Method and device for connecting lamination sections into a lamination stack

By using activator application and drying technology in lamination manufacturing, the quality and separation process of the adhesive layer are optimized, and the problem of long time spent on hot melt adhesive curing is solved, achieving efficient and accurate lamination connection and Improved stability.

CN112913127BActive Publication Date: 2024-11-26VOESTALPINE AUTOMOTIVE COMPONENTS DETTINGEN GMBH & CO KG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980059261.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-09-10
Filing Date
2019-09-10
Publication Date
2024-11-26
Estimated Expiration
2039-09-10

AI Technical Summary

Technical Problem

In the prior art, when manufacturing laminates, especially in the curing process of hot melt adhesive, there are problems of high time and energy consumption, and it is difficult to achieve uniform tackifier application and thickness control, which affects the quality of laminates.

Method used

After drying the adhesive layer with a fluid application device containing an activator, the laminated sheet belt is continuously conveyed to the separation device, and the laminated sheet parts are separated and laminated by clock control, and the adhesion is improved by using the two-stage cured epoxy resin system and filler. Stability and durability of agents.

Benefits of technology

The quality and uniformity of the adhesive layer are optimized, the connection accuracy and production efficiency of the laminated set are improved, the curing time and energy consumption are reduced, and the stability and performance of the laminated set are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112913127B_ABST
    Figure CN112913127B_ABST
Patent Text Reader

Abstract

The invention relates to a method and a device for connecting laminated parts (40) to form a laminated stack (46), wherein a laminated strip (12) having a curable polymer adhesive layer on its upper side (17) and / or lower side (18) is continuously transported through an application device (15, 15'), in which a fluid (16, 16') containing an activator is applied to the adhesive layer, the applied fluid (16, 16') is dried, the laminated strip (12) coated with the dried activator is continuously fed to a strip storage (20), the laminated strip (12) is fed from the strip storage (20) to a clocked separation device (30), in which laminated parts (40, 41, 42) are separated from the laminated strip (12) and stacked one above the other, and the separated and stacked laminated parts (40) are connected to one another to form a laminated stack (46) by means of the adhesive layer coated with the activator. The invention also relates to a laminated stack produced according to the method.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method and a device for connecting laminated parts to form a laminated core, and to a laminated core produced accordingly. Background Art

[0002] For example, a stack of laminated sheets made of interconnected laminated parts, in particular thin laminated sheets, is used as a magnetic core for the rotor and / or stator of an electric machine such as an electric motor instead of a conventional solid iron core. The stack of laminated sheets of such a magnetic core is made of a number of very thin electrical steel sheets. The electrical steel sheets are made of special alloys that have excellent properties in terms of conducting and enhancing magnetic fields. In the stack of laminated sheets, the individual thin laminated sheets are insulated from each other. These magnetic cores formed by the stack of laminated sheets are among the most important components of electric motors, which influence the efficiency of the electric motor when converting electrical energy into kinetic energy. The composition and stress-freeness of the laminated sheets, the value of their resistance and the integrity of the insulation are important influencing factors. These influencing factors are mainly determined by the method, in particular the way in which the laminated sheets are connected to each other in a planar or point-like manner, and the processing quality, such as stamping burrs.

[0003] The joining of thin laminations to form a stack is referred to in electrical engineering as "grouping". A stack is an ordered accumulation of a number of laminations which are initially movable relative to one another and which are connected to one another. The laminations are connected to form a stack, for example, by screwing or by means of clamps placed externally on the stack. Such connections allow the connection to be released, but the efficiency of the electric machine is usually adversely affected by such connecting means, for example by electrical short circuits or disturbed magnetic fields in the region of the connecting means.

[0004] Another known connection method is welding. In this case, the laminations are connected thermally and materially. The stamped and stacked laminations are clamped into the device and joined at the outer radius by a plurality of welds oriented orthogonally to the lamination plane. However, welding damages the laminations and their insulation and can lead to increased eddy current losses or influence the magnetic field. Although the freedom of design is hardly limited by the welds, the stack produced in this way cannot be disassembled again without being destroyed.

[0005] As a further connection method, so-called punching groups are known. In punching groups, electrical steel sheets are punched out of the raw material in one machine stroke, placed on a stack and connected to the stack. During punching and / or during placement or during connection, mechanical connections are produced in the electrical steel sheets, which interact with the connections of adjacent electrical steel sheets. These connections are elevations, also called bumps or granular structures, which are impressed into the electrical steel sheets. Since the insulating coating can be damaged in the deformed area, short circuits cannot be ruled out. In addition, the connection is structurally limited and the magnetic field is influenced by the local connection elements.

[0006] In addition, it is known to use adhesive as connecting device. In this method known as bonding group, hot-melt adhesive paint that can be thermoset is mostly used, with which electrical steel sheet is coated. Usually, hot-melt adhesive paint is utilized to coat raw material (approximate continuous lamination band). After separating each thin slice from the lamination band coated with hot-melt adhesive, thin slices are aligned with each other, stacked up and placed, and therefore form a stack. Subsequently, the stack of the lamination that has not yet been connected is heated to the reaction temperature of the hot-melt adhesive for a specific time period, typically 30 to 150 minutes. The reaction temperature is generally 150 to 250 degrees Celsius. During the thermal effect, the stack is loaded with a pressure of 2 to 6 Newtons per square millimeter by a clamping device. It is followed by a cooling stage that lasts up to 60 minutes. Although the complete and permanent connection of each thin slice can not damage the metal structure or the insulating layer owing to the use of hot-melt adhesive, the baking and cooling process are very time-consuming, and therefore it is difficult to be integrated into the continuous batch production.

[0007] This disadvantage is overcome by a nearly continuous method for producing a laminated stack, for example as described in the international patent application WO 2014 / 089593 A1, in which individual laminated parts or thin laminates are separated from a laminated strip at least partially coated with a curable polymer adhesive layer, stacked to form a laminated stack and connected to one another in a material-locking manner under pressure. In this method, an electrical steel strip pre-coated with a thermosetting hot-melt adhesive varnish is unwound from a coil, fed to a punching device, thin laminates are punched out of it and stacked to form a thin laminated stack with the adhesive-coated sides facing each other. Under the pressure of the upper tool of the punching device, the adhesive-coated surfaces facing each other establish a material-locking connection.

[0008] In order to reduce the time and energy consumption required for the curing of hot melt adhesives when manufacturing a laminated stack, it is proposed in the international patent application WO 2014 / 089593 A1 as mentioned above that a mixture consisting of water and a thermoplastic and / or cross-linkable tackifier such as polyvinyl alcohol is applied before punching out a laminated portion or a thin laminate. According to WO 2014 / 089593 A1, the mixture can also contain a water-soluble reaction accelerator such as 2-methylimidazole to improve the chemical reaction between the hot melt adhesive and the tackifier. Since the application of the tackifier mixture is carried out via a spraying device directly arranged in front of the punching tool in the method of WO 2014 / 089593 A1, a drying device is also arranged between the flushing device and the punching tool, and the drying device dries the applied mixture to prevent the belt conveyor or the punching tool from being contaminated by the aqueous tackifier mixture. In the stamping device itself, there is an activation device for conveying water vapor to the hot-melt adhesive lacquer / adhesion promoter coating, as well as a heating device for thermal activation. In contrast to the conventional method of bonding laminated stacks, thin laminates are punched out in a stamping tool, which are then usually manually stacked into stacks, extruded and cured in a separate oven. The method described in WO2014 / 089593 A1 enables nearly continuous production of electrical laminated stacks, wherein a continuous electrical tape is unwound from a coil and conveyed to a stamping device, and the cured electrical laminated stack is ejected from the stamping tool. Nevertheless, the method is carried out in a clock-controlled manner, because the electrical steel sheet tape stays in the stamping device and is transported further in a clock-controlled manner. However, it is difficult to apply the adhesive mixture with the required uniformity due to the clock-controlled transport of the tape. Summary of the invention

[0009] The object of the present invention is therefore to improve the method described in WO 2014 / 089593 A1 in such a way that the quality of the auxiliary coating applied before the punching process is improved, in particular with regard to the layer thickness and homogeneity of the coating.

[0010] This object is achieved by the method of claim 1. Advantageous developments of the method according to the invention are the subject matter of the dependent claims.

[0011] The invention therefore relates to a method for connecting laminated parts to form a laminated stack, wherein a laminated strip having a curable polymer adhesive layer on the upper side and / or the lower side is continuously transported through an application device, in which a fluid containing an activator is applied to the adhesive layer, the applied fluid is then dried, and the laminated strip coated with the dried activator is then continuously conveyed to a strip storage. The laminated strip is then conveyed from the strip storage to a clocked separation device, in which the laminated parts are separated from the laminated strip and stacked one above the other. Finally, the separated and stacked laminated parts are connected to one another to form a laminated stack by means of an adhesive layer coated with an activator located between the individual laminated parts.

[0012] According to the invention, therefore, it is proposed that a tape store is provided between the application of the fluid containing the activator for the polymer adhesive layer and the separating device in which the laminate parts are separated from the laminate web, so that before the tape store, in particular during the application of the fluid containing the activator, the laminate web can be transported continuously, while after the tape store, a clocked transport in the clock cycle of the separating device can be achieved. Due to the continuous transport of the laminate web through the application device, the quality of the layer of the fluid containing the activator can be optimized, since it is easier to apply a uniform and uniform thickness in continuous operation than in clocked operation. At the same time, the laminate parts can be separated with high precision, since in the region of the separating device, a clocked transport of the laminate web in the clock cycle of the separating device itself can be achieved.

[0013] The laminated strip used in the method according to the invention is preferably an electrical steel sheet, typically made of an iron-silicon alloy, which can be made into a non-grain-oriented laminate or a grain-oriented laminate. Non-grain-oriented electrical steel sheets are mainly used in rotating machines, such as electric motors, due to their isotropic magnetic properties.

[0014] The polymer adhesive layer that can be cured typically relates to the layer that is made of the hot-melt adhesive paint that can be heat-set, as described in European patent application EP 0 008 811 A1. Such material is also known by the name of "baking varnish". Some baking varnishes present thermoplastic characteristics, that is to say they can soften when heated, so that baking varnish can be bonded in a heated state, and solidify when cooled without chemical changes. Such thermoplastic synthetic resins are for example based on polyvinyl butyral, polyamide or polyester, but they have the following disadvantages: when the temperature rises in operation, the bonding effect can be reduced again. Other hot-melt adhesives that can be heat-set (it is also referred to as reactive hot-melt adhesives) can be hardened by chemical crosslinking when heating exceeds the plastic state. This hardening is irreversible, so that even when heated in operation, the stability of the laminated stack made with this hot-melt adhesive is still maintained. Preferred reactive hot-melt adhesives in the method of the present invention belong to epoxy resin systems. Such epoxy resin systems usually consist of a resin component and a hardener component, the term "epoxy resin" being used both for the predominantly liquid resin component and for the solid, crosslinked reaction product of resin and hardener.

[0015] Preferably, in the method according to the invention, a laminate tape is used, which is coated with a two-stage cured epoxy resin system, particularly preferably a bisphenol-based epoxy resin system with a suitable curing agent, such as a bisphenol-A-epichlorohydrin resin system with dicyandiamide as a curing agent. In the case of using a two-stage cured epoxy resin system, when the coated laminate tape is produced, the baking varnish layer is only partially crosslinked, so that the baking varnish layer is in a stable, flexible and dry but still reactive state at room temperature. This state of the resin system is called the B stage. Therefore, in the method according to the invention, preferably a laminate tape is used as the starting material, wherein the curable polymer adhesive layer (i.e., the baking varnish layer) is in this B state. Typically, the partially crosslinked baking varnish layer has a thickness of several microns. By transmitting heat, the baking varnish layer in the B state can be further reacted and converted into a completely crosslinked C state. In the method according to the invention, this occurs in the last step of connecting the upper and lower stacked laminate parts into a laminate stack.

[0016] The laminated strip can be coated with baking varnish on its upper side or lower side or on both sides. The upper side and lower side refer here to the transport of the horizontally extending strip into the separating device. If baking varnish layers are provided on both the upper side and the lower side, the thickness and degree of crosslinking of the layers can be different. When the separating device is operated with a punching tool arranged above the strip, the layer on the upper side of the strip can be designed to be thinner and more strongly crosslinked than on the lower side in order to minimize contamination of the punching tool. The typical layer thickness of the baking varnish on the more strongly pre-crosslinked upper side is then in the range of 1 to 5 μm, and the typical layer thickness on the less strongly pre-crosslinked lower side is in the range of 2 to 10 μm.

[0017] Advantageously, the baking varnish layer used in the method according to the invention contains a filler for improving the storage stability of the electrical tape coated with the curable baking varnish and for improving the durability of the baking varnish layer cured after the lamination stack is manufactured. Baking varnishes with suitable fillers are described, for example, in the international patent application WO 2016 / 151129 A1. Thus, for example, metal carbonates, metal sulfates, metal sulfites, metal silicates or metal phosphates or mixtures thereof can be used as fillers. Typically, such baking varnishes include 74 to 85 volume percent epoxy resin, 6 to 10 volume percent curing agent and 5 to 20 volume percent filler.

[0018] In this context, an activator is understood to be a substance which facilitates the curing reaction of the curable polymer adhesive layer, because the activator reduces the temperature at which curing occurs and / or accelerates the curing reaction, for example, the chemical crosslinking of the polymer adhesive layer. Suitable activators for epoxy resin systems are, for example, tertiary amines or imidazoles.

[0019] According to a preferred embodiment of the method of the present invention, the activator is an aqueous solution of imidazole as an active component, especially an aqueous solution of 2-ethyl-4-methylimidazole. Surprisingly, it is found that the mixture applied does not have to include a thermoplastic or cross-linkable tackifier as proposed in WO 2014 / 089593 A1 for accelerating the connection of the laminated parts during curing. In a particularly preferred embodiment, the liquid activator solution comprises 2 to 10 weight percents of 2-ethyl-4-methylimidazole, 80 to 90 weight percents of water, 0 to 15 weight percents of an organic solvent, such as 2-methoxypropanol and 0 to 2 weight percents of an additive, such as Ligaphob N90 (Ligaphob N90 is a sodium soap of industrial oleic acid, manufactured by Peter Greven GmbH & Co. KG located in Bad Münstereifel, Germany).

[0020] Particularly preferably, in the process according to the invention, a filler-containing bisphenol-A-epichlorohydrin resin system is used as baking varnish and 2-ethyl-4-methylimidazole is used as activator.

[0021] In the method according to the invention, a wide variety of devices can be used as tape storage. In its broadest form, the term tape storage includes continuous tape storage and discontinuous tape storage. The terms "continuous tape storage" and "discontinuous tape storage" refer here to the operating mode of the tape storage: the continuously operating tape storage continuously receives the laminated tape and simultaneously delivers it in a clocked manner. In the case of continuous reception and continuous delivery, the tape speed at the input and output of the tape storage varies within a certain period of time within the capacity of the tape storage. Clocked delivery is therefore a special case of a continuous tape storage, in which the tape can even be stopped at the output side of the tape storage, while the tape is still continuously conveyed on the input side. In contrast, a discontinuously operating tape storage is a tape storage in which the tape reception and the tape delivery are separated at least in time, but possibly also in place, i.e. at least during the preferably continuous delivery of the tape to the tape storage, the tape is not delivered from the tape storage, and during the clocked delivery of the tape, the tape is not received into the tape storage.

[0022] As mentioned above, laminated strips coated with partially crosslinked baking varnish (B-state) have been proven to be storage-stable, so that coated laminated strips can already be produced in steel mills. When producing laminated strips coated with partially crosslinked baking varnish, the application of activators cannot be carried out yet, because the activators will greatly reduce the storage stability of the baking varnish and cause the baking varnish to gradually solidify even at low storage temperatures. Since the production of the laminated stack is usually separated from the production of the laminated strip itself in time and place, the laminated strip coated with partially crosslinked baking varnish is typically provided in the form of a coil and auxiliary agents such as adhesion promoters and reaction accelerators described in WO 2014 / 089593 A1 are applied only shortly before the laminated strip is conveyed to the separation device. Surprisingly, it has now been found that by applying a fluid containing an activator and then drying the applied activator layer, the storage stability of the laminated strips produced in this way, which then have a partially crosslinked baking varnish layer and a dried activator layer, can be improved to the extent that the laminated strip can be temporarily stored. Therefore, in an embodiment of the method according to the invention, a discontinuous tape store is used, into which the laminated tape coated with the dry activator is first introduced. At a later point in time, the laminated tape is fed from the tape store to a clocked separation device. An example of a discontinuous tape store is a capstan on which the laminated tape coated with the dry activator is wound as a coil. The use of a discontinuous tape store can even be advantageous if, depending on the type of baking varnish and activator used, it is even desired that the baking varnish react further from the outset before being fed to the separation device. The laminated tape can then be stored in a space-saving manner in coil form for the required rest time after the application of the activator before the tape is fed to the separation device at the desired point in time.

[0023] However, in the method according to the invention, it is particularly preferred to use a continuous belt storage, that is to say a belt storage that is completely traversed by the laminated belt and is immediately fed to the clocked separation device after leaving the belt storage. Typical continuous belt storages are, for example, drop belts, which are designed in such a way that the laminated belt travels a dynamically variable path in the belt storage, for example via suitable movable deflection rollers, so that on the one hand, continuous feeding of the laminated belt is possible at the input end of the belt storage, but on the output end of the belt storage, clocked further transport in the clock cycle of the separation device is ensured.

[0024] Preferably, the fluid containing the activator is a liquid, for example a liquid in which the activator is dissolved in a liquid solvent, for example water. Therefore, within the scope of the present method, "drying" is to be understood as a process of removing the solvent from the applied fluid, so that after drying, only the activator and any non-volatile auxiliary agents present in the further fluid remain as a defined additional layer on the laminated strip coated with the baking varnish. This liquid is preferably applied to the strip surface by means of a roller or as a liquid jet.

[0025] According to another embodiment, the fluid containing the activator is an aerosol, which is generated in the application device, for example by atomizing a liquid. In this case, the laminated web is transported through the aerosol containing the activator, so that aerosol droplets can accumulate on the surface of the laminated web and can form a thin layer. In this case, a liquid is usually also present as an activator carrier, which must be removed in a subsequent drying process after the aerosol droplets have accumulated on the laminated web.

[0026] The presence of a tape storage device between the application of the fluid and the separation of the laminated parts from the laminated tape in the separation device also enables great flexibility in drying the applied fluid, because the spatial and temporal distance between the application of the fluid and the delivery of the laminated tape to the separation device is increased compared to the prior art. When using a discontinuous tape storage device, it is even possible to completely decouple from the tape speed in the separation device. Suitable drying variants include transporting the tape to the ambient air, which can be sufficient for drying in the case of a thin liquid layer. Alternatively, an air flow with a defined relative air humidity, especially an air humidity lower than that in the surrounding air, can also be directed to the laminated tape coated with the fluid. Another alternative to drying is to deliver hot air, especially hot air with low air humidity. If necessary, the tape itself can be heated in each of these drying methods to promote the evaporation of the solvent. Induction heating methods are preferably used here. However, in the case of heat transfer during the drying process of the activator, care must be taken to keep the temperature of the laminated web below the curing temperature of the baking varnish, ie the previously applied curable polymer adhesive layer.

[0027] If the drying of the applied fluid is accompanied by heating of the laminated web, a further embodiment of the method according to the invention can also provide that the laminated web is cooled immediately after the drying of the applied fluid by blowing ambient air or cooled ambient air through the laminated web. The laminated web is then preferably cooled before it is conveyed to the web storage.

[0028] The invention also relates to a device for connecting laminated parts to form a laminated stack, wherein a tape storage device is arranged between an application device for applying a fluid containing an activator and a separation device operating in a clocked manner. The subject of the invention is therefore also a device for connecting laminated parts to form a laminated stack, the device comprising: a conveying device for continuously conveying a laminated tape, the upper side and / or the lower side of which has a curable polymer adhesive layer; an application device for applying a fluid containing an activator to the adhesive layer of the laminated tape; a drying device for drying the applied fluid; a clocked separation device for separating laminated parts from the laminated tape; and a stacking and grouping device for stacking the separated laminated parts and connecting the laminated parts to form a laminated stack. The device according to the invention is characterized in that a tape storage device is arranged between the application device and the separation device.

[0029] According to a variant of the device according to the invention, the tape storage is a discontinuous tape storage and can be configured, for example, to receive a coil of a laminated tape coated with a baking varnish and a dried activator. In this case, the device according to the invention comprises two sub-devices that are independent of each other. The first sub-device comprises an application device for continuously applying and drying an activator fluid and a first part of a discontinuous tape storage for a laminated tape coated with a dried activator. In this first part, for example, with a capstan, the laminated tape coated with a dried activator is wound as a coil. The coil can be temporarily stored for a period of time and then transported to the second sub-device for further processing. The second sub-device comprises a second part of a discontinuous tape storage for a laminated tape coated with a dried activator, a separation device, and a stacking and grouping device. Therefore, the tape coated with the activator must be transported from the first sub-device to the second sub-device. Therefore, storage of the tape in the form of a coil is particularly provided. Since such a coil can be transported between the first sub-device and the second sub-device, the first and second sub-devices do not necessarily have to be in the same place. It is even conceivable that the coating with the activator in the first sub-device is carried out by a specialized manufacturer, while the separation / bonding group in the second sub-device is carried out by another specialized manufacturer.

[0030] According to another variant of the device according to the invention, the strip storage is a continuous strip storage and can be designed, for example, to produce a dynamically variable hanging strip of the laminated strip coated with baking varnish and dried activator.

[0031] The application device for the aqueous activator solution preferably comprises a minimum quantity lubrication device (Mindermengenschmiereinrichtung) (which is also called minimum quantity lubrication device) having a spray nozzle made of a corrosion-resistant material. Thus, commercially available and therefore inexpensive minimum quantity lubrication devices can be used. However, these commercially available devices are designed for delivering oily fluids without special requirements on the materials used, and they must be suitable for use in the method according to the invention at least in terms of the nozzles used, i.e. the nozzles are made of corrosion-resistant materials, for example of corrosion-resistant and acid / alkali-resistant stainless steel materials.

[0032] The invention also relates to a laminate stack comprising a plurality of laminates stacked one on top of the other, with an adhesive layer formed between them, the adhesive layer comprising a derivative of a crosslinked epoxy baking varnish and an activator, the crosslinked epoxy baking varnish preferably being based on a bisphenol-A-epichlorohydrin resin system, and wherein the activator comprises imidazole, preferably 2-ethyl-4-methylimidazole. During curing, the imidazole derivative irreversibly binds to the growing chains of the crosslinked baking varnish and thus functions as a crosslinking agent, which exhibits very good properties, such as a high glass transition temperature of the hardened network.

[0033] The thickness of the adhesive layer between the individual laminate parts is preferably in the micrometer range, preferably in the range of 2 to 10 μm. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] The invention is explained in more detail below with reference to the exemplary embodiments shown in the drawings.

[0035] in:

[0036] Figure 1 A schematic illustration of a device for producing a laminated core having a continuous belt storage device is shown;

[0037] Figure 2 a schematic diagram showing an adhesive layer between two lamination parts in a lamination stack; and

[0038] Figure 3 Shows a non-contiguous band memory Figure 1 Variations of the device. DETAILED DESCRIPTION

[0039] Figure 1 1 shows a device, generally designated by reference numeral 10, for carrying out the method according to the invention for continuously connecting laminated parts to form a laminated core. Figure 1In the device shown in , a continuous tape storage is used. The starting material for the method according to the invention is a laminated tape coated with a baking varnish, i.e. coated with a curable polymer adhesive layer, which in the example shown is provided in the form of a coil, which is also referred to as coil 11. After unwinding the coil 11, the laminated tape 12 coated with the baking varnish is usually passed through a tape transport device and a straightening device 13, which transports the tape in the direction of the arrow 14 and ensures a flat, non-warping position of the unwound tape after passing through the straightening device. After passing through the straightening device 13, the laminated tape 12 is continuously transported through an application device 15, in which a fluid 16 containing an activator is applied to the polymer adhesive layer already present on the upper side and / or lower side 17, 18 of the tape 12. If the tape 12 is to be coated with baking varnish both on the upper side 17 and on the lower side 18, a corresponding application device 15' is also provided below the tape 12 for applying an activator fluid 16', such as Figure 1 As shown by the dotted lines in . The application device 15, 15' includes a minimum quantity lubrication device having a nozzle made of corrosion-resistant and acid / alkali-resistant stainless steel material. The application device 15, 15' is connected to a drying device 19, 19', in which the applied fluid is dried. The drying device 19, 19' can, for example, have a fan for dry air or hot air and / or a heating device such as an induction heating unit for heating the laminate belt 12, so as to support the drying of the applied fluid layer. The heating of the laminate belt 12 is regulated in this case as follows, that is, the curing of the pre-applied baking varnish is avoided, so that the temperature of the laminate belt and the baking varnish layer is always kept below the curing temperature of the baking varnish. The drying devices 19, 19' can also be connected (in Figure 1 In the exemplary embodiment of the present invention, a cooling device (not shown) is provided, which cools the heated strip back to ambient temperature as quickly as possible, for example by means of a fan. However, such a cooling device is not absolutely necessary, but can be used in particular when the laminated strip is heated to a relatively high temperature close to the curing temperature of the baking varnish for drying the activator fluid. After the applied activator fluid has dried and, if necessary, cooled, the laminated strip 12 is guided to a strip storage 20, which is located in a Figure 1 In the example shown, the continuous belt storage 20 is symbolically represented by a return rail 21 through which the laminated belt 12 passes. The additional distance traveled by the belt 12 in the belt storage 20 can be dynamically changed via a movable deflection roller, which is moved in a manner that allows the belt 12 to move in a continuous manner. Figure 12 is symbolically indicated by arrow 22. Due to the dynamically changing travel of the hanging belt 21, the laminated belt 12 can be continuously fed to the input 23 of the belt storage 20, but is further transported in a clocked manner at the output 24 of the belt storage 20. For this purpose, a feed device 25 is connected downstream of the belt storage 20, which further transports the belt 12 to a separation device, which is generally designated by reference numeral 30.

[0040] In the example shown, the separation device 30 is a punching device, in which one or more punching tools 31, 32, 33 punch out a laminated portion 40 from the laminated strip 12. As shown, if there are multiple punching tools 31, 32, 33, the individual punching tools can either punch out a simple laminated portion 40 in parallel or produce a more complex laminated portion in multiple punching steps. In the example shown, the first and second punches 31, 32 can separate the laminated portions 41, 42 from the laminated strip 12, which are thrown out as discarded parts and are no longer required for the further production process of the laminated stack.

[0041] As symbolically indicated by arrows 34 , the upper tools of the punching tools 31 , 32 , 33 are moved up and down in a clocked manner, while the laminated strip is transported further by the strip feeder 25 in the same clock cycle.

[0042] The stamped laminated parts 40 are stacked one above the other in a columnar guide 43. The heatable inner wall of the guide 43 has a slightly tapered profile toward the bottom, so that the guide 43 applies resistance to the stacked laminated parts 40 in the form of a braking stack. The wall section 46 of the guide 41 is heated via a heating unit 45, so that the laminated parts 40 are heated to above the curing temperature of the baking varnish, and thus the laminated parts 40 are spliced ​​together under heating and pressure. For this purpose, the guide 41 is surrounded by a heating unit 43, which heats the laminated parts in the guide 43 to a temperature above the crosslinking temperature of the applied baking varnish, and thus ensures that the individual laminated parts 40 are connected to form a laminated stack 46 via the cured baking varnish layer 47 between the laminated parts 40 stacked one above the other.

[0043] exist Figure 2 , a schematic detail of a laminated core 46 having two laminated core parts 40 stacked one above the other and a cured baking varnish layer 47 located between them is shown in an enlarged manner.

[0044] The laminate strip 12 is preferably coated with a baking varnish both on the upper side 17 and on the lower side 18, so that when the laminate parts 40 are connected, a material-locking connection between the baking varnish layers of the laminate parts 40 placed one above the other is ensured. Depending on the adhesion properties of the baking varnish on the laminate parts themselves, a sufficiently strong connection of the laminate parts in a stack can also be achieved with only the laminate parts coated on one side.

[0045] When a certain number of laminated parts corresponding to the desired height of the laminated core 46 to be produced has been punched out, appropriate measures are taken to ensure that the laminated parts punched out subsequently (eg Figure 1 The lamination section 40a in the lamination is no longer attached to the last (uppermost) lamination section (e.g. Figure 1 40b), and thus, even after the paint has cured, a single stack 46 with the desired number of laminate parts can be easily sorted out from the laminate parts coming from the laminate part columns formed in the guide part 41. For this purpose, various measures can be provided to the person skilled in the art, which are described in more detail in the applicant's patent applications, such as EP 2 883 692 A1 or EP 30 89 335 A1, where corresponding separators, such as separator films or separator tabs, can be applied on the upper or lower side at several positions in the strip from which the laminate parts are punched out that should not have an adhesion effect with the subsequent laminate parts. For example, structured separator elements can also be inserted at appropriate positions, which separator elements do not have a great adhesion effect due to their small contact surface with the laminate parts and can therefore be easily removed again after being disassembled into individual stacks. A granular structure can also be embossed into the laminate parts, which serves as a distance retainer for the previous laminate parts and thus enables easier separation of the individual stacks. In Figure 1 , the application or introduction of suitable separating means is symbolically indicated by separating means feeders 35, 35' which, in the example shown, apply separating tabs 36, 36' to the upper and / or lower side of the strip at the desired locations. For example, when the laminated parts to be punched out have separating tabs on the upper and lower sides, the corresponding laminated parts will function as sacrificial sheets and not as part of a stack. When a laminated part, such as laminated part 40a, has separating tabs on the lower side, while the preceding laminated part, such as 40b, has separating tabs on the upper side, these laminated parts are still components of respective different stacks 46.

[0046] Figure 3 It is shown in Figure 1 A variant of the device having Figure 1 The variants of Figure 3A) is performed to apply the activator fluid, while in a later step ( Figure 3 B) is completed by punching out the lamination part. Figure 3 In, with Figure 1 In the embodiments of the present invention, corresponding elements that are identical or that fulfill similar functions are marked with the same reference numerals.

[0047] According to Figure 1 The implementation method of the method is the same as that of Figure 3 In the implementation method according to Figure 3 The first step of A begins with unwinding the laminated strip 12 from the coil 11 and subsequently straightening it in the straightening device 13. Then, the activator fluid is applied again in the application device 15 and the applied activator layer is subsequently dried in the drying device 19. Figure 1 As in the method of , the tape is then guided into a tape storage 20 along a transport direction symbolically indicated by arrow 14. Figure 1 In different forms, Figure 3 The tape memory 20 of the embodiment is a discontinuous tape memory. Figure 3 In the figure, the coil 50 is symbolically indicated, that is to say the laminated strip 12 previously coated with baking varnish and now also coated with a dried activator layer is wound on a capstan to form the coil 50. The coil 50 can now be temporarily stored.

[0048] After a storage time which is typically much shorter than the storage time for curing baking varnishes, the Figure 3 B, the coil 50 is fed to the separation device 30. After the coil 50 has been unwound and the strip has been straightened by the straightening device 13' if necessary, as has been combined Figure 1 As has already been described in the specific embodiment of the present invention, further processing takes place in the separation device via a clocked feed 25 .

[0049] It can be seen that even in Figure 3 In the variant of , the strip 12 pre-coated with baking varnish is also unwound from the initial coil 11 in a continuous process, followed by the application of the activating agent to be applied, drying and, if necessary, cooling, and winding on the coil 50 used as a discontinuous strip storage, while the further processing of the laminated strip 12 coated with activating agent after unwinding the coil 50 is carried out in a manner matched to the clock cycle of the separation device. Here, the strip storage 20, which is now in the form of a discontinuous strip storage, also ensures the separation of the continuous and clocked method steps.

Claims

1. A method for connecting laminated parts (40) to form a laminated stack (46), wherein: A laminated web (12) having a curable polymer adhesive layer on its upper side (17) and / or lower side (18) is continuously transported through an application device (15, 15') in which a fluid (16, 16') containing an activator is applied to the polymer adhesive layer. allowing the applied fluid (16, 16') to dry, The laminated tape (12) coated with the dry activator is continuously fed to a tape storage (20), The laminated web (12) is fed from the web storage (20) to a clock-controlled separation device (30), in which laminated parts (40, 41, 42) are separated from the laminated web (12) and stacked one above the other, and The polymer adhesive layer coated with an activator connects the separated and stacked laminate parts (40) to each other to form a laminate group (46), wherein the fluid (16, 16') applied to the laminated belt is dried by conveying air, wherein the laminated strip is heated during drying, The heating of the laminate tape is adjusted so that the temperature of the laminate tape and the curable polymer adhesive layer is always kept below the curing temperature of the curable polymer adhesive layer.

2. The method according to claim 1, characterized in that The curable polymer adhesive layer comprises a pre-crosslinked epoxy baking varnish applied in different layer thicknesses to the upper side (17) and the lower side (18).

3. The method according to claim 2, characterized in that The epoxy baking varnish is pre-crosslinked to different degrees on the upper side (17) and the lower side (18).

4. The method according to any one of claims 1 to 3, characterized in that The band memory (20) is a discontinuous band memory.

5. The method according to any one of claims 1 to 3, characterized in that The band memory (20) is a continuous band memory.

6. The method according to any one of claims 1 to 3, characterized in that The fluid (16, 16') containing the activating agent is applied as a liquid.

7. The method according to claim 6, characterized in that The liquid containing the activator is applied to the laminated web in the form of a liquid jet or by means of a roller.

8. The method according to any one of claims 1 to 3, characterized in that The fluid (16, 16') containing the activating agent is applied as an aerosol.

9. The method according to claim 8, characterized in that The laminated tape is conveyed through an aerosol containing an activating agent.

10. The method according to any one of claims 1 to 3, characterized in that The fluid (16, 16') applied to the laminated web is dried by supplying hot air or air with reduced relative humidity.

11. The method according to claim 1, characterized in that: After drying, the laminated strip is cooled.

12. A device for connecting laminated parts (40) to form a laminated stack (46), wherein: The device comprises: A conveying device (11, 13) for continuously conveying a laminated web (12) having a layer of a curable polymer adhesive on its upper side (17) and / or lower side (18), an application device (15, 15') for applying a fluid (16, 16') containing an activating agent to the adhesive layer of the laminate tape (12), a drying device (19, 19') for drying the applied fluid (16, 16'), a clock-controlled separation device (30) for separating laminated parts (40, 41, 42) from the laminated belt (12), stacking and grouping devices (43, 44, 45) for stacking the separated laminated parts (40) and for connecting the laminated parts (40) to form laminated groups (46), A tape storage device (20) is arranged between the application device (15, 15') and the separation device (30), The drying device has a fan for conveying air and a heating device for heating the laminate tape, wherein the heating of the laminate tape is adjusted so that the temperature of the laminate tape and the curable polymer adhesive layer is always maintained below the curing temperature of the curable polymer adhesive layer.

13. The device according to claim 12, characterized in that The tape storage (20) is configured to receive a roll (50) of laminate tape (12) coated with a curable polymer adhesive layer and a dried activator.

14. The device according to claim 12, characterized in that The tape storage device (20) is configured to produce a dynamically variable drape (21) of a laminate tape (12) coated with a curable polymer adhesive layer and a dried activator.

15. The device according to any one of claims 12 to 14, characterized in that The application device (15, 15') comprises a minimum quantity lubrication device having a nozzle made of a corrosion-resistant material.

16. A laminate stack (46), comprising a plurality of laminate parts (40) stacked one on top of the other, with an adhesive layer formed between them, the adhesive layer comprising a cross-linked epoxy baking varnish and a dry imidazole derivative as an activator, wherein: The imidazole derivative is irreversibly bonded to the crosslinked epoxy baking varnish, wherein the laminated core (46) is produced by the method according to any one of claims 1 to 11.

17. The lamination stack (46) according to claim 16, characterized in that The cross-linked epoxy baking varnish is based on a bisphenol-A-epichlorohydrin resin system, and / or the activator comprises 2-ethyl-4-methylimidazole.