Probe device and precooling method of probe card

By using dry air purging and temperature adjustment technology in the probe device, the problem of condensation during the pre-cooling process of the probe card is solved, and efficient detection in high or low temperature environments is achieved.

CN112394207BActive Publication Date: 2024-10-29TOKYO ELECTRON LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202010781653.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-08-06
Publication Date
2024-10-29
Estimated Expiration
2040-08-06

AI Technical Summary

Technical Problem

When performing wafer inspection, especially in high or low temperature environments, condensation may easily occur during the pre-cooling process of the probe card, affecting detection efficiency and accuracy.

Method used

A probe device is designed, including multiple inspection chambers, probe cards, probe card holding parts, chuck tops, sealing mechanisms, temperature adjustment parts and supply parts. Without placing the wafer, a sealed space is formed and pre-cooled through dry air purging and temperature adjustment to suppress condensation.

Benefits of technology

It effectively suppresses the occurrence of condensation and realizes pre-cooling of the probe card, ensuring detection efficiency and accuracy in high or low temperature environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112394207B_ABST
    Figure CN112394207B_ABST
Patent Text Reader

Abstract

The present invention provides a probe device and a precooling method for a probe card. The probe device has a plurality of inspection chambers, each of which includes a probe card, a probe card holding component, a chuck top, a sealing mechanism, a temperature regulating unit, and a supply unit. The probe card has a plurality of probes. The probe card holding component holds the probe card. The top of the chuck can hold a wafer. The sealing mechanism forms a closed space between the probe card holding component and the top of the chuck. The temperature regulating unit regulates the temperature of the top of the chuck. The supply unit supplies dry gas to the closed space. When no wafer is placed on the top of the chuck, the probe device purges the closed space with dry air, and then uses the cold energy of the top of the chuck whose temperature is regulated by the temperature regulating unit to precool the probe card. The present invention can suppress condensation and precool the probe card.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a probe device and a precooling method of a probe card. Background Art

[0002] As an example of an inspection device for inspecting a wafer formed with a large number of semiconductor devices, a probe device can be cited. The probe device includes a probe card having probes as a plurality of columnar contact terminals. In the probe device, the wafer is abutted against the probe card so that each probe contacts an electrode pad or a solder bump in the semiconductor device. In the probe device, the probe contacts an electrode pad or a solder bump. In the probe device, the conduction state of the circuit is detected by causing electricity to flow from each probe device to a circuit of a semiconductor device connected to each electrode pad or each solder bump.

[0003] Prior art literature

[0004] Patent Literature

[0005] Patent Document 1: Japanese Patent Application Publication No. 2018-049989 Summary of the invention

[0006] Technical problem to be solved by the invention

[0007] The present invention provides a probe device and a probe card precooling method capable of suppressing condensation and precooling a probe card.

[0008] Technical solutions for solving technical problems

[0009] A probe device according to one embodiment of the present invention is a probe device having a plurality of inspection chambers, each of which includes a probe card, a probe card holding component, a chuck top, a sealing mechanism, a temperature regulating unit, and a supply unit. The probe card has a plurality of probes. The probe card holding component holds the probe card. The chuck top can hold a wafer. The sealing mechanism forms a closed space between the probe card holding component and the chuck top. The temperature regulating unit regulates the temperature of the chuck top. The supply unit supplies dry gas to the closed space. When no wafer is placed on the chuck top, the probe device purges the closed space with dry air, and then pre-cools the probe card using the cold energy of the chuck top whose temperature is regulated by the temperature regulating unit.

[0010] Effects of the Invention

[0011] According to the present invention, it is possible to suppress the occurrence of condensation and perform pre-cooling of the probe card BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 This is a diagram showing an example of a probe device according to an embodiment of the present invention.

[0013] Figure 2 is along Figure 1 Cross-sectional view along line II-II in FIG.

[0014] Figure 3 This is a diagram showing an example of the structure of the probe device in a state where no wafer is placed on the top of the chuck according to the present embodiment.

[0015] Figure 4 This is a diagram showing an example of the structure of the probe device in a state where a wafer is placed on the top of the chuck according to the present embodiment.

[0016] Figure 5 This is a diagram showing an example of the configuration of the probe device in a state where the closed space S is purged before the probe card is transported according to the present embodiment.

[0017] Figure 6 This is a diagram showing an example of the configuration of the probe device in the present embodiment in a state where a closed space S in which a probe card is vacuum-adsorbed is purged.

[0018] Figure 7 This is a flowchart showing an example of a pre-cooling method of the probe card according to the present embodiment.

[0019] Figure 8 It is a diagram showing an example of the structure of the gap adjustment member.

[0020] Fig. 9 It is a diagram showing an example of the structure of the gap adjustment member.

[0021] Fig.10 It is a diagram showing an example of the structure of the gap adjustment member.

[0022] Fig.11 It is a diagram showing an example of a cross section of the structure of the gap adjustment member.

[0023] Fig.12 It is a diagram showing an example of a cross section of the structure of the gap adjustment member.

[0024] Description of Reference Numerals

[0025] 10 Probe device

[0026] 12a Examination Room

[0027] 12b Supply Department

[0028] 15 Tester

[0029] 18 Conveying device

[0030] 19 Probe Card

[0031] 20 Elastic Frame

[0032] 25 Probe

[0033] 29 Chuck Top

[0034] 32 Alignment

[0035] 33 Sealing mechanism

[0036] 70 Gap adjustment parts

[0037] S Confined Space

[0038] W chip. DETAILED DESCRIPTION

[0039] Embodiments of the probe device and the precooling method of the probe card of the present invention will be described in detail below with reference to the accompanying drawings. The technology of the present invention is not limited to the following embodiments.

[0040] In recent years, in order to improve the inspection efficiency of wafers, a probe device including multiple inspection chambers has been developed, which can detect semiconductor devices of wafers in other inspection chambers while the wafer is being transported to one inspection chamber by a transport device. In this probe device, when the wafer is brought into contact with the probe card, the wafer is placed on the top of the chuck, and the space between the probe card and the top of the chuck is evacuated to make the wafer abut against the probe card. Here, when the wafer is brought into contact with the probe card, the top of the chuck is placed on a stage, and the stage moves the top of the chuck toward the probe card. Subsequently, the top of the chuck is adsorbed to the probe card and separated from the stage.

[0041] However, in recent years, the inspection conditions for wafer inspection have become complicated, especially when inspections are often performed in high-temperature or low-temperature environments. Among them, a technology has been proposed that, in an inspection in a low-temperature environment, dry air is introduced into the space in order to prevent condensation when the vacuumed space is pressurized after the inspection. However, condensation may also occur in addition to the case of pressurizing the vacuumed space. For example, before inspecting the wafer, condensation may sometimes occur when the probe card is pre-cooled to the temperature at which the inspection is performed. In addition, pre-cooling in this embodiment refers to cooling to a temperature lower than room temperature (for example, -30°C to -10°C). The pre-cooling of the probe card is performed, for example, using radiant heat (coldness) from the top of the chuck that has been cooled to a low temperature, so condensation may sometimes occur on the top of the chuck, surrounding components, etc. For example, when the probe card is transported from outside the low dew point space, the probe card contains humid air, so condensation may sometimes occur when pre-cooling is performed as it is. Therefore, it is desired to suppress condensation and pre-cool the probe card.

[0042] [Structure of the probe device]

[0043] Figure 1: is a diagram showing an example of a probe device in one embodiment of the present invention. Figure 2 is along Figure 1 Cross-sectional view along line II-II in FIG. Figure 1 and Figure 2 The probe device 10 shown includes: an inspection area 12 for inspecting the electrical characteristics of each semiconductor device of a wafer W; a storage area 13 for storing the wafer W; and a transfer area 14 provided between the inspection area 12 and the storage area 13 .

[0044] In the inspection area 12, a plurality of testers 15 are arranged as interfaces for wafer inspection, and a plurality of inspection chambers 12a corresponding to the respective testers 15 are provided. Specifically, the inspection area 12 has a three-layer structure of a tester column composed of a plurality of testers arranged horizontally, and a tester-side camera 16 is arranged corresponding to each tester column. Each tester-side camera 16 moves horizontally along the corresponding tester column and is located in front of each tester 15, and can confirm the position of the wafer W and the like and the degree of inclination of the chuck top 29. In addition, a supply unit 12b for supplying a dry gas to the chuck top 29 described later is provided in each inspection chamber 12a. The supply unit 12b supplies, for example, dry air as a dry gas.

[0045] The loading and unloading area 13 is divided into a plurality of storage spaces 17. Ports 17a, aligners 17b, loaders 17c, and controllers 17d are arranged in each storage space 17. Port 17a receives a container, i.e., a FOUP, which stores a plurality of wafers. Aligner 17b performs wafer position alignment. In loader 17c, probe cards 19 are loaded and unloaded. Controller 17d controls the operation of each component.

[0046] The transport area 14 is provided with a transport device 18 that can move to the inspection area 12 and the carrying-in / carrying-out area 13. The transport device 18 receives the wafer W from the port 17a and transports it to each inspection chamber 12a, and also transports the wafer W after the electrical characteristic inspection of the semiconductor device is completed from each inspection chamber 12a to the port 17a.

[0047] While the transfer device 18 is transferring one wafer W between one inspection chamber 12a and the port 17a, other inspection chambers 12a can perform electrical characteristic inspections on semiconductor devices of other wafers W, thereby improving wafer inspection efficiency.

[0048] Figure 3 1 is a diagram showing an example of the structure of the probe device in the present embodiment in a state where no wafer is placed on the top of the chuck. Figure 3 1 shows a state where the wafer W is not placed in order to pre-cool the probe card 19. Figure 3The state in which the chuck top 29 is brought into contact with the gap adjustment member 70 provided on the probe card 19 is shown, and the structure of the inspection chamber 12a is mainly shown in a cross-sectional view. Figure 4 1 is a diagram showing an example of the structure of a probe device in a state where a wafer is placed on the top of a chuck according to the present embodiment. Figure 4 The state in which the wafer W is brought into contact with the probe card 19 is shown, and the structure of the inspection chamber 12 a is mainly shown in a cross-sectional view.

[0049] exist Figure 3 and Figure 4 In the embodiment, the tester 15 is installed on a pogo frame 20 fixed to a device frame (not shown). A probe card 19 is mounted on the lower part of the pogo frame 20. A flange 22 is arranged so as to surround the probe card 19.

[0050] The probe card 19 includes: a disk-shaped body 24; a large number of electrodes (not shown) arranged on substantially one surface of the upper surface of the body 24; and a large number of probes 25 arranged so as to protrude downward from the lower surface of the body 24. Each electrode is connected to a corresponding probe 25. When the wafer W abuts against the probe card 19, each probe 25 contacts the electrode pads and solder bumps of each semiconductor device formed on the wafer W.

[0051] In addition, the probe card 19 has a gap adjustment member 70, which maintains a constant gap between the probe card 19 and the chuck top 29 when the wafer W is not placed on the chuck top 29. The gap adjustment member 70 is, for example, in the form of a pin, and is made of stainless steel, aluminum, or copper, and three or more gap adjustment members are provided on the lower surface of the probe card 19. In addition, the gap adjustment member 70 may be, for example, a resin such as PEEK (Poly Ether Ether Ketone), other materials, or alloys. The length of the gap adjustment member 70 is longer than the probe 25 and shorter than the gap from the lower surface of the main body 24 of the probe card 19 to the upper surface of the chuck top 29, wherein the gap is the gap from the lower surface of the main body 24 of the probe card 19 to the upper surface of the chuck top 29 when the wafer W is placed on the chuck top 29 and the wafer W is in contact with the probe 25.

[0052] That is, Figure 3 As shown in FIG. 1 , the gap adjustment member 70 abuts against the chuck top 29 when no wafer W is mounted. Figure 4As shown, the gap adjusting member 70 is in a state where a gap is left between the chuck top 29 and the chuck top 29 when the wafer W is placed on the chuck top 29. In other words, the probe 25 does not contact the chuck top 29 when the wafer W is not placed on the chuck top 29, and the probe 25 contacts the wafer W when the wafer W is placed on the chuck top 29. Alternatively, the gap adjusting member 70 may be provided on the chuck top 29 side.

[0053] The elastic frame 20 has a main body 26 that is roughly flat and an elastic block insertion hole 27. The elastic block insertion hole 27 is a plurality of through holes that are provided through the main body 26 near the center portion. An elastic block (pogo block) 28 formed by arranging a plurality of elastic pins can be inserted into each elastic block insertion hole 27. The elastic block 28 is connected to an inspection circuit (not shown) of the tester 15 and contacts a large number of electrodes on the upper surface of the main body 24 in the probe card 19 installed in the elastic frame 20. The elastic block 28 allows current to flow to each probe 25 of the probe card 19 connected to the electrode, and allows current flowing from the circuit of each semiconductor device of the wafer W through each probe 25 to flow to the inspection circuit.

[0054] The flange 22 has an upper flange 22a and a lower flange 22b. In addition, the flange 22 has a cylindrical bellows 23 between the upper flange 22a and the lower flange 22b. The upper flange 22a is engaged with the elastic frame 20 and sealed using a packing. The lower flange 22b can move in the vertical direction relative to the elastic frame 20.

[0055] The lower flange 22b moves downward due to its own weight so that the lower surface of the lower flange 22b is located below the front end of each probe 25 of the probe card 19 until it contacts the chuck top 29. The bellows 23 is a metal corrugated structure that can be extended and retracted in the vertical direction. The lower end and the upper end of the bellows 23 are respectively in close contact with the upper surface of the lower flange 22b and the lower surface of the upper flange 22a.

[0056] The space between the elastic frame 20 and the base 21 of the tester 15 is sealed by the sealing member 30, and the base 21 is mounted to the elastic frame 20 by evacuating the space. The space between the elastic frame 20 and the probe card 19 is sealed by the sealing member 31, and the probe card 19 is mounted to the elastic frame 20 by evacuating the space.

[0057] The conveying device 18 has an aligner 32. The chuck top 29 can be placed on the aligner 32, and the wafer W can be placed on the upper surface of the chuck top 29. Figure 3In the figure, the wafer W is not placed, and the placement position is indicated by a dotted line. The chuck top 29 can be vacuum-adsorbed on the aligner 32, and the wafer W can be vacuum-adsorbed on the chuck top 29. Therefore, it is possible to prevent the wafer W from moving relative to the conveying device 18 when the conveying device 18 moves. In addition, the method of holding the chuck top 29 and the wafer W is not limited to vacuum adsorption, as long as it is a method that can prevent the chuck top 29 and the wafer W from moving relative to the aligner 32, for example, electromagnetic adsorption and holding by a clamp can be used. In addition, a height difference portion 29a is formed on the peripheral portion of the upper surface of the chuck top 29, and a sealing mechanism 33 is arranged on the height difference portion 29a.

[0058] The sealing mechanism 33 is adsorbed to the lower flange 22b by evacuating the closed space 33a in the sealing mechanism 33 formed when the sealing mechanism 33 abuts against the lower surface of the lower flange 22b. That is, the chuck top 29 is held on the flange 22 by the sealing mechanism 33, thereby forming a closed space S between the elastic frame 20 or the probe card 19 and the chuck top 29.

[0059] In addition, a flow path 50 and a heater 51 are provided inside the chuck top 29. A refrigerant is supplied to the flow path 50 from a cooling unit (not shown). The refrigerant supplied to the flow path 50 flows through the flow path 50 and then returns to the cooling unit. The heater 51 is connected to a heater power source (not shown), and power is supplied to the heater 51, thereby heating the chuck top 29. The temperature of the chuck top 29 is adjusted by cooling by the refrigerant circulating in the flow path 50 and heating by the heater 51.

[0060] The conveyor 18 can move toward the bottom of the probe card 19 in the inspection chamber 12a so that the wafer W placed on the chuck top 29 faces the probe card 19, and can move toward the probe card 19. The closed space S is formed when the gap adjustment member 70 abuts against the placement surface of the chuck top 29 ( Figure 3 ), or when the chuck top 29 abuts against the lower flange 22b and the wafer W abuts against the probe card 19 ( Figure 4 ) formed. In addition, the enclosed space S is before the probe card described later is transported ( Figure 5 ), or after the probe card 19 is vacuum-adsorbed onto the elastic frame 20 ( Figure 6 ) is the space formed when the chuck top 29 abuts against the lower flange 22b.

[0061] In the closed space S, the closed space S is evacuated via the vacuum passage 26a, thereby holding the chuck top 29 on the probe card 19 side. In addition, the method of holding the chuck top 29 is not limited to vacuum adsorption, as long as it is a method that can form the closed space S, for example, it can be electromagnetic adsorption and holding by a clamp. In addition, in the closed space S, before the chuck top 29 is held on the probe card 19 side by vacuum adsorption via the vacuum passage 26a, dry air is supplied to the closed space S via the dry air passage 29b. By releasing the supplied dry air from the vacuum passage 26a, the humid air in the closed space S can be purged. In addition, the movement of the conveying device 18 is controlled by the controller 17d, and the controller 17d grasps the position and movement amount of the conveying device 18.

[0062] The aligner 32 adjusts the relative position and inclination of the chuck top 29 with respect to the probe card 19. The temperature adjustment parts such as the flow path 50 and the heater 51 realize the inspection in a high temperature environment or a low temperature environment. Therefore, in the inspection in a high temperature environment or a low temperature environment, the aligner 32 can adjust the position change and inclination caused by the deformation of the probe card 19 and the chuck top 29 caused by the heat dissipation from the heater 51 or the heat absorption to the flow path 50. In addition, as an example of the temperature range of the chuck top 29, a range of 130°C to -30°C can be cited.

[0063] The aligner 32 has a base and a guide rail corresponding to each direction of X, Y, and Z. Each base can move along each guide. A chuck base in the shape of a roughly circular plate is provided in the Z portion provided on the Z base. The chuck base has a chuck top adsorption surface on the upper surface, and the chuck top 29 is vacuum adsorbed on the chuck top adsorption surface. Thus, the chuck top 29 can be placed and mounted on the aligner 32. At this time, the position of the chuck top 29 relative to the chuck base is specified using a positioning pin or a positioning block.

[0064] Furthermore, the aligner 32 has an upper confirmation camera for confirming the degree of inclination of the probe card 19 and the elastic frame 20. Furthermore, in the aligner 32, the inclination of the mounted chuck top 29 can be adjusted by moving the chuck base using an actuator.

[0065] [Purge of confined space S]

[0066] Next, use Figure 5 and Figure 6 , the purging of the confined space S is described. Figure 5 1 is a diagram showing an example of the structure of the probe device in the present embodiment in which the closed space S is purged before the probe card is transported. Figure 5 The diagram shows a state after maintenance or the like but before the probe card 19 is transported and no wafer W is placed on the chuck top 29 , and mainly shows the structure of the inspection chamber 12 a in a cross-sectional view.

[0067] exist Figure 5 In the state shown, the chuck top 29 rises to the position where the sealing mechanism 33 abuts against the lower flange 22b, and then the closed space 33a is evacuated to form a closed space S. That is, the chuck top 29 is not vacuum-adsorbed on the elastic frame 20 side in the closed space S, but the closed space S is sealed by the sealing mechanism 33. In this state, the closed space S is purged with dry air supplied via the dry air passage 29b. That is, in a state where the elastic frame 20, which is a probe card holding component, does not hold the probe card 19, the closed space S is formed by the sealing mechanism 33, and the formed closed space S is purged with dry air. In addition, the flow rate of the dry air is, for example, about 2L / minute. As a result, it is possible to purge the humid air in the closed space S after maintenance, etc.

[0068] Figure 6 1 is a diagram showing an example of the structure of the probe device in the present embodiment in a state of purging the closed space S in which the probe card is vacuum-adsorbed. Figure 6 The state after the probe card 19 is vacuum-adsorbed and before the chuck top 29 on which the wafer W is not mounted is vacuum-adsorbed is shown, and the structure of the inspection chamber 12a is mainly shown in a cross-sectional view.

[0069] exist Figure 6 In the state shown, Figure 5 Similarly, the chuck top 29 rises to a position where the sealing mechanism 33 contacts the lower flange 22b, and then the closed space 33a is evacuated to form a closed space S. That is, the chuck top 29 is not vacuum-adsorbed on the probe card 19 side in the closed space S, but the closed space S is sealed by the sealing mechanism 33. In this state, the closed space S is purged with dry air supplied through the dry air passage 29b. Figure 5 The closed space S is temporarily opened to transport the probe card 19 to the lower part of the elastic frame 20, and the elastic frame 20 holds the probe card 19. Next, the chuck top 29 without the wafer W is transported to the lower part of the probe card 19, and the chuck top 29 is raised again to the position where the sealing mechanism 33 abuts against the lower flange 22b, and then the closed space 33a is evacuated to form the closed space S. At this time, the gap adjustment component 70 is not in abutment with the chuck top 29. Thereafter, the closed space S is purged with dry air. In this way, the moisture inside the probe card 19 can also be removed.

[0070] [Probe card pre-cooling method]

[0071] Next, a method for precooling the probe card according to the present embodiment will be described. Figure 7This is a flowchart showing an example of a pre-cooling method of the probe card according to the present embodiment.

[0072] First, before transporting the probe card 19, the chuck top 29 is transported to the inspection chamber 12a where the probe card is precooled using the transport device 18. At this time, the chuck top 29 is in a state where no wafer is placed. The chuck top 29 is transported to the lower part of the elastic frame 20 using the transport device 18. The chuck top 29 is raised to a position where the sealing mechanism 33 contacts the lower flange 22b using the transport device 18, and the sealed space 33a in the sealing mechanism 33 contacting the lower flange 22b is evacuated, thereby forming a sealed space S (see FIG. 2 ). Figure 5 At this time, the chuck top 29 is held by the sealing mechanism 33 on the flange 22, and the closed space S is sealed by the sealing mechanism 33. In this state, the closed space S is purged with dry air supplied through the dry air passage 29b (step S1).

[0073] The transport device 18 is withdrawn from the inspection room 12a, and the cooling unit and the heater power supply (not shown) connected to the flow path 50 and the heater 51 are controlled to start temperature control so that the chuck top 29 has the same temperature as that during pre-cooling. That is, the chuck top 29 is pre-cooled before the probe card 19 is transported (step S2). In addition, the radiant heat (coldness) from the chuck top 29 is also used to cool other components such as the elastic frame 20.

[0074] Next, the probe card 19 is transported from the loader 17c to the inspection chamber 12a where the probe card is to be pre-cooled using the transport device 18. The probe card 19 is vacuum-adsorbed from the transport device 18 to the elastic frame 20 (step S3).

[0075] The chuck top 29 is transported to the probe card 19 to be pre-cooled by the transport device 18. At this time, the chuck top 29 is in a state where no wafer is placed. The chuck top 29 is transported to the lower part of the probe card 19 by the transport device 18. The chuck top 29 is raised by the transport device 18 to a position where the sealing mechanism 33 contacts the lower flange 22b, and the sealed space 33a in the sealing mechanism 33 contacting the lower flange 22b is evacuated, thereby forming a sealed space S (see FIG. 1 ). Figure 6 ). At this time, the sealed space S is in a state of being sealed by the sealing mechanism 33. In this state, the sealed space S is purged with dry air supplied through the dry air passage 29b (step S4).

[0076] After the sealed space S is purged, the chuck top 29 is further raised and abutted against the gap adjustment member 70 of the probe card 19. Then, the chuck top 29 is vacuum-adsorbed on the probe card 19 side (step S5). At this time, the gap between the chuck top 29 and the probe card 19 is kept constant by the gap adjustment member 70 (see FIG. 1 ). Figure 3 ).

[0077] The transport device 18 is withdrawn from the inspection room 12a, and a cooling unit and a heater power supply (not shown) connected to the flow path 50 and the heater 51 are controlled to start pre-cooling of the probe card (step S6).

[0078] When the pre-cooling of the probe card is completed, the chuck top 29 is transported from the inspection chamber 12a by the transport device 18, and the wafer W is placed on the chuck top 29. The chuck top 29 on which the wafer W is placed is transported to the inspection chamber 12a, and the wafer W and the chuck top 29 are vacuum-adsorbed on the elastic frame 20 (step S7). The wafer W is inspected (step S8), and after the inspection is completed, the wafer W is transported to, for example, the port 17a by the transport device 18.

[0079] As described above, it is possible to suppress the occurrence of condensation and pre-cool the probe card 19. In addition, it is possible to keep the distance between the probe card 19 and the chuck top 29 constant and pre-cool the probe card 19. In addition, since the distance between the probe card 19 and the chuck top 29 is kept constant, the pre-cooling of the probe card can be performed with a stable pre-cooling time in any inspection chamber 12a.

[0080] [Modification of the gap adjustment member]

[0081] Next, a modification of the gap adjusting member 70 will be described. Figures 8 to 10 It is a diagram showing an example of the structure of the gap adjustment member. Fig.11 and Fig.12 1 is a diagram showing an example of a cross section of the structure of the gap adjustment member. Figures 8 to 10 As shown in FIG. 1 , the gap adjustment members 70 a to 70 c are arranged from the lower surface of the main body 24 of the probe card 19 toward the front side in the figure. Fig.11 and Fig.12 In the cross section of the probe card 19 shown, the gap adjustment members 70 a to 70 c are arranged from the lower surface of the main body 24 to the lower side in the figure. Figure 8 The gap adjustment member 70 a shown is an example of a case where it is arranged in a circular ring shape on the outer peripheral side of the probe card 19 . Fig. 9 The gap adjusting members 70 b shown in the figure are an example in which three arc-shaped gap adjusting members 70 b are arranged on the outer peripheral side of the probe card 19 . Fig.10The gap adjusting members 70 c shown in the figure are an example in which two linear gap adjusting members 70 c are arranged at positions symmetrical with respect to the center line of the probe card 19 .

[0082] Fig.11 The cross section of the gap adjustment component has a straight line shape. Fig.12 The cross section of the gap adjustment member is shown to have an inverted T-shape. In addition, the gap adjustment member 70 is not limited to the gap adjustment members 70a to 70c as a modified example, and other shapes and arrangements are also possible.

[0083] As described above, according to the present embodiment, the probe device 10 is a probe device having a plurality of inspection chambers 12a, each of which includes a probe card 19, an elastic frame 20 as a probe card holding member, a chuck top 29, a sealing mechanism 33, a temperature regulating unit, and a supply unit 12b. The probe card 19 has a plurality of probes 25. The elastic frame 20 holds the probe card 19. The chuck top 29 can carry a wafer W. The sealing mechanism 33 forms a closed space S between the elastic frame 20 and the chuck top 29. The temperature regulating unit regulates the temperature of the chuck top 29. The supply unit 12b supplies dry gas to the closed space S. In a state where the chuck top 29 does not carry a wafer W, the probe device 10 purges the closed space S with dry gas, and then precools the probe card 19 using the coldness of the chuck top 29 whose temperature is regulated by the temperature regulating unit. As a result, it is possible to suppress the occurrence of condensation and precool the probe card.

[0084] In addition, according to the present embodiment, at least one of the probe card 19 and the chuck top 29 has a gap adjustment component 70 capable of maintaining a constant interval between the probe card 19 and the chuck top 29. One end of the gap adjustment component 70 is provided on at least one of the probe card 19 and the chuck top 29, and the other end is located on the side of the other of the probe card 19 and the chuck top 29. The probe device 10 purges the enclosed space with the dry gas in a state where the other end of the gap adjustment component 70 does not contact the other of the probe card 19 and the chuck top 29. Thereafter, the probe device 10 moves the chuck top 29 closer to the probe card 19 side, and performs pre-cooling in a state where the other end of the gap adjustment component 70 contacts the other of the probe card 19 and the chuck top 29. As a result, the interval between the probe card 19 and the chuck top 29 can be maintained constant, and the probe card 19 can be pre-cooled.

[0085] In addition, according to the present embodiment, the length of the gap adjustment member 70 is longer than the probe 25 and shorter than the distance between the probe card 19 and the chuck top 29, which is the distance between the probe card 19 and the chuck top 29 when the probe 25 contacts the wafer W when the wafer W is placed on the chuck top 29. As a result, the distance between the probe card 19 and the chuck top 29 can be kept constant, and the probe card 19 can be pre-cooled.

[0086] According to the present embodiment, the gap adjusting member 70 is pin-shaped, annular, arc-shaped, or linear. As a result, the gap between the probe card 19 and the chuck top 29 can be kept constant.

[0087] The embodiments disclosed in the present invention are illustrative in all aspects and should not be considered restrictive. The above embodiments may be omitted, replaced, and changed in various ways without departing from the scope and concept of the appended claims.

[0088] In addition, in the above-mentioned embodiment, dry air is supplied from the dry air passage 29b and released from the vacuum passage 26a, but the present invention is not limited thereto. For example, the dry air passage 29b may not be provided and the dry air may be supplied and released from the vacuum passage 26a. In addition, for example, the vacuum passage 26a may be provided on the chuck top 29 side.

Claims

1. A probe device having multiple inspection chambers, characterized in that: Each of the plurality of examination rooms comprises: a probe card having a plurality of probes; a probe card holding member for holding the probe card; A chuck top capable of holding a wafer; a sealing mechanism for forming a closed space between the probe card holding member and the top of the chuck; A temperature regulating unit for regulating the temperature of the top of the chuck; and a supply unit for supplying dry gas to the enclosed space, At least one of the probe card and the chuck top has a gap adjustment component capable of maintaining a certain interval between the probe card and the chuck top, one end of the gap adjustment component is arranged on at least one of the probe card and the chuck top, and the other end is located on a side of the other of the probe card and the chuck top. The length of the gap adjustment member is longer than the probe and shorter than the distance between the probe card and the top of the chuck, wherein the distance between the probe card and the top of the chuck is the distance between the probe card and the top of the chuck when the probe contacts the wafer when a wafer is placed on the top of the chuck. In a state where no chip is placed on the top of the chuck and the other end of the gap adjustment component does not contact the other of the probe card and the top of the chuck, the enclosed space is purged with the dry gas, and then the top of the chuck is moved closer to the probe card side so that the other end of the gap adjustment component contacts the other of the probe card and the top of the chuck, and the probe card is pre-cooled using the cold energy of the top of the chuck whose temperature is regulated by the temperature regulating unit.

2. The probe device according to claim 1, characterized in that: The gap adjustment component is pin-shaped, ring-shaped, arc-shaped or straight-line-shaped.

3. A method for precooling a probe card in a probe device for wafer inspection, characterized in that: The probe device comprises: A chuck top capable of holding a wafer; The probe card is formed with probes capable of contacting a wafer; a probe card holding member that holds the probe card; and a sealing mechanism for forming a closed space between the probe card holding member and the top of the chuck, At least one of the probe card and the chuck top has a gap adjustment component capable of maintaining a certain interval between the probe card and the chuck top, one end of the gap adjustment component is arranged on at least one of the probe card and the chuck top, and the other end is located on a side of the other of the probe card and the chuck top. The length of the gap adjustment member is longer than the probe and shorter than the distance between the probe card and the top of the chuck, wherein the distance between the probe card and the top of the chuck is the distance between the probe card and the top of the chuck when the probe contacts the wafer when a wafer is placed on the top of the chuck. The pre-cooling method of the probe card comprises: The step of conveying the top of the chuck without a wafer mounted thereon to the bottom of the probe card; The step of forming the closed space between the probe card holding member and the top of the chuck by the sealing mechanism; The step of purging the sealed space with dry gas in a state where no wafer is placed on the chuck top and the other end of the gap adjustment member does not contact the other of the probe card and the chuck top; and After the enclosed space is purged with the dry gas, the top of the chuck is moved closer to the probe card so that the other end of the gap adjustment component contacts the other of the probe card and the top of the chuck, and the probe card is pre-cooled using the cold energy of the top of the chuck.

4. The method for precooling a probe card according to claim 3, wherein: Also includes: A step of purging the sealed space with the dry gas in a state where the probe card holding member does not hold the probe card; and a step of opening the sealed space to convey the probe card to the lower part of the probe card holding member and holding the probe card in the probe card holding member, In the process of conveying, after the probe card is held by the probe card holding member, the chuck top is conveyed to the lower part of the probe card.

Citation Information

Patent Citations

  • Substrate inspection device

    JP2018049989A

  • Substrate inspection device

    CN109716147A

  • Inspecting device for semiconductor wafer

    JP2000294606A

  • Semiconductor wafer testing method, semiconductor wafer test device, and wafer tray

    JP2013219299A