Batteries and battery packs
The battery design addresses the trade-off between output and life performance by using a specific packaging structure to prevent electrode distortion, ensuring high output and long life through minimized gas-induced expansion.
Patent Information
- Application Number
- CN201880094043.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-09-21
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2038-09-21
AI Technical Summary
Lithium-ion secondary batteries face a trade-off between high output performance and long life performance, as reducing the thickness of the active material-containing layer to enhance output leads to electrode distortion and reduced life due to gas expansion, which increases internal resistance and reduces nominal capacity.
A battery design with specific dimensions and packaging constraints, including a square outer packaging container with thin side walls and a sealing plate, ensures the electrode group is less prone to distortion, maintaining both high output and long life performance by minimizing gas-induced expansion.
The battery design achieves improved life performance and output performance by preventing electrode twisting and maintaining structural integrity despite gas generation, while allowing for increased energy density and safety.
Smart Images

Figure CN112204791B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a battery and a battery pack. Background Art
[0002] In recent years, electric vehicles such as hybrid electric vehicles and plug-in electric vehicles have been rapidly popularized. As the power source of these electric vehicles, lithium ion secondary batteries are mainly used as non-aqueous electrolyte batteries that can be charged and discharged.
[0003] Lithium-ion secondary batteries can be manufactured, for example, by the following method. First, prepare a positive electrode and a negative electrode. The positive electrode and the negative electrode can be formed by coating a slurry containing a positive electrode active material and a negative electrode active material that can be inserted and released into and out of lithium ions on a current collector, drying the coating, and providing a positive electrode active material layer and a negative electrode active material layer. By winding such a positive electrode and a negative electrode in a manner of sandwiching a separator between them, a flat electrode group is produced. Next, the electrode group is placed in a container made of a metal such as aluminum or an aluminum alloy, and a sealing plate is welded to the opening of the container. Next, a non-aqueous electrolyte is injected into the container from a liquid injection port provided on the sealing plate. Then, a sealing member is welded to the liquid injection port to obtain a battery cell. Next, the battery cell is subjected to initial charging and aging treatment, thereby obtaining a lithium-ion secondary battery.
[0004] The nonaqueous electrolyte battery such as the lithium ion secondary battery obtained in this way is required to have high input and output performance.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: Japanese Patent Application Publication No. 2004-95357
[0008] Patent Document 2: Japanese Patent Application Publication No. 2012-182025 Summary of the invention
[0009] Problem that the invention aims to solve
[0010] An object of the present invention is to provide a battery and a battery pack that can achieve a long life.
[0011] Means for solving problems
[0012] According to an embodiment, a battery can be provided. The battery includes an outer packaging container, an electrode group and a sealing plate. The outer packaging container includes a bottom wall and a side wall. The side wall extends from the bottom wall in the first direction. An opening portion opposite to the bottom wall is provided on the outer packaging container. The electrode group includes a positive electrode, a negative electrode and an insulating layer. The positive electrode and the negative electrode are wound into a flat shape with the insulating layer sandwiched therebetween. The electrode group is housed in the outer packaging container in a manner such that the winding axis direction is orthogonal to the first direction. The sealing plate is mounted on the opening portion of the outer packaging container. The thickness of the positive electrode and the thickness of the negative electrode may be equal to or different from each other. The thickness T of each of these electrodes E The second direction is parallel to the winding axis direction. The third direction is perpendicular to the first direction and the second direction. The thickness T of the electrode is E (mm), the thickness T of the electrode group in the direction parallel to the third direction W (mm), the innermost height H of the electrode group in the direction parallel to the first direction IC (mm) satisfies the following formula (1).
[0013] 0.02≤(T E ×T W ) / H IC ≤0.04 (1)
[0014] According to another embodiment, a battery pack may be provided, wherein the battery pack includes the battery according to the embodiment. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a perspective view schematically showing an example of a battery according to an embodiment.
[0016] Figure 2 yes Figure 1 An exploded perspective view of the battery is shown.
[0017] Figure 3 yes Figure 2 The battery shown is an exploded perspective view of an electrode group.
[0018] Figure 4 yes Figure 3 A stereogram of the electrode assembly shown.
[0019] Figure 5 yes Figure 4 The electrode assembly is shown in a cross-sectional view along line VV.
[0020] Figure 6 yes Figure 3 to Figure 5 The electrode assembly shown is a cross-sectional view of a positive electrode.
[0021] Figure 7 This is a block diagram showing an example of a circuit of a battery pack according to an embodiment. DETAILED DESCRIPTION
[0022] (First embodiment)
[0023] Nonaqueous electrolyte battery requires excellent output performance sometimes.As the method for improving the output performance of nonaqueous electrolyte battery, it is effective to think that reducing the thickness containing active material layer.That is, if the thickness containing active material layer is thin, the moving distance of the lithium ion between positive pole and negative pole is shortened, and the relative area of positive pole and negative pole can also be increased.Thus, the internal resistance of electrode can be reduced, so it is thought that the output performance of nonaqueous electrolyte battery improves.
[0024] However, based on this knowledge, the present inventors conducted intensive research and found that although the output performance of the nonaqueous electrolyte battery can be improved if the thickness of the active material-containing layer is reduced, there is a problem that the life performance is significantly reduced.
[0025] Regarding the cause of this problem, the inventors and others have further studied and found that the decline in life performance is caused by the distortion of the electrode in the outer packaging member. That is, in the electrode of the non-aqueous electrolyte battery, through aging treatment and charging and discharging, a part of the non-aqueous solvent and electrolyte salt contained in the non-aqueous electrolyte decomposes, and sometimes produces gas. The gas is usually released to the outside of the electrode group through a porous body such as an active material layer and a diaphragm, and can be retained in the gap between the electrode group and the outer packaging member. At this time, the gas generated in the electrode can expand the gap between the electrode and the opposing electrode.
[0026] Here, if the thickness of the electrode is thin, there is a tendency that the rigidity of the electrode is low, so the gap between the electrode and the opposing electrode is easily expanded by the release of the gas. As a result, a large distortion may occur in the electrode. In this way, if a large distortion occurs in the electrode and a large gap exists locally between the electrodes, a reaction between the electrodes does not occur here, and the nominal capacity is reduced. In addition, the reaction between the electrodes may occur locally and concentratedly. Thus, the degradation of the electrode and the decomposition of the nonaqueous electrolyte are promoted, and the life performance of the battery is reduced. In addition, the internal resistance increases, which may also reduce the nominal capacity of the battery.
[0027] The battery involved in the embodiment comprises an outer packaging container, an electrode group and a sealing plate. The outer packaging container comprises a bottom wall and a side wall. The side wall extends from the bottom wall in the first direction. An opening portion opposite to the bottom wall is provided on the outer packaging container. The electrode group comprises a positive electrode, a negative electrode and an insulating layer. The positive electrode and the negative electrode are wound into a flat shape with the insulating layer sandwiched therebetween. The electrode group is housed in the outer packaging container in a manner such that the winding axis direction is orthogonal to the first direction. The sealing plate is mounted on the opening portion of the outer packaging container. The thickness of the positive electrode and the thickness of the negative electrode may be equal to or different from each other. The thickness T of each of these electrodes EThe second direction is parallel to the winding axis direction. The third direction is perpendicular to the first direction and the second direction. The thickness T of the electrode is E (mm), the thickness T of the electrode group in the direction parallel to the third direction W (mm), the innermost height H of the electrode group in the direction parallel to the first direction IC (mm) satisfies the following formula (1).
[0028] 0.02≤(T E ×T W ) / H IC ≤0.04 (1)
[0029] The battery according to the embodiment includes a relatively thin electrode having a thickness of 0.08 mm or less. In the battery according to the embodiment, the thickness T of the electrode group is adjusted so as to satisfy the above formula (1). W and the innermost height H of the electrode group IC , even with a relatively thin electrode, it is difficult for the electrode to be twisted. Thus, the battery involved in the embodiment can achieve excellent life performance. In addition, the battery involved in the embodiment can take into account both excellent life performance and excellent input and output performance.
[0030] Hereinafter, a battery according to an embodiment will be described in detail with reference to the drawings.
[0031] Figure 1 It is a perspective view schematically showing an example of a battery according to an embodiment.
[0032] Figure 1 The battery 20 shown includes an outer casing 200 , an electrode group and an electrolyte (not shown), a positive electrode terminal 6 , a negative electrode terminal 7 , and insulating gaskets 14 and 15 . Figure 1 The battery 20 shown is a rectangular battery containing an electrode group and an electrolyte (not shown) in an outer packaging member 200. The outer packaging member 200 includes an outer packaging container 1 having an opening and a sealing plate 5 mounted on the opening of the outer packaging container 1. A liquid injection port PO is provided on the sealing plate 5. The liquid injection port PO is welded by a sealing member (not shown).
[0033] like Figure 1 As shown, the outer package member 200 has a square shape. If the outer package member 200 has a square shape, the volume energy density of the battery 20 can be improved.
[0034] The outer packaging container 1 has a square can shape with a bottom wall, a pair of long side walls and a pair of short side walls, and an opening portion opposite to the bottom wall. The bottom wall is rectangular and has a pair of long sides parallel to the X-axis direction and a pair of short sides parallel to the Y-axis direction. A pair of long side walls extend from a pair of long sides of the bottom wall to the Z-axis direction. A pair of short side walls extend from a pair of short sides of the bottom wall to the Z-axis direction. Furthermore, the X-axis direction and the Y-axis direction are directions parallel to the bottom wall and intersecting each other. In addition, the Z-axis direction is a direction orthogonal to the X-axis direction and the Y-axis direction.
[0035] Here, the X-axis direction is parallel to the winding axis of the electrode group (not shown) and is parallel to the second direction. The Y-axis direction is parallel to the third direction. The Z-axis direction is parallel to the first direction.
[0036] The outer container 1 is formed of, for example, a metal plate, and examples of the metal include aluminum, an aluminum alloy, iron, and stainless steel.
[0037] The thickness of the plate constituting the long side wall of the outer packaging container 1 is preferably smaller than the thickness of the plate constituting the bottom wall of the outer packaging container 1, and smaller than the thickness of the plate constituting the short side wall of the outer packaging container 1. That is, the long side wall of the outer packaging container 1 is the part that occupies the largest area in the rectangular outer packaging member 200. Therefore, if the thickness of the plate constituting the long side wall of the outer packaging container 1 is thin, the heat dissipation of the battery 20 can be improved, and thus the life performance can be improved. The thickness of the plate constituting the long side wall of the outer packaging container 1 is preferably less than 2.0 mm, more preferably less than 1.0 mm, and further preferably less than 0.7 mm.
[0038] On the other hand, if the thickness of the plate constituting the long side wall of the outer packaging container 1 is too thin, the rigidity of the outer packaging container 1 decreases, and when gas is generated in the outer packaging container 1, the force for maintaining the shape of the electrode group is weak, and there is a concern that the battery characteristics may be degraded. The thickness of the plate constituting the long side wall of the outer packaging container 1 is preferably 0.3 mm or more, and more preferably 0.5 mm or more.
[0039] Furthermore, the thickness of the plate of the bottom wall, long side wall and short side wall of the outer packaging container 1 can be obtained by measuring the thickness of the central part of the plate with a micrometer. That is, the thickness of the plate of the bottom wall of the outer packaging container 1 can be obtained by the following method. First, the plate constituting the bottom wall is cut parallel to the YZ plane at the central position along the X-axis direction. Then, the thickness of the plate is measured at the central position along the Y-axis direction of the cut surface, as the thickness of the plate of the bottom wall of the outer packaging container 1. The thickness of the plate constituting the long side wall of the outer packaging container 1 can be obtained by the following method. First, the plate constituting the long side wall is cut parallel to the XY plane at the central position along the Z-axis direction. Then, the thickness of the plate is measured at the central position along the X-axis direction of the cut surface, as the thickness of the plate of the long side wall of the outer packaging container 1. The thickness of the plate constituting the short side wall of the outer packaging container 1 can be obtained by the following method. First, the plate constituting the short side wall is cut parallel to the XY plane at the central position along the Z-axis direction. Next, the thickness of the plate is measured at the center position along the Y-axis direction of the cut surface as the thickness of the plate of the short side wall of the outer packaging container 1. As a micrometer, for example, Quick-MiniPK-1012CPX manufactured by MITSUTOYO Co., Ltd. or a device having an equivalent function can be used.
[0040] The sealing plate 5 is placed parallel to the bottom wall of the outer packaging container 1. The sealing plate 5 is formed of the same material as the material of the outer packaging container 1. The sealing plate 5 may also be formed of a material different from that of the outer packaging container 1. The sealing plate 5 is mounted on the opening of the outer packaging container 1 by welding, for example. An insulating sheet (not shown) is provided on the main surface of the inner side of the container of the sealing plate 5. An exhaust hole or an exhaust valve may also be provided on the sealing plate 5 to discharge the gas generated in the outer packaging member 200 to the outside.
[0041] The positive terminal 6 and the negative terminal 7 are mounted on the sealing plate 5 with insulating washers 14 and 15 interposed therebetween. The positive terminal 6 and the negative terminal 7 may also be fixed to the sealing plate 5 by caulking. Unillustrated protrusions at the lower ends of the positive terminal 6 and the negative terminal 7 penetrate the sealing plate 5 and extend toward the inside of the outer packaging container 1. The positive terminals 6 and 7 are formed of metals such as aluminum, aluminum alloy, copper, or nickel.
[0042] The insulating washers 14 and 15 are formed of, for example, an insulating material. The insulating material is, for example, resin. In addition, the insulating washers 14 and 15 may be omitted.
[0043] It is preferable to appropriately select the width W of the outer packaging member 200 in the direction parallel to the second direction in accordance with the size of the electrode group housed therein. C Regarding the width W of the outer packaging member 200 CThe lower limit value is 70 mm or more according to one example, and 80 mm or more according to another example. C The upper limit value is, according to one example, 160 mm or less, and according to another example, 150 mm or less.
[0044] The width W of the outer packaging member 200 C The length can be obtained by measuring the length in the X-axis direction from one short side wall to the other short side wall at the center of the Y-axis direction and the Z-axis direction of the outer packaging member 200. For the measurement, for example, a micrometer such as Quick-Mini PK-1012CPX manufactured by MITSUTOYO Co., Ltd. or an instrument having an equivalent function can be used.
[0045] It is preferable to appropriately select the thickness T of the outer packaging member 200 in the direction parallel to the third direction in accordance with the size of the electrode group housed therein. C Regarding the thickness T of the outer packaging member 200 C The lower limit value is 10 mm or more according to one example, and 14 mm or more according to another example. C The upper limit value is 25 mm or less according to one example, and 24 mm or less according to another example. C If the thickness of the battery 20 is large, the size of the positive terminal 6 and the negative terminal 7 fixed to the sealing plate 5 and the size of the exhaust valve can be increased, thereby improving the safety of the battery 20.
[0046] The thickness T of the outer packaging member 200 C The length can be obtained by measuring the length in the Y-axis direction from one long side wall to the other long side wall at the center position along the X-axis direction and the Z-axis direction of the outer packaging member 200. For example, a micrometer such as Quick-Mini PK-1012CPX manufactured by MITSUTOYO Co., Ltd. or an instrument having an equivalent function can be used for the measurement.
[0047] It is preferable to appropriately select the height H of the outer packaging member 200 in the direction parallel to the first direction in accordance with the size of the electrode group housed therein. C Regarding the height H of the outer packaging member 200 C The lower limit value is 40 mm or more according to one example, and 45 mm or more according to another example. C The upper limit value is 85 mm or less according to one example, and 80 mm or less according to another example. CIf the thickness is low, the area of the long side wall of the outer packaging member 200 can be reduced, thereby improving the rigidity of the battery 20 .
[0048] The height H of the outer packaging member 200 C It can be obtained by measuring the length in the Z-axis direction from the bottom wall to the sealing plate 5 at the center position along the X-axis direction and the Y-axis direction of the outer packaging member 200. For the measurement, for example, a micrometer such as Quick-MiniPK-1012CPX manufactured by MITSUYO Co., Ltd. or an instrument having an equivalent function can be used.
[0049] Here, the outer packaging member 200 may expand and deform due to the gas generated inside the outer packaging member 200 during the charge / discharge and aging process of the battery 20. In particular, the long side wall portion is easily expanded by the internal gas, so the thickness T of the outer packaging member 200 is C Therefore, when measuring the width W of the outer packaging member 200, C , thickness T C and height H C When doing so, it is necessary to perform the exhaust treatment after exhausting the gas inside the outer packaging member 200 to the outside.
[0050] Thickness T of outer packaging component C and height H C It is preferable to satisfy the following formula (7).
[0051] 2.5≤H C / T C ≤3.5 (7)
[0052] Such a battery 20 can be said to have a higher H than a battery using a conventional outer packaging member. C Low, and thickness T C Such a battery 20 has a smaller area of the long side wall than a conventional battery, so that even if gas is generated inside the outer packaging member 200, it is difficult to expand and deform. Such a battery 20 tends to have a long life performance.
[0053] The width W of the outer packaging member 200 C and thickness T C It is preferable to satisfy the following formula (8).
[0054] 4.5≤W C / T C ≤6.5 (8)
[0055] Such a battery 20 has a thickness T of 1.3mm compared to a battery using a conventional outer casing member. C Such a battery 20 tends to have a longer lifespan than conventional batteries in that the electrode group is less likely to deteriorate.
[0056] The width W of the outer packaging member 200 C and height H C W C / H C It is preferably 1.3 or more and 2.2 or less. If such an outer packaging member 200 is used, there is a tendency that the life performance of the battery 20 is improved. That is, the ratio W of the conventional square outer packaging member C / H C Less than 1.3. Such an outer packaging member has excellent heat dissipation due to the large area of the long side wall. However, as mentioned above, the long side wall is easy to expand when gas is generated, so that the electrodes of the electrode group contained inside are also easy to expand, and the electrodes are easy to be twisted.
[0057] Here, an outer packaging member having a square shape is used as an example to explain, but the shape of the outer packaging member is not limited to a square. That is, the bottom wall of the outer packaging container 1 can also be circular, elliptical, or polygonal. In addition, the shape of the outer packaging container 1 can also be cylindrical or amorphous.
[0058] Figure 2 yes Figure 1 The expanded stereogram of the battery shown in FIG. Figure 2 As shown, the battery 20 contains an electrode group 2, a positive electrode lead 3, a negative electrode lead 4, fixing members 11 and 12, a positive electrode insulating cover 25, a negative electrode insulating cover 26, insulating cover fixing tapes 27 and 28, an insulating tape 30 and an electrolyte (not shown) in an outer packaging member 200.
[0059] The electrode group 2 includes a positive electrode, a negative electrode, and an insulating layer. The electrode group 2 is formed by winding the positive electrode and the negative electrode into a flat shape along a winding axis with an insulating layer interposed therebetween. The details of the electrode group 2 will be described later.
[0060] The fixing members 11 and 12 partially fix the positive electrode collector tab 8a and the negative electrode collector tab 9a in the electrode group 2, respectively. The fixing members 11 and 12 each have two clamping parts. The two clamping parts bundle a part of a plurality of collector tabs that are relatively wound through the innermost circumference. The details of the positive electrode collector tab 8a and the negative electrode collector tab 9a will be described later. The fixing members 11 and 12 are formed of metal such as aluminum, aluminum alloy, copper or nickel. In addition, the fixing members 11 and 12 can also be omitted.
[0061] The insulating tape 30 covers the electrode group 2 except for the positive electrode collector tab 8a and the negative electrode collector tab 9a. As the base material of the insulating tape 30, at least one resin selected from polyester (PET), polyimide, polyphenylene sulfide (PPS) and polypropylene can be used. In addition, the insulating tape 30 can also be omitted.
[0062] The positive lead 3 is electrically connected to the positive terminal 6 and the positive collector ear 8a. The positive lead 3 has a connecting plate 3a connected to the positive terminal 6, and the first and second clamping strips 3c and 3d connected to the positive collector ear 8a. The connecting plate 3a is in contact with the sealing plate 5 via an insulating sheet (not shown) provided on the main surface of the inner side of the container of the sealing plate 5. The protruding portion of the positive terminal 6 is embedded in the through hole 3b provided on the connecting plate 3a and is fixed by caulking. The first and second clamping strips 3c and 3d are divided into two strands from the connecting plate 3a, and are clamped between the fixing member 11 and the positive collector ear 8a. In addition, the positive lead 3 can also be omitted.
[0063] The negative electrode lead 4 is electrically connected to the negative electrode terminal 7 and the negative electrode collector ear 9a. The negative electrode lead 4 has a connecting plate 4a connected to the negative electrode terminal 7, and a first and second clamping strips 4c and 4d connected to the negative electrode collector ear 9a. The connecting plate 4a is in contact with the sealing plate 5 via an insulating sheet (not shown) provided on the main surface of the container inner side of the sealing plate 5. The protruding portion of the negative terminal 7 is embedded in the through hole 4b provided on the connecting plate 4a and is fixed by caulking. The first and second clamping strips 4c and 4d are divided into two strands from the connecting plate 4a, and are clamped between the fixing member 12 and the negative electrode collector ear 9a. In addition, the negative electrode lead 4 can also be omitted.
[0064] The positive electrode insulating cover 25 covers the side surface of the electrode group 2 along the X-axis direction in a manner that sandwiches the first and second clamping bars 3c, 3d of the positive electrode lead 3, the fixing member 11, and the positive electrode collector ear 8a. The positive electrode insulating cover 25 includes a first side wall 25b and a second side wall 25c facing each other, a back member 25d connecting them, a convex portion 25e provided on the first side wall, a convex portion 25f provided on the second side wall, a convex portion 25g provided on the back member 25d, and an extension portion 25h extending from the lower end of the first side wall 25b, the second side wall 25c, and the back member 25d. The convex portions 25e, 25f, and 25g are embedded in the side surface of the electrode group 2 in the X-axis direction in a manner that sandwiches the two clamping portions of the fixing member 11. A flow path groove 25i extending in the X-axis direction is provided in the extension portion 25h. The flow path groove 25i can hold an electrolyte not shown. Furthermore, the positive electrode insulating cover 25 may also be omitted.
[0065] The negative electrode insulating cover 26 has the same structure as the positive electrode insulating cover 25. The negative electrode insulating cover 26 covers the other side surface of the electrode group 2 along the X-axis direction so as to sandwich the first and second clamping bars 4c, 4d of the negative electrode lead 4, the fixing member 12, and the negative electrode collector tab 9a. The negative electrode insulating cover 26 may also be omitted.
[0066] The insulating cover fixing tapes 27 and 28 respectively fix the positive electrode insulating cover 25 and the negative electrode insulating cover 26 to the insulating tape 30. The insulating cover fixing tapes 27 and 28 may be omitted.
[0067] Figure 3 yes Figure 2 The battery shown is an exploded perspective view of an electrode group. Figure 3 The electrode group 2 shown includes a pair of electrodes, namely a positive electrode 8 and a negative electrode 9, and separators 10a and 10b as insulating layers. The electrode group 2 includes a sheet-like stacked body in which the negative electrode 9, the separator 10a, the positive electrode 8, and the separator 10b are stacked in this order. The electrode group 2 is formed by winding the stacked body into a flat shape along the winding axis WA in such a way that the separator 10b is located at the innermost circumference. The winding axis WA is parallel to the X-axis direction.
[0068] The positive electrode 8 includes a positive electrode collector 8c, a positive electrode active material layer 8b, and a positive electrode collector ear 8a. The positive electrode collector 8c has a strip shape, which has a pair of long sides parallel to the Z-axis direction and a pair of short sides parallel to the X-axis direction. The positive electrode active material layer 8b is provided in the X-axis direction of at least one main surface of the positive electrode collector 8c, from one long side to a position between one long side and the other long side. The length from the one long side to the position between the one long side and the other long side is taken as the width W of the positive electrode active material layer 8b in the direction parallel to the second direction. PE That is, the width W PE It can also be referred to as the length of the short side of the positive electrode active material layer 8b. In addition, the positive electrode active material layer 8b is provided from one short side to the other short side in the Z-axis direction of at least one main surface of the positive electrode collector 8c. The positive electrode collector tab 8a is a portion of the positive electrode collector 8c that is not covered by the positive electrode active material layer 8b. The positive electrode collector tab 8a extends in a direction different from the negative electrode collector tab 9a along the X-axis direction.
[0069] The positive electrode current collector 8c is, for example, a metal foil of aluminum, aluminum alloy, copper, or nickel. Furthermore, the positive electrode collector tab 8a may not be integrated with the positive electrode current collector 8c. That is, the positive electrode collector tab 8a may be formed by joining a metal foil to one long side of the positive electrode current collector 8c. As the metal foil, the same as that of the positive electrode current collector 8c may be used.
[0070] The positive electrode active material containing layer 8b may be provided on both main surfaces of the positive electrode current collector 8c or on one main surface. The positive electrode active material containing layer 8b contains a positive electrode active material. The positive electrode active material containing layer 8b may contain a conductive agent and a binder in addition to the positive electrode active material.
[0071] As the positive electrode active material, for example, a lithium transition metal composite oxide can be used. For example, a lithium transition metal composite oxide is LiCoO2, LiNi 1-x Co x O2(0<x<0.3), LiMn x Ni y Coz O2(0<x<0.5, 0<y≤0.8, 0≤z<0.5), LiMn 2-x M x O4 (M is at least one element selected from Mg, Co, Al and Ni, 0<x<0.2), LiMPO4 (M is at least one element selected from Fe, Co, Ni and Mn), etc.
[0072] The average particle size of the secondary particles of the positive electrode active material is preferably less than 10 μm, more preferably less than 6 μm. If the average particle size of the secondary particles of the positive electrode active material is small, the internal resistance is small, so there is a tendency for the heat dissipation accompanying charging and discharging to decrease. Therefore, if the average particle size of the secondary particles of the positive electrode active material is small, the life performance of the battery 20 can be improved.
[0073] The conductive agent can improve the electronic conductivity of the electrode. As the conductive agent, carbonaceous materials such as acetylene black, carbon black, and graphite can be used.
[0074] The binder can improve the adhesion between the active material, the conductive agent and the current collector. As the binder, polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVdF) and fluorine-based rubber can be used.
[0075] In the positive electrode active material containing layer, the mixing ratio of the positive electrode active material, the conductive agent and the binder is preferably in the range of 80-95 mass % of the positive electrode active material, 3-18 mass % of the conductive agent and 2-7 mass % of the binder.
[0076] The density of the positive electrode active material containing layer 8b is preferably 2.7 g / cm 3 Above and 3.3g / cm 3 If the density of the positive electrode active material layer 8b is within this range, the life performance of the battery 20 tends to be high. That is, if the density of the positive electrode active material layer 8b is 3.3 g / cm 3 If the density of the positive electrode active material layer 8b is 2.7 g / cm 3 If the distance between the positive electrode active material particles is above 1.5, the internal resistance tends to decrease.
[0077] The negative electrode 9 includes a negative electrode collector 9c, a negative electrode active material layer 9b, and a negative electrode collector ear 9a. The negative electrode collector 9c has a strip shape, which has a pair of long sides parallel to the Z direction and a pair of short sides parallel to the X direction. The negative electrode active material layer 9b is provided from one long side to a position between one long side and the other long side in the X-axis direction of at least one main surface of the negative electrode collector 9c. The length from the long side of the one side to the position between the long side of the one side and the other long side is taken as the width W of the negative electrode active material layer 9b in the direction parallel to the second direction. NE That is, the width W NE It can also be referred to as the length of the short side of the negative electrode active material layer 9b. In addition, the negative electrode active material layer 9b is provided from the short side of one side to the short side of the other side in the Z-axis direction of at least one main surface of the negative electrode collector 9c. The negative electrode collector tab 9a is a portion of the negative electrode collector 9c that is not covered by the negative electrode active material layer 9b. The negative electrode collector tab 9a extends in a direction different from the positive electrode collector tab 8a along the X-axis direction. Furthermore, the negative electrode collector tab 9a may also extend in the same direction as the positive electrode collector tab 8a.
[0078] The negative electrode current collector 9c is, for example, a metal foil of aluminum, aluminum alloy, copper, or nickel. Furthermore, the negative electrode current collector tab 9a may not be integrated with the negative electrode current collector 9c. That is, the negative electrode current collector tab 9a may be formed by joining a metal foil to one long side of the negative electrode current collector 9c. As the metal foil, the same as that of the negative electrode current collector 9c may be used.
[0079] The negative electrode active material containing layer 9b may be provided on both main surfaces of the negative electrode current collector 9c or on one main surface. The negative electrode active material containing layer 9b contains a negative electrode active material. The negative electrode active material containing layer 9b may contain a conductive agent and a binder in addition to the negative electrode active material.
[0080] As the negative electrode active material, it is preferred to use a material having a potential lower limit of 1.0 V (vs. Li / Li) that allows lithium ions to be charged and discharged. + ) or more. As such a compound, lithium titanium composite oxide is preferably used. Lithium titanium composite oxide has almost no volume change accompanying the charge and discharge reaction. Therefore, if lithium titanium composite oxide is used as the negative electrode active material, the expansion and contraction of the electrode can be suppressed. Therefore, if lithium titanium composite oxide is used as the negative electrode active material, it is more difficult to produce distortion of the electrode when gas is generated. In addition, the heat dissipation of lithium titanium composite oxide accompanying charge and discharge is small. Therefore, if lithium titanium composite oxide is used as the negative electrode active material, even if the area of the long side wall of the outer packaging member 200 is relatively small and the heat dissipation is low, the life performance of the battery 20 can be improved.
[0081] Examples of lithium-titanium composite oxides include Li-TiO2 having a spinel structure.4+x Ti5O 12 (0≤x≤3), Li with ramsdellite structure 2+y Ti3O7 (0≤y≤3) and orthorhombic titanium-containing oxides. Examples of orthorhombic titanium-containing oxides include sodium-containing niobium-titanium composite oxides. Examples of sodium-containing niobium-titanium composite oxides include compounds having the general formula Li 2+v Na 2-w M1 x Ti 6-y-z Nb y M2 z O 14+δ A compound represented by (0≤v≤4, 0<w<2, 0≤x<2, 0<y<6, 0≤z<3, y+z<6, -0.5≤δ≤0.5, M1 contains at least one selected from Cs, K, Sr, Ba, Ca, and M2 contains at least one selected from Zr, Sn, V, Ta, Mo, W, Fe, Co, Mn, Al).
[0082] If sodium-containing niobium-titanium composite oxide is used as the negative electrode active material, it is similar to using Li 4+x Ti5O 12 Compared with the above, the negative electrode potential can be lowered, so the voltage of the battery 20 can be increased.
[0083] The average primary particle size of the negative electrode active material is preferably less than 1 μm. If the average particle size of the primary particles of the negative electrode active material is small, the internal resistance is reduced, so there is a tendency for the heat dissipation accompanying charging and discharging to decrease. Therefore, if the average particle size of the primary particles of the negative electrode active material is small, the life performance of the battery 20 can be improved.
[0084] The negative electrode active material containing layer 9b may contain a negative electrode active material other than the lithium titanium composite oxide. Examples of such other negative electrode active materials include carbonaceous materials such as graphite, and tin-silicon alloy materials.
[0085] The conductive agent can improve the electronic conductivity of the electrode. As the conductive agent, acetylene black, carbon black, graphite, etc. can be used.
[0086] The binder can improve the adhesion between the active material, the conductive agent and the current collector. Examples of the binder include polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVdF), fluorine-based rubber, and styrene-butadiene rubber.
[0087] In the negative electrode active material containing layer 9 b , the mixing ratio of the negative electrode active material, the conductive agent, and the binder is preferably in the range of 73 to 98 mass % of the negative electrode active material, 0 to 20 mass % of the conductive agent, and 2 to 7 mass % of the binder.
[0088] The separators 10a and 10b function as insulating layers. The separators 10a and 10b are, for example, porous films or nonwoven fabrics. The porous films and nonwoven fabrics may each contain at least one compound selected from polyethylene, polypropylene, polyethylene terephthalate, and cellulose. The separators 10a and 10b may also be organic fiber films or inorganic films that cover at least a portion of the main surfaces of the positive electrode 8 and the negative electrode 9. In addition, as an insulating layer, a solid electrolyte layer may be used instead of the separators 10a and 10b.
[0089] The thickness of the diaphragm is preferably greater than 6 μm and less than 15 μm. When the thickness of the diaphragm is within this range, the safety, capacity and life performance of the battery 20 can be improved. That is, when the thickness of the diaphragm is greater than 6 μm, the probability of short circuit between the positive and negative electrodes can be reduced, thereby improving the safety and reliability of the battery 20. On the other hand, when the thickness of the diaphragm is less than 15 μm, the increase in the amount of auxiliary components in the battery 20 can be suppressed, thereby improving the energy density. In addition, when the thickness of the diaphragm is less than 15 μm, there are moderate gaps in the outer packaging member 200, so the battery 20 is difficult to expand when gas is generated, which can improve the battery characteristics.
[0090] The electrolyte not shown in the figure can be retained in the positive electrode 8, the negative electrode 9 and the separators 10a and 10b. The electrolyte can also be a non-aqueous electrolyte containing an electrolyte salt and an organic solvent. That is, the battery involved in the embodiment can also be a non-aqueous electrolyte battery. The non-aqueous electrolyte can be liquid or gel. The liquid non-aqueous electrolyte can be prepared by dissolving the electrolyte in an organic solvent. The gel non-aqueous electrolyte can be prepared by gelling the liquid non-aqueous electrolyte using a polymer material. The concentration of the electrolyte salt in the liquid non-aqueous electrolyte is, for example, greater than 0.5 mol / L and less than 2.5 mol / L.
[0091] As the electrolyte, for example, lithium salts such as lithium perchlorate (LiCl4), lithium hexafluorophosphate (LiPF6), lithium tetrafluoroborate (LiBF4), lithium hexafluoroarsenate (LiAsF6), lithium trifluoromethanesulfonate (LiCF3SO3), and lithium bistrifluoromethanesulfonyl imide [LiN(CF3SO2)2] or mixtures thereof can be cited. As the electrolyte, preferably, it is difficult to oxidize even at high potential, and LiPF6 is most preferred.
[0092] As the organic solvent, for example, cyclic carbonates such as propylene carbonate (PC), ethylene carbonate (EC), and vinylene carbonate can be listed, and chain carbonates such as diethyl carbonate (DEC), dimethyl carbonate (DMC), and methyl ethyl carbonate (MEC), and cyclic ethers such as tetrahydrofuran (THF), 2 methyltetrahydrofuran (2MeTHF), and dioxolane (DOX), and chain ethers such as dimethoxyethane (DME), diethoxyethane (DEE), and gamma-butyrolactone (GBL), acetonitrile (AN), and sulfolane (SL), etc. Such organic solvents can be used alone or as a mixture of two or more.
[0093] Examples of the polymer material include polyvinylidene fluoride (PVdF), polyacrylonitrile (PAN), and polyethylene oxide (PEO).
[0094] Furthermore, as the non-aqueous electrolyte, a room-temperature molten salt (ionic melt) containing lithium ions or the like may be used.
[0095] Regarding the coating width W of the electrode group 2 in the direction parallel to the second direction W The lower limit of the coating width W of the electrode group 2 is 85 mm or more according to one example, and 90 mm or more according to another example. W The upper limit value is 130 mm or less according to one example, and 125 mm or less according to another example. Here, the coating width W of the electrode group 2 is W , the width W of the positive electrode active material layer in the direction parallel to the second direction PE and a width W of the negative electrode active material layer in a direction parallel to the second direction NE The width of the active material layer is the larger one. PE and the width W of the negative electrode active material layer NE If they are the same size, the width of either one is taken as the coating width W. W .
[0096] Coating width W of electrode group 2 W It can be obtained by the following method. First, in an inert gas atmosphere such as argon, the battery 20 is disassembled, and the electrode group 2 is taken out from the outer packaging member 200. Then, the electrode group 2 is immersed in an organic solvent such as ethyl methyl carbonate for 24 hours. Then, the electrode group 2 is taken out from the organic solvent and immersed in an organic solvent such as ethyl methyl carbonate for 24 hours. Then, the electrode group 2 is taken out from the organic solvent, and it is vacuum dried at a temperature of 90°C to remove the electrolyte from the electrode group 2. In this way, the cleaned electrode group 2 is obtained.
[0097] Next, the electrode group 2 after washing is unfolded, and the sheet-like positive electrode 8 and negative electrode 9 are taken out. Next, the width of the positive electrode active material layer 8b and the negative electrode active material layer 9b in the direction parallel to the second direction is measured in the positive electrode 8 and the negative electrode 9, respectively, that is, the width in the direction parallel to the short side of the positive electrode active material layer 8b and the negative electrode active material layer 9b. The measurement is performed at five locations in the positive electrode active material layer 8b and the negative electrode active material layer 9b that are arranged at equal intervals along the long side direction, and the average values thereof are respectively taken as the width W of the positive electrode active material layer. PE and the width W of the negative electrode active material layer NE Then, these widths W PE and width W NE The larger width of the electrode group 2 is taken as the coating width W W In addition, for example, a digital meter ID-H0530543 series manufactured by MITSUTOYO CO., LTD. or a device having an equivalent function thereto can be used for the measurement.
[0098] Figure 4 yes Figure 3 A stereogram of the electrode assembly shown.
[0099] Regarding the thickness T of the electrode group 2 in the direction parallel to the third direction W The lower limit value of is 13 mm or more according to one example, and 14 mm or more according to another example. W The upper limit value is 24 mm or less according to one example, and 23 mm or less according to another example. If the thickness T of the electrode group 2 W As the thickness increases, the rigidity of the electrode group 2 increases, so that the electrode group 2 is less likely to deform when gas is generated, and the life performance of the battery 20 tends to be improved.
[0100] The thickness T of the electrode group 2 W It can be obtained by the following method. First, obtain the cleaned electrode group 2 by the same method as described above. Next, in the cleaned electrode group 2, place it on a table in such a way that the surface parallel to the XZ plane becomes the bottom surface. Next, place a weight on the other surface parallel to the XZ plane in such a way that a load of 100 kPa is achieved relative to the surface. Next, at the center of the X-axis direction and the Z-axis direction of the electrode group 2, use a vernier caliper to measure the length from one surface to the other surface, that is, the length of the electrode group 2 in the Y-axis direction. This length is taken as the thickness T of the electrode group 2. W For the measurement, for example, a digital meter ID-H0530543 series manufactured by MITSUTOYO CO., LTD. or a device having an equivalent function thereto can be used.
[0101] Regarding the height H of the electrode group 2 in the direction parallel to the first directionW The lower limit value is 35 mm or more according to one example, and 40 mm or more according to another example. W The upper limit value is 75 mm or less according to one example, and 73 mm or less according to another example. W As the value is lower, the life performance of the battery 20 tends to be improved.
[0102] The height H of the electrode group 2 W It can be obtained by the following method. First, the cleaned electrode group 2 is placed on a table in the same manner as above so that the surface parallel to the XZ plane is horizontal. Then, a weight is placed on the other surface parallel to the XZ plane so that a load of 100 kPa is achieved relative to the surface. Then, at the center of the X-axis direction and the Y-axis direction, the length of the electrode group 2 in the Z-axis direction is measured with a vernier caliper. This length is taken as the height H of the electrode group 2. W For the measurement, for example, a digital meter ID-H0530543 series manufactured by MITSUTOYO CO., LTD. or a device having an equivalent function thereto can be used.
[0103] The nominal capacity A of the battery 20 is preferably 4 Ah or more, and more preferably 5 Ah or more. That is, the battery 20 according to the embodiment can be suitably used as a high-capacity battery. The upper limit of the nominal capacity A is not particularly limited, but is 17 Ah according to one example.
[0104] The nominal capacity of the battery 20 is the discharge capacity obtained by the following method. First, the battery is charged at a constant current of 0.05C to the maximum operating voltage at 25°C. Then, the battery is further charged to a current value of 0.01C while maintaining the maximum operating voltage. Then, the battery is discharged at a rate of 0.05C to the end voltage to obtain the discharge capacity.
[0105] Furthermore, the above-mentioned "maximum operating voltage" is the maximum voltage at which the battery can be used without danger or defect, and is a value inherent in each battery. The maximum operating voltage is, for example, the voltage described as "charging voltage" and "safety-guaranteed maximum voltage" in the battery manual. In addition, the "termination voltage" is the lowest operating voltage at which the battery can be used in a manner that suppresses overdischarge of either the positive electrode or the negative electrode, that is, suppresses battery degradation, and is a value inherent in each battery.
[0106] In the battery 20, the relative area S (m 2 ) and the nominal capacity A (Ah) preferably satisfy the following formula (6).
[0107] 3.5≤A / S≤10 (6)
[0108] Such a battery 20 can achieve both excellent life performance and excellent output performance. That is, the ratio A / S of the nominal capacity A and the relative area S is less than 3.5, which can be expressed as the thickness T of the electrode. E In addition, the ratio A / S is greater than 10, which can indicate the thickness T of the electrode. E The ratio A / S is preferably 3.9 or more and 10 or less.
[0109] Here, the relative area S is the area of the active material layer on one side, between the area containing the positive electrode active material layer 8b and the area containing the negative electrode active material layer 9b in a pair of opposite positive electrodes 8 and negative electrodes 9. That is, when the area containing the positive electrode active material layer 8b and the area containing the negative electrode active material layer 9b are different, the relative area S is the area of the active material layer on the smaller side. In addition, when the area containing the positive electrode active material layer 8b and the area containing the negative electrode active material layer 9b are equal, the relative area S is the area of the active material layer on one side.
[0110] Furthermore, when the positive electrode active material layer 8b and the negative electrode active material layer 9b are arranged on the two main surfaces of each collector, the total area of the active material layer arranged on one main surface of the collector and the area of the active material layer arranged on the other main surface of the collector is taken as the relative area S.
[0111] The relative area S can be calculated, for example, by the following method. First, the electrode group 2 after washing is obtained by the above method. Next, the electrode group 2 is unfolded, and the sheet-like positive electrode 8 and negative electrode 9 are taken out. Next, the length of the long side and the length of the short side of the positive electrode active material layer 8b and the negative electrode active material layer 9b provided on one main surface of the collector are measured, and the area of the positive electrode active material layer 8b and the negative electrode active material layer 9b are calculated respectively. Next, the length of the long side and the length of the short side of the positive electrode active material layer 8b and the negative electrode active material layer 9b provided on the other main surface of the collector are measured, and the area of the other side containing the positive electrode active material layer 8b and the negative electrode active material layer 9b is calculated respectively. The total value of the area of one side and the area of the other side obtained in this way is respectively used as the area containing the positive electrode active material layer 8b and the area containing the negative electrode active material layer 9b. Furthermore, when the active material layer is provided on only one main surface, the calculation of the area of the other side is omitted.
[0112] In addition, when the area containing the positive electrode active material layer 8b and the area containing the negative electrode active material layer 9b are different from each other, the smaller area is taken as the relative area S. In addition, when the area containing the positive electrode active material layer 8b and the area containing the negative electrode active material layer 9b are equal to each other, the area of one side is taken as the relative area S. In addition, in the measurement, for example, a digital meter ID-H0530543 series manufactured by MITSUTOYO Co., Ltd. or an apparatus having an equivalent function thereto can be used.
[0113] Figure 5 yes Figure 4 A cross-sectional view of the electrode assembly along line VV is shown. Figure 5 The cross-sectional view shown is a cross-sectional view obtained by cutting the electrode group 2 in parallel with the YZ plane. Figure 5 In FIG. 1 , the thick solid line represents the positive electrode 8 , the dotted line represents the negative electrode 9 , and the thin solid lines represent the separators 10 a and 10 b .
[0114] like Figure 5 As shown, the innermost surface of the electrode group 2, i.e., the innermost peripheral surface, is composed of a portion 10b-1 of the separator 10b and a portion 9-1 of the negative electrode 9. A through hole is formed in the portion surrounded by the innermost peripheral surface along the direction orthogonal to the Y-axis direction and the Z-axis direction, i.e., the X-axis direction. By making the portions 10b-1 of the separator contact each other and the separator 10b-1 and the portion 9-1 of the negative electrode 9, the through hole can be blocked at the center position along the X-axis direction of the electrode group 2.
[0115] The innermost peripheral height H of the electrode group 2 in the direction parallel to the first direction IC According to one example, the lower limit value of the height H is 26 mm or more. IC The upper limit value is 53 mm or less according to one example. IC , in the electrode group 2, the length of the straight portion is substantially equal to the length of the portion of the electrode extending in the Z-axis direction without bending. The electrode located in the straight portion is more likely to be twisted when gas is generated in the electrode group 2 than the electrode located in the portion other than the straight portion, i.e., the R portion. Therefore, if the innermost circumference height H of the electrode group 2 is reduced, IC , reducing the proportion of the straight portion in electrode group 2 makes it more difficult for the electrode to be twisted.
[0116] Here, the innermost height H IC To pass Figure 5 The distance between the straight line parallel to the Y-axis direction and the straight line passing through the point P1 and parallel to the Y-axis direction is shown. Points P1 and P2 are located at the innermost surface and are farthest from each other in the Z-axis direction.
[0117] The innermost height H of the electrode group 2 ICIt can be obtained by the following method. First, the electrode group 2 after cleaning is obtained by the above method. Then, the electrode group 2 is cut at 5 locations parallel to the YZ plane. Next, the fold of the innermost diaphragm 10b in the cut surface is visually confirmed. That is, in the diaphragm 10b, the place where it is bent due to a large external force during winding can be visually confirmed as a fold. The fold at the head of the electrode group 2 is taken as point P1, and the fold next to the head of the roll is taken as point P2. Next, use a vernier caliper to measure the distance between the straight line passing through point P1 and parallel to the Y-axis direction and the straight line passing through point P2 and parallel to the Y-axis direction. Perform this operation at 5 locations on the cut surface, and take their average value as the innermost circumference height H of the electrode group 2. IC For the measurement, for example, a digital meter ID-H0530543 series manufactured by MITSUTOYO CO., LTD. or a device having an equivalent function thereto can be used.
[0118] Here, the separator 10b is described as being located at the innermost circumference of the electrode group 2, but the positive electrode may be located at the innermost circumference, or the negative electrode may be located at the innermost circumference. In this case, in the positive electrode or the negative electrode located at the innermost circumference of the electrode group 2, by confirming the fold at the beginning of the winding of the electrode group 2 and the fold next to the fold at the beginning of the winding, the height H of the innermost circumference can be obtained in the same way as in the case of the separator 10b. IC .
[0119] The thickness T of the electrode group 2 is preferably W (mm) and the innermost height H of the electrode group 2 IC (mm) satisfies the following formula (5).
[0120] 1.8≤H IC / T W ≤3.2 (5)
[0121] Such a battery 20 can achieve excellent life performance. That is, if the height H of the innermost circumference of the electrode group 2 is IC The thickness T of the electrode group W The ratio H IC / T W When the ratio H is 1.8 or more, the gas is easily released from the electrode group 2 to the outside when the gas is generated. IC / T W When the ratio is 3.2 or less, the force for the electrode group 2 to maintain its shape is moderate, and deformation of the electrode group 2 can be suppressed when gas is generated.
[0122] Figure 6 yes Figure 3 to Figure 5 The electrode assembly shown is a cross-sectional view of a positive electrode. Figure 6The positive electrode 8 shown includes a positive electrode collector 8c, a positive electrode active material containing layer 8b1 provided on one main surface of the positive electrode collector 8c, a positive electrode active material containing layer 8b2 provided on the other main surface of the positive electrode collector 8c, and a positive electrode collector tab 8a.
[0123] What is the thickness of the positive electrode? PE , is the thickness T of the positive electrode collector 8c PE1 , the thickness T of the positive electrode active material layer 8b1 PE2 and the thickness T of the positive electrode active material layer 8b2 PE3 Furthermore, when the positive electrode active material layer 8b is provided only on one surface of the positive electrode current collector 8c, the thickness T of the positive electrode is PE is the thickness T of the positive electrode current collector 8c PE1 , the thickness T of the positive electrode active material layer 8b1 PE2 or the thickness T of the positive electrode active material layer 8b2 PE3 The total value of the negative electrode thickness T NE It can also be related to the thickness T of the positive electrode PE Calculate in the same way.
[0124] The thickness of the positive electrode is T PE and the thickness of the negative electrode T NE The thickness T of the positive electrode can be the same or different. PE Preferably, the thickness T of the negative electrode NE If the thickness of the positive electrode is T PE T NE The thicker the thickness, the higher the safety of the battery 20 tends to be.
[0125] The thickness of the electrode is T E It can be obtained by the following method. First, the electrode group 2 after cleaning is obtained by the above method. Next, the electrode group 2 is unfolded, and the sheet-like positive electrode 8 and negative electrode 9 are taken out. Next, the thickness of the positive electrode and the negative electrode are measured at 50 points in the positive electrode 8 and the negative electrode 9 where the positive electrode active material layer 8b and the negative electrode active material layer 9b are provided, and their average value is taken as the thickness of each electrode. Regarding the 50 points, in the positive electrode active material layer 8b and the negative electrode active material layer 9b, the points are set as the intersections of 10 straight lines parallel to the short sides arranged at equal intervals along the long sides and 5 straight lines parallel to the long sides arranged at equal intervals along the short sides. The thickness T thus obtained is PE and T NE The thicker thickness is taken as the electrode thickness T E Furthermore, at a thickness of T PE and T NE If the values are the same, the thickness of either electrode is taken as the thickness T of the electrode. E .
[0126] The thickness of the electrode is T E is greater than or equal to 0.03 mm and less than or equal to 0.08 mm. E is greater than 30 μm and less than 80 μm. If the thickness T of the electrode E Within this range, the life performance of the battery 20 can be improved. That is, if the thickness T of the electrode E If the thickness is less than 0.03 mm, the electrode rigidity is too low, and the electrode is easily distorted when releasing gas. E If the thickness is greater than 0.08 mm, the electrode rigidity is too high, and it is difficult to generate a gap between the electrodes when gas is generated, and it is difficult to release gas from the electrodes. Therefore, the gas is retained between the electrodes, and a large gap may be generated locally. In addition, if the electrode thickness T E If it is larger than 0.08 mm, the internal resistance will increase, and the heat generated by charging and discharging will increase.
[0127] The thickness of the electrode is T E , the thickness of the electrode group T W and the height H of the innermost circumference of the electrode group IC The following formula (1) is satisfied.
[0128] 0.02≤(T E ×T W ) / H IC ≤0.04 (1)
[0129] Compared with the conventional electrode group, the electrode group 2 has a thickness T E Thin, the thickness T of the electrode group 2 W The inner surface of the electrode group 2 has a height H IC In such an electrode group 2, since the thickness of the electrode group 2 is relatively thick, the rigidity of the electrode group 2 itself is high, even if the thickness of the electrode is E The electrode is relatively thin, so it is difficult for the electrode to be twisted when gas is generated in the electrode group. In addition, due to the height H of the inner circumference IC The thickness T of the electrode is relatively low, so the proportion of the straight part in the electrode group 2 is small, and the electrode is less likely to be twisted. Therefore, the battery satisfying the above formula (1) can achieve excellent life performance. E and the thickness T of the electrode group W The product of the innermost height H of the electrode group IC The ratio (T E ×T W ) / H IC It is preferably 0.02 or more and 0.033 or less.
[0130] The thickness of the electrode is T E(mm) and the height H of the electrode group W (mm) preferably satisfies the following formula (2).
[0131] 800≤H W / T E ≤1500 (2)
[0132] If such an electrode group 2 is provided, the life performance of the battery 20 can be improved. W The thickness of the electrode T E The ratio H W / T E When the H is 800 or more, the gas is easily discharged from the electrode when the gas is generated, and the gas is difficult to stay between the electrodes, which tends to suppress the expansion of the local distance between the electrodes. W / T E If the internal resistance of the battery 20 is lowered to 800 or more, the capacity can be increased. W / T E When the value is 1500 or less, the electrode is unlikely to be distorted when gas is generated, the internal resistance of the battery 20 is reduced, and the capacity can be increased.
[0133] The thickness of the electrode is T E and the coating width W of the electrode group W It is preferable to satisfy the following formula (3).
[0134] 1600≤W W / T E ≤2500 (3)
[0135] The battery 20 having such an electrode group 2 tends to have a high life performance. W The thickness of the electrode T E W W / T E If the W is greater than 1600 and less than 2500, the gas is easily discharged from the electrode when the gas is generated, and there is also a tendency that the electrode group is less likely to be twisted. W / T E When the electrode group has a density of 1600 or more and 2500 or less, the battery performance is unlikely to be degraded when gas is generated.
[0136] The thickness of the electrode group is T W and the electrode thickness T E It is preferable to satisfy the following formula (4).
[0137] 250≤T W / T E ≤450 (4)
[0138] Such a battery 20 can improve the life performance. That is, if the thickness T of the electrode group W The thickness of the electrode T E T W / T E If the ratio T is 250 or more, the force for the electrode group 2 to maintain its shape is moderate, so that deformation of the electrode group 2 can be suppressed when gas is generated. W / T E When the temperature is 450 or less, gas can be easily discharged from the electrode group 2 to the outside when gas is generated, and battery characteristics can be improved.
[0139] The battery according to the above-described embodiment has a relatively thin electrode having a thickness of 0.08 mm or less. E and the thickness T of the electrode group W The product of the innermost height H of the electrode group IC The ratio (T E ×T W ) / H IC By setting it to be greater than 0.02 and less than 0.04, even if the electrode has a relatively thin thickness, it is possible to make it difficult for the electrode to be twisted. Thus, the battery involved in the embodiment can achieve excellent life performance. In addition, the battery involved in the embodiment can also take into account excellent life performance and excellent input and output performance. In addition, the battery involved in the embodiment is suitable for use as a secondary battery.
[0140] (Second embodiment)
[0141] According to a second embodiment, a battery pack is provided. The battery pack according to the second embodiment includes the battery according to the first embodiment. The number of batteries (single cells) included in the battery pack can be set to one or more.
[0142] A plurality of batteries may be electrically connected in series, in parallel, or in a combination of series and parallel to form a battery pack. A battery pack may also include a plurality of battery packs.
[0143] The battery pack may further include a protection circuit. The protection circuit has a function of controlling the charge and discharge of the battery. In addition, as the protection circuit of the battery pack, a circuit included in a device (such as an electronic device, a car, etc.) that uses the battery pack as a power source can also be used.
[0144] In addition, the battery pack may further include external terminals for power supply. The external terminals for power supply are used to output current from the battery to the outside and input current into the battery. In other words, when the battery pack is used as a power source, the current is supplied to the outside through the external terminals for power supply. In addition, when the battery pack is charged, the charging current (including the regenerative energy of the vehicle power) is supplied to the battery pack through the external terminals for power supply.
[0145] Next, an example of a battery pack according to a second embodiment will be described with reference to the drawings.
[0146] Figure 7 This is a block diagram showing an example of a circuit of a battery pack according to an embodiment. Figure 7 The battery pack shown includes a plurality of flat batteries 20 .
[0147] A plurality of cells 20 are stacked in such a manner that the negative and positive external terminals extending outward are all aligned in the same direction and are fastened with adhesive tape to form a battery pack. Figure 7 As shown, they are electrically connected in series with each other.
[0148] The printed circuit wiring substrate is arranged opposite to the side surfaces from which the negative and positive external terminals of the plurality of battery cells 20 extend. Figure 7 As shown, the printed wiring board is equipped with a thermistor 251, a protection circuit 261, and a terminal 271 for supplying power to an external device. In addition, an insulating plate (not shown) is mounted on the surface of the printed wiring board facing the battery pack to avoid unnecessary connection with the wiring of the battery pack.
[0149] The positive electrode side lead 281 is connected to the positive electrode external terminal of the single cell 20 located at the bottom layer of the battery assembly, and its front end is inserted into the positive electrode side connector 29 of the printed circuit wiring board to make an electrical connection. The negative electrode side lead 301 is connected to the negative electrode external terminal of the single cell 20 located at the top layer of the battery assembly, and its front end is inserted into the negative electrode side connector 31 of the printed circuit wiring board to make an electrical connection. These connectors 29 and 31 are connected to the protection circuit 261 through wirings 32 and 33 formed on the printed circuit wiring board, respectively.
[0150] The thermistor 251 detects the temperature of each single cell 20 and sends its detection signal to the protection circuit 261. Under specified conditions, the protection circuit 261 can cut off the positive side wiring 34a and the negative side wiring 34b between the protection circuit 261 and the terminal 271 for powering the external device. An example of a specified condition is when a signal is received from the thermistor 251 that the temperature of the single cell 20 is above a specified temperature. In addition, other examples of specified conditions are when overcharging, overdischarging, overcurrent, etc. of the single cell 20 are detected. The detection of overcharging, etc. is performed on each single cell 20 or all the single cells 20. When detecting each single cell 20, the battery voltage can be detected, and the positive electrode potential or the negative electrode potential can also be detected. In the latter case, a lithium electrode used as a reference electrode is inserted into each single cell 20. Figure 7 In the battery pack, wirings 35 for voltage detection are connected to the single cells 20 , respectively, and detection signals are sent to the protection circuit 261 through these wirings 35 .
[0151] Figure 7 The battery pack shown has a form in which a plurality of cells 20 are connected in series, but the battery pack according to the second embodiment may also be connected in parallel to increase the battery capacity. Alternatively, the battery pack according to the second embodiment may also include a plurality of cells 20 connected in a combination of series connection and parallel connection. The assembled battery pack may also be connected in series or in parallel.
[0152] also, Figure 7 The battery pack shown includes a plurality of cells 20 , but the battery pack according to the second embodiment may include a single cell 20 .
[0153] In addition, the form of the battery pack can be appropriately changed according to the purpose. As the purpose of the battery pack, it is preferably expected to be used for the cycle characteristics under the large current characteristics. Specifically, it can be listed as a power supply for a digital camera, a two-wheeled to four-wheeled hybrid electric vehicle, a two-wheeled to four-wheeled electric vehicle, a power-assisted bicycle, etc. It is particularly suitable for vehicle use.
[0154] In a vehicle equipped with the battery pack according to the present embodiment, the battery pack can recover, for example, regenerative energy of the vehicle's power.
[0155] The battery pack of the second embodiment described in detail above includes the battery of the first embodiment. Therefore, the battery pack according to the second embodiment can achieve excellent life performance.
[0156] Example
[0157] Hereinafter, examples will be described.
[0158] <Example 1>
[0159] [Production of positive electrode]
[0160] As a positive electrode active material, lithium nickel cobalt manganese composite oxide LiNi 0.33 Co 0.33 Mn 0.33 O2. A positive electrode active material, acetylene black, graphite and polyvinylidene fluoride are mixed in a mass ratio of 100:2:3:3 to obtain a mixture. The mixture is mixed with N-methyl-2-pyrrolidone, kneaded and stirred with a planetary mixer to prepare a positive electrode slurry. The positive electrode slurry is applied to both main surfaces of an aluminum foil having a thickness of 12 μm in such a manner that a local uncoated portion can be formed, and the coating is dried. The dried coating is compressed by roller pressing to prepare a positive electrode.
[0161] [Production of negative electrode]
[0162] As the negative electrode active material, lithium titanate Li4Ti5O 12 . A negative electrode active material, graphite and polyvinylidene fluoride are mixed in a mass ratio of 100:10:5 to obtain a mixture. The mixture is mixed with N-methyl-2-pyrrolidone, kneaded and stirred with a planetary mixer to prepare a negative electrode slurry. The negative electrode slurry is applied to both main surfaces of an aluminum foil having a thickness of 12 μm in such a manner that a local uncoated portion can be formed, and the coating is dried. The dried coating is compressed by roller pressing to prepare a negative electrode.
[0163] [Production of electrode group]
[0164] The negative electrode, the first separator, the positive electrode and the second separator are stacked in this order to obtain a stack. As the first and second separators, a cellulose nonwoven fabric with a thickness of 14 μm is used. The porosity of the first and second separators is 60%. Then, the stack is moved into a winding device and wound into a spiral shape. Then, the wound stack is subjected to a pressurization treatment to obtain a flat electrode group.
[0165] [Preparation of liquid non-aqueous electrolyte]
[0166] Ethylene carbonate and dimethyl carbonate were mixed at a volume ratio of 1:1 to prepare a non-aqueous solvent. Lithium hexafluorophosphate LiPF6 as an electrolyte was dissolved in the non-aqueous solvent to a concentration of 1 mol / L. In this way, a liquid non-aqueous electrolyte was prepared.
[0167] [Battery Assembly]
[0168] Prepare a sealing plate having a positive lead electrically connected to the positive terminal and a negative lead electrically connected to the negative terminal. The uncoated portion of the positive electrode disposed at the end of one side of the electrode group is joined to the positive lead by ultrasound. In addition, the uncoated portion of the negative electrode disposed at the end of the other side of the electrode group is joined to the negative lead by ultrasound. In this way, a sealing plate is installed on the electrode group. Next, the electrode group is inserted into an outer packaging container, and the sealing plate and the outer packaging can are welded. Next, a liquid non-aqueous electrolyte is injected into the outer packaging container from the injection port provided on the sealing plate. Then, an aluminum sealing member is embedded in the injection port, and the surrounding of the sealing member is welded to the sealing body. In this way, a battery is obtained.
[0169] <Examples 2 to 12 and Comparative Examples 1 to 3>
[0170] The batteries of Examples 2 to 12 and Comparative Examples 1 to 3 were obtained by the same method as described in Example 1, except that the type of positive electrode active material, the type of negative electrode active material, the density of the layer containing the positive electrode active material, the thickness of the positive electrode, the thickness of the negative electrode, the thickness of the separator, the size of the outer packaging member, the size of the electrode group, etc. were changed as shown in Tables 1 to 3 below.
[0171] <Evaluation Test>
[0172] [Cycle test]
[0173] First, at 25°C, charge the battery with a constant current at a rate of 0.05C to the maximum operating voltage. Next, while maintaining the maximum operating voltage, charge the battery further until the current value reaches 0.01C. Then, discharge the battery at a rate of 0.05C to the termination voltage to obtain the discharge capacity. The discharge capacity obtained at this time is referred to as the nominal capacity A. The charge and discharge of the battery is regarded as one cycle, and 1000 cycles are performed at 55°C. The discharge capacity of the battery after 1000 cycles is measured as the discharge capacity A1. The ratio of the discharge capacity A1 to the nominal capacity A is calculated as the capacity retention rate.
[0174] Furthermore, the maximum operating voltage of the batteries involved in Examples 1 to 8, 12 and Comparative Examples 1 to 3 was 2.8 V, and the end voltage was 1.3 V. In addition, the maximum operating voltage of the batteries involved in Examples 9 and 10 was 2.9 V, and the end voltage was 1.5 V. In addition, the maximum operating voltage of the battery involved in Example 11 was 3.1 V, and the end voltage was 1.5 V.
[0175] Next, the thickness T of the outer packaging member after the cycle test was measured. C1 As a result, the thickness T of the outer packaging member after the cycle test C1The results were substantially the same in Examples 1 to 12 and Comparative Examples 1 to 3. This indicates that gas was generated inside the outer casing member in all batteries through the cycle test.
[0176] Table 3 shows their results.
[0177] The data on the positive electrode, negative electrode and separator are compiled in Table 1 below.
[0178]
[0179] The data for the electrode sets are compiled in Table 2 below.
[0180]
[0181] The data on the batteries are summarized in the following Table 3. In Examples 1 to 12 and Comparative Examples 1 to 3 in Table 3, the relative area S is the area containing the positive electrode active material layer.
[0182]
[0183] It is clear from Tables 2 and 3 that the thickness of the electrode T E and the thickness T of the electrode group W The product of the innermost height H of the electrode group IC The ratio (T E ×T W ) / H IC The capacity retention rate of the batteries according to Examples 1 to 12, which is 0.02 or more and 0.04 or less, is higher than that of the batteries according to (T E ×T W ) / H IC The capacity maintenance rates of the batteries according to Comparative Examples 1 to 3 were less than 0.02.
[0184] In addition, as is clear from the comparison between Example 1 and Example 2, in both the positive electrode and the negative electrode, a high capacity retention rate is achieved regardless of whether the positive electrode is thick or the negative electrode is thick.
[0185] In addition, it is clear from the comparison of Examples 1, 2, 9 and 12 that a high capacity retention rate is achieved even when the types of negative electrode active materials are different. In addition, it is clear from the comparison of Example 9 and Example 1 that a high capacity retention rate is achieved even when the types of positive electrode active materials are different.
[0186] The battery according to the above-described embodiment has a relatively thin electrode having a thickness of 0.08 mm or less. E and the thickness T of the electrode group W The product of the innermost height H of the electrode group IC The ratio (T E×T W ) / H IC By setting the ratio to be greater than 0.02 and less than 0.04, even if the electrode is relatively thin, it is difficult for the electrode to be twisted. Thus, the battery according to the embodiment can achieve excellent life performance. In addition, the battery according to the embodiment can also achieve both excellent life performance and excellent input and output performance.
[0187] Several embodiments of the present invention have been described, but these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other ways, and various omissions, substitutions, and changes can be made without departing from the scope of the subject matter of the invention. These embodiments and their variations are included in the scope and subject matter of the invention, and are also included in the invention described in the claims and their equivalents.
Claims
1. A battery comprising: An outer packaging container comprises a bottom wall and a side wall extending from the bottom wall in a first direction, and is provided with an opening portion facing the bottom wall. An electrode group comprising a positive electrode, a negative electrode and an insulating layer, wherein the positive electrode and the negative electrode are wound into a flat shape with the insulating layer interposed therebetween, and the electrode group is housed in the outer packaging container in such a manner that the winding axis direction is orthogonal to the first direction, and a sealing plate mounted on the opening of the outer packaging container; The thickness T of the positive electrode PE and the thickness T of the negative electrode NE The thicknesses T of these electrodes are equal to or different from each other. E is 0.03 mm or more and 0.08 mm or less, When a direction parallel to the winding axis direction is defined as a second direction and a direction perpendicular to the first direction and the second direction is defined as a third direction, The thickness T of the electrode E , the thickness T of the electrode group in a direction parallel to the third direction W , the innermost height H of the electrode group in a direction parallel to the first direction IC Satisfying the following formula (1), the thickness T E , the thickness T W and the innermost height H IC The unit is mm, The thickness T of the electrode E is the thickness T of the positive electrode PE and the thickness T of the negative electrode NE The thickness of the thicker side is the thickness of the positive electrode T PE and the thickness of the negative electrode T NE When the electrode thickness T is the same value, E is the thickness of either side, The innermost circumference height H IC is the distance between a straight line passing through point P1 and parallel to the third direction, and a straight line passing through point P2 and parallel to the third direction, point P1 and point P2 being located at positions farthest from each other along the first direction on the innermost peripheral surface of the electrode group, 0.02≤(T E ×T W ) / H IC ≤0.04 (1)。 2. The battery according to claim 1, wherein The negative electrode contains a lithium-titanium composite oxide.
3. The battery according to claim 1 or 2, wherein: The height H of the electrode group in a direction parallel to the first direction W and the thickness T of the electrode E Satisfying the following formula (2), the height H W The unit is mm, 800≤H W / T E ≤1500 (2)。 4. The battery according to claim 1 or 2, wherein The positive electrode includes a positive electrode current collector and a positive electrode active material-containing layer provided on at least one of the positive electrode current collectors and containing a positive electrode active material. The negative electrode includes a negative electrode current collector and a negative electrode active material-containing layer provided on at least one side of the negative electrode current collector and containing a negative electrode active material. The width of the positive electrode active material layer in the direction parallel to the second direction and the width of the negative electrode active material layer in the direction parallel to the second direction are equal to or different from each other, and at least one of the widths is set as the coating width W of the electrode group. W hour, The coating width W of the electrode group W and the thickness T of the electrode E Satisfying the following formula (3), the width W W The unit is mm, 1600≤W W / T E ≤2500 (3)。 5. The battery according to claim 1 or 2, wherein The thickness T of the electrode E and the thickness T of the electrode group W Satisfies the following formula (4): 250≤T W / T E ≤450 (4)。 6. The battery according to claim 1 or 2, wherein: The thickness T of the electrode group W and the innermost height H of the electrode group IC Satisfies the following formula (5): 1.8≤H IC / T W ≤3.2 (5)。 7. The battery according to claim 1 or 2, wherein: The positive electrode includes a positive electrode current collector and a positive electrode active material-containing layer provided on at least one of the positive electrode current collectors and containing a positive electrode active material. The density of the positive electrode active material layer is 2.7 g / cm 3 Above and 3.3g / cm 3 the following.
8. The battery according to claim 1 or 2, wherein: The insulating layer is a separator having a thickness of 6 μm or more and 15 μm or less.
9. The battery according to claim 4, wherein The area of the positive electrode active material containing layer and the area of the negative electrode active material containing layer are equal to or different from each other, and when the area of at least one of them is taken as the relative area S, The relative area S and the nominal capacity A of the battery satisfy the following formula (6), and the unit of the relative area S is m 2 , the unit of the nominal capacity A is Ah, 3.5≤A / S≤10 (6).
10. The battery according to claim 1 or 2, wherein The outer packaging container includes a pair of long side walls and a pair of short side walls as the side walls, wherein the long side walls are side walls extending from the long sides of the bottom wall toward the first direction, and the short side walls are side walls extending from the short sides of the bottom wall toward the first direction. The thickness of the long-side side wall is greater than or equal to 0.3 mm and less than or equal to 0.7 mm.
11. The battery according to claim 1 or 2, wherein: In the outer packaging container to which the sealing plate is attached, the thickness T of the outer packaging container in the direction parallel to the third direction is C and the height H of the outer packaging container in a direction parallel to the first direction. C Satisfying the following formula (7), the thickness T C and the height H C The unit is mm, 2.5≤H C / T C ≤3.5 (7)。 12. The battery according to claim 1 or 2, wherein: In the outer packaging container to which the sealing plate is attached, the width W of the outer packaging container in the direction parallel to the second direction is C and the thickness T of the outer packaging container in the direction parallel to the third direction. C Satisfying the following formula (8), the width W C The unit is mm, 4.5≤W C / T C ≤6.5 (8)。 13. The battery according to claim 1 or 2, wherein: The nominal capacity is 4Ah or more. 14 . A battery pack comprising the battery according to claim 1 .