Memory Components

By using a shallow isolation structure with a dielectric constant less than 3.9 and an alternately stacked insulating layer and conductive layer structure in three-dimensional memory components, the problem of component size increase caused by too many common source lines is solved, and the electronic characteristics and storage capacity are improved. .

CN112614844BActive Publication Date: 2024-10-15MACRONIX INTERNATIONAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201910986718.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-10-04
Filing Date
2019-10-17
Publication Date
2024-10-15
Estimated Expiration
2040-04-26

AI Technical Summary

Technical Problem

In the production process of three-dimensional memory components, too many common source lines lead to an increase in component size, affecting storage capacity and electronic characteristics.

Method used

A memory element design including a substrate, a stacked structure, a channel structure and a shallow isolation structure is adopted. The stacked structure is composed of alternately stacked insulating layers and conductive layers. The channel structure passes through the stacked structure and is electrically connected to the substrate. Shallow isolation The structures are made of materials with a dielectric constant less than 3.9, and blocks are separated into sub-blocks through these structures to reduce the number of conductive layers.

Benefits of technology

It effectively reduces the size of the memory element, while improving the electrical characteristics between the conductive layers, reducing the capacitance and charging delay time, and enhancing the performance of the element.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112614844B_ABST
    Figure CN112614844B_ABST
Patent Text Reader

Abstract

The present invention discloses a memory element, which includes a substrate, a stacked structure, a plurality of channel structures, a plurality of storage layers and a plurality of shallow isolation structures. The substrate has an upper surface. The stacked structure is located on the upper surface of the substrate, wherein the stacked structure includes a plurality of insulating layers and a plurality of conductive layers alternately stacked on the upper surface. The channel structure passes through a portion of the stacked structure and is electrically connected to the substrate. Each storage layer surrounds each corresponding channel structure. The shallow isolation structure extends from a top surface of the stacked structure toward the substrate, wherein each shallow isolation structure includes a substance, and the dielectric constant of the substance is less than 3.9.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure belongs to the field of semiconductor technology and relates to a semiconductor structure, and in particular to a memory element. Background Art

[0002] Recently, as the demand for more excellent memory devices has gradually increased, various three-dimensional (3D) memory devices, such as 3D NAND memory devices or 3D ROM memory devices, have been provided. Such 3D memory devices can achieve higher storage capacity and have more excellent electronic characteristics, such as good data retention reliability and operation speed.

[0003] During the manufacturing process of the three-dimensional memory device, a plurality of common source lines electrically connected to the substrate need to be formed to divide the three-dimensional memory device into a plurality of blocks and sub-blocks. However, too many common source lines may cause the size of the three-dimensional memory device to become larger.

[0004] Therefore, there is a need to provide an advanced memory element and a manufacturing method thereof to solve the problems faced by the prior art. Summary of the invention

[0005] In the present disclosure, a memory device and a method for manufacturing the same are provided to solve at least part of the above problems.

[0006] According to one embodiment of the present invention, a memory element includes a substrate, a stacked structure, a plurality of channel structures, a plurality of storage layers, and a plurality of shallow isolation structures. The substrate has an upper surface. The stacked structure is located on the upper surface of the substrate, wherein the stacked structure includes a plurality of insulating layers and a plurality of conductive layers alternately stacked on the upper surface. The channel structure passes through a portion of the stacked structure and is electrically connected to the substrate. Each storage layer surrounds each corresponding channel structure. The shallow isolation structure extends from a top surface of the stacked structure toward the substrate, wherein each shallow isolation structure includes a substance having a dielectric constant less than 3.9.

[0007] According to one embodiment of the present invention, a method for manufacturing a memory element includes the following steps. First, a substrate is provided, the substrate having an upper surface. Then, a stacked structure is formed on the upper surface of the substrate, wherein the stacked structure includes a plurality of insulating layers and a plurality of conductive layers stacked on the upper surface of the substrate. A plurality of channel structures and a plurality of storage layers are formed through a portion of the stacked structure, the channel structures are electrically connected to the substrate, and each storage layer surrounds each corresponding channel structure. A plurality of upper openings are formed through an upper portion of the stacked structure. Thereafter, a plurality of shallow isolation structures are formed in the upper openings, the shallow isolation structures extending from a top surface of the stacked structure toward the substrate, wherein each shallow isolation structure includes a substance having a dielectric constant less than 3.9.

[0008] According to one embodiment of the present invention, a method for manufacturing a memory element includes the following steps. First, a substrate is provided, the substrate having an upper surface. Then, a stacked body is formed on the upper surface of the substrate, wherein the stacked body includes a plurality of insulating layers and a plurality of sacrificial layers alternately stacked on the upper surface of the substrate. A plurality of channel structures and a plurality of storage layers are formed through the stacked body, the channel structures are electrically connected to the substrate, and the storage layers surround the corresponding channel structures. A plurality of vertical openings are formed through the stacked body. The sacrificial layers are removed through the vertical openings. A plurality of conductive layers are formed at the position where the sacrificial layers are removed, so that the insulating layers and conductive layers alternately stacked on the upper surface form a stacked structure. Thereafter, a plurality of upper openings are formed through an upper portion of the stacked structure. A plurality of shallow isolation structures are formed in the upper openings, the shallow isolation structures extending from a top surface of the stacked structure toward the substrate, wherein each shallow isolation structure includes a substance having a dielectric constant less than 3.9.

[0009] In order to better understand the above and other aspects of the present invention, the following embodiments are specifically described in detail with reference to the accompanying drawings. However, the scope of protection of the present invention shall be subject to the scope defined by the claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1A A top view of a memory device according to an embodiment of the present disclosure is shown.

[0011] Figure 1B Draw along Figure 1A FIG. 1 is a cross-sectional view of a memory element according to an embodiment of the present disclosure along the AA′ line.

[0012] FIG. 2A to FIG. 2F A cross-sectional view is shown of a method for forming a memory device according to an embodiment of the present disclosure.

[0013] Figure 3 FIG. 4 is a cross-sectional view of a memory device according to another embodiment of the present disclosure.

[0014] FIG. 4A to FIG. 4F FIG. 5 is a cross-sectional view illustrating a method for forming a memory device according to another embodiment of the present disclosure.

[0015] Figure 5 FIG. 4 is a cross-sectional view of a memory device according to another embodiment of the present disclosure.

[0016]

Explanation of symbols

[0017] 100, 200, 300, 400, 500: memory components

[0018] 110, 210, 410: substrate

[0019] 110a, 210a, 410a: upper surface

[0020] 111, 211, 411: Insulation column

[0021] 112, 212, 412: Channel structure

[0022] 114, 214, 414: Storage layer

[0023] 116, 216, 416: Cover layer

[0024] 120, 220, 420: Conductive connection structure

[0025] 124, 224, 324, 424, 524: Shallow isolation structure

[0026] 124s, CL1s: bottom surface

[0027] 218, 418: vertical opening

[0028] 222, 422: upper opening

[0029] 224t, 324t, 424t, 524t, S1a, S2a, S4a: Top surface

[0030] 324a, 524a: Air gap

[0031] 324b, 524b: Oxide lining

[0032] 1241: First side

[0033] 1242: Second side

[0034] B1, B2: Block

[0035] B1a, B1b, B1c, B1d, B2a, B2b, B2c, B2d: sub-blocks

[0036] CL1, CL1a, CL1b, CL1c, CL2, CL2a, CL2b, CL2c: Conductive layer

[0037] D1, D2: distance

[0038] H1, H2: Depth

[0039] IL1, IL2, IL4: Insulation layer

[0040] M: Storage unit

[0041] Q2, Q4: Internal opening

[0042] P2, P4: channel opening

[0043] S1, S2, S4: laminated structure

[0044] S2', S4': laminated body

[0045] T: Transistor

[0046] V2, V4: Through hole

[0047] W1, W2, W3: Width DETAILED DESCRIPTION

[0048] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments and with reference to the accompanying drawings.

[0049] In the detailed description below, various specific details are provided to provide an overall understanding of the embodiments of the present disclosure for ease of explanation. However, it should be understood that one or more embodiments can be implemented without adopting these specific details. In other cases, in order to simplify the drawings, known structures and elements are represented by schematic diagrams.

[0050] Figure 1A A top view of a memory device 100 according to an embodiment of the present disclosure is shown; Figure 1B Draw along Figure 1A FIG. 1 is a cross-sectional view of a memory element 100 according to an embodiment of the present disclosure, taken along line AA′.

[0051] Please refer to Figure 1A , a plurality of conductive connection structures 120 are arranged parallel to the upper surface 110a of the substrate 110 (shown in FIG. Figure 1B ) extends in a first direction (e.g., the X-axis direction) to divide the memory element 100 into a plurality of blocks B1, B2, ... Each block B1, B2, ... includes a plurality of shallow isolation structures 124. The shallow isolation structure 124 divides the block B1 into a plurality of sub-blocks B1a, B1b, B1c, B1d, and divides the block B2 into a plurality of sub-blocks B2a, B2b, B2c, B1d. In the present embodiment, each block has three shallow isolation structures 124, but the present invention is not limited thereto. In other embodiments, each block may have two or more than three shallow isolation structures. In some embodiments, the conductive connection structure 120 is a common source line.

[0052] Please also refer to Figure 1A and Figure 1BThe memory device 100 includes a substrate 110, a stacked structure S1, a plurality of insulating pillars 111, a plurality of channel structures 112, a plurality of storage layers 114, a plurality of shallow isolation structures 124, and a plurality of conductive connection structures 120. The stacked structure S1 is formed on the upper surface 110a of the substrate 110. The stacked structure S1 includes a plurality of insulating layers IL1 and a plurality of conductive layers CL1 alternately stacked (e.g., along the Z axis) on the upper surface 110a of the substrate 110, and a cap layer 116 located at the top portion of the stacked structure S1.

[0053] In some embodiments, the substrate 110 may be a silicon substrate or other suitable substrates. The insulating layer IL1 and the cap layer 116 may be formed of oxides, such as silicon dioxide (SiO2). In some embodiments, the material of the cap layer 116 may be the same as the material of the insulating layer IL1. The conductive layer CL1 may be formed of a conductive material, such as tungsten (W), aluminum (Al), titanium nitride (TiN), tantalum nitride (TaN), doped or undoped polysilicon (poly-silicon) or other suitable materials.

[0054] In the embodiments of the present invention, only the numbers of insulating layers and conductive layers are illustrated for example, but the present invention is not limited thereto. In some embodiments, the numbers of insulating layers and conductive layers may be any appropriate numbers.

[0055] The conductive connection structure 120 passes through (eg, along the Z axis) the stacked structure S1 and is electrically connected to the substrate 110 . The conductive connection structure 120 divides the memory device 100 into a plurality of blocks B1 , B2 . . . The conductive layers CL1 between different blocks B1 , B2 . . . are completely separated by the conductive connection structure 120 .

[0056] The channel structure 112 passes through (e.g., along the Z axis) a portion of the stacked structure S1 and is electrically connected to the substrate 110. The top of the channel structure 112 may be electrically connected to a bit line (not shown). In some embodiments, the channel structure 112 may be formed of a semiconductor material, such as doped or undoped polysilicon. In some embodiments, the insulating pillar 111 passes through (e.g., along the Z axis) a portion of the stacked structure S1 and is surrounded by the channel structure 112.

[0057] The storage layer 114 surrounds the corresponding channel structure 112. In some embodiments, the storage layer 114 may be formed of a composite layer (ie, ONO layer) including a silicon oxide layer, a silicon nitride layer, and a silicon oxide layer.

[0058] In some embodiments, the conductive connection structure 120 and the shallow isolation structure 124 extend along a first direction (for example, the X-axis direction) respectively, and are arranged along a second direction (for example, the Y-axis direction) on the substrate 110. The first direction and the second direction are both parallel to the upper surface 110a of the substrate 110, and the first direction is staggered with the second direction (for example, there may be a non-straight angle between the first direction and the second direction).

[0059] The shallow isolation structure 124 may extend from the top surface S1a of the stacked structure S1 in a direction toward the substrate 110 (e.g., in the Z-axis direction), pass through the upper portion of the stacked structure S1, and separate each block (e.g., B1, B2) into a plurality of sub-blocks (e.g., B1a, B1b, B1c, B1d, B2a, B2b, B2c, B1d). Each shallow isolation structure 124 includes a material having a dielectric constant less than 3.9. For example, the shallow isolation structure 124 may include a low-k material or an air gap. The low-k material may be fluorine-doped silicon dioxide, carbon-doped oxide, porous silicon dioxide, spin-on organic polymeric dielectric, spin-on silicon based polymeric dielectric, or other suitable materials. In the present embodiment, the shallow isolation structure 124 passes through the first top conductive layer CL1a, the second top conductive layer CL1b and the third top conductive layer CL1c (i.e., three conductive layers) sequentially disposed below the top surface S1a. However, the present invention is not limited thereto, and the shallow isolation structure 124 may pass through more than three conductive layers. The shallow isolation structure 124 has a bottom surface 124s, and the bottom surface 124s faces the top surface 110a of the substrate 110. In the normal direction (e.g., the third direction or the Z-axis direction) of the top surface 110a of the substrate 110, the depth H1 of the shallow isolation structure 124 is smaller than the depth H2 of the conductive connection structure 120. The depth H1 is equivalent to the distance between the top surface S1a of the stacked structure S1 and the bottom surface 124s of the shallow isolation structure 124, and the depth H2 is equivalent to the distance between the top surface S1a of the stacked structure S1 and the top surface 110a of the substrate 110.

[0060] In some embodiments, the width W1 of the shallow isolation structure 124 may be between about 40 nm and about 145 nm. The depth H1 of the shallow isolation structure 124 may be greater than 130 nm.

[0061] In some embodiments, a conductive layer CL1 that is closest to the bottom surface 124s among the conductive layers CL1 through which the shallow isolation structure 124 passes has a bottom surface CL1s, and the distance between the bottom surface CL1s of the conductive layer CL1 and the upper surface 110a of the substrate 110 may be equal to or greater than the distance between the bottom surface 124s of the shallow isolation structure 124 and the upper surface 110a of the substrate 110. In this embodiment, the third top conductive layer CL1c is a conductive layer that is closest to the bottom surface 124s among the conductive layers through which the shallow isolation structure 124 passes (i.e., the first top conductive layer CL1a, the second top conductive layer CL1b, and the third top conductive layer CL1c), and the distance D1 between the bottom surface CL1s of the third top conductive layer CL1c and the upper surface 110a of the substrate 110 is greater than the distance D2 between the bottom surface 124s of the shallow isolation structure 124 and the upper surface 110a of the substrate 110.

[0062] In some embodiments, the shallow isolation structure 124 directly contacts the corresponding plurality of conductive layers CL1. In this embodiment, the shallow isolation structure 124 directly contacts the corresponding first top conductive layer CL1a, second top conductive layer CL1b and third top conductive layer CL1c, but the invention is not limited thereto.

[0063] In some embodiments, the conductive layer through which the shallow isolation structure 124 passes can be used as a serial selection line. In this embodiment, the first top conductive layer CL1a, the second top conductive layer CL1b, and the third top conductive layer CL1c can be used as a serial selection line. In other words, the shallow isolation structure 124 can pass through three or more conductive layers located on the upper portion of the stacked structure S1, and each shallow isolation structure 124 separates the three or more conductive layers on the upper portion of the stacked structure S1 into two electrically independent serial selection lines.

[0064] In the present embodiment, since the serial selection lines (e.g., the first top conductive layer CL1a, the second top conductive layer CL1b, and the third top conductive layer CL1c) in different sub-blocks B1a, B1b, B1c, and B1d are separated by the shallow isolation structure 124 including a material with a dielectric constant less than 3.9, when voltage operation is performed on the serial selection lines of the sub-blocks B1a, B1b, B1c, and B1d, the capacitance between the serial selection lines in the different sub-blocks B1a, B1b, B1c, and B1d can be reduced, thereby avoiding the voltage interference between the serial selection lines in different sub-blocks. For example, the voltage interference between the third top conductive layer CL1c located on the first side 1241 of the shallow isolation structure 124 and the voltage interference between the third top conductive layer CL1c located on the second side 1242 of the shallow isolation structure 124 can be reduced. The first side 1241 is located on the opposite side of the second side 1242, for example, referring to Figure 1BAlong the second direction (y direction), the first side 1241 and the second side 1242 are arranged opposite to each other. Therefore, compared with the comparative example without the shallow isolation structure having a low dielectric constant, the present disclosure can reduce the capacitance between the serial selection lines of different sub-blocks through the arrangement of the shallow isolation structure 124, and can reduce the charging delay time of the serial selection lines of different sub-blocks, so that the voltage of the serial selection line is more stable, so that the serial selection line can have better electrical characteristics, so that the memory element can have better performance.

[0065] Furthermore, since the shallow isolation structure 124 of the present invention corresponds to multiple conductive layers (for example, 3 or more conductive layers), it can more effectively prevent leakage current from being generated during the boost period compared to the comparative example in which the shallow isolation structure only corresponds to 1 conductive layer.

[0066] In some embodiments, each intersection between the top conductive layer (e.g., top conductive layers CL1a, CL1b, and CL1c) serving as a string selection line and the memory layer 114 may form a transistor T, and each intersection between other conductive layers CL serving as a word line and the memory layer 114 may form a memory cell M. The transistor T and the memory cell M are connected in series via the channel structure 120 and may together form a memory cell string.

[0067] In a second direction (e.g., the Y-axis direction) parallel to the upper surface 110a of the substrate 110, the width W1 of the shallow isolation structure 124 vertically projected on the substrate 110 is smaller than the width W2 of the conductive connection structure 120 vertically projected on the substrate 110. That is, in a second direction (e.g., the Y-axis direction) parallel to the upper surface 110a of the substrate 110, the maximum width of the shallow isolation structure 124 is smaller than the maximum width of the conductive connection structure 120. In some embodiments, the width W1 of the shallow isolation structure 124 in the second direction is equal to or smaller than the width W3 of the diameter of the channel structure 112 in the second direction. In some embodiments, the width W1 of the shallow isolation structure 124 is, for example, between 40 and 145 nm. In the present embodiment, the second direction (e.g., the Y-axis direction) is, for example, perpendicular to the length direction (e.g., the X-axis direction) of the conductive connection structure 120 and the shallow isolation structure 124, but the present invention is not limited thereto, as long as there is a non-straight angle between the X-axis direction and the Y-axis direction.

[0068] In the present embodiment, three shallow isolation structures 124 are disposed between two adjacent conductive connection structures 120, and one block (e.g., B1) is divided into four sub-blocks (e.g., B1a, B1b, B1c, and B1d). However, the present invention is not limited thereto, and in other embodiments, two or more shallow isolation structures 124 may be disposed between two adjacent conductive connection structures 120. Compared with the comparative example of using a plurality of conductive connection structures 120 to divide one block of a memory element into a plurality of sub-blocks, since the present disclosure uses a shallow isolation structure 124 to divide one block into a plurality of sub-blocks, the width of the shallow isolation structure 124 along the second direction (e.g., the Y axis) is smaller than the width of the conductive connection structure 120 along the second direction (e.g., the Y axis), so the shallow isolation structure 124 occupies a smaller space in the memory element 100, and the size of the memory element 100 can be reduced.

[0069] In some embodiments, the memory device 100 may be Figure 2A to Figure 2F , Figure 3 , Figure 4A to Figure 4F and Figure 5 The memory element 200, 300, 400 or 500 is formed by a process method, but the present invention is not limited thereto, and the method for forming the memory element disclosed in the present invention also includes other suitable process methods. In addition, Figure 2A to Figure 2F , Figure 3 , Figure 4A to Figure 4F and Figure 5 The cross-sectional view of the memory element shown corresponds to Figure 1B 1 is a cross-sectional view of a memory element 100 .

[0070] FIG. 2A to FIG. 2F FIG. 2 is a cross-sectional view showing a method for forming a memory device 200 according to an embodiment of the present disclosure.

[0071] Please refer to Figure 2A A substrate 210 is provided, and a stacked body S2' is formed on the upper surface 210a of the substrate 210. The stacked body S2' includes a plurality of insulating layers IL2 and a plurality of conductive layers CL2 alternately stacked on the upper surface 210a of the substrate 210 in sequence (eg, by a deposition process).

[0072] In some embodiments, the substrate 210 may be a silicon substrate or other suitable substrate. The insulating layer IL2 may be formed of an oxide, such as silicon dioxide. The conductive layer CL2 may be doped or undoped polysilicon or other suitable materials, such as an n-type doped polysilicon layer.

[0073] Please refer to Figure 2B, a plurality of channel openings P2 are formed through (for example, along the Z direction) the stacked body S2' and exposing the upper surface 210a of the substrate 210 by an etching method (for example, dry etching). Next, a storage material is formed on the stacked body S2' and in these channel openings P2 by a deposition process. Next, a portion of the storage material located in the channel openings P2 is removed by an etching process to form a plurality of through holes V2 that expose the upper surface 210a of the substrate 210. Thereafter, a conductive material and an insulating material are filled in the through hole V2 to form a plurality of channel structures 212, a plurality of insulating pillars 211 and a storage layer 214. The channel structure 212 can be formed of doped or undoped polysilicon material. The storage layer 214 can be composed of a composite layer (i.e., an ONO layer) including a silicon oxide layer, a silicon nitride layer and a silicon oxide layer. Thereafter, a cap layer 216 covering the stack body S2' is formed by a deposition process, and a stack structure S2 including the stack body S2' and the cap layer 216 is formed. The stack structure S2 has a top surface S2a. The channel structure 212 passes through a portion of the stack structure S2 and is electrically connected to the substrate 110. Each storage layer 214 surrounds the corresponding channel structure 212.

[0074] Please refer to Figure 2C , a plurality of vertical openings 218 are formed through the stacked structure S2 by an etching process (e.g., a dry etching process). In this embodiment, the vertical openings 218 pass through the cap layer 216 and the stacked structure S2 and expose the upper surface 210a of the substrate 210. Then, a portion of the conductive layer CL2 is removed from the vertical openings 218.

[0075] Please refer to Figure 2D , an insulating material is filled in the vertical opening 218. Afterwards, a portion of the insulating material is removed to form an inner opening Q2. The inner opening Q2 passes through the stacked structure S2 and exposes the upper surface 210a of the substrate 210. Thereafter, a conductive material is filled in the inner opening Q2 by a deposition process to form a conductive connection structure 220. The conductive connection structure 220 may include tungsten (W), aluminum (Al), titanium nitride (TiN), tantalum nitride (TaN) or other suitable materials.

[0076] Please refer to Figure 2E , a plurality of upper openings 222 are formed by an etching process (e.g., a dry etching process). The upper openings 222 pass through the upper portion of the stacked structure S2. The upper openings 222, for example, pass through three conductive layers (i.e., the first top conductive layer CL2a, the second top conductive layer CL2b, and the third top conductive layer CL2c), but the present invention is not limited thereto. In some embodiments, the upper openings 222 may pass through more than three conductive layers.

[0077] Please refer to Figure 2F , a low dielectric constant material is filled into the upper opening 222 by a deposition process to form a shallow isolation structure 224 in the upper opening 222. In this way, the memory element 200 is formed. In the present embodiment, the shallow isolation structure 224 passes through three conductive layers (i.e., the first top conductive layer CL2a, the second top conductive layer CL2b, and the third top conductive layer CL2c), but the present invention is not limited thereto. In some embodiments, the shallow isolation structure 224 may pass through more than three conductive layers. The shallow isolation structure 224 includes a material with a dielectric constant less than 3.9. In some embodiments, the top surface 224t of the shallow isolation structure 224 may be coplanar with the top surface S2a of the stacked structure S2.

[0078] Figure 3 A cross-sectional view of a memory device 300 according to an embodiment of the present disclosure is shown. The method of forming the memory device 300 is similar to the memory device 200 , except for the material of the shallow isolation structure 324 .

[0079] Please refer to Figure 3 , after such Figure 2A to Figure 2E After the formation steps shown, an insulating material is filled into the upper opening 222 by a deposition process to form an oxide liner 324b and an air gap 324a covered by the oxide liner 324b in the upper opening 222. In the present embodiment, the shallow isolation structure 324 passes through three conductive layers (i.e., the first top conductive layer CL2a, the second top conductive layer CL2b, and the third top conductive layer CL2c), but the present invention is not limited thereto. In some embodiments, the shallow isolation structure 324 may pass through more than three conductive layers. In some embodiments, the top surface 324t of the shallow isolation structure 324 may be coplanar with the top surface S2a of the stacked structure S2.

[0080] FIG. 4A to FIG. 4F FIG. 4 is a cross-sectional view showing a method for forming a memory device 400 according to an embodiment of the present disclosure.

[0081] Please refer to Figure 4A A substrate 410 is provided, and a stacked body S4' is formed on the upper surface 410a of the substrate 410. The stacked body S4' includes a plurality of insulating layers IL4 and a plurality of sacrificial layers SL4 alternately stacked on the upper surface 410a of the substrate 410 in sequence (eg, by a deposition process).

[0082] In some embodiments, the substrate 410 may be a silicon substrate or other suitable substrates. The insulating layer IL4 may be formed of oxide, such as silicon dioxide. The sacrificial layer SL4 may be formed of silicon nitride (SiN).

[0083] Please refer to Figure 4B, a plurality of channel openings P4 are formed through (for example, along the Z direction) the stack body S4' and exposing the upper surface 410a of the substrate 410 by etching (for example, dry etching). Next, a storage material is formed on the stack body S4' and in these channel openings P4 by a deposition process. Next, a portion of the storage material located in the channel openings P4 is removed by an etching process to form a plurality of through holes V4 that expose the upper surface 410a of the substrate 410. Thereafter, a conductive material and an insulating material are filled in the through hole V4 to form a plurality of channel structures 412, a plurality of insulating pillars 411 and a storage layer 414. The channel structure 412 can be formed of doped or undoped polysilicon material. The storage layer 414 can be composed of a composite layer (i.e., an ONO layer) including a silicon oxide layer, a silicon nitride layer and a silicon oxide layer. The channel structure 412 passes through the stack body S4' and is electrically connected to the substrate 410. Each storage layer 414 surrounds each corresponding channel structure 412. Afterwards, a cap layer 416 covering the stack body S4' is formed by a deposition process. The cap layer 416 may be formed of an oxide, such as silicon dioxide.

[0084] Please refer to Figure 4C A plurality of vertical openings 418 are formed through the stack body S4 ′ and the cover layer 416 by an etching process (eg, a dry etching process). In the present embodiment, the vertical openings 418 expose the upper surface 410 a of the substrate 410 .

[0085] Please refer to Figure 4D , a pull back process is performed to remove the sacrificial layer SL4 through the vertical opening 418. The pull back process may be an isotropic etching (eg, wet etching), and may be a highly selective etching, such as selectively etching silicon nitride without etching silicon dioxide and polysilicon.

[0086] Thereafter, the positions where the sacrificial layer SL4 is removed are filled with a conductive material to form a conductive layer CL4 between the insulating layers IL4. Thus, a plurality of insulating layers IL4 and a plurality of conductive layers CL4 alternately stacked on the upper surface 410a and a cap layer 416 form a stacked structure S4. The conductive layer CL4 may include tungsten (W), aluminum (Al), titanium nitride (TiN), tantalum nitride (TaN) or other suitable materials.

[0087] Please refer to Figure 4E, an insulating material is filled in the vertical opening 418. Afterwards, a portion of the insulating material is removed to form an inner opening Q4. The inner opening Q4 passes through the stacked structure S4 and exposes the upper surface 410a of the substrate 410. Thereafter, a conductive material is filled in the inner opening Q4 by a deposition process to form a conductive connection structure 420. The conductive connection structure 420 may include tungsten (W), aluminum (Al), titanium nitride (TiN), tantalum nitride (TaN) or other suitable materials.

[0088] Thereafter, a plurality of upper openings 422 are formed by an etching process (e.g., a dry etching process). The upper openings 422 pass through the upper portion of the stacked structure S4. The upper openings 422, for example, pass through three conductive layers (i.e., the first top conductive layer CL4a, the second top conductive layer CL4b, and the third top conductive layer CL4c), but the present invention is not limited thereto. In some embodiments, the upper openings 422 may pass through more than three conductive layers.

[0089] Please refer to Figure 4F , a low dielectric constant material is filled into the upper opening 422 by a deposition process to form a shallow isolation structure 424 in the upper opening 422. In this way, the memory element 400 is formed. In the present embodiment, the shallow isolation structure 424 passes through three conductive layers (i.e., the first top conductive layer CL4a, the second top conductive layer CL4b, and the third top conductive layer CL4c), but the present invention is not limited thereto. In some embodiments, the shallow isolation structure 424 may pass through more than three conductive layers. The shallow isolation structure 424 includes a material having a dielectric constant less than 3.9. In some embodiments, the top surface 424t of the shallow isolation structure 424 may be coplanar with the top surface S4a of the stacked structure S4.

[0090] Figure 5 A cross-sectional view of a memory device 500 according to an embodiment of the present disclosure is shown. The method of forming the memory device 500 is similar to the memory device 400 , except for the material of the shallow isolation structure 524 .

[0091] Please refer to Figure 5 , after such Figure 4A to Figure 4E After the formation steps shown, an insulating material is filled into the upper opening 422 by a deposition process to form an oxide liner 524b and an air gap 524a covered by the oxide liner 524b in the upper opening 422. In the present embodiment, the shallow isolation structure 524 passes through three conductive layers (i.e., the first top conductive layer CL5a, the second top conductive layer CL5b, and the third top conductive layer CL5c), but the present invention is not limited thereto. In some embodiments, the shallow isolation structure 524 may pass through more than three conductive layers. In some embodiments, the top surface 524t of the shallow isolation structure 524 may be coplanar with the top surface S4a of the stacked structure S4.

[0092] The present disclosure provides a memory element and a manufacturing method thereof. The memory element of the present disclosure can be applied to a three-dimensional NAND gate memory element or a three-dimensional read-only memory.

[0093] According to one embodiment of the present disclosure, a memory element includes a substrate, a stacked structure, a plurality of channel structures, a plurality of storage layers, and a plurality of shallow isolation structures. The substrate has an upper surface. The stacked structure is located on the upper surface of the substrate, wherein the stacked structure includes a plurality of insulating layers and a plurality of conductive layers alternately stacked on the upper surface. The channel structure passes through a portion of the stacked structure and is electrically connected to the substrate. Each storage layer surrounds the corresponding channel structure. The shallow isolation structure extends from a top surface of the stacked structure toward the substrate, wherein the shallow isolation structure includes a substance having a dielectric constant less than 3.9.

[0094] Compared to the comparative example of the shallow isolation structure without the material of low dielectric constant, since the memory element of the present invention includes the shallow isolation structure, and the shallow isolation structure includes the material with dielectric constant less than 3.9, the capacitance value between the top conductive layers (serial selection lines) located on different sides (different sub-blocks) of the shallow isolation structure can be reduced, and the charging delay time of the top conductive layers (serial selection lines) of different sub-blocks can be reduced, so that the voltage of the top conductive layer (serial selection line) is more stable, so the top conductive layer (serial selection line) can have better electrical characteristics, so that the memory element can have better performance.

[0095] In summary, although the present invention has been disclosed as above by way of embodiments, it is not intended to limit the present invention. A person skilled in the art with common knowledge in the technical field to which the present invention belongs may make various modifications and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

[0096] The specific embodiments described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A memory element, characterized in that: include: A substrate (110) having an upper surface (110a); A stacked structure (S1) located on the upper surface of the substrate, wherein the stacked structure includes a plurality of insulating layers (IL1) and a plurality of conductive layers (CL1) alternately stacked on the upper surface; A plurality of channel structures (112) passing through a portion of the stacked structure and electrically connected to the substrate; A plurality of storage layers (114), the storage layers surrounding the corresponding channel structures; as well as A plurality of shallow isolation structures (124) extending from a top surface (S1a) of the stacked structure toward the substrate, wherein each of the shallow isolation structures comprises a material having a dielectric constant less than 3.9; Each of the shallow isolation structures passes through three or more conductive layers located on the upper portion of the stacked structure, and separates the three or more conductive layers on the upper portion of the stacked structure into two electrically independent serial selection lines.

2. The memory device of claim 1, wherein the substance is fluorine-doped silicon dioxide, carbon-doped oxide, porous silicon dioxide, spin-on organic polymer dielectric, spin-on silicon-based polymer dielectric, or air gap. 3 . The memory device as claimed in claim 1 , further comprising a plurality of conductive connection structures, the conductive connection structures passing through the stacked structure and electrically connected to the substrate.

4. The memory device as claimed in claim 3, wherein the conductive connection structures and the shallow isolation structures extend along a first direction respectively and are arranged along a second direction on the substrate, the first direction and the second direction are both parallel to the upper surface of the substrate, and the first direction is staggered with the second direction, In the second direction, the width of each shallow isolation structure is smaller than the width of each conductive connection structure, and in the normal direction of the upper surface of the substrate, the depth of each shallow isolation structure is smaller than the depth of each conductive connection structure. 5 . The memory device as claimed in claim 3 , wherein the conductive connection structures divide the memory device into a plurality of blocks, and the shallow isolation structures divide each of the blocks into a plurality of sub-blocks. 6 . The memory device as claimed in claim 3 , wherein there are two or more shallow isolation structures between two adjacent conductive connection structures.

7. The memory device as claimed in claim 1, wherein the shallow isolation structures extend along a first direction and are arranged along a second direction on the substrate, the first direction and the second direction are both parallel to the upper surface of the substrate, and there is a non-straight angle between the first direction and the second direction, In the second direction, the width of each shallow isolation structure is equal to or smaller than the width of each channel structure. 8 . The memory device as claimed in claim 1 , wherein the shallow isolation structures directly contact the corresponding conductive layers.