A semiconductor device and its fabrication method

By forming a dielectric layer on the sidewalls of the shallow isolation trench and performing chemical mechanical polishing, the problem of material etching on the sidewalls of the shallow isolation trench is solved, and the performance and integration of the semiconductor device are improved.

CN111968947BActive Publication Date: 2024-10-25SEMICON MFG INT (SHANGHAI) CORP +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN201910417235.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-05-20
Publication Date
2024-10-25
Estimated Expiration
2039-05-20

AI Technical Summary

Technical Problem

In the prior art, the sidewall material of the shallow isolation trench is etched to varying degrees during the etching process, which affects the performance of the semiconductor device.

Method used

A first dielectric layer is formed on the sidewalls of the shallow isolation trench to protect the sidewall material from being etched, and the second dielectric layer is planarized through chemical mechanical polishing during the etching and removal process of the single diffusion interruption material. , control the width of the shallow isolation trench.

Benefits of technology

It effectively protects the shallow isolation trench sidewall materials, avoids performance damage, and ensures the performance stability and integration of semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111968947B_ABST
    Figure CN111968947B_ABST
Patent Text Reader

Abstract

The present invention provides a method for forming a semiconductor device, comprising the following steps: providing a substrate, on which at least two adjacent transistor regions are formed; a shallow isolation trench is formed at the junction of the adjacent transistor regions. In order to protect the material on the sidewalls of the shallow isolation trench from being etched to varying degrees in subsequent etching, a first dielectric layer can be formed on the sidewalls of the shallow isolation trench to protect the material on the sidewalls of the shallow isolation trench from being etched away, to prevent the width of the shallow isolation trench from increasing, so that the performance of the semiconductor device is better. Furthermore, the present invention also provides a semiconductor device, in which a first dielectric layer is formed on the sidewalls of the shallow isolation trench to protect the material on the sidewalls of the shallow isolation trench from being etched away, to prevent the width of the shallow isolation trench from increasing, so that the performance of the semiconductor device is better.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for forming the same. Background Art

[0002] In the field of semiconductor manufacturing, isolation structures are often used to isolate a number of materials disposed on a semiconductor substrate. Among these isolation structures, a shallow isolation trench structure is used because the shallow isolation trench is well suited for semiconductor devices with smaller device sizes. Similarly, a single diffusion break (SDB) is a technology used for technology expansion to obtain integrated circuits with the same functions in a smaller design area. The single diffusion break can be used to reduce the circuit area of ​​a semiconductor device, thereby supporting the formation of high-density integrated circuits.

[0003] However, in the current single diffusion interruption process, due to the source / drain cavity formed near the shallow isolation trench area, the material retained on the sidewall of the shallow isolation trench of the single diffusion interruption will be etched to varying degrees, affecting the integrity of the sidewall material of the shallow isolation trench, thereby affecting the performance of the semiconductor device. Figure 1a-1f As shown, in the prior art, the process of the semiconductor device 10 is as follows Figure 1a As shown, a substrate is provided, and a transistor region is formed on the substrate. Figure 1b As shown, the transistor region is etched to form a shallow isolation trench 101. Figure 1c As shown, the shallow isolation trench 101 is filled with an isolation material 103. Figure 1d , 1e As shown, the isolation material 103 is etched and removed. Figure 1f As shown, an oxide film layer is filled in the side of the transistor region away from the substrate and in the shallow isolation trench 101 to form a semiconductor device 10. In this process, after the shallow isolation trench 101 is formed, the isolation material 103 is etched, which will inevitably cause different degrees of etching on the material of the sidewall 102 of the shallow isolation trench 101, making the width of the shallow isolation trench 101 wider, thereby affecting the performance of the semiconductor device 10.

[0004] Therefore, the present invention aims to provide a method for manufacturing a semiconductor device, which can effectively protect the material on the sidewall of the shallow isolation trench from being etched and damaged, thereby preventing the performance of the semiconductor device from being affected. Summary of the invention

[0005] The purpose of the present invention is to solve the problem in the prior art that the material on the sidewall of the shallow isolation trench is etched to different degrees during the etching operation, which affects the performance of the semiconductor device.

[0006] The present invention provides a method for forming a semiconductor device, comprising the following steps: providing a substrate, on which at least two adjacent transistor regions are formed; forming a shallow isolation trench at the junction of the adjacent transistor regions; forming a first dielectric layer on the sidewall of the shallow isolation trench; filling a single diffusion interruption material in the shallow isolation trench on a side of the transistor region away from the substrate, and etching and removing the single diffusion interruption material.

[0007] By adopting the above technical solution, a shallow isolation trench is formed at the junction of adjacent transistor regions. In order to protect the material on the sidewall of the shallow isolation trench from being etched to varying degrees in subsequent etching, a first dielectric layer can be formed on the sidewall of the shallow isolation trench to protect the material on the sidewall of the shallow isolation trench from being etched away, thereby improving the performance of the semiconductor device.

[0008] Furthermore, at least two adjacent transistor regions are formed on the substrate, including the following steps: at least two fins are formed on the substrate; a cushion oxide layer is deposited around the at least two fins; a coating layer is deposited on a side of the cushion oxide layer away from the substrate and around the at least two fins; and a second dielectric layer is deposited on a side of the coating layer away from the substrate.

[0009] By adopting the above technical solution, at least two fins are formed on the substrate; a pad oxide layer is deposited around the at least two fins; a cladding layer is deposited on the side of the pad oxide layer away from the substrate and around the at least two fins; a second dielectric layer is deposited on the side of the cladding layer away from the substrate to form a complete semiconductor device. The second dielectric layer is deposited on the side of the cladding layer away from the substrate to protect the cladding layer and the substrate materials.

[0010] Furthermore, a shallow isolation trench is formed at the junction of at least two adjacent transistor regions, including: etching the second dielectric layer and the cladding layer at the junction of the two adjacent transistor regions to form the shallow isolation trench.

[0011] The above technical solution is adopted to form a shallow isolation trench, which is used to subsequently form a shallow isolation trench structure to isolate numerous components on the semiconductor device.

[0012] Furthermore, before forming the shallow isolation trench, the method further includes: performing chemical mechanical polishing on a side of the second dielectric layer away from the substrate.

[0013] By adopting the above technical solution, chemical-mechanical planarization (CMP), also known as chemical-mechanical polishing, is performed on the side of the second dielectric layer away from the substrate. Chemical-mechanical polishing is a technology in the semiconductor device manufacturing process. Chemical etching is used to flatten the second dielectric layer. The surface of the planarized second dielectric layer makes it easier to form the pattern in dry etching. The smooth surface of the second dielectric layer also makes it possible to use smaller metal patterns, thereby improving the integration of semiconductor devices.

[0014] Furthermore, when the single diffusion interruption material is etched and removed, it includes: etching the single diffusion interruption material filled on the side of the transistor region away from the substrate; and removing the single diffusion interruption material filled in the shallow isolation trench.

[0015] By adopting the above technical solution, the single diffusion interrupt material filled on the side of the transistor area away from the substrate is etched, and the single diffusion interrupt material filled in the shallow isolation trench is removed, so as to protect the width of the shallow isolation trench from changing in subsequent processes, so that the width of the shallow isolation trench is easy to control, so as to form a semiconductor device with better performance.

[0016] Further, L>2D, wherein L is the width of the shallow isolation trench, and D is the thickness of the first dielectric layer.

[0017] By adopting the above technical solution, L>2D, where L is the width of the shallow isolation trench and D is the thickness of the first dielectric layer, the first dielectric layer can be filled on the side wall of the shallow isolation trench to protect the material of the side wall of the shallow isolation trench from being etched away, thereby improving the performance of the semiconductor device.

[0018] Furthermore, the thickness of the second dielectric layer is greater than or equal to the width of the first dielectric layer.

[0019] Furthermore, after etching and removing the single diffusion interruption material, the method further includes: performing dielectric deposition treatment on the sidewall of the shallow isolation trench; and / or depositing an oxide film layer on the side of the transistor region away from the substrate in the shallow isolation trench.

[0020] By adopting the above technical solution, an oxide film layer is deposited in a shallow isolation trench on a side of the transistor region away from the substrate, so as to improve the performance of the semiconductor device.

[0021] Further, the material of the substrate is silicon carbide or silicon germanium; the material of the pad oxide layer is silicon oxide or silicon oxynitride;

[0022] The material of the first dielectric layer and the second dielectric layer is at least one of titanium nitride, hafnium oxide, hafnium oxynitride, hafnium silicon oxide, and silicon nitride;

[0023] The material of the oxide film layer is at least one of silicon oxide, silicon oxynitride and titanium oxide; the material of the coating layer is silicon or silicon dioxide.

[0024] Furthermore, the present invention also provides a semiconductor device, which is manufactured based on the above-mentioned method for forming a semiconductor device.

[0025] By adopting the above technical scheme, the present invention also provides a semiconductor device, in which a first dielectric layer is formed on the sidewall of the shallow isolation trench, so as to protect the material on the sidewall of the shallow isolation trench from being etched to varying degrees in subsequent etching, thereby improving the performance of the semiconductor device.

[0026] The beneficial effects of the present invention are:

[0027] The present invention provides a method for forming a semiconductor device, comprising the following steps: providing a substrate, on which at least two adjacent transistor regions are formed; and forming a shallow isolation trench at the junction of the adjacent transistor regions. In order to protect the material on the sidewalls of the shallow isolation trench from being etched to varying degrees in subsequent etching, a first dielectric layer can be formed on the sidewalls of the shallow isolation trench to protect the material on the sidewalls of the shallow isolation trench from being etched away, thereby improving the performance of the semiconductor device. Furthermore, the present invention also provides a semiconductor device, in which a first dielectric layer is formed on the sidewalls of the shallow isolation trench to protect the material on the sidewalls of the shallow isolation trench from being etched away, thereby preventing the width of the shallow isolation trench from becoming larger, thereby improving the performance of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1a-1f A process flow chart of semiconductor device manufacturing provided by the prior art;

[0029] Figure 2 A flow chart of a method for forming a semiconductor device provided by an embodiment of the present invention;

[0030] Figure 3a-3g A process flow chart of manufacturing a semiconductor device provided by an embodiment of the present invention.

[0031] Prior art reference numerals:

[0032] 10: semiconductor device; 101: shallow isolation trench; 102: sidewall; 103: isolation material;

[0033] Figure numerals of this embodiment:

[0034] 300: semiconductor device; 310: substrate; 311: transistor region; 312: first fin; 313: second fin; 320: NMOS transistor; 330: PMOS transistor; 340: shallow isolation trench; 350: pad oxide layer; 360: cladding layer; 3701: first dielectric layer; 3702: second dielectric layer; 380: oxide film layer; 390: single diffusion interrupt material. DETAILED DESCRIPTION

[0035] The following specific embodiments illustrate the implementation of the present invention, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. Although the description of the present invention will be introduced in conjunction with the preferred embodiment, this does not mean that the features of this invention are limited to this implementation. On the contrary, the purpose of introducing the invention in conjunction with the implementation is to cover other options or modifications that may extend based on the claims of the present invention. In order to provide a deep understanding of the present invention, the following description will include many specific details. The present invention can also be implemented without using these details. In addition, in order to avoid confusion or blurring the focus of the present invention, some specific details will be omitted in the description. It should be noted that the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict.

[0036] It should be noted that in this specification, similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, it does not need to be further defined and explained in the subsequent drawings.

[0037] In the description of this embodiment, it should be noted that the terms "upper", "lower", "inner", "bottom", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, or are the orientations or positional relationships in which the inventive product is usually placed when used. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0038] The terms “first”, “second”, etc. are only used for distinguishing descriptions and should not be understood as indicating or implying relative importance.

[0039] In the description of this embodiment, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in this embodiment can be understood according to specific circumstances.

[0040] In order to make the objectives, technical solutions and advantages of the present invention more clear, the embodiments of the present invention will be further described in detail below with reference to the accompanying drawings.

[0041] The invention aims to solve the problem in the prior art that the material on the sidewall of the shallow isolation trench is etched to different degrees during the etching operation, thereby affecting the performance of the semiconductor device.

[0042] The present invention provides a method for forming a semiconductor device, such as Figure 2 As shown, the following steps are included:

[0043] S11: providing a substrate, on which at least two adjacent transistor regions are formed; a shallow isolation trench is formed at the junction of the adjacent transistor regions.

[0044] like Figure 3a As shown, a substrate 310 is provided, on which at least two adjacent transistor regions 311 are formed, and a shallow isolation trench 340 is formed at the junction of at least two adjacent transistor regions 311. Specifically, the transistor region 311 may be formed as follows Figure 3a The NMOS transistor 320 and the PMOS transistor 330 shown in the figure, the NMOS transistor 320 and the PMOS transistor 330 together form a CMOS transistor (complementary metal oxide semiconductor), that is, the semiconductor device 300 referred to in this embodiment. At least two adjacent transistor regions 311 are distributed on the substrate 310 in parallel with each other along the length extension direction of the substrate 310. In addition, the at least two adjacent transistor regions 311 may not be limited to the embodiment of the present invention. Figure 3a The two transistor regions 311 shown may also be three adjacent transistor regions 311 or other numbers of transistor regions 311, which may be selected according to actual needs, and this embodiment does not specifically limit this. The widths of the transistor regions 311 are generally equal, or may be unequal, and the widths of the transistor regions 311 may also be set according to actual needs, and this embodiment does not specifically limit this.

[0045] In addition, the material of the substrate 310 is silicon carbide or silicon germanium or other materials. In detail, for the PMOS transistor 330, the material of its substrate 310 can be silicon germanium, etc., which is used to enhance the mobility of the majority carriers in the channel of the PMOS transistor 330, thereby enhancing the performance of the PMOS transistor 330. For the NMOS transistor 320, the material of its substrate 310 can be silicon carbide, etc., which is used to enhance the mobility of the majority carriers in the channel of the NMOS transistor 320, thereby enhancing the performance of the NMOS transistor 320. The specific material selection of the substrate 310 is set according to actual needs, and this embodiment does not specifically limit this.

[0046] like Figure 3a As shown, at least two adjacent transistor regions 311 are formed on the substrate 310, including the following steps: at least two fins are formed on the substrate 310; a cushion oxide layer 350 is deposited around the at least two fins; a cladding layer 360 is deposited on a side of the cushion oxide layer 350 away from the substrate 310 and around the at least two fins; and a second dielectric layer 3702 is deposited on a side of the cladding layer 360 away from the substrate 310.

[0047] Specifically, at least two fins may include: Figure 3a The first fin 312 and the second fin 313 are shown. The first fin 312 and the second fin 313 can be formed by methods or processes such as photolithography patterning and etching processes. Further, a pad oxide layer 350 is deposited around the first fin 312 and the second fin 313, and a coating layer 360 is deposited on the side of the pad oxide layer 350 away from the substrate 310 and on the first fin 312 and the second fin 313, so as to form a complementary transistor having an NMOS transistor 320 and a PMOS transistor 330, that is, a CMOS transistor, that is, a semiconductor device 300 referred to in this embodiment. Since the CMOS transistor is composed of a PMOS transistor 330 and an NMOS transistor 320, it is characterized by low power consumption and strong durability. Specifically, a gate circuit composed of a pair of MOS in CMOS is either turned on when the PMOS transistor 330 is turned on, or when the NMOS transistor 320 is turned on, or both are turned off, which is much more efficient than a linear triode (BJT), so the power consumption is very low. In addition, the material of the pad oxide layer 350 is silicon oxide or silicon oxynitride or other materials, which are selected according to actual needs and are not specifically limited in this embodiment.

[0048] More specifically, Figure 3a As shown, a second dielectric layer 3702 is deposited on the side of the cladding layer 360 away from the substrate 310. Specifically, the second dielectric layer 3702 is deposited on the side of the cladding layer 360 away from the substrate 310. The second dielectric layer 3702 is used to maintain the insulation between the circuit and the layers of the semiconductor device 300, and is also commonly referred to as a substrate. The material of the cladding layer 360 is silicon or silicon dioxide or other materials, which is used to protect the stability of the material of the semiconductor device 300. The specific selection is based on actual needs, and this embodiment does not specifically limit this.

[0049] like Figure 3b As shown, a shallow isolation trench 340 is formed at the junction of at least two adjacent transistor regions 311 , including: etching the second dielectric layer 3702 and the cladding layer 360 at the junction of two adjacent transistor regions 311 to form the shallow isolation trench 340 .

[0050] Specifically, the adjacent transistor regions 311 are etched (for example, by using conventional photolithography patterning and etching processes), and shallow isolation trenches 340 are formed at the junctions of the adjacent transistor regions 311. In this embodiment, the second dielectric layer 3702 and the cladding layer 360 at the junctions of two adjacent transistor regions 311 are etched, so that shallow isolation trenches 340 are formed at the junctions of the NMOS transistor 320 and the PMOS transistor 330. The shallow isolation trenches 340 are used to subsequently fill oxide therein to form an isolation structure, which is used to isolate numerous components on the semiconductor device 300.

[0051] like Figure 3a , 3b As shown, before forming the shallow isolation trench 340 , the process further includes: performing chemical mechanical polishing on the side of the second dielectric layer 3702 away from the substrate 310 .

[0052] Specifically, before forming the shallow isolation trench 340, the process further includes: performing chemical-mechanical polishing (ILD0 CMP, Interlayer dielectric 0Chemical-Mechanical Polishing) on ​​the side of the second dielectric layer 3702 away from the substrate 310. Chemical-mechanical polishing is a technology in the semiconductor device manufacturing process. Chemical etching is used to flatten the second dielectric layer 3702. The surface of the planarized second dielectric layer 3702 makes it easier to form the pattern in the dry etching. The smooth surface of the second dielectric layer 3702 also makes it possible to use smaller metal patterns, thereby improving the integration of the semiconductor device 300.

[0053] S12: forming a first dielectric layer on the sidewalls of the shallow isolation trench.

[0054] like Figure 3c As shown, specifically, a first dielectric layer 3701 is formed on the sidewall of the shallow isolation trench 340. In order to protect the material on the sidewall of the shallow isolation trench 340 from being etched to varying degrees in subsequent etching, a first dielectric layer 3701 (ALD SIN DEP) may be formed on the sidewall of the shallow isolation trench 340 to protect the material on the sidewall of the shallow isolation trench 340 from being etched away, so that the performance of the semiconductor device 300 is better. It can also be used to control the width of the shallow isolation trench 340 to be unaffected, prevent the size of the semiconductor device 300 from changing, and make the performance of the semiconductor device 300 better.

[0055] The material of the first dielectric layer 3701 is at least one of titanium nitride, hafnium oxide, hafnium oxynitride, hafnium silicon oxide, and silicon nitride, which is selected according to actual needs, and this embodiment does not specifically limit this. In addition, it should be understood that when the first dielectric layer 3701 is formed on the sidewall of the shallow isolation trench 340, the second dielectric layer 3702 can also be deposited on the side of the transistor region 311 away from the substrate 310 at the same time, that is, the thickness of the second dielectric layer 3702 becomes thicker after this step, and the specific thickness of the deposited second dielectric layer 3702 is selected according to actual needs, and this embodiment does not specifically limit this.

[0056] like Figure 3c As shown, further, L>2D, wherein L is the width of the shallow isolation trench 340 and D is the thickness of the first dielectric layer 3701 .

[0057] Specifically, L>2D, where L is the width of the shallow isolation trench 340, and D is the thickness of the first dielectric layer 3701, so that the first dielectric layer 3701 can be filled on the sidewall of the shallow isolation trench 340 to protect the material of the sidewall of the shallow isolation trench 340 from being etched away, so that the performance of the semiconductor device 300 is better. The specific width of the shallow isolation trench 340, the thickness of the first dielectric layer 3701, and the ratio of the width of the shallow isolation trench 340 to the thickness of the first dielectric layer 3701 can be set according to actual needs, and this embodiment does not specifically limit this.

[0058] like Figure 3c As shown, further, the thickness of the second dielectric layer 3702 is greater than or equal to the width of the first dielectric layer 3701. Specifically, the thickness of the second dielectric layer 3702 is greater than the width of the first dielectric layer 3701, or the thickness of the second dielectric layer 3702 is equal to the width of the first dielectric layer 3701, which can be selected according to actual needs. In short, the width of the first dielectric layer 3701 should be moderate, which can be used to protect the material of the sidewall of the shallow isolation trench 340 from being etched, and can also ensure that the first dielectric layer 3701 does not affect the width of the shallow isolation trench 340 after filling the shallow isolation trench 340, so that the width of the shallow isolation trench 340 is easy to control, and further improve the performance of the semiconductor device 300.

[0059] It should be understood that the material of the second dielectric layer 3702 is at least one of titanium nitride, hafnium oxide, hafnium oxynitride, hafnium silicon oxide, and silicon nitride, which is selected according to actual needs, and this embodiment does not specifically limit this. In addition, the material of the second dielectric layer 3702 and the first dielectric layer 3701 can be the same or different, which is set according to actual needs, and this embodiment does not specifically limit this.

[0060] S13: filling a single diffusion interruption material in the shallow isolation trench and on the side of the transistor region 311 away from the substrate, and etching and removing the single diffusion interruption material.

[0061] like Figure 3d As shown, a single diffusion interrupt material 390 (SDB PH) is filled on the side of the transistor region 311 in the shallow isolation trench 340 away from the substrate 310. The single diffusion interrupt material 390 is suitable for forming a semiconductor device 300 with a shallow isolation trench 340 with a t-shaped single diffusion interruption below the 10nm node. In addition, the material of the single diffusion interrupt material 390 can be silicon dioxide or silicon oxycarbide, etc., and may not be limited to the materials given in this embodiment. The specific selection is based on actual needs, and this embodiment does not make specific limitations on this.

[0062] like Figure 3e , Figure 3f As shown, further, when the single diffusion interruption material 390 is etched and removed, it includes: etching the single diffusion interruption material 390 filled on the side of the transistor region 311 away from the substrate 310 and removing the single diffusion interruption material 390 filled in the shallow isolation trench 340 (SDB ET), and then performing single diffusion interruption material removal (SDB STRIP)

[0063] Specifically, the single diffusion interruption material 390 is filled on the side of the transistor region 311 away from the substrate 310 . The single diffusion interruption material 390 is suitable for forming a semiconductor device 300 with a t-shaped single diffusion interruption shallow isolation trench 340 structure below the 10 nm node.

[0064] The single diffusion interruption material 390 filled in the shallow isolation trench 340 is removed to protect the width of the shallow isolation trench 340 from changing in subsequent processes, so that the width of the shallow isolation trench 340 is easy to control to form a semiconductor device 300 with better performance.

[0065] like Figure 3g As shown, further, after etching and removing the single diffusion interrupt material 390, it also includes: performing dielectric deposition treatment on the sidewall of the shallow isolation trench 340; and / or depositing an oxide film layer 380 on the side of the transistor region 311 in the shallow isolation trench 340 away from the substrate 310.

[0066] Specifically, after the single diffusion interruption material 390 is etched and removed, the sidewall of the shallow isolation trench 340 is subjected to dielectric deposition processing, which can be as follows: Figure 3gAs shown, the sidewalls of the shallow isolation trench 340 are subjected to dielectric deposition treatment, which can specifically make the thickness of the first dielectric layer 3701 in the shallow isolation trench 340 thicker. Alternatively, after etching and removing the single diffusion interruption material 390, an oxide film layer 380 is deposited on the side of the transistor region 311 in the shallow isolation trench 340 away from the substrate 310 to improve the performance of the semiconductor device 300. Alternatively, after etching and removing the single diffusion interruption material 390, the sidewalls of the shallow isolation trench 340 are subjected to dielectric deposition treatment, which can be as follows Figure 3g As shown, dielectric deposition is performed on the sidewall of the shallow isolation trench 340, specifically, the thickness of the first dielectric layer 3701 in the shallow isolation trench 340 is increased. In addition, an oxide film layer 380 is deposited on the side of the transistor region 311 in the shallow isolation trench 340 away from the substrate 310 to improve the performance of the semiconductor device 300.

[0067] The material of the oxide film layer 380 can be at least one of silicon oxide, silicon oxynitride, titanium oxide, and silicon nitride, which can be selected according to actual needs, and this embodiment does not specifically limit this. In addition, the material of the oxide film layer 380 can be deposited in the shallow isolation trench 340 and on the side of the NMOS transistor 320 and the PMOS transistor 330 away from the substrate 310 by chemical vapor deposition, and the oxide film layer 380 can be flattened by chemical mechanical polishing, so that the performance of the semiconductor device 300 is better.

[0068] like Figure 3g As shown, the present invention further provides a semiconductor device 300 , which is manufactured based on the above-mentioned method for forming a semiconductor device, and will not be described in detail here.

[0069] Specifically, the semiconductor device 300 provided by the present invention provides a substrate 310, on which at least two adjacent transistor regions 311 are formed, and a shallow isolation trench 340 is formed at the junction of at least two adjacent transistor regions 311. Specifically, the transistor region 311 may be formed as follows: Figure 3a The NMOS transistor 320 and the PMOS transistor 330 shown in the figure together form a CMOS transistor, namely the semiconductor device 300 in this embodiment. At least two adjacent transistor regions 311 are distributed on the substrate 310 in parallel with each other along the length extension direction of the substrate 310.

[0070] like Figure 3gAs shown, further, in the conventional single diffusion interruption process, a first fin 312 and a second fin 313 are formed on a substrate 310, and then, parts of the first fin 312 and the second fin 313 are removed or cut (for example, by using conventional photolithography patterning and etching processes) to form a shallow isolation trench 340 at the junction of the NMOS transistor 320 and the PMOS transistor 330. Then, the shallow isolation trench 340 is filled with a single diffusion interruption material 390, i.e., a single diffusion interruption. The single diffusion interruption material 390 is suitable for forming a semiconductor device 300 with a shallow isolation trench 340 structure of a t-type single diffusion interruption below the 10nm node. In addition, the material of the single diffusion interruption material 390 can be silicon dioxide or silicon oxycarbide, etc., and may not be limited to the materials given in this embodiment. It is selected according to actual needs, and this embodiment does not specifically limit this.

[0071] like Figure 3g As shown, further, a first dielectric layer 3701 is formed on the sidewall of the shallow isolation trench 340 to protect the material on the sidewall of the shallow isolation trench 340 from being etched to varying degrees in subsequent etching, so that the performance of the semiconductor device 300 is better. The material of the first dielectric layer 3701 is at least one of titanium nitride, hafnium oxide, hafnium oxynitride, hafnium silicon oxide, and silicon nitride, which is selected according to actual needs and is not specifically limited in this embodiment.

[0072] The method for forming a semiconductor device provided in this embodiment includes the following steps: providing a substrate, on which at least two adjacent transistor regions are formed; a shallow isolation trench is formed at the junction of adjacent transistor regions; a first dielectric layer is formed on the sidewalls of the shallow isolation trench; a single diffusion interruption material is filled in the shallow isolation trench on the side of the transistor region away from the substrate, and the single diffusion interruption material is etched and removed. In order to protect the material on the sidewall of the shallow isolation trench from being etched to varying degrees in subsequent etching, a first dielectric layer can be formed on the sidewall of the shallow isolation trench to protect the material on the sidewall of the shallow isolation trench from being etched away, so that the performance of the semiconductor device is better. Furthermore, a single diffusion interruption material is filled in the shallow isolation trench on the side of the NMOS transistor and the PMOS transistor away from the substrate, and the single diffusion interruption material is etched and removed to form a semiconductor device.

[0073] In addition, this embodiment also provides a semiconductor device, in which a first dielectric layer is formed on the sidewalls of the shallow isolation trench, so as to protect the material on the sidewalls of the shallow isolation trench from being etched to varying degrees in subsequent etching, thereby improving the performance of the semiconductor device.

[0074] Although the present invention has been illustrated and described with reference to certain preferred embodiments of the present invention, it should be understood by those skilled in the art that the above is a further detailed description of the present invention in conjunction with specific embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. Those skilled in the art may make various changes in form and details, including making several simple deductions or substitutions, without departing from the spirit and scope of the present invention.

Claims

1. A method for forming a semiconductor device, It is characterized in that The following steps are involved: Providing a substrate, on which at least two adjacent transistor regions are formed; A shallow isolation trench is formed at the junction of at least two adjacent transistor regions; forming a first dielectric layer on the sidewalls of the shallow isolation trench; Filling a single diffusion interruption material in the shallow isolation trench on a side of the transistor region away from the substrate, and etching and removing the single diffusion interruption material; When etching and removing the single diffusion interruption material, it includes: Etching the single diffusion interruption material filled on a side of the transistor region away from the substrate; The single diffusion interruption material filled in the shallow isolation trench is removed.

2. The method for forming a semiconductor device according to claim 1, It is characterized in that At least two adjacent transistor regions are formed on the substrate, comprising the following steps: At least two fins are formed on the substrate; depositing a pad oxide layer around the at least two fins; Depositing a cladding layer on a side of the pad oxide layer away from the substrate and around the at least two fins; A second dielectric layer is deposited on a side of the cladding layer away from the substrate.

3. The method for forming a semiconductor device according to claim 2, It is characterized in that A shallow isolation trench is formed at the junction of at least two adjacent transistor regions, comprising: etching the second dielectric layer and the cladding layer at the junction of two adjacent transistor regions to form the shallow isolation trench.

4. The method for forming a semiconductor device according to claim 3, It is characterized in that Before forming the shallow isolation trench, the method further includes: performing chemical mechanical polishing on a side of the second dielectric layer away from the substrate.

5. The method for forming a semiconductor device according to claim 1, It is characterized in that L>2D, wherein L is the width of the shallow isolation trench, and D is the thickness of the first dielectric layer.

6. The method for forming a semiconductor device according to claim 3, It is characterized in that The thickness of the second dielectric layer is greater than or equal to the width of the first dielectric layer.

7. The method for forming a semiconductor device according to claim 2, It is characterized in that After etching and removing the single diffusion interruption material, the method further includes: Performing dielectric deposition processing on the sidewalls of the shallow isolation trench; and / or An oxide film layer is deposited in the shallow isolation trench on a side of the transistor region away from the substrate.

8. The method for forming a semiconductor device according to claim 7, It is characterized in that The material of the substrate is silicon carbide or silicon germanium; The material of the pad oxide layer is silicon oxide or silicon oxynitride; The material of the first dielectric layer and the second dielectric layer is at least one of titanium nitride, hafnium oxide, hafnium oxynitride, hafnium silicon oxide, and silicon nitride; The material of the oxide film layer is at least one of silicon oxide, silicon oxynitride and titanium oxide; The material of the coating layer is silicon or silicon dioxide.

9. A semiconductor device, It is characterized in that The semiconductor device is manufactured based on the method for forming a semiconductor device according to any one of claims 1 to 8.

Citation Information

Patent Citations

  • Shallow trench isolation structure and forming method thereof

    CN101577242A

  • Shallow trench isolation structure and manufacturing method thereof

    CN107871706A

  • Method of forming finned semiconductor devices with trench isolation

    US20100015778A1

  • Hybrid STI Gap-Filling Approach

    US20100230757A1

  • Fin-type field effect transistors with single-diffusion breaks and method

    US9935104B1