A method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature

By oxidation and cracking reaction of low-molecular-weight perfluoropolyether waste with oxidation medium gas at high temperatures, high-value small-molecular-weight acyl fluoride is generated, which solves the problem of difficult waste utilization and achieves efficient resource recycling and environmental protection benefits.

CN114149318BActive Publication Date: 2024-11-05ZHEJIANG NOAH FLUOROCHEMICAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111261696.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-28
Publication Date
2024-11-05
Estimated Expiration
2041-10-28

AI Technical Summary

Technical Problem

The low-molecular weight perfluoropolyether waste in the prior art is difficult to utilize, resulting in waste of resources and environmental pollution. The high-temperature cracking technology has problems such as complex by-products and difficult separation.

Method used

Low molecular weight perfluoropolyether waste is used to undergo oxidation cracking reaction with the oxidation medium gas at high temperature to generate small molecular weight acyl fluoride, and the selectivity and utilization rate of the target product are improved by controlling the reaction conditions and structural design.

Benefits of technology

It has achieved the generation of high-value acyl fluoride gas, has market value, promoted green chemical industry and environmental protection, and improved the utilization efficiency and diversified utilization of raw materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003325681430000011
    Figure BDA0003325681430000011
  • Figure BDA0003325681430000021
    Figure BDA0003325681430000021
  • Figure BDA0003325681430000022
    Figure BDA0003325681430000022
Patent Text Reader

Abstract

The invention discloses a method for synthesizing low-molecular-weight acyl fluoride by oxidative cracking of a low-molecular-weight perfluoropolyether waste at high temperature, it uses low-molecular-weight perfluoropolyether waste as raw material, and oxidative cracking reaction occurs at high temperature with oxidizing medium gas, the long carbon chain of polymer is cracked to generate the acyl fluoride of low molecular weight (C1~C4), reaction temperature is 400~700 DEG C, reaction residence time is 10 200s, oxidizing medium is oxygen or ozone, and product is controllably cracked into high-value products such as carbonyl fluoride, perfluoroacetyl fluoride, perfluoropropionyl fluoride and perfluorobutyryl fluoride. The method of the present invention can obtain high-value acyl fluoride gas by thermal cracking, can be applied to the fields such as electronic industry cleaning agent, etching agent, pesticide intermediate, fluorine-containing material monomer, further can effectively utilize low-molecular-weight perfluoropolyether waste, realize the circulation of green chemical industry, reduce environmental damage.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of fluorine chemical industry, and in particular to a method for synthesizing low-molecular-weight acyl fluoride by oxidative cracking of low-molecular-weight perfluoropolyether waste at high temperature. Background Art

[0002] The "shielding" effect of the CF bond in the perfluoropolyether molecule on the main chain makes it very chemically inert, non-flammable, anti-oxidant, anti-corrosive and radiation-resistant. Its thermal stability, lubricity and insulation are significantly better than those of hydrocarbon polyethers. As a lubricant, only perfluoropolyether has an operating temperature range of -100 to 400°C, and there is almost no shear thinning phenomenon. Even at very high shear rates, it still maintains a certain viscosity and always maintains low volatility. Because its molecules do not contain chlorine, it is used in high-load bearings and will not corrode the bearings due to pressure. These characteristics make perfluoropolyether widely used as a lubricant for computer hard disks, which minimizes the wear and friction of the probe and disk surfaces.

[0003] The type of perfluoropolyether depends on the monomer used for polymerization. According to the different monomers and polymerization methods, there are currently four main types of perfluoropolyether products, namely Z, Y, K and D types. The first two are photocatalytic polymerization products, and the latter two are anionic polymerization products.

[0004] The synthesis method of the Z and Y types produced by the Italian Osmont Company is as follows:

[0005] Type Z: A linear polymer formed by photooxidation of tetrafluoroethylene under the action of ultraviolet light. Its structural formula is CF3O-(CF2CF2O) m -(CF2O) n -CF3, the average molecular weight of the product is 10 3 -10 5 between:

[0006]

[0007] Type Y: Hexafluoropropylene is oxidized by ultraviolet light to form perfluoropolyether, with the structural formula CF3O-(C3F6O-) m (-CF2O-) n The average molecular weight of CF3, Y type is generally around 10 3 ~10 4 between:

[0008]

[0009] Type K: Hexafluoropropylene oxide is polymerized under the catalysis of F- ions and then fluorinated to form a perfluoropolyether with a CF3- side chain, the structural formula of which is CF3CF2CF2O (CF(CF3)CF2O) m CF2CF3

[0010]

[0011] Type D: A polymer obtained by polymerization of tetrafluoroethylene oxide and direct fluorination of the product, with the structural formula C3F7O (CF2CF2CF2O) m C2F5.

[0012] Due to the excellent viscosity-temperature performance, low volatility, good extreme pressure, chemical indifference to oxidants, and insolubility in liquid fuels of perfluoropolyether, it can be used for lubrication and sealing of gear pumps, pressure gauges, metal joints, and threaded fasteners in liquid fuel and oxidant systems in liquid fuel rocket engines. Patent CN103145971A reports the synthesis of perfluoropolyether by hexafluoropropylene oxide and alkali metal fluoride in aprotic solvents to prepare perfluoropolyether products with higher molecular weight. Patent CN105906795 mentions the method and application of synthesizing perfluoropolyether oil, but the patent also mentions that the synthesis method disclosed in the prior art needs to use metal hydrides to remove impurities from the hexafluoropropylene oxide raw materials, which has the problems of low conversion rate and low average molecular weight of the product. That is, a large amount of low molecular weight waste will be generated, and these wastes are difficult to meet industrial needs, and at the same time, they will cause process interference and a large amount of waste in the stabilization process.

[0013] Table a

[0014]

[0015] According to the physical properties of PFPE products in Table a above, it can be seen that when used as PFPE lubricants and other applications, no matter what type, molecular weight requirements are required, and there is no corresponding use for low molecular weight products. The molecular weight is low and the boiling point is also low, which easily leads to the product failing to meet customer needs and having no available market prospects. Therefore, no matter which company's products are, low molecular weight perfluoropolyether oils are treated as waste, but due to the excellent performance of perfluoropolyether, which has corrosion resistance, radiation resistance, thermal stability and insulation, it is difficult to handle such waste. Random discarding and filling will greatly cause environmental pollution, which is not conducive to green chemical industry.

[0016] High temperature pyrolysis is a new technology for waste treatment developed in recent years. In the early 1990s, scientists discovered that burning organic matter would generate toxic substances - dioxins. Therefore, as a new way of waste treatment, this technology is generally favored by all countries. It is considered to be a new way to recycle, harmlessly treat and reduce waste. All countries have invested a lot of manpower and material resources in research and development, and have achieved good results.

[0017] Pyrolysis is a process that utilizes the thermal instability of organic matter in garbage to heat it, causing it to crack, and then condense to form various new gases, liquids and solids, from which products are extracted. The pyrolysis yield depends on the chemical structure and physical form of the raw materials and the temperature and speed of pyrolysis. Under high temperature and high speed heating conditions, the molecular structure of organic matter undergoes comprehensive cracking. The temperature at which the entire pyrolysis process starts is different for different organic matter compositions. Different temperature ranges carry out different reaction processes, and the composition of the products is also different.

[0018] Patent CN109534972 Method for preparing perfluoropentanone by cracking hexafluoropropylene dimer, specifically relates to a method for preparing perfluoropentanone by cracking hexafluoropropylene dimer. The preparation method comprises: hexafluoropropylene dimer enters an oxidation furnace and undergoes cracking reaction with oxygen under the condition of a first catalyst; the cracking product is separated to obtain perfluoroacetyl fluoride. The patent realizes the cracking of perfluoroolefin compounds under the condition of oxygen and high temperature to generate perfluoroacyl fluoride.

[0019] Patent CN109607507A introduces a method for preparing carbonyl fluoride by cracking perfluoro compounds and carbonyl fluoride. The patent introduces the high temperature cracking effect of perfluoroolefin C=C, perfluoroacyl fluoride-COF compound and perfluorocarbonyl fluoride-C(O)-. The above patents are all about the cracking of small molecules, the purpose of which is to obtain the target product, and a catalyst is required. In actual use, it does not have much versatility and practical environmental significance.

[0020] Patent CN101462925 - A method for generating tetrafluoroethylene by cracking polytetrafluoroethylene, the patent adopts an oxygen-free environment and a catalyst to crack tetrafluoroethylene, thereby realizing the recovery of raw materials and the treatment of waste plastics. However, this method is prone to generate perfluoroisobutylene during the thermal cracking process, which is colorless, odorless and highly toxic, and has great health damage to operators.

[0021] Patent CN109734070 - a method for cracking waste PTFE into carbonyl fluoride, also involves washing waste polytetrafluoroethylene, cutting it into small particles of 100 microns, and then thermally cracking it. However, the simplest, most commonly used, and least expensive method for recovering PTFE is mechanical crushing, which uses mechanical force to chemically change the waste material to obtain a relatively small powder, which is then mixed with other PTFE materials and reused. In comparison, high-temperature cracking does not have much advantage, and the by-products obtained need further purification and are difficult to separate.

[0022] Patent 106031876 - Catalyst for preparing isobutylene by ether cracking and its preparation method, using ether as cracking raw material to obtain isobutylene. This method does not need to add other catalysts that are harmful to the environment, and the reaction temperature is relatively low, but the actual use of this method is relatively poor, there are many types of catalysts, and the price of rare earth oxides is high, and the product obtained is methanol, which has no economic value and poor practicality.

[0023] In addition, in the high-temperature cracking technology of the prior art, the main purpose is usually just to crack the raw materials, and the components of the obtained cracking gas are usually relatively complex, making it difficult to obtain a cracking gas product with high economic value. Summary of the invention

[0024] In view of the above technical problems existing in the prior art, the object of the present invention is to provide a method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature. Through the method of the present invention, different experimental conditions can be adopted for reaction according to different perfluoropolyether waste structures, thereby improving the selectivity of the target product and improving the utilization rate of the raw materials.

[0025] The method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature is characterized in that the low molecular weight perfluoropolyether waste is an oligomer containing one or more polymer fragments of polymer fragment 1, polymer fragment 2, polymer fragment 3 and polymer fragment 4 in its molecular structure, and its molecular weight is below 1500; the low molecular weight perfluoropolyether waste is used as a raw material, and an oxidative cracking reaction is carried out with an oxidizing medium gas at a high temperature, and the reaction formula of the polymer fragment in the raw material molecule and the oxidizing medium gas includes at least one of the following:

[0026]

[0027] The main product generated by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature is low molecular weight acyl fluoride, including at least one of perfluoropropionyl fluoride shown in formula (5), perfluoroacetyl fluoride shown in formula (6), and carbonyl fluoride shown in formula (7).

[0028] The main chain of the perfluoropolyether is an ether chain composed of at least one repeating unit structure of -CF2O-, -CF2CF2O-, -CF2CF2CF2O- or -CF(CF3)CF2O-. In the polymer molecular structure of the low molecular weight perfluoropolyether waste of the present application, the short group at one end of the polymer chain is CF3O-, C2F5O- or C3F7O-, and the short group at the other end of the polymer chain is CF3-, C2F5- or C3F7-.

[0029] Furthermore, the low molecular weight perfluoropolyether waste is specifically at least one of the following raw materials:

[0030] Z-type perfluoropolyether CF3O-(CF2CF2O) m -(CF2O) n -CF3;

[0031] Y-type perfluoropolyether CF3O-(C3F6O) m -(CF2O) n -CF3;

[0032] K-type perfluoropolyether CF3CF2CF2 (OCF3CFCF2) m CF2CF3;

[0033] D-type perfluoropolyether C3F7O(CF2CF2CF2O) m C2F5;

[0034] Among them, the molecular weight of low molecular weight perfluoropolyether waste is below 1500 and the boiling point is within 250°C.

[0035] In this reaction, the CO bond of the perfluoropolyether is broken and oxidized by high temperature and oxidation conditions to generate -COF, where different products are obtained according to different polyether repeating units. For example, after the -CF2CF2CF2O- and -CF(CF3)CF2O- structures are broken, perfluoropropionyl fluoride can generally be obtained. The -CF2O- and -CF2CF2O- structures mainly obtain carbonyl fluoride and perfluoroacetyl fluoride. Polyethers of different configurations have multiple repeating units and can obtain more than two acyl fluoride products.

[0036] In the present application, the main products generated by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature are four components: perfluoropropionyl fluoride, perfluoroacetyl fluoride, carbonyl fluoride and perfluorobutyryl fluoride. The total volume fraction of these four components in the cracking gas is more than 80%, preferably more than 90%.

[0037] The method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature is characterized in that the specific reaction process is: firstly, the low molecular weight perfluoropolyether waste is introduced into a vaporization chamber for preheating and vaporization, the vaporized raw material and the oxidizing medium gas are introduced into a reactor together for high temperature oxidative cracking reaction, the cracked gas after the reaction is discharged from the gas outlet of the reactor and collected by a gas collecting device; wherein the main products generated by the reaction are four components of perfluoropropionyl fluoride, perfluoroacetyl fluoride, carbonyl fluoride and perfluorobutyryl fluoride, and the oxidizing medium gas is oxygen or ozone.

[0038] Furthermore, the preheating vaporization temperature is 180-300°C, preferably 200-220°C.

[0039] The material of the reactor is stainless steel 304, stainless steel 316L, carbon steel, nickel or copper. The material of the reactor is preferably stainless steel 304 or stainless steel 316L. Although nickel tubes have better effects and are not easy to be blocked by dust accumulation, they are too expensive and the cost performance of the material is relatively low.

[0040] The oxidizing medium used is oxygen or ozone, preferably oxygen, which has low toxicity, better safety performance and low price.

[0041] When oxygen is used as the oxidizing medium gas, the ratio of the volume flow rate of oxygen to the mass flow rate of the perfluoropolyether raw material is 2.5 to 30:1, preferably 7.5 to 15:1, the unit of the volume flow rate is ml / min, and the unit of the mass flow rate is g / min.

[0042] When ozone is selected as the oxidizing medium gas, the ratio of the volume flow rate of ozone to the mass flow rate of the perfluoropolyether raw material is 1:0.4-3, preferably 1:0.8-1, the unit of the volume flow rate is ml / min, and the unit of the mass flow rate is g / min.

[0043] Furthermore, the temperature of the high-temperature oxidative cracking reaction is 400-700°C, preferably 500-700°C; when the vaporized raw material and the oxidizing medium gas are introduced into the reactor together for reaction, the residence reaction time is 10s-200s, preferably 40-200s.

[0044] Furthermore, the cracking gas is also detected and analyzed during the reaction process, and the specific process is: the cracking gas is introduced into an absorption liquid for absorption, and the absorption liquid can be alcohols such as methanol, ethanol, and propanol, but because methanol has better reaction activity and reacts faster with acyl fluorides, the absorption liquid is preferably methanol. The amines in the absorption liquid are used to neutralize the HF generated by the reaction of acyl fluorides and alcohols, and the purpose is to remove acid. Therefore, the absorption liquid is a methanol solution containing amine compounds, and the four components of perfluoropropionyl fluoride, perfluoroacetyl fluoride, carbonyl fluoride and perfluorobutyryl fluoride in the cracking gas all react with methanol to generate corresponding ester compounds and HF by-products, and the amine compounds in the methanol solution are used to neutralize the HF by-products, and finally form a sample detection liquid, which is then detected and analyzed by gas chromatography.

[0045] Based on the raw material structure of low molecular weight perfluoropolyether waste, different acyl fluorides can be obtained by reaction in a reactor and an oxidizing medium. However, since acyl fluorides are corrosive and highly active, they easily react with moisture in the air, and the proportion and content cannot be directly determined by gas chromatography. Therefore, after being absorbed by methanol and reacting with it to generate products such as dimethyl carbonate, methyl perfluoroacetate, methyl perfluoropropionate and methyl perfluorobutyrate, they are then detected by gas chromatography, making all types of products non-corrosive and all of them pass standard calibration. The reaction of acyl fluorides with methanol is shown in the following formula:

[0046]

[0047] It can be seen that by detecting and analyzing the contents of products such as dimethyl carbonate, methyl perfluoroacetate, methyl perfluoropropionate and methyl perfluorobutyrate, the contents of the corresponding acyl fluoride raw materials can be deduced, and the cracking gas generated by the reaction can be indirectly analyzed in this way.

[0048] The content of amine compounds in the methanol solution should achieve the following absorption effect: after the amine compounds in the methanol solution neutralize the HF byproducts generated by absorption, the pH of the mixed solution is neutral or weakly alkaline, that is, in the range of pH=7-9.

[0049] Compared with the prior art, the present invention has the following beneficial effects:

[0050] 1. The present invention can effectively utilize low molecular weight perfluoropolyether waste. The acyl fluoride products after the low molecular weight perfluoropolyether waste is cracked with the oxidizing medium gas, i.e., C1-C4 small molecule acyl fluoride, can be divided into carbonyl fluoride, perfluoroacetyl fluoride, perfluoropropionyl fluoride and perfluorobutyryl fluoride according to the number of perfluoroalkyl groups in the carbon chain. Carbonyl fluoride (COF2), also known as carbon-based fluoride, fluorophosgene, can be used as cleaning gas and etching gas for semiconductor manufacturing equipment, fluorination gas and raw materials of organic compounds, and intermediates and fluorinating agents for organic synthesis. As a cleaning gas for semiconductor manufacturing equipment, high-purity COF2 is required, which can replace traditional PFC, has excellent effect and less environmental burden. Perfluoroacetyl fluoride and perfluoropropionyl fluoride are important fluorine-containing compounds, which are widely used and can be used as cleaning agents, etching agents, pesticide intermediates, fluorine-containing material monomers, etc. in the electronics industry. Perfluorobutyryl fluoride can generally be used to synthesize perfluorobutyric acid, methyl perfluorobutyrate and synthesize specific fluorine-containing intermediates. The current preparation methods of perfluorobutyryl fluoride mainly include chemical synthesis and electrolysis. Thermal cracking can effectively reuse low molecular weight polyethers, reuse previous waste materials, and crack them to generate acyl fluoride products with market value, which can not only achieve green chemical industry and environmental protection, but also have economic value, and realize efficient and diversified utilization of raw materials.

[0051] The method of the invention can effectively utilize low molecular weight perfluoropolyether waste, realize the cycle of green chemical industry and reduce environmental damage.

[0052] 2. The present invention uses thermal cracking to obtain high-value acyl fluoride gas, which can be used in cleaning agents, etching agents, pesticide intermediates, fluorine-containing material monomers, etc. in the electronics industry.

[0053] 3. The process design of the present invention is novel, the conditions are controllable, the operation is simple and safe, the device and equipment used are simple, and industrial production can be quickly realized. DETAILED DESCRIPTION

[0054] The present invention will be further described below in conjunction with specific embodiments, but the protection scope of the present invention is not limited thereto.

[0055] The raw materials used in the specific implementation method are partly from common commodities on the market. After the cracking gas is absorbed by the absorption liquid, the main detection means used are gas chromatography and mass spectrometry. Unless otherwise specified, the reactor is made of stainless steel 304 and the oxidizing medium is oxygen. In the embodiment of the present application, the structural formula of the perfluoropolyether waste is one of the following:

[0056] Z-type perfluoropolyether CF3O-(CF2CF2O) m -(CF2O) n -CF3;

[0057] Y-type perfluoropolyether CF3O-(C3F6O) m -(CF2O) n -CF3;

[0058] K-type perfluoropolyether CF3CF2CF2 (OCF3CFCF2) m CF2CF3;

[0059] D-type perfluoropolyether C3F7O(CF2CF2CF2O) m C2F5.

[0060] Embodiment 1:

[0061] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber for preheating and vaporization through a peristaltic pump. The flow rate was controlled by a flow controller to be 4g / min, and the temperature of the vaporization chamber was 200°C. The vaporized K-type perfluoropolyether raw material and oxygen (oxygen flow rate 30mL / min) were introduced into the reactor for high-temperature oxidation cracking reaction. The temperature of the reactor was controlled to be 500°C. The reaction residence time of the K-type perfluoropolyether raw material and oxygen in the reactor was 44s. After the reaction, the cracking gas flow was precooled to below 80°C and then introduced into the absorption liquid (the absorption liquid was a mixture of methanol and triethylamine) to absorb and form a sample detection liquid. The excess gas (including excess oxygen) insoluble in the absorption liquid was collected by the air bag. After the reaction, the absorption liquid gained 1.19kg and the air bag gained 0.11kg. The substances in the absorption liquid and the air bag were analyzed by gas quality, and the calculated reaction results are shown in Table 1.

[0062] Acyl fluoride products can react with methanol, while other products cannot react with methanol. Therefore, acyl fluoride products can be absorbed by methanol absorption liquid and gain weight. Therefore, we calculate the yield by differential weight method. In this embodiment 1, 1.3 kg of raw materials, the liquid absorbed by methanol gained weight by 1.19 kg, and other gases were collected by air bags with 0.11 kg. We believe that the weight gain of methanol absorption liquid is the weight of acyl fluoride products.

[0063] In Table 1, the yield of acyl fluoride products = the mass of methanol absorption liquid absorbed 1.19kg / the mass of raw materials 1.3kg * 100%. The yield of other products = the mass of air bag absorbed 0.11kg / the mass of raw materials 1.3kg * 100%. During the high-temperature oxidative cracking reaction, the total mass of oxygen introduced is small, which is almost negligible compared to the K-type perfluoropolyether raw material. Due to operational errors and slight air leakage in the air bag, the calculated result of the total yield in Table 1 may be less than 100% in the experiment. Therefore, the pyrolysis effect of this application is mainly evaluated by the yield of acyl fluoride products.

[0064] Table 1

[0065]

[0066] In Table 1, the acyl fluoride products refer to four components: perfluorobutyryl fluoride, perfluoropropionyl fluoride, perfluoroacetyl fluoride and carbonyl fluoride, and the molar ratios of perfluorobutyryl fluoride, perfluoropropionyl fluoride, perfluoroacetyl fluoride and carbonyl fluoride are 2.8%, 64%, 9.1% and 24.1% respectively.

[0067] In the following examples, the ratios of acyl fluoride products all refer to molar ratios, and the yield calculation formula of acyl fluoride products refers to the method in Example 1.

[0068] Embodiment 2:

[0069] 1.3kg Z-type perfluoropolyether (average molecular weight of 1000) was pumped into the vaporization chamber for preheating and vaporization through a peristaltic pump. The flow rate was controlled by a flow controller to be 4g / min, and the temperature of the vaporization chamber was 200°C. The vaporized Z-type perfluoropolyether raw material and oxygen (oxygen flow rate 30mL / min) were introduced into the reactor for high-temperature oxidation cracking reaction. The temperature of the reactor was controlled to be 500°C. The reaction residence time of the Z-type perfluoropolyether raw material and oxygen in the reactor was 44s. After the reaction, the cracking gas flow was precooled to below 80°C and then introduced into the absorption liquid (the absorption liquid was a mixture of methanol and triethylamine) to absorb and form a sample detection liquid. The excess gas that was not absorbed and was insoluble in the absorption liquid was collected with an air bag. After the reaction, the absorption liquid gained 1.205kg and the air bag gained 0.08kg. The gas quality analysis of the substances in the absorption liquid and the air bag was performed respectively, and the calculated reaction results are shown in Table 2.

[0070] Table 2

[0071]

[0072] Embodiment 3:

[0073] 1.3kg of D-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber for preheating and vaporization by a peristaltic pump. The flow rate was controlled by a flow controller to be 4g / min, and the temperature of the vaporization chamber was 200°C. The vaporized D-type perfluoropolyether raw material and oxygen (oxygen flow rate 30mL / min) were introduced into the reactor for high-temperature oxidation cracking reaction. The temperature of the reactor was controlled to be 500°C. The reaction residence time of the D-type perfluoropolyether raw material and oxygen in the reactor was 44s. After the reaction, the cracking gas flow was precooled to below 80°C and then introduced into the absorption liquid (the absorption liquid was a mixture of methanol and triethylamine) to absorb and form a sample detection liquid. The excess gas that was not absorbed and was insoluble in the absorption liquid was collected with an air bag. After the reaction, the absorption liquid gained 1.201kg and the air bag gained 0.095kg. The gas quality analysis of the substances in the absorption liquid and the air bag was performed respectively, and the calculated reaction results are shown in Table 3.

[0074] Table 3

[0075]

[0076] Embodiment 4:

[0077] 1.3kg Y-type perfluoropolyether (average molecular weight of 1000) was pumped into the vaporization chamber for preheating and vaporization by a peristaltic pump. The flow rate was controlled by a flow controller to be 4g / min, and the temperature of the vaporization chamber was 200°C. The vaporized Y-type perfluoropolyether raw material and oxygen (oxygen flow rate 30mL / min) were introduced into the reactor for high-temperature oxidation cracking reaction. The temperature of the reactor was controlled to be 500°C. The reaction residence time of the Y-type perfluoropolyether raw material and oxygen in the reactor was 44s. After the cracking gas flow was precooled to below 80°C, it was introduced into the absorption liquid (the absorption liquid was a mixture of methanol and triethylamine) to absorb and form a sample detection liquid. The excess gas that was not absorbed and was insoluble in the absorption liquid was collected by an air bag. After the reaction, the absorption liquid gained 1.210kg and the air bag gained 0.088kg. The substances in the absorption liquid and the air bag were analyzed by gas quality, and the calculated reaction results are shown in Table 4.

[0078] Table 4

[0079]

[0080] According to the experimental results of Examples 1-4, it can be seen that different perfluoropolyether structures can obtain different proportions of acyl fluoride products under the same cracking conditions (the gas phase volume ratio results of each component in the product acyl fluoride products are summarized in Table 5 using different perfluoropolyether types as raw materials), and different raw materials can be selected according to the needs of the target product.

[0081] Table 5

[0082] Perfluoropolyether type Perfluorobutyryl fluoride Perfluoropropionyl fluoride Perfluoroacetyl fluoride Carbonyl fluoride K-Type 2.8% 64% 9.1% 24.1% Z-Type 0.2% 1.5% 42.3% 56% Type D 2.4% 56% 9.9% 26.2% Y-Type 1.7% 19.2% 8.1% 72%

[0083] (The conditions in Table 5 above are pyrolysis temperature 500°C, residence time 44s, oxygen rate 30mL / min)

[0084] Embodiment 5:

[0085] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber for preheating and vaporization through a peristaltic pump. The flow rate was controlled by a flow controller at 1g / min, and the temperature of the vaporization chamber was 200°C. The vaporized K-type perfluoropolyether raw material and oxygen (oxygen flow rate 30mL / min) were introduced into the reactor for high-temperature oxidation cracking reaction. The temperature of the reactor was controlled at 500°C. The reaction residence time of the K-type perfluoropolyether raw material and oxygen in the reactor was 176s. After the reaction, the cracking gas flow was precooled to below 80°C and then introduced into the absorption liquid (the absorption liquid was a mixture of methanol and triethylamine) to absorb and form a sample detection liquid. The excess gas that was not absorbed and was insoluble in the absorption liquid was collected with an air bag. After the reaction, the absorption liquid gained 1.249kg and the air bag gained 0.050kg. The substances in the absorption liquid and the air bag were analyzed by gas quality, and the calculated reaction results are shown in Table 6.

[0086] Table 6

[0087]

[0088] Embodiment 6:

[0089] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber for preheating and vaporization through a peristaltic pump. The flow rate was controlled by a flow controller to be 8g / min, and the temperature of the vaporization chamber was 200°C. The vaporized K-type perfluoropolyether raw material and oxygen (oxygen flow rate 30mL / min) were introduced into the reactor for high-temperature oxidation and cracking reaction. The reactor temperature was controlled to be 500°C, and the reaction residence time was 22s. After the reaction, the gas flow was precooled to below 80°C and then introduced into a mixed solution of methanol and triethylamine for absorption. The excess gas that was not absorbed was collected with an air bag. After the reaction, the absorption liquid gained 1.11kg and the air bag gained 0.19kg. The substances in the absorption liquid and the air bag were analyzed by gas quality, and the calculated reaction results are shown in Table 7.

[0090] Table 7

[0091]

[0092] It can be seen from the experimental results of Examples 1, 5 and 6 that increasing the space velocity of the raw material and changing the residence time of the cracking can also change the yield and gas phase ratio of the product (the experimental results of Examples 1, 5 and 6 are summarized in Table 8).

[0093] Table 8

[0094]

[0095] Embodiment 7:

[0096] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber for preheating and vaporization by a peristaltic pump. The flow rate was controlled by a flow controller to be 4g / min, and the temperature of the vaporization chamber was 200°C. The vaporized K-type perfluoropolyether raw material and oxygen (oxygen flow rate 30mL / min) were introduced into the reactor for high-temperature oxidation cracking reaction. The temperature of the reactor was controlled to be 700°C. The reaction residence time of the K-type perfluoropolyether raw material and oxygen in the reactor was 44s. After the cracking gas flow was precooled to below 80°C, it was introduced into the absorption liquid (the absorption liquid was a mixture of methanol and triethylamine) to absorb and form a sample detection liquid. The excess gas that was not absorbed and was insoluble in the absorption liquid was collected with an air bag. After the reaction, the absorption liquid gained 1.250kg and the air bag gained 0.051kg. The substances in the absorption liquid and the air bag were analyzed by gas quality, and the calculated reaction results are shown in Table 9.

[0097] Table 9

[0098]

[0099] Embodiment 8:

[0100] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber for preheating and vaporization by a peristaltic pump. The flow rate was controlled by a flow controller to be 4g / min, and the temperature of the vaporization chamber was 200°C. The vaporized K-type perfluoropolyether raw material and oxygen (oxygen flow rate 30mL / min) were introduced into the reactor for high-temperature oxidation cracking reaction. The temperature of the reactor was controlled to be 400°C. The reaction residence time of the K-type perfluoropolyether raw material and oxygen in the reactor was 44s. The cracked gas flow after the reaction was precooled to below 80°C and then introduced into the absorption liquid (the absorption liquid was a mixture of methanol and triethylamine) to absorb and form a sample detection liquid. The excess gas that was not absorbed and was insoluble in the absorption liquid was collected with an air bag. After the reaction, the absorption liquid gained 1.050kg and the air bag gained 0.250kg. The substances in the absorption liquid and the air bag were analyzed by gas quality, and the calculated reaction results are shown in Table 10.

[0101] Table 10

[0102]

[0103] According to the above experiments, different temperatures will also affect the experimental results. This may be because too high a temperature will promote the breakage of CC, resulting in the formation of short-chain acyl fluoride products (the experimental results of Examples 1, 7 and 8 are summarized in Table 11).

[0104] Table 11

[0105]

[0106] Embodiment 9:

[0107] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber through a peristaltic pump for preheating and vaporization. The flow rate was controlled by a flow controller at 4g / min, and the temperature of the vaporization chamber was 200°C. The vaporized raw materials were introduced into the reactor together with oxygen at a flow rate of 60mL / min for reaction. The temperature of the reactor was controlled at 500°C, and the reaction residence time was 44s. After the reaction, the gas flow was precooled to below 80°C and then introduced into a mixed solution of methanol and triethylamine for absorption. The excess gas that was not absorbed was collected with an air bag. After the reaction, the absorption liquid gained 1.23kg and the air bag gained 0.07kg. The gas quality analysis of the substances in the absorption liquid and the air bag was performed respectively, and the calculated reaction results are shown in Table 12.

[0108] Table 12

[0109]

[0110] Embodiment 10:

[0111] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber through a peristaltic pump for preheating and vaporization. The flow rate was controlled by a flow controller at 4g / min, and the temperature of the vaporization chamber was 200°C. The vaporized raw materials and oxygen were introduced into the reactor for reaction. The oxygen was 10mL / min, the temperature of the reactor was controlled at 500°C, and the reaction residence time was 44s. After the reaction, the gas flow was precooled to below 80°C and then introduced into a mixture of methanol and triethylamine for absorption. The excess gas that was not absorbed was collected with an air bag. After the reaction, the absorption liquid gained 0.89kg and the air bag gained 0.41kg. The gas quality analysis of the substances in the absorption liquid and the air bag was performed respectively, and the calculated reaction results are shown in Table 13.

[0112] Table 13

[0113]

[0114] The increase in the amount of oxygen can effectively increase the bond breaking of CO. The lack of oxygen will lead to the formation of C=C and the generation of various olefins, and the by-products will increase.

[0115] Embodiment 11:

[0116] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber through a peristaltic pump for preheating and vaporization. The flow rate was controlled at 4g / min by a flow controller. The vaporized raw materials and oxygen were introduced into the reactor for reaction. The oxygen was 30mL / min, the temperature of the vaporization chamber was 200°C, the temperature of the reactor was controlled at 500°C, and the reaction residence time was 44s. After the reaction, the gas flow was precooled to below 80°C and then introduced into a mixture of methanol and triethylamine for absorption. The excess gas that was not absorbed was collected with an air bag. The material of the reactor was a nickel tube. After the reaction, the absorption liquid gained 1.24kg and the air bag gained 0.059kg. The gas quality analysis of the substances in the absorption liquid and the air bag was performed respectively, and the calculated reaction results are shown in Table 14.

[0117] Table 14

[0118]

[0119] The cracking effect of nickel tubes is not much different from that of stainless steel tubes, but the material is not easy to be blocked by carbon accumulation, and the service life is longer. However, the price of nickel tubes is relatively more expensive.

[0120] Embodiment 12:

[0121] 1.3kg of K-type perfluoropolyether (average molecular weight of 1100) was pumped into the vaporization chamber through a peristaltic pump for preheating and vaporization. The flow rate was controlled at 4g / min by a flow controller. The vaporized raw materials were introduced into the reactor together with ozone for reaction. The ozone was 5mL / min, the temperature of the vaporization chamber was 200°C, the temperature of the reactor was controlled at 500°C, and the reaction residence time was 44s. After the reaction, the gas flow was precooled to below 80°C and then introduced into a mixture of methanol and triethylamine for absorption. The excess gas that was not absorbed was collected with an air bag. After the reaction, the absorption liquid gained 1.14kg and the air bag gained 0.16kg. The gas quality analysis of the substances in the absorption liquid and the air bag was performed respectively, and the calculated reaction results are shown in Table 15.

[0122] Table 15

[0123]

[0124] Compared with oxygen, ozone has stronger oxidizing properties and higher efficiency, and only requires a smaller amount to be effective. However, ozone is toxic, more expensive, and has an impact on the environment. Therefore, the oxidizing medium is preferably oxygen.

[0125] Comparative Example 1:

[0126] 1.3kg of K-type perfluoropolyether (average molecular weight of 5000) was pumped into the preheating tube by a peristaltic pump for preheating (preheating temperature of 300°C), and the flow rate was controlled by a flow controller to be 4g / min. The raw materials preheated at 300°C were introduced into the reactor together with oxygen (oxygen flow rate of 10mL / min) for reaction. The reactor was heated to the cracking temperature, and the perfluoropolyether raw materials were vaporized and cracked in the reactor. The reaction residence time was 44s. The gas flowing out of the reactor was precooled to below 80°C, and the raw materials that were not fully reacted were condensed and collected (recorded as undecomposed raw materials). The precooled gas was introduced into a mixed solution of methanol and triethylamine for absorption, and the excess gas that was not absorbed was collected with an air bag.

[0127] Using the above operation process, when the cracking temperature of the reactor was changed to 500℃, 700℃ and 1000℃, the gas quality analysis of the absorption liquid and the substances in the gas bag was carried out respectively, and the calculated reaction results are shown in Table 16.

[0128] Table 16 Pyrolysis results of K-type perfluoropolyether with molecular weight of 5000 at different temperatures

[0129]

[0130] Comparative Example 2:

[0131] 1.3kg of K-type perfluoropolyether (average molecular weight of 5000) was pumped into the preheating tube by a peristaltic pump for preheating (preheating temperature of 300°C), and the flow rate was controlled by a flow controller to 4g / min. The raw materials preheated at 300°C were introduced into the reactor together with oxygen for reaction. The reactor was heated to a cracking temperature of 1000°C, and the perfluoropolyether raw materials were vaporized and cracked in the reactor. The reaction residence time was 44s. The gas flowing out of the reactor was precooled to below 80°C, and the raw materials that were not fully reacted were condensed and collected (recorded as undecomposed raw materials). The precooled gas was introduced into a mixed solution of methanol and triethylamine for absorption, and the excess gas that was not absorbed was collected with an air bag.

[0132] Using the above operation process, the oxygen flow rate was changed to 10mL / min, 50mL / min, and 100mL / min, and the gas quality analysis of the absorption liquid and the substances in the air bag was performed respectively. The calculated reaction results are shown in Table 17.

[0133] Table 17 Pyrolysis results of K-type perfluoropolyether with molecular weight of 5000 at different temperatures

[0134]

[0135] High molecular weight perfluoropolyether has better stability and higher boiling point. It is difficult to completely crack it when used as a cracking raw material. There are still some high molecular weight raw materials that cannot be cracked, which limits the efficiency of use. Secondly, high molecular weight polyether oil has high economic value, and it does not have the concept of economic appreciation and green recycling for the synthesis of perfluoroacyl fluoride.

[0136] The contents described in this specification are merely an enumeration of implementation forms of the inventive concept, and the protection scope of the present invention should not be regarded as being limited to the specific forms described in the embodiments.

Claims

1. A method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature, characterized in that The low molecular weight perfluoropolyether waste is specifically at least one of the following raw materials: Z-type perfluoropolyether CF3O-(CF2CF2O) m -(CF2O) n -CF3; Y-type all-carbon fluoride CF3O-(C3F6O) m -(CF2O) n -CF3; K-type perfluoropolyether CF3CF2CF2O (CF(CF3)CF2O) m CF2CF3; D-type perfluoropolyether C3F7O(CF2CF2CF2O) m C2F5; Among them, the molecular weight of low molecular weight perfluoropolyether waste is below 1500 and the boiling point is within 250°C; The specific reaction process is as follows: firstly, low molecular weight perfluoropolyether waste is introduced into a vaporization chamber for preheating and vaporization, and the vaporized raw material and oxidizing medium gas are introduced into a reactor together for high temperature oxidation cracking reaction, and the cracking gas after the reaction is discharged from the gas outlet of the reactor and collected by a gas collecting device; wherein, the main products generated by the reaction are four components: perfluoropropionyl fluoride, perfluoroacetyl fluoride, carbonyl fluoride and perfluorobutyryl fluoride; When the oxidizing medium gas is oxygen, the ratio of the volume flow rate of oxygen to the mass flow rate of the perfluoropolyether raw material is 7.5 to 15:1, the unit of the volume flow rate is ml / min, and the unit of the mass flow rate is g / min; When the oxidizing medium gas is ozone, the ratio of the volume flow rate of ozone to the mass flow rate of the perfluoropolyether raw material is 1:0.8-1, the unit of the volume flow rate is ml / min, and the unit of the mass flow rate is g / min; The temperature of the high-temperature oxidation cracking reaction is 500-700° C. When the vaporized raw material and the oxidizing medium gas are introduced into the reaction furnace for reaction, the residence reaction time is 40-200 seconds.

2. A method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature as claimed in claim 1, characterized in that The main products generated by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature are four components: perfluoropropionyl fluoride, perfluoroacetyl fluoride, carbonyl fluoride and perfluorobutyryl fluoride. The total volume fraction of the four components in the cracking gas is more than 80%.

3. A method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature as claimed in claim 2, characterized in that The total volume fraction of the four components in the cracked gas is more than 90%.

4. A method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature as claimed in claim 1, characterized in that The preheating vaporization temperature is 180-300°C; the reaction furnace is made of stainless steel 304, stainless steel 316L, carbon steel, nickel or copper.

5. A method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature as claimed in claim 4, characterized in that The preheating vaporization temperature is 200-220°C.

6. A method for synthesizing low molecular weight acyl fluoride by oxidative cracking of low molecular weight perfluoropolyether waste at high temperature as claimed in claim 1, characterized in that During the reaction, the cracking gas is also detected and analyzed. The specific process is: the cracking gas is introduced into an absorption liquid for absorption, and the absorption liquid is a methanol solution containing amine compounds. The four components of perfluoropropionyl fluoride, perfluoroacetyl fluoride, carbonyl fluoride and perfluorobutyryl fluoride in the cracking gas react with methanol to generate corresponding ester compounds and HF by-products. The amine compounds in the methanol solution are used to neutralize the HF by-products to finally form a sample detection liquid, which is then detected and analyzed by gas chromatography.