Semiconductor device and method for forming the same
By forming isolation regions and protruding fins on the semiconductor substrate, etching recesses and growing the epitaxial region, and adjusting the fin spacer height to form an asymmetric FinFET epitaxial region profile and a tilted silicide region, the problem of high contact resistance in FinFET is solved. problem, improving contact quality and cleanliness.
Patent Information
- Application Number
- CN202110743405.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-12-18
- Filing Date
- 2021-07-01
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-07-01
AI Technical Summary
In the formation of fin field effect transistors (FinFETs), it is difficult to achieve the merged epitaxial region of source/drain regions with asymmetrical profiles using existing technology, resulting in high contact resistance.
By forming an isolation region on a semiconductor substrate and growing protruding fins thereon, etching to form a recess and growing an epitaxial region so that the top surface of the combined epitaxial region is lower on the side facing a certain side than the side facing away from it, using fin spacers to adjust the epitaxial region The relationship between the height of the region and the asymmetric epitaxial region profile is formed, and a tilted silicide region is formed on it to reduce the contact resistance.
The asymmetric epitaxial region profile of the source/drain region is achieved, which reduces the contact resistance, increases the contact area, and increases the convenience of cleaning the bottom of the opening.
Smart Images

Figure CN113764352B_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention relate to semiconductor devices and methods of forming the same. Background Art
[0002] In the formation of a FinFET, source / drain regions are typically formed by forming a semiconductor fin, recessing the semiconductor fin to form a recess, and growing an epitaxial region from the recess. Epitaxial regions grown from the recesses of adjacent semiconductor fins can merge with each other, and the resulting epitaxial region can have a flat top surface. Source / drain contact plugs are formed to electrically connect to the source / drain regions. Summary of the Invention
[0003] According to one aspect of an embodiment of the present invention, a method for forming a semiconductor device is provided, comprising: forming an isolation region extending into a semiconductor substrate; forming a first plurality of protruding fins and a second protruding fin above the isolation region, wherein the first plurality of protruding fins include: an outer fin away from the second protruding fin and an inner fin closest to the second protruding fin; etching the first plurality of protruding fins to form a first recess; growing a first epitaxial region from the first recess, wherein the first epitaxial regions are merged to form a merged epitaxial region; etching the second protruding fin to form a second recess; and growing a second epitaxial region from the second recess, wherein a top surface of the merged epitaxial region is lower on a side facing the second epitaxial region than on a side facing away from the second epitaxial region.
[0004] According to another aspect of an embodiment of the present invention, a semiconductor device is provided, comprising: a semiconductor substrate; a first plurality of isolation regions and a second plurality of isolation regions extending into the semiconductor substrate; a first stripe group comprising a first plurality of semiconductor strips between the first plurality of isolation regions; a second stripe group comprising at least one second semiconductor strip between the second plurality of isolation regions; a first fin group comprising a first plurality of semiconductor fins overlapping with corresponding first plurality of semiconductor strips; a second fin group comprising at least one second semiconductor fin overlapping with at least one second semiconductor strip; a plurality of epitaxial regions, each epitaxial region comprising a portion filling a first recess extending into one of the first plurality of semiconductor fins, wherein the plurality of epitaxial regions are merged to form a merged epitaxial region; and a second epitaxial region comprising a second portion filling a second recess extending into the at least one second semiconductor fin, wherein a top surface of the merged epitaxial region is inclined toward the second epitaxial region, and a first portion near the top surface of the second epitaxial region is lower than a second portion away from the second epitaxial region.
[0005] According to another aspect of an embodiment of the present invention, a semiconductor device is provided, comprising: a plurality of semiconductor fins; a plurality of gate stacks located on the top surfaces and sidewalls of the plurality of semiconductor fins; a plurality of epitaxial regions, each epitaxial region being between two of the plurality of semiconductor fins and joining the sidewalls, wherein the plurality of epitaxial regions are merged into a merged epitaxial region, and the outermost epitaxial region of the plurality of epitaxial regions is the shortest of the plurality of epitaxial regions; a silicide region in contact with the top surface of the merged epitaxial region; and a contact plug located above the silicide region and in contact with the silicide region. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] Various aspects of the present invention are best understood from the following detailed description when read in conjunction with the accompanying drawings. It should be emphasized that, in accordance with standard practice in the industry, various components are not drawn to scale and are used for illustrative purposes only. In fact, the dimensions of various components may be arbitrarily increased or decreased for clarity of discussion.
[0007] Figure 1 、 Figure 2 、 Figure 3A 、 Figure 3B 、 Figure 3C 、 Figure 4A 、 Figure 4B 、 Figure 5-Figure 8 、 Figure 9A 、 Figure 9B 、 Figure 10 、 Figure 11A and Figure 11B Illustrated are perspective and cross-sectional views of intermediate stages in forming a fin field effect transistor (FinFET), according to some embodiments.
[0008] Figure 12 A perspective view of a recess in a semiconductor fin is shown, in accordance with some embodiments.
[0009] Figure 13 A perspective view of a structure having shallow trench isolation (STI) regions and semiconductor fins is shown in accordance with some embodiments.
[0010] Figure 14 A process flow for forming n-type FinFETs and p-type FinFETs is shown in accordance with some embodiments. DETAILED DESCRIPTION
[0011] The following disclosure provides many different embodiments or examples for implementing the different features of the present invention. Specific embodiments or examples of components and arrangements are described below to simplify the present invention. Of course, these are merely examples and are not intended to be limiting. For example, in the following description, forming a first component above or on a second component may include an embodiment in which the first component and the second component are directly in contact with each other, and may also include an embodiment in which an additional component may be formed between the first component and the second component so that the first component and the second component may not be in direct contact. In addition, the present invention may repeat reference numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity and does not itself indicate the relationship between the various embodiments and / or configurations discussed.
[0012] Furthermore, for ease of description, spacing terms such as "below," "beneath," "lower," "above," "upper," etc., may be used herein to describe the relationship of one element or component to another element or component as illustrated in the figures. Spacing terms are intended to encompass different orientations of the device in use or during operation in addition to the orientations depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and spacing descriptors used herein should be interpreted accordingly.
[0013] A fin field effect transistor (FinFET) and a method for forming the same are provided. According to some embodiments of the present disclosure, a merged epitaxial region serving as the source / drain region of a FinFET has an asymmetric profile, wherein the epitaxial regions grown from different fins have different heights, and the top surface of the merged epitaxial region is inclined. Therefore, when source / drain silicide regions and source / drain contact plugs are formed to connect to the epitaxial region, both the top surface and the sidewalls of the epitaxial region are in contact with the source / drain silicide region, and thus the contact resistance is reduced. The embodiments discussed herein will provide examples to enable the subject matter of the present disclosure to be made or used, and one of ordinary skill in the art will readily understand the modifications that may be made while remaining within the intended scope of the different embodiments. Throughout the various views and illustrative embodiments, similar reference numerals are used to indicate similar elements. Although method embodiments may be discussed as being performed in a particular order, other method embodiments may be performed in any logical order.
[0014] Figure 1 、 Figure 2 、 Figure 3A 、 Figure 3B 、 Figure 3C 、 Figure 4A 、 Figure 4B 、 Figure 5-Figure 8 、 Figure 9A 、 Figure 9B 、 Figure 10 、 Figure 11A and Figure 11BFIG2 shows a cross-sectional view of an intermediate stage in the process of forming a FinFET and corresponding source / drain regions according to some embodiments of the present disclosure. The corresponding process is also schematically reflected in FIG2 . Figure 14 In the process shown.
[0015] Figure 1 A perspective view of the initial structure is shown. The initial structure includes a wafer 10, which further includes a substrate 20. The substrate 20 may be a semiconductor substrate, which may be a silicon substrate, a silicon germanium substrate, or a substrate formed of other semiconductor materials. The top surface of the substrate 20 may have a (100) surface plane. The substrate 20 may be doped with p-type or n-type impurities. An isolation region 22 such as a shallow trench isolation (STI) region may be formed to extend from the top surface of the substrate 20 into the substrate 20. Figure 14 In the process flow shown in , the corresponding process is shown as process 202. The portion of substrate 20 between adjacent STI regions 22 is also referred to as semiconductor strips 24. According to some embodiments, the top surfaces of semiconductor strips 24N and 24P and the top surfaces of STI regions 22 may be substantially flush with each other.
[0016] STI regions 22 may include a pad oxide (not shown), which may be a thermal oxide formed by thermal oxidation of a surface layer of substrate 20. The pad oxide may also be a silicon oxide layer deposited using, for example, atomic layer deposition (ALD), high-density plasma chemical vapor deposition (HDPCVD), or chemical vapor deposition (CVD). STI regions 22 may also include a dielectric material over the pad oxide, wherein the dielectric material may be formed using flowable chemical vapor deposition (FCVD), spin coating, or the like.
[0017] The wafer 10 includes a first device region and a second device region adjacent to each other. Each device region is used to form a FinFET therein. The FinFET formed in each of the first device region and the second device region can be an n-type FinFET or a p-type FinFET. In an exemplary embodiment, the first device region is used to form an n-type FinFET, and the second device region is used to form a p-type FinFET. Therefore, the first device region and the second device are referred to as device regions 100N and 100P, respectively. In order to distinguish the components in the n-type device region 100N and the p-type device region 100P from each other, the components formed in the n-type device region 100N can be represented by a reference numeral followed by the letter "N", and the components formed in the p-type device region 100P can be represented by a reference numeral followed by the letter "P". For example, the semiconductor strip 24 in the n-type device region 100N is referred to as 24N, and the semiconductor strip 24 in the p-type device region 100P is referred to as 24P. According to some embodiments, semiconductor strip 24N is formed of (or includes) silicon (without germanium), while semiconductor strip 24P is replaced by silicon germanium. According to alternative embodiments, semiconductor strips 24N and 24P are both formed of or include silicon without germanium.
[0018] Reference Figure 2 , STI region 22 is recessed so that the tops of semiconductor strips 24N and 24P protrude higher than top surface 22A of STI region 22 to form protruding fins 24N′ and 24P′, respectively. Figure 14 In the illustrated process flow, the corresponding process is shown as process 204. The portions of semiconductor strips 24N and 24P in STI regions 22 are still referred to as semiconductor strips. Etching can be performed using a dry etching process, wherein a mixture of HF and NH3 can be used as the etching gas. Etching can also be performed using a mixture of NF3 and NH3 as the etching gas. During the etching process, plasma may be generated. Argon gas may also be included. According to an alternative embodiment of the present disclosure, recessing of STI regions 22 is performed using a wet etching process. The etching chemical may include, for example, an HF solution.
[0019] In accordance with some embodiments, the fins used to form the FinFETs may be formed / patterned by any suitable method. For example, the fins may be patterned using one or more photolithographic processes, including double patterning or multiple patterning processes. Typically, double patterning or multiple patterning processes combine photolithography and self-aligned processes, thereby allowing for the production of patterns having, for example, a pitch smaller than that obtainable using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed over a substrate and patterned using a photolithographic process. Spacers are formed next to the patterned sacrificial layer using a self-aligned process. The sacrificial layer is then removed, and the remaining spacers or mandrels may then be used to pattern the fins.
[0020] Reference Figure 3A 、 Figure 3B and Figure 3C , a dummy gate stack 30 is formed on the top surface and sidewalls of the protruding fins 24N' and 24P'. Figure 14 This is shown as process 206 in the illustrated process flow. Figure 3B The cross section shown is from Figure 3A The reference sections B1-B1 and B2-B2 are obtained. Figure 3B and subsequently Figure 11B , the top surface 22A of the STI region 22 can be shown (also refer to Figure 3A ) level, and the semiconductor fin 24' is higher than the top surface 22A. The bottom surface 22B of the STI region 22 (also refer to Figure 3A ) are also shown in the cross-sectional view. STI regions 22 are located at a level between 22A and 22B and are not shown in the cross-sectional view because they are in a different plane than shown. Figure 3B and Figure 11B Shown in.
[0021] from Figure 3A The reference cross section CC in Figure 3C The cross section shown, except Figure 3A A portion of the device region 100P is shown. According to some embodiments, the protruding fins 24N' may be positioned closely together to form a fin group. The protruding fins 24P' may also be positioned close to each other to form a fin group. The inner group spacing S1 ( Figure 3C ) is less than the inner group spacing S2 between adjacent fin groups. According to some embodiments, both fin groups are multi-fin fin groups, such as Figure 3C According to an alternative embodiment, one of the fin groups is a single fin group. For example, there may be no Figure 3C The rightmost fin in the image is shown, so there is a 2-fin fin group on the left and a single-fin fin group on the right. According to some embodiments, each fin group may also include more than two fins.
[0022] The dummy gate stack 30 may include a dummy gate dielectric 32 ( Figure 3B ) and a dummy gate electrode 34 over the dummy gate dielectric 32. The dummy gate electrode 34 can be formed using, for example, amorphous silicon or polycrystalline silicon, and other materials can also be used. Each dummy gate stack 30 can also include one (or more) hard mask layers 36 on the dummy gate electrode 34. The hard mask layer 36 can be formed of silicon nitride, silicon carbonitride, etc. The length direction of the dummy gate stack 30 is also perpendicular to the length direction of the protruding fin 24'.
[0023] Next, gate spacers 38 ( Figure 3A and Figure 3C ).exist Figure 14 In the process flow shown, the corresponding process is also shown as process 206. According to some embodiments of the present disclosure, the gate spacer 38 is formed of a dielectric material such as silicon oxynitride (SiCN), silicon nitride, silicon oxynitride (SiOCN), etc., and can have a single-layer structure or a multi-layer structure including multiple dielectric layers. The formation process includes depositing a conformal spacer layer and then performing an anisotropic etching process to form the gate spacer 38 (and the fin spacer 39). According to some embodiments of the present disclosure, the gate spacer 38 is a multi-layer gate spacer. For example, each gate spacer 38 may include a SiN layer and a SiOCN layer above the SiN layer. Figure 3A and Figure 3C Also shown are fin spacers 39 formed on the sidewalls of the protruding fins 24'. Figure 14 In the illustrated process flow, each process is also illustrated as process 206 .
[0024] According to some embodiments of the present disclosure, the fin spacers 39 (including 39A, 39B, and 39C) are formed by the same process used to form the gate spacers 38. For example, in the process used to form the gate spacers 38, a blanket dielectric layer is deposited to form the gate spacers 38, and when the dielectric layer is etched, some portions may remain on the sidewalls of the protruding fins 24'N and 24P', thereby forming the fin spacers 39.
[0025] Reference Figure 4A and Figure 4B , forming a first epitaxial mask 40N. Figure 4B Shown Figure 4A Reference section B2-B2 in Figure 14 As shown, the corresponding process is shown as process 208 in process flow 200. According to some embodiments, epitaxial mask 40N is formed of a dielectric material, which may be SiON, SiOCN, AlO, SiN, SiOC, SiO2, etc. The material of epitaxial mask 40N is also different from the material of fin spacer 39 and STI region 22. According to some embodiments of the present disclosure, epitaxial mask 40N is deposited using a conformal deposition process such as atomic layer deposition (ALD), chemical vapor deposition (CVD), etc. According to some embodiments, an etch mask 42N is formed, which may be formed of or include a photoresist. Other layers such as a bottom anti-reflective coating (BARC) may or may not be formed as part of etch mask 42N. Etch mask 42N is patterned to cover n-type FinFET region 100N and expose p-type FinFET region 100P. An etching process is then performed to remove portions of epitaxial mask 40N in p-type FinFET region 100P without removing portions of epitaxial mask 40N in n-type FinFET region 100N. The etching process is an isotropic process that can be a dry etching process or a wet etching process.
[0026] Next, the protruding fin 24P' is recessed by etching to form a recess 44P. Figure 14 The process flow 200 is shown as process 210. The etch mask 42N is also removed and can be removed before or after etching the protruding fin 24P'. According to some embodiments, the etching of the protruding fin 24P' is performed until the recess 44P extends below the top of the fin spacer 39 ( Figure 4A ) and is higher than the top surface of the STI region 22. Figure 4A In FIG. 1 , dotted lines are shown to represent the etched portion of the protruding fin 24P′. The dotted lines also show the top surface and sidewalls of the portion of the protruding fin 24P′ that is directly below the dummy gate stack 30 (see FIG. 1 ). Figure 3B ).
[0027] According to some embodiments of the present disclosure, the recessing of the protruding fin 24' is performed by a dry etching step. The dry etching can be performed using a process gas such as C2F6, CF4, SO2, HBr, a mixture of Cl2 and O2, a mixture of HBr, Cl2, O2 and CF2, etc. The etching can be anisotropic. According to some embodiments of the present disclosure, such as Figure 4B As shown, the sidewalls of the protruding fin 24' facing the recess 40 are substantially vertical and substantially flush with the outer sidewalls of the gate spacer 38. The surface of the sidewalls of the protruding fin 24' facing the recess 40 may be on the (110) surface of the protruding fin 24P'.
[0028] According to some embodiments, during the etching of the protruding fins 24', the fin spacers 39 are also etched and their height is reduced. The etching of the fin spacers 39 can be performed while the fins 24' are recessed, wherein one or more etching gases used to etch the fin spacers 39 are added to the etching gas used to recess the protruding fins 24'. According to some embodiments, the fin spacers 39 include external fin spacers, such as fin spacers 39A and 39C ( Figure 4A ), which are located on the outside of the outermost fins in a fin group. Fin spacers 39 also include internal fin spacers, such as fin spacers 39B1 and 39B2, which are located between fins in the same fin group. Throughout this specification, external fin spacers 39 include fin spacers 39C facing the adjacent fin group and fin spacers 39A facing away from the adjacent fin group.
[0029] In some embodiments, the process conditions for etching fin spacers 39 are adjusted so that the height H1 of outer spacer 39A is higher than the heights H2 and H3 of inner spacers 39B1 and 39B2, which are connected to each other due to the small inner fin pitch. In addition, the process for etching the fin spacers is adjusted so that the heights H2 and H3 of inner spacers 39B1 and 39B2 are greater than the height H4 of outer spacer 39C, thereby obtaining the relationship (H1>H2&H3>H4). Height H2 can be greater than, equal to, or less than height H3. The ratios of heights H1, H2, H3, and H4 can also be within a desired range. In some embodiments, the ratios H1 / H2 and H1 / H3 can be greater than approximately 1.05 and can be within a range between approximately 10 nm and approximately 30 nm. The ratios H2 / H4 and H3 / H4 can be greater than approximately 1.2 and can be within a range between approximately 5 nm and approximately 20 nm.
[0030] The etching of the fin spacers can be performed using a fluorine-containing gas such as a mixture of CF4, O2, and N2, a mixture of NF3 and O2, or a mixture of SF6, SF6, and O2. The gas used to bombard the outer spacer 39A is argon. The process conditions that can be adjusted include, but are not limited to, the partial pressures of the etching gas and the bombardment gas, the bias voltage, etc. In addition, the loading effect can be used to help achieve the desired height of the fin spacer. For example, the ratio S2 / S1, that is, the ratio of the inner group spacing S2 to the inner group spacing S1, can be adjusted to adjust the loading effect, thereby adjusting the heights H1, H2, H3, and H4.
[0031] According to some embodiments, after etching the protruding fin 24P′, an additional etching process is performed to further etch the fin spacer 39 and adjust the height of the protruding fin 39. According to an alternative embodiment, etching is skipped. The etching process (if performed) can also be performed using an anisotropic etching process, which uses, for example, a process gas similar to that in the formation of the fin spacer. According to some embodiments, the formation of the fin spacer 39 may not achieve this relationship (H1>H2&H3>H4). For example, in the previous formation of the fin spacer 39, the heights H2 and H3 may be unfavorably smaller than the height H4. Therefore, an etching process is performed to adjust the height of the fin spacer. Alternatively, the relationship (H1>H2 and H3>H4) may have been achieved by the previously formed fin spacer 39, but the ratio between the fin spacer heights H1, H2, H3 and H4 is not satisfactory. Therefore, an additional etching process can be performed to adjust the ratio to the desired value.
[0032] Figure 5 FIG. 4 shows the formation of epitaxial region 48P according to some embodiments, which may include epitaxial layers 48PA, 48PB, and 48PC. Figure 14As shown, the corresponding process is shown as process 212 in process flow 212. Epitaxial layers 48PA, 48PB and 48PC are formed by a selective epitaxial process. The deposition of epitaxial layers 48PA, 48PB and 48PC can be performed using RPCVD, PECVD, etc. According to some embodiments, the deposition of epitaxial layer 48PA is performed by a non-conformal deposition process so that the bottom of epitaxial layer 48PA is thicker than the sidewall portion. According to some embodiments, epitaxial layers 48PA, 48PB and 48PC are formed of SiGeB or include SiGeB. The process gas may include silicon-containing gases such as silane, disilane (Si2H6), dichlorosilane (DCS), etc., germanium-containing gases such as germane (GeH4), digermane (Ge2H6), etc., and process gases containing dopants such as B2H6, etc. The boron concentration of epitaxial layer 48PA can be about 1×10 20 / cm 3 to about 6×10 20 / cm 3 The germanium atomic percentage may be in the range of between about 15% to about 40% and may be gradient, with an upper portion having a higher germanium atomic percentage than a corresponding lower portion.
[0033] Epitaxial layer 48PB may have a higher boron concentration than the boron concentration in epitaxial layer 48PA. For example, the boron concentration in epitaxial layer 48PB may be about 6×10 20 / cm 3 to about 3×10 21 / cm 3 Furthermore, the germanium atomic percentage in epitaxial layer 48PB is higher than the germanium atomic percentage in epitaxial layer 48PA. For example, according to some embodiments, the germanium atomic percentage in epitaxial layer 48PB may be in a range between about 40% and about 60%.
[0034] The top end of the epitaxial layer 48PB is close to the top end of the protruding fin 24P′. Figure 11B Shown Figure 5 The cross-sectional view of reference section B2-B2 in FIG. 1 shows that opposite ends of the epitaxial layer 48PB are flush with the top surface of the protruding fin 24P′, while the surface of the top middle portion of the epitaxial layer 48PB may be lower than, flush with, or slightly higher than the top surface of the protruding fin 24P′. Figure 5 As shown, epitaxial layers 48PB grown from adjacent recesses are merged, and air gap 46P is sealed under epitaxial layer 48PB. The top surface of the merged epitaxial layer 48PB may have a non-planar profile (also referred to as having a wavy (concave) shape), and the middle portion between adjacent fins 24P' (and corresponding recesses 44P) is lower than the portions on the opposite sides thereof. In addition, the left portion of epitaxial layer 48PB closer to protruding fin 24N' is shorter than the right portion of epitaxial layer 48PB.
[0035] The top surface of epitaxial layer 48PC may have a non-wavy (convex) shape. In addition, the right side of the top surface is highest and the left side is lower. According to some embodiments, epitaxial layer 48PC includes silicon SiGeB. According to some embodiments, the boron concentration in epitaxial layer 48PC may be about 8×10 20 / cm 3 to about 1×10 21 / cm 3 In addition, the germanium atomic percentage in epitaxial layer 48PC is lower than the germanium atomic percentage in epitaxial layer 48PB. For example, according to some embodiments, the germanium atomic percentage in epitaxial layer 48PC may be in a range between about 45% and about 55%. Throughout the specification, epitaxial layers 48PA, 48PB, and 48PC are collectively referred to as epitaxial layer (region) 48P, and hereinafter also collectively referred to as source / drain region 48P.
[0036] The deposition process for forming each of epitaxial layers 48PA, 48PB, and 48PC may include an etch-back process after deposition. The etch-back may be performed using an etching gas (e.g., HCl) and may or may not include a silicon-containing gas such as SiH4. The etch-back results in and improves the formation of (111) facets.
[0037] Throughout this specification, the protruding fins 24P' and 24N' that are closest to their adjacent fin group 24N' (the second and third protruding fins from the left) in a fin group are referred to as inner fins, and the protruding fins 24P' and 24N' that are farthest from the adjacent fin group 24N' (the first and fourth protruding fins from the left) in a fin group are referred to as outer fins. Similarly, the portion of the epitaxial region grown based on the inner fin is referred to as the inner portion, and the portion of the epitaxial region grown based on the outer fin is referred to as the outer portion. Because the fin spacers have heights that conform to the relationship (H1>H2 and H3>H4), epitaxial layers 48PB and 48PC have an asymmetric profile, with the inner portions of epitaxial layers 48PB and 48PC being shorter than the outer portions of epitaxial layers 48PB and 48PC. For example, the raised height RH1 of the top end of the inner portion of epitaxial layer 48PB is lower than the raised height RH2 of the top end of the outer portion of epitaxial layer 48PB. The raised height is the height of epitaxial region 48P above the corresponding protruding fin 24P'. The height difference (RH2-RH1) can be greater than about 2 nm and can be within a range of about 2 nm to about 15 nm. In addition, height H5 can be less than height H6, and height H7 can be less than H8, which means that the height of the epitaxial region generally decreases from the outer portion to the inner portion. In general, if the center line 50P between the inner fin 24P' and the outer fin 24P' is used as a reference, the inner portion of the epitaxial region 48P is shorter than the corresponding outer portion. In addition, the top surface of the epitaxial region 48P is tilted toward its adjacent fin group, which is caused by the adjusted heights H1, H2, H3 and H4 of the fin spacers 39.
[0038] After forming the epitaxial region 48P, the epitaxial mask 40N is removed. Figure 14 The process flow 200 is shown as process 214. Next, Figure 6 As shown, an epitaxial mask 40P is formed to protect the epitaxial region 48P while keeping the n-type device region 100N open. Figure 14 As shown, the corresponding process is shown as process 216 in process flow 200. Etch mask 42P can be formed to pattern epitaxial mask 40P and removed after patterning epitaxial mask 40P. Protruding fin 24N' is recessed to form recess 44N. Figure 14As shown, the corresponding process is shown as process 218 in process flow 200. According to some embodiments, the top surface of the remaining protruding fins 24N' is lower than the top end of the fin spacer 39. During the process of etching the protruding fins 24N', the fin spacer 39 is also recessed to achieve the relationship (H1'>H2' and H3'>H4'). According to some embodiments, after the protruding fins 24N' are recessed, an additional etching process is used to further etch the fin spacer 39, and the height of the protruding fins 39 is adjusted so that the relationship (H1'>H2' and H3'>H4') is achieved, and the ratio between the fin spacer heights H1', H2', H3' and H4' is adjusted to obtain the desired ratio. In the additional etching process, the protruding fin 24N' is not recessed. According to an alternative embodiment, the additional etching process is skipped.
[0039] Figure 7 FIG2 shows a selective epitaxial growth process for forming epitaxial layers 48NA, 48NB, and 48NC in n-type FinFET region 100N. Figure 14 The process flow shown is shown as process 220. The cross-sectional shape of the epitaxial layers 48NA, 48NB and 48NC in reference cross section B1-B1 can also be Figure 11B According to some embodiments, the deposition of epitaxial layers 48NA, 48NB, and 48NC may be performed using RPCVD, PECVD, or the like. In the discussion of epitaxial layers 48NA, 48NB, and 48NC ( Figure 11A and Figure 11B ), phosphorus is used as an exemplary n-type dopant, and other n-type dopants (such as arsenic, antimony, etc.) or combinations thereof may also be used. Moreover, in the epitaxial layers 48PA, 48PB, and 48PC ( Figure 11A and Figure 11B ), boron is discussed as an example of a p-type dopant, but other p-type dopants, such as indium, may be used.
[0040] According to some embodiments, epitaxial layer 48NA is formed of or includes silicon phosphorus (SiP). Epitaxial layer 48NA may have a thickness of about 1×10 20 / cm 3 and about 8×10 20 / cm 3 In the deposition process, an etching gas such as HCl is added to the process gas to achieve selective deposition on semiconductors rather than dielectrics. A carrier gas such as H2 and / or N2 may also be included in the process gas, for example, at a flow rate in a range of about 500 sccm to about 5000 sccm.
[0041] According to some embodiments, epitaxial layer 48NB includes SiP, and phosphorus has a second phosphorus concentration that is higher than the phosphorus concentration in epitaxial layer 48NA. For example, according to some embodiments, the phosphorus concentration in epitaxial layer 48NB may be about 8×10 20 / cm 3 to about 5×10 21 / cm 3 The process gas used to form the epitaxial layer 48NB may be similar to the process gas in forming the epitaxial layer 48NA.
[0042] like Figure 7 As shown, the top of epitaxial layer 48NB is close to the top of protruding fin 24N' and can be higher or lower than the top of protruding fin 24N'. Epitaxial layers 48NB grown from adjacent recesses are merged, and air gap 46N is sealed under epitaxial layer 48NB. The top surface of merged epitaxial layer 48NB can have a non-planar profile (also known as having a wavy shape), with the middle portion between adjacent semiconductor fins 24N' lower than the portions on the opposite sides thereof.
[0043] According to some embodiments, epitaxial layer 48NC includes phosphorus silicon. In addition, germanium may be doped, for example, with a germanium atomic percentage between about 1% and about 5%. According to some embodiments, the phosphorus concentration in epitaxial layer 48NC may be between about 1×10 21 / cm 3 to about 3×10 21 / cm 3 The process gas used to form epitaxial layer 48NC can be similar to the process gas used to form epitaxial layer 48NB, except that a germanium-containing gas such as germanium, digermane, etc. can be added. Throughout this specification, epitaxial layers 48NA, 48NB, and 48NC are collectively referred to as epitaxial layers or epitaxial regions 48N, and hereinafter also collectively referred to as source / drain regions 48N.
[0044] The deposition process for forming each of epitaxial layers 48NA, 48NB, and 48NC may include an etch-back process after deposition. The etch-back may be performed using an etching gas (e.g., HCl) and may or may not include a silicon-containing gas such as SiH4. The etch-back results in and improves the formation of (111) facets. In addition, epitaxial layers 48NA, 48NB, and 48NC may have (110) facets formed.
[0045] Because fin spacers 39 have heights having the following relationship (H1' > H2' and H3' > H4'), epitaxial layers 48NB and 48NC have an asymmetric profile, with the inner portions of epitaxial layers 48NB and 48NC growing from the recess of the inner fin being shorter than the outer portions of epitaxial layers 48NB and 48NC growing from the recess of the outer fin. For example, the raised height RH3 of the top of the inner portion of epitaxial layer 48NC is lower than the raised height RH4 of the top of the outer portion of epitaxial layer 48NC. The height difference (RH4-RH3) may be greater than approximately 2 nm and may be within a range between approximately 2 nm and approximately 10 nm. Furthermore, height H5' may be less than height H6', and height H7' may be less than H8', meaning that the height decreases from the outer portion to the inner portion of source / drain region 48N as in a conventional trench. Overall, if centerline 50N is used as a reference, the inner portion of epitaxial region 48N is lower than the corresponding outer portion.
[0046] After forming the epitaxial region 48N, the epitaxial mask 40P is removed, and Figure 8 The resulting structure is shown in Figure 14 In the process flow 200 shown in FIG, the corresponding process is shown as process 222. Next, referring to Figure 9A , a contact etch stop layer (CESL) 52 and an interlayer dielectric (ILD) 54 are formed over the epitaxial regions 48P and 48N and over the dummy gate stack 30 ( Figure 3A and 4B ). The corresponding process is Figure 14 This is shown as process 224 in the illustrated process flow 200. Planarization, such as a chemical mechanical polishing (CMP) process or a mechanical grinding process, is performed to remove excess portions of the CESL 52 and the ILD 54 until the dummy gate stack 30 ( Figure 8 ) was exposed.
[0047] like Figure 9B As shown, the dummy gate stack 30 is replaced with a replacement gate stack 56 ( Figure 3A and Figure 4B ).exist Figure 14 In the process flow shown in FIG, the corresponding process is shown as process 226. It should be understood that the epitaxial region 48P shown is shown as being based on a single fin group, but it can also be formed based on two fin groups, such as Figure 9A The replacement gate stack 56 includes a gate dielectric 58 that also includes an interface layer 58A ( Figure 11B ), and a high-k dielectric 58B ( Figure 11B ). The replacement gate stack 56 also includes a gate electrode 60 over the high-k dielectric 58B. Referring again to Figure 9BAfter forming the replacement gate stack 56, the replacement gate stack 56 is recessed to form trenches between the gate spacers 38. A dielectric material such as silicon nitride, silicon oxynitride, etc. is filled into the resulting trenches. A hard mask 62 ( Figure 9B ).
[0048] Next, refer to Figure 10 , ILD 54 and CESL 52 are etched to form source / drain contact openings 64. Figure 14 In the illustrated process flow, the corresponding process is shown as process 228. Epitaxial layers 48NC and 48PC are also etched through, and the top surfaces of epitaxial layers 48NB and 48PB are exposed. The etch can be controlled to stop on epitaxial layers 48NB and 48PB, with minimal overetching of epitaxial layers 48NB and 48PB. For example, opening 64 can extend into epitaxial regions 48NB and 48PB to a depth ranging from approximately 1 nm to approximately 3 nm. The exposed top surfaces of epitaxial layers 48NB and 48PB are wavy, with recessed portions being lower than opposite portions on opposite sides of the central portion, resulting in the exposed top surfaces of epitaxial layers 48NB and 48PB having a V-shaped cross-sectional profile. The etch of ILD 54 is controlled so that opening 64 extends downward and also etches some side corners of epitaxial regions 48NC and 48PC, exposing the sidewalls of epitaxial layers 48NB and 48PB, and removing some side corner portions. Since the top surfaces of the inner portions of epitaxial regions 48N and 48P are lower than the top surfaces of the corresponding outer portions, it is easier to clean the bottom of opening 64 .
[0049] Next, if Figure 11A and Figure 11B As shown, source / drain silicide regions 66N and 66P are formed. Figure 14 In the process flow shown in , the corresponding process is shown as process 230 . Figure 11B Shown Figure 11A The cross-sectional views in reference sections B1-B1 and B2-B2, Figure 11A Shown in Figure 11B The cross-sectional view of the reference section CC in FIG. Reference sections B1-B1, B2-B2, CC are also Figure 3A According to some embodiments of the present disclosure, the formation of the source / drain silicide regions 66N and 66P includes depositing a metal layer extending into the opening 64, such as a titanium layer, a cobalt layer, etc. ( Figure 10 ), and then an annealing process is performed to react the bottom of the metal layer with the epitaxial layers 48NB and 48PB to form silicide regions 66N and 66P, respectively. The remaining unreacted metal layer can be removed. Then, source / drain contact plugs 68 are formed in the trenches 64 and electrically connected to the source / drain silicide regions 66N and 66P. Figure 14In the process flow shown in FIG, the corresponding process is shown as process 232. Thus, an N-type FinFET 70N and a P-type FinFET 70P are formed, and the source / drain regions 48N and 48P are electrically interconnected through the contact plug 68.
[0050] like Figure 11A As shown, the top surface of each of epitaxial regions 48P and 48N is asymmetric and tilted, with the top surface of the inner portion being lower than the corresponding outer portion. Silicide regions 66N and 66P are tilted accordingly. According to some embodiments, the top surface of the inner portion of each silicide region 66N and 66P is lower than the corresponding outer portion by a height difference ΔH1 and ΔH2, which may be greater than about 2 nm and may be in a range between about 2 nm and about 10 nm. Furthermore, if a cut line 67 is formed on the top surface of silicide regions 66N and 66P, the tilt angles θ1 and θ2 may be greater than about 6 degrees and may be in a range between about 6 degrees and about 45 degrees, or in a range between about 20 degrees and about 45 degrees.
[0051] It is observed that by forming an asymmetric profile for epitaxial regions 48N and 48P, and by making the inner portions of the epitaxial regions lower than the corresponding outer portions, silicide side portions 66N′ and 66P′ are formed (and enlarged) in addition to the portions of silicide regions 66N and 66P directly above epitaxial regions 48N and 48P. This results in an increase in contact area and a decrease in contact resistance. In comparison, if epitaxial regions 48N and 48P were formed to have a symmetrical profile, portions 66N′ and 66P′ of the silicide regions might not be formed or might be smaller, and the contact area and contact resistance would be higher.
[0052] In the above examples, n-type source / drain regions and p-type source / drain regions are discussed and described as examples. According to other embodiments, both FinFETs can be n-type FinFETs or p-type FinFETs. These figures are similar to the above except that the flip symmetry of the two n-type FinFETs or p-type FinFETs is higher. Figure 11A . Moreover, one of the fin groups can be a single fin group, while the other can be a multi-fin group. Although two fin groups are used as an example, the fin group can include three or more fins. In addition, although in the above example, the p-type epitaxial region is formed before the n-type epitaxial region, according to alternative embodiments, the n-type epitaxial region can also be formed before the p-type epitaxial region.
[0053] Figure 121 shows a perspective view of the structure, in which recesses 44N and 44P and protruding fins 24N' and 24P' are shown. It should be understood that recesses 44N and 44P can be formed in the same etching process and thus can coexist at the same time. Alternatively, recesses 44N and 44P can be formed by different processes and thus may not exist at the same time, such as Figure 4A and Figure 6 shown.
[0054] Figure 13 Schematic diagrams of n-type FinFET 68N and p-type FinFET 68P are shown. Silicide regions and contact plugs are not shown. Epitaxial region 48N of n-type FinFET 70N and epitaxial region 48P of p-type FinFET 70P also have asymmetric profiles. According to some embodiments, height H48N of epitaxial region 48N is greater than height H48P of epitaxial region 48P. Furthermore, height H22N of STI region 22N within the inner group spacing of the corresponding fin group in n-type FinFET 70N is shallower than height H22N of STI region 22P within the inner group spacing of the corresponding fin group in p-type FinFET 70P.
[0055] exist Figure 13 In the example shown, the portion of epitaxial region 48P on the inner fin facing epitaxial region 48N is shorter than the portion of epitaxial region 48P on the outer fin facing away from epitaxial region 48N. The portion of epitaxial region 48N on the inner fin facing epitaxial region 48P is shorter than the portion of epitaxial region 48N on the outer fin facing away from epitaxial region 48P. According to other embodiments, the portion of epitaxial region 48P on the inner fin facing epitaxial region 48N can be taller than the portion of epitaxial region 48P on the outer fin facing away from epitaxial region 48N. The portion of epitaxial region 48N on the inner fin facing epitaxial region 48P can also be taller than the portion of epitaxial region 48N on the outer fin facing away from epitaxial region 48P. These embodiments can be implemented by forming an additional n-type epitaxial region (not shown) on the right side of the illustrated epitaxial region 48N in a first formation process, and forming an additional p-type epitaxial region (not shown) on the left side of the illustrated epitaxial region 48P in a second formation process.
[0056] The disclosed embodiments have several advantageous features. By forming epitaxial regions with asymmetric profiles, the source / drain silicide regions can extend to the sidewalls of the corresponding epitaxial source / drain regions, thereby reducing contact resistance. Furthermore, because the inner portion of the epitaxial region is shorter, cleaning the bottom of the opening is easier.
[0057] According to some embodiments of the present disclosure, a method includes: forming an isolation region extending into a semiconductor substrate; forming a first plurality of protruding fins and a second plurality of protruding fins above the isolation region, wherein the first plurality of protruding fins includes: an outer fin distal to the second protruding fin and an inner fin proximal to the second protruding fin; etching the first plurality of protruding fins to form a first recess; growing a first epitaxial region from the first recess, wherein the first epitaxial regions are merged to form a merged epitaxial region; etching the second protruding fin to form a second recess; and growing a second epitaxial region from the second recess, wherein a top surface of the merged epitaxial region is lower on a side facing the second epitaxial region than on a side facing away from the second epitaxial region. In one embodiment, the method further includes forming a plurality of fin spacers on sidewalls of the first plurality of protruding fins, wherein the plurality of fin spacers includes a first outer fin spacer facing the second epitaxial region and a second outer fin spacer facing away from the second epitaxial region, wherein the second outer fin spacer is taller than the first outer fin spacer. In one embodiment, the first outer fin spacer and the second outer fin spacer have bottoms that contact a top surface of the isolation region. In one embodiment, the plurality of fin spacers further include inner fin spacers between adjacent fins in the first plurality of protruding fins, wherein the inner fin spacers are shorter than the first outer fin spacers and taller than the second outer fin spacers. In one embodiment, the inner fin and the outer fin overlap the inner semiconductor stripe and the outer semiconductor stripe, respectively, and wherein the first epitaxial region includes an outer portion directly above the outer semiconductor stripe and an inner portion directly above the inner semiconductor stripe, wherein a first elevated height of the outer portion is higher than a second elevated height of the inner portion. In one embodiment, the bottom of the first recess is higher than a top surface of the isolation region. In one embodiment, the method further includes forming a first silicide region on the merged epitaxial region, wherein the first silicide region is tilted, with a first portion of the first silicide region closer to the second epitaxial region being lower than a second portion of the first silicide region farther from the second epitaxial region. In one embodiment, a tangent line formed on the additional top surface of the first silicide region has a tilt angle greater than approximately 6 degrees. In one embodiment, the method further includes forming a second silicide region on the second epitaxial region; and forming a contact plug connected to the first silicide region and the second silicide region.
[0058] According to some embodiments of the present disclosure, a device includes: a semiconductor substrate; a first plurality of isolation regions and a second plurality of isolation regions extending into the semiconductor substrate; a first stripe group including a first plurality of semiconductor stripes between the first plurality of isolation regions; a second stripe group including at least one second semiconductor stripe between the second plurality of isolation regions; a first fin group including a first plurality of semiconductor fins overlapping corresponding first plurality of semiconductor stripes; a second fin group including at least one second semiconductor fin overlapping at least one second semiconductor stripe; a plurality of epitaxial regions, each epitaxial region including a portion filling a first recess extending into one of the first plurality of semiconductor fins, wherein the plurality of epitaxial regions are merged to form a merged epitaxial region; and a second epitaxial region including a second portion filling a second recess extending into the at least one second semiconductor fin, wherein a top surface of the merged epitaxial region is inclined toward the second epitaxial region, with a first portion proximate the top surface of the second epitaxial region being lower than a second portion distal to the second epitaxial region. In one embodiment, the first plurality of semiconductor stripes include outer stripes farthest from the second fin group and inner stripes closest to the second fin group, wherein the outer portion of the merged epitaxial region overlapping the outer stripes is higher than the inner portion of the merged epitaxial region overlapping the inner stripes. In one embodiment, the merged epitaxial region is of a first conductivity type, and the second epitaxial region is of a second conductivity type opposite to the first conductivity type. In one embodiment, the merged epitaxial region and the second epitaxial region have the same conductivity type. In one embodiment, the device further comprises a first silicide region on the merged epitaxial region, wherein the first silicide region is tilted, wherein a first portion of the first silicide region closer to the second epitaxial region is lower than a second portion of the first silicide region farther from the second epitaxial region. In one embodiment, the device further comprises: a second silicide region located on the second epitaxial region, wherein the second silicide region is tilted toward the first silicide region; and a contact plug connected to the first silicide region and the second silicide region. In one embodiment, the device further comprises: a plurality of fin spacers located on sidewalls of the first plurality of semiconductor fins, wherein the plurality of fin spacers comprises a first outer fin spacer facing the second epitaxial region and a second outer fin spacer facing away from the second epitaxial region, wherein the second outer fin spacer is taller than the first outer fin spacer. In one embodiment, the plurality of fin spacers further includes inner fin spacers between adjacent fins in the first plurality of semiconductor fins, wherein a height of the inner fin spacers is less than a height of the second outer fin spacers and greater than a height of the first outer fin spacers.
[0059] According to some embodiments of the present disclosure, a device includes: a plurality of semiconductor fins; a plurality of gate stacks located on top surfaces and sidewalls of the plurality of semiconductor fins; a plurality of epitaxial regions, each epitaxial region being between two of the plurality of semiconductor fins and engaging the sidewalls, wherein the plurality of epitaxial regions are merged into a merged epitaxial region, and the outermost epitaxial region of the plurality of epitaxial regions is the shortest of the plurality of epitaxial regions; a silicide region contacting the top surface of the merged epitaxial region; and a contact plug located above and in contact with the silicide region. In one embodiment, the device further includes: an additional epitaxial region adjacent to the merged epitaxial region, wherein the outermost epitaxial region is closest to the additional epitaxial region in the plurality of semiconductor fins; and a second silicide region contacting the other top surface of the additional epitaxial region, wherein the contact plug also contacts the second silicide region. In one embodiment, the device further comprises: a plurality of fin spacers on sidewalls of the plurality of epitaxial regions, wherein the plurality of fin spacers comprises a first external fin spacer on a sidewall of an outermost fin among the plurality of semiconductor fins, and a second external fin spacer on an opposite side of the plurality of semiconductor fins from the first external fin spacer, wherein the first external fin spacer is taller than the second external fin spacer.
[0060] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the present disclosure. Those skilled in the art will appreciate that they can easily use this disclosure as a basis for designing or modifying other processes and structures for achieving the same purpose and / or achieving the same advantages of the embodiments introduced herein. Those skilled in the art will also appreciate that such equivalent structures do not depart from the spirit and scope of the present invention, and that they can make various changes, substitutions, and modifications in the present invention without departing from the spirit and scope of the present invention.
Claims
1. A method for forming a semiconductor device, comprising: forming an isolation region extending into the semiconductor substrate; forming a first plurality of protruding fins and a second protruding fin over the isolation region, wherein the first plurality of protruding fins includes outer fins away from the second protruding fins and inner fins closest to the second protruding fins; etching the first plurality of protruding fins to form a first recess; growing a first epitaxial region from the first recess, wherein the first epitaxial regions are merged to form a merged epitaxial region; etching the second protruding fin to form a second recess; growing a second epitaxial region from the second recess, wherein a top surface of the merged epitaxial region is lower on a side facing the second epitaxial region than on a side facing away from the second epitaxial region; and forming a plurality of fin spacers on sidewalls of the first plurality of protruding fins, wherein the plurality of fin spacers comprises: a first external fin spacer facing the second epitaxial region; A second outer fin spacer is disposed away from the second epitaxial region, wherein the second outer fin spacer is taller than the first outer fin spacer.
2. The method according to claim 1, wherein: The first external fin spacer is the shortest among the plurality of fin spacers.
3. The method according to claim 2, wherein: The first outer fin spacer and the second outer fin spacer have bottoms contacting a top surface of the isolation region.
4. The method according to claim 1, wherein: The plurality of fin spacers further includes inner fin spacers between adjacent fins in the first plurality of protruding fins, wherein the inner fin spacers are shorter than the second outer fin spacers and taller than the first outer fin spacers.
5. The method according to claim 1, wherein: The inner fin and the outer fin overlap with the inner semiconductor strip and the outer semiconductor strip, respectively, and wherein the first epitaxial region comprises: An outer portion is directly above the outer semiconductor strip and an inner portion is directly above the inner semiconductor strip, wherein a first elevated height of the outer portion is higher than a second elevated height of the inner portion.
6. The method according to claim 1, wherein: A bottom of the first recess is higher than a top surface of the isolation region.
7. The method according to claim 1, further comprising: A first silicide region is formed on the merged epitaxial region, wherein the first silicide region is inclined, and a first portion of the first silicide region closer to the second epitaxial region is lower than a second portion of the first silicide region farther from the second epitaxial region.
8. The method according to claim 7, wherein: A cut line formed on the additional top surface of the first silicide region has an inclination angle greater than 6 degrees.
9. The method according to claim 7, further comprising: forming a second silicide region on the second epitaxial region; as well as Contact plugs connected to the first silicide region and the second silicide region are formed.
10. A semiconductor device comprising: Semiconductor substrate; a first plurality of isolation regions and a second plurality of isolation regions extending into the semiconductor substrate; a first stripe group comprising a first plurality of semiconductor strips between the first plurality of isolation regions; a second stripe group including at least one second semiconductor stripe between the second plurality of isolation regions; a first fin group including a first plurality of semiconductor fins overlapping a corresponding first plurality of semiconductor strips; a second fin group including at least one second semiconductor fin overlapping at least one second semiconductor strip; a plurality of epitaxial regions, each including a portion filling a first recess extending into one of the first plurality of semiconductor fins, wherein the plurality of epitaxial regions are merged to form a merged epitaxial region; and A second epitaxial region includes a second portion filling a second recess extending into the at least one second semiconductor fin, wherein a top surface of the merged epitaxial region is inclined toward the second epitaxial region, a first portion of the top surface closer to the second epitaxial region is lower than a second portion farther from the second epitaxial region, wherein the merged epitaxial region is separated from the second epitaxial region, the first portion of the top surface overlaps an inner strip of the first plurality of semiconductor strips, and wherein a first isolation region of the first plurality of isolation regions is continuously connected to a second isolation region of the second plurality of isolation regions to form a continuous isolation region, and wherein the continuous isolation region is physically connected to a sidewall of the inner strip.
11. The semiconductor device according to claim 10, wherein: The first plurality of semiconductor strips include an outer strip farthest from the second fin group and an inner strip closest to the second fin group, wherein an outer portion of the merged epitaxial region overlapping the outer strip is taller than an inner portion of the merged epitaxial region overlapping the inner strip.
12. The semiconductor device according to claim 10, wherein: The merged epitaxial region is of a first conductivity type, and the second epitaxial region is of a second conductivity type opposite to the first conductivity type.
13. The semiconductor device according to claim 10, wherein: The merged epitaxial region and the second epitaxial region have the same conductivity type.
14. The semiconductor device according to claim 10, further comprising a first silicide region on the merged epitaxial region, wherein: The first silicide region is inclined, and a first portion of the first silicide region closer to the second epitaxial region is lower than a second portion of the first silicide region farther from the second epitaxial region.
15. The semiconductor device according to claim 14, further comprising: a second silicide region located on the second epitaxial region, wherein the second silicide region is inclined toward the first silicide region; and A contact plug is connected to the first silicide region and the second silicide region.
16. The semiconductor device according to claim 10, further comprising: A plurality of fin spacers are located on sidewalls of the first plurality of semiconductor fins, wherein the plurality of fin spacers include a first external fin spacer facing the second epitaxial region and a second external fin spacer away from the second epitaxial region, wherein the second external fin spacer is taller than the first external fin spacer.
17. The semiconductor device according to claim 16, wherein: The plurality of fin spacers further includes inner fin spacers between adjacent fins in the first plurality of semiconductor fins, wherein a height of the inner fin spacers is less than a height of the second outer fin spacers and greater than a height of the first outer fin spacers.
18. A semiconductor device comprising: a plurality of semiconductor fins; a plurality of gate stacks located on top surfaces and sidewalls of the plurality of semiconductor fins; a plurality of epitaxial regions, respectively between two of the plurality of semiconductor fins and joining sidewalls of the two of the plurality of semiconductor fins, wherein the plurality of epitaxial regions are merged into a merged epitaxial region, the merged epitaxial region is separated from other epitaxial regions, and the apex of the outermost epitaxial region of the plurality of epitaxial regions is the lowest among the apex of all the plurality of epitaxial regions; a silicide region in contact with a top surface of the merged epitaxial region; and A contact plug is located above the silicide region and contacts the silicide region.
19. The semiconductor device according to claim 18, further comprising: an additional epitaxial region adjacent to the merged epitaxial region, wherein an outermost epitaxial region is closest to the additional epitaxial region of the plurality of epitaxial regions; and A second silicide region contacts the additional top surface of the additional epitaxial region, wherein the contact plug also contacts the second silicide region.
20. The semiconductor device according to claim 18, further comprising: A plurality of fin spacers are located on side walls of the plurality of epitaxial regions, wherein the plurality of fin spacers include a first external fin spacer on the side wall of an outermost fin among the plurality of semiconductor fins, and a second external fin spacer on a side opposite to the first external fin spacer among the plurality of semiconductor fins, wherein the first external fin spacer is taller than the second external fin spacer.