III-V compound semiconductor layer stack with electrical isolation provided by a trap-rich layer
By forming a stack of polycrystalline layers and III-V compound layers on the semiconductor substrate, the problem of electrical leakage of semiconductor structures in high-voltage power electronic devices is solved, and higher electrical isolation and lower radio frequency losses are achieved.
Patent Information
- Application Number
- CN202110684415.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-07-21
- Filing Date
- 2021-06-21
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-06-21
AI Technical Summary
The existing semiconductor structures are susceptible to high capacitance and electrical leakage between component bodies in high voltage power electronic devices, resulting in high sensitivity, and existing improvement measures have not yet effectively solved the problem of electrical isolation.
Using a semiconductor substrate composed of a single crystal semiconductor material, a layer stack of polycrystalline layers and III-V compound semiconductor materials is formed. The substrate lattice is damaged by ion implantation process and recrystallized by heat treatment to form a polycrystalline with high resistivity. The layer and a single crystal layer are combined with the epitaxial growth process to form a stack of III-V compound semiconductor layers to build an active device structure.
It significantly improves electrical isolation capability, reduces RF loss, and improves the linearity and operation stability of high electron mobility transistors.
Smart Images

Figure CN113964178B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to semiconductor device manufacturing and integrated circuits, and more particularly to a semiconductor structure including electrical isolation and a method for forming the semiconductor structure including electrical isolation. Background Art
[0002] When formed using bulk semiconductor wafers, device structures such as high voltage power electronic devices are susceptible to high capacitance and body-to-body leakage. One measure that can be taken to reduce sensitivity is to provide the bulk semiconductor wafer with triple well isolation, which surrounds the active device region containing the device structure. Another measure that can be taken to reduce sensitivity is to replace the bulk wafer with a silicon-on-insulator wafer, where the top silicon layer provides the active device region and a buried oxide (BOX) layer is provided between the active device region and the substrate located below the buried insulator layer.
[0003] High voltage power electronic devices such as high electron mobility transistors can be manufactured using III-V compound semiconductors to take advantage of their material properties, such as carrier mobility greater than that of silicon. III-V compound semiconductors are obtained by combining group III elements (aluminum, gallium, indium) with group V elements (nitrogen, phosphorus, arsenic, antimony). High electron mobility transistors may include heterojunctions between III-V compound semiconductor materials with different band gaps, such as a heterojunction between binary gallium nitride and ternary aluminum gallium nitride. During operation, a two-dimensional electron gas is formed near the interface at the heterojunction of the high electron mobility transistor. The two-dimensional electron gas defines the channel of the high electron mobility transistor.
[0004] While these approaches have proven suitable for their intended purposes, there is a need for semiconductor structures having improved electrical isolation and methods of forming semiconductor structures including improved electrical isolation. Summary of the invention
[0005] In one embodiment of the present invention, a structure includes a semiconductor substrate composed of a single crystal semiconductor material, a layer stack located on the semiconductor substrate, and a polycrystalline layer located in the semiconductor substrate. The layer stack includes a semiconductor layer composed of a III-V compound semiconductor material, and the polycrystalline layer extends laterally below the layer stack.
[0006] In one embodiment of the present invention, a method includes forming a polycrystalline layer in a semiconductor substrate composed of a single crystal semiconductor material, and forming a layer stack on the semiconductor substrate. The layer stack includes a semiconductor layer composed of a III-V compound semiconductor material, and the polycrystalline layer extends laterally below the layer stack. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] The accompanying drawings, which are included in and constitute a part of this specification, illustrate various embodiments of the present invention and, together with the general description of the present invention made above and the detailed description of these embodiments made below, are used to explain these embodiments of the present invention. In the accompanying drawings, like reference numerals represent similar features in different views.
[0008] Figure 1-4 Cross-sectional views of structures at successive stages of fabrication in a process recipe according to an embodiment of the present invention are shown.
[0009] Figure 5-7 Cross-sectional views of structures at successive stages of fabrication in a process recipe are shown in accordance with an alternative embodiment of the present invention. DETAILED DESCRIPTION
[0010] Please refer to Figure 1 According to an embodiment of the present invention, a semiconductor substrate 10 comprising a single crystal semiconductor material (e.g., single crystal silicon) is provided. The semiconductor substrate 10 may be a bulk substrate comprising a single crystal semiconductor material (e.g., single crystal silicon). In an alternative embodiment, the semiconductor substrate 10 may be a silicon-on-insulator substrate or an engineered substrate. In one embodiment, the semiconductor substrate 10 may be a high resistivity bulk substrate comprising single crystal silicon having a resistivity greater than or equal to 1000 ohm-cm. In one embodiment, the semiconductor substrate 10 may be a high resistivity bulk substrate comprising single crystal silicon having a resistivity in a range from 1000 ohm-cm to 50,000 ohm-cm. In an alternative embodiment, the semiconductor substrate 10 may be a low resistivity bulk substrate comprising single crystal silicon having a resistivity less than 1000 ohm-cm. In one embodiment, the single crystal semiconductor material of the semiconductor substrate 10 may be oriented with a (111) surface normal. The choice of substrate resistivity is driven by the need to minimize RF losses in semiconductor substrate 10 for both active devices (such as field effect transistors) and passive devices (such as inductors or transmission lines). Increasing the resistivity of semiconductor substrate 10 can reduce RF losses for both active and passive devices.
[0011] An implantation layer 14 including damaged or amorphous semiconductor material is formed in the semiconductor substrate 10. The implantation layer 14 may be formed by an ion implantation process that introduces energetic ions, as indicated schematically by a single arrow, with the ion trajectory passing through the semiconductor substrate 10 along a path. The energetic ions lose energy along their path through random scattering events with nuclei and electrons in the semiconductor material they pass through. The energy loss in the nuclear collision causes the target atoms of the semiconductor substrate 10 to shift from their original lattice positions, thereby damaging the lattice structure of the semiconductor substrate 10 and generating point defects. The lattice structure of the semiconductor substrate 10 is damaged or amorphized within the implantation layer 14 compared to an undamaged region 16 of the single crystalline semiconductor material of the semiconductor substrate 10 located below the lower boundary of the implantation layer 14. Due to the use of a high dose of implanted species, the implantation layer 14 of the semiconductor substrate 10 may be changed from a crystalline semiconductor material (e.g., single crystal silicon) to a damaged or amorphous semiconductor material (e.g., amorphous silicon).
[0012] The ions may be generated from a suitable source gas and implanted into the semiconductor substrate 10 using an ion implantation tool with one or more implantation conditions. The implantation conditions (e.g., ion species, dose, energy) of the ion implantation process may be selected to adjust the characteristics of the implanted layer 14. In one embodiment, the ions may be generated from an inert gas, such as He, Ne, Ar, Kr, Xe, Rn, or Og. In an alternative embodiment, the ions may be O ions, N ions, Ge ions, Si ions, or other elements that do not or minimally dope the semiconductor wafer. In one embodiment in which the semiconductor substrate 10 will remain crystalline at the top surface 12, the ion dose is selected to be less than a threshold ion dose, beyond which it is impossible to recrystallize the damaged semiconductor material in the implanted layer 14 by subsequent annealing. In one embodiment, the Ar ion dose may be greater than 1x10 14 ions / cm2. In one embodiment, the Ar ion dose may be 1x10 14 ions / cm2 to 5x10 15 ions / square centimeter. In one embodiment, the Ar ion energy may be in the range of about 30 keV to about 1000 keV. The energy and dosage of other inert gas species may be similar. The energy and dosage of non-inert gas elements may be similar or lower. For example, if O is used, a lower dosage may be used, that is, 10 to 1000 times lower. The ion implantation conditions may include a single implantation, multiple implantations performed at different energies, segmented implantations, etc. A thin silicon dioxide layer (not shown) may be laid on the top surface 12 of the semiconductor substrate 10 before performing the ion implantation process and removed after the ion implantation process.
[0013] Please refer to Figure 2 , wherein similar reference numerals denote Figure 1In the next manufacturing stage of the process method, the semiconductor substrate 10 is subjected to a heat treatment (ie, an annealing process), which causes the implantation layer 14 ( Figure 1 ) undergoes the heat treatment. In one embodiment, the heat treatment for heat treating the implanted layer 14 of the semiconductor substrate 10 may be a rapid thermal annealing. In one embodiment, the rapid thermal annealing may be performed by using, for example, a bank of flash lamps to heat the semiconductor substrate 10 to a peak temperature in the range of 900° C. to 1125° C. and having a dwell time of 30 milliseconds to 5 seconds at the peak temperature, and in a specific embodiment, the peak temperature may be 1000° C., which is maintained for a dwell time of less than or equal to 1 second.
[0014] The thermal treatment recrystallizes a portion of the damaged semiconductor material of the implanted layer 14 into a polycrystalline layer 18 in the semiconductor substrate 10, the polycrystalline layer 18 comprising grains of polycrystalline semiconductor material (e.g., polycrystalline silicon) and defects outside the polycrystalline grains as residual damage. The defects may include trapped atoms of the implanted species (e.g., argon). The thermal treatment also recrystallizes the damaged semiconductor material of the implanted layer 14 between the polycrystalline layer 18 and the top surface 12 into a layer 24 of the semiconductor substrate 10, which comprises a single crystal semiconductor material (e.g., single crystal silicon). Compared to the polycrystalline layer 18, the recrystallized single crystal semiconductor material in the layer 24 is free of polycrystalline grains and defects.
[0015] In this representative embodiment, polycrystalline layer 18 may include a single layer of polycrystalline semiconductor material. In an alternative embodiment, if multiple implant energies (i.e., implant depths) are used to form implant layer 14, the implantation and thermal treatment may result in multiple layers of polycrystalline semiconductor material. Recrystallized single crystal layer 24 is located between upper boundary 20 of polycrystalline layer 18 and top surface 12, and semiconductor substrate 10 includes single crystal semiconductor material located below lower boundary 22 of polycrystalline layer 18. In one embodiment, polycrystalline layer 18 may be thinner than implant layer 14 ( Figure 1 In an alternative embodiment where the implanted layer 14 is recrystallized by furnace annealing as the thermal treatment, the polycrystalline layer 18 may extend completely to the top surface 12 of the semiconductor substrate 10. The furnace annealing may be performed at a temperature in the range of 900°C to 1100°C.
[0016] The polycrystalline layer 18 may be characterized as a trap-rich material having a resistivity greater than or equal to the resistivity of the single crystalline semiconductor material of the semiconductor substrate 10. In one embodiment, the polycrystalline layer 18 may have a resistivity greater than or equal to 1000 ohm-cm. In one embodiment, the resistivity of the polycrystalline layer 18 may be in a range of 10,000 ohm-cm to 1,000,000 ohm-cm. In one embodiment, the single crystalline semiconductor material of the substrate may have a resistivity of 1,000 ohm-cm to 10,000 ohm-cm, and the polycrystalline layer 18 may have a resistivity 10 to 100 times greater (i.e., in a range of 10,000 to 1,000,000 ohm-cm).
[0017] Please refer to Figure 3 , wherein similar reference numerals denote Figure 2 , and in the next manufacturing stage of the process method, a layer stack 25 including one or more non-Group IV semiconductor layers is formed on the top surface 12 of the semiconductor substrate 10. In one embodiment, the layer stack 25 may include one or more layers composed of Group III-V compound semiconductor materials. In one embodiment, the layer stack 25 may include multiple layers composed of different Group III-V compound semiconductor materials.
[0018] In one embodiment, the layer stack 25 may include a buffer layer 26, a channel layer 28, a spacer layer 30, and a barrier layer 32. The layers 26, 28, 30, 32 may be formed successively by using an epitaxial growth process such as metal organic chemical vapor deposition. The layers 26, 28, 30, 32 may each have a crystal structure that is single crystalline, or substantially single crystalline with varying degrees of crystal defects. The layers 26, 28, 30, 32 may also have a plurality of sublayers having different compositions or doping. The buffer layer 26 may have a plurality of sublayers that are adjusted in terms of material composition, doping, and / or layer thickness to accommodate the lattice mismatch between the material of the semiconductor substrate 10 and the material of the channel layer 28. The buffer layer 26 may include a seed layer adjacent to the semiconductor substrate 10 that includes a material such as aluminum nitride. The channel layer 28 disposed above the buffer layer 26 may include a III-V compound semiconductor material such as gallium nitride. A spacer layer 30 and a barrier layer 32 are disposed above the channel layer 28, with the spacer layer 30 being located between the channel layer 28 and the barrier layer 32. The spacer layer 30 may be thin and may include a material such as aluminum nitride. The barrier layer 32 may include a material such as aluminum gallium nitride, aluminum nitride, or indium aluminum nitride, which provides an interface with the channel layer 28 having a different composition. The spacer layer 30 and the barrier layer 32 together with the material properties of the channel layer 28 contribute to the generation of a two-dimensional electron gas at the interface filled with highly mobile and abundant electrons during device operation.
[0019] Please refer to Figure 4, wherein similar reference numerals denote Figure 3 , and in the next manufacturing stage of the process method, the layer stack 25 of compound III-V semiconductor materials can be used to form an active device structure 31. For example, the active device structure 31 can be a high-electron-mobility transistor (HEMT) including a gate electrode 34, a source region 36, and a drain region 38. The gate electrode 34 can be composed of a metal, such as a metal nitride, and can be patterned using a photolithography and etching process to define a given shape. To form the source region 36 and the drain region 38, an opening can be patterned in the spacer layer 30 and the barrier layer 32 using a photolithography and etching process, and then a metal, such as a metal nitride, which can be patterned using a photolithography and etching process, is deposited. The source region 36 and the drain region 38 can directly contact the channel layer 28, and metal atoms from the source and drain regions 36, 38 can diffuse into the channel layer 28. Although not shown, the layer stack 25 may be patterned using photolithography and etching processes associated with forming the active device structure 31 to define raised mesas that are capped by subsequently deposited dielectric material.
[0020] Then, the middle process and the back-end process are performed, which include forming contacts, vias, and lines of the interconnect structure 40 coupled to the active device structure 31. In one embodiment, a passive device 42, such as an inductor, a capacitor, a resistor, or a transmission line, may be formed by the back-end process in the interconnect structure 40. In one embodiment, the active device structure 31 may not exist, and only the passive device 42 may exist.
[0021] The polycrystalline layer 18 characterized by high electrical resistance may improve the linearity of the active device structure 31 during operation.
[0022] Please refer to Figure 5 , wherein similar reference numerals denote Figure 2 , and in the next manufacturing stage of the process method according to the alternative embodiment, after forming the implant layer 14, but before the thermal treatment to convert the implant layer 14 into the polycrystalline layer 18, a dielectric layer 46 can be deposited on the top surface 12 of the semiconductor substrate 10. The dielectric layer 46 can be patterned using photolithography and etching processes to cover the area 48 of the semiconductor substrate 10 and not cover (expose) the area 50 of the semiconductor substrate 10. The dielectric layer 46 can be composed of silicon nitride and / or silicon dioxide. In one embodiment, the dielectric layer 46 can include a silicon dioxide sublayer formed by thermal oxidation and a thicker silicon nitride sublayer formed on the silicon dioxide sublayer by liquid phase chemical vapor deposition.
[0023] Please refer to Figure 6 , wherein similar reference numerals denote Figure 5and in the next manufacturing stage of the process method, such as combining Figure 2 The thermal treatment is performed to convert the implanted layer 14 into a polycrystalline layer 18. A single crystalline semiconductor material layer 24 is formed from the implanted layer 14 during the thermal treatment and is located between the polycrystalline layer 18 and the top surface 12 in a region 50 where the dielectric layer 46 is not present on the top surface 12. A segment 18a of the polycrystalline layer 18 located below the dielectric layer 46 in the region 48 is thicker than a segment 18b of the polycrystalline layer 18 located in the region 50. Specifically, the polycrystalline layer 18 located in the region 50 has a thickness t1, and the segment 18a of the polycrystalline layer 18 located in the region 48 has a thickness t2 that is greater than the thickness t1. In one embodiment, the segment 18a of the polycrystalline layer 18 may have an upper boundary that coincides or substantially coincides with the top surface 12 of the semiconductor substrate 10. In one embodiment, the segments 18a, 18b of the polycrystalline layer 18 and the single crystalline layer 24 may have a thickness in a range of about 100 nanometers (nm) to about one (1) micrometer (um).
[0024] Please refer to Figure 7 , wherein similar reference numerals denote Figure 6 and in the next manufacturing stage of the process method, the dielectric layer 46 is removed and a layer stack 25 is formed on the top surface 12 of the semiconductor substrate 10, such as in combination with Figure 3 In one embodiment, by using the layer stack 25, an active device structure 31 ( Figure 4 ).
[0025] The section of the layer stack 25 in region 48 formed over the thicker section 18a of the polycrystalline layer 18 has a different crystalline state than the section of the layer stack 25 in region 50 formed over the layer of single crystalline semiconductor material 24. In particular, the section of the layer stack 25 in region 48 may be disordered, while the layer stack 25 in region 50 may have a single crystalline or substantially single crystalline crystal structure, due to the presence of the polycrystalline layer 18 in region 48 that delays crystallization as a non-single crystalline template at the top surface 12 for the epitaxial growth process. In one embodiment, the section of the layer stack 25 formed over the thicker section 18a of the polycrystalline layer 18 may include amorphous III-V semiconductor material in the portions of the layers 26, 28, 30, 32 associated with this section of the layer stack 25. The section of the layer stack 25 formed in the region 48 may reduce mechanical stress, thereby allowing the use of a thinner semiconductor substrate 10 , and the section of the layer stack 25 formed in the region 50 may provide electrical isolation for subsequently formed active device structures 31 .
[0026] The above method is used for the manufacture of integrated circuit chips. The manufacturer can distribute the resulting integrated circuit chips in raw wafer form (e.g., as a single wafer with multiple unpackaged chips), as a bare chip, or in a packaged form. In the latter case, the chip is provided in a single-chip package (e.g., a plastic carrier having pins attached to a motherboard or other higher-level carrier) or in a multi-chip package (e.g., a ceramic carrier having single-sided or double-sided interconnects or embedded interconnects). In any case, the chip can be integrated with other chips, discrete circuit elements and / or other signal processing devices as part of an intermediate product or a final product.
[0027] Terms modified by approximate language such as "about," "approximately," and "substantially" cited herein are not limited to the exact value specified. The approximate language may correspond to the precision of the instrument used to measure the value, and may represent + / -10% of the value unless otherwise dependent on the precision of the instrument.
[0028] Terms such as "vertical", "horizontal", etc. are cited herein as examples to establish a reference frame and are not limiting. The term "horizontal" as used herein is defined as a plane parallel to the conventional plane of the semiconductor substrate, regardless of its actual three-dimensional spatial orientation. The terms "vertical" and "orthogonal" refer to directions perpendicular to the horizontal plane as just defined. The term "lateral" refers to a direction within the horizontal plane.
[0029] A feature that is "connected" or "coupled" to another feature may be directly connected or coupled to the other feature, or one or more intermediate features may be present. A feature may be "directly connected" or "directly coupled" to another feature if there are no intermediate features. A feature may be "not directly connected" or "not directly coupled" to another feature if there are at least one intermediate feature. A feature that is "on" or "in contact with" another feature may be directly on or in direct contact with the other feature, or one or more intermediate features may be present. A feature may be directly "on" or "in direct contact with" another feature if there are no intermediate features. A feature may not be "directly" "on" or "not directly in contact with" another feature if there are at least one intermediate feature.
[0030] The description of various embodiments of the present invention is for illustrative purposes and is not intended to be exhaustive or limited to the disclosed embodiments. Many modifications and variations will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the described embodiments. The terms used herein are selected to best explain the principles of the embodiments, practical applications, or technical improvements over commercially known technologies, or to enable those of ordinary skill in the art to understand the embodiments disclosed herein.
Claims
1. A semiconductor structure comprising: a semiconductor substrate comprising a single crystalline semiconductor material, the semiconductor substrate having a top surface; a layer stack located on the top surface of the semiconductor substrate, the layer stack comprising a first layer composed of a first III-V compound semiconductor material; as well as A polycrystalline layer is located in the semiconductor substrate, the polycrystalline layer extends laterally below the layer stack, the polycrystalline layer includes a first segment having a first thickness and a second segment having a second thickness greater than the first thickness, and the second segment of the polycrystalline layer has a boundary that substantially coincides with the top surface of the semiconductor substrate.
2. The semiconductor structure according to claim 1, wherein: The single crystalline semiconductor material of the semiconductor substrate is oriented with a (111) surface normal.
3. The semiconductor structure according to claim 2, wherein: The polycrystalline layer has a resistivity in a range of 10,000 ohm-cm to 1,000,000 ohm-cm.
4. The semiconductor structure according to claim 1, wherein: The polycrystalline layer includes an upper boundary and a lower boundary, and the semiconductor substrate includes a layer of the single crystalline semiconductor material between the top surface and the upper boundary of the polycrystalline layer.
5. The semiconductor structure according to claim 1, wherein: The first III-V compound semiconductor material of the first layer has a substantially single-crystalline crystal structure.
6. The semiconductor structure of claim 1, wherein: The first III-V compound semiconductor material of the first layer over the first section of the polycrystalline layer is substantially single crystalline, and the first III-V compound semiconductor material of the first layer over the second section of the polycrystalline layer is disordered.
7. The semiconductor structure of claim 1, further comprising: An active device includes a gate electrode located on the layer stack.
8. The semiconductor structure of claim 7, wherein: The active device is a high electron mobility transistor.
9. The semiconductor structure of claim 1, further comprising: an interconnect structure located above the layer stack and the polycrystalline layer; as well as A passive device is located in the interconnect structure.
10. The semiconductor structure of claim 1, wherein: The layer stack comprises a second layer consisting of a second III-V compound semiconductor material, and the second III-V compound semiconductor material has a different composition than the first III-V compound semiconductor material.
11. The semiconductor structure of claim 9, wherein: The first III-V compound semiconductor material is gallium nitride.
12. A semiconductor structure comprising: a semiconductor substrate comprising a single crystal semiconductor material; a layer stack located on the semiconductor substrate, the layer stack comprising a first layer composed of a first III-V compound semiconductor material; as well as a polycrystalline layer in the semiconductor substrate, the polycrystalline layer extending laterally below the layer stack, the polycrystalline layer comprising a first section having a first thickness and a second section having a second thickness greater than the first thickness, The first III-V compound semiconductor material of the first layer located above the first section of the polycrystalline layer is substantially single crystalline, and the first III-V compound semiconductor material of the first layer located above the second section of the polycrystalline layer is disordered.
13. The semiconductor structure of claim 12, wherein: The layer stack comprises a second layer consisting of a second III-V compound semiconductor material, and the second III-V compound semiconductor material has a different composition than the first III-V compound semiconductor material.
14. The semiconductor structure of claim 12, further comprising: An active device includes a gate electrode located on the layer stack above the first section of the polycrystalline layer.
15. A method of forming a semiconductor structure, comprising: forming a polycrystalline layer in a semiconductor substrate, wherein the semiconductor substrate comprises a single crystalline semiconductor material; and forming a layer stack on a top surface of the semiconductor substrate, The layer stack includes a layer composed of a III-V compound semiconductor material, the polycrystalline layer extends laterally below the layer stack, the polycrystalline layer includes a first segment having a first thickness and a second segment having a second thickness greater than the first thickness, and the second segment of the polycrystalline layer has a boundary that substantially coincides with the top surface of the semiconductor substrate.
16. The method of claim 15, wherein: Forming the polycrystalline layer in the semiconductor substrate composed of the single crystalline semiconductor material includes: implanting ions into the semiconductor substrate to cause crystalline damage to the single crystalline semiconductor material of the semiconductor substrate in an implanted layer below the top surface of the semiconductor substrate; and The implanted layer of the semiconductor substrate is recrystallized by an annealing process to generate the polycrystalline layer.
17. The method of claim 16, wherein: The polycrystalline layer has a resistivity in a range of 10,000 ohm-cm to 1,000,000 ohm-cm.
18. The method of claim 16, further comprising: A patterned dielectric layer is disposed over the top surface of the semiconductor substrate, the patterned dielectric layer exposing a first region of the semiconductor substrate and covering a second region of the semiconductor substrate.
19. The method of claim 18, wherein: The patterned dielectric layer is laid before recrystallizing the implanted layer of the semiconductor substrate.
20. The method of claim 15, further comprising: A gate electrode of an active device is formed on the layer stack.
21. The method of claim 15, wherein: The single crystalline semiconductor material of the semiconductor substrate is oriented with a (111) surface normal.