Wiring substrate, electronic device, and electronic module

By designing a thickness gradient metal film structure on the wiring substrate, the problems of Joule thermal stress concentration and insufficient heat dissipation are solved, and the reliability and heat dissipation performance of electronic devices and modules are improved.

CN113228259BActive Publication Date: 2024-10-25KYOCERA CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980085720.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-12-26
Filing Date
2019-12-25
Publication Date
2024-10-25
Estimated Expiration
2039-12-25

AI Technical Summary

Technical Problem

The stress concentration of Joule heat when the existing wiring substrate is energized leads to reduced component reliability and insufficient heat dissipation characteristics, affecting the stability of electronic devices and modules.

Method used

A metal film structure with a thickness gradient is designed. The first metal film extends from one side of the substrate to the side, and the second metal film extends from the side to the other side, forming a gradient structure to evenly diffuse Joule heat and pass through the close contact layer and barrier. layer and conductor layer increase the strength and stability of the membrane.

Benefits of technology

It effectively reduces the stress concentration caused by Joule heat, improves the low-loss transmission of current, enhances the heat dissipation characteristics and electrical characteristics reliability of the substrate, and reduces the risk of peeling of the metal film.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113228259B_ABST
    Figure CN113228259B_ABST
Patent Text Reader

Abstract

The wiring substrate comprises: a substrate having a first surface, a second surface on the opposite side of the first surface, and side surfaces respectively connected to the first surface and the second surface; a first metal film, which is arranged from the first surface to the side surface; and a second metal film, which is arranged from the second surface to the first metal film located on the side surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a wiring substrate, an electronic device, and an electronic module. Background Art

[0002] Japanese Patent Application Laid-Open No. 10-284436 discloses a technique for making ohmic contact between a silicon carbide substrate and an electrode on the substrate. The so-called ohmic contact refers to a resistive contact without a Schottky barrier, and through the ohmically contacted electrode, current can flow from the electrode to the substrate in the same way as current flows through a metal resistor. Summary of the invention

[0003] The wiring substrate of the present disclosure comprises:

[0004] A substrate having a first surface, a second surface opposite to the first surface, and side surfaces respectively connected to the first surface and the second surface;

[0005] a first metal film disposed from the first surface to the side surface; and

[0006] A second metal film is arranged from the second surface to the first metal film located on the side surface.

[0007] The electronic device disclosed herein comprises:

[0008] The above wiring substrate; and

[0009] An electronic component is mounted on the wiring substrate.

[0010] The electronic module disclosed in the present invention has:

[0011] The electronic device mentioned above; and

[0012] A module substrate on which the electronic device is mounted. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 It is a longitudinal sectional view showing a wiring substrate according to an embodiment of the present disclosure.

[0014] Figure 2 It is shown Figure 1 A top view of a wiring substrate.

[0015] Figure 3 It is shown Figure 1 Rear view of the wiring substrate.

[0016] Figure 4 yes Figure 1 Sectional view of arrow AA line.

[0017] Figure 5It is a longitudinal cross-sectional view showing an electronic device and an electronic module according to an embodiment of the present disclosure. DETAILED DESCRIPTION

[0018] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the accompanying drawings.

[0019] Figure 1 It is a longitudinal sectional view showing a wiring substrate according to an embodiment of the present disclosure. Figure 2 It is shown Figure 1 A top view of a wiring substrate. Figure 3 It is shown Figure 1 Rear view of the wiring substrate. Figure 4 yes Figure 1 The arrow AA line section view. Figure 2 and Figure 3 In FIG. 1 , the wiring conductors 41 and 42 are indicated by two-dot chain lines, and the state in which the wiring conductors 41 and 42 are removed is shown.

[0020] The wiring board 1 of this embodiment is a submount interposed between an electronic component and an object to be mounted, for example, on a module board or a package. The wiring board 1 includes a substrate 10 , a first metal film 20 , a second metal film 30 , and film-like wiring conductors 41 , 42 .

[0021] The substrate 10 is formed of a semiconductor material such as SiC (silicon carbide) or an insulating ceramic material such as aluminum nitride or aluminum oxide. The substrate 10 has a first surface 11, a second surface 12 located on the opposite side of the first surface 11, and side surfaces 13 connected to the first surface 11 and the second surface 12. The side surface 13 is located at one edge e1 ( Figure 1 ) and one edge e2 of the second surface 12 ( Figure 1 ). The edges e1 and e2 are located in the same direction in the first surface 11 and the second surface 12. The side surface 13 may be a cut surface obtained by cutting.

[0022] The first metal film 20 is arranged from the first surface 11 to the side surface 13. Specifically, the first metal film 20 on the first surface 11 is formed integrally with the first metal film 20 along the side surface 13, and is continuous at the edge e1. The first metal film 20 located on the first surface 11 has a thickness gradient in which the thickness increases as it approaches the side surface 13. The first metal film 20 located on the side surface 13 has a thickness gradient in which the thickness increases as it approaches the first surface 11. Therefore, the thickness of the first metal film 20 at the edge e1 is greater than the thickness of the two ends of the first metal film 20 farthest from the edge e1 on the first surface 11 side and the side surface 13 side.

[0023] like Figure 4As shown, the first metal film 20 is composed of a laminated adhesion layer L1, a barrier layer L2, and a conductor layer L3 from the side close to the substrate 10. The adhesion layer L1 is a metal having a higher degree of adhesion to the substrate 10 than the conductor layer L3, for example, Ti (titanium) can be applied. The barrier layer L2 is a metal having the property of suppressing the diffusion of components between the layers, for example, Pt (platinum) can be applied. The conductor layer L3 is a metal with a higher conductivity than the adhesion layer L1, for example, Au (gold) can be applied. The adhesion layer L1, the barrier layer L2, and the conductor layer L3 of the first metal film 20 may have the thickness gradient of the first metal film 20 described above, or any one layer may have the thickness gradient described above.

[0024] The second metal film 30 is arranged from the second surface 12 to the first metal film 20 located on the side surface 13. Specifically, the second metal film 30 on the second surface 12 is formed integrally with the second metal film 30 along the side surface 13, and is continuous at the edge e2. The second metal film 30 located on the second surface 12 has a thickness gradient in which the thickness increases as it approaches the side surface 13. The second metal film 30 located on the side surface 13 has a thickness gradient in which the thickness increases as it approaches the second surface 12. Therefore, the thickness of the second metal film 30 at the edge e2 is greater than the thickness of the two ends of the second metal film 30 farthest from the edge e2 on the second surface 12 side and the side surface 13 side.

[0025] like Figure 4 As shown, the second metal film 30 is composed of a bonding layer L1, a barrier layer L2, and a conductor layer L3 stacked from the side close to the substrate 10. The material of each layer is the same as that of each layer of the first metal film 20. In the bonding layer L1, the barrier layer L2, and the conductor layer L3 of the second metal film 30, each layer may have the thickness gradient of the second metal film 30 described above, or any layer may have the thickness gradient of the second metal film 30 described above.

[0026] Although the thickness gradient of the first metal film 20 along the side surface 13 and the thickness gradient of the second metal film 30 along the side surface 13 have opposite trends, the magnitudes of the gradients can be roughly the same. Therefore, on the surface of the side surface 13, the thickness of the film that combines the first metal film 20 and the second metal film 30 can become roughly constant from the side close to one edge e1 to the side close to the other edge e2. According to the above structure, when power is turned on, the Joule heat generated at the interface between the first metal film 20 and the second metal film 30 on the side surface 13 can be evenly diffused, and the stress concentration generated in the first metal film 20 and the second metal film 30 based on the above Joule heat can be reduced. Here, the direction from the second surface 12 to the first surface 11 is called the height. Hereinafter, the same.

[0027] Furthermore, the average thickness of the first metal film 20 along the side surface 13 and the average thickness of the second metal film 30 along the side surface 13 can be substantially the same. In addition, the length in the height direction of the side surface 13 on which the first metal film 20 is formed and the length in the height direction of the side surface 13 on which the second metal film 30 is formed can be substantially the same, for example, by setting the length in the height direction of the side surface 13 on which the second metal film 30 is formed to be substantially the same, for example, to be substantially the entire region in the height direction of the substrate 10. According to the above-mentioned structure, the thickness of the first metal film 20 and the thickness of the second metal film 30 can be substantially the same at the center in the height direction of the substrate 10. Therefore, the film stress generated in the first metal film 20 and the second metal film 30 on the side surface 13 can be made uniform. The so-called film stress here includes the stress applied during film formation and the stress generated due to the difference in thermal expansion coefficient with the substrate 10.

[0028] The wiring conductor 41 is a part for mounting electronic components and electrically connecting to the electronic components, and is formed on the first surface 11 through the first metal film 20. The wiring conductor 42 on the other side is a part for bonding to the installation destination, and is formed on the second surface 12 through the second metal film 30. As the wiring conductors 41 and 42, for example, AuSz (gold tin) can be applied. In the case of AuSz as the material, a barrier film such as Pt (platinum) can also be interposed between the wiring conductor 41 and the first metal film 20 and between the wiring conductor 42 and the second metal film 30.

[0029] In the figure, the thickness gradient of the first metal film 20 on the first surface 11 and the thickness gradient of the second metal film 30 on the second surface 12 are exaggerated. The actual thickness gradient is about the same as the tolerance of the parallelism of the first surface 11 and the second surface 12 of the substrate 10, so the parallelism of the upper surface of the wiring conductor 41 and the lower surface of the wiring conductor 42 is different from that shown in the figure and becomes relatively high.

[0030] like Figure 2 As shown, alignment marks 23a to 23c are formed on the first metal film 20 on the first surface 11 side. The alignment marks 23a to 23c are marks for recognizing from an image of a camera or the like when mounting an electronic component on the wiring substrate 1 or mounting the wiring substrate 1 to a mounting destination, and adjusting the orientation and position of the wiring substrate 1. The alignment marks 23a to 23c are formed by the film formation pattern of the first metal film 20, including a portion without a metal film. The alignment marks 23a to 23c are formed by patterning the first metal film 20 during film formation or by etching the first metal film 20.

[0031] The alignment marks 23a to 23c are arranged on the first surface 11 on a side farther from the side surface 13 than the center of the first metal film 20 located on the first surface 11. The alignment marks 23a to 23c may be arranged on the second surface 12 on a side farther from the side surface 13 than the center of the second metal film 30 located on the second surface 12. The alignment marks 23a to 23c may also be arranged on the opposite side of the side surface 13 than the wiring conductor 41.

[0032] <Manufacturing method>

[0033] Next, a method for manufacturing the first metal film 20 and the second metal film 30 having the above-described thickness gradient will be described.

[0034] The first metal film 20 is formed by using a vacuum film forming device such as evaporation or sputtering. The substrate 10 is arranged in the vacuum film forming device so that the edge e1 faces the source of the film forming material. In the case where the first surface 11 is orthogonal to the side surface 13, the first surface 11 and the side surface 13 are inclined 45 degrees relative to the source of the film forming component through the above-mentioned configuration. By performing the film forming process under the above-mentioned configuration, it is possible to form a first metal film 20 in which the thickness of the edge e1 is partially thick and the thickness decreases as it is farther away from the edge e1. For the second metal film 30, similarly, in the vacuum film forming device, the edge e2 of the substrate 10 is arranged to face the source of the film forming component, and the film forming process is performed, thereby achieving the above-mentioned thickness gradient.

[0035] When forming the first metal film 20 and the second metal film 30, a photoresist is formed on the surfaces of the substrate 10 other than the first surface 11, the second surface 12, and the side surface 13, thereby omitting the formation of metal films on other surfaces. The photoresist may also be formed on the edge portions of the first surface 11, the second surface 12, and the side surface 13 adjacent to the surfaces other than these surfaces, and the film forming process is performed.

[0036] <Electronic Devices and Electronic Modules>

[0037] Figure 5 2 is a cross-sectional view showing an electronic device and an electronic module according to an embodiment of the present disclosure.

[0038] The electronic device 60 according to the present embodiment is configured by mounting the electronic component 50 on the wiring substrate 1. Although not shown in the figure, the electronic device 60 may also have a structure further including a package that houses the wiring substrate 1 and the electronic component 50.

[0039] As the electronic component 50, various electronic components can be applied, such as optical elements such as LD (Laser Diode), PD (Photo Diode), LED (Light Emitting Diode), imaging elements such as CCD (Charge Coupled Device) type and CMOS (Complementary Metal Oxide Semiconductor) type, piezoelectric resonators such as quartz resonators, surface acoustic wave elements, semiconductor elements such as semiconductor integrated circuit elements (IC: Integrated Circuit), capacitor elements, inductor elements or resistors.

[0040] The electronic component 50 and the wiring conductor 41 of the wiring substrate 1 may be connected via a bonding material such as solder, or after the electronic component 50 is bonded to the wiring substrate 1 , a terminal of the electronic component 50 and the wiring conductor 41 may be electrically connected via a bonding wire or the like.

[0041] The electronic module 100 according to the present embodiment is formed by mounting an electronic device 60 on a module substrate 110. In addition to mounting the electronic device 60, other electronic devices, electronic components, and electrical components may be mounted on the module substrate 110. The module substrate 110 is provided with an electrode pad 111, and the electronic device 60 is bonded to the electrode pad 111 via a bonding material 113 such as solder. Figure 5 In the embodiment, the wiring conductors 42 of the wiring substrate 1 are joined to the electrode pads 111 . However, when the electronic device 60 has a package, the wiring conductors of the package may be joined to the electrode pads 111 of the module substrate 110 .

[0042] As described above, according to the wiring substrate 1 of the present embodiment, the first metal film 20 is arranged from the first surface 11 of the substrate 10 to the side surface 13, and the second metal film 30 is arranged from the second surface 12 of the substrate 10 to the first metal film 20 located on the side surface 13. Therefore, when a current flows from the first surface 11 side to the second surface 12 side of the substrate 10, a large amount of current flows through the first metal film 20 and the second metal film 30 on the side surface 13. Therefore, the Joule heat generated in the substrate 10 can be suppressed, and for example, when it is necessary to dissipate heat from the electronic components mounted on the wiring substrate 1, the heat dissipation characteristics through the substrate 10 can be improved.

[0043] Furthermore, according to the wiring substrate 1 of the present embodiment, it is possible to allow current to flow from the first surface 11 of the substrate 10 to the second surface 12 via the conductor. The resistance of the first metal film 20 and the second metal film 30 is four orders of magnitude or more smaller than the resistance of the semiconductor substrate 10. Therefore, according to the wiring substrate 1 of the present embodiment, it is possible to allow current to flow from the first surface 11 to the second surface 12 with less loss, and the generation of Joule heat can be significantly reduced.

[0044] Furthermore, the first metal film 20 existing across the first surface 11 side and the second metal film 30 existing across the second surface 12 side are stacked on the side surface 13 of the substrate 10. With the above-mentioned structure, for example, even if heat is applied to the wiring substrate 1 and stress is generated at the interface between the substrate 10 and the first metal film 20 or the second metal film 30 due to the difference in thermal expansion coefficient, the first metal film 20 or the second metal film 30 can be prevented from peeling off from the side surface 13.

[0045] Furthermore, according to the wiring substrate 1 of the embodiment, the first metal film 20 located on the first surface 11 has a thickness gradient in which the thickness increases as it approaches the side surface 13, and the first metal film 20 located on the side surface 13 has a thickness gradient in which the thickness increases as it approaches the first surface 11. In addition, the second metal film 30 located on the second surface 12 has a thickness gradient in which the thickness increases as it approaches the side surface 13, and the second metal film 30 located on the side surface 13 has a thickness gradient in which the thickness increases as it approaches the second surface 12. According to the above-mentioned thickness gradient, the strength of the first metal film 20 and the second metal film 30 can be improved at the edges e1 and e2 where stress is easily concentrated, and the generation of cracks at the edges e1 and e2 can be suppressed. Therefore, the low resistance from the first surface 11 to the second surface 12 of the substrate 10 is firmly maintained, and the reliability of the electrical characteristics can be improved.

[0046] Furthermore, according to the wiring substrate 1 of the embodiment, the thickness of the first metal film 20 and the second metal film 30 combined can be made uniform from the first surface 11 side to the second surface 12 side on the side surface 13. According to the above-mentioned structure, when power is applied, the Joule heat generated at the interface between the first metal film 20 and the second metal film 30 on the side surface 13 can be uniformly diffused, and the stress concentration generated in the first metal film 20 and the second metal film 30 due to the above-mentioned Joule heat can be reduced. Therefore, the low resistance from the first surface 11 to the second surface 12 of the substrate 10 is firmly maintained, and the reliability of the electrical characteristics can be improved.

[0047] Furthermore, according to the wiring substrate 1 of the embodiment, the thickness of the first metal film 20 and the thickness of the second metal film 30 can be made substantially the same at the center in the height direction of the substrate 10. According to the above-mentioned structure, the film stress generated in the first metal film 20 and the second metal film 30 on the side surface 13 can be made uniform in the height direction, and by making the film stress uniform, the peeling of the first metal film 20 or the second metal film 30 can be further suppressed.

[0048] Furthermore, according to the wiring substrate 1 of the embodiment, the first metal film 20 and the second metal film 30 each include the adhesion layer L1, the barrier layer L2, and the conductor layer L3. Therefore, on the first surface 11 and the second surface where the first metal film 20 or the second metal film 30 exists alone, high stability of the first metal film 20 and the second metal film 30 can be obtained. Furthermore, on the side surface 13 where the first metal film 20 and the second metal film 30 exist in an overlapping manner, high stability of the first metal film 20 and the second metal film 30 can also be obtained by the above-mentioned three-layer structure.

[0049] Furthermore, according to the wiring substrate 1 of the embodiment, the alignment marks 23a to 23c are arranged on the side away from the side surface 13. According to the above arrangement, the alignment marks 23a to 23c do not narrow the cross section in the main current path from the first metal film 20 on the first surface 11 to the second metal film 30 on the second surface 12. Therefore, the current can flow from the first metal film 20 on the first surface 11 to the second metal film 30 on the second surface 12 with low loss, and the Joule heat generated in the first metal film 20 and the second metal film 30 can be further reduced.

[0050] Furthermore, according to the electronic device 60 and the electronic module 100 of the present embodiment, the Joule heat generated by the substrate 10 in the wiring substrate 1 is reduced, thereby improving the heat dissipation of the electronic component 50. Therefore, the reliability of the electronic device 60 and the electronic module 100 can be improved.

[0051] The embodiments of the present disclosure have been described above. In addition, in the above-mentioned embodiments, a semiconductor is cited as an example as a material for a substrate, but the substrate may also be configured to include an insulating material. In addition, in the above-mentioned embodiments, an example is shown in which the first metal film and the second metal film are formed on substantially the entire area in the height direction of the side surface of the wiring substrate, but a structure in which the first metal film and the second metal film are stacked only on a portion of the side surface in the height direction is also possible. In addition, in the above-mentioned embodiments, an example is shown in which the first metal film and the second metal film are three-layer structures, but the material of each layer can be appropriately changed, and the first metal film or the second metal film may be a multi-layer structure other than three layers, or may be a single-layer structure. In addition, in the above-mentioned embodiments, the side on which the electronic components are mounted is described as the first side, but the side on which the electronic components are mounted may also be the second side. That is, the stacking order of the metal films on the side surface may also be different from that on the other side. Figure 1 The stacking order shown is opposite. The description of this embodiment is illustrative in all aspects, and the present invention is not limited to the above. The present disclosure can also be applied to embodiments that are appropriately combined, changed, replaced, added, omitted, etc. as long as they are not contradictory. Moreover, it can be understood that the countless variations that are not illustrated can be obtained by imagination without departing from the scope of the present invention.

[0052] -Industrial Applicability-

[0053] The present disclosure can be utilized in a wiring substrate, an electronic device, and an electronic module.

Claims

1. A wiring substrate comprising: A substrate having a first surface, a second surface opposite to the first surface, and a side surface connected to an end of the first surface and an end of the second surface and serving as a part of an outer surface of the substrate; a first metal film disposed from the first surface to the side surface; and a second metal film, the second metal film being arranged from the second surface to the first metal film located on the side surface, The first metal film located on the first surface has a thickness gradient in which the thickness increases as it approaches the side surface. The first metal film located on the side surface has a thickness gradient in which the thickness increases as it approaches the first surface. The second metal film located on the second surface has a thickness gradient in which the thickness increases as it approaches the side surface. The second metal film located on the side surface has a thickness gradient in which the thickness increases as it approaches the second surface.

2. The wiring substrate according to claim 1, wherein: The first metal film and the second metal film each include an adhesion layer, a barrier layer, and a conductor layer.

3. The wiring substrate according to claim 1 or 2, wherein: The wiring substrate also has an alignment mark, which is located in the first surface at a position farther from the side surface than the center of the first metal film located on the first surface, or in the second surface at a position farther from the side surface than the center of the second metal film located on the second surface.

4. An electronic device comprising: The wiring substrate according to any one of claims 1 to 3; and An electronic component is mounted on the wiring substrate.

5. An electronic module comprising: The electronic device of claim 4; and A module substrate on which the electronic device is mounted.