A TCL anti-aging sound insulation cotton

By arranging an anti-aging film on the surface of the sound-insulating cotton and combining a multi-layer structure internally, the deficiencies of the existing sound-insulating cotton materials in terms of environmental protection, flame retardancy and anti-aging properties are solved, the sound insulation effect and strength are significantly improved, and the requirements of modern society are satisfied. Higher requirements for sound insulation materials.

CN112743934BActive Publication Date: 2024-10-08HUBEI TIANYUN NOISE REDUCTION & ANTIVIBRATION NEW MATERIAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011593511.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-29
Publication Date
2024-10-08
Estimated Expiration
2040-12-29

AI Technical Summary

Technical Problem

Existing sound insulation cotton materials cannot meet the growing social needs in terms of environmental protection, decoration, flame retardancy and anti-aging properties, especially in automobile or home appliance interior materials. Traditional materials have limited low-frequency noise absorption effect and do not have Good flame retardant and safety properties.

Method used

A TCL anti-aging sound insulation cotton is designed. By setting an anti-aging film on the surface and using a multi-layered sound insulation structure combination internally, including a mixed fiber layer, a soft resin plate layer and an elastic layer, water-based elastic resin and graphene are used. Modified epoxy resin and other materials increase the anti-aging and sound insulation effect of sound insulation cotton.

Benefits of technology

It significantly improves the sound insulation effect and anti-aging performance of the sound insulation cotton, enhances its strength and service life, meets the requirements of environmental protection, flame retardancy, comfort and durability, and has good market potential value and application prospects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112743934B_ABST
    Figure CN112743934B_ABST
Patent Text Reader

Abstract

The invention relates to an anti-aging sound-insulating cotton, which comprises an anti-aging film on the surface, wherein the inner layer of the anti-aging film is provided with a mixed fiber layer, wherein the inner layer of the mixed fiber layer is provided with a soft resin board layer; the inner layer of the soft resin board layer is provided with a light metal mesh layer, wherein the inner layer of the light metal mesh layer is provided with an elastic layer; the inner layer of the elastic layer is provided with a foam plastic layer, wherein the interior of the foam plastic layer is provided with elastic reinforcing ribs; the anti-aging sound-insulating cotton designed by the invention improves the anti-aging effect of the sound-insulating cotton by coating the anti-aging film on the surface, and the interior is combined with sound insulation layers of different levels, structures and materials, thereby significantly improving the sound insulation effect of the sound-insulating cotton; through the coordination and cooperation of the internal metal mesh layer, the elastic layer and the reinforcing ribs, the strength of the sound-insulating cotton is improved from the side, and the structure and constituent materials of the sound-insulating cotton are strengthened as a whole, and the sound-insulating cotton has good market potential value and application prospects, and is practical and creative.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of sound insulation cotton materials, and in particular relates to a TCL anti-aging sound insulation cotton. Background Art

[0002] In today's society, noise pollution has become one of the major environmental pollution issues that has attracted worldwide attention after water pollution and air pollution. Using sound-absorbing and sound-insulating materials for sound insulation and silencing is a common means of controlling noise pollution. At present, the commonly used sound insulation cottons on the market include glass fiber sound insulation cotton, sponge, polyester fiber sound insulation cotton, etc. Glass fiber cotton is prone to cause skin itching and respiratory allergies, which is harmful to the human body and is not suitable for indoor use. Most sponges are closed-cell foam materials with limited sound absorption performance and are more suitable for use in the field of thermal insulation. The bandwidth of ordinary polyester fiber sound insulation cotton is relatively narrow, and it only has good absorption of medium and high frequency sounds, and has limited absorption effect on low frequency sounds. The sound insulation cotton used for automobile or home appliance interior materials not only needs good sound insulation performance, but also needs to meet the requirements of safety, flame retardancy, green environmental protection, comfort and durability.

[0003] On the one hand, with the increasing requirements of practical life and fire safety, people have higher and higher requirements for the flame retardancy of sound insulation cotton. At present, flame retardant technology has entered a new stage of development. In the future, the flame retardant technology of sound insulation materials is developing in the direction of high efficiency, economy and environmental protection. Since inorganic flame retardants have the advantages of low toxicity, good thermal stability, no precipitation, long-lasting flame retardant effect, no corrosive gas, low price, and small smoke emission, the application of inorganic flame retardants in various aspects is gradually replacing organic flame retardants. Therefore, the research on synthetic inorganic flame retardants is of great significance; however, since organic flame retardants are still in large quantities, the combination of inorganic flame retardants and organic flame retardants is a desirable transition method.

[0004] At present, the demand for sound insulation materials is growing rapidly, and traditional sound-absorbing materials can no longer meet people's higher requirements for environmental protection, decoration, flame retardancy and anti-aging. Therefore, researching, developing and applying new environmentally friendly sound-absorbing, flame retardant and anti-aging materials has become the direction of efforts. Summary of the invention

[0005] The purpose of the present invention is to provide an anti-aging film on the surface of the sound insulation cotton and to combine various levels of sound insulation structures inside, so as to improve the sound insulation effect, improve the surface anti-aging property of the sound insulation cotton and increase the service life of the sound insulation cotton.

[0006] To achieve the above object, the present invention provides the following technical solutions:

[0007] A TCL anti-aging sound insulation cotton, the sound insulation cotton comprises an anti-aging film on the surface, the edge of the anti-aging film is provided as a sound insulation cotton edge seal, the inner layer of the anti-aging film is provided with a mixed fiber layer, and the inner layer of the mixed fiber layer is provided with a soft resin board layer;

[0008] The anti-aging film contains the following components by weight percentage: 25-50% of water-based elastic resin, 15-25% of polycarbonate, 3-8% of composite anti-aging agent, 1-2% of dispersant, 15-20% of elastic powder, 5-13% of pigment and 10-15% of filler;

[0009] The mixed fiber layer contains the following components by weight percentage: 20-30% glass fiber, 15-25% asbestos fiber, 20-25% ceramic fiber, 10-15% carbon fiber, 20-35% nylon fiber and 5-15% filler;

[0010] The soft resin board layer contains the following components by weight percentage: 25-35% of water-based elastic resin, 15-25% of graphene-modified epoxy resin, 15-25% of ABS resin, 10-25% of natural rubber, 20-45% of solvent, 1-2% of dispersant, 3-6% of matting agent, 2-5% of curing agent, 1-3% of curing accelerator and 5-8% of filler, wherein the sum of the weight percentages of the various components is 1.

[0011] Preferably, the inner layer of the soft resin board layer is provided with a light metal mesh layer, and the inner layer of the light metal mesh layer is provided with an elastic layer.

[0012] Preferably, the inner layer of the elastic layer is provided with a foam plastic layer, and the interior of the foam plastic layer is provided with elastic reinforcing ribs.

[0013] Preferably, a plurality of vacuum sound insulation cavities are provided inside the resin board layer, and the vacuum sound insulation cavities are filled with sound insulation particles.

[0014] Preferably, a plurality of mutually intertwined sound insulation channels are arranged inside the elastic layer, and the sound insulation channels are not connected to each other.

[0015] Preferably, the elastic layer comprises the following combination of components in parts by weight: 30-45 parts of natural rubber, 20-30 parts of graphene-modified nitrile rubber, 10-15 parts of carbon fiber-modified styrene-butadiene rubber, 5-15 parts of modified nano-graphene, 3-9 parts of toughening agent, 2-8 parts of nano-white carbon black, 3-5 parts of nano-calcium carbonate, 1-3 parts of coupling agent, 2-4 parts of compatibilizer, 0.5-1.5 parts of mildewproof agent, 1-2 parts of antioxidant, 0.5-1.2 parts of anti-aging agent and 0.5-1 part of ultraviolet absorber.

[0016] Preferably, the lightweight metal mesh layer is woven from lightweight metal fibers, and the porosity of the lightweight metal mesh layer is 0.2-0.5; the lightweight metal mesh fibers constituting the lightweight metal mesh layer are hollow metal fibers, which are filled with elastic rubber.

[0017] As a preferred embodiment, the composite anti-aging agent is 2-hydroxy-4-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 A mixture of 2-hydroxy-4-n-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 The mass ratio is 1:10~15:13~18:15~20:16~25.

[0018] Preferably, the anti-aging film, the mixed fiber layer, the soft resin board layer, the light metal mesh layer and the elastic layer are symmetrically distributed on both sides of the foam plastic layer.

[0019] Preferably, the mixed fiber layer has the same thickness as the elastic layer and the foam plastic layer, the thickness of the lightweight metal mesh layer is 1 / 3 to 1 / 2 of the thickness of the mixed fiber layer; the thickness of the soft resin board layer is twice the thickness of the mixed fiber layer, and the thickness of the anti-aging film is 1 / 10 to 1 / 5 of the thickness of the mixed fiber layer.

[0020] Beneficial effects of the present invention: The TCL anti-aging sound insulation cotton designed by the present invention improves the anti-aging effect of the sound insulation cotton by coating the anti-aging film on the surface, and is internally combined with sound insulation layers of different levels, structures and materials, which can significantly improve the sound insulation effect of the sound insulation cotton. The coordination and cooperation of the internal metal mesh layer, elastic layer and reinforcing ribs improves the strength of the sound insulation cotton from the side, and the structure and constituent materials of the sound insulation cotton are strengthened as a whole. It has good market potential value and application prospects, and is practical and creative. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a schematic diagram of the overall structure of the TCL anti-aging sound insulation cotton of the present invention.

[0022] Figure 2 It is a schematic diagram of the partial structure of the TCL anti-aging sound insulation cotton of the present invention.

[0023] In the figure: 1. Anti-aging film; 2. Mixed fiber layer; 3. Soft resin board layer; 4. Lightweight metal mesh layer; 5. Elastic layer; 6. Foam plastic layer; 7. Vacuum sound insulation chamber; 8. Sound insulation particles; 9. Sound insulation channel; 10. Elastic reinforcement ribs. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0025] like Figure 1 , 2 As shown, a TCL anti-aging sound insulation cotton includes an anti-aging film 1 on the surface, the edge of the anti-aging film 1 is set as the sound insulation cotton edge sealing, the inner layer of the anti-aging film 1 is set with a mixed fiber layer 2, and the inner layer of the mixed fiber layer 2 is set with a soft resin board layer 3.

[0026] Furthermore, the anti-aging film 1 contains the following components by weight percentage: 50% of water-based elastic resin, 15% of polycarbonate, 4% of composite anti-aging agent, 1% of dispersant, 15% of elastic powder, 5% of pigment and 10% of filler;

[0027] Furthermore, the mixed fiber layer 2 contains the following components by weight percentage: 20% glass fiber, 15% asbestos fiber, 20% ceramic fiber, 10% carbon fiber, 30% nylon fiber and 5% filler;

[0028] Furthermore, the soft resin board layer 3 contains the following components by weight: 25% water-based elastic resin, 15% graphene-modified epoxy resin, 15% ABS resin, 10% natural rubber, 20% solvent, 2% dispersant, 3% matting agent, 3% curing agent, 2% curing accelerator and 5% filler.

[0029] Furthermore, a light metal mesh layer 4 is provided inside the soft resin plate layer 3 , and an elastic layer 5 is provided inside the light metal mesh layer 4 .

[0030] Furthermore, a foam plastic layer 6 is provided inside the elastic layer 5 , and elastic reinforcing ribs 10 are provided inside the foam plastic layer 6 .

[0031] Furthermore, a plurality of vacuum sound insulation cavities 7 are provided inside the resin plate layer 3 , and sound insulation particles 8 are filled inside the vacuum sound insulation cavities 7 .

[0032] Furthermore, a plurality of mutually intertwined sound insulation channels 9 are arranged inside the elastic layer 5 , and the sound insulation channels 9 are not connected to each other.

[0033] Furthermore, the elastic layer 5 includes the following combined components in parts by weight: 45 parts of natural rubber, 20 parts of graphene-modified nitrile rubber, 15 parts of carbon fiber-modified styrene-butadiene rubber, 5 parts of modified nano-graphene, 9 parts of toughening agent, 2 parts of nano-silica, 5 parts of nano-calcium carbonate, 1 part of coupling agent, 2 parts of compatibilizer, 0.5 parts of mildewproof agent, 1 part of antioxidant, 0.5 parts of anti-aging agent and 1 part of ultraviolet absorber.

[0034] Furthermore, the lightweight metal mesh layer 4 is woven from lightweight metal fibers, and the porosity of the lightweight metal mesh layer 4 is 0.5; the lightweight metal mesh fibers constituting the lightweight metal mesh layer 4 are hollow metal fibers, and elastic rubber is filled inside the fibers.

[0035] Furthermore, the composite anti-aging agent is 2-hydroxy-4-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 A mixture of 2-hydroxy-4-n-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 The mass ratio is 1:15:18:20:25.

[0036] Furthermore, the anti-aging film 1 , the mixed fiber layer 2 , the soft resin board layer 3 , the lightweight metal mesh layer 4 and the elastic layer 5 are symmetrically distributed on both sides of the foam plastic layer 6 .

[0037] Furthermore, the thickness of the mixed fiber layer 2 is the same as that of the elastic layer 5 and the foam plastic layer 6, the thickness of the lightweight metal mesh layer 4 is 1 / 2 of the thickness of the mixed fiber layer 2; the thickness of the soft resin board layer 3 is twice the thickness of the mixed fiber layer 2, and the thickness of the anti-aging film 1 is 1 / 5 of the thickness of the mixed fiber layer 2.

[0038] Example 2

[0039] The difference between this embodiment and embodiment 1 is that:

[0040] The anti-aging film 1 contains the following components by weight percentage: 25% of water-based elastic resin, 25% of polycarbonate, 8% of composite anti-aging agent, 2% of dispersant, 20% of elastic powder, 5% of pigment and 15% of filler;

[0041] The mixed fiber layer 2 contains the following components by weight: 20% glass fiber, 15% asbestos fiber, 25% ceramic fiber, 15% carbon fiber, 20% nylon fiber and 5% filler;

[0042] The soft resin plate layer 3 contains the following components by weight percentage: 25% of water-based elastic resin, 15% of graphene-modified epoxy resin, 17% of ABS resin, 10% of natural rubber, 20% of solvent, 2% of dispersant, 3% of matting agent, 2% of curing agent, 1% of curing accelerator and 5% of filler;

[0043] The elastic layer 5 includes the following components in parts by weight: 30 parts of natural rubber, 20 parts of graphene-modified nitrile rubber, 10 parts of carbon fiber-modified styrene-butadiene rubber, 15 parts of modified nanographene, 3 parts of toughening agent, 2 parts of nano-white carbon black, 3 parts of nano-calcium carbonate, 1 part of coupling agent, 2 parts of compatibilizer, 0.5 parts of mildewproof agent, 1 part of antioxidant, 1.2 parts of anti-aging agent and 0.5 parts of ultraviolet absorber;

[0044] The light metal mesh layer 4 is woven from light metal fibers, and the porosity of the light metal mesh layer 4 is 0.2; the light metal mesh fibers constituting the light metal mesh layer 4 are hollow metal fibers, and elastic rubber is filled inside the fibers;

[0045] The composite anti-aging agent is 2-hydroxy-4-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 A mixture of 2-hydroxy-4-n-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 The mass ratio is 1:10:13:15:16;

[0046] The thickness of the mixed fiber layer 2 is the same as that of the elastic layer 5 and the foam plastic layer 6; the thickness of the lightweight metal mesh layer 4 is 1 / 3 of the thickness of the mixed fiber layer 2; the thickness of the soft resin board layer 3 is twice the thickness of the mixed fiber layer 2; and the thickness of the anti-aging film 1 is 1 / 10 of the thickness of the mixed fiber layer 2.

[0047] Example 3

[0048] The difference between this embodiment and embodiment 1 is that:

[0049] The anti-aging film 1 contains the following components by weight percentage: 40% of water-based elastic resin, 20% of polycarbonate, 8% of composite anti-aging agent, 2% of dispersant, 15% of elastic powder, 5% of pigment and 10% of filler;

[0050] The mixed fiber layer 2 contains the following components by weight: 25% glass fiber, 20% asbestos fiber, 20% ceramic fiber, 10% carbon fiber, 20% nylon fiber and 5% filler;

[0051] The soft resin plate layer 3 contains the following components by weight percentage: 25% of water-based elastic resin, 18% of graphene-modified epoxy resin, 15% of ABS resin, 10% of natural rubber, 20% of solvent, 1% of dispersant, 3% of matting agent, 2% of curing agent, 1% of curing accelerator and 5% of filler;

[0052] The elastic layer 5 includes the following components in parts by weight: 35 parts of natural rubber, 25 parts of graphene-modified nitrile rubber, 12 parts of carbon fiber-modified styrene-butadiene rubber, 13 parts of modified nanographene, 4 parts of toughening agent, 5 parts of nano-white carbon black, 3 parts of nano-calcium carbonate, 2 parts of coupling agent, 2 parts of compatibilizer, 1 part of mildewproof agent, 1 part of antioxidant, 0.9 parts of anti-aging agent and 0.8 parts of ultraviolet absorber;

[0053] The light metal mesh layer 4 is woven from light metal fibers, and the porosity of the light metal mesh layer 4 is 0.3; the light metal mesh fibers constituting the light metal mesh layer 4 are hollow metal fibers, and elastic rubber is filled inside the fibers;

[0054] The composite anti-aging agent is 2-hydroxy-4-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 A mixture of 2-hydroxy-4-n-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 The mass ratio is 1:12:15:18:24;

[0055] The thickness of the mixed fiber layer 2 is the same as that of the elastic layer 5 and the foam plastic layer 6; the thickness of the lightweight metal mesh layer 4 is 1 / 3 of the thickness of the mixed fiber layer 2; the thickness of the soft resin board layer 3 is twice the thickness of the mixed fiber layer 2; and the thickness of the anti-aging film 1 is 1 / 8 of the thickness of the mixed fiber layer 2.

[0056] In the present invention, the TCL anti-aging sound insulation cotton designed by the present invention improves the anti-aging effect of the sound insulation cotton by coating the anti-aging film on the surface, and is internally combined with sound insulation layers of different levels, different structures and different materials, which can significantly improve the sound insulation effect of the sound insulation cotton. Through the coordination and cooperation of the internal metal mesh layer, elastic layer and reinforcing ribs, the strength of the sound insulation cotton is improved from the side, and the structure and constituent materials of the sound insulation cotton are strengthened as a whole. It has good market potential value and application prospects, and is practical and creative.

[0057] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A TCL anti-aging sound insulation cotton, Features: The sound insulation cotton comprises an anti-aging film (1) on the surface, the edge of the anti-aging film (1) is arranged as a sound insulation cotton edge seal, the inner layer of the anti-aging film (1) is arranged with a mixed fiber layer (2), and the inner layer of the mixed fiber layer (2) is arranged with a soft resin board layer (3); The inner layer of the soft resin plate layer (3) is provided with a light metal mesh layer (4), and the inner layer of the light metal mesh layer (4) is provided with an elastic layer (5); The anti-aging film (1) contains the following components by weight percentage: 25-50% of water-based elastic resin, 15-25% of polycarbonate, 3-8% of composite anti-aging agent, 1-2% of dispersant, 15-20% of elastic powder, 5-13% of pigment and 10-15% of filler; The mixed fiber layer (2) contains the following components by weight: 20-30% glass fiber, 15-25% asbestos fiber, 20-25% ceramic fiber, 10-15% carbon fiber, 20-35% nylon fiber and 5-15% filler; The soft resin plate layer (3) contains the following components by weight percentage: 25-35% of water-based elastic resin, 15-25% of graphene-modified epoxy resin, 15-25% of ABS resin, 10-25% of natural rubber, 20-45% of solvent, 1-2% of dispersant, 3-6% of matting agent, 2-5% of curing agent, 1-3% of curing accelerator and 5-8% of filler, wherein the sum of the weight percentages of the various components is 1; The elastic layer (5) comprises the following components in parts by weight: 30-45 parts of natural rubber, 20-30 parts of graphene-modified nitrile rubber, 10-15 parts of carbon fiber-modified styrene-butadiene rubber, 5-15 parts of modified nanographene, 3-9 parts of toughening agent, 2-8 parts of nano-white carbon black, 3-5 parts of nano-calcium carbonate, 1-3 parts of coupling agent, 2-4 parts of compatibilizer, 0.5-1.5 parts of mildewproof agent, 1-2 parts of antioxidant, 0.5-1.2 parts of anti-aging agent and 0.5-1 part of ultraviolet absorber; The composite anti-aging agent is 2-hydroxy-4-n-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 mixture of Among them, 2-hydroxy-4-octyloxybenzophenone, didodecyl thiodipropionate, β-(3,5-di-tert-butyl-4-hydroxyphenyl) propionate, γ-FeO(OH), CaTiO 3 The mass ratio is 1:10~15:13~18:15~20:16~25.

2. The TCL anti-aging sound insulation cotton according to claim 1, Features: The inner layer of the elastic layer (5) is provided with a foam plastic layer (6), and the interior of the foam plastic layer (6) is provided with elastic reinforcing ribs (10).

3. The TCL anti-aging sound insulation cotton according to claim 1, Features: A plurality of vacuum sound insulation cavities (7) are arranged inside the soft resin board layer (3), and sound insulation particles (8) are filled inside the vacuum sound insulation cavities (7).

4. The TCL anti-aging sound insulation cotton according to claim 2, Features: A plurality of mutually intertwined sound insulation channels (9) are arranged inside the elastic layer (5), and the sound insulation channels (9) are not connected to each other.

5. The TCL anti-aging sound insulation cotton according to claim 1, Features: The light metal mesh layer (4) is woven from light metal fibers, and the porosity of the light metal mesh layer (4) is 0.2 to 0.5; The light metal mesh fibers constituting the light metal mesh layer (4) are hollow metal fibers, the interior of which is filled with elastic rubber.

6. A TCL anti-aging sound insulation cotton according to claim 1 or 2, Features: The anti-aging film (1), the mixed fiber layer (2), the soft resin board layer (3), the light metal mesh layer (4) and the elastic layer (5) are symmetrically distributed on both sides of the foam plastic layer (6).

7. The TCL anti-aging sound insulation cotton according to claim 6, Features: The thickness of the mixed fiber layer (2) is the same as that of the elastic layer (5) and the foam plastic layer (6), and the thickness of the lightweight metal mesh layer (4) is 1 / 3 to 1 / 2 of the thickness of the mixed fiber layer (2); The thickness of the soft resin board layer (3) is twice the thickness of the mixed fiber layer (2), and the thickness of the anti-aging film (1) is 1 / 10 to 1 / 5 of the thickness of the mixed fiber layer (2).