IGBT device structure and process
By designing the leakage detection area in the IGBT device and using the polysilicon layer and metal interconnection structure, the problem of hard-to-find leakage in the device process is solved, timely detection and diagnosis of leakage is achieved, and the stability and reliability of the device are improved.
Patent Information
- Application Number
- CN202110804458.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-07-16
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-07-16
AI Technical Summary
IGBT devices are prone to leakage problems during the manufacturing process. In particular, high-current insulated gate bipolar transistors are more sensitive, and leakage is difficult to detect and solve in time due to phosphorus contamination and interface state defects.
An IGBT device structure is designed, including a leakage detection area. By adding a polysilicon layer and metal interconnection between the terminal ring area and the cutoff area, an online test structure is formed, which can detect leakage in time and determine its size, and perform debugging and diagnosis based on the process. .
It achieves timely detection and diagnosis of surface leakage of IGBT devices, improves the stability and reliability of the device, and avoids leakage problems caused by phosphorus contamination and interface state defects.
Smart Images

Figure CN113571497B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor devices, and in particular to a structure of an IGBT device.
[0002] The invention also relates to a process method of the IGBT device. Background Art
[0003] Insulated Gate Bipolar Transistor (IGBT) is a semiconductor power electronic device that combines the gate electrode voltage control characteristics of a metal oxide semiconductor field effect transistor (MOSFET) with the Darlington structure of a bipolar junction transistor (BJT). It has the characteristics of voltage control, large input impedance, low driving power, small on-resistance, low switching loss and high operating frequency. It is an ideal semiconductor power switching device with a switching frequency between 10K and 100K Hz, and has broad development and application prospects.
[0004] At present, as the current density requirements of IGBTs are getting higher and higher, the current of the device in the on-state is also getting larger and larger. The active area on the surface of the device is also getting larger and larger. During the device manufacturing process, the range of the active area surface contacting the external process gas increases. Especially for insulated gate bipolar transistors and other power devices, there are many reasons and ways to cause leakage. In the process of power device structure production, it often happens that the surface of the device is contaminated by phosphorus, phosphorus is absorbed by the surface of the device, boron in the device body is precipitated, and the interface state of the device surface is not repaired enough, which makes it more likely to cause leakage. Especially in the manufacturing process of high-current insulated gate bipolar transistors, it is more sensitive to leakage and needs to prevent leakage. Because phosphorus contamination on the surface of semiconductor devices is difficult to detect, even if it is inferred, it is difficult to verify, so it is more difficult to solve it in a targeted manner. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide an IGBT device with an additional leakage detection structure, which can promptly detect leakage in the power device process, and determine the size of the leakage by testing the device structure, and debug and diagnose the process to solve the leakage problem.
[0006] Another technical problem to be solved by the present invention is to provide a process method for the IGBT device.
[0007] The IGBT device structure of the present invention is formed in a semiconductor substrate. On the cross-sectional plane of the semiconductor substrate, the substrate is defined to have an upper surface and a lower bottom surface, and the horizontal direction perpendicular to the longitudinal direction of the upper surface and the lower bottom surface is the left and right sides; in the longitudinal direction of the device, the bottom layer, that is, the lower bottom surface, is the back metal, the collector region is above the back metal, the field stop layer is above the collector region, and the base region is above the field stop layer;
[0008] In the horizontal direction, the device is divided into multiple regions, namely, a cell region, a terminal ring region, a leakage detection region and a cut-off region; the leakage detection region is located between the terminal ring region and the cut-off region.
[0009] A further improvement is that the leakage detection area includes a first P-type body region, and heavily doped P-type contact regions are provided on both sides of the first P-type body region; the substrate surface above the first P-type body region also has a polysilicon layer; and the substrate surface of the leakage detection area has a dielectric layer or a passivation layer.
[0010] A contact hole is provided above the P-type contact area to form a lead-out, the contact hole penetrates through the dielectric layer and extends into the P-type contact area, and a metal layer is provided above the contact hole to form a metal interconnection;
[0011] The polysilicon layer, in a top view, extends on the substrate surface in a serpentine shape or in other wiring forms that can be adjusted to form different lengths;
[0012] PAD regions are formed at both ends of the polysilicon layer.
[0013] A further improvement is that the thickness of the polysilicon layer is 8000 to 15000Å; the width of the polysilicon layer is 1 to 4um.
[0014] A further improvement is that the PAD area is made of metal and is formed by a sputtering process; the metal thickness of the formed PAD area is 1 to 6.5 um.
[0015] A further improvement is that in the cell region, the shallow layer of the substrate is a second P-type body region, the second P-type body region includes a plurality of first heavily doped N-type regions arranged equidistantly, and the first heavily doped N-type regions are located in a shallow layer of the second P-type body region;
[0016] A plurality of parallel trenches each pass through the first heavily doped N-type region and the second P-type body region, the bottom of the trench is located in the base region, the trench is filled with a polysilicon layer, and the surface of the substrate in the cell region is covered with a metal layer;
[0017] The substrate surface of the terminal region has a first field oxide, the field oxide is covered with a polysilicon layer, and the polysilicon layer extends from the field oxide to the substrate surface of the terminal region; a metal layer is also provided above the polysilicon layer, and a dielectric layer is provided between the metal layer and the polysilicon layer, and the metal layer is connected to the polysilicon layer through a contact hole;
[0018] The substrate in the terminal region also has a P-type implantation region, and the P-type implantation region is connected to the metal layer on the polysilicon layer in the terminal region through a contact hole;
[0019] The substrate surface of the cut-off region has field oxygen, and the substrate on the side of the field oxygen away from the leakage detection region has a second heavily doped N-type region, the boundary of the field oxygen overlaps with the edge of the second heavily doped region, and a contact hole leads the second heavily doped N-type region to the metal layer on the surface of the cut-off region.
[0020] The process method of the IGBT device structure of the present invention comprises the following process steps:
[0021] Step 1, providing a semiconductor silicon substrate, and forming a silicon oxide layer on the surface of the substrate;
[0022] Step 2, performing photolithography and etching processes to form a window for etching a groove pattern on the silicon oxide layer;
[0023] Step 3, performing trench etching to form a gate trench of the IGBT device on the semiconductor silicon substrate; after the trench is formed, forming an oxide film on the surface of the silicon substrate;
[0024] Step 4, depositing a layer of polysilicon on the entire surface of the silicon substrate;
[0025] Step 5, coating photoresist and performing photolithography and etching to form a polysilicon pattern; the polysilicon pattern includes a polysilicon shape forming a leakage detection area and a polysilicon gate formed in a trench;
[0026] Step 6, depositing an insulating film on the entire device surface;
[0027] Step 7: Photolithography and etching process, etching to open a contact hole window on the insulating film;
[0028] Step 8: After etching the insulating film, remove the photoresist and continue etching the silicon substrate downwards using the insulating film as a hard mask;
[0029] Step 9, performing contact hole doping injection, performing doping injection in the silicon substrate at the bottom of the contact hole to form a contact area; the contact area doping injection at the bottom of the contact hole includes performing P-type doping at the bottom of the contact hole in the leakage detection area, and performing N-type doping at the bottom of the contact hole in other areas;
[0030] Step 10, performing a metal interconnect sputtering process to form a metal interconnect layer;
[0031] Step 11, depositing a passivation layer;
[0032] Step 12: Coat a polyimide layer, and after exposure and development, further etch to open the passivation layer window to expose the leakage detection area, thus forming a complete leakage detection structure.
[0033] A further improvement is that in the first step, the silicon oxide layer is used as a barrier layer for trench etching, the thickness of the silicon oxide layer is 1 to 2 um, and the silicon oxide layer is formed by a field oxygen process.
[0034] A further improvement is that in the step 3, the oxide film is used as a gate oxide film and is formed by a high-temperature furnace tube process exceeding 1000 degrees Celsius, and its thickness is 800 to 1500Å.
[0035] A further improvement is that in step 4, the thickness of the polysilicon is 8000 to 15000Å.
[0036] A further improvement is that in the fifth step, the width of the polysilicon in the leakage detection area is less than 4 um.
[0037] A further improvement is that in the sixth step, the insulating film forming process adopts a furnace tube process and a CVD process, and the thickness of the formed insulating film is 1 to 2 um.
[0038] A further improvement is that the insulating film is a silicon oxide film or a silicon nitride film.
[0039] A further improvement is that in the step 8, the silicon substrate is continuously etched downward in the contact hole window opened by the insulating film, and the etching depth of the silicon substrate is 0.2 to 0.5 um.
[0040] A further improvement is that in the step 9, the contact area of the leakage detection area is doped with P-type ion implantation, the implanted impurity is boron, and the implantation dose is 1E14-5E15CM -2 ; The contact area below the contact hole in other areas is subjected to N-type heavy doping ion implantation to form a contact area below the contact hole, the implanted impurity is arsenic, and the doping concentration of the contact area is 1E19~5E20CM -3 ; The contact area depth in the silicon substrate is 0.2~0.5um.
[0041] A further improvement is that in the step 10, the thickness of the metal interconnection layer is 1 to 5 um; after the metal is sputtered to reach the designed thickness, a photolithography development and etching process is performed, and the metal is patterned with a wet or dry etching process with the photoresist to form metal interconnections, including forming a test PAD in the leakage detection area.
[0042] A further improvement is that in step 11, the passivation layer is a silicon nitride layer having a thickness of 100 to 1000Å.
[0043] A further improvement is that after the fifth step and before the insulating film is formed, a general boron ion injection process is further included, with an injection dose of 1E12 to 1E14 cm -2 , and then carry out a high-temperature furnace tube pushing trap process above 1000 degrees Celsius.
[0044] The IGBT device structure described in the present invention utilizes the space between the terminal ring area and the cut-off area to design a new leakage detection structure for online testing on the device surface in a targeted manner. Combined with the process of the trench insulated gate transistor of the semiconductor power device, leakage in the power device process can be detected in time, solving the problem that the existing IGBT device structure cannot timely capture the leakage caused by the monitoring device structure being contaminated by phosphorus ions or the interface state defects on the device surface not being repaired in time. Monitoring can be effectively achieved to timely detect leakage, determine the size of leakage, and improve the process. It can determine whether the leakage comes from the semiconductor surface, test the size of the leakage, perform diagnosis, find the source of leakage and improve it. The purpose of improving the stability and reliability of semiconductor devices is achieved. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Figure 1 It is a cross-sectional structural diagram of the trench gate insulated gate bipolar transistor IGBT of the present invention, which is divided into a main body cell, a terminal area, a leakage detection area and a cut-off area.
[0046] Figure 2 It is a cross-sectional structural diagram of the terminal and cut-off connection of the trench insulated gate bipolar transistor IGBT of the present invention, wherein the main characteristic structure of the present invention is that a test structure is designed in the area located at the terminal and cut-off connection part to capture the surface leakage of the device.
[0047] Figure 3 The top view of the leakage detection area provided by the present invention provides a two-terminal test PAD.
[0048] Description of Reference Numerals
[0049] 1 is the back metal, 2 is the collector region (P type), 3 is the field stop layer (N+), 4 is the base region (N-), 5 is the second P type body region, 6 is the polysilicon gate, 7 is the P type doped region, 8 is the first P type body region, 9 is the contact region (P+), 10 is the second heavily doped N type region (contact region), 11 is the contact hole, 12 is the metal layer, 13 is the field oxygen, 14 is the leakage detection polysilicon, 15 is the polysilicon field plate, 16 is the silicon oxide dielectric layer, 17 is the first heavily doped N type region, and W is the leakage detection polysilicon width. DETAILED DESCRIPTION
[0050] The following is a specific implementation of the present invention in conjunction with the accompanying drawings, and the technical solutions in the present invention are clearly and completely described, but the present invention is not limited to the following implementations. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. According to the following description and claims, the advantages and features of the present invention will be clearer. It should be noted that the drawings are all in a very simplified form and use non-precise ratios, which are only used to conveniently and clearly assist in explaining the embodiments of the present invention. All other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0051] It should be understood that the present invention can be implemented in different forms, and should not be interpreted as being limited to the embodiments proposed here. On the contrary, providing these embodiments will make disclosure thorough and complete, and the scope of the present invention will be fully conveyed to those skilled in the art. In the accompanying drawings, for clarity, the size and relative size of the layer and the zone may be exaggerated, and the same reference numerals represent the same elements from beginning to end. It should be understood that when an element or layer is referred to as "on ... ", "adjacent to ... ", "connected to " or "coupled to " other elements or layers, it can be directly on other elements or layers, adjacent to it, connected or coupled to other elements or layers, or there can be an intervening element or layer. On the contrary, when an element is referred to as "directly on ... ", "directly adjacent to ... ", "directly connected to " or "directly coupled to " other elements or layers, there is no intervening element or layer. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, zones, layers and / or parts, these elements, components, zones, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer or part discussed below may be represented as a second element, component, region, layer or part.
[0052] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further described below with reference to specific diagrams.
[0053] In the process of power device structure production, phosphorus is sometimes absorbed by the device surface and boron in the device body is precipitated, which makes the device surface easily contaminated by phosphorus and generates leakage paths. Especially in the manufacturing process of high-current insulated gate bipolar transistors, leakage is more sensitive and needs to be prevented.
[0054] The present invention discloses a novel structure of a semiconductor IGBT device. Figure 1As shown, by utilizing the space between the terminal ring area and the cut-off area, combined with the process of the trench insulated gate transistor of the semiconductor power device, leakage in the power device process can be discovered in time, and the size of the leakage can be determined by testing the device structure, and debugging and diagnosis can be performed in combination with the process to solve the leakage problem. The cross section of the IGBT device structure is divided into several parts, such as the cell area, the terminal area, the leakage detection area, and the cut-off area, in the horizontal direction.
[0055] The substrate has an upper surface and a lower bottom surface, and the horizontal direction perpendicular to the longitudinal direction of the upper surface and the lower bottom surface is defined as the left and right sides, such as Figure 1 In the device, in the vertical direction, the bottom layer, that is, the bottom surface, is the back metal 1, above the back metal 1 is the P-type collector region 2, above the collector region is the N-type heavily doped field stop layer 3, and above the field stop layer is the N-type lightly doped base region 4.
[0056] The above four-layer structure is consistent across the entire device cross-section, including the cell region, terminal region, leakage detection region, and cut-off region. The back metal is used as the bottom electrode to form the collector of the IGBT device.
[0057] In the cell region, the shallow layer of the substrate is the second P-type body region 5, and the P-type body region 5 includes a plurality of equally spaced heavily doped N-type regions 17, and the heavily doped N-type regions are located in the shallow layer of the second P-type body region. A plurality of parallel trenches each pass through the heavily doped N-type region and the P-type body region, the bottom of the trench is located in the base region, a gate dielectric layer, such as a silicon oxide layer, is attached to the inner wall of the trench, and then a polysilicon layer is filled in the trench to form a trench-type gate 6.
[0058] The surface of the substrate in the cell region is covered with a metal layer 12 to form a gate electrode.
[0059] In the terminal region, the substrate surface of the terminal region has a field oxide 13, the field oxide 13 is covered with a polysilicon layer 15, and the polysilicon layer extends from the field oxide to the substrate surface of the terminal region; there is also a metal layer 12 above the polysilicon layer, and a dielectric layer is separated from the metal layer and the polysilicon layer, and the metal layer is connected to the polysilicon layer 15 through a contact hole 11.
[0060] The substrate of the terminal area also has a P-type doped area 7, and the P-type injection area is connected to the metal layer 12 on the polysilicon layer of the terminal area through another contact hole 11; the field oxygen 13 of the terminal area is located above the boundary of the P-type doped area 7, that is, part of the field oxygen is located above the P-type injection area, and the other part is located on the substrate surface outside the P-type injection area.
[0061] The leakage detection area is located between the terminal ring area and the cut-off area. In the leakage detection area, Figure 2, which is a cross-sectional view of the structure of the leakage detection area, includes a first P-type body region 8; on both sides of the P-type body region 8, namely, the side close to the terminal region and the side away from the terminal region, there are also heavily doped P-type contact regions 9; the substrate surface above the P-type body region 8 also has a polysilicon layer 14. The substrate of the entire leakage detection area is also covered with a silicon oxide dielectric layer.
[0062] A contact hole 11 is provided above the P-type contact region 9 to form a lead-out. The contact hole penetrates through the dielectric layer and extends into the P-type contact region. A metal layer is provided above the contact hole to form a metal interconnection.
[0063] The polysilicon layer 14 above the P-type body region 8 of the leakage detection region is, in a top view, Figure 3 As shown, it extends on the surface of the substrate in a tortuous serpentine shape or in other adjustable routing forms of different lengths; the width of the polysilicon does not exceed 4um, and the thickness of the polysilicon is 8000-15000Å. The length of the polysilicon routing and the thickness of the polysilicon can be adjusted as needed. A PAD area is also formed at both ends of the polysilicon layer. The PAD is made of metal and is a test point external to the leakage detection area. Various electrical signal tests can be performed on the PAD by probing. The metal thickness of the PAD area is generally 1-6.5um. The thicker the PAD, the greater the current it can withstand and the higher the durability of use, but it will also bring additional process costs.
[0064] Continue to refer Figure 1 In the cut-off region, the substrate surface has a field oxygen 13, and the substrate on the side of the field oxygen away from the leakage detection region has a heavily doped N-type region 10. The boundary of the field oxygen overlaps with the edge of the second heavily doped region, and a contact hole 11 leads the second heavily doped N-type region 10 to the metal layer 12 on the surface of the cut-off region to form an electrode.
[0065] The above structure constitutes the entire device structure of the present invention. The present invention adds a leakage detection area between the terminal area and the cut-off area, which can timely capture phosphorus ions or defects contaminated on the device surface, and can timely discover the leakage generated in the power device process. It can also conduct tests in combination with the device structure to determine the size of the leakage, and conduct debugging and diagnosis in combination with the process to solve the leakage problem.
[0066] In a certain actual detection scenario, the above leakage detection structure works as follows:
[0067] 1. At the four ports of PAD 12, use the Kelvin connection method to apply voltage symmetrically at both ends and collect current at the other two ports.
[0068] 2. The voltage ranges from 5V to 200V, with a step gradient of 50V each.
[0069] 4. The leakage specification is set to less than 1E-7 amperes.
[0070] 5. After the wafer process is completed, set up the test program.
[0071] 6. Define the coordinate position of the test PAD corresponding to the probe card.
[0072] 7. Set the test specifications into the test procedure.
[0073] 8. After the wafer process is completed, it enters the test machine and the probe card starts the corresponding test program.
[0074] 9. The probe card finds the corresponding test position based on the coordinates.
[0075] 10. Insert the probe into the corresponding PAD position for testing.
[0076] 11. Collect leakage current data and compare with set specifications.
[0077] If the leakage current data is less than the upper limit of the specification, record the data for archiving and release it to the next site. If the leakage current data is higher than the upper limit of the specification, record the data and alarm, and ask the engineer to handle it.
[0078] The above structure is manufactured by the following process method, wherein the process parameters involved are for reference only.
[0079] In the first step, a semiconductor silicon substrate is provided, and a silicon oxide layer with a thickness of 1.5 um is formed on the surface of the substrate by a field oxygen process; the silicon oxide layer serves as a barrier layer for subsequent etching of the gate trench of the IGBT device.
[0080] Step 2: coating photoresist, performing photolithography and etching processes, and forming a window for etching a groove pattern on the silicon oxide layer.
[0081] The third step is to perform trench etching to form a gate trench of the IGBT device on the semiconductor silicon substrate. After the trench is formed, a layer of oxide film is formed on the surface of the silicon substrate as a gate oxide film of the trench gate. The gate oxide film formation process adopts a high-temperature furnace tube process exceeding 1000 degrees Celsius, and finally the thickness of the gate oxide film is 1200Å.
[0082] Step 4: deposit a layer of polysilicon on the entire surface of the silicon substrate; the thickness of the polysilicon is 10000Å. The specific thickness of the polysilicon deposition needs to completely fill the trench gate and accumulate to a certain thickness on the substrate surface, which will be used to make the trench gate later, and also form the polysilicon pattern of the leakage detection area.
[0083] Step 5: Apply photoresist and perform photolithography and etching to form a polysilicon pattern; the polysilicon pattern includes the polysilicon shape forming the leakage detection area and the polysilicon gate formed in the trench. The width of the polysilicon in the leakage detection area is less than 4um, such as 2um or 3um.
[0084] After completion, a boron ion general injection process is carried out with an injection dose of 1E12~1E14CM-2, and then a high-temperature furnace tube well pushing process at more than 1000 degrees Celsius is carried out.
[0085] Step 6: deposit an insulating film on the entire device surface. The insulating film can be a silicon oxide film or a silicon nitride film. The forming process uses a furnace tube process and a CVD process, and the thickness of the formed insulating film is 2um.
[0086] Step 7: Photolithography and etching process, etching an etching window to open a contact hole on the insulating film.
[0087] Step 8: After etching the insulating film, remove the photoresist and continue to etch the silicon substrate downward using the insulating film as a hard mask; the etching depth of the silicon substrate under the insulating film is 0.2 to 0.5 um, and the parameter used in this embodiment is 0.4 um.
[0088] Step 9, perform contact hole doping injection, perform doping injection in the silicon substrate at the bottom of the contact hole to form a contact area; the contact area doping injection at the bottom of the contact hole includes P-type doping at the bottom of the contact hole in the leakage detection area, and N-type doping at the bottom of the contact hole in other areas. The contact area doping injection impurity in the leakage detection area is boron, and the injection dose is 1E14~5E15CM -2 The impurity injected into the contact area of other regions is arsenic, and the doping concentration of the contact area is 1E19~5E20CM -3 ; The contact area depth in the silicon substrate is 0.2~0.5um.
[0089] Step 10: Perform a metal interconnect sputtering process to form a metal interconnect layer. The thickness of the metal interconnect layer is 3um. After the metal sputtering reaches the designed thickness, a photolithography development and etching process is performed, and a wet or dry etching process is performed with the photoresist to pattern the metal. A test PAD in the leakage detection area is also formed. The metal thickness of the test PAD can be slightly thicker than the thickness of the metal interconnect layer to improve the mechanical strength of the PAD and the current capacity of the PAD.
[0090] In step 11, a 1000Å thick silicon nitride layer is deposited as a passivation layer to protect the device surface.
[0091] Step 12: Coat a polyimide layer, and after exposure and development, further etch to open the passivation layer window to expose the leakage detection area, thus forming a complete leakage detection structure.
[0092] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for illustrating the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which shall fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. An IGBT device structure, characterized in that: The device is formed in a semiconductor substrate. On a cross-sectional plane of the semiconductor substrate, the substrate is defined to have an upper surface and a lower bottom surface, and the horizontal direction perpendicular to the longitudinal direction of the upper surface and the lower bottom surface is the left and right sides; in the longitudinal direction of the device, the lowest layer, that is, the lower bottom surface is a back metal, above the back metal is a collector region, above the collector region is a field stop layer, and above the field stop layer is a base region; In the horizontal direction, the device is divided into multiple regions, namely, a cell region, a terminal region, a leakage detection region, and a cut-off region; the leakage detection region is located between the terminal region and the cut-off region; The leakage detection area includes a first P-type body region, and heavily doped P-type contact regions are respectively provided on both sides of the first P-type body region; the substrate surface above the first P-type body region also has a polysilicon layer; A contact hole is provided above the P-type contact area to form a lead-out, the contact hole penetrates through the dielectric layer and extends into the P-type contact area, and a metal layer is provided above the contact hole to form a metal interconnection; The polysilicon layer, in a top view, extends on the substrate surface in a serpentine shape or in other wiring forms that can be adjusted to form different lengths; PAD regions are formed at both ends of the polysilicon layer.
2. The IGBT device structure according to claim 1, characterized in that: The thickness of the polysilicon layer is 8000-15000Å; the width of the polysilicon layer is 1-4um.
3. The IGBT device structure according to claim 1, characterized in that: The PAD area is made of metal and is formed by a sputtering process; the metal thickness of the formed PAD area is 1 to 6.5 um.
4. The IGBT device structure according to claim 1, characterized in that: In the cell region, the shallow layer of the substrate is a second P-type body region, the second P-type body region includes a plurality of first heavily doped N-type regions arranged equidistantly, and the first heavily doped N-type regions are located in a shallow layer of the second P-type body region; A plurality of parallel trenches each pass through the first heavily doped N-type region and the second P-type body region, the bottom of the trench is located in the base region, the trench is filled with a polysilicon layer, and the surface of the substrate in the cell region is covered with a metal layer; The substrate surface of the terminal region has a first field oxide, the field oxide is covered with a polysilicon layer, and the polysilicon layer extends from the field oxide to the substrate surface of the terminal region; a metal layer is also provided above the polysilicon layer, and a dielectric layer is provided between the metal layer and the polysilicon layer, and the metal layer is connected to the polysilicon layer through a contact hole; The substrate in the terminal region also has a P-type implantation region, and the P-type implantation region is connected to the metal layer on the polysilicon layer in the terminal region through a contact hole; The substrate surface of the cut-off region has field oxygen, and the substrate on the side of the field oxygen away from the leakage detection region has a second heavily doped N-type region, the boundary of the field oxygen overlaps with the edge of the second heavily doped N-type region, and a contact hole leads the second heavily doped N-type region to the metal layer on the surface of the cut-off region.
5. A process for manufacturing the IGBT device structure according to claim 1, characterized in that: The process steps include: Step 1, providing a semiconductor silicon substrate, and forming a silicon oxide layer on the surface of the substrate; Step 2, performing photolithography and etching processes to form a window for etching a groove pattern on the silicon oxide layer; Step 3, performing trench etching to form a gate trench of the IGBT device on the semiconductor silicon substrate; After the grooves are formed, an oxide film is formed on the surface of the silicon substrate; Step 4, depositing a layer of polysilicon on the entire surface of the silicon substrate; Step 5, coating photoresist and performing photolithography and etching to form a polysilicon pattern; the polysilicon pattern includes a polysilicon shape forming a leakage detection area and a polysilicon gate formed in a trench; Step 6, depositing an insulating film on the entire device surface; Step 7: Photolithography and etching process, etching to open a contact hole window on the insulating film; Step 8: After etching the insulating film, remove the photoresist and continue etching the silicon substrate downwards using the insulating film as a hard mask; Step 9, performing contact hole doping injection, performing doping injection in the silicon substrate at the bottom of the contact hole to form a contact area; the contact area doping injection at the bottom of the contact hole includes performing P-type doping at the bottom of the contact hole in the leakage detection area, and performing N-type doping at the bottom of the contact hole in other areas; Step 10, performing a metal interconnect sputtering process to form a metal interconnect layer; Step 11, depositing a passivation layer; Step 12: Coat a polyimide layer, and after exposure and development, further etch to open the passivation layer window to expose the leakage detection area, thus forming a complete leakage detection structure.
6. The process method for the IGBT device structure according to claim 5, characterized in that: In the first step, the silicon oxide layer is used as a barrier layer for trench etching. The thickness of the silicon oxide layer is 1 to 2 um and is formed by a field oxygen process.
7. The process method for the IGBT device structure according to claim 5, characterized in that: In the third step, the oxide film is used as a gate oxide film and is formed by a high-temperature furnace tube process exceeding 1000 degrees Celsius, and its thickness is 800 to 1500Å.
8. The process method for the IGBT device structure according to claim 5, characterized in that: In the fourth step, the thickness of the polysilicon is 8000 to 15000 Å.
9. The process method for the IGBT device structure according to claim 5, characterized in that: In the fifth step, the width of the polysilicon in the leakage detection area is less than 4 um.
10. The process method for the IGBT device structure according to claim 5, characterized in that: In the sixth step, the insulating film is formed by furnace tube process and CVD process, and the thickness of the formed insulating film is 1-2 um.
11. The process method for the IGBT device structure according to claim 10, characterized in that: The insulating film is a silicon oxide film or a silicon nitride film.
12. The process for the IGBT device structure according to claim 5, characterized in that: In the eighth step, the silicon substrate is continuously etched downward in the contact hole window opened by the insulating film, and the etching depth of the silicon substrate is 0.2-0.5 um.
13. The process method for the IGBT device structure according to claim 5, characterized in that: In the ninth step, the contact area of the leakage detection area is doped with P-type ion implantation, the implanted impurity is boron, and the implantation dose is 1E14-5E15CM -2 ; The contact area below the contact hole in other areas is implanted with N-type heavily doped ions to form the contact area below the contact hole. The implanted impurity is arsenic. The doping concentration of the contact area is 1E19-5E20CM -3 ; The contact area depth in the silicon substrate is 0.2~0.5um.
14. The process method for the IGBT device structure according to claim 5, characterized in that: In the step 10, the thickness of the metal interconnection layer is 1 to 5 um; after the metal sputtering reaches the designed thickness, photolithography development and etching processes are performed, and the metal is patterned with a wet or dry etching process with the photoresist to form metal interconnections, including forming a test PAD in the leakage detection area.
15. The process method for the IGBT device structure according to claim 5, characterized in that: In the step 11, the passivation layer is a silicon nitride layer, and the thickness thereof is 100 to 1000Å.
16. The process method for the IGBT device structure according to claim 5, characterized in that: After step 5 and before the insulating film is formed, a general boron ion injection process is also included, with an injection dose of 1E12 to 1E14 cm -2 , and then carry out a high-temperature furnace tube pushing trap process above 1000 degrees Celsius.
Citation Information
Patent Citations
IGBT (insulated gate bipolar transistor) chip integrating temperature and current sensing function
CN102881679A