Semiconductor device and method for forming the same

By using a flat probe tip to contact a soft metal sacrificial test pad, the high cost of needle-shaped probe tips and the material limitations of flat tips in the prior art are solved, achieving efficient and low-cost semiconductor wafer testing and simplifying downstream processing.

CN113658932BActive Publication Date: 2024-11-12TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110843953.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-03-08
Filing Date
2021-07-26
Publication Date
2024-11-12
Estimated Expiration
2041-07-26

AI Technical Summary

Technical Problem

In existing semiconductor wafer testing, needle-shaped probe tips are costly, difficult to maintain, and leave marks after testing, while flat tips can only be used for soft materials, resulting in low testing efficiency and complex downstream processing.

Method used

The test is performed by contacting the soft metal sacrificial test pad with a flat probe tip, and the pad is removed after the test. Soft metal materials such as tin or lead-tin alloy are used as sacrificial test pads. The pads are removed after the test to avoid leaving traces.

Benefits of technology

Reduce testing time, increase yield, lower costs, and simplify downstream processing, while remaining compatible with SoC and SoIC processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113658932B_ABST
    Figure CN113658932B_ABST
Patent Text Reader

Abstract

The device includes a semiconductor die. The semiconductor die includes a device layer, an interconnect layer above the device layer, a conductive pad above the interconnect layer, a conductive seed layer directly on the conductive pad, and a passivation layer that seals the conductive pad and the conductive seed layer. Embodiments of the present application also relate to semiconductor devices and methods for forming the same.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present application relate to semiconductor devices and methods of forming the same. Background Art

[0002] The semiconductor integrated circuit (IC) industry has experienced exponential growth. Technological advances in IC materials and design have produced generations of ICs, each with smaller and more complex circuits than the previous one. During the evolution of ICs, functional density (i.e., the number of interconnected devices per chip area) has generally increased, while geometry size (i.e., the smallest component (or line) that can be formed using a manufacturing process) has decreased. This scaling down process generally provides benefits by increasing production efficiency and reducing associated costs. This scaling down has also increased the complexity of processing and manufacturing ICs, and similar developments in IC processing and manufacturing are needed to achieve these advances.

[0003] For example, one area of ​​manufacturing that has room for improvement is wafer testing, a mechanism for determining device performance and manufacturing defects. Before singulation (removing circuit elements (such as chips) from semiconductor wafers), the electrical performance of test structures and functional devices on the wafer is evaluated. Wafer test systems typically use probe cards, which include hundreds or thousands of probe tips for making firm electrical connections to test pads on the wafer. The probe tips can be needle tips (or rounded tips) or flat tips. Compared to flat tips, needle tips are more expensive to manufacture, more difficult to maintain, and have a shorter service life than flat tips. In addition, the use of needle tips typically leaves marks on the test pads after testing, which is undesirable for subsequent processing. Flat tips can be used for larger test areas and are more economically feasible than needle tips, but can only be used to contact soft materials. Summary of the invention

[0004] Some embodiments of the present application provide a semiconductor device, comprising: a semiconductor die, including a device layer, an interconnect layer above the device layer, a conductive pad above the interconnect layer, a conductive seed layer directly on the conductive pad, and a passivation layer sealing the conductive pad and the conductive seed layer.

[0005] Other embodiments of the present application provide a method for forming a semiconductor device, comprising: providing an integrated circuit (IC) die, wherein the IC die comprises an interconnect layer, a first passivation layer above the interconnect layer, and a conductive pad above the first passivation layer and electrically connected to the interconnect layer; forming a seed layer above the conductive pad; forming a sacrificial test pad above the seed layer; performing a test on the IC die, wherein performing the test comprises contacting a flat probe tip with the sacrificial test pad; and removing the sacrificial test pad after performing the test.

[0006] Still other embodiments of the present application provide a method for forming a semiconductor device, comprising: providing an integrated circuit (IC) die, wherein the IC die comprises an interconnect layer, a first passivation layer above the interconnect layer, and a conductive pad above the first passivation layer and electrically connected to the interconnect layer; forming a patterned mask above the conductive pad, wherein the patterned mask provides an opening above the conductive pad; forming a seed layer above the conductive pad in the opening; forming a sacrificial test pad above the seed layer in the opening; removing the patterned mask; performing a test on the IC die, wherein performing the test comprises contacting the sacrificial test pad with a probe tip; after performing the test, removing the sacrificial test pad; and forming a second passivation layer above the first passivation layer, the conductive pad, and the seed layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] When read in conjunction with the accompanying drawings, various aspects of the present disclosure can be best understood from the following detailed description. It should be emphasized that, in accordance with standard practice in the industry, the various components are not drawn to scale. In fact, for the sake of clarity of discussion, the size of the various components can be arbitrarily increased or reduced.

[0008] Figure 1 A flow chart of a method for manufacturing a wafer and an IC according to an embodiment of the present disclosure is shown.

[0009] Figure 2A , Figure 2B , Figure 2C , Figure 2D , Figure 2E , Figure 2F , Figure 2G , Figure 2H and Fig.2I According to the embodiment of the present disclosure Figure 1 A cross-sectional view of a portion of a semiconductor device during various fabrication stages in a method.

[0010] Figure 3 A flow chart of a method of manufacturing a wafer and an IC according to another embodiment of the present disclosure is shown.

[0011] Figure 4A , Figure 4B , Figure 4C , Figure 4D , Figure 4E , Figure 4F , Figure 4G , Figure 4H , Fig. 4I and Figure 4J According to the embodiment of the present disclosure Figure 3 A cross-sectional view of a portion of a semiconductor device during various fabrication stages in a method.

[0012] Figure 5 A flow chart of a method for manufacturing a wafer and an IC according to an embodiment of the present disclosure is shown.

[0013] Figure 6A-1 , Figure 6A-2 , Figure 6A-3 , Figure 6A-4 , Figure 6B-1 , Figure 6B-2 , Figure 6B-3 , Figure 6B-4 and Figure 6C According to the embodiment of the present disclosure Figure 5 A cross-sectional view of a portion of a semiconductor device during various fabrication stages in a method.

[0014] Figure 7 A flow chart of a method for manufacturing a wafer and an IC according to an embodiment of the present disclosure is shown.

[0015] Figure 8A-1 , Figure 8A-2 , Figure 8B-1 and Figure 8B-2 According to the embodiment of the present disclosure Figure 7 A cross-sectional view of a portion of a semiconductor device during a manufacturing stage in a method. DETAILED DESCRIPTION

[0016] The following disclosure provides many different embodiments or examples of different components for implementing the provided subject matter. Specific examples of components and arrangements are described below to simplify the present disclosure. Of course, these are merely examples and are not intended to be limiting. For example, in the following description, a first component formed above or on a second component may include an embodiment in which the first component and the second component are formed in direct contact, and may also include an embodiment in which an additional component may be formed between the first and second components so that the first and second components may not be in direct contact. In addition, the present disclosure may repeat reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself specify the relationship between the various embodiments and / or the structures discussed.

[0017] In addition, spatially relative terms, such as "under," "beneath," "lower," "above," "upper," and the like, may be used herein for ease of description to describe the relationship of one element or component to another element or component shown in the figures. Spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or in other orientations), and the spatially relative descriptors used herein may likewise be interpreted accordingly. In addition, when "about," "approximately," and the like are used to describe a value or a range of values, unless otherwise indicated, the term encompasses values ​​within some variation (e.g., + / - 10% or other variation) of the described value, based on the particular technology disclosed herein and according to the knowledge of those skilled in the art. For example, the term "about 5 nm" encompasses a size range from 4.5 nm to 5.5 nm, 4.0 nm to 5.0 nm, and the like.

[0018] The present disclosure generally relates to semiconductor devices and methods of forming the same. More specifically, the present disclosure relates to methods and structures for testing integrated circuit (IC) dies and assembling known good dies (KGDs) into SoC (system on chip) packages or SoIC (system on integrated chip) packages.

[0019] Before the IC dies are assembled into a SoC or SoIC package, the IC dies are tested to ensure that they are good (known good dies). Testing of the IC dies can be performed using a probe tip to electrically contact a test pad (such as an aluminum (Al) pad) on the IC die. One type of probe tip is a needle tip. The use of a needle tip requires a high degree of precision in tip alignment, which reduces test throughput. Moreover, the use of a needle tip typically leaves marks on the test pad, which is undesirable in some applications and may require downstream processing to remove the marks. On the other hand, this reduces manufacturing yield. Another type of probe tip is a flat tip. A flat tip can be used for a larger test area and is more economically feasible than a needle tip, but can only be used to contact soft materials (e.g., materials softer than aluminum).

[0020] The present disclosure provides a method and structure for solving the above-mentioned problems by performing a test using a flat probe tip. In an embodiment of the present disclosure, a seed layer is formed above a test pad (such as an Al pad) of an IC die, and a soft metal material such as tin (Sn) is formed above the seed layer. The IC die is tested by contacting the flat probe tip with the soft metal material. After the test is completed, the soft metal material is removed, and no probe traces are left on the seed layer and the test pad. Then, the IC die is processed by a downstream process to form a SoC or SoIC. For example, a planarization layer can be formed above the seed layer and the test pad, and a bonding pad can be formed above the planarization layer. In addition, a plurality of ICs can be bonded to form a SoIC or a portion thereof using hybrid bonding. For another example, microbumps and solder balls can be formed directly on the seed layer or the test pad to form a SoC. The present disclosure provides the following benefits. First, by using a flat probe, the test time can be reduced, the yield can be increased, and the test cost can be reduced. Secondly, using the disclosed method, the probe test will not leave traces on the test pad, which simplifies downstream processing. Third, the disclosed method and structure are compatible with SoC process flow and SoIC process flow. Figures 1 to 8B-2 These and other aspects of the disclosure are discussed further below.

[0021] Figure 1 A flow chart of a method 10 of manufacturing (including testing and assembling) a semiconductor structure (also referred to as a structure, semiconductor device, or device) 100 in accordance with various aspects of the present disclosure is shown. Structure 100 may include one or more IC dies tested and assembled in accordance with embodiments of the present disclosure. Method 10 is merely an example and is not intended to limit the present disclosure beyond the scope expressly recited in the claims. Other operations may be provided before, during, and after method 10, and some of the operations described may be replaced, eliminated, or moved for other embodiments of the method. Figure 2A-2I Method 10 is described.

[0022] At operation 12, method 10 ( Figure 1 ) is provided or disposed with structure 100 during an intermediate manufacturing stage. In one embodiment, structure 100 is a semiconductor wafer having one or more IC dies formed thereon. Figure 2A , the structure 100 includes a device layer 110, an interconnect layer 120 above the device layer 110, and a passivation layer 130 above the interconnect layer 120. The device layer 110 and the interconnect layer 120 are electrically connected through various conductive features 112 such as contacts, vias, wirings, and the like.

[0023] The device layer 110 includes a substrate, which may include an elemental semiconductor such as silicon or germanium and / or a compound semiconductor such as silicon germanium, silicon carbide, gallium arsenide, indium arsenide, gallium nitride, and indium phosphide. Other exemplary substrates include alloy semiconductors such as silicon germanium carbide, gallium arsenide phosphide, and indium gallium phosphide. The substrate may have one or more layers defined therein. In some embodiments, the substrate layer includes an epitaxial layer. In one such embodiment, the substrate includes an epitaxial layer overlying a bulk semiconductor. Other layered substrates include semiconductor-on-insulator (SOI) substrates. In one such SOI substrate, the substrate includes a buried oxide (BOX) layer formed by a process such as isolation by implantation of oxygen (SIMOX). The device layer 110 includes various functional devices or components formed in or on the substrate, such as field effect transistors (FETs), metal oxide semiconductor (MOS) transistors, bipolar junction transistors (BJTs), imaging sensors, memory devices such as SRAMs, and combinations thereof. The functional devices or components may be insulated from each other by isolation components such as shallow trench isolation (STI) components.

[0024] The interconnect layer 120 includes a combination of a plurality of patterned dielectric layers 124 and a patterned conductive layer 122 to form an interconnect configured to couple various functional components in the device layer 110. The dielectric layer 124 may include materials such as oxides formed from tetraethyl orthosilicate (TEOS), undoped silicate glass, or doped silicon oxide, such as borophosphosilicate glass (BPSG), fluorine-doped silicate glass (FSG), phosphosilicate glass (PSG), boron-doped silicate glass (BSG), and / or other suitable dielectric materials. The dielectric layer 124 may be deposited by a PECVD process, a flowable CVD (FCVD) process, or other suitable deposition techniques. The conductive layer 122 may include copper (Cu), aluminum (Al), tungsten (W), cobalt (Co), other metals, metal nitrides such as titanium nitride (TiN), titanium aluminum nitride (TiAlN), tungsten nitride (WN), tantalum nitride (TaN), or combinations thereof, and may be formed by CVD, PVD, plating, and / or other suitable processes.

[0025] A passivation layer 130 is formed over the interconnect layer 120 using a suitable process, such as a deposition process and a chemical mechanical polishing (CMP) process. In one embodiment, the passivation layer 130 includes a dielectric material, such as silicon oxide (SiO2), silicon nitride (Si3N4), silicon oxynitride (SiON), or a combination thereof, and may include a single layer of dielectric material or multiple layers of dielectric material.

[0026] At operation 14, method 10 ( Figure 1 ) forming a conductive pad 132 over the passivation layer 130, such as Figure 2B. Conductive pad 132 penetrates passivation layer 130 and is electrically connected to top metal layer 122 in interconnect layer 120. In an embodiment, conductive pad 132 includes an aluminum (Al) pad and may be referred to as an aluminum (Al) pad. In alternative embodiments, conductive pad 132 may include other conductive materials, such as aluminum copper alloy (AlCu), copper (Cu), or titanium (Ti). In one embodiment, operation 14 includes patterning passivation layer 130 using photolithography and etching processes to form an opening therein. The opening exposes an area of ​​the top metal layer in interconnect layer 120. Subsequently, operation 14 includes depositing a layer of one or more conductive materials into the opening and depositing over the top surface of passivation layer 130. Then, operation 14 includes patterning a layer of one or more conductive materials to remove portions thereof. The remaining portion of the layer of one or more conductive materials becomes conductive pad 132. In an embodiment, conductive pad 132 may be deposited using electroplating, chemical plating, CVD, PVD, or other deposition techniques, and has a thickness in the range of about 2 μm to about 5 μm.

[0027] At operation 16, according to an embodiment, method 10 ( Figure 1 ) A patterned mask 133 is formed over the passivation layer 130 and the conductive pad 132, such as Figure 2C As shown in . The patterned mask 133 provides an opening 135 directly above the conductive pad 132 and exposes a portion of the conductive pad 132. In an embodiment, one opening 135 is provided above one conductive pad 132. In an embodiment, the patterned mask 133 is formed using a process including deposition, photolithography, and etching. In an embodiment, the patterned mask 133 includes a patterned photoresist (or resist). In another embodiment, the patterned mask 133 includes a patterned resist above a patterned anti-reflective coating (ARC) layer. In various embodiments, the patterned mask 133 may include other materials. The material of the patterned mask 133 is selected to provide etching selectivity relative to the passivation layer 130 and the conductive pad 132. For example, the patterned mask 133 may be etched or removed in an etching process in which there is no or minimal etching of the passivation layer 130 and the conductive pad 132. As shown in Figure 2C As shown in FIG. 1 , some areas of the conductive pad 132 are covered by a patterned mask 133 .

[0028] At operation 18, method 10 ( Figure 1 ) forms a seed layer 134 in the opening 135 and on the conductive pad 132, such as in Figure 2D In an embodiment, the seed layer 134 is formed directly on the conductive pad 132. The seed layer 134 serves as a connection between the conductive pad 132 and the subsequently deposited sacrificial test pad 136 ( Figure 2E) between the adhesive layer and / or barrier layer. Therefore, the selection of the material for seed layer 134 depends on the material of conductive pad 132 and sacrificial test pad 136. In an embodiment, conductive pad 132 includes aluminum, and seed layer 134 includes titanium copper (TiCu). For example, seed layer 134 may include a titanium layer and a copper layer above the titanium layer. In an embodiment, the titanium layer may have a thickness of about 100 Å. to about The copper layer may have a thickness in the range of about to about The titanium layer serves as an adhesion and barrier layer to prevent copper diffusion, while the copper layer serves as a seed layer for depositing sacrificial test pad 136. In some embodiments, seed layer 134 includes a nickel layer as a stress buffer layer. The nickel layer may have a thickness in the range of about 500 nm to about 1000 nm. In some embodiments, seed layer 134 includes a titanium nitride layer. ALD, PVD, CVD, or other techniques may be used to deposit seed layer 134.

[0029] At operation 20, method 10 ( Figure 1 ) forming a sacrificial test pad 136 over the seed layer 134, such as Figure 2E As shown in . In an embodiment, the sacrificial test pads 136 include a soft material so that they can be contacted by a flat probe tip for testing. In an embodiment, the sacrificial test pads 136 include a material softer than aluminum. In an embodiment, the sacrificial test pads 136 include tin (Sn). In an alternative embodiment, the sacrificial test pads 136 include a lead-tin alloy (PbSn). The PbSn alloy may have a high lead-tin ratio (more lead than tin), in an embodiment, such as about 95% lead and about 5% tin. The PbSn alloy may have a low lead-tin ratio (less lead than tin), such as about 37% lead and about 63% tin in an embodiment, or about 40% lead and about 60% tin in another embodiment. In some embodiments, the sacrificial test pads 136 include a lead-free solder material, such as a compound having tin (Sn), silver (Ag) and copper (Cu). In another embodiment, the compound further contains zinc (Zn), thereby producing a Sn-Ag-Cu-Zn compound. In another embodiment, the compound further includes manganese (Mn), making it a Sn-Ag-Cu-Mn compound. In various embodiments, the sacrificial test pad 136 may include other materials. In an embodiment, the sacrificial test pad 136 may be deposited using electroplating, chemical plating, or other deposition techniques, and may have a thickness in a range of about 1 μm to about 2 μm.

[0030] At operation 22, method 10 ( Figure 1 ) removes the patterned mask 133 from the structure 100, in an embodiment such as Figure 2FIn an embodiment, the patterned mask 133 includes a patterned resist and can be removed using a resist stripping or other method. In various embodiments, operation 22 can remove the patterned mask 133 using a stripping, ashing or etching method without etching the passivation layer 130, the conductive pad 132, the seed layer 134 and the sacrificial test pad 136.

[0031] At operation 24, method 10 ( Figure 1 ) Tests are performed on the structure 100 by electrically contacting the probe tip 138 with the sacrificial test pad 136. Operation 24 may include aligning the probe tip 138 with the sacrificial test pad 136, electrically contacting the sacrificial test pad 136 with the probe tip 138, applying a test stimulus to the structure 100 including the IC die, collecting responses from the structure 100, and analyzing the responses. Various IC dies in the structure 100 may be identified as good dies (passed the test) or bad dies (failed the test). In an embodiment, the identified good dies are passed to downstream processing, such as being packaged as separate chips or joined with other known good dies to form a SoC or SoIC. In an embodiment, the probe tip 138 is a flat tip. The manufacture and maintenance of the flat probe tip is more economical than the needle tip, so the manufacturing cost can be reduced. The sacrificial test pad 136 is designed with a soft material, allowing the flat probe tip 138 to form a firm electrical connection therewith. In an alternative embodiment, the probe tip 138 may be a needle tip. In various embodiments, the probe tip 138 may have any suitable shape. In some embodiments, contacting the probe tip 138 to the sacrificial test pad 136 may leave a mark on the sacrificial test pad 136 .

[0032] At operation 26, for example, after the test is completed, method 10 ( Figure 1 ) removes the sacrificial test pad 136 from the structure 100. The sacrificial test pad 136 may be removed by a suitable etching process, such as a wet etch or a dry etch that is selective to the material of the sacrificial test pad 136, and has little or no etching of the passivation layer 130, the seed layer 134, and the conductive pad 132. Traces on the sacrificial test pad 136 caused by the test (operation 24) are also removed. In an embodiment, the resulting structure 100 is Figure 2H Shown in.

[0033] At operation 28, method 10 ( Figure 1 ) forms a passivation layer 140 that seals the seed layer 134 and the conductive pad 132, such as Fig.2I As shown in Fig.2IAs shown in , the passivation layer 140 is deposited over the passivation layer 130, the conductive pad 132, and the seed layer 134. In an embodiment, the passivation layer 140 may include the same or similar material as the passivation layer 130. In an embodiment, the passivation layer 140 includes a dielectric material, such as silicon oxide (SiO2), silicon nitride (Si3N4), silicon oxynitride (SiON), or a combination thereof, and may include a layer of dielectric material or multiple layers of dielectric material. The passivation layer 140 may be formed by CVD, PECVD, flowable CVD, or other suitable methods. The seed layer 134 is sealed between the conductive pad 132 and the passivation layer 140. The method 10 may be performed with respect to the structure 100 with further steps, such as packaging or bonding, which will be referred to later. Figure 5 and Figure 7 Have a discussion.

[0034] Figure 3 A flow chart of a method 10 of manufacturing a semiconductor structure 100 according to another embodiment of the present disclosure is shown. Figure 3 The method 10 in the present invention is merely an example and is not intended to limit the present disclosure beyond the scope explicitly recited in the claims. Additional operations may be provided before, during, and after the method 10, and some of the operations described may be replaced, eliminated, or moved for additional embodiments of the method. Figure 4A-4J Method 10 is described.

[0035] At operation 12, method 10 ( Figure 3 ) is provided or disposed with structure 100 during an intermediate manufacturing stage. In an embodiment, structure 100 is a semiconductor wafer having one or more IC dies formed thereon. Figure 4A , the structure 100 includes a device layer 110 , an interconnect layer 120 above the device layer 110 , and a passivation layer 130 above the interconnect layer 120 . Figure 3 Operation 12 and Figure 1 The operation 12 is the same as in.

[0036] At operation 13, method 10 ( Figure 3 ) A seed layer 131 is formed over the passivation layer 130. According to one embodiment, for example, Figure 4B The seed layer 131 is deposited on the top surface of the passivation layer 130 and in the opening 129 ( Figure 4B120). The seed layer 131 is electrically connected to the top metal layer in the interconnect layer 120 through the opening 129. In an embodiment, operation 13 includes patterning the passivation layer 130 using a photolithography and etching process to form an opening 129 therein. The opening 129 exposes an area of ​​the top metal layer in the interconnect layer 120. Subsequently, operation 13 includes depositing a seed layer 131 in the opening 129 and over the top surface of the passivation layer 130. In an embodiment, the seed layer 131 is used as a conductive pad 132 ( Figure 4D ) of copper deposition. For example, the seed layer 131 may include titanium and copper. For example, the seed layer 131 may include a titanium layer and a copper layer above the titanium layer. In an embodiment, the titanium layer may have a thickness of about to about The copper layer may have a thickness in the range of about to about The titanium layer is used as an adhesion and barrier layer to prevent copper diffusion, while the copper layer is used as a seed layer for depositing the conductive pad 132. In various embodiments, the seed layer 131 may include copper, copper alloy, aluminum, titanium, titanium alloy, or a combination thereof. The seed layer 131 may include one or more layers of metal and may be formed by ALD, CVD, or PVD processes.

[0037] At operation 15, according to an embodiment, method 10 ( Figure 3 ) A patterned mask 133 is formed over the seed layer 131, such as Figure 4C . The patterned mask 133 provides openings 135 directly above the openings 129 and exposes a portion of the seed layer 131. From a top view, each opening 135 is larger than the corresponding opening 129. The size and shape of the openings 135 are appropriately designed for the conductive pads 132 ( Figure 4D ). In an embodiment, the patterned mask 133 is formed using a process including deposition, photolithography, and etching. In an embodiment, the patterned mask 133 includes a patterned photoresist (or resist). In another embodiment, the patterned mask 133 includes a patterned resist over a patterned anti-reflective coating (ARC) layer. In various embodiments, the patterned mask 133 may include other materials. The material of the patterned mask 133 is selected to provide etching selectivity relative to the passivation layer 130, the seed layer 131, and the conductive pad 132. For example, the patterned mask 133 may be etched or removed in an etching process, which has no or minimal etching on the passivation layer 130 and the conductive pad 132.

[0038] At operation 17, according to an embodiment, method 10 ( Figure 3 ) forming a conductive pad 132 on the seed layer 131, such as Figure 4DAs shown in . A portion of the conductive pad 132 is deposited to fill the opening 129, and another portion of the conductive pad 132 is deposited over the passivation layer 130. The shape and size of the conductive pad 132 are limited by the shape and size of the opening 135. The conductive pad 132 is electrically connected to the top metal layer in the interconnect layer 120 through the seed layer 131. In an embodiment, the conductive pad 132 includes a copper (Cu) pad and may be referred to as a copper (Cu) pad. In alternative embodiments, the conductive pad 132 may include other conductive materials, such as aluminum, aluminum-copper alloy (AlCu), or titanium (Ti). In an embodiment, the conductive pad 132 may be deposited using electroplating, chemical plating, CVD, PVD, or other deposition techniques, and may have a thickness in the range of about 2 μm to about 5 μm.

[0039] At operation 19, method 10 ( Figure 3 ) Another seed layer 134 is formed in the opening 135 and on the conductive pad 132, such as Figure 4E In an embodiment, the seed layer 134 is formed directly on the conductive pad 132. In an embodiment, the seed layer 134 serves as a conductive pad 132 and a subsequently deposited sacrificial test pad 136 ( Figure 4F ) between the conductive pads 132 and the sacrificial test pads 136. Therefore, the selection of the material for the seed layer 134 depends on the materials of the conductive pads 132 and the sacrificial test pads 136. In an embodiment, the conductive pads 132 include copper, the seed layer 134 includes nickel, and the sacrificial test pads 136 include tin or other suitable solder materials. For example, the nickel layer may have a thickness in the range of about 500 nm to about 1000 nm. In various embodiments, the seed layer 134 includes other suitable materials, such as a titanium nitride layer. The seed layer 134 may be deposited using ALD, PVD, or CVD. In an embodiment of method 10, operation 19 is optional and the seed layer 134 may be omitted.

[0040] At operation 21, method 10 ( Figure 3 ) forming a sacrificial test pad 136 over the seed layer 134, such as Figure 4F. In an embodiment of method 10 in which seed layer 134 is omitted, sacrificial test pads 136 are deposited directly on conductive pads 132. In an embodiment, sacrificial test pads 136 include a soft material so that they can be contacted by a flat probe tip for testing. In an embodiment, sacrificial test pads 136 include a material softer than aluminum. In an embodiment, sacrificial test pads 136 include tin (Sn). In an alternative embodiment, sacrificial test pads 136 include a lead-tin alloy (PbSn). In an embodiment, the PbSn alloy may have a high lead-tin ratio (more lead than tin), such as about 95% lead and about 5% tin. The PbSn alloy may have a low lead-tin ratio (less lead than tin), such as about 37% lead and about 63% tin in an embodiment, or about 40% lead and about 60% tin in another embodiment. In some embodiments, sacrificial test pads 136 include a lead-free solder material, such as a compound with tin (Sn), silver (Ag), and copper (Cu). In a further embodiment, the compound further includes zinc (Zn), making a Sn-Ag-Cu-Zn compound. In another further embodiment, the compound further includes manganese (Mn), making a Sn-Ag-Cu-Mn compound. In various embodiments, the sacrificial test pad 136 may include other materials. In an embodiment, the sacrificial test pad 136 may be deposited using electroplating, chemical plating, or other deposition techniques, and may have a thickness in the range of about 1 μm to about 2 μm.

[0041] At operation 23, method 10 ( Figure 3 ) removes the patterned mask 133 and the portion of the seed layer 131 directly below the patterned mask 133, such as in Figure 4G As shown in Figure 4G In the embodiment shown in , from a top view, the remaining seed layer 131, the conductive pad 132, the seed layer 134 (if present), and the sacrificial test pad 136 are coextensive. In an embodiment, operation 23 can remove the patterned mask 133 using a first method, and remove the portion of the seed layer 131 directly below the patterned mask 133 using a second method. For example, in an embodiment, the patterned mask 133 is a patterned resist and can be removed using a resist strip, and a portion of the seed layer 131 is removed using an etching process that is selective to the material of the seed layer 131, and little to no etching of the sacrificial test pad 136, the passivation layer 130, the seed layer 134 (if present), and the conductive pad 132. The etching can be dry etching, wet etching, or other suitable etching methods.

[0042] At operation 24, method 10 ( Figure 3 ) Testing of structure 100 is performed by contacting probe tip 138 with sacrificial test pad 136, such as in Figure 4H This is consistent with Figure 1 The same as operation 24 in. At operation 26, method 10 ( Figure 3 ) After completing the test of the structure 100, the sacrificial test pad 136 is removed, such as in Fig. 4I If a seed layer 134 is present, it is deposited on the conductive pad 132, and the conductive pad 132 is deposited on the crystal layer 131. Figure 1 The operation 26 in is the same.

[0043] At operation 27, method 10 ( Figure 3 ) A passivation layer 140 is formed over the passivation layer 130 and seals the seed layer 134 (if present), the conductive pad 132 and the seed layer 131, such as in Figure 4J Other aspects of operation 27 are the same as those of operation 28.

[0044] From operation 28 ( Figure 1 ) or operation 27( Figure 3 ), method 10 may continue to further process structure 100. Figure 5 An embodiment of a method 10 for such further processing is shown in Figure 7 Another embodiment of a method 10 for such further processing is shown in FIG. Figure 5 and Figure 7 The method 10 in the embodiment is merely an example and is not intended to limit the present disclosure beyond the scope explicitly recited in the claims. Figure 5 and Figure 7 Additional operations are provided before, during, and after the method 10 in the embodiment of the present invention, and some of the operations described may be replaced, eliminated, or moved for additional embodiments of the method. Figure 6A-1 Figure 6A-4 , Figure 6B-1 Figure 6B-4 and Figure 6C describe Figure 5 The following is an embodiment of the method 10. Figure 8A-1 Figure 8A-2 and Figure 8B-1 Figure 8B-2 describe Figure 7 An embodiment of method 10.

[0045] refer to Figure 5 , method 10 starts from operation 28 ( Figure 1 and Fig.2I ) or operation 27( Figure 3 and Figure 4J) proceeds to operation 30. At operation 30, method 10 forms a metal bonding pad and a bonding pad via. Figure 6A-1 , Figure 6A-2 , Figure 6A-3 and Figure 6A-4 It shows that Fig.2I An example of a structure 100 performing operation 30 on the structure 100 is shown. Figure 6A-1 , a dielectric layer 144 is formed over the passivation layer 140, a bonding pad 146 is formed in the dielectric layer 144, and a bonding pad via 142 is formed to connect the bonding pad 146 to the top metal layer in the interconnect layer 120. The dielectric layer 144 may include silicon oxide (SiO2), silicon nitride (Si3N4), silicon oxynitride (SiON), a low-k material, or other suitable dielectric material. In an embodiment, the bonding pad 146 and the bonding pad via 142 may include a metal, such as copper, and in alternative embodiments may include other metals or metal alloys, such as gold, silver, aluminum, nickel, palladium, tungsten, or compounds thereof. The top metal layer in the interconnect layer 120 may include the same or different material as the bonding pad 146 and the bonding pad via 142. Reference Figure 6A-2 In this embodiment, at least one bonding pad via 142 is disposed on the seed layer 134 and connects the bonding pad 146 to the seed layer 134 and the conductive pad 132. Figure 6A-3 In this embodiment, at least one bonding pad via 142 is disposed on an area of ​​the conductive pad 132 that is not covered by the seed layer 134. The area on the conductive pad 132 for locating the bonding pad via 142 can be defined by the area covered by the patterned mask 133 ( Figure 2C ). refer to Figure 6A-4 In this embodiment, operation 30 further forms an etch stop layer 148 between the passivation layer 140 and the dielectric layer 144. The etch stop layer 148 includes a dielectric material different from the dielectric layer 144, and may include silicon oxide (SiO2), silicon nitride (Si3N4), silicon oxynitride (SiON), or other suitable dielectric materials. Figure 6A-1 , Figure 6A-2 , Figure 6A-3 and Figure 6A-4 Any of the components shown in can be combined to form additional embodiments of structure 100. For example, in some embodiments, structure 100 includes some bonding pad vias 142 disposed on the top metal layer of interconnect layer 120, some bonding pad vias 142 disposed on seed layer 134, and some bonding pad vias disposed on conductive pads 132. Figure 6A-1 , Figure 6A-2 and Figure 6A-3 Any of the embodiments shown in may further include an etch stop layer 148 .

[0046] Figure 6B-1 , Figure 6B-2 , Figure 6B-3 and Figure 6B-4 It shows that Figure 4J An example of a structure 100 in which operation 30 is performed on the structure 100 is shown in FIG. Figure 6B-1 , a dielectric layer 144 is formed over the passivation layer 140, a bonding pad 146 is formed in the dielectric layer 144, and a bonding pad via 142 is formed to connect the bonding pad 146 to the top metal layer in the interconnect layer 120. The materials for the dielectric layer 144, the bonding pad 146, and the bonding pad via 142 have been discussed above. Figure 6B-2 In this embodiment, at least one bonding pad via 142 is disposed on the seed layer 134 and is electrically connected to the seed layer 134 and the conductive pad 132. Figure 6B-3 In this embodiment, the seed layer 134 is omitted in the structure 100, and at least one bonding pad via 142 is placed on the top metal layer in the interconnect layer 120. Figure 6B-4 In this embodiment, the seed layer 134 is omitted in the structure 100, and at least one bonding pad via 142 is placed on the conductive pad 132. Figure 6B-1 , Figure 6B-2 , Figure 6B-3 and Figure 6B-4 Any of the embodiments shown in can further include an etch stop layer 148 between the passivation layer 140 and the dielectric layer 144. Figure 6B-1 , Figure 6B-2 , Figure 6B-3 and Figure 6B-4 Any of the components shown may be combined to form additional embodiments of the structure 100. For example, in some embodiments, the structure 100 includes some bonding pad vias 142 disposed on the top metal layer of the interconnect layer 120, and some bonding pad vias 142 disposed on the seed layer 134. For example, in some embodiments, the structure 100 includes some bonding pad vias 142 disposed on the top metal layer of the interconnect layer 120, and some bonding pad vias disposed on the conductive pads 132.

[0047] At operation 32, method 10 ( Figure 5 ) proceeds to bonding structure 100 (or a known good die or KGD) to other structures (or other KGDs) to form an integrated system on chip (SoIC). Figure 6CAs shown in FIG. 1 , a KGD 100A is bonded to another KGD 100B, for example, using hybrid bonding, where the bonding pads 146 on the two KGDs are bonded together, and the corresponding dielectric layers 144 are bonded together. A hybrid bonding process refers to the bonding of two surfaces, each of which contains at least two substantially different materials (hybrid surfaces). Figure 6C In the example shown in FIG. 1 , each of KGDs 100A and 100B may be Figure 6A-1 to Figure 6B-4 One of the forms shown, or other variations made by embodiments of method 10.

[0048] At operation 34, method 10 ( Figure 5 ) for further manufacturing steps. For example, method 10 may form a packaged assembly that seals or includes the KGDs bonded in operation 32, such as KGD 100A and KGD 100B. For example, method 10 may form bonding pads 202, bumps or solder balls 204, and passivation layer 206 to produce SoIC 200, such as in Figure 6C as shown in .

[0049] refer to Figure 7 , method 10 starts from operation 28 ( Figure 1 and Fig.2I ) or operation 27( Figure 3 and Figure 4J ) proceeds to operation 40. At operation 40, the method 10 forms micro bumps disposed on the seed layer 134 or the conductive pad 132. Figure 8A-1 and Figure 8A-2 It shows that Fig.2I An example of a structure 100 in which operation 40 is performed on the structure 100 is shown in FIG. Figure 8A-1 , forming a microbump 160 in direct contact with the seed layer 134, and forming a solder ball 162 on the microbump 160. The microbump 160 may include copper or other suitable metals or metal compounds. The solder ball 162 may include PbSn or a lead-free solder material such as tin, copper, silver, zinc and / or other metals. In the present embodiment, the seed layer 134 or the conductive pad 132 is much larger than the microbump 160 and the solder ball 162 (i.e., has a much larger footprint). In some examples, the footprint of the conductive pad 132 may be at least 5 times larger than the footprint of the microbump 160. Therefore, in the case of a sacrificial test pad 136 (which has a conductive pad 132 (such as in Figure 2G and Figure 4HIt is much easier to probe on the sacrificial test pad 136 (approximately the same footprint as shown in FIG) than on the microbump 160 or the solder ball 162. Therefore, most of the testing can be performed by probing on the sacrificial test pad 136 instead of probing on the microbump 160 or the solder ball 162 to increase the test throughput. After the test is completed and the sacrificial test pad 136 is removed, the microbump 160 and the solder ball 162 are formed. In an embodiment, the microbump 160 and the solder ball 162 can be placed on the seed layer 134 (in Figure 8A-1 ), or in an alternative embodiment, microbumps 160 and solder balls 162 may be placed on conductive pads 132 (as shown in Figure 8A-2 In some embodiments, some of the micro bumps 160 and the solder balls 162 are disposed on the seed layer 134 , and some of the micro bumps 160 and the solder balls 162 are disposed on the conductive pads 132 . Figure 8B-1 and 8B-2 It shows that Figure 4J The structure 100 shown in FIG. 1 is an example of a structure 100 that performs operation 40. Figure 8B-1 In an embodiment, microbumps 160 and solder balls 162 are disposed on seed layer 134. Figure 8B-2 In another embodiment where the seed layer 134 is omitted, the micro bumps 160 and the solder balls 162 are placed on the conductive pads 132 .

[0050] Although not intended to be limiting, one or more embodiments of the present disclosure provide many benefits to semiconductor devices and processes for forming the same. For example, embodiments of the present disclosure can be used to test IC dies with reduced test time, increased yield, and reduced cost. For another example, embodiments of the present disclosure allow probe testing on IC dies without leaving traces on test pads, which simplifies downstream processes. In addition, the disclosed methods and structures are compatible with SoC processes and SoIC processes.

[0051] In one exemplary aspect, the present disclosure is directed to a device including a semiconductor die. The semiconductor die includes a device layer, an interconnect layer above the device layer, a conductive pad above the interconnect layer, a conductive seed layer directly on the conductive pad, and a passivation layer encapsulating the conductive pad and the conductive seed layer.

[0052] In one embodiment of the device, the conductive pad comprises aluminum and the conductive seed layer comprises titanium copper. In another embodiment, the conductive pad comprises one of aluminum, aluminum copper, copper and titanium; and the conductive seed layer comprises one of titanium copper, titanium nitride and nickel.

[0053] In some embodiments where the passivation layer is a first passivation layer, the device further comprises a second passivation layer above the interconnect layer, wherein the conductive pad penetrates the second passivation layer and is electrically connected to the interconnect layer, wherein the first passivation layer is disposed above the second passivation layer, the conductive pad and the conductive seed layer.

[0054] In some embodiments, the device further comprises a conductive component, which passes through the passivation layer and is directly disposed on the conductive seed layer. In another embodiment, the device further comprises a conductive component, which passes through the passivation layer and is directly disposed on the region of the conductive pad.

[0055] In some embodiments, a top surface of the conductive seed layer is substantially planar.In some embodiments, the device further includes another semiconductor die bonded to the semiconductor die.

[0056] In another example aspect, the present disclosure is directed to a method comprising providing an integrated circuit (IC) die, wherein the IC die comprises an interconnect layer, a first passivation layer over the interconnect layer, and a conductive pad over the first passivation layer and electrically connected to the interconnect layer. The method also comprises forming a seed layer over the conductive pad; and forming a sacrificial test pad over the seed layer; performing a test on the IC die, wherein performing the test comprises contacting a flat probe tip with the sacrificial test pad; and after performing the test, removing the sacrificial test pad.

[0057] In an embodiment, the method further comprises forming a patterned mask over the conductive pad before forming the seed layer, wherein the patterned mask provides an opening directly over the conductive pad, and wherein the seed layer and the sacrificial test pad are formed within the opening. For further this embodiment, the method further comprises removing the patterned mask after forming the sacrificial test pad and before performing the test.

[0058] In an embodiment of the method, the conductive pad comprises aluminum, the seed layer comprises titanium copper, and the sacrificial test pad comprises tin. In another embodiment, the conductive pad comprises one of aluminum copper, copper and titanium, and the sacrificial test pad comprises tin (Sn), lead tin alloy (Pb x Sn 1-x ) or a compound having tin (Sn), silver (Ag) and copper (Cu).

[0059] In an embodiment, the method further comprises forming a second passivation layer over the first passivation layer, the conductive pad, and the seed layer. In a further embodiment, the method comprises forming a conductive component passing through the second passivation layer and disposed on the seed layer. In another further embodiment, the method comprises forming a conductive component passing through the second passivation layer and disposed on an area of ​​the conductive pad on which the seed layer is not disposed. In another further embodiment, the method comprises forming a conductive component passing through the first and second passivation layers and disposed on the interconnect layer. In yet another further embodiment, the method comprises forming a metal bonding pad over the second passivation layer.

[0060] In yet another example aspect, the present disclosure is directed to a method. The method includes providing an integrated circuit (IC) die, wherein the IC die includes an interconnect layer, a first passivation layer above the interconnect layer, and a conductive pad above the first passivation layer and electrically connected to the interconnect layer. The method also includes forming a patterned mask above the conductive pad, wherein the patterned mask provides an opening above the conductive pad; forming a seed layer above the conductive pad in the opening; forming a sacrificial test pad above the seed layer in the opening; removing the patterned mask; performing a test on the IC die, wherein performing the test includes contacting the sacrificial test pad with a probe tip; after performing the test, removing the sacrificial test pad; and forming a second passivation layer above the first passivation layer, the conductive pad, and the seed layer.

[0061] In an embodiment of the method, the conductive pad comprises one of aluminum, aluminum copper, copper and titanium, and the seed layer comprises one of titanium copper, titanium nitride and nickel. In an embodiment, after forming the second passivation layer, the method further comprises bonding the IC die to another IC die.

[0062] The foregoing summarizes the components of several embodiments so that those of ordinary skill in the art can better understand the various aspects of the present disclosure. Those of ordinary skill in the art should understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to achieve the same purpose and / or achieve the same advantages as the embodiments introduced herein. Those of ordinary skill in the art should also recognize that such equivalent constructions do not depart from the spirit and scope of the present disclosure, and that they can make various changes, substitutions and modifications herein without departing from the spirit and scope of the present disclosure.

Claims

1. A semiconductor device, comprising: A semiconductor die comprising a device layer, an interconnect layer above the device layer, a conductive pad above the interconnect layer, a conductive seed layer directly on the conductive pad, and a passivation layer sealing the conductive pad and the conductive seed layer, the conductive seed layer being sealed between the conductive pad and the passivation layer, Wherein, the passivation layer directly contacts the side surface of the conductive pad.

2. The semiconductor device according to claim 1, wherein The conductive pad includes aluminum, and the conductive seed layer includes titanium copper.

3. The semiconductor device according to claim 1, wherein The conductive pad includes one of aluminum, aluminum copper, copper and titanium; and the conductive seed layer includes one of titanium copper, titanium nitride and nickel.

4. The semiconductor device according to claim 1, wherein: The passivation layer is a first passivation layer and further includes a second passivation layer above the interconnection layer, wherein the conductive pad penetrates the second passivation layer and is electrically connected to the interconnection layer, wherein the first passivation layer is disposed above the second passivation layer, the conductive pad, and the conductive seed layer. 5 . The semiconductor device of claim 1 , further comprising a conductive member passing through the passivation layer and disposed directly on the conductive seed layer. 6 . The semiconductor device according to claim 1 , further comprising a conductive member penetrating the passivation layer and disposed directly on a region of the conductive pad. 7 . The semiconductor device of claim 1 , wherein a top surface of the conductive seed layer is substantially flat. 8 . The semiconductor device of claim 1 , further comprising another semiconductor die bonded to the semiconductor die.

9. A method of forming a semiconductor device, comprising: Providing an integrated circuit die, wherein the integrated circuit die includes an interconnect layer, a first passivation layer over the interconnect layer, and a conductive pad over the first passivation layer and electrically connected to the interconnect layer; forming a seed layer above the conductive pad; forming a sacrificial test pad above the seed layer; performing a test on the integrated circuit die, wherein performing the test includes contacting a flat probe tip with the sacrificial test pad; as well as After performing the test, the sacrificial test pad is removed without removing the seed layer.

10. The method according to claim 9, further comprising: Before forming the seed layer, forming a patterned mask over the conductive pad, wherein the patterned mask provides an opening directly over the conductive pad; as well as After forming the sacrificial test pad and before performing the test, the patterned mask is removed.

11. The method of claim 9, wherein the conductive pad comprises aluminum, the seed layer comprises titanium copper, and the sacrificial test pad comprises tin.

12. The method of claim 9, wherein the conductive pad comprises one of aluminum copper, copper and titanium, and the sacrificial test pad comprises tin (Sn), lead tin alloy (Pb x Sn 1-x ) or a compound having tin (Sn), silver (Ag) and copper (Cu).

13. The method according to claim 9, further comprising: A second passivation layer is formed over the first passivation layer, the conductive pad, and the seed layer.

14. The method according to claim 13, further comprising: A conductive feature is formed through the second passivation layer and disposed on the seed layer.

15. The method according to claim 13, further comprising: A conductive member is formed that passes through the second passivation layer and is disposed on a region of the conductive pad on which the seed layer is not disposed.

16. The method according to claim 13, further comprising: A conductive feature is formed through the first and second passivation layers and disposed on the interconnect layer.

17. The method according to claim 13, further comprising: A metal bond pad is formed over the second passivation layer.

18. A method of forming a semiconductor device, comprising: Providing an integrated circuit die, wherein the integrated circuit die includes an interconnect layer, a first passivation layer over the interconnect layer, and a conductive pad over the first passivation layer and electrically connected to the interconnect layer; forming a patterned mask over the conductive pad, wherein the patterned mask provides an opening over the conductive pad; forming a seed layer over the conductive pad in the opening such that the seed layer is formed narrower than the conductive pad; forming a sacrificial test pad over the seed layer in the opening; removing the patterned mask; performing a test on the integrated circuit die, wherein performing the test includes contacting the sacrificial test pad with a probe tip; After performing the test, removing the sacrificial test pad; as well as A second passivation layer is formed over the first passivation layer, the conductive pad, and the seed layer.

19. The method of claim 18, wherein the conductive pad comprises one of aluminum, aluminum copper, copper, and titanium, and the seed layer comprises one of titanium copper, titanium nitride, and nickel.

20. The method according to claim 18, after forming the second passivation layer, further comprising: The integrated circuit die is bonded to another integrated circuit die.