Flattening process, device and method for manufacturing articles
Through the combination of a multi-region chuck system and a cladding chuck, the height change and inhomogeneity problems in planarization technology in semiconductor manufacturing are solved, the focus depth and feature filling capabilities are improved, and the device quality is improved.
Patent Information
- Application Number
- CN202080051149.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-08-15
- Filing Date
- 2020-07-17
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-07-17
AI Technical Summary
The existing planarization technology has high variation and non-uniformity problems in semiconductor manufacturing, which affects the addition of layered substrates and device quality, especially in ArFi laser, extreme ultraviolet lithography and nanoimprint lithography technologies.
Using a multi-area chuck system and a cladding chuck, the cladding plate is gradually deflected by applying pressure and vacuum, combined with droplet patterning technology of forming materials, the contact and curing process between the cladding plate and the substrate is optimized to achieve a more uniform Flattening.
The focus depth, critical dimensional uniformity and feature filling capability are improved, the non-filling defects and excessive constraints are reduced, and the quality of the planarized film layer and the accuracy of device manufacturing are enhanced.
Smart Images

Figure CN114127911B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to substrate processing and, more particularly, to surface planarization in semiconductor manufacturing. Background Art
[0002] Planarization technology is useful in manufacturing semiconductor devices. For example, the process for forming semiconductor devices includes repeatedly adding material to and removing material from a substrate. The process can produce a layered substrate with irregular height variations (i.e., topography), and as more layers are added, the substrate height variation increases. Height variations have an adverse effect on the ability to add more layers to the layered substrate. In addition, the semiconductor substrate (e.g., silicon wafer) itself is not always completely flat and may include initial surface height variations (i.e., topography). One way to solve this problem is to flatten the substrate between layering steps. Various lithography patterning methods benefit from patterning on a flat surface. In ArFi laser-based lithography, flattening improves depth of focus (DOF), critical dimension (CD), and critical dimension uniformity. In extreme ultraviolet lithography (EUV), flattening improves feature layout and DOF. In nanoimprint lithography (NIL), flattening improves feature filling and CD control after pattern transfer.
[0003] Planarization techniques, sometimes referred to as inkjet-based adaptive planarization (IAP), involve dispensing a variable droplet pattern of a polymerizable material between a substrate and a superstrate, wherein the droplet pattern varies based on the substrate topography. The superstrate is then contacted with the polymerizable material, after which the material polymerizes on the substrate and the superstrate is removed. Improvements in planarization techniques, including IAP techniques, are needed to improve, for example, overall wafer processing and semiconductor device manufacturing. Summary of the invention
[0004] A method is provided. The method includes holding a superstrate with a superstrate chuck. Applying pressure to deflect the superstrate toward a substrate. The deflection of the superstrate gradually extends in a radial direction. Maintaining the application of a vacuum applied to a periphery of the superstrate, and the superstrate is continuously held by the chuck while the superstrate is deflected by the pressure. Releasing the vacuum from the periphery of the superstrate and releasing the superstrate from the chuck.
[0005] The cover plate chuck may include a central region aligned with a central portion of the cover plate and a series of annular regions. The series of annular regions may include a peripheral annular region aligned with a periphery of the cover plate and at least one inner annular region between the central region and the peripheral annular region. The step of applying pressure to deflect the cover plate may also include applying pressure through the central region and maintaining a vacuum applied through the series of annular regions, releasing the vacuum from the annular regions and applying pressure through the inner annular regions after the central portion of the cover plate has been deflected by the pressure, and releasing the vacuum from the peripheral annular regions.
[0006] The series of annular regions may include a plurality of inner annular regions. The vacuum is sequentially released from the inner regions, and pressure is sequentially applied to the cover plate in a radial direction through the inner rings. The method may also include dispensing the formable material contact portion on the substrate, contacting the cover plate with the formable material contact portion, and applying a pressure corresponding to the flow front of the formable material contact portion to the cover plate. Preferably but optionally, the formable material contact portion is dispensed in the form of a plurality of droplets deposited on the substrate. Pressure may be applied to the central region to control the initial height within a determined range and maintain a predetermined curvature of the cover plate.
[0007] The method may further include curing the formable material contact portion after the cover sheet is released from the chuck, moving the lateral position of the cover sheet relative to the curing source during curing, re-holding the cover sheet with the chuck; and separating the cover layer from the cured formable material contact portion.
[0008] A multi-zone chuck system is also provided. The multi-zone chuck system includes a substrate chuck for holding a substrate and a cover plate chuck for holding a cover plate. The system also includes a pressure source configured to apply pressure and vacuum to the cover plate via multiple ports of the cover plate chuck. Preferably, the pressure is applied sequentially to multiple zones of the cover plate so that the cover plate is gradually deflected toward the substrate from one zone to another. When the cover plate is deflected by the pressure, the vacuum is applied to the periphery of the cover plate.
[0009] The cover plate chuck may include a plurality of concentric ridges that define the cover plate chuck as a central region and a series of annular regions, the series of annular regions including a peripheral region aligned with the periphery of the cover plate and at least one inner annular region between the central region and the peripheral annular region. The pressure source may be configured to sequentially apply pressure via a port in the central region, while applying vacuum via a port in a series of annular regions, applying pressure via a port in the inner annular region and maintaining vacuum in the peripheral annular region, and releasing vacuum from a port in the peripheral annular region. The central region of the cover plate chuck includes an air cavity that is aligned with the center of the cover plate while contacting the cover plate with a formable material. The multi-region chuck system may also include a formable material dispenser configured to dispense a plurality of droplets of a formable material onto a substrate. The cover plate chuck is configured to advance the cover plate so that it contacts the formable material on the substrate. The pressure source is configured to sequentially apply pressure to an area corresponding to a flow front of the formable material.
[0010] The multi-zone chuck system may further include a curing source configured to cure the formable material after the cover is released from the cover chuck. The substrate chuck is configured to move a lateral position of the substrate relative to the curing source. The curing source is configured to control the size of the beam with reference to the diameter of the cover during curing. The curing source may also be configured to control a tilt angle of the beam incident on the cover.
[0011] A method for forming a layer is also provided. The method includes dispensing a formable material on a substrate, holding a cover plate with a chuck, and advancing the cover plate through the chuck to contact the formable material. Pressure is sequentially applied to multiple areas of the cover plate so that the cover plate is gradually deflected toward the substrate from one area to another. When the cover plate is deflected by the pressure, a vacuum is applied to the periphery of the cover plate. The cover plate is then released from the chuck. Then, a curing process is performed on the formable material behind the chuck with a curing source.
[0012] The method may also include moving the lateral position of the substrate relative to the curing source during curing. The beam size of the curing source may be controlled with reference to the diameter of the cover plate. The tilt angle of the beam incident on the cover plate may be adjusted. The method also includes re-holding the cover plate by the cover plate chuck; and separating the cover plate from the cured formable material.
[0013] These and other objects, features and advantages of the present disclosure will become apparent when the following detailed description of exemplary embodiments of the present disclosure is read in conjunction with the accompanying drawings and the appended claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] By referring to the embodiments shown in the accompanying drawings, embodiments of the present invention can be described in more detail so that the features and advantages of the present invention can be understood in detail. However, it should be noted that the accompanying drawings only illustrate typical embodiments of the present invention and therefore should not be considered as limiting the scope of the present invention, as the present invention may allow other equally effective embodiments.
[0015] Figure 1 is a schematic diagram showing a planarization system;
[0016] FIG. 2A to FIG. 2C The planarization process is shown;
[0017] FIG. 3A to FIG. 3B A multi-zone cover plate chuck in one embodiment is shown;
[0018] FIG. 4A to FIG. 4E The operation of a superstrate chuck for forming a layer on a substrate is shown;
[0019] Figure 5 Yes FIG. 4A to FIG. 4E Flow chart of the flattening process shown;
[0020] Fig. 6A shows a separation crack that starts at the edge of a stack of substrate and superstrate in one embodiment, and Figure 6B shows the alignment of a retractable pin with a substrate notch for initiating such a separation crack;
[0021] Figure 6C shows a separation crack that starts at the edge of a substrate and superstrate stack in another embodiment;
[0022] FIG. 7A to FIG. 7C shows a top view of a stack of substrate and superstrate plates as a separation crack initiates and propagates around the periphery of the stack;
[0023] Figure 8 showing a separated base plate and superstrate;
[0024] Fig. 9 As shown in Figure 7 and Figure 8 Flow chart of the separation process shown;
[0025] Fig.10 shows a separation crack initiating at an edge of a substrate and superstrate stack in yet another embodiment;
[0026] Fig.11A and Fig. 11B A multi-zone cover plate chuck in another embodiment is shown with improved zone sealing; and
[0027] Fig.12 Shows Fig.11A and Fig. 11B A magnified view of an exemplary groove structure within the area of the overlay chuck.
[0028] In all drawings, unless otherwise indicated, the same reference numerals and characters are used to represent similar features, elements, components or parts of the illustrated embodiments. In addition, although the present disclosure will now be described in detail with reference to the accompanying drawings, the present disclosure is so completed in conjunction with the illustrative exemplary embodiments. It is intended that changes and modifications may be made to the described exemplary embodiments without departing from the true scope and spirit of the present disclosure as defined by the appended claims. DETAILED DESCRIPTION
[0029] Flattening system
[0030] Figure 1 A system for planarization is shown. Planarization system 100 is used to planarize a film on substrate 102. Substrate 102 can be coupled to substrate chuck 104. Substrate chuck 104 can be, but is not limited to, a vacuum chuck, a pin chuck, a slot chuck, an electrostatic chuck, an electromagnetic chuck, and / or the like.
[0031] The substrate 102 and the substrate chuck 104 may also be supported by a substrate positioning stage 106. The substrate positioning stage 106 may be positioned along an x-axis, a y-axis, a z-axis, a θ-axis, a ψ-axis, and a One or more of the axes provide translational and / or rotational motion. The substrate positioning stage 106, substrate 102, and substrate chuck 104 may also be positioned on a pedestal (not shown). The substrate positioning stage may be part of a positioning system.
[0032] Separated from the substrate 102 is a cover plate 108 having a working surface 112 facing the substrate 102. The cover plate 108 can be formed of materials including, but not limited to, fused silica, quartz, silicon, organic polymers, siloxane polymers, borosilicate glass, fluorocarbon polymers, metals, hardened sapphire, and / or the like. In an embodiment, the cover plate is easily transparent to ultraviolet light. The surface 112 is generally of the same or slightly smaller area size than the surface of the substrate 108.
[0033] The overlay 108 may be coupled to or held by an overlay chuck 118. The overlay chuck 118 may be, but is not limited to, a vacuum chuck, a pin chuck, a slot chuck, an electrostatic chuck, an electromagnetic chuck, and / or other similar chuck types. The overlay chuck 118 may be configured to apply stress, pressure, and / or strain to the overlay 108 that varies on the overlay 108. In an embodiment, the overlay chuck is also easily transparent to ultraviolet light. The overlay chuck 118 may include systems such as a region-based vacuum chuck, an actuator array, a pressure capsule, etc., which may apply a pressure differential to the rear surface of the overlay 108 to bend and deform the template. In one embodiment, the overlay chuck 118 includes a region-based vacuum chuck that may apply a pressure differential to the rear surface of the overlay, causing the overlay to bend and deform, as described in further detail herein.
[0034] The overlay chuck 118 can be coupled to a flattening head 120, which is part of a positioning system. The flattening head 120 can be movably coupled to the bridge. The flattening head 120 can include one or more actuators, such as voice coil motors, piezoelectric motors, linear motors, nut and screw motors, etc., configured to move the flattening head 120 in at least the z-axis direction and potentially in other directions (e.g., x-axis, y-axis, θ-axis, ψ-axis, and The cover chuck 118 is moved relative to the substrate 102 on an axis.
[0035] The planarization system 100 may also include a fluid dispenser 122. The fluid dispenser 122 may also be movably connected to the bridge member. In one embodiment, the fluid dispenser 122 and the planarization head 120 share one or more of all positioning components. In an alternative embodiment, the fluid dispenser 122 and the planarization head move independently of each other. The fluid dispenser 122 can be used to deposit droplets of a liquid formable material 124 (e.g., a photocurable polymerizable material) onto the substrate 102, wherein the volume of the deposited material varies over the area of the substrate 102 at least in part based on its topographic profile. Different fluid dispensers 122 can use different techniques to dispense the formable material 124. When the formable material 124 is jettable, an inkjet-type dispenser can be used to dispense the formable material. For example, thermal inkjet, microelectromechanical system (MEMS)-based inkjet, valve jetting, and piezoelectric inkjet are common techniques for dispensing jettable liquids.
[0036] The planarization system 100 may also include a curing system including a radiation source 126 that directs actinic energy, such as ultraviolet radiation, along an exposure path 128. The planarization head 120 and the substrate positioning system 106 may be configured to position the superstrate 108 and the substrate 102 to overlap the exposure path 128. The radiation source 126 sends actinic energy along the exposure path 128 after the superstrate 108 has contacted the formable material 124. Figure 1 The exposure path 128 is shown when the cover plate 108 is not in contact with the formable material 124. This is done for illustration purposes so that the relative positions of the various components can be easily identified. Those skilled in the art will understand that when the cover plate 108 is in contact with the formable material 124, the exposure path 128 does not substantially change.
[0037] The planarization system 100 may also include a camera 136 positioned to observe the expansion of the formable material 124 as the superstrate 108 contacts the formable material 124 during the planarization process. Figure 1 The optical axis 138 of the live camera imaging field is shown. Figure 1 As shown, the planarization system 100 may include one or more optical components (dichroic mirrors, beam combiners, prisms, lenses, mirrors, etc.) that combine actinic radiation with light to be detected by the camera 136. The camera 136 may include one or more of a CCD, a sensor array, a linear camera, and a photodetector configured to collect a wavelength of light to show a contrast between areas under the superstrate 108 and in contact with the formable material 124 and areas under the superstrate 108 but not in contact with the formable material 124. The camera 136 may be configured to provide an image of the expansion of the formable material 124 under the superstrate 108, and / or an image of the separation of the superstrate 108 from the solidified formable material 124. The camera 136 may also be configured to measure interference fringes that change as the formable material 124 expands between the gap between the surface 112 and the substrate surface.
[0038] The planarization system 100 can be regulated, controlled and / or directed by one or more processors 140 (controllers) that communicate with one or more components and / or subsystems, such as the substrate chuck 104, the substrate positioning stage 106, the overlay chuck 118, the planarization head 120, the fluid dispenser 122, the radiation source 126 and / or the camera 136. The processor 140 can operate based on instructions in a computer-readable program stored in a non-transitory computer memory 142. The processor 140 can be or include one or more of a CPU, an MPU, a GPU, an ASIC, an FPGA, a DSP, and a general-purpose computer. The processor 140 can be a dedicated controller, or can be a general-purpose computing device suitable for use as a controller. Examples of non-transitory computer-readable memory include, but are not limited to, RAM, ROM, CD, DVD, Blu-ray, hard disk drives, network attached storage (NAS), intranet-connected non-transitory computer-readable storage devices, and Internet-connected non-transitory computer-readable storage devices.
[0039] In operation, the planarization head 120, the substrate positioning stage 106, or both, change the distance between the superstrate 118 and the substrate 102 to define a desired space (a bounded physical extent in three dimensions) to be filled with the formable material 124. For example, the planarization head 120 can move toward the substrate and apply a force to the superstrate 108 so that the superstrate contacts and expands a droplet of the formable material 124, as described in further detail herein.
[0040] Planarization process
[0041] The planarization process includes FIG. 2A to FIG. 2C The steps are schematically shown in FIG. Figure 2A As shown, the formable material 124 is dispensed onto the substrate 102 in the form of droplets. As previously described, the substrate surface has some topography, which can be known based on previous processing operations or can be measured using a profiler, AFM, SEM, or an optical surface profiler based on optical interference effects (such as Zygo NewView 8200). The local volume density of the deposited formable material 124 varies depending on the substrate topography. Then, the cover plate 108 is positioned to contact the formable material 124.
[0042] Figure 2BThe post-contact step is shown after the superstrate 108 has been in full contact with the formable material 124 but before the polymerization process begins. When the superstrate 108 contacts the formable material 124, the droplets merge to form a formable material film 144 that fills the space between the superstrate 108 and the substrate 102. Preferably, the filling process is performed in a uniform manner without any air or bubbles trapped between the superstrate 108 and the substrate 102, thereby minimizing non-filling defects. The polymerization process or curing of the formable material 124 can be initiated with actinic radiation (e.g., ultraviolet radiation). For example, Figure 1 The radiation source 126 can provide actinic radiation, causing the formable material film 144 to cure, harden and / or crosslink, thereby defining a cured planarization layer 146 on the substrate 102. Alternatively, the curing of the formable material film 144 can also be initiated by using heat, pressure, chemical reaction, other types of radiation, or any combination of these. Once the cured planarization layer 146 is formed, the superstrate 108 can be separated therefrom. Figure 2C A cured planarization layer 146 is shown on the substrate 102 after separation of the superstrate 108. The substrate and the cured layer may then be subjected to additional known steps and processes for device (article) fabrication, including, for example, patterning, curing, oxidation, layer formation, deposition, doping, planarization, etching, formable material removal, dicing, bonding, and packaging, etc. The substrate may be processed to produce a plurality of articles (devices).
[0043] Spread, fill and cure planarization material between superstrate and substrate
[0044] When the droplets of formable material expand, merge and fill the gap between the cover plate and the substrate, a solution for minimizing the capture of air or bubbles between the cover plate 108 and the substrate is to position the cover plate so that it makes initial contact with the formable material at the center of the substrate, and further contact then advances radially in a center-to-periphery manner. This requires deflection or bending of the cover plate or the substrate or both to produce a curvature profile in the cover plate. However, in view of the fact that the cover plate 108 generally has an area size that is the same or similar to that of the substrate 102, a useful entire cover plate bending curvature profile requires both a significant vertical deflection of the cover plate and the accompanying vertical movement performed by the cover plate chuck and the flattening assembly. For control, precision and system design considerations, this significant vertical deflection and movement may be undesirable. This cover plate profile can be obtained by, for example, applying back pressure to the inner area of the cover plate. However, in doing so, a peripheral holding area is still required to keep the cover plate on the cover plate chuck. If the peripheral edges of the cover plate and the substrate are clamped flatly during the process of the expansion and merging of the droplet of the formable material, then there is no available cover plate curvature profile in this flat clamping area. This may impair the expansion and merging of the droplet, which may also cause non-filling defects in this area. In addition, once the expansion and filling of the formable material are completed, the resulting stack of the cover plate chuck, the clamped cover plate, the formable material, the substrate and the substrate chuck can be an over-constrained system. This may result in an uneven flattening profile of the resulting planarized film layer. That is, in such an over-constrained system, all flatness errors or variations from the cover plate chuck, including the flatness of the front and back surfaces, can be transferred to the cover plate and affect the uniformity of the planarized film layer.
[0045] In order to solve the above problem, in one embodiment, Figure 3A and Figure 3B As shown, a multi-region cover plate chuck 118 is provided. The cover plate chuck 118 includes a central region 301 and a series of annular regions 303 surrounding the central region 301. The annular regions 303 can be defined as a peripheral annular region 303b surrounding the edge, periphery or periphery of the cover plate chuck 118 and a plurality of inner annular regions 303a located between the central region 301 and the peripheral annular regions 303b. The plurality of annular regions 303 can be defined by a series of ridges 307 protruding from the surface of the cover plate chuck 118. As shown in FIG. Figure 3A and Figure 3B As shown, ridges 307 may be formed around the central region 301. In each of the annular regions 303, at least one port 305 is formed for connection through the superstrate chuck 118 to allow a pressure source to apply positive or negative pressure, such as a vacuum, to the superstrate held thereby.
[0046] Figure 3B1 shows a side cross-sectional view of the cover plate chuck 118. Each ridge 307 protrudes a certain height from the surface of the cover plate chuck 118. The ridges 307 include peripheral ridges 307b surrounding the peripheral annular region 303b and a series of internal ridges 307a between the central region 301 and the peripheral annular region 303b. Figure 3B As shown, the inner ridges 307a have substantially the same height, while the height of the peripheral ridges 307b is less than the height of the inner ridges 307a. The central region 301 of the cover plate chuck 118 can be in the form of a circular cavity so that a pressure source (not shown) can apply air or gas pressure through associated channels 308 and ports 305 to deflect the central portion of the retained cover plate. Vacuum pressure can also be applied to the central region 301 through the same channels and ports. The central region 301 of the cover plate chuck 118 can be aligned with the central portion of the retained cover plate. Similarly, the peripheral annular region 303a can be aligned with the periphery or periphery of the retained cover plate. The surrounding annular region 303 is also provided with corresponding channels 308 and ports 305 for applying pressure or vacuum.
[0047] Go to FIG. 4A to FIG. 4E , depicting a process for contacting, expanding, and merging droplets of deposited formable material 124. Figure 4A As shown, before the cover plate 108 contacts the formable material 124, a positive pressure (indicated by arrow P) is applied to the retained cover plate 108 through the port 305 of the central region 301 of the cover plate chuck 118 to deflect the central portion of the cover plate 108 toward the formable material 124. The pressure P is applied to the central region 301 to control the initial deflection within a predetermined range and maintain a predetermined curvature of the cover plate 108, as shown in FIG. Figure 4A At the same time, negative pressure, preferably vacuum (indicated by arrow V), is applied to the cover plate 108 through the port 305 in the annular region 303 to hold the cover plate 108 with the cover plate chuck 118. Figure 4B As shown, the superstrate 108 is then brought into initial contact with the droplet of formable material 124 .
[0048] Then, by sequentially releasing the vacuum (V) from the inner annular region 303a proximate to the central region 301, the deflection of the superstrate 108 extends from the central portion in a radially outward direction. In this manner, the droplets of formable material contact, expand, and merge to form a film layer having a fluid front that advances radially outward as the superstrate contacts and conforms to the substrate. The pressure P applied through the central region 301 is maintained at a desired value while the vacuum is sequentially released from the inner annular region 303a. The pressure P may also be applied to the superstrate 108 through the channels 308 and ports 305 in the inner annular region 303a from which the vacuum has been released. In Figure 4CIn the illustrated embodiment, the vacuum has been sequentially released from the three inner rings 303a closest to the inner region 301, and as the vacuum has been sequentially released, pressure P is sequentially applied. During this sequential vacuum release and pressurization process, the planarization head may also move downward.
[0049] The deflection of the cover plate 108 then continues in a radial direction until the vacuum is released from all of the inner annular regions 303a while maintaining the vacuum V applied via the outer annular region 303b. For each of the inner annular regions 303a, once the vacuum is released, a pressure P is also applied. Figure 4D As shown, when the vacuum has been released from all of the inner annular regions 303a, the superstrate 108 deflects to conform to the substrate 102, except for the periphery of the substrate 108 which continues to be held by the superstrate chuck 118 via the vacuum V applied through the peripheral regions 303b. In this manner, the edge of the superstrate 108 is maintained in a deflected, curved state for eventual expansion and merging of droplets of formable material dispensed at the periphery of the substrate 102. In addition, the peripheral ridges 307b, which are lower relative to the inner ridges 307a, help maintain this curvature.
[0050] exist Figure 4E , the vacuum applied through the peripheral annular region 303b is then released so as to completely release the superstrate 108 from the superstrate chuck 118. This provides a number of advantages. First, by releasing the periphery of the superstrate 108 from the peripheral annular region 303b that has been held in a curved state, the expansion and merging of the remaining droplets of formable material can be completed in the same center-to-periphery radial manner, thereby continuing to minimize air or gas capture and the resulting non-filling defects. Specifically, the peripheral ridge 307b that is recessed relative to the internal ridge 307a allows the superstrate 108 to maintain a desired curvature before release. Second, by completely releasing the superstrate 108 from the superstrate chuck 118, any over-constraint of the superstrate 108 caused by the clamped state is eliminated, thereby reducing local non-uniform flattening that may occur due to such a constrained condition. Third, releasing the superstrate 108 from the superstrate chuck 118 eliminates any chuck non-flatness errors or variations from being transmitted to the superstrate 108, which also reduces local non-uniform flattening variations.
[0051] Once the cover plate 108 is released, curing energy can be applied to cure the formable material to form a planarized layer. As previously described, the curing source can be a light beam for curing the formable material 124. In one embodiment, the size of the light beam can be adjusted or controlled with reference to the diameter of the cover plate. The light beam can also be controlled to be incident on the substrate at a predetermined angle. During curing, the lateral position of the substrate 102 relative to the curing source (i.e., in the XY plane) can be adjusted. After the curing process, the cover plate 108 is re-held by the cover plate chuck 118, and then the cover plate 108 is separated from the substrate, as further described herein.
[0052] Figure 5 A flow chart of a planarization process as shown in FIGS. 3 and 4 is shown. In step 501, a droplet of formable material 124 is dispensed onto the substrate 102. In step S502, a central region of the superstrate 108 is deflected toward the droplet of formable material 124. Then, in step S503, the deflected superstrate 108 is advanced by the superstrate chuck 118 to contact the formable material 124. In step S504, the deflection of the superstrate 108 extends from the central region of the superstrate 108 toward the periphery. Then, in step S506, the superstrate 108 is held by the superstrate chuck 118 (e.g., by a vacuum applied to the periphery of the superstrate 108) to stop applying force (e.g., by a vacuum applied to the periphery of the superstrate 108) to hold the superstrate 108, so that the superstrate 108 is released (i.e., unclamped) from the superstrate chuck 118. In step S507, the formable material 124 is cured. After curing, the superstrate 108 is re-held by the superstrate chuck 118 to separate the superstrate 108 from the cured formable material 146.
[0053] When using, for example, a UV curable material as the formable material 124, it is desirable that the overlay chuck 118 be transparent, have high UV light transmittance to facilitate UV curing (as well as high light transmittance for imaging, such as by Figure 1 Camera 136 shown). As described above, as shown in Figures 3 and 4, pneumatic supply channel 308 and port 305, area 303 and ridge 307 are integrated into the cover plate. These structures may cause problems for UV curing. Specifically, the UV transmittance in the area below ridge 307 and channel 308 can be significantly reduced compared to areas without such features, resulting in insufficient or uneven curing of the formable material. This phenomenon is sometimes referred to as the "shadow effect". The shadow effect may be particularly evident at the edges of ridge 307. In addition, when the cover plate 100 is clamped to the ridge 307, there will be a thin air gap because the two surfaces are not optically in contact with each other. This type of thin gap can sometimes completely block UV rays. This phenomenon is called the "thin film effect" between the ridge and the cover plate.
[0054] One solution to the "shadow effect" described above involves movement of the stack of the cover plate and substrate on the wafer stage in the x, y, and / or theta coordinates after the cover plate is unclamped (i.e., released) from the cover plate chuck. By moving the wafer stage in this manner during UV exposure, areas of the cover plate and substrate that would otherwise remain under the channels, ports, and ridges can be periodically moved to areas under the cover plate chuck where the chuck features are not present. The required relative motion can be estimated from equation (1) below:
[0055]
[0056] Among them, I mis the expected average intensity within the range of motion, I h is the high intensity (i.e., the maximum or “biggest” intensity) within the featureless region of the chuck, I l is the intensity at the object feature (i.e., the lowest value or “low” intensity), and w h Is to achieve I m The estimated range of motion, w l is the object feature width (e.g., the width of a ridge, port, or channel). For example, assuming 100% UV transmittance in a featureless region, and assuming the desired I m is 90% of this value, and further assuming that w i =1mm, then according to equation (1), the expected relative motion range w h =8.0mm. Alternatively, the UV light source can be moved by tilting or tilting the UV light source relative to the cover plate chuck to change the angle of the UV light incident on the cover plate chuck, which can also reduce shadow effects near object features. The "thin film effect" can be avoided by relative movement in the z-axis direction to create sufficient clearance between the cover plate and the cover plate chuck, for example, by loosening the cover plate and moving the wafer stage away from the cover plate chuck in the z-axis direction. The various solutions described above can be applied individually or in combination to improve the uniformity of the total UV dose in certain areas and minimize shadows and thin film effects. In various embodiments, the applied UV beam can be smaller than, the same size as, or larger than the substrate or cover plate. In one embodiment, the applied UV beam can be larger than the substrate by a certain size that accommodates the above-mentioned relative movement w h , while continuing to expose the entire substrate to UV light.
[0057] Separating the superstrate from the cured planarization film
[0058] Once the formable material is solidified and a planarized film layer is formed, the superstrate needs to be removed or released from the formed layer. However, when the superstrate and the substrate have the same or similar area sizes, it is difficult to initiate and propagate a separation crack between the superstrate and the formed layer, which is necessary to completely separate the superstrate from the formed layer. Figure 8 The structure and method shown in the figure solve this problem. Fig. 6A and Figure 6B As shown, the substrate chuck 604 includes retractable pins 606 located on the periphery of the chuck that can be aligned with notches 608 on the substrate 102. Such notches (e.g., wafer notches) are common for semiconductor wafers and are used to orient the wafer during processing and handling. In operation, the retractable pins 606 are positioned to align with the notches 608 located on the substrate 102. To cause separation, the pins 606 move upward through the notches 608 and contact a point 610 on the edge of the cover plate 108, as shown in FIG. Fig. 6AAs shown. The force applied by the pin 606 is sufficient to initiate a separation crack 601 between the superstrate 108 and the solidified layer 146 on the substrate 102. Once the crack 601 is created, the edge of the superstrate 108 is deflected toward the superstrate chuck 118 by applying vacuum pressure through the port 305 of the superstrate chuck 118. This is achieved by making the ridge 307b of the superstrate chuck 118 shorter than the adjacent ridge 307a, which provides space for the edge of the superstrate 108 to deflect away from the substrate 102 toward the superstrate chuck 118. The force applied to create the crack 601 may depend on the geometric and physical conditions of the superstrate, the planarization film layer, and the substrate. Alternatively, as Figure 6C As shown, the crack 601 can be generated by introducing a positive pressure between the substrate 102 and the cover plate 108. Here, the substrate chuck 614 includes a nozzle 616 connected to a positive fluid pressure source (not shown). When the nozzle 616 is activated, the positive fluid pressure P I The fluid pressure is delivered to a point 610 at the edge of the superstrate 118 by a nozzle 616 to initiate a separation crack 601 with sufficient force. The positive fluid pressure may include a flow of clean dry air, helium, or nitrogen. When the crack 601 is generated, the superstrate 102 is held in the superstrate chuck 118 and the substrate 102 is held by the substrate chuck 104.
[0059] Figure 7 to Figure 8 The progress of the separation is shown. Fig. 7A A top view of the cover plate 118 is shown in full contact with the shaping layer on the substrate (as shown by the shaded area). Figure 7B 6. As described above, a separation crack 601 has been induced. Once the crack 601 is induced, a high flow of negative pressure or vacuum is applied to the outer annular region 303b of the superstrate chuck 118 so as to engage the edge of the superstrate 108 and expand the separation crack 601 around the outer annular region 303b. This expansion proceeds circumferentially in both directions from the notch 608, as indicated by arrows C. To assist in the expansion of the crack 601 around the outer annular region 303b, additional lateral gas flow (not shown) may be provided between the substrate 102 and the superstrate 108 as the crack expansion proceeds. Figure 7C The crack 601 is shown fully extended around the outer annular region 303b.
[0060] Once the separation crack has fully propagated around the outer annular region, an upward motion may be applied along the Z-axis direction of the cover plate 108 to complete the separation of the cover plate 108 from the solidified layer on the substrate. Figure 8The cover plate 108 is shown completely separated from the substrate 102. At the completion of the separation, the significant upward movement of the cover plate 108 relative to the substrate 102 may cause shear stresses in the remaining contact area between the cover plate 108 and the substrate 102. Alternatively, the Z-direction movement may be stopped at an earlier desired position, and the separation may be advanced and ended by continuing to apply vacuum pressure to the inner and / or central annular regions. Such shear stresses may be minimized by applying vacuum to one or more inner annular regions 303a and / or the central region 301 during the continuous separation process.
[0061] Fig. 9 As shown in Figure 7 and Figure 8 Flow chart of the separation process shown. In step S901, a separation crack is induced between the cover plate 108 and the solidified layer. Then, in step S902, the separation crack is extended around the periphery of the cover plate 108. In step S903, the remaining portion of the cover plate is separated from the solidified layer. In the embodiments discussed above, the separation of the cover plate 108 and the substrate 102 includes the steps of generating the crack by mechanical force such as a pin or air pressure, applying vacuum pressure to the outer area to extend the crack, firmly holding the cover plate 108, and moving the cover plate 108 upward and away from the substrate 102 in the Z direction with sufficient safety to avoid the force of loosening the cover plate upward, and applying vacuum to the center of the cover plate 108 during the upward movement in the Z direction to complete the separation. Optionally or in combination with the above-mentioned Z-direction movement scheme, the expansion of the separation can also be affected by continuously applying an in-plane (or lateral) directional flow with high pressure from one or more sides of the substrate (not shown).
[0062] In the embodiment of FIG. 6, by means of a mechanical pin 606 ( Fig. 6A ) or fluid nozzle 616 ( Figure 6B ) exerts an upward force through the wafer notch 608 to initiate a crack. Fig.10 Another embodiment of a substrate chuck configured to induce a separation crack is shown. Here, the substrate chuck 624 includes a separate retractable pin 626 that can induce a separation crack when the cover plate 108 and the substrate are arranged non-concentrically. This non-concentric arrangement causes a portion 628 of the cover plate 108 to be suspended above the substrate 102. The crack 602 can be generated by applying a force to the suspended portion 110 through the movement of the pin 626. Optionally, the suspended portion 608 can also be obtained by using a cover plate that is slightly larger than the substrate. In this way, the cover plate 108 can still be arranged concentrically with the substrate 102. In either case, the substrate chuck 624 can also include a mechanical pin or nozzle, such as in Fig. 6A or Figure 6B As in the embodiment of or otherwise, the mechanical pins or nozzles are spaced apart from the pin 626 to create multiple points around the circumference of the sheathing for initiating separation cracks.
[0063] Clamp plate chuck
[0064] As described above, the superstrate 108 is preferably held or supported by a superstrate chuck 118 that applies pressure or vacuum (negative pressure) to the volume between the superstrate and the chuck surface within the annular region 303 defined by the ridges 307 extending from the chuck surface. Except for the outermost ridges 307a, the inner ridges 307b are preferably of the same height so that the depth of the gap between adjacent inner ridges 307b remains constant. The ridge height (i.e., the depth of the gap) is typically kept very small, for example, on the order of tens to thousands of microns, for reasons such as minimizing gas filling or emptying response time, ridge stiffness characteristics, limiting thermal effects (such as expansion or contraction), etc. In operation, when a vacuum is applied to the annular region to hold the superstrate against the ridges of the region, a vacuum seal is created at the superstrate-ridge interface. However, when sufficient force or pressure is applied to the superstrate in the opposite direction of the chuck vacuum, the substrate can be lifted off the ridges of the chuck. At a certain gap between the cover plate and the ridge, the vacuum seal fails or leaks, causing the vacuum pressure in this area to decrease or even become zero. The cover plate may then inadvertently loosen from the chuck. Furthermore, even if the cover plate does not become loose, vacuum leaks can undermine the desired level of control, for example, when the cover plate is in the chuck of FIG4 and FIG5. Figure 5 When the vacuum pressure in the adjacent annular areas is released sequentially during the process. Figure 5 During the process of , such leakage at the outer ridges can also negatively affect the controlled maintenance of the desired outer edge curvature of the cladding. Fig. 9 During the process, leakage from the external ridges can disrupt the initiation and propagation of separation cracks.
[0065] To deal with this undesirable leakage, Fig.11A and 11B As shown, a cover plate chuck 1118 is provided, which includes a groove structure 1109. Similar to the cover plate chuck 118, the cover plate chuck 1118 also includes a plurality of ridges 307, which can be defined as a series of internal ridges 307a and peripheral ridges 307b protruding from the surface 1119 of the cover plate chuck 1118. Fig. 11B and Fig.12As shown, surface 1119 is a holding or fixing surface for holding or fixing cover plate 108. A series of inner regions 303a are defined by ridges 307a. In at least one of the annular regions 303, grooves 1109 are formed that are recessed from the surface of chuck 1118. The grooves may be concentric and located between corresponding ridges of the annular regions. Grooves 1109a formed in the inner annular region 303a are located at a position away from the center of chuck 1118 relative to the width of the associated inner annular region. In contrast, grooves 1109b formed in the peripheral annular region 303b are located at an area close to the center of substrate chuck 1118 relative to the width of the outer annular region. That is, grooves 1109a formed in the inner annular region 303a are formed at the outer diameter of the corresponding inner annular region 303a, while grooves 1109b formed in the peripheral annular region 303b are formed at the inner diameter of the peripheral region 303b.
[0066] In operation, the grooves 1109 act as a buffer that provides a uniform source of high vacuum pressure that continues to act on the superstrate even in the presence of gaps between the superstrate at ridges distal to the grooves. In this manner, the sequential radial release of the vacuum and the application of positive pressure to the central region and adjacent annular regions can be performed in a controlled manner. That is, the vacuum pressure applied in a given annular region can be maintained even if a positive pressure is applied to the adjacent inner region in an amount that can deflect the superstrate to a sufficient level to create a gap at the distal ridge. In other words, the provision of the grooves 1109 enables some leakage to be tolerated without disrupting the intended process. Similarly, grooves 1109b located in the peripheral annular region having a smaller outer ridge height are used so as to maintain sufficient vacuum pressure in the outer annular region even in the presence of small gaps at the outer ridges. This enables the outer periphery of the superstrate to be maintained at the desired curvature for the final expansion and merging of the deposited droplets of formable material (see Figure 4D ) and the initiation and propagation of separation cracks (see, e.g., FIG6 ), even in the presence of some leakage.
[0067] Fig.12 is an enlarged cross-sectional view of an exemplary groove structure 1109b. The specific groove dimensions and relative positions within the annular region required to achieve the desired vacuum buffer performance depend on the cover plate chuck ridge height and annular region width. Fig.12In the example shown, groove 1109b is located within annular region 303b and is recessed from the chuck surface. In this example, the height h1 of outer ridge 307b is less than the height h2 of inner ridge 307a. In typical use, the difference in ridge height can be in the range of about 5 microns to about 50 microns. Annular region 303b has a width d. Groove 1109b is positioned such that the first edge is at a distance d1 from ridge 307b, and the second edge is at a distance d2 from ridge 307a. Groove 1109b has a depth h3 and a width d3. In this embodiment, the relationship between these parameters satisfies the following condition:
[0068] h1 <h2
[0069] h3>10h2
[0070] d3<0.5d
[0071] d1>d2+d3.
[0072] The port 305 that connects the groove 1109b to a pressure source (not shown) intersects the groove or is located within the groove. If the port does not intersect the groove, the necessary high pressure cannot be maintained and the groove will be ineffective. In the above embodiment, the outer ridge h1 is where the leak is expected to occur. For the inner annular groove 1109b, the ridge heights can be the same, i.e., h1=h2. In this case, the distance d1 is measured from the specified ridge (i.e., h1 or h2) where the leak is expected to occur. For example, in Fig.11A and Fig. 11B In the embodiment of the present invention, the inner annular region 303a includes grooves 1109a that are located closer to the outer ridges of their respective annular regions (measured radially from the center of the chuck) to mitigate leakage from the inner ridges during sequential vacuum release and subsequent pressurization of the annular regions, as shown in Figures 4 to 5. Figure 5 The associated process is described in.
[0073] In view of this description, further modifications and alternative embodiments of various aspects will be apparent to those skilled in the art. Therefore, this description should be interpreted as being illustrative only. It should be understood that the forms shown and described herein will be considered as examples of embodiments. Elements and materials may replace the elements and materials illustrated and described herein, parts and processes may be reversed, and certain features may be utilized independently, all of which will be apparent to those skilled in the art after having benefited from this specification.
Claims
1. A method comprising: retaining a cladding plate with a cladding plate chuck, the cladding plate chuck comprising a central region aligned with a central portion of the cladding plate and a series of annular regions including a peripheral annular region aligned with a periphery of the cladding plate and one or more inner annular regions between the central region and the peripheral annular region; applying pressure to deflect the cover plate toward the substrate to gradually extend, the deflection of the cover plate being in a radial direction, further comprising: applying pressure through the central region and maintaining the vacuum applied through the series of annular regions; After the central portion of the cladding plate has been deflected by pressure, sequentially releasing vacuum from the inner annular region and sequentially applying pressure in a radial direction through the inner annular region; and releasing vacuum from the peripheral annular region; and The cover plate is released from the cover plate chuck.
2. The method according to claim 1, further comprising: dispensing a contact portion of formable material on said substrate; contacting the cover plate with a formable material contact portion; as well as Pressure is applied to the cover plate corresponding to the flow front of the contact portion of the formable material.
3. The method of claim 2, wherein the formable material contact portion is dispensed as a plurality of droplets deposited on the substrate.
4. The method of claim 1, wherein pressure is applied to the central region to control the initial height within a determined range and maintain a predetermined curvature of the cladding panel.
5. The method according to claim 1, further comprising: solidifying the formable material contact portion after releasing the cover sheet from the cover sheet chuck; During curing, moving the lateral position of the cover sheet relative to a curing source; re-holding the cover plate with the cover plate chuck; and The superstrate is separated from the contacting portion of the solidified formable material.
6. A multi-zone chuck system comprising: a substrate chuck for holding a substrate; a cladding plate chuck for holding a cladding plate, the cladding plate chuck comprising a central region aligned with a central portion of the cladding plate, a peripheral annular region aligned with a periphery of the cladding plate, and one or more inner annular regions between the central region and the peripheral annular region; as well as a pressure source configured to apply pressure and vacuum to the superstrate via a plurality of ports of the superstrate chuck, wherein The pressure source is configured to sequentially apply pressure to a plurality of regions of the cladding plate through ports in the inner annular region so that the cladding plate gradually deflects in a radial direction from one region to another toward the substrate, and The vacuum applied to the perimeter of the superstrate is maintained while the superstrate is deflected by the pressure.
7. The multi-zone chuck system of claim 6, wherein the central region of the superstrate chuck includes an air cavity that is aligned with the center of the superstrate while the superstrate is in contact with the formable material.
8. The multi-zone chuck system of claim 6, further comprising a formable material dispenser configured to dispense a plurality of droplets of the formable material onto the substrate, wherein: The superstrate chuck is configured to advance the superstrate to bring the superstrate into contact with the formable material on the substrate; and The pressure source is configured to sequentially apply pressure to areas corresponding to a flow front of the formable material.
9. The multi-zone chuck system of claim 8, further comprising a curing source configured to cure the formable material after the superstrate is released from the superstrate chuck.
10. The multi-zone chuck system of claim 9, wherein the substrate chuck is configured to move a lateral position of the substrate relative to the curing source.
11. The multi-zone chuck system of claim 9, wherein the curing source is configured to control a size of a beam with reference to a diameter of the superstrate during curing.
12. The multi-zone chuck system of claim 9, wherein the curing source is configured to control a tilt angle of a light beam incident on the cover plate.
13. A method for forming a layer, comprising: dispensing a formable material onto a substrate; holding a cover sheet with a chuck and advancing the cover sheet through the chuck into contact with the formable material, the chuck comprising a central region aligned with a central portion of the cover sheet, a peripheral annular region aligned with a periphery of the cover sheet, and one or more inner annular regions between the central region and the peripheral annular region; sequentially applying pressure to a plurality of regions of the cladding plate through the inner annular region so that the cladding plate gradually deflects in a radial direction from one region to another toward the substrate; sequentially releasing the vacuum applied to the one region while applying pressure to the other region; continuously applying a vacuum to a perimeter of the cover plate while deflecting the cover plate by pressure; releasing the cover plate from the chuck; as well as The formable material behind the chuck is cured with a curing source.
14. The method of claim 13, further comprising moving a lateral position of the substrate relative to the curing source during curing.
15. The method of claim 13, further comprising controlling a size of a beam of the curing source with reference to a diameter of the superstrate.
16. The method of claim 13, further comprising controlling a tilt angle of the light beam incident on the cover plate.