Energy storage device stacking

Through inkjet material deposition and laser ablation technology, the problem of low formation and processing efficiency of solid-state thin film battery stacking is solved, and the production and battery connection of high-efficiency energy storage devices are realized, reducing costs and improving battery performance.

CN112470304BActive Publication Date: 2024-11-26DYSON TECH LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980048217.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-07-20
Filing Date
2019-07-19
Publication Date
2024-11-26
Estimated Expiration
2039-07-19

AI Technical Summary

Technical Problem

The prior art energy storage device stack formation and processing for solid-state thin film batteries has low efficiency, resulting in difficulty in commercial application.

Method used

The first and second materials are deposited on the stack of energy storage devices using inkjet material deposition technology to form an effective electrode layer connection and laser ablation of exposed portions to achieve reliable battery connection, reducing material migration and improving deposition accuracy .

Benefits of technology

A flexible, effective and reliable production of energy storage devices is achieved, reducing production costs, and improving the parallel connection capability and discharge rate of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112470304B_ABST
    Figure CN112470304B_ABST
Patent Text Reader

Abstract

A method includes obtaining a stack for an energy storage device, the stack including a first electrode layer and an electrolyte layer. The method includes depositing a first material on an exposed portion of the first electrode layer and an exposed portion of the electrolyte layer. The method includes depositing a second material on the first material and forming a second electrode layer of the stack, and providing an electrical connection to the second electrode layer to connect to another such second electrode layer through the second material. The electrolyte layer is between the first electrode layer and the second electrode layer. The first material thereby insulates the exposed portion of the first electrode layer and the electrolyte layer from the second material. An apparatus for maintaining top-down inkjet material deposition is also disclosed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a stack for an energy storage device and more particularly, but not exclusively, to a method and apparatus for handling a stack for an energy storage device. Background Art

[0002] A known method for producing an energy storage device such as a solid-state thin-film battery comprising an electrode layer, an electrolyte layer and a current collector layer is to first form a stack comprising a first current collector layer, an electrode layer, an electrolyte layer, a second electrode layer and a second current collector layer formed on a substrate. The stack is then cut into individual parts to form individual cells. A protective layer may then be applied to each cell, for example, to prevent passivation of the layers and possible short circuits.

[0003] To make electrical connections with the cells, for example to electrically connect the current collectors of multiple cells stacked one on top of another, portions of the protective layer may be removed, for example by etching. Alternatively, a mask may be applied prior to the coating process to ensure that a portion of each current collector is exposed.

[0004] However, known formation and processing of stacks for energy storage devices such as solid-state thin film batteries can be inefficient, making efficient commercialization difficult. It is therefore desirable to provide efficient methods for forming and processing stacks for energy storage devices. Summary of the invention

[0005] According to a first aspect of the present invention, a method is provided, comprising: obtaining a stack for an energy storage device, the stack comprising a first electrode layer and an electrolyte layer; depositing a first material on an exposed portion of the first electrode layer and an exposed portion of the electrolyte layer; depositing a second material on the first material and forming a second electrode layer of the stack, and providing an electrical connection to the second electrode layer to connect to another such second electrode layer through the second material, wherein the electrolyte layer is located between the first electrode layer and the second electrode layer; whereby the first material insulates the exposed portions of the first electrode layer and the electrolyte layer from the second material.

[0006] Depositing the second material on the first material and forming and providing connections from the second electrode layer may allow efficient and / or reliable connection of parallel cells formed from the stack, and thus, for example, for efficient production of energy storage devices therefrom.

[0007] In an example, depositing the first material comprises inkjet material deposition of the first material. Depositing the first material by inkjet material deposition such as inkjet printing can allow for flexible, efficient and / or reliable deposition. For example, inkjet printing can be performed at relatively low (e.g., ambient) temperatures and / or pressures, e.g., compared to thermal spraying, and thus can allow for economical and / or efficient deposition and thus battery production.

[0008] In an example, the stack includes a substrate adjacent to one of the first electrode layer and the second electrode layer, wherein the other of the first electrode layer and the second electrode layer is an anode layer. Having the stack in this configuration can allow the anode material to be used as the second material, which can provide efficient energy storage device production.

[0009] In an example, the second material is an anode material for forming an anode layer. For example, the anode material can be relatively cheap. For example, the anode material can be cheap compared to conductive ink and / or to cathode material. Therefore, using the anode material to provide the anode layer with electrical connections to other such anode layers of other batteries can allow for reduced costs of battery production, and therefore can allow for more efficient battery production. As another example, deposition of the anode material can be relatively fast and / or cheap, for example, by flood deposition, for example, compared to inkjet printing.

[0010] In an example, the first electrode layer and the electrolyte layer are recessed from the substrate so that the substrate provides a ledge portion on which the first material and / or the second material is at least partially supported. Having a ledge portion can allow the first material and / or the second material to be supported during and / or after deposition, and / or can prevent or reduce undesirable migration of the first material and / or the second material, which in turn can facilitate accurate deposition of the first material and / or the second material.

[0011] In an example, another such second electrode layer belongs to another such stack. This may provide a parallel connection of the separate batteries formed by the stack. Connecting batteries in parallel may provide an energy storage device with a relatively large discharge rate, which may be useful in certain applications.

[0012] In an example, the stack includes the other second electrode layer, and another electrolyte layer between the other second electrode layer and the first electrode layer, wherein depositing the first material also includes depositing the first material on the exposed portion of the other electrolyte layer, wherein depositing the second material also includes depositing the second material to contact the other second electrode layer, thereby connecting the second electrode layer and the other second electrode layer via the second material, so that the first material further insulates the exposed portion of the other electrolyte layer from the second material. Such a stacking arrangement can provide layers constituting multiple batteries on one substrate. This may be an effective arrangement because it can reduce the amount of substrate, anode and / or cathode material required to form multiple batteries.

[0013] In an example, the electrolyte layer, the first electrode layer and the first further electrolyte layer are recessed from the further second electrode layer so that the further second electrode layer provides a ledge on which the first material and / or the second material is supported. Having a ledge portion may allow the first material and / or the second material to be supported during and / or after deposition, and / or may prevent or reduce undesired migration of the first material and / or the second material, which in turn may facilitate accurate deposition of the first material and / or the second material.

[0014] In an example, the method comprises laser ablating the stack, and exposing one or more of the exposed portions by laser ablating the stack. Laser ablation can provide an efficient, reliable, fast and effective way to expose portions of the stack to allow connection of cells formed therefrom, which in turn can provide efficient energy storage device production.

[0015] According to a second aspect of the present invention, a stack for an energy storage device is provided, the stack comprising a first electrode layer, a second electrode layer and an electrolyte layer between the first electrode layer and the second electrode layer, the stack comprising a first material on a portion of the first electrode layer and a portion of the electrolyte layer; a second material, which is on the first material and forms the second electrode layer and provides an electrical connection to the second electrode layer to be connected to another such second electrode layer through the second material, wherein the first material insulates the first electrode layer and portions of the electrolyte layer from the second material.

[0016] According to a third aspect of the present invention, there is provided an energy storage device formed by the method of the first aspect.

[0017] Also provided is an apparatus comprising: a first inkjet material deposition component arranged to deposit material on a first side of a stack for an energy storage device; a second inkjet material deposition component arranged to deposit material on a second side of the stack, the second side being opposite to the first side; and a plurality of rollers arranged to guide movement of the stack between the first inkjet material deposition component and the second inkjet material deposition component so that the first side of the stack is presented as a top-down inkjet material deposition for material from the first inkjet material deposition component to the stack, and so that the second side of the stack is presented as a top-down inkjet material deposition for material from the second inkjet material deposition component to the stack.

[0018] Performing inkjet material deposition from the top down, such as inkjet printing, can allow materials to be accurately and efficiently deposited onto the stack.Even in the case where the stack includes layers on both sides of the substrate, ensuring that both sides of the stack are presented as top-down printing can allow materials to be accurately and efficiently deposited onto the stack.

[0019] In an example, the apparatus is arranged to perform the method according to the first aspect.

[0020] Other features and advantages of the present invention will become apparent from the following description of preferred embodiments of the invention, given by way of example only, which description refers to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 is a schematic diagram showing a stack for an energy storage device according to an example;

[0022] Figure 2 is a diagram showing a method for processing according to an example Figure 1 A schematic diagram of a method of stacking to make an energy storage device;

[0023] Figure 3 is a flow chart illustrating a method of processing a stack according to an example;

[0024] Figure 4 and Figure 5 is a schematic diagram showing one way of processing a stack according to a first example;

[0025] Figure 6 and Figure 7 is a schematic diagram showing one way of processing a stack according to a second example; and

[0026] Figure 8 is a schematic diagram showing one way of implementing processing according to either of the first and second examples. DETAILED DESCRIPTION

[0027] Details of the methods, structures and devices according to the examples will become apparent with reference to the accompanying drawings, according to the examples. In this specification, many specific details of certain examples are set forth for the purpose of explanation. Reference to "example" or similar language in the specification means that a particular feature, structure or characteristic described in conjunction with the example is included in at least one example, but not necessarily in other examples. It should also be noted that certain examples are schematically described, in which certain features are omitted and / or must be simplified in order to facilitate explanation and understanding of the concepts underlying the examples.

[0028] Figure 1 A stack 100 of layers for an energy storage device is shown. For example, Figure 1 The stack 100 may be used as part of a thin film energy storage device having a solid electrolyte.

[0029] The stack 100 includes a substrate 102, a cathode layer 104, an electrolyte layer 106, and an anode layer 108. Figure 1In the example of FIG. 1 , the anode layer 108 is further away from the substrate 102 than the cathode layer 104, and the electrolyte layer 106 is located between the cathode layer 104 and the anode layer 108. The substrate 102 contacts the cathode layer 104 and supports the stack. Although in this example, the substrate 102 contacts the cathode layer 104, in other examples, there may be other layers (not shown) between the substrate 102 and the cathode layer 104.

[0030] In some examples, substrate 102 may be or may include nickel foil; however, it should be understood that any suitable metal may be used, such as aluminum, copper, or steel, or metallized materials including metallized plastics, such as aluminum on polyethylene terephthalate (PET). In some examples, substrate 102 may not be metallic and / or may not conduct electrical current. For example, in some examples, substrate may be polyethylene terephthalate (PET).

[0031] The cathode layer 104 may serve as a positive current collecting layer. The cathode layer 104 may form a positive electrode layer (i.e., corresponding to the cathode during discharge of a battery of an energy storage device including the stack 100). The cathode layer 104 may include a material suitable for storing lithium ions through a stable chemical reaction, such as lithium cobalt oxide, lithium iron phosphate, or an alkali metal polysulfide salt.

[0032] Anode layer 108 may serve as a negative current collecting layer. Anode layer 108 may form a negative electrode layer (ie, corresponding to the anode during discharge of a battery including an energy storage device of stack 100). Anode layer 108 may include lithium metal, graphite, silicon, or indium tin oxide.

[0033] In some examples, anode layer 108 may include a negative current collector and a separate negative electrode layer (not shown). In these examples, the negative electrode layer may include lithium metal, graphite, silicon, or indium tin oxide, and / or the negative current collector may include nickel foil. However, it should be understood that any suitable metal may be used, such as aluminum, copper, or steel, or metallized materials including metallized plastics, such as aluminum on polyethylene terephthalate (PET).

[0034] The electrolyte layer 106 may include any suitable material that is ionically conductive but is also an electrical insulator, such as lithium phosphorus oxynitride (LiPON). The electrolyte layer 106 may be a solid layer and may be referred to as a fast ion conductor. A solid electrolyte layer may have a structure between a liquid electrolyte and a crystalline solid, where a liquid electrolyte, for example, lacks a regular structure and contains ions that can move freely. Crystalline materials, for example, have a regular structure with an ordered arrangement of atoms that may be arranged in a two-dimensional or three-dimensional lattice. The ions of a crystalline material are generally immobile and therefore may not be able to move freely throughout the material.

[0035] For example, stack 100 may be fabricated by depositing cathode layer 104 on substrate 102. Electrolyte layer 106 is subsequently deposited on cathode layer 104, and then anode layer 108 is deposited on electrolyte layer 106. Each layer of stack 100 may be deposited by flooding, which provides a simple and efficient way to produce highly uniform layers, although other deposition methods are possible.

[0036] Figure 1 The stack 100 may be processed to fabricate an energy storage device.

[0037] exist Figure 2 The schematic diagram shows the Figure 1 A general overview of an example of a process of stacking 100 .

[0038] exist Figure 2 In the example, stack 100 is processed to make an energy storage device. In this example, stack 100 is flexible, allowing it to be wound around roll 112, for example as part of a roll-to-roll manufacturing process (sometimes referred to as a reel-to-reel manufacturing process). Stack 100 can be gradually unwound from roll 112 and processed.

[0039] exist Figure 2 In an example of FIG. 1 , a cut or groove may be formed in the stack 100 using the first laser 114. The first laser 114 is arranged to apply a laser beam 116 to the stack 100 to remove a portion of the stack 100 by laser ablation, thereby forming the cut or groove.

[0040] After forming the cutouts or grooves, an insulating material system 118 can be used to introduce an electrically insulating material into or into the region of at least some of the cutouts or grooves. An electrically insulating material can be considered to be non-conductive, so it can conduct a relatively small amount of current when subjected to an electric field. Typically, the current conducted by an electrically insulating material (sometimes referred to as an insulator) is less than that of a semiconductor material or a conductive material. However, there is still a small amount of current flowing through the electrically insulating material under the influence of an electric field, because even an insulator may include a small amount of charge carriers that carry the current. In the examples herein, the material can be considered to be electrically insulating, where the material is electrically insulating enough to perform the function of an insulator. For example, this function can be performed when the material fully insulates one element from another element to avoid a short circuit.

[0041] Reference Figure 2 After the electrical insulating material is introduced, the stack 110 is cut to form individual cells for an energy storage device. In some examples, hundreds or even thousands of cells may be cut from a roll of the stack 100, allowing multiple batteries to be manufactured in an efficient manner.

[0042] exist Figure 2In the embodiment, the cutting operation is performed using a second laser 122, which is arranged to apply a laser beam 124 to the stack 100. Each cut may, for example, pass through the center of the insulating plug so that the plug is divided into two parts, each part forming a protective covering on the exposed surface including the edge to which it has been attached.

[0043] Although not in Figure 2 , but it will be appreciated that after the insulating material is introduced (or otherwise), the stack may be folded back on itself to form a z-fold structure having, for example, tens, possibly hundreds, or even thousands of layers, with each insulating plug aligned. The laser cutting process performed by the second laser 122 may then be used to cut the z-fold structure for each of the aligned plug groups in a single cutting operation.

[0044] After cutting the battery, electrical connectors can be arranged along opposite sides of the battery so that a first electrical connector on one side of the battery contacts (multiple) cathode layers 104, but is prevented from contacting other layers by an electrically insulating material. Similarly, a second electrical connector on the opposite side of the battery can be arranged to contact (multiple) anode layers 108, but is prevented from contacting other layers by an insulating material. Thus, the insulating material can reduce the risk of short circuits between the anode and cathode layers 104, 108 and other layers in each battery. The first and second electrical connectors can, for example, comprise a metallic material applied to the edge of the stack 100. Thus, the batteries can be effectively connected in parallel.

[0045] The foregoing description provides a general overview of an example of a stack 100 for an energy storage device, and examples of processes that may be applied to the stack 100 (e.g., for manufacturing an energy storage device). The following description provides examples of processes for forming and / or processing a stack (which may be similar to those described above). Figure 1 Exemplary methods and apparatus for stack 100 (the same or similar to the described stack) may provide improvements in the formation and processing efficiency of stack 200, and therefore, for efficiently producing energy storage devices, such as batteries produced therefrom.

[0046] refer to Figure 3 , schematically illustrates a method of processing an energy storage device stack 200 according to an example.

[0047] In summary, the method includes obtaining a stack for an energy storage device in step 201, the stack including a first electrode layer and an electrolyte layer. The method further includes, in step 203, depositing a first material on an exposed portion (e.g., a surface) of the first electrode layer and an exposed portion (e.g., a surface) of the electrolyte layer. The method further includes, in step 205, depositing a second material on the first material and forming a second electrode layer of the stack to provide an electrical connection from the second electrode layer for connection to another such second electrode layer through the second material. The electrolyte layer is between the first electrode layer and the second electrode layer. The first material insulates the exposed portions (e.g., surfaces) of the first electrode layer and the electrolyte layer from the second material.

[0048] As explained in more detail below, the method may allow for an efficient and / or reliable parallel connection of batteries for an energy storage device and thus, for example, for an efficient production of an energy storage device.

[0049] Reference now Figure 4 and Figure 5 , schematically shows a stack 200 according to a first example (ie, it can be based on reference Figure 3 ) obtained by an example of step 201 of the described method.

[0050] Stack 200 can be compared with reference Figure 1 The stack 100 described is similar. However, Figure 4 The stack 200 does not yet include an anode layer. More specifically, Figure 4 In the example shown, the energy storage device stack 200 includes a substrate layer 202, a cathode layer 204, and an electrolyte layer 206 (but at this stage, there is no anode layer 208, but see Figure 5 anode layer 208).

[0051] exist Figure 4 and 5 In the example shown, the first electrode layer 204 is a cathode layer 204 and the second electrode layer 208 is an anode layer 208. The layers 202-208 of the stack 200 may be similar to those of the reference Figure 1 The layers of the stack 100 described are the same or similar. For example, the cathode layer 204 may include a cathode electrode and a cathode current collector ( Figure 4 ), and the anode layer 208 may include an anode electrode and an anode current collector ( Figure 4 (not shown). Figure 4 and 5In the example shown, the electrolyte layer 206 is between the cathode layer 204 and the anode layer 208 (once it is formed), the cathode layer 204 is adjacent to the substrate layer 202, the electrolyte layer 206 is adjacent to the cathode layer 204, and the anode layer 208 (once it is formed) is adjacent to the electrolyte layer 206. In this example, the substrate layer 202 is adjacent to the cathode layer 204 relative to the anode layer 208. In this example, the substrate layer 202 can be or include a non-conductive material such as polyethylene terephthalate (PET), although other materials can be used.

[0052] like Figure 4 As shown, the energy storage device stack 200 has a cutout 212 formed therein. The cutout 212 may be formed in the stack 200 by laser ablation (not shown). The cutout 212 is formed in a first side 200a of the stack 200 away from the base layer 202. Figure 4 As shown, cut 212 passes through each of electrolyte layer 206 and cathode layer 204, but not through substrate layer 202. Laser ablation to form the cuts may expose portions of substrate, cathode, and electrolyte layers 202, 204, 206, such as surfaces (e.g., edges) 273, 274, 276.

[0053] In some examples, and as Figure 4 and 5 As shown, the cutout 212 is defined only by exposed portions 274, 276 of the cathode and electrolyte layers 204, 206 (which in this example may also be considered as the sides of the cutout 212), and by exposed portions (e.g., ledge 273) of the substrate layer 202 (e.g., which in this example may also be considered as forming the base or bottom surface of the cutout 212). For example, the stack 200 may represent a segmented battery for an energy storage device, such as one that has been segmented from a larger stack structure (not shown). In these examples, Figure 4 and Figure 5 The portion of the stack 200 schematically shown in FIG. 1 may be the end of a terminal of a battery. In other words, in these examples, the stack 200 may be Figure 4 and Figure 5 It should be understood that in some examples, reference may be made to Figures 4 to 8 to describe the stacking of each example described in this article.

[0054] However, in other examples, the cutout 212 may be in the form of a groove. In the case where the cutout 212 is a groove, Figure 4 and 5It can be considered that only the left side of the groove is shown. As used herein, the term "groove" can refer to a channel, slot or groove that can be continuous or discontinuous, and in some examples can be elongated, and can only partially extend through the layers 202-206 of the stack 200. For example, the groove can be defined on a first side by exposed portions 274, 276 of the cathode and electrolyte layers 204, 206 (which can also be considered as the first side portion of the groove in this example), on a second side by an exposed ledge 273 of the substrate layer 202 (which can also be considered as the base surface or bottom surface forming the groove in this example), and on a third side (similar to the first side) by exposed portions, such as surfaces (not shown) of the cathode and electrolyte layers (not shown) of the stack 200 (which can also be considered as the second side portion of the groove in this example). One or more such grooves 212 can be formed to divide the stack 200 into partial battery structures, but without (at this stage) completely separating those individual battery structures. It should be understood that in some examples, reference can be made to Figures 4 to 8 to describe the stacking of each example described in this article.

[0055] In the example where the cutout 212 is a groove, the (or each) groove may have a depth extending into the stack 200 in a direction substantially perpendicular to the plane of the layers 202-206; a width substantially perpendicular to the depth (in Figure 4 In the sense that each groove has a width and depth in the plane of the page), and a length extending in a direction substantially parallel to the plane of the layers 202-208 and substantially perpendicular to the width (i.e., in the plane of the page). Figure 4 In the case of multiple first grooves, they can be substantially parallel to each other in depth and length. Therefore, it should be understood that although reference will be made to cutouts 212 below, in each of the examples described herein, cutouts 212 can take the form of grooves, and in some examples there can be multiple such grooves formed in stack 200.

[0056] In either case, due to the cutout 212, as Figure 4 As shown, the first electrode layer (cathode layer 204 in this example) and the electrolyte layer 206 are recessed from the substrate layer 202 such that the substrate layer 202 provides a ledge portion, such as a surface 273, on which, for example, the first material 210 and / or the second material 214 can be at least partially supported.

[0057] It should be noted that Figure 4 (similar to other figures) are schematic diagrams for illustration purposes only. For example, Figure 4 The sizes and relative spacing of the features (eg, layers 202 - 206 , cutouts 212 or recesses) shown in are merely schematic and are used only to illustrate the example structures and processes described herein.

[0058] As used herein, "laser ablation" may refer to the removal of material from stack 200 using a laser-based process. Such removal of material may include any of a number of physical processes. For example, the removal of material may include (but is not limited to) melting, melt expulsion, vaporization (or sublimation), photolysis (single photon), photolysis (multi-photon), mechanical shock, thermomechanical shock, other shock-based processes, surface plasma processing, and removal by evaporation (ablation).

[0059] Specific reference Figure 4 , depositing the first material 210 on the exposed portion of the first electrode layer (in this example, the cathode layer 202), such as the surface 274, and the exposed portion of the electrolyte layer 206, such as the surface 276 (according to reference Figure 3 203 of the method described above).

[0060] The first material 210 is an electrically insulating material. An electrically insulating material can be considered non-conductive and therefore can conduct a relatively small amount of current when subjected to an electric field. Typically, an electrically insulating material (sometimes referred to as an insulator) conducts less current than a semiconductor material or a conductive material. However, a small amount of current still flows through the electrically insulating material under the influence of an electric field, because even an insulator may include a small amount of charge carriers that carry the current. In the examples herein, a material can be considered electrically insulating where the material is sufficiently electrically insulating to perform the function of an insulator. For example, this function can be performed where the material is sufficiently insulating to prevent a short circuit.

[0061] exist Figure 4 In the example shown, the first (insulating) material 210 is deposited by inkjet material deposition. That is, in this example, the deposition of the first material 210 uses inkjet technology to accurately deposit the first material 210 as droplets 224. In this example, the first material 210 is deposited in the form of ink by inkjet printing. The ink solidifies to form a solid material. However, it will be understood that in other examples, the first material can be deposited in a form other than ink, but can still be deposited using inkjet technology.

[0062] As mentioned, in this example, the first material is deposited by inkjet printing. That is, in this example, depositing the first material 210 includes inkjet printing the first material 210. In this example, the insulating ink is inkjet printed from an inkjet printing component (e.g., a nozzle 220 of a deposition device 230). The nozzle 220 prints droplets 224 of the insulating ink on the exposed portion 274 of the cathode layer 204 and the exposed portion 276 of the electrolyte layer 206.

[0063] In this example, the inkjet printing of the first material 210 is performed from top to bottom. In other words, in this example, the droplet 224 travels from the nozzle 220 to the stack 200 at a speed that has a component in the same direction as the force acting on the droplet 224 due to gravity. Performing the inkjet printing from top to bottom can allow the first material 210 to be accurately and efficiently deposited.

[0064] exist Figure 4 In the example of , the first (insulating) material 210 so printed is deposited onto and supported by the exposed portion or ledge 273 of the substrate layer 202. In this example, the print nozzle 220 is angled relative to the plane of the stack 200 to direct the ink droplets 224 into the corner region of the cutout 212, which is bounded by the exposed surfaces 274, 276 of the cathode and electrolyte layers 204, 206 and the ledge 273 provided by the substrate layer 202. This can allow the first material 210 supported by the ledge 273 to accumulate on the exposed portions 274, 276 of the cathode and electrolyte layers 204, 206, thereby covering the exposed portions 274, 276 of the cathode and electrolyte layers 204, 206.

[0065] Once printed, the insulating ink 210 can be cured. For example, the insulating ink can be cured by evaporation of a carrier solvent of the insulating ink, for example, occurring at ambient temperature. As another example, the curing of the insulating ink can be facilitated by an external curing device (not shown), such as by a heat source or an ultraviolet (UV) light source (not shown), for example, if the curing of the insulating ink is thereby facilitated.

[0066] Depositing the first material 210 by inkjet material deposition, such as inkjet printing, can allow for flexible, efficient, and / or reliable deposition. For example, inkjet printing can allow for more flexible, efficient, and / or reliable deposition than, for example, thermal spraying, in which the material is sprayed onto the stack at high temperature and vacuum. For example, thermal spraying can rely on the edges of the stack to be exposed and substantially perpendicular to the direction of spraying to be covered, or rely on wetting the material onto the edges. This can limit the placement of the stack or layers of the stack and can be unreliable. However, the higher degree of spatial and directional control provided by inkjet printing can allow small areas of the stack to be precisely and reliably targeted, which can increase the flexibility and reliability of deposition and, therefore, the efficiency of the resulting battery. As another example, the high temperatures associated with thermal spraying can deform or damage the stack or layers of the stack. However, deposition by inkjet printing can be performed at relatively low, such as ambient temperatures, and can therefore reduce or prevent damage to the stack, thereby improving battery production efficiency. As another example, the vacuum conditions and / or high temperatures associated with thermal spraying can be energy intensive and, therefore, can result in uneconomical or inefficient deposition. However, inkjet printing may be performed at relatively low (eg, ambient) temperatures and / or pressures, and may therefore allow for economical and / or efficient deposition and, therefore, battery production.

[0067] Reference Figure 5 , as already mentioned in reference Figure 4 The first material 210 is deposited as described, and the second material 214 is deposited on the first material 210 and forms the second electrode layer 208 (in this example, the anode layer 208) of the stack 200 and provides electrical connections from the second electrode layer 208 (according to reference Figure 3 205 of the method described above).

[0068] The second material 214 is used to form the second electrode layer 208 and to electrically connect the formed second electrode layer 208 to another such second electrode layer ( Figure 4 or Figure 5 200). The first material 210 insulates (i.e., electrically insulates) the exposed portions 276, 274 of the first electrode layer 204 and the electrolyte layer 206 from the second material 214. Thus, electrical connections of the second electrode layer 208 can be provided to other such second electrode layers (not shown) of other such stacked portions or batteries (not shown) via the second material 214 to allow parallel electrical connection of batteries, but the second material 214 does not cause a short circuit between the first electrode layer 204 and the second electrode layer 208 of the stack 200.

[0069] The second material 214 is used to connect (eg, electrically connect) the second electrode layer 208 to another such second electrode layer ( Figure 4 or Figure 5 208 to the anode layer 208 of the battery. The first material 210 insulates (i.e., electrically insulates) the exposed portions 276, 274 of the cathode layer 204 and the electrolyte layer 206 from the second material 214, thereby preventing a short circuit between the anode layer 208 and the cathode layer 204. Therefore, the electrical connection of the anode layer 208 of the battery can be via the second material 214 to allow parallel electrical connection of the battery, but the second material 214 does not cause a short circuit between the anode layer 208 and the cathode layer 204. The connection of multiple batteries can allow the production of a relatively large capacity energy storage device. Connecting batteries in parallel can provide an energy storage device that can have a relatively large discharge rate, which may be useful in certain applications.

[0070] The second material 214 is a conductive material. For example, the second material 214 can have a lower electrical resistance, for example, a substantially lower electrical resistance, than the first material 210. In any case, the second material 214 has a conductivity sufficient to provide an effective electrical connection.

[0071] In this example, the second material 214 is or includes an anode material. For example, the second material 214 may be or include anode material. Figure 1 The anode layer 108 described above may be the same material as the anode layer 108 described above. In some examples, the anode material 214 may include a material that acts as a negative electrode layer once deposited. For example, the anode material 214 may be or include one or more of lithium metal, graphite, silicon, or indium tin oxide. In some examples, the anode 214 material may include a material that acts as a current collector once deposited. For example, the anode material may be or include nickel or other metal. In examples where the anode layer 208 will include a negative current collector and a separate negative electrode layer (not shown), depositing the second material 214 may include depositing one or both of the negative electrode material and the negative current collector material, such as on the negative current electrode material, thereby forming the anode layer 208.

[0072] The second (anode) material 214 is deposited on the electrolyte layer 206. That is, in this example, the second (anode) material 214 is deposited on and supported by the second exposed surface or ledge 277 of the electrolyte layer 206, thereby completing the stacked anode layer 208. In other words, once the second (anode) material 208 is deposited on the electrolyte layer, the stack includes the substrate layer 202, the cathode layer 204 and the electrolyte layer 206, and the anode layer 208, wherein the electrolyte layer 206 is located between the cathode layer 204 and the anode layer 208, and the anode layer 208 is distal to the substrate layer 208 (i.e., the cathode layer 204 is proximal to the substrate layer 202). The second (anode) material 214 is also deposited on the first material 210 and on the ledge 273 of the substrate layer 202, and is supported by it.

[0073] The second (anode) material 214 can be deposited by a vapor deposition process, such as a physical vapor deposition process, such as overflow deposition, but other deposition methods can be used. For example, the deposition device 220b of the deposition apparatus 230 can be arranged to deposit 226b the second (anode) material 214 on substantially the entire first side 200a of the stack 200.

[0074] The second (anode) material 214 is used to connect (e.g., electrically connect) to another such anode layer ( Figure 4 or Figure 5 For example, the conductive anode material 214 can provide an electrical connection from the anode layer 208 to the formed anode layer (not shown) of other cells, thereby connecting the anodes of the cells in parallel. In this example, therefore, the second material 214 can form a positive terminal of an energy storage device including such a cell.

[0075] The first material 210 insulates (i.e., electrically insulates) the exposed portions 274, 276 of the cathode layer 204 and the electrolyte layer 206 from the second (anode) material 214, thereby preventing a short circuit between the anode layer 208 and the cathode layer 204. Thus, the electrical connection of the anode layer 208 of the battery can be through the second material 214 to allow parallel electrical connection of the batteries, but the second material 214 does not cause a short circuit between the anode layer 208 and the cathode layer 204.

[0076] Depositing the anode material as the second material 214 can allow efficient battery production. For example, depositing the anode material to form the anode layer 208 can allow the obtained stack 200 to not need to include an anode layer, and allow the deposited anode material to form the anode layer 208. For example, this can reduce the total amount of conductive material used to make a battery from the stack 200 compared to if a separate conductive material is added to the already formed anode layer to provide electrical connection from it. As another example, the anode material can be relatively cheap. For example, the anode material can be cheap compared to other materials that can be used to provide electrical contact from the anode layer. As another example, the anode material can be cheap compared to the cathode material. Therefore, using the anode material to provide the anode layer 208 with electrical connections to other such anode layers of other batteries can allow for reduced costs of battery production, and therefore can allow for more efficient battery production. As another example, the deposition of the anode material can be relatively fast and / or cheap, for example, compared to other methods for depositing materials, such as by overflow deposition. As another example, it may be efficient to deposit the second (anode) material 214 using the same or similar methods and / or means to form the layers of the resulting stack 200, for example, as opposed to providing separate methods and / or means for each function.

[0077] exist Figure 4 and 5 In the first example, the stack 200 has only one of each of the electrolyte layer 206 and the cathode layer 204 supported on the substrate layer 202. It will be appreciated that this need not necessarily be the case, as described below with reference to Figure 6 and 7 Described in more detail.

[0078] refer to Figure 6 , shows a stack 200 ′ according to a second example (ie, it can be based on reference Figure 3 The stack 200' may be similar to that of step 201 of the method described above. Figure 4 The stack 200 is described, therefore, for the sake of brevity, the same features will not be described in detail. Like features are represented by like reference numerals.

[0079] Figure 6 Stacking 200' with Figure 4 The difference of stack 200 is that Figure 6 The stack 200' includes another second electrode layer 208a (another anode layer 208a in this example) and another electrolyte layer 206a between the other second electrode layer 208a and the first electrode layer (the cathode layer 204 in this example). More specifically, in this example, the stack 200' includes not only the substrate layer 202, the cathode layer 204, the electrolyte layer 206 and the anode layer 208 (once formed, see Figure 7 ), and further includes a first further electrolyte layer 206a (on which the cathode layer 204 is deposited), another cathode layer 204a (on which the first further electrolyte layer 206a is deposited), a second further electrolyte layer 206b (on which the another cathode layer 204a is deposited), and another cathode layer 204a (on which the second further electrolyte layer 206b is deposited). The other cathode layer 204a is adjacent to the substrate layer 202, and the anode layer 208 is away from the substrate layer 202 in these layers.

[0080] The stack 200' of this second example may be referred to as a "multi-stack" or "multi-battery" stack because the stack 200' has been formed on one substrate layer 202 that can constitute multiple batteries. For example, the cathode layer 204, the electrolyte layer 206, and the anode layer 208 (once formed) may constitute a first battery, the cathode layer 204, the first another electrolyte layer 206a, and the another anode layer 204a may constitute a second battery, and the another anode layer 206a, the second another electrolyte layer 206b, and the another cathode layer 204a may constitute a third battery of the multi-battery stack 200'. That is, in these examples, the another anode layer 208a may serve as the anode layer of both the second battery and the third battery, and the cathode layer 204 may serve as the cathode layer of both the first battery and the second battery. This may be an effective arrangement because it may reduce the amount of anode and / or cathode material required to form multiple batteries.

[0081] Figure 6 The cutout 212' in the stack 200' is such that the cathode layer 204 and the electrolyte layer 206 are aligned with the first further electrolyte layer 206a and recessed from the further anode layer 208a, such that the further anode layer 208a provides an exposed portion or surface or ledge 279. The cutout 212' or recess also aligns the further anode layer 208a, the second further electrolyte layer 206b, and the further cathode layer 204a and recessed from the substrate layer 202, such that the substrate layer 202 provides an exposed portion or surface or ledge 279. In this example, the cutout 212' can be formed by multiple cutting steps, such as by laser ablation using different and / or offset laser beams. For example, the cut 212' can be formed by first cutting the stack 200' to expose the electrolyte layer 206, the cathode layer 204 and portions 276, 274, 276a of the first further electrolyte layer 206a, and the ledge 279 of the further anode layer 208a; and then cutting the stack 200' to expose the further cathode layer 204a, the second further electrolyte layer 206b and portions 274a, 276b, 278a of the further anode layer 208a, and the ledge 273 of the substrate layer 202.

[0082] and Figure 4 The stack of 200 is the same as in Figure 6In the example of , the first material 210 is deposited on the exposed edges 274, 276 of the cathode layer 204 and the electrolyte layer 206. However, in this example, the first material is also deposited on the exposed portion 276a of the first further electrolyte layer 206a and is supported by the ledge 279 of the further anode layer 208a. Figure 6 In the stack 200', the first material 210 is also deposited on the exposed portions 276b, 274a of the second further electrolyte layer 206a and the further cathode layer 204a and supported by the ledge 273 of the substrate layer 202. As a result, the exposed portion 278a of the further anode layer 208a remains exposed. The first material can be deposited, for example, by inkjet printing, for example, as described in reference Figure 4 and Figure 5 as described.

[0083] Reference Figure 7 ,and Figure 5 As with the stack 200 of FIG. 1 , a second (anode) material 214 is deposited on the first material 210 and forms a second electrode layer (anode layer 208 in this example). Figure 7 In the stack 200', a second (anode) material 214 is deposited to contact another second electrode layer (in this example, another anode layer 208). Specifically, the second material 214 is deposited to contact the exposed portion 278a of the other anode layer 278a. As a result, the anode layer 208 and the other anode layer 208 are connected (electrically connected) via the second material 214. In this example, the second material 214 is at least partially supported by the ledge 279 of the other anode layer 208a and the ledge 273 of the substrate layer 202. The first material 210 electrically insulates the exposed portions 274, 276, 276a, 274a, 276b of the cathode layer 204, the electrolyte layer 204, the first other electrolyte layer 206a, the other cathode layer 204a and the second other electrolyte layer 206b from the second material 214.

[0084] The second (anode) material 214 may be made of the same material as described above. Figure 4 and Figure 5 The deposition may be carried out in the same manner as described, for example using flood deposition.

[0085] The second (anode) material 214 provides an electrical connection from the anode layer 208 of the first and second cells of the multi-cell stack 200″ to another anode layer 208a of a third cell of the multi-cell stack, thereby connecting the first through third cells in parallel. Thus, the second material 214 can form a positive terminal of an energy storage device including such a cell. The first material 210 enables the cathode layer 204, the electrolyte layer 206, the first further electrolyte layer 206a, the further cathode layer 204a and the second further electrolyte layer 206a to be electrically connected to each other. The exposed portions 274, 276, 276a, 274a, 276b of the anode layer 208, 208a are insulated (e.g., electrically insulated) from the second material 214, thereby preventing a short circuit between the anode layer 208, 208a and the cathode layer 204, 204a. Therefore, the electrical connection of the anode layer 208, 208a of the battery can be via the second material 214 to allow parallel electrical connection of the battery, but the second material 214 does not cause a short circuit between the anode layer 208, 208a and the cathode layer 204, 204a.

[0086] In such Figure 6 and 7 Providing electrical connections between cells in a multi-cell stack 200' can provide efficient cell production. For example, the multi-cell stack 200' can reduce the amount of substrate layer 202 for each cell, and thus can reduce the cost associated with providing the substrate layer 202. As another example, the second material 214 connecting multiple cells can be deposited in a single deposition, for example, compared to electrically connecting cells one by one, which can reduce time and therefore reduce costs.

[0087] It will be appreciated that although only three cells are provided in the multi-cell stack 200', in other examples, there may be more or fewer cells. For example, the multi-cell stack 200' may include a plurality of cells, wherein the stack 200' includes at least a first electrode layer 204, an electrolyte layer 206, a second electrode layer 208, another electrolyte layer 206a, 206b, and another second electrode layer 208a.

[0088] It should be understood that although in the above examples, the anode, electrolyte and cathode layers 204, 204, 208, 204a, 206a, 208a, 206b are formed on the substrate layer 202 only towards the first side 200a of the stack 200a, and the deposition of the first material 210 and the second material 210 is performed only on the first side 200a of the stack, this need not necessarily be the case, and in some examples, the anode, electrolyte and cathode layers (not shown) may additionally be formed on the substrate layer 202 towards the second side 200b of the stack. The additional layers (not shown) on the second side 200b of the substrate 202 may be, for example, mirror images of the layers 204, 204, 208, 204a, 206a, 208a, 206b, including the cutouts 212, 212' in the layers on the first side 200a of the substrate layer 202 in the first and / or second examples described.

[0089] In these examples, the first material 210 and the second material 214 can be made in the same manner as described above with reference to Figures 3 to 7 Deposited in the same or similar manner as described.

[0090] In the case where the first material 210 is deposited by inkjet material deposition (e.g., inkjet printing), even in the case where the anode, electrolyte, and cathode layers are also formed on the second side 200b of the substrate layer 202, for example, as described with reference to Figure 4 As described, it may also be beneficial to maintain a top-down arrangement for inkjet material deposition.

[0091] Figure 8 An exemplary arrangement of a deposition apparatus 230 is schematically shown that facilitates top-down inkjet material deposition (such as inkjet printing) of a first material 210 onto a stack 200, 200' having layers formed on both sides 200a, 200b of a substrate.

[0092] Reference Figure 8 The deposition device 230 includes rollers 252a, 252b, 252c, which are arranged to guide the movement of the stack 200, 200' so that the first side 200a of the stack 200, 200' is presented for top-down inkjet material deposition, such as inkjet printing, of the first material 210 from a first inkjet material deposition component (e.g., an inkjet printing nozzle 220'), and the second side 200b of the stack 200, 200' is presented for top-down inkjet material deposition, such as inkjet printing, of the first material 210 from a second inkjet material deposition component (e.g., an inkjet printing nozzle 220").

[0093] More specifically, if Figure 8 As shown, for example, as a reference Figure 2As part of the described roll-to-roll type process, the stack 200, 200' travels over rollers 252a, 252b, 252c in a first travel direction 238. The stack 200, 200' passes through and is tensioned between the first roller 252a and the second roller 252b with the first side 200a of the stack 200, 200' facing upward toward the first nozzle 220'. As the stack 200, 200' passes through the second roller 252b, the stack 200-, 200, 200' is inverted. The stack 200, 200' passed through the second roller 252b and the third roller 252c and tensioned therebetween causes the second side 200b of the stack 200, 200' to face upward toward the second nozzle 220". In this way, top-down printing of the first material 210 can be provided in a roll-to-roll type process, which can, for example, be substantially continuous. This can provide efficient battery production. Performing inkjet printing from top to bottom can allow accurate and efficient deposition of the first material 210.

[0094] It will be appreciated that while in each of the above examples the first material 210 is described as being deposited by inkjet material deposition such as inkjet printing, this need not be the case and in some examples the first material 210 may be deposited by methods other than inkjet material deposition.

[0095] It will be understood that reference Figures 3 to 8 The product of each of the examples described may be an intermediate product of an energy storage device production process, and in some examples, further processing may be performed on the stack 200, 200' to produce an energy storage device.

[0096] In the various examples described above, the intermediate product takes the form of a stack 200, 200' for an energy storage device, the stack 200, 200' comprising a first electrode layer 204, a second electrode layer 208, and an electrolyte layer 206 between the first electrode layer 204 and the second electrode layer 208. The stack 200, 200' comprises a first material 210 on a portion 274 of the first electrode layer 204 (i.e., the portion 274 to be exposed but covered by the first material 210) and a portion 276 of the electrolyte layer 206 (i.e., the portion 276 to be exposed but covered by the first material 210). The stack comprises a second material 214 on the first material 210 and forming the second electrode layer 208, and providing electrical connection from the second electrode layer 208 for connection to another second electrode layer 208a through the second material 214. The first material 210 insulates the exposed portions 274, 276 of the first electrode layer 204 and the electrolyte layer 206 from the second material 214.

[0097] The above examples should be understood as illustrative examples of the present invention. It should be understood that any feature described with respect to any one example can be used alone or in combination with other features described, and can also be used in combination with one or more features of any other example or any combination of other examples. In addition, without departing from the scope of the present invention defined in the appended claims, equivalents and modifications not described above may also be adopted.

Claims

1. A method for obtaining an energy storage device, comprising: obtaining a stack for an energy storage device, the stack comprising a first electrode layer and an electrolyte layer; depositing a first material on the exposed portion of the first electrode layer and the exposed portion of the electrolyte layer; and depositing a second material on the first material and forming a stacked second electrode layer, and providing electrical connection to the second electrode layer to connect to another such second electrode layer through the second material, wherein the electrolyte layer is between the first electrode layer and the second electrode layer; whereby the first material insulates the exposed portions of the first electrode layer and the electrolyte layer from the second material, wherein the stack comprises another second electrode layer, and another electrolyte layer between the another second electrode layer and the first electrode layer, wherein depositing the first material further comprises depositing the first material on an exposed portion of the another electrolyte layer, and wherein depositing the second material further comprises depositing the second material to contact the another second electrode layer, thereby connecting the second electrode layer and the another second electrode layer via the second material, such that the first material further insulates the exposed portion of the another electrolyte layer from the second material, The electrolyte layer, the first electrode layer and the further electrolyte layer are recessed from the further second electrode layer such that the further second electrode layer provides a ledge on which the first material and / or the second material are supported.

2. The method according to claim 1, wherein: Depositing the first material includes inkjet material deposition of the first material.

3. The method according to claim 1 or 2, wherein: The stack includes a substrate adjacent to one of the first electrode layer and the second electrode layer, wherein the other of the first electrode layer and the second electrode layer is an anode layer.

4. The method according to claim 3, wherein: The second material is an anode material for forming an anode layer.

5. The method according to claim 4, wherein: The first electrode layer and the electrolyte layer are recessed from the substrate such that the substrate provides a ledge portion on which the first material and / or the second material is at least partially supported.

6. The method according to any one of claims 1 to 2, wherein: The method comprises laser ablating the stack, and wherein one or more of the exposed portions are exposed by the laser ablating the stack.

7. A stack for an energy storage device, the stack comprising a first electrode, a second electrode layer and an electrolyte layer between the first electrode layer and the second electrode layer, the stack comprising a first material on a portion of the first electrode layer and a portion of the electrolyte layer; a second material on the first material and forming the second electrode layer and providing an electrical connection to the second electrode layer to connect to another such second electrode layer through the second material, wherein the first material insulates the portion of the first electrode layer and the portion of the electrolyte layer from the second material, in, The stack comprises another second electrode layer, and another electrolyte layer between the another second electrode layer and the first electrode layer, wherein depositing the first material further comprises depositing the first material on an exposed portion of the another electrolyte layer, and wherein depositing the second material further comprises depositing the second material to contact the another second electrode layer, thereby connecting the second electrode layer and the another second electrode layer via the second material, such that the first material further insulates the exposed portion of the another electrolyte layer from the second material, The electrolyte layer, the first electrode layer and the further electrolyte layer are recessed from the further second electrode layer such that the further second electrode layer provides a ledge on which the first material and / or the second material are supported.

8. An energy storage device formed according to the method of any one of claims 1 to 6.