a punched part W is punched out from the electromagnetic steel sheet ES (so-called outer shape punching).
[0092] The overlap 20 and the through hole 22 are selectively formed. That is, the overlap 20 is formed in a predetermined region of the electromagnetic steel sheet ES where the blanking part W1 is to be formed, and the through hole 22 is formed in a predetermined region of the electromagnetic steel sheet ES where the blanking part W2 is to be formed.
[0093] The through hole 22 is formed as follows. Figure 4A As shown, the blanking device 130 operates based on the command signal from the controller Ctr, and clamps the electromagnetic steel sheet ES by the punch plate 133 and the stripper plate 134. Subsequently, the punch P1 moves downward through the through hole 134a of the stripper plate 134, and the tip end portion of the punch P1 pushes the electromagnetic steel sheet ES into the die hole D1a. As a result, the through hole 22 is formed in the electromagnetic steel sheet ES.
[0094] The stacked rivet 20 is formed as follows. Figure 4BAs shown, the blanking device 130 operates based on the command signal from the controller Ctr, and clamps the electromagnetic steel sheet ES by the punch plate 133 and the stripper plate 134. Subsequently, the punch P2 moves downward through the through hole 134b of the stripper plate 134, and the tip of the punch P2 pushes the electromagnetic steel sheet ES into the die hole D2a. As a result, the overlapped rivet 20 is formed on the electromagnetic steel sheet ES.
[0095] The punching of the punched component W from the electromagnetic steel sheet ES is performed as follows. Figure 5 As shown, the punching device 130 operates based on the command signal from the controller Ctr, and clamps the electromagnetic steel sheet ES by the punch plate 133 and the stripper plate 134. Subsequently, the punch P3 moves downward through the through hole 134c of the stripper plate 134, and the tip of the punch P3 pushes the electromagnetic steel sheet ES into the die hole D3a. As a result, a punched component W is punched out from the electromagnetic steel sheet ES.
[0096] When the punch P3 is used to punch out the punched component W2 from the electromagnetic steel sheet ES, the electromagnetic steel sheet ES is not processed by the pressing protrusion P3a because the pressing protrusion P3a is inserted into the through hole 22. At the same time, when the punch P3a is used to punch out the punched component W1 from the electromagnetic steel sheet ES, the pressing protrusion P3a presses the concave portion 20a of the corresponding stack rivet 20. As a result, the protrusion 20b of the stack rivet 20 is pressed into the concave portion 20a of the stack rivet 20 or the through hole 22, so that the two components fit each other.
[0097] The blanked parts W punched out from the electromagnetic steel sheet ES by the punch P3 are stacked on the column 132b to form a standing temporary stack 11. The standing temporary stack 11 is transferred from the column 132b to the stand 132c by the push rod 132d, and is further transferred to the pressing device 200 by the conveyor Cv.
[0098] Next, the temporary stack 11 conveyed to the pressing device 200 is placed on the clamping member 201 in an upright state. At this time, the lower end surface S2 of the stack 10 abuts against the clamping member 201. Next, the controller Ctr instructs the lifting mechanism 203 to lower the clamping member 202. As a result, the temporary stack 11 is clamped between the clamping members 201 and 202, and the temporary stack 11 is pressed with a load L1. As a result, the gap between the blanked parts W is reduced, and the stack 10 (see Figure 7 The stacked body 10 is conveyed to the inverting device 300 in an upright state.
[0099] Next, the stacked body 10 conveyed to the inverting device 300 is placed on the clamping member 301 in an upright state. Next, the controller Ctr instructs the lifting mechanism 303 to lower the clamping member 302. As a result, the stacked body 10 is clamped between the clamping members 301, 302. In this state, the controller Ctr rotates the clamping members 301, 302 and the lifting mechanism 303 as a whole by 180° together with the stacked body 10 supported by the inverting mechanism 304 and clamped by the clamping members 301, 302. As a result, the stacked body 10 is inverted and in an inverted state (see Figure 7 The stacked body 10 is conveyed to the stacking thickness measuring device 400 in an inverted state.
[0100] Next, the stack 10 transported to the stacking thickness measuring device 400 is placed on the clamping part 401 in an inverted state. At this time, the upper end surface S1 of the stack 10 abuts against the clamping part 401. Next, the controller Ctr commands the lifting mechanism 403 to lower the clamping part 402. As a result, the stack 10 is clamped between the clamping parts 401 and 402, and the stack 10 is pressed with a load L2. In this state, the controller Ctr commands the distance sensor 404 to measure the distance between the clamping parts 401 and 402. The distance sensor 404 transmits the measured data as data of the stacking thickness of the stack 10 to the controller Ctr. As a result, the stacking thickness of the stack 10 is measured (see Figure 7 The thickness T0 of the laminated body 10 before being pressed with the load L2 can be measured by various known methods, and can be measured by using, for example, a distance sensor using ultrasonic waves or the like, a ruler, or the like.
[0101] Next, the controller Ctr determines whether the data of the stacking thickness transmitted from the distance sensor 404 is within a predetermined standard (see Figure 7 Step S15). When the controller Ctr determines that the stacking thickness of the stacked body 10 is outside the predetermined standard ( Figure 7 In step S15 of the embodiment of the present invention, if the stacked body 10 is not present, the stacked body 10 is likely to be a defective product, and the stacked body 10 is excluded from the manufacturing line (see Figure 7 When the stacking thickness of the stack 10 is greater than a predetermined standard, at least one blanked component W may be removed from the stack 10 so that the stacking thickness of the stack 10 is within the predetermined standard, and the stack 10 may be returned to the manufacturing line.
[0102] On the other hand, when the controller Ctr determines that the stacking thickness of the stacked body 10 is within the predetermined standard ( Figure 7 In step S15, the stacked body 10 is conveyed to the magnet attaching device 500 in an inverted state, and the stacked body 10 is placed on the lower mold 510 (such as Figure 6). At this time, the upper end surface S1 of the stacked body 10 abuts against the base member 511. Next, the permanent magnets 12 are inserted into the respective magnetic insertion holes 16. The permanent magnets 12 can be inserted into the respective magnetic insertion holes 16 manually or by using a robot (not shown) included in the magnet attachment device 500 based on a command signal of the controller Ctr.
[0103] Next, the upper mold 520 is placed on the stacked body 10. Thereafter, the stacked body 10 is clamped from the stacking direction by the lower mold 510 and the upper mold 520, and the stacked body 10 is pressed with a load L3. At this time, the protrusion 20b protruding upward from the lower end surface S2 of the stacked body 10 is accommodated in the concave portion 521c of the upper mold 520, and the lower end surface S2 abuts against the upper mold 520.
[0104] Next, resin particles P are placed in each receiving hole 521b. When the resin particles P are melted by the built-in heat source 522 of the upper mold 520, the molten resin is injected into each magnetic insertion hole 16 through the plunger 530. At this time, the stacked body 10 is heated to, for example, about 150°C to 180°C by the built-in heat source 522. Thereafter, when the molten resin solidifies, a solidified resin 14 is formed in the magnetic insertion hole 16. Thus, the permanent magnet 12 is attached to the stacked body 10 together with the solidified resin 14 (see Figure 7 When the lower mold 510 and the upper mold 520 are removed from the laminated body 10, the rotor laminated core 1 is completed.
[0105] [Effect]
[0106] In the above-described embodiment, when the stacking thickness of the stacked body 10 is measured by the stacking thickness measuring device 400, the protrusion 20b protruding from the lower end surface S2 does not contact the clamping member 401. That is, the stacked body 10 is placed on the clamping member 401 in a state where the upper end surface S1 without the protrusion 20b protruding faces downward. Therefore, the stacked body 10 supported by the clamping member 401 does not become unstable during the stacking thickness measurement process. Therefore, the stacking thickness measurement process can be advantageously performed after the process of forming the stacked body 10 by the punching device 130.
[0107] In the present embodiment, when the permanent magnet 12 is attached to the magnetic socket 16 of the laminated body 10 by the magnet attachment device 500, the protrusion 20b protruding from the lower end surface S2 does not contact the lower die 510 (base member 511). That is, the laminated body 10 is placed on the lower die 510 in a state where the upper end surface S1 without the protrusion 20b protruding faces downward. Therefore, the laminated body 10 supported by the lower die 510 does not become unstable during the magnet attachment process. Therefore, the magnet attachment process can be advantageously performed after the process of forming the laminated body 10 by the punching device 130.
[0108] In the present embodiment, the stacked body 10 formed by the punching device 130 is inverted by the inverting device 300 so that the lower end surface S2 faces upward and the protrusion 20b protrudes upward. Therefore, in the subsequent stacking thickness measurement process or magnet attachment process, the upper end surface S1 without the protrusion 20b protruding abuts against the upper surface (support surface) of the clamping member 401 or the lower mold 510. Accordingly, the stacked body 10 can be supported more stably by the clamping member 401 or the lower mold 510.
[0109] In the present embodiment, the stack rivet 20 is a V-shaped stack rivet, and the protrusion 20b from the lower end surface S2 tends to be larger. However, as described above, the stacked body 10 is placed on the clamping member 401 or the lower die 510 in a state where the upper end surface S1 without the protrusion 20b protruding faces downward. Therefore, even if the stacked body 10 includes a V-shaped stack rivet, the stacked body 10 can be supported more stably by the clamping member 401 or the lower die 510.
[0110] In the present embodiment, the load L1 for pressing the temporary laminate 11 is set to be equal to or greater than the load L3 during the molding of the laminate 10 (for example, the injection of the molten resin into the magnetic socket 16). Therefore, since the temporary laminate 11 is sufficiently pressed, the springback during the molding of the laminate 10 is prevented. In other words, by setting the load L1 when pressing the temporary laminate 11 to be equal to or greater than the load L3 when molding the laminate 10, the stacking thickness of the laminate 10 is less likely to change before and after the molding of the laminate 10. Accordingly, the molding process after the pressing process can be advantageously performed.
[0111] [Modifications]
[0112] Although the embodiments according to the present disclosure have been described in detail above, various modifications may be made to the above-described embodiments within the scope of the gist of the present invention.
[0113] (1) Although the stacked body 10 formed by the punching device 130 is inverted by the inverting device 300 and then conveyed to the stacked thickness measuring device 400 and the magnet attaching device 500 in the above-described embodiment, the manufacturing device 100 may not include the inverting device 300, and may convey the stacked body 10 in an upright state to the stacked thickness measuring device 400 and the magnet attaching device 500 without inverting the stacked body 10. Specifically, as Figure 8As shown, the clamping part 401 may include a plurality of openings 401a. The plurality of openings 401a can respectively accommodate the protrusions 20b protruding downward from the lower end surface S2 of the stack 10. The opening 401a can be a through hole that penetrates the clamping part 401, or can be a recess provided on the upper surface of the clamping part 401. Alternatively, an opening that can accommodate all the plurality of protrusions 20b protruding downward from the lower end surface S2 of the stack 10 can be provided in the clamping part 401. For example, the opening can be an annular groove. An opening similar to the opening 401a of the clamping part 401 can be provided in the base part 511 of the lower mold 510 of the magnet attachment device 500. In these cases, since the protrusion 20b of the stack rivet 20 is accommodated in the opening portion 401a, in the subsequent stack thickness measurement process or magnet attachment process, the flat surface of the lower end surface S2 except for the protrusion 20b abuts against the upper surface (support surface) of the clamping member 401 or the lower mold 510. Accordingly, the stacked body can be supported more stably by the clamping member 401 and the base member 511 without the need to perform a process of inverting the stacked body 10.
[0114] (2) Although in the above embodiment, the base member 521 of the upper mold 520 is provided with a plurality of recessed portions 521c, one opening portion that can accommodate all of the plurality of protrusions 20b protruding upward from the lower end surface S2 of the stacked body 10 may be provided in the base member 521. For example, the opening portion may be an annular groove.
[0115] (3) In the case where the upper mold 520 is not provided with the recessed portion 521 c , the protrusion 20 b protruding from the lower end surface S2 of the stacked body 10 may abut against the lower surface of the upper mold 520 .
[0116] (4) The opening may be provided in the lower surface of the clamping member 402, and the protrusion 20b may be accommodated in the opening when the clamping members 401, 402 clamp the stacked body 10. At this time, the lower end surface S2 of the stacked body 10 excluding the protrusion 20b abuts against the lower surface of the clamping member 402.
[0117] (5) As shown in FIG. 9 , the manufacturing device 100 may further include a stacked rivet measuring device 600, which includes a support member 601 and a sensor 602. The stacked rivet measuring device 600 may measure the protrusion amount of the protrusion 20 b of the stacked rivet 20 or the depth of the recess 20 a of the stacked rivet 20. The support member 601 is not particularly limited as long as it can support the stacked body 10, and the support member may be, for example, a rectangular flat plate. The sensor 602 may be, for example, a non-contact or contact distance sensor.
[0118] Specifically, Fig. 9AAs shown, the stacked body 10 in an inverted state inverted by the inverting device 300 can be placed on the support member 601, and the protrusion amount of the protrusion 20b protruding upward can be measured from above the stacked body 10 by the sensor 602. Fig. 9B As shown, the stacked body 10 in an upright state can be placed on a support member 601, and the depth of the recessed portion 20a included in the upper end surface S1 facing upward can be measured from above the stacked body 10 using a sensor 602. Fig. 9C As shown, a plurality of through holes 601a capable of accommodating the protrusions 20b of the stack rivet 20 may be provided in the support member 601. The stacked body 10 in an upright state may be placed on the support member 601 so that each protrusion 20b is located in each through hole 601a, and the protrusion amount of the protrusion 20b protruding downward may be measured from below the support member 601 by the sensor 602. In these cases, it is possible to determine whether the lower end surface S2 faces upward or downward based on the detection of the presence of the protrusion 20b or the recess 20a by the sensor 602.
[0119] When the stacking thickness of the stacked body 10 is greater than the standard, at least one punched component W can be removed (peeled off) from the stacked body 10 to adjust the stacking thickness. However, if the punched component W is mistakenly removed from the lower end surface S2 side of the stacked body 10, the punched component W2 provided with the through hole 22 may be removed. Therefore, since the entire protrusion 20b inserted into the through hole 22 is exposed to the outside, the protrusion amount of the protrusion 20b from the lower end surface S2 of the stacked body 10 increases. In this case, the stacked body 10 may be in a more unstable state. At this time, it is possible to determine whether the punched component W is mistakenly removed from the lower end surface S2 side based on the detection of the protrusion amount change of the protrusion 20b performed by the sensor 602 as described above.
[0120] (6) Although the stacking thickness of the stacked body 10 is measured after the stacked body 10 is formed and before the stacked body 10 is molded in the above-described embodiment, the stacking thickness measurement process of the stacked body 10 may be performed at any time after the stacked body 10 is formed. For example, the stacking thickness of the stacked body 10 may be measured after the stacked body 10 is molded. In this case, the stacking thickness of the stacked body 10 is also measured after the temporary stacked body 11 is pressed with the load L1 so that the stacking thickness of the stacked body 10 is difficult to change, so that the stacking thickness of the stacked body 10 can be measured more accurately.
[0121] (7) Although the laminated body 10 is molded in the above embodiment, other processes may be performed on the laminated body 10. For example, the peripheral surface of the laminated body 10 may be welded, or an identification code may be formed on the surface of the laminated body 10 (engraving process).
[0122] In the case where the stack 10 is subjected to welding processing, a plurality of punched parts W are combined by a weld bead. If the temporary stack 11 is subjected to welding processing while being pressed with a load P3 without being subjected to a pressing processing, a plurality of stamped parts W are combined together by a weld bead in a state where the gaps between the plurality of stamped parts W are reduced to a certain extent. However, since a plurality of punched parts W tend to expand in the stacking direction due to springback, damage (cracks, etc.) may occur in the weld bead. However, since the stacking thickness of the stack 10 of the present disclosure hardly changes before and after the processing of the stack 10, damage to the weld bead is less likely to occur.
[0123] In the case where the stack 10 is subjected to an imprinting process, an identification code is formed by irradiating the surface (e.g., the upper end face or the lower end face) of the stack 10 with a laser beam. If the temporary stack 11 has not been subjected to a pressing process, since the stacking thickness of the stack 10 is unstable, when the stack is irradiated with a laser beam to form an identification code on the surface of the stack 10, the distance between the laser source and the stack 10 may change. Therefore, the quality of the identification code may change. However, since the stacking thickness of the stack 10 of the present disclosure is almost unchanged before and after the processing of the stack 10, the quality of the identification code formed on the surface of the stack 10 can be advantageously maintained. It should be noted that during the imprinting process of the stack 10, the stack 10 is preferably pressed with a predetermined load (e.g., load L3).
[0124] The identification code has a function of storing individual information (for example, product type, manufacturing date and time, materials used therein or manufacturing line), which is used to identify the individual of the rotor laminated core 1 having the identification code. The identification code is not particularly limited as long as the individual information can be stored by a combination of light patterns and dark patterns, and can be, for example, a barcode or a two-dimensional code. The two-dimensional code can be, for example, a QR code (registered trademark), a data matrix, or a Vericode. Alternatively, the identification code can also be configured by combining various other colors besides white and black, as long as its contrast can be improved. For example, the identification code can be a layered two-dimensional code (a two-dimensional shape code obtained by multi-layering color information). The layered two-dimensional code can be, for example, a PM code (registered trademark) or the like.
[0125] (8) Although in the above embodiment, the temporary stack 11 is pressed by the pressing device 200 to form the stack 10 and then the stack 10 is inverted by the inverting device 300, the temporary stack 11 may be pressed by the pressing device 200 to form the stack 10 after being inverted by the inverting device 300.
[0126] (9) The manufacturing apparatus 100 may not include the pressing device 200 , and the pressing of the temporary stack 11 by the pressing device 200 may not be performed.
[0127] (10) The stacking rivets 20 used to interlock the blanked parts W may be so-called cut-and-stand stacking rivets, such as Fig.10 As shown. The cut-stand rivet is formed by a cut-stand piece that is partially cut from the electromagnetic steel sheet ES. The terminal end of the cut-stand piece is fitted to the inner peripheral surface of the through hole 22 of the adjacent punched part W2 or the cut-stand piece of the adjacent punched part W1, so that the plurality of punched parts W are interlocked with each other. In this case, the protrusion amount of the protrusion 20b from the lower end surface S2 also tends to become larger. As described above, even if the stacked body 10 includes the cut-stand rivet, the stacked body 10 can be supported more stably.
[0128] (11) The stack rivet 20 for interlocking the punched parts W with each other may be a so-called round stack rivet having a cylindrical shape.
[0129] (12) A magnet group composed of two or more permanent magnets 12 can be inserted into each magnetic socket 16. In this case, in one magnetic socket 16, multiple permanent magnets 12 can be arranged in the length direction of the magnetic socket 16. In one magnetic socket 16, multiple permanent magnets 12 can also be arranged in the extension direction of the magnetic socket 16. In one magnetic socket 16, multiple permanent magnets 12 can be arranged in the extension direction while multiple permanent magnets 12 can be arranged in the length direction.
[0130] (13) In the above-described embodiment, the resin particles P contained in the containing hole 421b of the upper mold 420 are melted by the built-in heat source 422, and the molten resin is injected into the magnetic socket 16 into which the permanent magnet 12 is inserted. However, the permanent magnet 12 may also be retained in the magnetic socket 16 by various other methods. For example, the magnetic socket 16 may be filled with resin by heating the laminated body 10 in a state where the permanent magnet 12 and the resin particles P are inserted into the magnetic socket 16 and melting the resin particles P in the magnetic socket 16. Furthermore, for example, the magnetic socket 16 may be filled with resin by inserting the heated permanent magnet 12 into the magnetic socket 16 in a state where the resin particles P are inserted into the magnetic socket 16 and melting the resin particles P by the heat of the permanent magnet 12.
[0131] (14) Although the rotor laminated core 1 is described in the above embodiment, the present invention can also be applied to a stator laminated core. In this case, the stator laminated core may be a split type stator laminated core combining a plurality of core blocks or a non-split type stator laminated core.
[0132] [Summarize]
[0133] Example 1. A method for manufacturing a laminated core (1) according to an example of the present disclosure comprises: stacking a plurality of punched parts (W) to form a laminate (10), the laminate (10) comprising a pair of (first and second) end faces (S2, S1), the plurality of punched parts (W) being interlocked in the stacking direction of the laminate (10) by a stacking rivet (20), and the laminate (10) being formed so that a protrusion (20b) of the stacking rivet (20) protrudes downward from a first end face (S2) in a downward state; placing the laminate (10) on a support portion (401, 510) so that the protrusion (20b) does not contact a support surface of the support portion (401, 510); and processing the laminate (10) in a state where the laminate (10) is placed on the support portion (401, 510). In this case, the protrusion (20b) of the stack rivet (20) does not contact the support surface of the support portion (401, 510). Therefore, the stacked body (10) placed on the support portion (401, 510) does not become unstable during subsequent processing. Accordingly, subsequent processing can be advantageously performed.
[0134] Example 2. In the method of Example 1, placing the stacked body (10) on the support portion (401, 510) may include placing the stacked body (10) on the support portion (401, 510) after inverting the stacked body (10) so that the first end surface (S2) faces upward and the protrusion (20b) protrudes upward. In this case, the second end surface (S1) located on the side where no protrusion (20b) protrudes abuts against the support surface of the support portion (401, 510). Therefore, the stacked body (10) can be supported more stably by the support portion (401, 510).
[0135] Example 3. In the method of Example 1, placing the stack (10) on the support (401) may include supporting the end face (S2) of the stack on the support surface so that the protrusion is located in the opening (401a) provided in the support surface of the support portion (401). In this case, since the protrusion (20b) of the stack rivet (20) is accommodated in the opening (20a), the first end face (S2) located on the side where the protrusion (20b) protrudes abuts the support surface of the support portion (401). Therefore, the stack (10) can be supported more stably by the support portion (401).
[0136] Example 4. In the method of any one of Examples 1 to 3, the stack rivet (20) may be a V-shaped stack rivet or a cut-and-stand stack rivet. In this case, even if the stack includes a V-shaped stack rivet or a cut-and-stand stack rivet whose protrusion (20b) tends to have a larger protrusion amount, the stack can be supported more stably by the support portion (401, 510).
[0137] Example 5. The method of any one of Examples 1 to 4 may also include measuring the amount of protrusion of the protrusion (20b) from the first end face (S2). In this case, it is possible to determine whether the first end face (S2) is facing upward or downward based on the detection of the presence of the protrusion (20b). Moreover, when the stacking thickness of the stack (10) is greater than the standard, at least one punched component (W) can be removed (peeled off) from the stack (10) to adjust the stacking thickness, and it is possible to determine whether the punched component (W) is erroneously removed from the first end face (S2) side based on the detection of the change in the protrusion amount of the protrusion (20b).
[0138] Example 6. The method of any one of Examples 1 to 5 may further include measuring the depth of the recess (20a) of the stack rivet (20) on the second end surface (S1). In this case, it is possible to determine whether the second end surface (S1) is facing upward or downward based on the detection of the presence of the recess (20a).
[0139] Example 7. The method of any one of Examples 1 to 6 may further include pressing the stack (11) with a first load (L1). Processing of the stack (10) may include: after pressing the stack (10) with the first load (L1), processing the stack (10) while pressing the stack (10) with a second load (L3) equal to or less than the first load (L1). In this case, the first load (L1) for pressing the stack (11) may be equal to or greater than the second load (L3) when processing the pressed stack (10). Therefore, since the stack (11) is sufficiently pressed, rebound during processing of the pressed stack (10) is prevented. In other words, by setting the load (first load (L1) when pressing the stack (11) to be equal to or greater than the load (second load L3) when processing the pressed stack (10), the stacking thickness of the pressed stack (10) is less likely to change before and after processing. Accordingly, processing after the pressing process can be advantageously performed.
[0140] This application is based on patent application JP2018-041009 filed on March 7, 2018, the contents of which are incorporated herein by reference.
[0141] Industrial Applicability
[0142] According to the manufacturing method of the laminated core of the present disclosure, subsequent processing can be advantageously performed after the laminated bodies are interlocked by the stack rivets.
Claims
1. A method for manufacturing a laminated iron core, the method for manufacturing a laminated iron core forming a laminated body by stacking a plurality of punched parts, the laminated body comprising a pair of first end faces and a second end face, the first end face having a through hole, and the plurality of punched parts being interlocked in a stacking direction of the laminated body by stacking rivets, the manufacturing method include: forming the stacked body so that the protrusion of the stacked rivet extends at least the length of the through hole, and the extended protrusion protrudes downward from the first end surface in a downward state; placing the stacked body on a support portion so that the protrusions are not in contact with a support surface of the support portion; measuring a protrusion amount of the protrusion from the first end surface to determine whether the first end surface faces upward or downward; as well as The stacked body is processed in a state where the stacked body is placed on the support portion.
2. A method for manufacturing a laminated iron core, the method for manufacturing a laminated iron core forming a laminated body by stacking a plurality of punched parts, the laminated body comprising a pair of first end faces and a second end face, the first end face having a through hole, and the plurality of punched parts being interlocked in a stacking direction of the laminated body by stacking rivets, the manufacturing method include: forming the stacked body so that the protrusion of the stacked rivet extends at least the length of the through hole, and the extended protrusion protrudes downward from the first end surface in a downward state; placing the stacked body on a support portion so that the protrusions are not in contact with a support surface of the support portion; measuring the depth of the recess of the stack rivet on the second end surface to determine whether the first end surface faces upward or downward; as well as The stacked body is processed in a state where the stacked body is placed on the support portion.
3. The manufacturing method according to claim 1 or 2, in, Placing the stacked body on the support portion includes placing the stacked body on the support portion after inverting the stacked body so that the first end surface faces upward and the protrusion protrudes upward.
4. The manufacturing method according to claim 1 or 2, in, Placing the stacked body on the support portion includes supporting the end surface of the stacked body on the support surface of the support portion so that the protrusion is located within an opening provided in the support surface.
5. The manufacturing method according to claim 1 or 2, in, The stack rivet is a V-shaped stack rivet or a cut-and-sew stack rivet.
6. The manufacturing method according to claim 3, in, The stack rivet is a V-shaped stack rivet or a cut-and-sew stack rivet.
7. The manufacturing method according to claim 4, in, The stack rivet is a V-shaped stack rivet or a cut-and-sew stack rivet.
8. The manufacturing method according to claim 1 or 2, further comprising: include: The stack is pressed with a first load, wherein The processing of the stacked body includes, after pressing the stacked body with the first load, processing the stacked body while pressing the stacked body with a second load, the second load being equal to or smaller than the first load.
9. The manufacturing method according to claim 3, further comprising: include: The stack is pressed with a first load, wherein The processing of the stacked body includes, after pressing the stacked body with the first load, processing the stacked body while pressing the stacked body with a second load, the second load being equal to or smaller than the first load.
10. The manufacturing method according to claim 4, further comprising: include: The stack is pressed with a first load, wherein The processing of the stacked body includes, after pressing the stacked body with the first load, processing the stacked body while pressing the stacked body with a second load, the second load being equal to or smaller than the first load.
11. The manufacturing method according to claim 5, further comprising: include: The stack is pressed with a first load, wherein The processing of the stacked body includes, after pressing the stacked body with the first load, processing the stacked body while pressing the stacked body with a second load, the second load being equal to or smaller than the first load.
12. The manufacturing method according to claim 6, further comprising: include: The stack is pressed with a first load, wherein The processing of the stacked body includes, after pressing the stacked body with the first load, processing the stacked body while pressing the stacked body with a second load, the second load being equal to or smaller than the first load.
13. The manufacturing method according to claim 7, further comprising: include: The stack is pressed with a first load, wherein The processing of the stacked body includes, after pressing the stacked body with the first load, processing the stacked body while pressing the stacked body with a second load, the second load being equal to or smaller than the first load.