Touch sensor and method of manufacturing the same
By forming dummy holes and contact holes on the electrode layer of the touch sensor, and using narrow-width conductive metal bridges, the visual recognition problem during the bridge formation process is solved, and a low-resistance and low-visibility touch sensor is achieved.
Patent Information
- Application Number
- CN202011175606.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-28
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2040-10-28
Smart Images

Figure CN112783361B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a touch sensor and a method for manufacturing the same, in particular, in an upper connection method (top bridge) in which a bridge is formed on the upper side, a bridge area can be visually identified due to selective etching during bridge formation, and the present invention relates to a touch sensor capable of preventing this problem. Background Art
[0002] A touch sensor of a smartphone or the like is an input device that receives a command by touch. According to the sensing method of the touch portion, the touch sensor includes a resistive type, a capacitive type, an ultrasonic type, an infrared type, etc. Recently, the capacitive type is mainly used for the touch sensor.
[0003] The capacitive type uses a transparent substrate with a conductive film formed on it. When a user touches the surface of the coated transparent substrate while a certain amount of current flows through the surface of the transparent substrate, the amount of current changes at the contact surface. The capacitive type detects this current change to detect whether it is touched.
[0004] The touch sensor includes a plurality of sensing units arranged on a transparent substrate along the X-axis and the Y-axis. The first array sensing unit and the second array sensing unit arranged along the X-axis direction and the Y-axis direction, respectively, may be connected to the first wiring portion and the second wiring portion, respectively, at the edge of the transparent substrate. The first wiring portion and the second wiring portion may extend along the side edge of the transparent substrate to be connected to the electrode pad portion at the lower edge of the transparent substrate. The electrode pad portion may be connected to a printed circuit board (FPCB, etc.) through an anisotropic conductive film (ACF) or the like. Thus, the electrode pad portion may transmit the touch signal of the sensing unit to the control unit (IC chip, etc.).
[0005] The touch sensor uses bridges to electrically connect the spaced apart second array sensing cells. There are two types of bridges: bottom bridges (connecting sensing cells on their underside) and top bridges.
[0006] However, as described in Korean Patent Registration No. 1217591 entitled "Capacitive Touch Sensor", when the above connection method forms a bridge, the conductive metal layer as a material constituting the bridge may be selectively etched. In this case, the transparent conductive layer (metal oxide, etc.) constituting the sensing unit may be etched together. Therefore, there may be a problem in visually recognizing the bridge area. Summary of the invention
[0007] Technical issues
[0008] The present invention is to solve such problems in the prior art, and an object of the present invention is to provide a touch sensor capable of solving the problem of visually recognizing a bridge area when the bridge is formed by the above connection method, and a method for manufacturing the same.
[0009] Problem Solution
[0010] The touch sensor of the present invention for achieving this purpose may include a base layer, an electrode layer, an insulating layer, a plurality of bridges, and the like.
[0011] The base layer may support an electrode layer or the like assembled thereon.
[0012] The electrode layer may include first array sensing units connected and arranged in a first direction on the base layer, and second array sensing units spaced apart from the first array sensing units and spaced apart in a second direction. The first sensing units and the second sensing units may be provided with dummy holes.
[0013] The insulating layer may be formed on the electrode layer. The insulating layer may be provided with contact holes connecting adjacent second array sensing units in the second direction.
[0014] A bridge may be formed on the contact hole and the insulating layer to electrically connect adjacent second array sensing units.
[0015] In the touch sensor of the present invention, the width of the bridge may be narrower than the width of the contact hole.
[0016] In the touch sensor of the present invention, the second array sensing unit may be provided with an etching hole formed by removing a region other than a bridge region in the contact hole. In this case, the passivation layer may fill the etching hole.
[0017] In the touch sensor of the present invention, the contact holes and the dummy holes may form the same pattern.
[0018] In the touch sensor of the present invention, the contact holes and the dummy holes may have the same shape, the same area, and the same interval.
[0019] In the touch sensor of the present invention, the bridge may be made of a conductive metal, and the electrode layer may be made of a transparent metal oxide.
[0020] The touch sensor of the present invention may further include a passivation layer formed on the insulating layer and the bridge and filling the etching hole.
[0021] The method for manufacturing a touch sensor of the present invention may include the following steps: forming an electrode layer on a base layer, the electrode layer having first array sensing units connected and arranged in a first direction, second array sensing units spaced apart from the first array sensing units and spaced apart in a second direction, and dummy holes in the first array sensing units and the second array sensing units except for a bridge contact area of the second array sensing units; forming an insulating layer on the electrode layer; forming a contact hole in a bridge contact area in the insulating layer; forming a conductive metal layer for a bridge to electrically connect the contact hole and an adjacent second array sensing unit on the insulating layer; and forming a bridge having a width narrower than that of the contact hole by etching the conductive metal layer.
[0022] In the method of manufacturing the touch sensor of the present invention, the step of forming the bridge may include etching the second array sensing unit in a region other than the bridge region in the contact hole.
[0023] The method of manufacturing a touch sensor of the present invention may further include the step of forming a passivation layer on the insulating layer, the bridge, and the etching holes of the second array sensing unit.
[0024] In the method of manufacturing the touch sensor of the present invention, the step of forming the dummy holes may include forming the dummy holes to have the same shape, the same area, and the same interval.
[0025] In the method of manufacturing the touch sensor of the present invention, the step of forming the contact holes may include forming the contact holes to have the same shape, the same area, and the same interval as the dummy holes.
[0026] Beneficial Effects
[0027] According to the touch sensor and the manufacturing method thereof having such a configuration of the present invention, a dummy hole having the same shape, area and pitch as the contact hole of the insulating layer can be formed in the electrode layer. Thus, the present invention can prevent or minimize the problem of visibility of the contact hole area caused by etching of the electrode layer during the bridge formation process.
[0028] According to the touch sensor and manufacturing method of the present invention, there is no need to worry about the visibility problem caused by etching of the electrode layer during the bridge formation process. Therefore, there is no obstacle in minimizing the width of the bridge within the tolerance range of the resistance. In addition, the bridge material can be selected to use a low-resistance metal. Therefore, a low-resistance touch sensor is easily realized.
[0029] In addition, according to the touch sensor and the manufacturing method of the present invention, there is no problem even when etching the electrode layer during the bridge forming process. Therefore, there is no limitation when selecting a selective etching solution for the bridge. Therefore, the bridge etching process can be easily and quickly performed by appropriately selecting an etching solution. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 is an assembled perspective view of a touch sensor according to the present invention.
[0031] Figure 2 is an exploded perspective view of a touch sensor according to the present invention.
[0032] Figure 3 is a plan view of a bridge region in a touch sensor according to the present invention.
[0033] Figure 4A and Figure 4B is a cross-sectional view of a bridge region in a touch sensor according to the present invention taken along lines AA′ and BB′.
[0034] FIG. 5A to FIG. 5E A method for manufacturing a touch sensor according to the present invention is shown. DETAILED DESCRIPTION
[0035] Hereinafter, the present invention will be described in detail with reference to the accompanying drawings.
[0036] Figure 1 and Figure 2 They are respectively an assembled perspective view and an exploded perspective view of a touch sensor according to the present invention.
[0037] like Figure 1 and Figure 2 As shown in FIG. 1 , the touch sensor according to the present invention may include a base layer 100 , an electrode layer 200 , an insulating layer 300 , a bridge 500 , a passivation layer 400 , and the like.
[0038] The base layer 100 is a base that supports the electrode layer 200 and the like combined thereon. The base layer 100 may generally be a base film. When the touch sensor is manufactured by a transfer method, the base layer 100 may be a separation layer and the like.
[0039] If the base film has good transparency, mechanical strength and thermal stability, it is not limited. Specific examples of the base film may include thermoplastic resins, for example, polyester resins such as polyethylene terephthalate, polyethylene isophthalate, polyethylene naphthalate and polybutylene terephthalate; cellulose resins such as diacetyl cellulose and triacetyl cellulose; polycarbonate resins; acrylic resins such as polymethyl (meth) acrylate and polyethyl (meth) acrylate; styrene resins such as polystyrene and acrylonitrile-styrene copolymers; polyolefin resins such as polyethylene, polypropylene, polyolefins having a cyclic structure or a norbornene structure, and ethylene-propylene copolymers; vinyl chloride resins; amide resins such as nylon and aromatic polyamides; imide resins; polyether sulfone resins; sulfone resins; polyether ether ketone resins; polyphenylene sulfide resins; vinyl alcohol resins; vinylidene chloride resins; vinyl butyral resins; allyl resins (allylate resins); polyoxymethylene resins; and epoxy resins. Moreover, a film composed of a blend of thermoplastic resins can be used as the base film. In addition, heat-curable or UV-curable resins such as (meth)acrylates, urethanes, acrylic urethanes, epoxy resins, and silicone resins can be used as the base film.
[0040] An organic polymer film can be used as a separation layer. For example, at least one selected from the group consisting of polyimide, polyvinyl alcohol, polyamic acid, polyamide, polyethylene, polystyrene, polynorbornene phenylmaleimide copolymer, polyazobenzene, polyphenylene phthalamide, polyester, polymethyl methacrylate, polyarylate, cinnamate polymer, coumarin polymer, phthalimide polymer, chalcone polymer and aromatic acetylene polymer can be used as a separation layer.
[0041] The electrode layer 200 is used to sense a touch signal and may be formed on the base layer 100. The electrode layer 200 may include first array sensing units 210 connected and arranged in a first direction, and second array sensing units 220 spaced apart from the first array sensing units 210 and spaced apart in a second direction.
[0042] The first array sensing unit 210 and the second array sensing unit 220 may be spaced apart in the form of islands. The second array sensing units 220 spaced apart from each other may be electrically connected through a bridge 500 to be described later.
[0043] The first array sensing unit 210 and the second array sensing unit 220 may be provided with dummy holes H1. The dummy holes H1 may be formed to have the same pattern, i.e., the same shape, area, and spacing. The dummy holes H1 may be configured in various shapes, such as polygons (such as triangles, squares, and pentagons) or curved shapes (such as circles and ellipses). The dummy holes H1 may be formed to have the same pattern, i.e., the same shape, area, and spacing as the contact holes H2 of the insulating layer 300 to be described later. Thus, the visibility of the contact hole H2 region may be prevented or minimized when etching the electrode layer 200 during the process of forming the bridge 500.
[0044] The electrode layer 200 may have a structure in which a transparent metal oxide, a thin film metal, and a transparent metal oxide are sequentially stacked. In this case, the transparent metal oxide may have a thickness of 10 to 60 nm, and the thin film metal may have a thickness of 5 to 20 nm. The electrode layer 200 may have a structure in which a thin film metal and a transparent metal oxide are sequentially stacked. In this case, the thin film metal may have a thickness of 50 to 300 nm, and the transparent metal oxide may have a thickness of 5 to 50 nm. Alternatively, the electrode layer 200 may be formed only of a thin film metal. In this case, the thin film metal may have a thickness of 50 to 300 nm.
[0045] In the electrode layer 200, gold (Au), silver (Ag), copper (Cu), molybdenum (Mo), aluminum (Al), palladium (Pd), neodymium (Nd), silver-palladium-copper alloy (APC), etc. can be used as metal. In the electrode layer 200, metal oxide can be used. The metal oxide can be indium tin oxide (ITO), indium zinc oxide (IZO), indium zinc tin oxide (IZTO), aluminum zinc oxide (AZO), gallium zinc oxide (GZO), fluorine tin oxide (FTO), zinc oxide (ZnO), indium tin oxide-silver-indium tin oxide (ITO-Ag-ITO), indium zinc oxide-silver-indium zinc oxide (IZO-Ag-IZO), indium zinc tin oxide-silver-indium zinc tin oxide (IZTO-Ag-IZTO), aluminum zinc oxide-silver-aluminum zinc oxide (AZO-Ag-AZO), etc.
[0046] The insulating layer 300 may be formed on the electrode layer 200 while filling the dummy holes H1 and the spaces between the first array sensing units 210 and the second array sensing units 220 .
[0047] The insulating layer 300 may have a plurality of contact holes H2 for connecting adjacent second array sensing units 220 in the second direction. One contact hole H2 may be formed at each end of the second array sensing unit 220 in the second direction. The contact hole H2 is generally configured as a square, but the shape is not limited thereto, and shapes such as a pentagon, a circle, etc. are possible. The shape, area, and spacing of the contact hole H2 may be a criterion for determining the shape, area, and spacing of the dummy hole H1 formed in the electrode layer 200.
[0048] The insulating layer 300 may be formed of a curable prepolymer, a curable polymer, or a plastic polymer.
[0049] The bridge 500 electrically connects adjacent second array sensing units 220 in the second direction, and may be formed inside the contact hole H2 and on a portion of the upper surface of the insulating layer 300 .
[0050] The length of the bridge 500 may be at least equal to the distance between the contact holes H2. The width of the bridge 500 may be less than the width of the contact holes H2. Thus, it may be desirable to prevent or minimize visibility of the bridge 500 region.
[0051] The bridge 500 may be made of a conductive metal oxide, but it is preferably made of a conductive metal to achieve a narrow width and low resistance. Silver (Ag), gold (Au), copper (Cu), aluminum (Al), platinum (Pt), palladium (Pd), chromium (Cr), titanium (Ti), tungsten (W), niobium (Nb), tantalum (Ta), vanadium (V), iron (Fe), manganese (Mn), cobalt (Co), nickel (Ni), zinc (Zn), molybdenum (Mo), calcium (Ca) or its alloy (e.g., silver-palladium-copper (APC)) may be used as a conductive metal. These may be used alone or in combination of two or more. The bridge 500 may also have a covering layer on the conductive metal. The covering layer may be made of a transparent conductive oxide such as indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO), indium zinc tin oxide (IZTO), and cadmium tin oxide (CTO).
[0052] The passivation layer 400 may be formed on the insulating layer 300 and the bridge 500. The width of the bridge 500 may be narrower than the width of the contact hole H2. Thus, when a portion of the second array sensing unit 220 is removed by etching, the passivation layer 400 may fill the etched region of the second array sensing unit 220. The passivation layer 400 may be made of an organic film or the like.
[0053] Figure 3 is a plan view of a bridge region in a touch sensor according to the present invention. Figure 4A and Figure 4B is a cross-sectional view of a bridge region in a touch sensor according to the present invention taken along lines AA′ and BB′.
[0054] like Figure 3 As shown, the bridge 500 may electrically connect the adjacent second array sensing units 220. At this time, the bridge 500 may be formed as a so-called thin line bridge having a width narrower than that of the contact hole H2.
[0055] like Figure 4A As shown, in the stacked structure of the touch sensor, the insulating layer 300 is formed on the upper surface of the electrode layer 200. The bridge 500 may penetrate the insulating layer 300 to connect the second array sensing unit 220. The passivation layer 400 may be formed on the upper surface of the insulating layer 300 and the bridge 500 to protect the bridge 500. Figure 4A As shown, dummy holes H1 (which are spaced apart at the same distance as the distance between the contact holes H2) are formed in the second array sensing unit 220 along the direction in which the contact holes H2 are arranged (ie, along the second direction).
[0056] like Figure 4B As shown, in the second array sensing unit 220, the region other than the bridge 500 region is removed from the contact hole H2 region to form an etching hole H3. The passivation layer 400 protecting the bridge 500 may fill the etching hole H3 and the contact hole H2. Figure 4B In the embodiment, dummy holes H1 (which are spaced apart at the same distance as the distance between the contact holes H2) are formed in the first array sensing unit 210 in a direction perpendicular to the arrangement direction of the contact holes H2 (ie, in the first direction).
[0057] FIG. 5A to FIG. 5E A method for manufacturing a touch sensor according to the present invention is shown.
[0058] In the method for manufacturing a touch sensor according to the present invention, Figure 5A As shown, a transparent conductive layer (such as metal oxide) is first formed on the base layer 100, and then the electrode layer 200 may be formed by a method such as photolithography. The electrode layer 200 may be formed by coating, stamping, etc. The electrode layer 200 includes a first array sensing unit 210 connected and arranged in a first direction, and a second array sensing unit 220 spaced apart from the first array sensing unit 210 and spaced apart in a second direction.
[0059] like Figure 5A As shown, the electrode layer 200 may include dummy holes H1 in the first array sensing unit 210 and the second array sensing unit 220 except for the contact area of the bridge 500 of the second array sensing unit 220. The dummy holes H1 may be formed and arranged in the same form as the shape, area, and pitch of the contact holes H2 to be formed in the insulating layer 300 in a subsequent process.
[0060] like Figure 5B As shown, the insulating layer 300 may be formed on the electrode layer 200. The insulating layer 300 may fill the dummy hole H1 and the space between the first array sensing unit 210 and the second array sensing unit 220 and be formed thereon.
[0061] like Figure 5C As shown, a contact hole H2 may be formed in the insulating layer 300. The contact hole H2 may open a contact region of an adjacent second array sensing unit 220. The contact hole H2 may be formed as follows: Figure 5C The contact holes H2 may be formed into a rectangular shape in the step, or may be formed into other shapes, such as a circle. Here, the shape, area, and spacing of the contact holes H2 may become the standard of the pattern of the dummy holes H1 in the electrode layer 200. Therefore, the contact holes H2 in this step need to be formed to have the same Figure 5A The pattern of the dummy holes H1 formed in the embodiment is the same as the pattern (shape, area, pitch, etc.).
[0062] like Figure 5D As shown, a conductive metal layer 510 for forming a bridge 500 may be formed inside the contact hole H2 and on the insulating layer 300 in the contact hole H2 region. The conductive metal layer 510 may be formed of only a conductive metal having a low resistance, such as gold (Au), silver (Ag), copper (Cu), molybdenum (Mo), aluminum (Al), palladium (Pd), neodymium (Nd), silver-palladium-copper alloy (APC), etc., or a capping layer made of a transparent conductive oxide such as indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO), indium zinc tin oxide (IZTO), cadmium tin oxide (CTO), etc. may be further formed on top of the conductive metal.
[0063] like Figure 5E As shown, the bridge 500 having a width narrower than that of the contact hole H2 may be formed by etching the conductive metal layer 510. At this time, the second array sensing unit 220 except for the bridge 500 region in the contact hole H2 may be etched and removed together during the etching process of the conductive metal layer 510. Therefore, an etching hole H3 may be formed in the second array sensing unit 220.
[0064] Thereafter, a passivation layer 400 may be formed on the insulating layer 300 and the bridge 500. At this time, the passivation layer 400 may fill the contact hole H2 of the insulating layer 300 and the etching hole H3 of the second array sensing unit 220. The passivation layer 400 may be formed by evaporation, sputtering, or the like.
[0065] Above, the present invention has been described by embodiments, which are intended to illustrate the present invention. Those skilled in the art will be able to change or modify these embodiments in other forms. However, since the scope of the present invention is limited by the following claims, these changes or modifications may be interpreted as being included within the scope of the present invention.
[0066] [Description of Reference Numerals]
[0067] 100: base layer 200: electrode layer
[0068] 210: first array sensing unit 220: second array sensing unit
[0069] 300: Insulation layer 400: Passivation layer
[0070] 500: bridge 510: conductive metal layer
[0071] H1: dummy hole H2: contact hole
[0072] H3: Etched holes
Claims
1. A touch sensor, include: base layer; an electrode layer formed on the base layer and comprising first array sensing units connected and arranged along a first direction, and second array sensing units spaced apart from the first array sensing units and spaced apart from each other in a second direction, wherein dummy holes are provided in areas of the first array sensing units and the second array sensing units except for a bridge member contact area of the second array sensing units; an insulating layer, the insulating layer being formed on the electrode layer and being provided with a contact hole for connecting adjacent second array sensing units in the second direction in a region where the bridge member contacts the region; as well as a bridge formed on the contact hole and the insulating layer to electrically connect adjacent second array sensing units, The width of the bridge is narrower than the width of the contact hole, and the second array sensing unit is provided with an etching hole formed by removing an area other than an area where the bridge is located from an area where the contact hole of the second array sensing unit is located. 2 . The touch sensor according to claim 1 , wherein the contact holes and the dummy holes form the same pattern. 3 . The touch sensor according to claim 2 , wherein the contact hole and the dummy hole have the same shape, the same area, and the same interval. 4 . The touch sensor of claim 1 , further comprising a passivation layer formed on the insulating layer and the bridge and filling the contact hole and the etching hole.
5. The touch sensor according to any one of claims 1 to 4, in: The bridge member is made of a conductive metal; and The electrode layer is made of transparent metal oxide.
6. A method for manufacturing a touch sensor, the method The following steps are involved: forming an electrode layer on the base layer, the electrode layer having first array sensing units connected and arranged in a first direction, second array sensing units spaced apart from the first array sensing units and spaced apart from each other in a second direction, and dummy holes formed in regions of the first array sensing units and the second array sensing units except for a bridge contact region of the second array sensing units; forming an insulating layer on the electrode layer; forming a contact hole in the insulating layer in a region where the bridge contact region is located; forming a conductive metal layer for a bridge in the contact hole and on the insulating layer to electrically connect adjacent second array sensing units; forming the bridge having a width narrower than a width of the contact hole by etching the conductive metal layer, The step of forming the bridge comprises etching a region other than a region where the bridge is located in the region where the contact hole of the second array sensing unit is located to form an etching hole. 7 . The method of manufacturing a touch sensor according to claim 6 , further comprising the step of forming a passivation layer on the insulating layer and the bridge, wherein the passivation layer fills the contact hole and the etching hole. 8 . The method of manufacturing a touch sensor according to claim 6 , wherein the step of forming the dummy holes comprises forming the dummy holes to have the same shape, the same area, and the same interval. 9 . The method of manufacturing a touch sensor according to claim 8 , wherein the step of forming the contact holes comprises forming the contact holes to have the same shape, the same area, and the same interval as the dummy holes.
Citation Information
Patent Citations
Capacitive touch sensor
KR101217591B1
Touch screen panel including touch sensor
CN105760010A
Touch screen panel
CN106970724A
High-performance touch sensor and manufacturing method thereof
CN108509096A
Touch sensor and display device including the same
KR1020180097337A