Electrically functional polymer microneedle arrays

By forming microneedles and through holes on the polymer substrate of the biosensor device and coating the electrodes with a conductive material layer, the problems of difficulty in application and complex manufacturing of biosensor devices in the prior art are solved, and efficient sample detection and adaptation are achieved Mass-produced biosensor device.

CN112041982BActive Publication Date: 2024-12-03INTERNATIONAL BUSINESS MACHINE CORPORATION
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980028644.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-05-16
Filing Date
2019-04-09
Publication Date
2024-12-03
Estimated Expiration
2039-04-09

AI Technical Summary

Technical Problem

Existing biosensor devices are difficult to apply in end users and are not designed to be suitable for mass manufacturing, especially due to insufficient production of sweat samples, the manufacturing process is complex and difficult to scale.

Method used

Biosensor device for fabricating microneedles and through-holes using structured polymer substrates. By forming microneedle arrays and through-holes on the substrate, coating electrodes with a layer of conductive material, simplifying the manufacturing process and improving mechanical stability, suitable for in vivo detection and other applications.

Benefits of technology

A biosensor device is realized that is easy to manufacture and application, which can effectively detect interstitial fluid and other samples, is suitable for long-term wear and mass production, simplifies the process flow and improves the mechanical stability of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112041982B_ABST
    Figure CN112041982B_ABST
Patent Text Reader

Abstract

A sensor device, such as a biosensor, may include a polymer substrate that is structured to form multiple groups of microneedles and corresponding through holes. The microneedles each extend from a base surface of the substrate. Each through hole extends through the thickness of the substrate to form a corresponding group of holes on the base surface, wherein each hole is adjacent to a corresponding microneedle. The device also includes two electrodes, including a sensing electrode and a reference electrode, each electrode including a layer of conductive material, the conductive material layer coating an area of ​​the substrate, thereby coating at least some of the microneedles and adjacent portions of the base surface. Related devices, equipment, and methods of making and using such devices can be provided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure generally relates to the field of sensor devices (particularly biosensors) having microneedles and electrodes for detecting fluids (particularly physiological fluids). The present invention further relates to related methods of manufacture and operation. Background Art

[0002] A sensor is a device or module for detecting an event or change in a property (e.g., chemical, physical) of the sensor or in the sensor's environment. The sensed signal is usually processed by an electronic device that it comprises or to which it is connected, for example remotely. As an important class of sensors, biosensors make it possible to obtain data about a person's physiological state and, as such, enable a range of health and medical applications.

[0003] Being able to selectively detect biomarkers would make it possible to more efficiently reach useful information without resorting to large amounts of data manipulation. Current technology used in biosensors is trending towards sweat sensing. Sweat is indeed an interesting medium for probing. However, an inherent disadvantage of sweat is that it requires a lot of physical activity to generate sufficient sample volume unless relying on sweat-inducing drugs, which are generally not appropriate.

[0004] Microneedle electrode arrays are known that overcome this limitation by detecting interstitial fluids. However, currently known devices are painful, difficult to apply, and / or inconvenient to wear for extended periods of time for end users. In addition, the design of such devices may not be suitable for mass production.

[0005] The paper "Development of Low-Cost Rapid Fabrication of Sharp Polymer Microneedles for In Vivo Glucose Biosensing Applications" (C. Barrett, K. Dawson, C. O'Mahony and A. O'Riordan, ECS Journal of Solid State Science and Technology, 4(10) S3053-S3058 (2015)) describes the fabrication of a minimally invasive transcutaneous sensor for direct in vivo detection of glucose in interstitial fluid based on a dual molding technique using PDMS polymer. However, the fabrication method described in this paper is considered by the inventors to be not easily scalable. In addition, the process for pre-patterning the electrode material is quite complex to implement in production. Summary of the invention

[0006] According to a first aspect, the present invention is implemented as a sensor device, such as a biosensor. The device includes a polymer substrate, which is structured to form a microneedle group and corresponding through holes. The microneedles each extend from the base surface of the substrate. Each of the through holes extends through the thickness of the substrate, thereby forming a corresponding group of holes on the base surface. Each hole is adjacent to (i.e., next to) a corresponding microneedle. The device further includes two or more electrodes, which include a sensing electrode and a reference electrode. Each electrode includes a conductive material layer, which coats the area of ​​the substrate, thereby coating at least some of the microneedles and the adjacent parts of the base surface.

[0007] Providing through holes and corresponding holes adjacent to the needles maintains the mechanical stability of the structured polymer substrate and simplifies the manufacturing process, especially when compared to solutions that rely on hollow needles, for example. This design further facilitates the release of the substrate during the stripping process step, as described in the preferred manufacturing method described herein. In addition, the present method makes it possible to coat any area of ​​the polymer substrate, including the inner conduits of the through holes. In summary, the above design makes it easy to manufacture sensor devices with assembly characteristics, such as biosensors. Such devices can be used, for example, for in vivo detection of interstitial fluid, or for food or drug testing, among other examples.

[0008] In the preferred embodiments described herein, each microneedle has one (preferably only one) facet that is substantially perpendicular to the base surface of the substrate, which in practice results in a sharper needle. For example, the holes of the through-holes may each be adjacent to and located at the base of a vertical facet of a corresponding one of the microneedles. The standard deviation of the angles between such vertical facets and the base surface of the substrate is, for example, less than 4°.

[0009] Preferably, the average height of the microneedles is less than or equal to 400 μm. This height is measured perpendicular to and from the base of the substrate. On the other hand, in order to be able to properly detect the sample, it is usually necessary to make the average height greater than or equal to 30 μm, or even 100 μm.

[0010] In an embodiment, the microneedles form an array of microneedles, whereby the microneedles are distributed on the base surface of the polymer substrate according to a 2D lattice. In practice, the average first adjacent distance between the vertices of the microneedles in the array should preferably be less than or equal to 3 mm. Each first adjacent distance is measured parallel to the base surface of the polymer substrate. Although advantageously, a condition can be imposed between the first adjacent distance and the needle height. That is, the average first adjacent distance is preferably greater than or equal to 3 times the average height of the microneedles, wherein the average height is between 30 μm and 400 μm.

[0011] Preferably, each layer of conductive material of the electrode coats a corresponding, non-overlapping portion of the base surface of the substrate, eg, around the apertures, and also coats the microneedle facets.

[0012] In an embodiment, the sensor device further comprises one or more additional electrodes. Each additional electrode comprises a layer of conductive material which partially coats a corresponding portion of the base surface of the substrate (this includes, for example, the facets of the microneedles arranged on this portion), wherein the corresponding portion does not overlap with any portion of the base surface coated by the material layers of the other electrodes of the device.

[0013] The material layer of the electrode may notably be structured so as to coat complementary portions of the base surface of the polymer substrate, which complementary portions may for example be arranged in different sections of the base surface of the substrate.

[0014] Furthermore, one or each of the electrodes is preferably structured to electrically connect to opposite sides of the substrate (the base surface being located on one of the opposite sides) to facilitate connection to / from the electrodes.

[0015] In an embodiment, the polymer substrate comprises a photosensitive polymer, such as SU-8 polymer, although other negative photoresists may be used, for example.

[0016] The sensor device will typically include a readout electronics unit. However, in a variant, the device may be provided as a set of parts, wherein the readout unit is mechanically attachable and thereby electrically connectable to a sensing part of the device. In other variants, connecting wires may be used. In all cases, the readout electronics unit may include a housing and electronics enclosed in the housing, wherein the electronics and the housing are configured such that the electronics can be placed in electrical communication with the electrodes. In operation of the sensor device, the electronics are otherwise configured to read signals obtained from the electrodes.

[0017] According to another aspect, the present invention is embodied as a method of making a sensor device. The method essentially involves patterning and structuring a polymer substrate to form multiple sets of microneedles and through-holes, and electrodes coating areas of the substrate, as in the sensor device described above.

[0018] Nevertheless, preferably and according to a preferred aspect, the present invention is implemented as a manufacturing method, wherein a conductive material layer is patterned on a sacrificial layer, which coats a mold structured to form a reverse pattern. In fact, the conductive material layer and the sacrificial layer can be advantageously patterned as a stack that completely coats the structured mold. Then, the polymer substrate is complementary patterned on the conductive material layer to form a group of microneedles according to the reverse pattern. In this way, each microneedle extends from the base surface of the substrate. The polymer substrate is otherwise structured to present a group of through holes, each of which extends through the thickness of the polymer substrate, thereby forming a group of corresponding holes on the base surface of the polymer substrate. In addition, each hole is adjacent to a corresponding one of the formed microneedles. Finally, the sacrificial layer is removed to release the polymer substrate with the conductive material layer formed thereon. Finally, a sensor device is obtained, which has electrodes formed by the material layer. Due to the appropriately defined electrode pattern, the conductive material layer coats the area of ​​the substrate, thereby coating at least some of the microneedles and the adjacent parts of the base surface of the substrate.

[0019] In an embodiment, this manufacturing method further includes a series of initial steps (before the conductive material layer is patterned onto the sacrificial material), the goal of which is to obtain the desired inverse pattern and enable an easy stripping process. That is, a silicon oxide substrate is first obtained, wherein the oxide layer is on top of the substrate. Then, the oxide layer is patterned to form an opening through the residual portion of the oxide layer. Next, the silicon substrate is etched through the formed opening to obtain the reverse pattern, thereby producing a cavity that is complementarily shaped with the subsequently obtained microneedle. The residual portion of the oxide layer is then removed to obtain a structured mold. Finally, a sacrificial layer is deposited on the structured mold to allow subsequent patterning of the electrode layer that remains on the substrate after release. However, note that the sacrificial layer is preferably deposited on the mold as a metal stack together with other metal layers.

[0020] Preferably, the patterning of the polymer substrate consists in selectively exposing the polymer to a radiation source, which makes it possible to increase in practice the sharpness of the needles, as observed by the inventors.

[0021] In a preferred embodiment, the above steps of patterning the material layer, complementary patterning of the polymer substrate, and removal of the sacrificial layer are performed on a wafer level. In this case, after release, the wafer-level polymer substrate is separated to obtain several sensor devices, each sensor device comprising a structured polymer substrate with corresponding electrodes and microneedle groups, through holes and holes as described above.

[0022] According to a last aspect, the invention is implemented as a method for analyzing a fluid. Basically, the method relies on a sensor device as described above, which is applied to a body (e.g., a food or medicine, a part of a human body or an animal, etc.). A polymer matrix is ​​applied to the body, for example, so that the microneedles slightly penetrate into the body. This allows the fluid from the body to contact one or more surfaces of the electrodes exposed to the body. The signals obtained from the electrodes are then read, for example, due to a readout electronic unit such as described above.

[0023] Devices, apparatus, methods of manufacture and methods of use of a sensor device as described above embodying the invention will now be described by way of non-limiting examples and with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The accompanying drawings are used to further illustrate various embodiments and explain various principles and advantages according to the present disclosure. In the accompanying drawings, the same reference numerals refer to the same or functionally similar elements throughout the various views, and the accompanying drawings are incorporated into and form a part of this specification together with the following detailed description. In the accompanying drawings:

[0025] Figure 1 is a 2D cross-sectional view of a sensor device showing the device applied to a body to detect interstitial fluid from the body, as in an embodiment of the present invention;

[0026] Figure 2 According to the implementation mode Figure 1 2D cross-sectional view of the sensing portion of a similar sensor device showing microneedles and through-holes formed in a polymer substrate. Figure 3 The cutting plane A-A shown in FIG.

[0027] Figure 3 is corresponding to Figure 2 A top view of a cross section of , showing a sensor device having four electrodes formed on top of the polymer substrate and arranged in quadrants as in an embodiment;

[0028] Figures 4 to 6 Shown according to Figure 3 A top view of a device of a variation of wherein the electrodes formed on top of the polymer substrate have a different arrangement;

[0029] Figure 7 yes Figure 2 an enlarged portion of a 2D cross-sectional view of FIG. 1 , further illustrating the sensor device in operation as in an embodiment;

[0030] Figure 8 is a scanning electron microscope image of a structured polymer surface of an actual sensor device according to an embodiment, which is otherwise similar to Figure 3 The device shown;

[0031] Fig. 9 is a sequence showing high-level manufacturing steps of a sensor device according to an embodiment;

[0032] Fig.10 Yes Fig. 9 an enlarged portion of a 2D cross-sectional view of a mold obtained after step S50 onto which an electrode material has been patterned as a metal layer stack, as in a preferred manufacturing method; and

[0033] Fig.11 and Fig.12 As shown in Fig. 9 2D cross-sectional view of the polymer substrate obtained after steps S80 and S90.

[0034] The accompanying drawings show simplified representations of devices or parts thereof as involved in the embodiments. The technical features depicted in the accompanying drawings are not necessarily to scale. Similar or functionally similar elements in the accompanying drawings have been assigned the same reference numerals unless otherwise specified. DETAILED DESCRIPTION

[0035] Reference Figures 1 to 8 First, an aspect of the present invention regarding a sensor device 1 is described. Device 1 ( Figure 1 ) basically comprises a structured polymer substrate 10 ( Figure 2-3 and 7-8), the structured polymer substrate can accommodate multiple variations 10a-10c ( Figure 4-6 ), electrodes are coated on these variants to sense fluids, as explained below.

[0036] like Figure 2-3 As shown in Figures 7-8, the polymer substrate 10 is structured to form: (i) a group of microneedles 16; and (ii) a group of corresponding vias 17. The microneedles 16 each extend from the base surface S of the substrate 10. The microneedles 16 are not hollow needles; rather, they are comparable to sharp solid rods or tips. The vias 17 each extend through the thickness of the substrate 10. Each via 17 forms a corresponding hole 18 on the base surface S. Each hole 18 is adjacent to a corresponding one of the microneedles 16. That is, each hole 18 is adjacent to the corresponding microneedle and preferably in close proximity to the corresponding microneedle: the holes are arranged far enough away from the needle position so that the microneedles 16 are not hollow needles.

[0037] The device 1 further comprises two or more electrodes 11-15a. The electrodes comprise at least a sensing electrode and a reference electrode. Each electrode 11-15a comprises a layer of conductive material coating an area of ​​the substrate 10. In fact, each electrode 11-15a coats at least some of the microneedles 16 and adjacent portions of the base surface S, such as Figure 2 and3 In a variation, three or more electrodes 11 - 15 a may be similarly formed on the substrate 10 .

[0038] like Figures 2 to 7 As further shown in FIG. 1 , the conductive material layer of the electrode should preferably coat the area of ​​the substrate 10 around the hole 18 so as not to obstruct the through hole 17. That is, there is a hole in the electrode layer that coincides with the hole 18. In this case, the free hole 18 and the through hole 17 form an access port, which can be used, for example, in particular for optical access (insertion depth), or for the introduction of antibacterial and / or inflammatory gels, or still for perspiration (e.g. Figure 7 assuming in ).

[0039] However, in a variant, it may be desirable to keep a freestanding membrane above the hole 18, for example, to prevent liquid from draining from the insertion area or to selectively filter certain liquid components. In such a variant, the polymer film can be applied as a layer of the stack 70, for example, by spin coating or electrodeposition, so as to maintain the polymer film suspended above the hole 18 in the final device structure. For example, by electrodepositing a suitable polymer (polypyrrole, polyaniline, etc.) of sufficient thickness (e.g., greater than 5 μm), the polymer film can be further made impermeable to moisture. On the contrary, a polymer film permeable to selected molecules such as caffeine can be obtained by electrodeposition of a matrix such as molecular imprinted polypyrrole. Such selective membranes can prove useful in practice, for example, when it is desired to drain certain analytes from the insertion area, or conversely, when certain compounds are introduced into the insertion area by the polymer film at a defined rate and purity.

[0040] Providing through holes 17 and corresponding holes 18 adjacent to the needles maintains the mechanical stability of the structured polymer substrate 10, especially when compared to solutions that rely on hollow needles, for example. This design also facilitates the release of the substrate 10 during the peeling process step, as involved in the preferred manufacturing method described below. In summary, the present method makes it possible to easily manufacture sensor devices with assembly characteristics.

[0041] More specifically refer to Figure 2 , 7: In an embodiment, each microneedle 16 has a facet 16p that is substantially perpendicular to the base plane S of the substrate 10. Each microneedle 16 preferably has only one such perpendicular facet 16p. Imposing perpendicular facets 16p in the manufacture of the needles produces sharper needles in practice. Note that the term "perpendicular facet" as used herein refers to an angle formed by the facet 16p with the base plane S (or equivalently with the average plane of the substrate 10 (which is a substantially planar object)), wherein this angle is between 82° and 98°, and preferably between 87° and 93°. In fact, the manufacturing method disclosed herein does allow obtaining fairly perpendicular facets 16p, i.e., an angle of 90° with the substrate 10 with a standard dispersion that is typically less than 4°. That is, the angle formed by the perpendicular facets 16p is substantially equal to 90±2°.

[0042] In an embodiment, Figures 2 to 8 As shown, the holes 18 of the through holes 17 are each adjacent to and located at the base of the vertical facet 16p of the corresponding microneedle in the microneedle 16. This enables easy drainage of sweat or other fluids, or the introduction of gels or fluids near the needles, without compromising the integrity of the polymer of the needle structure. The hole should generally have a rectangular shape, or at least present one side whose length is substantially equal to the width of the vertical facet. In addition, other hole shapes, such as semicircular holes, can be easily processed.

[0043] More specifically refer to Figure 7 , the average height of the microneedles 16 is preferably less than or equal to 400 μm. The height of the microneedles is measured perpendicular to and from the base surface S. That is, this height is the distance from the apex of the needle 16 to the base plane surface S of the substrate 10. On the other hand, it is typically necessary to make this average height greater than or equal to 30 μm, or even 100 μm, to facilitate sample collection. In addition, manufacturing constraints and tolerances can usually impose a minimum height on the needle.

[0044] Now refer to Figure 3-6 In a top view of the microneedles 16, the microneedles 16 may generally form an array of microneedles 16. That is, the microneedles 16 are preferably distributed on the base surface S according to a 2D lattice. Typically, a highly symmetrical pattern (e.g., such as a square or hexagonal lattice) is relied upon, but other lattice patterns (e.g., diamond or rectangular) are contemplated. Although the needles are preferably formed in typical applications, the needles do not have to be systematically formed at each lattice position, such as Figure 6 As shown, this incidentally simplifies the design and manufacturing process.

[0045] exist Figure 3-5 In the example of , it is assumed that the average first neighbor distance between the vertices of the microneedles 16 is less than or equal to 3 mm. This upper limit leads to a lower limit on the surface density of the needles, which is sufficient for typical biosensing applications. Each first neighbor distance is measured here parallel to the base surface S. Figures 3 to 5 In the example of , this distance corresponds to a lattice step of the 2D lattice (square). In addition, the first neighbor distance can be forced to be greater than or equal to three times the average height of the microneedles 16, whose average height is preferably greater than or equal to 30μm and less than or equal to 400μm, as described above. Indeed, since the inventors have concluded from different tests they have performed that, given a reasonable average needle height, the imposition of such a condition allows a sufficiently sparse array of needles 10, 10a–10c, which is most suitable for biosensing applications, for example, for detecting interstitial fluids. That is, the resulting design happens to be painless enough for users who wear the sensor for a long time, while still allowing sufficient amounts of fluid to be detected in practice. As a result, the average (first neighbor) distance between the vertices of these needles will typically be greater than 90μm (although it can reach the mm range). It is preferably greater than or equal to 360μm, assuming 120μm high needles.

[0046] In terms of overall dimensions, the thickness of the polymer substrate 10, 10a-10c (i.e., excluding the needles) will typically be between 50 μm and 500 μm. The edge length of the polymer substrate may be, for example, between 1 mm and 20 mm. The overall shape of the substrate 10 may notably be rectangular, circular, or have any shape adapted to the sensing application under consideration (e.g., advantageously conforming to the epithelial surface on which it is intended to be placed).

[0047] In terms of materials, the polymer material used for the structured substrate 10, 10a-10c preferably comprises a photosensitive polymer, for example an epoxy-based photosensitive polymer, such as SU-8 polymer. In a variant, other negative photoresists can be considered, such as the so-called or Polymer. However, many other polymer materials are contemplated. In addition, each electrode 11-15a is typically composed of a metal layer 71-75 (or more likely a stack 70 of metal layers, see Fig.10 ) with a thickness typically between 5 nm and 500 nm (per layer). In a preferred embodiment, such a stack 70 comprises gold 72, 74 (100 nm) and titanium 71, 75 (10 nm), wherein the gold layer 75 forms the exposed surface and the titanium layer (one or more layers) is used to promote adhesion between the gold and the polymer material used for the structured substrate 10, 10a-10c. In addition to gold, other metals of interest for sensing applications include platinum and silver. The metals can be further processed, for example by electrochemical or thermal oxidation or chemical chlorination, to obtain the sensing material of interest. Other materials known per se such as ceramics (e.g. TiN, RuO2, IrO x ) or polymers (e.g., membranes for ion selective electrodes or ISEs) can also be deposited onto the microneedles 16 as part of the manufacturing process or after the polymer is released, as described below with reference to preferred manufacturing methods.

[0048] like Figure 3-6 As shown, each layer of conductive material of electrodes 11-15a may be deposited so as to coat corresponding non-overlapping portions of the base surface S of structured substrate 10, 10a-10c, for example around apertures 18, and so as to also coat the facets of microneedles 16 (including vertical facets 16p).

[0049] In addition to the sensing electrode and the reference electrode, the sensor device 1 may also include one or more additional electrodes. Figures 3 to 6 In the embodiment shown in , the sensor device 1 further comprises two or three additional electrodes 13, 14, 15a. Similar to the electrodes 11, 12, such additional electrodes each comprise one or more layers of conductive material, which comprise a layer partially coating a respective portion of the base surface S of the substrate. The respective portion does not overlap with any portion of the base surface S that is otherwise coated by the material layers of the other electrodes 11, 12, etc. of the device. That is, all electrodes are arranged on different portions of the base surface S so as not to be in direct electrical contact.

[0050] For example, a layer of material for an electrode may be structured to coat a complementary portion of the base surface S. Such a complementary portion may be more or less compact, e.g. Figures 3 to 5 or, on the contrary, to form a mixed or cross pattern, such as Figure 6 In all cases, the conductive coatings may be laterally separated from one another on the base surface S so as not to be in direct electrical contact with one another. In a variant, an electrical barrier may be explicitly deposited on the surface S to prevent direct electrical contact. In other variants, the trenches may be opened laterally after the deposition of the electrode material layer, for example so that the electrode pattern can be customized according to a specific application.

[0051] For example, Figure 3 The electrodes 11 - 15a are shown arranged in quadrants. Figure 4 A cross shape is shown, where the electrode pattern is symmetrical about a central cross electrode that can be used, for example, as a reference electrode. Figure 5 Concentric electrode shapes with radial symmetry (in-plane) are described, which can be advantageously used in applications where radially symmetric pressure on the microneedles 16 is required. Figure 6 The interdigitated pattern of allows large-area (in-plane) interaction between electrodes, which is suitable for impedance / conductance measurements, for example. More generally, given the available area, the pattern can be adapted to match the impedance / conductance measurement needs.

[0052] Note that with Figure 3-6 In contrast to the depiction of FIG. 1 , the orientation of the holes 18 and the vertical facets 16p may vary from one needle to another or from one part of the surface to another. That is, the needles and holes 18 need not be systematically oriented in the same manner.

[0053] exist Figure 3 In the example of , the complementary parts on which the electrodes are patterned are arranged in different sectors of the base surface S of the structured substrate. That is, the periphery of such complementary parts forms quadrants. More generally, the outer limits of the sectors can form any 2D convex shape.

[0054] As in Figure 2 , Figure 7 and Fig.11 , Fig.12 As further seen in the drawings, in embodiments, the electrodes 11-15a may be further structured so as to electrically connect opposite sides of the substrate 10. That is, the electrode material is arranged to connect the base surface S on one side to the opposite side of the substrate. For example, for ergonomic reasons, the conductive material layer 71-75 used to form the electrodes may be applied to the structured polymer substrate uninterruptedly on the adjacent sides of the structured polymer substrate so as to electrically connect the top surface of the substrate to the bottom surface. That is, as Figure 1 and 7 As shown, the structured side of the substrate 10 can be applied to the body to collect and analyze trace amounts of fluid produced by the body, while the readout electronic device 3 (see Figure 1 ) may be provided on the side opposite to the side where the read signal is obtained from the electrodes 11 - 15 a , in operation of the sensor device 1 .

[0055] For details, see Figure 1 , the sensor device 1 may further comprise a readout electronics unit 3, 5, wherein the readout electronics unit comprises a housing 5 and an electronics 3 enclosed in the housing 5. The electronics 3 and the housing 5 are configured such that the electronics 3 can be arranged to be in electrical communication with the electrodes 11-15a, so that the units 3, 5 read signals obtained from the electrodes 11-15a during operation of the device 1. The electronics units 3, 5 may also be designed as peripheral devices, which may, for example, be removably connected to the sensing portion 10 of the device 1. For example, the housing 5 and / or the structured substrate 10 may accommodate a snap-fit ​​mechanism to connect the electronics 3 to the electrodes 11-15a on the structured substrate 10. Thus, the device 1 of the present invention may be provided as a set of components.

[0056] More precisely refer to Figure 7, we now discuss another aspect of the present invention, which relates to a method for analyzing a fluid using the sensor device 1 as described above. Basically, the sensing portion of the device 1 (i.e., the structured polymer substrate 10) is first applied to the body 200 (e.g., to human or animal skin, food, or a drug such as a gelling agent) at S200. Depending on the application, the microneedles 16 may or may not need to penetrate slightly into the body. Applying the substrate 10 to the body allows the fluid produced by the body to contact the exposed surfaces of the electrodes 11-15a. Next, at S300, the signals obtained from the electrodes 11 to 15a are read, for example by the electronic units 3, 5 and in order to collect data about the body or its state, such as Figure 7 As suggested in .

[0057] To further demonstrate the readout principle, now refer to Figure 1 A preferred embodiment is described in which a cross section of a body part 200 representing human skin is depicted. It notably shows the dermis 203, i.e., the skin layer between the epidermis 202 (below the stratum corneum 201) and the subcutaneous tissue (including the epidermis 204). Here, it is assumed that the sensing device 1 includes a sensing electrode, the exposed surface of which is composed of TiN, and a reference electrode, the exposed surface of which is AgCl. When inserted into a medium 200 containing H3O+ ions, such as is the case in the interstitial fluid present in the dermis region 203, a potential difference between the sensing electrode and the reference electrode can be sensed, which potential difference is related to the H3O+ in the medium by the Nernst equation. + In this example, the readout unit 3, 5 electrically connected to the electrodes may comprise a high impedance voltmeter and a data acquisition and logic unit which in combination provide a means for recording a voltage signal varying with time.

[0058] If necessary, further signal processing electronics may be included (or remotely connected to the readout unit 3, 5) for filtering, amplifying and transforming the measured signals. A communication protocol such as the so-called I2C or UART protocol may be implemented for data communication within the readout unit 3, 5 and in a bus connecting the readout unit 3, 5 to a further computing system. If necessary, the readout unit 3, 5 may further comprise a wireless communication unit for transmitting data to the computing system, e.g. due to any suitable wireless communication standard.

[0059] In an embodiment, the sensing electrode and the reference electrode may have exposed surfaces made of the same material (e.g., gold), in which case the potential difference between them is expected to be zero. Nevertheless, a current may be applied to these electrodes by means of an external circuit (e.g., forming part of the electronic device 3) such that the amplitude of the current will vary sinusoidally over time so as to produce a sinusoidally varying voltage on the two electrodes. There, the relationship between the transient voltage and the current pattern can be used to obtain an impedance sensor sensitive to the medium surrounding the two electrodes. For impedance sensing, the readout unit 3, 5 will typically include a signal generator and an impedance bridge. As an alternative to the impedance bridge, a lock-in amplifier or a frequency response analyzer may be implemented in the readout unit 3, 5 in order to perform impedance measurements. As in the variants induced above, the readout unit 3, 5 may further include additional units for the intended operation, such as a data acquisition unit, a logic unit, a signal processing unit, and a communication unit.

[0060] The biosensing applications considered here are not limited to in vivo sensing. As mentioned before, the present device can also be used to sense the properties of food or even pharmaceutical products or any material still used for in vitro processing.

[0061] According to another aspect, the present invention can be further implemented as a method for manufacturing the sensor device 1. Basically, this manufacturing method revolves around patterning and structuring S10-S90 ( Fig. 9 ) polymer substrate 10 to form a set of microneedles 16 and a corresponding set of vias 17, and electrodes 11-15a, as previously described with reference to Figure 1-8 As described.

[0062] Reference Fig. 9 A particularly interesting aspect of the present invention relates to a manufacturing method that relies on reverse patterning. In this method, a conductive material layer 11-15a is patterned onto a sacrificial layer 73 in S50, which is applied to a mold 55 structured in S10-S40 to form the desired reverse pattern.

[0063] Next, at S60-S70, the polymer substrate 90 is patterned complementarily to the conductive material layer to form the microneedle group 16, ie, according to the reverse pattern obtained previously. The microneedles 16 thus formed extend from the base surface S of the substrate 90 exposed to the mold.

[0064] At S70, the polymer substrate is otherwise structured to form a substrate 100 having a set of through holes 17, wherein each through hole 17 extends through the thickness of the substrate 100, thereby forming a corresponding set of holes 18 on the base surface S of the substrate 100. This is done so that each hole 18 is adjacent to a corresponding one of the microneedles 16.

[0065] Finally, at S80, the sacrificial layer 73 is removed, which allows the substrate 100 to be released at S90. In this way, a structured substrate 10, 10a-10c can be easily obtained, as previously described with reference to Figure 1 –8 described.

[0066] As previously mentioned, at S50, the electrode material is preferably patterned into a layer stack 70. The order of the layers 71-75 involved in the stack 70 patterned at step S50 ensures that the conductive material layer 11-15a remains on the substrate when the substrate is released by removing the sacrificial layer 73 at S80. In this way, a device 1 is obtained, which exhibits an electrode 11-15a formed by said material layer 11-15a, wherein such a layer coats a specific area of ​​the structured substrate 10 as previously explained with reference to the present device 1.

[0067] Preferably, at S70, vias 17 are formed by a photolithography patterning process. For example, at S60, polymer 100 may be first spin-coated onto mold 55 and then baked (not shown), and then at S70, vias 17 may be patterned due to this photolithography process.

[0068] Fig.11 and Fig.12 Shown respectively in Fig. 9 2D cross-sectional view of the polymer substrate obtained after steps S80 and S90. That is, after the patterning process S60-S70, the polymer substrate 90 is coated with an electrode ( Fig.11 Then, if desired, another backside coating ( Fig.12 ) also allows the substrate to be coated on opposite sides. In this way, the electrode 11 can be patterned so as to electrically connect the opposite sides of the substrate 10, such as Fig.12 shown.

[0069] Note that the mold 55 obtained at step S40 and then released at step S80 can advantageously be reused for a new cycle of steps S50 - S90. After release, a residual layer of material (eg, Ti / Au) will likely remain on the mold 80 for reasons explained below.

[0070] In an embodiment, the manufacturing method may further involve a series of initial steps (before patterning the conductive material layer 70 at S50) aimed at obtaining a mold 55, 80 structured according to the desired reverse pattern. That is, at S10, a silicon oxide substrate 51, 52 having an oxide layer 52 formed on top of the substrate 51, 52 may first be obtained. Then, at S20, the oxide layer 52 may be patterned to form an opening (through a residual portion 52p of the oxide layer). Next, at S30, the silicon substrate 51 is etched through the formed opening to obtain the reverse pattern, thereby producing a cavity 60, which is shaped complementarily to the subsequently obtained microneedle 16. Finally, at S40, the residual portion 52p of the oxide layer 52 is removed to obtain a structured mold 55, on which a sacrificial layer 73 is deposited (e.g., as part of a metal stack 70).

[0071] As described above, pre-patterning the electrode material on the mould allows for improved control over the final electrode positions; this further simplifies the manufacture of the device 1, as the structured mould can subsequently be reused.

[0072] For example, at S10, a 2μm SiO2 thermal substrate 10 can be first obtained by growing a silicon oxide layer SiO2 on a silicon (Si) surface by a dry or wet oxidation process. Then, at step S20, the top oxide layer 52 is patterned by relying on inductively coupled plasma (ICP) etching and a hard mask 52p including an opening is thereby formed. Next, at step S30, KOH etching through the opening allows a cavity 60 to be defined within the bulk Si substrate 10, which draws a reverse pattern for the needle. The structured Si substrate 55 will then be used as a mold 55 for a structured polymer substrate 10. Finally, at S40, after the remaining portion 52p of the hard mask has been removed, at S50, a sacrificial layer 73 (e.g., which includes chromium as part of a metal layer stack 70) is deposited, and at S50, an electrode material is patterned at selected locations on the sacrificial layer 73 using a shadow mask.

[0073] In a preferred embodiment, the deposited metal stack comprises chromium 73 (50 nm), gold 74 (100 nm) and titanium 75 (10 nm) deposited in this order onto the silicon mold 55, thereby obtaining a pre-patterned mold 80. The Cr / Au / Ti layer sequence can, for example, be deposited successively on the residual Ti / Au bilayer of the mold 85, as obtained from the previous cycle S10-S90 (i.e., when the mold 85 is reused). After the deposition (S60) and patterning (S70) of the polymer substrate 90, at S80, the etching of the chromium 73 makes it possible to easily release the polymer structure 100 at S90 together with the gold and titanium metallization layers 74, 75, wherein the gold layer forms an exposed surface. The titanium layer is used to promote adhesion between the gold 74 and the polymer 100. Instead of gold, other metals may include molybdenum or silver, as described above. The metals may be further processed, for example by electrochemical or thermal oxidation or chemical chlorination, to obtain other sensing materials of interest. As evoked earlier, additional materials such as ceramics or polymers may be used further in the manufacturing process S10 - S90 or after the polymer is released at S90 .

[0074] In S50, when the mold 55, 80 is processed for the first time, the metal stack Ti / Au / Cr / Au / Ti (in Fig.10 71-75 in the figure) are successively deposited on the structured mold 55. At S80, the subsequent etching of the chromium 73 makes it possible to release the polymer structure 100 together with the Au / Ti layers 74, 75 thereon at S90, while the residual Ti / Au bilayers 71, 72 remain on the mold 85, which can be reused for the next cycle, as described above.

[0075] In a preferred embodiment, step S70 may further include selectively exposing the polymer material to a suitable radiation source to allow the needle sharpness to increase, as observed by the inventors. For example, a photosensitive polymer (e.g., SU-8) may be first spin-coated on the structured mold 80. Thereafter, the spin-coated polymer structure 100 is placed in a vacuum oven at a slightly elevated temperature (e.g., 50° C.) for a sufficient time (e.g., 1-2 hours) to remove the air trapped in the mold. The coated mold thus obtained is then removed from the vacuum oven and heated to 95° C. for at least 10 hours to complete the so-called soft baking step, which removes some solvents and increases the viscosity of the polymer. The polymer coating is then exposed to an ultraviolet (UV) light source through a mask that defines the pattern of the polymer portion to be removed, according to the recommended exposure dose for the specific polymer. After exposure, the hard baking step of the polymer is completed, for example, by heating the coated mold to 95° C. with a residence time of 15 minutes at this temperature. After all exposure and heat treatment steps, the coated mold is finally placed in a developer liquid (e.g., SU-8 propylene glycol methyl ether acetate, or PGMEA, for SU-8) to remove the undesirable polymer parts in the final device structure. As will be appreciated by those skilled in the art, the temperature and duration described in the above examples can be adjusted according to the characteristics of the specific polymer used (e.g., chemical composition, thickness, etc.). Once all undesirable parts of the polymer have been removed, in step S80, the coated mold is immersed in a Cr etchant liquid and sufficient time is allowed for Cr etching to release the polymer substrate 100. Prior to S80, it may be beneficial to increase the hydrophilicity of the polymer coating by applying a short plasma ashing step to the coated mold (not shown).

[0076] In a particularly advantageous embodiment, steps S10-S90 can be performed 24 on the wafer level. That is, assuming that a suitably structured wafer-level mold 55 is available, the steps of patterning (S50) the material layer 11-15a, complementarily patterning (S60-S70) the polymer substrate and removing (S80) the sacrificial layer 73 can be implemented on the wafer level. Then, after the sacrificial layer 73 has been removed (S80) to release (S90) the wafer-level polymer layer, the latter can be separated to obtain several sensing components. That is, each component finally obtained comprises a structured polymer substrate portion 10 with corresponding electrodes 11-15a and a plurality of groups of microneedles 16, through holes 17 and holes 18.

[0077] For example, after release (S90), the polymer 100 may be separated into components by cutting it. As an alternative to cutting the polymer substrate 10, the edges of individual devices (e.g., like the through-holes 17) may be predefined during patterning of the polymer substrate 10 at the wafer level. Thus, upon removal of the sacrificial layer and the predefined sacrificial edges, the individual device components 10 may be subsequently released without further separation. As another variant, the pre-cut lines may be patterned to facilitate subsequent splitting, for example, by breaking the device parts by hand.

[0078] Although the present invention has been described with reference to a limited number of embodiments, variants and drawings, it will be understood by those skilled in the art that various changes may be made and equivalents may be substituted without departing from the scope of the present invention. Specifically, without departing from the scope of the present invention, the features (similar devices or similar methods) listed in a given embodiment, variant or shown in the drawings may be combined with or replace another feature in another embodiment, variant or drawing. Different combinations of features described with respect to any of the above embodiments or variations are accordingly contemplated, which are still within the scope of the appended claims. In addition, many minor modifications may be made to adapt specific situations or materials to the teachings of the present invention without departing from its scope. Therefore, the present invention is not intended to be limited to the specific embodiments disclosed, but the present invention will include all embodiments falling within the scope of the appended claims. In addition, many other variations other than those explicitly touched upon above may be envisioned. For example, other materials other than those explicitly cited may be envisioned.

Claims

1. A sensor device, comprising: A polymer substrate structured to form: a set of microneedles each extending from a base surface of the polymer substrate; as well as a plurality of through holes each extending through the thickness of the polymer substrate to form a corresponding plurality of holes on the base surface, wherein each of the holes is adjacent to a corresponding one of the microneedles; as well as at least two electrodes, including a sensing electrode and a reference electrode, each electrode including a layer of conductive material coating areas of the polymer substrate that are not in direct electrical contact with each other, thereby coating at least some of the microneedles and adjacent portions of the base surface to form an electrode pattern, The reference electrode includes a conductive material layer coated on a plurality of microneedles in a cross-shaped pattern to form a central cross-shaped electrode, so that the electrode pattern on the polymer substrate is symmetrical with respect to the central cross-shaped electrode.

2. The sensor device according to claim 1, wherein: The layer of conductive material coats a portion of the polymer substrate around the hole so as not to block the through hole.

3. The sensor device according to claim 1, wherein: Each microneedle has a facet that is substantially perpendicular to the base surface of the substrate.

4. The sensor device according to claim 3, wherein: The holes of the through-holes are each adjacent to and based on the vertical facet of a corresponding one of the microneedles.

5. The sensor device according to claim 4, wherein: The microneedles each have only one facet, which is substantially perpendicular to the base surface.

6. The sensor device according to claim 5, wherein: The standard deviation of the angles between the vertical facets and the base of the microneedles was less than 4°.

7. The sensor device according to claim 1, wherein: The microneedles have an average height less than or equal to 400 microns, measured perpendicular to and from the base surface.

8. The sensor device according to claim 7, wherein: The average height is greater than or equal to 30 microns.

9. The sensor device according to claim 8, wherein: The average height is greater than or equal to 100 microns.

10. The sensor device according to claim 1, wherein: The microneedles form an array of microneedles, whereby the microneedles are distributed on the base surface according to a 2D lattice.

11. The sensor device according to claim 10, wherein: An average first-neighbor distance between vertices of the microneedles in the array is less than or equal to 3 mm, each first-neighbor distance being measured parallel to the base surface.

12. The sensor device according to claim 11, wherein: The average first adjacent distance is greater than or equal to three times an average height of the microneedles, wherein the average height is greater than or equal to 30 microns and less than or equal to 400 microns.

13. The sensor device according to claim 1, wherein: Each of the layers of conductive material of the electrodes coats a respective non-overlapping portion of the base surface of the polymer substrate.

14. The sensor device according to claim 13, wherein: The sensor device further comprises one or more additional electrodes, each additional electrode comprising a layer of conductive material partially coating a respective portion of the base surface of the polymer substrate, wherein the respective portion does not overlap with any portion of the base surface coated by the material layers of other electrodes of the sensor device.

15. The sensor device according to claim 13, wherein: The two material layers are further structured so as to coat complementary portions of the base surface.

16. The sensor device according to claim 15, wherein: The complementary portions are arranged in different sections of the base surface of the polymer substrate.

17. The sensor device according to claim 13, wherein: The or each electrode is further structured so as to electrically connect opposite sides of the polymer substrate, the base surface being located on one of the opposite sides.

18. The sensor device according to claim 1, wherein: The polymer substrate includes a photosensitive polymer.

19. The sensor device according to claim 1, wherein: The polymer substrate includes an epoxy-based photopolymer.

20. The sensor device according to claim 1, wherein: The sensor device further comprises a readout electronics unit, the readout electronics unit comprising: a housing; and an electronic device enclosed in the housing, in The electronics and the housing are configured such that the electronics may be placed in electrical communication with the electrodes, the electronics otherwise being configured to read signals obtained from the electrodes during operation of the sensor device.

21. A method of manufacturing a sensor device, the method comprising: Patterning and structuring polymer substrates to form: a set of microneedles each extending from a base surface of the polymer substrate; as well as a plurality of through holes each extending through the thickness of the polymer substrate to form a corresponding plurality of holes on the base surface, wherein each of the holes is adjacent to a corresponding one of the microneedles; as well as at least two electrodes, including a sensing electrode and a reference electrode, each electrode including a layer of conductive material coating areas of the polymer substrate that are not in direct electrical contact with each other, thereby coating at least some of the microneedles and adjacent portions of the base surface to form an electrode pattern, The reference electrode includes a conductive material layer coated on a plurality of microneedles in a cross-shaped pattern to form a central cross-shaped electrode, so that the electrode pattern on the substrate is symmetrical with respect to the central cross-shaped electrode.

22. A method of manufacturing a sensor device, the method comprising: patterning a layer of conductive material onto a sacrificial layer coated with a mold, the mold being structured to form a reverse pattern; complementarily patterning a polymer substrate on the conductive material layer to form a set of microneedles according to the reverse pattern, wherein each of the microneedles extends from a base surface of the polymer substrate, wherein the polymer substrate is structured to exhibit a set of through holes, each through hole extending through the thickness of the polymer substrate, thereby forming a set of corresponding holes on the base surface, each of the holes being adjacent to a respective one of the formed microneedles, the structured polymer substrate also exhibiting at least two electrodes, including a sensing electrode and a reference electrode, each electrode comprising a conductive material layer coating areas of the polymer substrate that are not in direct electrical contact with each other, thereby coating at least some of the set of microneedles and adjacent portions of the base surface to form an electrode pattern, and wherein the reference electrode comprises a conductive material layer coated on a plurality of microneedles in a cross-shaped pattern to form a central cross-shaped electrode, such that the electrode pattern on the polymer substrate is symmetrical with respect to the central cross-shaped electrode; as well as The sacrificial layer is removed to release the polymer substrate having the conductive material layer formed thereon to obtain a sensor device having electrodes formed by the material layer, wherein the material layer coats areas of the polymer substrate, thereby coating at least some of the microneedles and adjacent portions of the base surface of the polymer substrate.

23. The manufacturing method according to claim 22, wherein before patterning the conductive material layer, the method further comprises: obtaining a silicon oxide substrate having an oxide layer on top of the silicon oxide substrate; patterning the oxide layer to form an opening through a remaining portion of the oxide layer; etching the silicon substrate through the formed openings to obtain the reverse pattern, thereby generating cavities that are shaped complementarily to the subsequently obtained microneedles; removing said remaining portion of said oxide layer to obtain a structured mold; as well as The sacrificial layer is deposited on the structured mold.

24. The manufacturing method according to claim 22, wherein: Complementarily patterning the polymer substrate further comprises selectively exposing the polymer to a radiation source.

25. The manufacturing method according to claim 22, wherein: The steps of patterning the material layer, complementarily patterning the polymer substrate and removing the sacrificial layer are performed at the wafer level, And wherein the method further comprises: after removing the sacrificial layer: The polymer substrate is separated to obtain several sensor devices, each sensor device comprising a structured polymer substrate with corresponding electrodes and microneedle groups, through-holes and wells.

26. A method of analyzing a fluid, the method comprising: A sensor device is provided, the sensor device comprising: A polymer substrate structured to form: a set of microneedles each extending from a base surface of the polymer substrate; and a plurality of through holes each extending through the thickness of the polymer substrate to form a corresponding plurality of holes in the base surface, wherein each of the holes is adjacent to a corresponding one of the microneedles; and at least two electrodes, including a sensing electrode and a reference electrode, each electrode including a layer of conductive material coating areas of the polymer substrate that are not in direct electrical contact with each other, thereby coating at least some of the microneedles and adjacent portions of the base surface to form an electrode pattern, wherein the reference electrode comprises a conductive material layer coated on a plurality of microneedles in a cross-shaped pattern to form a central cross-shaped electrode, such that the electrode pattern on the polymer substrate is symmetrical with respect to the central cross-shaped electrode, applying the polymer substrate to the body so that the microneedles penetrate into the body and fluid from the body contacts the exposed surfaces of the electrodes, and The signals obtained from these electrodes are read.