A kind of synthetic method of phosphoric acid ester

Through solvent-free method and intelligent feeding box technology, the addition rate and heat emission of phosphorus pentoxide are controlled, and the unstable and color problems of mono-dial ester ratio in phosphate synthesis are solved, and efficient and stable phosphate synthesis is achieved, which is suitable for industrialization. Production.

CN112409403BActive Publication Date: 2024-11-26成都科宏达化学有限责任公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011168044.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-10-28
Publication Date
2024-11-26
Estimated Expiration
2040-10-28

AI Technical Summary

Technical Problem

In the existing phosphate synthesis methods, the unstable feeding of phosphorus pentoxide leads to a large difference in the proportion of mono-dial ester, which affects the product quality and color. The existing technology will affect the performance of phosphate esters when solving the problem by adding solvents.

Method used

The solvent-free method is used to synthesize phosphate esters, and the addition rate and amount of phosphorus pentoxide are controlled by setting reaction conditions and intelligent feeding tanks, and combined with the heat discharge of the circulating pump, the reaction stability and product quality are ensured.

Benefits of technology

It has achieved high esterification rate, colorless transparent products, stability and green environmental protection technology of phosphate esters, and can control the proportion of single and double esters, which is suitable for industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112409403B_ABST
    Figure CN112409403B_ABST
Patent Text Reader

Abstract

The invention discloses a method for synthesizing phosphate, comprising the steps of: (1) adding an organic alcohol to a reactor; (2) adding phosphorus pentoxide to a charging box in proportion, setting the charging box rotation speed, and controlling the addition time of phosphorus pentoxide for 1-3h; opening a circulating pump during the feeding process to control the circulating liquid speed; the surface layer of the charging box is provided with a plurality of small holes, and phosphorus pentoxide overflows from the small holes through the rotation of the box body into the reactor to react with the organic alcohol; (3) after the phosphorus pentoxide is fed, the reactor temperature is raised to 70-90°C, and the reaction is continued for 5-7h to obtain a phosphate product. The present invention adopts a solvent-free method to prepare phosphate, by controlling the feeding mode of phosphorus pentoxide, setting a material circulation device at the same time, ensuring the addition amount and quality of phosphorus pentoxide, timely discharging the heat generated by the reaction, ensuring the stability of the reaction, making the prepared phosphate product stable, the esterification rate is high, and the system is colorless and transparent, without decolorization, and the product does not contain any decolorizing agent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of chemical synthesis, in particular to a method for synthesizing phosphate ester. Background Art

[0002] As an important type of surfactant, phosphate esters are widely used in chemical fiber, textile, leather, plastic, papermaking, printing and dyeing, metal processing and daily chemicals. They are used as detergents, oils, antistatic agents, emulsifiers, liquid ion exchangers and pharmaceuticals.

[0003] At present, the preparation of phosphate esters is usually prepared by reacting alcohols with phosphorylation reagents. The phosphorylation reagents reported so far include phosphorus trichloride, phosphorus pentoxide, etc. Among them, phosphorus pentoxide is reported the most and is the most commonly used, because the phosphorus pentoxide method is simple and easy to operate, and the yield of phosphate ester is high. Since phosphorus pentoxide is a strong oxidant and a strong dehydrating agent, it is easy to produce different degrees of color changes during the reaction process, and it is easy to undergo polymerization to form polyphosphoric acid byproducts during the reaction, thereby affecting the use effect of the product; at the same time, since most of the existing phosphorus pentoxide additions are manually added in steps, and since the reaction of organic alcohols with phosphorus pentoxide is an acylation exothermic reaction, the amount of phosphorus pentoxide added each time cannot be guaranteed, resulting in a large difference in the ratio of monoesters and diesters of phosphate esters synthesized in different batches, poor reproducibility, and unstable product quality.

[0004] In order to improve the color and poor reproducibility of phosphate products, most of the existing technologies use a method of adding solvents. For example, Patent Publication No. CN1068599C discloses a method for synthesizing colorless fatty alcohol polyoxyethylene ether phosphate, which uses fatty alcohol polyoxyethylene ether as a raw material, adds phosphorus pentoxide to carry out an esterification reaction, and synthesizes colorless phosphate by adding water before the esterification reaction; however, adding water to the reaction system will increase the phosphoric acid content in the reaction product, affecting the performance and use of the phosphate; therefore, it is urgently needed to develop a method for synthesizing colorless phosphate suitable for industrial production and with a controllable ratio of monoesters and diesters. Summary of the invention

[0005] The purpose of the present invention is to solve the problems existing in the prior art and provide a method for synthesizing phosphate ester, which adopts a solvent-free method to synthesize colorless phosphate ester, has the characteristics of mild reaction conditions, stable product quality, high esterification rate, green environmental protection, etc., and can control the content of monoester and diester in phosphate ester by setting the reaction conditions.

[0006] In order to solve the above problems, the present invention provides the following technical solutions:

[0007] A method for synthesizing a phosphate ester comprises the following steps:

[0008] (1) Adding organic alcohol into a reactor; setting the temperature of the reactor to 40-60° C.;

[0009] (2) adding phosphorus pentoxide to a feeding box in proportion, setting the rotation speed of the feeding box, and controlling the addition time of phosphorus pentoxide to 1-3 hours; starting a circulation pump during the addition of phosphorus pentoxide to control the circulation liquid speed; the surface layer of the feeding box is provided with a plurality of small holes, and the phosphorus pentoxide overflows from the small holes into the reactor through the rotation of the box body to react with the organic alcohol;

[0010] (3) After the addition of phosphorus pentoxide in step (2) is completed, the temperature of the reactor is raised to 70-90° C. and the reaction is continued for 5-7 hours to obtain a phosphate ester product.

[0011] Preferably, the organic alcohol in step (1) is fatty alcohol (ROH), fatty alcohol polyoxyethylene ether (RO(C2H4O) m H), alkanolamide (RCONHCH2CH2OH), alkylphenol polyoxyethylene ether (C 35-36 H 64-66 O 10-21 ), any one of the organic fluorine alcohols, wherein R is C n H 2n-1 , n=8-22, m=2-20.

[0012] Preferably, the mass ratio of phosphorus pentoxide to organic alcohol in step (2) is 0.25-0.7:1.25-3.

[0013] Preferably, the feeding box in step (2) is provided with an intelligent display screen for setting the rotation speed of the feeding box and controlling the amount of phosphorus pentoxide added to the reactor per unit time; at the same time, the amount of phosphorus pentoxide added each time is ensured, the stability of the reaction is ensured, and the product quality is more balanced.

[0014] Preferably, the rotation speed of the feeding box is 12-32 r / s. At this rotation speed, the amount of phosphorus pentoxide added to the reactor per unit time can be controlled, thereby ensuring the stability of the reaction and making the product quality more balanced.

[0015] Preferably, the circulation rate of the circulating liquid in step (2) is 4-10 ml / s. By setting a circulating pump outside the reactor and circulating the circulating liquid (mixed liquid of organic alcohol and phosphorus pentoxide) externally, the heat generated in the reaction can be removed in time after the circulating liquid contacts the outer circulation tube, thereby avoiding the problem that a large amount of heat generated by the reaction of organic alcohol and phosphorus pentoxide cannot be released, causing carbonization of the organic alcohol carbon chain and deepening of the product color.

[0016] Preferably, the aperture of the small hole in step (2) is 5-10 mm; the small hole is arranged in the feeding box, so that the phosphorus pentoxide solid powder can be more easily overflowed from the feeder, while some larger impurity particles are difficult to overflow from the box and cannot enter the reactor, thereby ensuring the quality of the added reaction materials.

[0017] Another object of the present invention is to provide a device for phosphate synthesis reaction, comprising a reactor, a feeding bin, and a material circulation system, wherein a nitrogen inlet and a nitrogen outlet are respectively provided on both sides of the top of the reactor, a stirring device is provided inside the reactor, the upper end of the reactor is connected to the feeding bin, a rotary feeding box is provided in the feeding bin, and a rubber sealing layer is provided between the rotary feeding box and the feeding bin; a plurality of small holes are provided on the rotary feeding box; the rotary feeding box is connected to a feeding motor, and the feeding motor is externally connected to a feeding intelligent display screen; the material circulation system comprises a circulation pipeline, a circulation pump, and a circulation intelligent display screen, the material circulation system is connected to the reactor through a circulation pipeline, a No. 1 circulation feed valve, a No. 2 circulation feed valve, a circulation pump, and a circulation discharge valve are sequentially provided on the circulation pipeline, and the circulation pump is externally connected to a circulation intelligent display screen.

[0018] The working principle of the device of the present invention is as follows: adding organic alcohol to a reactor, starting a stirring device, opening a nitrogen inlet and a nitrogen outlet at the same time, raising the temperature of the reactor to 40-60 DEG C, adding measured phosphorus pentoxide to a rotary feeding box, setting the rotation speed of the rotary feeding box through an intelligent display screen, and controlling the amount of phosphorus pentoxide added to the reactor per unit time; during the rotation of the feeding box, the phosphorus pentoxide overflows from a small hole through the rotation of the feeding box body and enters the reactor; during the feeding process, opening a No. 1 circulation feeding valve, a No. 2 circulation feeding valve, and a circulation discharging valve, and simultaneously starting a circulation pump, and controlling the amount of external circulation of the circulating liquid through the circulation intelligent display screen; after the addition of the phosphorus pentoxide is completed, raising the temperature of the reactor to 70-90 DEG C, continuing the reaction for 5-7 hours, and discharging after the reaction is completed.

[0019] Compared with the prior art, the present invention has the following beneficial effects:

[0020] (1) The present invention adopts a solvent-free method to prepare phosphate ester. No solvent is added during the entire reaction process. By controlling the feeding method of phosphorus pentoxide and setting a material circulation device, the amount and quality of phosphorus pentoxide added are guaranteed, the heat generated by the reaction is discharged in time, and the stability of the reaction is guaranteed. The prepared phosphate ester product is stable and has a high esterification rate. The system is colorless and transparent, no decolorization is required, and the product does not contain any decolorizing agent.

[0021] (2) The synthetic method of the phosphate ester of the present invention can achieve controllable ratio of the red monoester and diester of the phosphate ester product by controlling the raw material ratio and experimental reaction conditions, which is of great significance to actual production.

[0022] (3) The synthetic method of the phosphate ester of the present invention is green and environmentally friendly from raw materials to products, and no three wastes are generated, which meets the requirements of green technology.

[0023] (4) The phosphate synthesis method of the present invention has simple process, mild conditions, strong operability, and is suitable for industrial production. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 The figure is a schematic diagram of the structure of the device for the phosphate synthesis reaction of the present invention.

[0025] In the above drawings, the component names corresponding to the reference numerals are as follows:

[0026] 1-reactor; 2-nitrogen inlet; 3-stirring device; 4-nitrogen outlet; 5-small hole; 6-rotating feeding box; 7-rubber sealing layer; 8-feeding intelligent display screen; 9-feeding motor; 10-circulation pump; 11-circulation intelligent display screen; 12-No. 1 circulation material valve; 13-No. 2 circulation feed valve; 14-circulation discharge valve; 15-material discharge valve; 16-feeding bin. DETAILED DESCRIPTION

[0027] In order to make the purpose, technical solutions and advantages of the present invention clearer, the present invention is further described in detail with reference to the accompanying drawings below. The described embodiments should not be regarded as limiting the present invention. All other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0028] Example 1

[0029] A method for synthesizing phosphate esters comprises the following steps: 15 kg of fatty alcohol polyoxyethylene ether (C 12 H 25 (OC2H4)2OH) is added to the reactor, 2.7kg P2O5 is added to the feeding box, the reactor temperature is set to 40°C, the feeding box rotation speed is set to 25r / s through the intelligent display screen 7, and the addition is completed in 2 hours. During the P2O5 addition process, the circulation pump is started at the same time, and the speed of the circulating liquid external circulation is controlled by the intelligent display screen 11 to be 8ml / s. After the P2O5 is added, the reactor temperature is raised to 70°C, the reaction is continued for 6h, and the reaction is terminated to obtain colorless and transparent phosphate.

[0030] QB / T 2949-2008 phosphate was used to determine the content of phosphate active matter, and the potentiometric titration method in Song Minggui's "Synthesis of Fatty Alcohol Phosphate Polyoxyethylene Ether" was used to detect the content of monoester and diester phosphate in phosphate. The test showed that the content of phosphate active matter was 97.7%, of which the content of monoester phosphate was 31.2% and the content of diester phosphate was 61.5%. The obtained phosphate product was a colorless and transparent solution.

[0031] Example 2

[0032] A method for synthesizing phosphate esters comprises the following steps: 6.25 kg of fatty alcohol polyoxyethylene ether (C 12 H 25 (OC2H4)2OH) is added to the reactor, 1.25kg P2O5 is added to the feeding box, the reactor temperature is set to 50°C, the feeding box rotation speed is set to 12r / s through the intelligent display 7, and the addition is completed in 2 hours. During the P2O5 addition process, the circulation pump is started at the same time, and the speed of the circulating liquid external circulation is controlled by the intelligent display 11 to be 4ml / s. After the P2O5 is added, the reactor temperature is raised to 80°C, the reaction is continued for 5h, and the reaction is terminated to obtain colorless phosphate.

[0033] After testing, the content of active matter in the obtained phosphate ester was 98.2%, of which the content of monophosphate ester was 33.4% and the content of diester phosphate was 62.7%. The obtained phosphate ester product was a colorless transparent solution.

[0034] Example 3

[0035] A method for synthesizing phosphate esters comprises the following steps: 10 kg of tristyrylphenol polyoxyethylene ether (C 50 H 82 O 17 ) is added to the reactor, 2kg P2O5 is added to the feeding box, the temperature of the reactor is set to 55°C, the rotation speed of the feeding box is set to 18r / s through the intelligent display screen 7, and the addition is completed in 2 hours. During the P2O5 addition process, the circulation pump is started at the same time, and the speed of the circulating liquid external circulation is controlled by the intelligent display screen 11 to be 6ml / s. After the P2O5 is added, the temperature of the reactor is raised to 85°C, and the reaction is continued for 7h. The reaction is terminated to obtain a light yellow phosphate ester.

[0036] After testing, the content of active matter in the obtained phosphate ester was 83.2%, of which the content of monophosphate ester was 27.4%, and the content of diester phosphate was 52.1%. The obtained phosphate ester product was a light yellow solution.

[0037] Example 4

[0038] A method for synthesizing phosphate esters comprises the following steps: 15 kg of perfluorohexylethyl alcohol (C8H5F 13 O) add to the reactor, add 2kg P2O5 into the feeding box, set the reactor temperature to 45°C, set the feeding box rotation speed to 18r / s through the intelligent display screen 7, and add it in 2 hours. During the P2O5 addition process, start the circulation pump at the same time, and control the speed of the circulating liquid external circulation to 6ml / s by the intelligent display screen 11. After the P2O5 is added, the reactor temperature is raised to 85°C, and the reaction is continued for 7h. The reaction is terminated to obtain a colorless and transparent phosphate.

[0039] After testing, the content of active matter in the obtained phosphate ester was 90.3%, of which the content of monophosphate ester was 30.6%, and the content of diester phosphate was 53.6%. The obtained phosphate ester product was a colorless transparent solution.

[0040] Example 5

[0041] A method for synthesizing a phosphate ester comprises the following steps: 12 kg of dodecanol (C8H5F 13 O) add to the reactor, add 3.5kg P2O5 into the feeding box, set the reactor temperature to 60°C, set the feeding box rotation speed to 32r / s through the intelligent display screen 7, and add it in 2 hours. During the P2O5 addition process, start the circulation pump at the same time, and control the speed of the circulating liquid external circulation at 10ml / s by the intelligent display screen 11. After the P2O5 is added, the reactor temperature is raised to 90°C, and the reaction is continued for 7h. The reaction is terminated to obtain a colorless and transparent phosphate.

[0042] After testing, the content of active matter in the obtained phosphate ester was 98.2%, of which the content of monophosphate ester was 32.8%, and the content of diester phosphate was 63.7%. The obtained phosphate ester product was a colorless transparent solution.

[0043] Comparative Example 1

[0044] A method for synthesizing phosphate esters comprises the following steps: 15 kg of fatty alcohol polyoxyethylene ether (C 12 H 25 (OC2H4)OH) was added into the reactor, and 2.7 kg of P2O5 was added manually in steps. The temperature of the reactor was set to 40°C and the addition was completed in 2 hours. After the addition of P2O5 was completed, the temperature of the reactor was raised to 70°C and the reaction was continued for 6 hours. The reaction was terminated to obtain a dark yellow phosphate ester.

[0045] After testing, the content of active matter of phosphate ester was 82.2%, that of monophosphate ester was 28.2%, that of diester phosphate was 48.1%, and the product was a dark yellow solution.

[0046] Comparative Example 2

[0047] A method for synthesizing phosphate esters comprises the following steps: 15 kg of fatty alcohol polyoxyethylene ether (C 12 H 25 (OC2H4)OH) was added into the reactor, 2.7 kg P2O5 was added manually in steps, the reactor temperature was set to 40°C, the feed box rotation speed was set to 25 r / s through the intelligent display 7, the addition was completed in 2 hours, the reactor temperature was raised to 80°C, the reaction was continued for 6 hours, and the reaction was terminated to obtain a dark yellow phosphate ester.

[0048] After testing, the content of active matter in the obtained phosphate ester was 92.6%, of which the content of monophosphate ester was 32.2% and the content of diester phosphate was 55.2%. The obtained phosphate ester product was a light yellow solution.

[0049] Comparative Example 3

[0050] A method for synthesizing phosphate esters comprises the following steps: 10 kg of fatty alcohol polyoxyethylene ether (C 12 H 25 (OC2H4)OH) is added into the reactor, 3kg P2O5 is added into the screw feeder (product of Huabo Company), the temperature of the reactor is set at 40°C, and the addition is completed in 2 hours. During the addition of P2O5, the circulation pump is started at the same time, and the speed of the external circulation of the circulating liquid is controlled by the intelligent display screen 11 to be 8ml / s. After the addition of P2O5, the temperature of the reactor is raised to 70°C, and the reaction is continued for 6h. The reaction is terminated to obtain dark brown phosphate.

[0051] After testing, the content of active matter of phosphate ester was 66.1%, that of monophosphate ester was 25.2%, that of diester phosphate was 33.9%, and the product was a dark brown solution.

[0052] Comparative Example 4

[0053] A method for synthesizing phosphate esters comprises the following steps: 15 kg of fatty alcohol polyoxyethylene ether (C 12 H 25 (OC2H4)OH) is added to the reactor, and 2.7kg P2O5 is added manually step by step. The temperature of the reactor is set to 40°C and the addition is completed in 2 hours. During the addition of P2O5, the circulation pump is started at the same time, and the speed of the external circulation of the circulating liquid is controlled by the intelligent display screen 11 to be 8ml / s. After the addition of P2O5, the temperature of the reactor is raised to 70°C, and the reaction is continued for 6h. The reaction is terminated to obtain a dark yellow phosphate solution.

[0054] After testing, the active matter content of phosphate ester was 75.4%, the monoester of phosphate was 26.7%, the diester of phosphate was 44.7%, and the product was a dark yellow solution.

[0055] The above is only a preferred embodiment of the present invention. It should be understood that the present invention is not limited to the form disclosed herein, and should not be regarded as excluding other embodiments, but can be used in various other combinations, modifications and environments, and can be modified within the scope of the concept described herein through the above teachings or the technology or knowledge of the relevant field. Any modification, equivalent substitution, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for synthesizing a phosphoric acid ester, characterized in that: The steps include: (1) Adding organic alcohol into a reactor; setting the temperature of the reactor to 40-60° C.; (2) adding phosphorus pentoxide to the feeding box in proportion, setting the rotation speed of the feeding box, and controlling the addition time of phosphorus pentoxide to 1-3h; starting the circulation pump during the addition of phosphorus pentoxide to control the circulation liquid speed; the surface layer of the feeding box is provided with a plurality of small holes, and the phosphorus pentoxide overflows from the small holes through the rotation of the box body into the reactor to react with the organic alcohol; the feeding box is provided with an intelligent display screen for setting the rotation speed of the feeding box and controlling the amount of phosphorus pentoxide added to the reactor per unit time, and the rotation speed of the feeding box is 12-32r / s; (3) After the addition of phosphorus pentoxide in step (2) is completed, the temperature of the reactor is raised to 70-90° C. and the reaction is continued for 5-7 hours to obtain a phosphate ester product; The organic alcohol described in step (1) is any one of fatty alcohol, fatty alcohol polyoxyethylene ether, alkanolamide, alkylamide polyoxyethylene ether, organic silicon alcohol, and organic fluorine alcohol; the molecular formula of the fatty alcohol is ROH, and the molecular formula of the fatty alcohol polyoxyethylene ether is RO(C2H4O) m H, m = 2-20; the molecular formula of the alkanolamide is RCONHCH2CH2OH; wherein R in the molecular formula of the fatty alcohol, fatty alcohol polyoxyethylene ether, and alkanolamide is C n H 2n-1 , wherein n=8-22; the molecular formula of the alkylamide polyoxyethylene ether is C 35-36 H 64-66 O 10-21 ; The mass ratio of phosphorus pentoxide to organic alcohol in step (2) is 0.25-0.7:1.25-3.

2. The method for synthesizing phosphate ester according to claim 1, characterized in that: The circulation rate of the circulating fluid in step (2) is 4-10 ml / s.

3. The method for synthesizing phosphate ester according to claim 1, characterized in that: The diameter of the small hole in step (2) is 5-10 mm.