Semiconductor structure and method for forming the same

By adding a sacrificial layer in the FinFET structure to expand the distance between the epitaxial layer and the gate, the problem of large parasitic capacitance in existing FinFETs is solved, and device performance is improved.

CN113764279BActive Publication Date: 2024-11-01SEMICON MFG INT (SHANGHAI) CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010492606.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-06-03
Publication Date
2024-11-01
Estimated Expiration
2040-06-03

AI Technical Summary

Technical Problem

There are large parasitic capacitances in the existing FinFET structure, which affects device performance and requires a more efficient and reliable technical solution to reduce the parasitic capacitance between the gate and epitaxial layer.

Method used

By forming a sacrificial layer on the side wall material layer, the distance between the epitaxial layer and the gate is increased, thereby reducing the parasitic capacitance between the epitaxial layer and the gate and improving device performance.

Benefits of technology

The parasitic capacitance between the epitaxial layer and the gate is effectively reduced, and the device performance is improved, especially when the semiconductor device size is reduced, reducing the problem of increasing parasitic capacitance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113764279B_ABST
    Figure CN113764279B_ABST
Patent Text Reader

Abstract

The present application provides a semiconductor structure and a method for forming the same, the semiconductor structure comprising: a semiconductor substrate, a fin formed on the semiconductor substrate, the fin comprising a first part and a second part, and the semiconductor substrate further comprising a dielectric layer covering the sidewall and top surface of the second part of the fin, a gate layer covering part of the dielectric layer, and a hard mask layer covering the top surface of the gate layer; a sidewall located on the sidewall of the gate layer; an epitaxial layer located in the fin on both sides of the gate layer and protruding from the fin, wherein there is a gap between the part of the epitaxial layer protruding from the fin and the gate layer. The semiconductor structure and the method for forming the same described in the present application can improve device performance by reducing the parasitic capacitance between the epitaxial layer and the gate by increasing the distance between the epitaxial layer and the gate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for forming the same. Background Art

[0002] As semiconductor technology advances, the demand for higher storage capacity, faster processing systems, higher performance and lower costs continues to increase. In order to meet these demands, the semiconductor industry continues to scale down the size of semiconductor devices, and the design of three-dimensional structures such as fin field-effect transistors (FinFETs) has become a hot topic in the semiconductor field.

[0003] However, the current FinFET still has the problem of large parasitic capacitance, and a more effective and reliable technical solution is needed. Summary of the invention

[0004] The present application provides a semiconductor structure and a method for forming the same, which can reduce the parasitic capacitance between a gate and an epitaxial layer.

[0005] One aspect of the present application provides a method for forming a semiconductor structure, comprising: providing a semiconductor substrate, on which a fin is formed, the fin comprising a first part and a second part, and the semiconductor substrate further comprising a dielectric layer covering the sidewall and top surface of the second part of the fin, a gate layer covering a portion of the dielectric layer, and a hard mask layer covering the top surface of the gate layer; forming a sidewall material layer on the sidewall of the gate layer, the top surface and sidewall of the hard mask layer, and the surface of the dielectric layer; forming a sacrificial layer on the surface of the sidewall material layer; etching the sacrificial layer, the sidewall material layer, the dielectric layer, and the fin, forming openings in the fins on both sides of the gate layer, removing the sacrificial layer and the sidewall material layer on the top surface of the hard mask layer; growing an epitaxial layer in the opening; and removing the sacrificial layer.

[0006] In some embodiments of the present application, the semiconductor substrate further includes an isolation structure covering a sidewall of the first portion of the fin, and a top surface of the isolation structure is coplanar with a top surface of the first portion of the fin.

[0007] In some embodiments of the present application, the bottom of the opening is lower than the top surface of the isolation structure.

[0008] In some embodiments of the present application, the material of the sacrificial layer includes silicon oxide, and the material of the spacer material layer includes silicon nitride, low-K value silicon nitride, or a mixed layer of silicon nitride and low-K value silicon nitride.

[0009] In some embodiments of the present application, the material of the sacrificial layer includes silicon nitride, and the material of the spacer material layer includes low-K value silicon nitride.

[0010] In some embodiments of the present application, the thickness of the sacrificial layer is 2 nanometers to 6 nanometers.

[0011] In some embodiments of the present application, a method of forming the opening includes dry etching.

[0012] In some embodiments of the present application, the method of removing the sacrificial layer includes wet etching.

[0013] In some embodiments of the present application, the etching solution of the wet etching includes phosphoric acid or hydrofluoric acid.

[0014] In some embodiments of the present application, a top surface of the epitaxial layer is higher than a top surface of the fin and lower than a top surface of the dielectric layer.

[0015] Another aspect of the present application also provides a semiconductor structure, including: a semiconductor substrate, on which a fin is formed, the fin including a first part and a second part, and the semiconductor substrate also including a dielectric layer covering the side wall and top surface of the second part of the fin, a gate layer covering a portion of the dielectric layer, and a hard mask layer covering the top surface of the gate layer; sidewalls located on the side walls of the gate layer; an epitaxial layer located in the fins on both sides of the gate layer and protruding from the fins, wherein there is a gap between the portion of the epitaxial layer protruding from the fin and the gate layer.

[0016] In some embodiments of the present application, the semiconductor substrate further includes an isolation structure covering a sidewall of the first portion of the fin, and a top surface of the isolation structure is coplanar with a top surface of the first portion of the fin.

[0017] In some embodiments of the present application, the bottom of the epitaxial layer is lower than the top surface of the isolation structure.

[0018] In some embodiments of the present application, a width of a gap between a portion of the epitaxial layer protruding from the fin and the gate layer is 2 nanometers to 6 nanometers.

[0019] In some embodiments of the present application, a top surface of the epitaxial layer is higher than a top surface of the fin and lower than a top surface of the dielectric layer.

[0020] The semiconductor structure and the method for forming the same described in the present application can reduce the parasitic capacitance between the epitaxial layer and the gate by increasing the distance between the epitaxial layer and the gate, thereby improving device performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] The following drawings describe in detail the exemplary embodiments disclosed in this application. The same reference numerals represent similar structures in several views of the drawings. Those skilled in the art will understand that these embodiments are non-limiting, exemplary embodiments, and the drawings are only used for the purpose of illustration and description, and are not intended to limit the scope of this application. Other embodiments may also accomplish the inventive intent in this application. It should be understood that the drawings are not drawn to scale. Among them:

[0022] Figures 1 to 4 It is a structural schematic diagram of each step in a method for forming a semiconductor structure;

[0023] Figure 5 is a longitudinal cross-sectional view of a semiconductor structure;

[0024] Figures 6 to 11 It is a structural schematic diagram of each step in the method for forming a semiconductor structure described in an embodiment of the present application;

[0025] Fig.12 It is a longitudinal cross-sectional view of the semiconductor structure described in an embodiment of the present application. DETAILED DESCRIPTION

[0026] The following description provides specific application scenarios and requirements of the present application, with the purpose of enabling those skilled in the art to make and use the content in the present application. It will be apparent to those skilled in the art that various local modifications to the disclosed embodiments are apparent, and the general principles defined herein may be applied to other embodiments and applications without departing from the spirit and scope of the present application. Therefore, the present application is not limited to the embodiments shown, but to the widest scope consistent with the claims.

[0027] The technical solution of the present invention is described in detail below in conjunction with the embodiments and drawings.

[0028] Figures 1 to 4 It is a structural schematic diagram of each step in a method for forming a semiconductor structure.

[0029] refer to Figure 1 As shown, a semiconductor substrate 100 is provided, on which a fin 110 is formed, the fin 110 includes a first portion 111 and a second portion 112, and the semiconductor substrate 100 also includes a dielectric layer 120 covering the sidewall and top surface of the second portion 112 of the fin 110, a gate layer 130 covering a portion of the dielectric layer 120, and a hard mask layer 140 covering the top surface of the gate layer 130.

[0030] Continue to refer Figure 1The semiconductor substrate 100 further includes an isolation structure 150 covering the sidewalls of the first portion 111 of the fin 110 , and a top surface of the isolation structure 150 is coplanar with a top surface of the first portion 111 of the fin 110 .

[0031] refer to Figure 2 As shown, a spacer material layer 160 a is formed on the sidewalls of the gate layer 130 , the top surface and sidewalls of the hard mask layer 140 , and the surface of the dielectric layer 120 .

[0032] refer to Figure 3 As shown, the sidewall material layer 160a, the dielectric layer 120 and the fin 110 are etched to form openings 170 in the fins 110 on both sides of the gate layer 130, and the sidewall material layer 160a on the sidewall 140 of the hard mask layer and the isolation structure 150 is removed to form the sidewall 160.

[0033] refer to Figure 4 An epitaxial layer 180 is grown in the opening 170. The epitaxial layer 180 is used as a source or a drain in the semiconductor structure.

[0034] Figure 5 A longitudinal cross-sectional view of a semiconductor structure.

[0035] refer to Figure 5 , Figure 5 For along Figure 4 The longitudinal cross-section of the dotted line portion. The width of the portion of the epitaxial layer 180 located in the fin 110 is greater than the width of the portion of the epitaxial layer 180 above the fin 110. The distance between the portion of the epitaxial layer 180 above the fin 110 and the gate layer 130 is the thickness of the sidewall 160. The gate layer 130 will be replaced with a metal gate in the subsequent process, and the distance between the portion of the epitaxial layer 180 above the fin 110 and the gate layer 130 is equal to the distance between the portion of the epitaxial layer 180 above the fin 110 and the metal gate.

[0036] As the size of semiconductor devices decreases, the thickness of the sidewall 160 will also decrease, and the distance between the portion of the epitaxial layer 180 that is higher than the fin 110 and the metal gate will also decrease. When the epitaxial layer 180 and the metal gate are connected to a power source, the parasitic capacitance generated between the metal gate and the epitaxial layer 180 will increase, affecting device performance.

[0037] In view of the above problems, an embodiment of the present application provides a semiconductor structure and a method for forming the same. A sacrificial layer is formed on the sidewall material layer, and the distance between the epitaxial layer and the gate layer is the thickness of the sacrificial layer plus the thickness of the sidewall material layer. The distance between the epitaxial layer and the gate layer is increased, and the parasitic capacitance between the epitaxial layer and the gate is reduced, which can improve the device performance.

[0038] Figures 6 to 11 It is a structural schematic diagram of each step in the method for forming a semiconductor structure described in an embodiment of the present application.

[0039] refer to Figure 6 As shown, a semiconductor substrate 200 is provided, on which a fin 210 is formed, wherein the fin 210 includes a first portion 211 and a second portion 212, and the semiconductor substrate 200 also includes a dielectric layer 220 covering the sidewall and top surface of the second portion 212 of the fin 210, a gate layer 230 covering a portion of the dielectric layer 220, and a hard mask layer 240 covering the top surface of the gate layer 230.

[0040] In some embodiments of the present application, the material of the semiconductor substrate 200 includes (i) an elemental semiconductor, such as silicon or germanium, etc.; (ii) a compound semiconductor, such as silicon carbide, gallium arsenide, gallium phosphide, or indium phosphide, etc.; (iii) an alloy semiconductor, such as silicon germanium carbide, silicon germanium, gallium arsenide phosphide, or gallium indium phosphide, etc.; or (iv) a combination of the above. In addition, the semiconductor substrate 200 may be doped (e.g., a P-type substrate or an N-type substrate). In some embodiments of the present application, the semiconductor substrate 200 may be doped with a P-type dopant (e.g., boron, indium, aluminum, or gallium) or an N-type dopant (e.g., phosphorus or arsenic).

[0041] In some embodiments of the present application, the material of the dielectric layer 220 includes silicon oxide. In some embodiments of the present application, the method of forming the dielectric layer 220 includes a thermal oxidation process.

[0042] The material of the gate layer 230 includes polysilicon. The method of forming the gate layer 230 includes: forming a gate material layer on the isolation structure 250 and the dielectric layer 220; forming a patterned hard mask layer 240 on the gate material layer; and etching the gate material layer using the patterned hard mask layer 240 as a mask to form the gate layer 230. For example, etching can be performed using a dry etching process, a wet etching process, or a combination thereof.

[0043] In some embodiments of the present application, the material of the hard mask layer 240 includes silicon nitride. The hard mask layer 240 can protect the gate layer 230 from being affected when the fin is subsequently etched back.

[0044] Continue to refer Figure 6 The semiconductor substrate 200 further includes an isolation structure 250 covering the sidewalls of the first portion 211 of the fin 210 , and a top surface of the isolation structure 250 is coplanar with a top surface of the first portion 211 of the fin 210 .

[0045] The isolation structure 250 is used to isolate adjacent active areas. The isolation structure 250 may be made of a dielectric material. In some embodiments of the present application, the material of the isolation structure 250 may include silicon oxide, silicon nitride, silicon oxynitride and / or other suitable insulating materials. In some embodiments of the present application, the isolation structure 250 may include a multilayer structure.

[0046] refer to Figure 7 As shown, a spacer material layer 260 a is formed on the sidewalls of the gate layer 230 , the top surface and sidewalls of the hard mask layer 240 , and the surface of the dielectric layer 220 .

[0047] In some embodiments of the present application, the method of forming the spacer material layer 260a on the sidewall of the gate layer 230, the top surface of the hard mask layer 240, and the surface of the dielectric layer 220 includes a chemical vapor deposition process or a physical vapor deposition process.

[0048] In a conventional semiconductor structure formation method, after forming the sidewall material layer, the sidewall material layer, the dielectric layer and the fin are etched to form an opening in the fin, and then an epitaxial layer is formed in the opening by epitaxial growth. The distance between the portion of the epitaxial layer that is higher than the top surface of the fin and the gate layer is the thickness of the sidewall material layer. As the size of the semiconductor structure decreases, the thickness of the sidewall material layer also decreases, and the distance between the epitaxial layer and the gate layer decreases, resulting in an increase in the parasitic capacitance between the epitaxial layer and the gate. In the semiconductor structure formation method provided in the embodiment of the present application, a sacrificial layer is formed on the sidewall material layer 260a, and the distance between the epitaxial layer and the gate layer is the thickness of the sacrificial layer plus the thickness of the sidewall material layer. The distance between the epitaxial layer and the gate layer increases, and then the parasitic capacitance between the epitaxial layer and the gate decreases, which can improve device performance.

[0049] refer to Figure 8 As shown, a sacrificial layer 261 is formed on the surface of the spacer material layer 260a.

[0050] In some embodiments of the present application, the method of forming the sacrificial layer 261 on the surface of the spacer material layer 260 a includes a chemical vapor deposition process or a physical vapor deposition process.

[0051] The sacrificial layer 261 needs to be removed later, while the sidewall material layer of the gate layer 230 needs to be retained. Therefore, when etching to remove the sacrificial layer 261, it is necessary to ensure that the etching selectivity ratio of the material of the sacrificial layer 261 and the sidewall material can achieve the etching. In some embodiments of the present application, the material of the sacrificial layer 261 includes silicon oxide, and the material of the sidewall material layer 260a includes silicon nitride, low-K value silicon nitride, or a mixed layer of silicon nitride and low-K value silicon nitride. In other embodiments of the present application, the material of the sacrificial layer 261 includes silicon nitride, and the material of the sidewall material layer 260a includes low-K value silicon nitride.

[0052] In some embodiments of the present application, the thickness of the sacrificial layer 261 is 2 nanometers to 6 nanometers, for example, 3 nanometers, 4 nanometers or 5 nanometers. The function of the sacrificial layer 261 is to increase the distance between the epitaxial layer and the gate. The thickness of the sacrificial layer 261 represents the distance that can be increased, so the thickness of the sacrificial layer 261 can affect the device performance of the semiconductor structure. In actual processes, the thickness of the sacrificial layer 261 can be determined according to actual needs.

[0053] refer to Fig. 9 As shown, the sacrificial layer 261, the sidewall material layer 260a, the dielectric layer 220 and the fin 210 are etched to form openings 270 in the fins 210 on both sides of the gate layer 230, and the sacrificial layer 261 and the sidewall material layer 260a on the top surface of the hard mask layer 240 and the isolation structure 250 are removed to form the sidewall 260 located on the sidewall of the gate layer 230.

[0054] In some embodiments of the present application, the bottom of the opening 270 is lower than the top surface of the isolation structure 250. The bottom of the epitaxial layer formed subsequently is lower than the top surface of the isolation structure 250, which can effectively improve device performance.

[0055] In some embodiments of the present application, the method for forming the opening 270 includes dry etching. The sacrificial layer 261, the sidewall material layer 260a, the dielectric layer 220 and the fin 210 are made of different materials. If wet etching is used, it will be affected by the different etching selectivities of different materials and cannot be etched. However, plasma dry etching can simultaneously etch the sacrificial layer 261, the sidewall material layer 260a, the dielectric layer 220 and the fin 210.

[0056] In some embodiments of the present application, the method of forming the opening 270 includes isotropic dry etching, and the width of the portion of the opening 270 located in the fin 210 is greater than the width of the portion of the opening 270 above the fin 210 .

[0057] refer to Fig.10 As shown, an epitaxial layer 280 is grown in the opening 270 .

[0058] In some embodiments of the present application, the top surface of the epitaxial layer 270 is higher than the top surface of the fin 210 and lower than the top surface of the dielectric layer 220 .

[0059] The epitaxial layer 280 may include an epitaxially grown semiconductor material. In some embodiments of the present application, the epitaxially grown semiconductor material is the same material as the material of the semiconductor substrate 200. In other embodiments of the present application, the epitaxially grown semiconductor material may include a material different from the material of the semiconductor substrate 200. The epitaxially grown semiconductor material may include: (i) a semiconductor material, such as germanium or silicon; (ii) a compound semiconductor material, such as silicon phosphide or silicon carbon phosphide; or (iii) a semiconductor alloy, such as silicon germanium or gallium arsenic phosphide.

[0060] In some embodiments of the present application, for example, the epitaxial layer 280 can be grown by (i) chemical vapor deposition (CVD), such as low-pressure CVD (LPCVD), atomic layer CVD (ALCVD), ultra-high vacuum CVD (UHVCVD), reduced pressure CVD (RPCVD) or any suitable CVD; (ii) molecular beam epitaxy (MBE) process; (iii) any suitable epitaxial process; or (iv) a combination of the above.

[0061] In some embodiments of the present application, the epitaxial layer 280 may be P-type or N-type. In some embodiments of the present application, for example, the P-type epitaxial layer 280 may include SiGe and may be in-situ doped using a P-type dopant (e.g., boron, indium, or gallium) during the epitaxial growth process. For P-type in-situ doping, a P-type doping precursor may be used, including but not limited to diborane (B2H6), boron trifluoride (BF3), and / or other P-type doping precursors. In some embodiments of the present application, for example, the N-type epitaxial layer 280 may include Si and may be in-situ doped using an N-type dopant (e.g., phosphorus or arsenic) during the epitaxial growth process. For N-type in-situ doping, an N-type doping precursor may be used, including but not limited to phosphine (PH3), arsine (AsH3), and / or other N-type doping precursors.

[0062] refer to Fig.11 As shown, the sacrificial layer 261 is removed.

[0063] In some embodiments of the present application, the method of removing the sacrificial layer 261 includes wet etching.

[0064] In some embodiments of the present application, the etching solution of the wet etching includes phosphoric acid or hydrofluoric acid.

[0065] Fig.12 It is a longitudinal cross-sectional view of the semiconductor structure described in an embodiment of the present application.

[0066] refer to Fig.12 , Fig.12 For along Fig.11 The longitudinal cross-section of the dotted line portion. The width of the portion of the epitaxial layer 280 located in the fin 210 is greater than the width of the portion of the epitaxial layer 280 above the fin 210. The distance between the portion of the epitaxial layer 280 above the fin 210 and the gate layer 230 is the thickness of the sidewall 260 plus the thickness of the sacrificial layer 261 that has been removed. The gate layer 230 will be replaced with a metal gate in subsequent processes, and the distance between the portion of the epitaxial layer 280 above the fin 210 and the gate layer 230 is equal to the distance between the portion of the epitaxial layer 280 above the fin 210 and the metal gate.

[0067] and Figure 5 Compared with the semiconductor structure shown, in the semiconductor structure formed by the semiconductor formation method described in the embodiment of the present application, the distance between the portion of the epitaxial layer 280 that is higher than the fin 210 and the metal gate is larger. When the epitaxial layer 280 and the metal gate are connected to a power supply, the parasitic capacitance generated between the metal gate and the epitaxial layer 280 is smaller, which can improve the device performance.

[0068] The method for forming a semiconductor structure described in the present application increases the distance between the epitaxial layer and the gate through the sacrificial layer, thereby reducing the parasitic capacitance between the epitaxial layer and the gate, thereby improving device performance.

[0069] The embodiment of the present application also provides a semiconductor structure, referring to Fig.11 and Fig.12 The semiconductor structure includes: a semiconductor substrate 200, on which a fin 210 is formed, the fin 210 includes a first portion 211 and a second portion 212, and the semiconductor substrate 200 also includes a dielectric layer 220 covering the sidewall and top surface of the second portion 212 of the fin 210, a gate layer 230 covering a portion of the dielectric layer 220, and a hard mask layer 240 covering the top surface of the gate layer 230; a sidewall 260 located on the sidewall of the gate layer 230; an epitaxial layer 280 located in the fin 210 on both sides of the gate layer 230 and protruding from the fin 210, wherein a gap exists between the portion of the epitaxial layer 280 protruding from the fin 210 and the gate layer 230.

[0070] In some embodiments of the present application, the material of the semiconductor substrate 200 includes (i) an elemental semiconductor, such as silicon or germanium, etc.; (ii) a compound semiconductor, such as silicon carbide, gallium arsenide, gallium phosphide, or indium phosphide, etc.; (iii) an alloy semiconductor, such as silicon germanium carbide, silicon germanium, gallium arsenide phosphide, or gallium indium phosphide, etc.; or (iv) a combination of the above. In addition, the semiconductor substrate 200 may be doped (e.g., a P-type substrate or an N-type substrate). In some embodiments of the present application, the semiconductor substrate 200 may be doped with a P-type dopant (e.g., boron, indium, aluminum, or gallium) or an N-type dopant (e.g., phosphorus or arsenic).

[0071] In some embodiments of the present application, the material of the dielectric layer 220 includes silicon oxide.

[0072] In some embodiments of the present application, the material of the gate layer 230 includes polysilicon.

[0073] In some embodiments of the present application, the material of the hard mask layer 240 includes silicon nitride. The hard mask layer 240 can protect the gate layer 230 .

[0074] The semiconductor substrate 200 further includes an isolation structure 250 covering the sidewalls of the first portion 211 of the fin 210 . The top surface of the isolation structure 250 is coplanar with the top surface of the first portion 211 of the fin 210 .

[0075] The isolation structure 250 is used to isolate adjacent active areas. The isolation structure 250 may be made of a dielectric material. In some embodiments of the present application, the material of the isolation structure 250 may include silicon oxide, silicon nitride, silicon oxynitride and / or other suitable insulating materials. In some embodiments of the present application, the isolation structure 250 may include a multilayer structure.

[0076] In some embodiments of the present application, the bottom of the epitaxial layer 280 is lower than the top surface of the isolation structure 250 , which can effectively improve device performance.

[0077] In some embodiments of the present application, the top surface of the epitaxial layer 280 is higher than the top surface of the fin 210 and lower than the top surface of the dielectric layer 220 .

[0078] In some embodiments of the present application, the width of the gap between the portion of the epitaxial layer 280 protruding from the fin and the gate layer is 2 nanometers to 6 nanometers, for example, 3 nanometers, 4 nanometers or 5 nanometers. The spacing between the portion of the epitaxial layer 280 protruding from the fin and the gate layer is the width of the gap plus the thickness of the sidewall, so the width of the gap can affect the device performance of the semiconductor structure. In actual processes, the width of the gap can be determined according to actual needs.

[0079] The epitaxial layer 280 may include an epitaxially grown semiconductor material. In some embodiments of the present application, the epitaxially grown semiconductor material is the same material as the material of the semiconductor substrate 200. In other embodiments of the present application, the epitaxially grown semiconductor material may include a material different from the material of the semiconductor substrate 200. The epitaxially grown semiconductor material may include: (i) a semiconductor material, such as germanium or silicon; (ii) a compound semiconductor material, such as silicon phosphide or silicon carbon phosphide; or (iii) a semiconductor alloy, such as silicon germanium or gallium arsenic phosphide.

[0080] In some embodiments of the present application, the epitaxial layer 280 may be P-type or N-type. In some embodiments of the present application, for example, the P-type epitaxial layer 280 may include SiGe and may be in-situ doped using a P-type dopant (e.g., boron, indium, or gallium) during the epitaxial growth process. For P-type in-situ doping, a P-type doping precursor may be used, including but not limited to diborane (B2H6), boron trifluoride (BF3), and / or other P-type doping precursors. In some embodiments of the present application, for example, the N-type epitaxial layer 280 may include Si and may be in-situ doped using an N-type dopant (e.g., phosphorus or arsenic) during the epitaxial growth process. For N-type in-situ doping, an N-type doping precursor may be used, including but not limited to phosphine (PH3), arsine (AsH3), and / or other N-type doping precursors.

[0081] refer to Fig.12 , Fig.12 For along Fig.11 The longitudinal cross-section of the dotted line portion. The width of the portion of the epitaxial layer 280 located in the fin 210 is greater than the width of the portion of the epitaxial layer 280 above the fin 210. The distance between the portion of the epitaxial layer 280 above the fin 210 and the gate layer 230 is the thickness of the sidewall 260 plus the thickness of the sacrificial layer 261 that has been removed. The gate layer 230 will be replaced with a metal gate in subsequent processes, and the distance between the portion of the epitaxial layer 280 above the fin 210 and the gate layer 230 is equal to the distance between the portion of the epitaxial layer 280 above the fin 210 and the metal gate.

[0082] and Figure 5 Compared with the semiconductor structure shown, in the semiconductor structure formed by the semiconductor formation method described in the embodiment of the present application, the distance between the portion of the epitaxial layer 280 that is higher than the fin 210 and the metal gate is larger. When the epitaxial layer 280 and the metal gate are connected to a power supply, the parasitic capacitance generated between the metal gate and the epitaxial layer 280 is smaller, which can improve the device performance.

[0083] The semiconductor structure described in the present application can improve device performance by reducing the parasitic capacitance between the epitaxial layer and the gate by increasing the distance between the epitaxial layer and the gate.

[0084] In summary, after reading the contents of this application, those skilled in the art will appreciate that the aforementioned application contents may be presented only in an exemplary manner and may not be restrictive. Although not explicitly stated herein, those skilled in the art will appreciate that this application is intended to encompass various reasonable changes, improvements and modifications to the embodiments. These changes, improvements and modifications are within the spirit and scope of the exemplary embodiments of this application.

[0085] It should be understood that the term "and / or" used in this embodiment includes any or all combinations of one or more of the associated listed items. It should be understood that when an element is referred to as being "connected" or "coupled" to another element, it can be directly connected or coupled to the other element, or intermediate elements may also be present.

[0086] Similarly, it will be understood that when an element such as a layer, region or substrate is referred to as being "on" another element, it can be directly on the other element or intervening elements may also be present. In contrast, the term "directly" means there are no intervening elements.

[0087] It should also be understood that the terms “comprising,” “containing,” “including,” or “comprising,” when used in this application document, indicate the presence of the recited features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups thereof.

[0088] It should also be understood that although the terms first, second, third, etc. can be used to describe various elements, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. Therefore, without departing from the teachings of the present application, the first element in some embodiments can be referred to as the second element in other embodiments. The same reference numerals or the same reference signs represent the same elements throughout the specification.

[0089] As used herein, the term "low K" refers to a small dielectric constant. In the field of semiconductor device structure and manufacturing process, low K refers to a dielectric constant that is smaller than the dielectric constant of SiO2 (eg, smaller than 3.9).

[0090] In addition, the present specification describes exemplary embodiments by reference to idealized exemplary cross-sectional views and / or plan views and / or stereograms. Therefore, differences from the illustrated shapes due to, for example, manufacturing techniques and / or tolerances are foreseeable. Therefore, the exemplary embodiments should not be interpreted as being limited to the shapes of the regions shown herein, but should include deviations in shapes caused by, for example, manufacturing. For example, an etched region shown as a rectangle will typically have circular or curved features. Therefore, the region shown in the figure is schematic in nature, and its shape is not intended to illustrate the actual shape of the region of the device nor to limit the scope of the exemplary embodiments.

Claims

1. A method for forming a semiconductor structure, characterized in that: include: Providing a semiconductor substrate, on which a fin is formed, the fin comprising a first portion and a second portion, and the semiconductor substrate further comprising a dielectric layer covering the sidewall and top surface of the second portion of the fin, a gate layer covering a portion of the dielectric layer, and a hard mask layer covering the top surface of the gate layer; Forming a spacer material layer on the sidewall of the gate layer, the top surface and sidewall of the hard mask layer, and the surface of the dielectric layer; forming a sacrificial layer on the surface of the sidewall material layer; Etching the sacrificial layer, the sidewall material layer, the dielectric layer and the fins to form openings in the fins on both sides of the gate layer, and removing the sacrificial layer and the sidewall material layer on the top surface of the hard mask layer; growing an epitaxial layer in the opening; The sacrificial layer is removed to form a gap between a portion of the epitaxial layer protruding from the fin and the gate layer.

2. The method for forming a semiconductor structure according to claim 1, wherein: The semiconductor substrate further includes an isolation structure covering the sidewall of the first portion of the fin, wherein a top surface of the isolation structure is coplanar with a top surface of the first portion of the fin.

3. The method for forming a semiconductor structure according to claim 2, wherein: The bottom of the opening is lower than the top surface of the isolation structure.

4. The method for forming a semiconductor structure according to claim 1, wherein: The material of the sacrificial layer includes silicon oxide, and the material of the spacer material layer includes silicon nitride, low-K value silicon nitride, or a mixed layer of silicon nitride and low-K value silicon nitride.

5. The method for forming a semiconductor structure according to claim 1, wherein: The material of the sacrificial layer includes silicon nitride, and the material of the spacer material layer includes low-K value silicon nitride.

6. The method for forming a semiconductor structure according to claim 1, wherein: The thickness of the sacrificial layer is 2 nanometers to 6 nanometers.

7. The method for forming a semiconductor structure according to claim 1, wherein: The method of forming the opening includes dry etching.

8. The method for forming a semiconductor structure according to claim 1, wherein: The method of removing the sacrificial layer includes wet etching.

9. The method for forming a semiconductor structure according to claim 8, wherein: The wet etching solution includes phosphoric acid or hydrofluoric acid.

10. The method for forming a semiconductor structure according to claim 1, wherein: The top surface of the epitaxial layer is higher than the top surface of the fin and lower than the top surface of the dielectric layer.

11. A semiconductor structure formed by the method for forming a semiconductor structure according to any one of claims 1 to 10, characterized in that: include: A semiconductor substrate, on which a fin is formed, the fin comprising a first portion and a second portion, and the semiconductor substrate further comprising a dielectric layer covering a sidewall and a top surface of the second portion of the fin, a gate layer covering a portion of the dielectric layer, and a hard mask layer covering a top surface of the gate layer; A sidewall, located on a sidewall of the gate layer; The epitaxial layer is located in the fins on both sides of the gate layer and protrudes from the fins, wherein a gap exists between a portion of the epitaxial layer protruding from the fins and the gate layer.

12. The semiconductor structure according to claim 11, wherein: The semiconductor substrate further includes an isolation structure covering the sidewall of the first portion of the fin, wherein a top surface of the isolation structure is coplanar with a top surface of the first portion of the fin.

13. The semiconductor structure according to claim 12, wherein: The bottom of the epitaxial layer is lower than the top surface of the isolation structure.

14. The semiconductor structure according to claim 11, wherein: The width of the gap between the portion of the epitaxial layer protruding from the fin and the gate layer is 2 nanometers to 6 nanometers.

15. The semiconductor structure according to claim 11, wherein: The top surface of the epitaxial layer is higher than the top surface of the fin and lower than the top surface of the dielectric layer.