Semiconductor device and method for manufacturing the same

By forming the active area and trench isolation structure on the semiconductor substrate, and filling it with an inversion polysilicon layer and a buried word line structure, the leakage current problem of MOS devices under the DRAM process node is solved and the device performance is improved. and reliability.

CN114267640BActive Publication Date: 2024-10-25CHANGXIN MEMORY TECH INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010973871.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-09-16
Publication Date
2024-10-25
Estimated Expiration
2040-09-16

AI Technical Summary

Technical Problem

As the DRAM process node reaches 20nm and below, MOS devices have serious problems with substrate leakage current and gate-induced drain leakage (GIDL) current, causing word line transistor switching characteristics to drift and device performance and reliability to decline.

Method used

The active area and trench isolation structure are formed on the semiconductor substrate, filled with an inversion polysilicon layer, and a buried word line structure is formed within it. Leakage is reduced through the gate oxide layer, gate barrier layer and insulating filling layer. current.

Benefits of technology

Effectively reduce leakage current, improve the turn-on speed and performance of transistors, reduce GIDL current, and enhance device reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114267640B_ABST
    Figure CN114267640B_ABST
Patent Text Reader

Abstract

The invention discloses a semiconductor device and a method for preparing the same, the method comprising: providing a semiconductor substrate, wherein an active region and a trench isolation structure located between the active regions are formed in the semiconductor substrate; forming a first groove in the active region; filling the first groove with an inverted polysilicon layer that is doped inversely to the active region; forming a second groove, wherein the second groove penetrates the polysilicon layer and a portion of the semiconductor substrate, and a portion of the inverted polysilicon layer located on the side of the second groove is retained; and forming a buried word line structure in the second groove. The method for preparing a semiconductor device according to an embodiment of the present invention can reduce the GIDL current of the semiconductor device and improve the performance and reliability of the semiconductor device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for preparing the same. Background Art

[0002] Dynamic Random Access Memory (DRAM) is a semiconductor device commonly used in electronic devices such as computers, including a memory cell array for storing data and a peripheral circuit located outside the memory cell array. Each memory cell usually includes a transistor (word line), a bit line and a capacitor. The word line voltage on the transistor (word line) can control the opening and closing of the transistor, so that the data information stored in the capacitor can be read through the bit line, or the data information can be written into the capacitor.

[0003] With the continuous development of process technology, the size of transistors is getting smaller, and the channel electric field strength of MOS devices is constantly increasing. As the process node of DRAM reaches 20nm and below, the substrate leakage current and gate-induced drain leakage (GIDL) current problems of MOS devices are becoming more and more serious, which will cause the switching characteristics of word line transistors to drift, and the performance and reliability of devices will be seriously reduced. Summary of the invention

[0004] The object of the present invention is to provide a method for preparing a semiconductor device, wherein the semiconductor device prepared by the method can reduce leakage current and improve performance.

[0005] In order to solve the above technical problems, the present invention provides a method for preparing a semiconductor device, comprising: providing a semiconductor substrate, wherein an active area and a trench isolation structure located between the active areas are formed in the semiconductor substrate; forming a first groove in the active area; filling the first groove with an inverted polysilicon layer that is doped in an anti-type manner to the active area; forming a second groove, wherein the second groove passes through the polysilicon layer and a portion of the semiconductor substrate, and retains a portion of the inverted polysilicon layer located on the side of the second groove; and forming a buried word line structure in the second groove.

[0006] According to some embodiments of the present invention, before the step of forming the first groove in the active area, the following steps are included: forming a patterned mask layer on the surface of the semiconductor substrate.

[0007] According to some embodiments of the present invention, the depth of the first groove is 20nm-150nm, and the width of the first groove is 30nm-100nm.

[0008] According to some embodiments of the present invention, the depth of the second groove is 50nm-300nm, and the width of the second groove is 20nm-50nm.

[0009] According to some embodiments of the present invention, the formation of the buried word line structure includes: forming a gate oxide layer on the surface of the second groove; forming a gate barrier layer on the surface of the gate oxide layer, the gate barrier layer covering the bottom surface and part of the side surface of the gate oxide layer; forming a gate conductive layer on the surface of the gate barrier layer, the gate conductive layer filling part of the second groove; forming an insulating filling layer on the gate barrier layer and the gate conductive layer, the insulating filling layer filling the remaining second groove.

[0010] Optionally, the steps of forming a gate barrier layer and forming a gate conductive layer include: forming a primary barrier layer on the surface of the gate oxide layer; forming a primary conductive layer on the surface of the primary barrier layer and filling the second groove; removing part of the primary conductive layer and the primary barrier layer, and retaining part of the primary conductive layer and the primary barrier layer located in the bottom area of ​​the second groove to form the gate barrier layer and the gate conductive layer.

[0011] Optionally, in the step of removing part of the primary conductive layer and the primary barrier layer, the height of the removed part of the primary conductive layer and the primary barrier layer is 20 nm-150 nm.

[0012] Optionally, upper surfaces of the gate conductive layer and the gate barrier layer are flush, and the upper surface of the gate barrier layer is not lower than a lower surface of a portion of the inverted polysilicon layer located on a side of the second groove.

[0013] The present invention also provides a semiconductor device.

[0014] A semiconductor device according to an embodiment of the present invention includes: a semiconductor substrate, the semiconductor substrate being provided with an active area and a trench isolation structure located between the active areas; a buried word line structure, the buried word line structure being located in the active area; and an inverted polysilicon layer, the inverted polysilicon layer being located on a side of the buried word line structure and being inversely doped with the active area.

[0015] According to some embodiments of the present invention, the buried word line structure includes: a gate oxide layer, a gate barrier layer, a gate conductive layer and an insulating filling layer, the gate barrier layer is located on the surface of the gate conductive layer, the insulating filling layer is located above the gate conductive layer and the gate barrier layer, and the gate oxide layer is located on the surface of the gate barrier layer and the insulating filling layer.

[0016] Optionally, an upper surface of the gate barrier layer is flush with an upper surface of the gate conductive layer and is not lower than a lower surface of the inversion polysilicon layer.

[0017] Optionally, the upper surface of the inversion polysilicon layer is flush with the upper surface of the gate oxide layer, the thickness of the inversion polysilicon layer is 5nm-25nm, and the height of the inversion polysilicon layer is 20nm-150nm.

[0018] Optionally, the gate barrier layer has a thickness of 2nm-7nm. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 A schematic diagram of a process for preparing a semiconductor device according to an embodiment of the present invention;

[0020] Figure 2-Figure 10 Schematic cross-sectional views of various steps of a method for manufacturing a semiconductor device according to an embodiment of the present invention.

[0021] Reference numerals:

[0022] 100: semiconductor devices;

[0023] 1: semiconductor substrate, 11: trench isolation structure, 12: active area;

[0024] 21: gate oxide layer, 22: gate barrier layer, 23: gate conductive layer, 24: insulating filling layer, 25: initial conductive layer, 26: primary barrier layer;

[0025] 3: inverted polysilicon layer, 31: first groove, 32: second groove;

[0026] 4: Mask layer. DETAILED DESCRIPTION

[0027] A method for preparing a semiconductor device according to the present invention will be further described in detail below in conjunction with the accompanying drawings and specific embodiments.

[0028] A method for manufacturing a semiconductor device 100 according to an embodiment of the present invention will be described below with reference to the accompanying drawings.

[0029] like Figure 1 As shown, a method for preparing a semiconductor device 100 according to an embodiment of the present invention may include providing a semiconductor substrate 1, in which an active area 12 and a trench isolation structure 11 located between the active areas 12 are formed; forming a first groove 31 in the active area 12; filling the first groove 31 with an inverted polysilicon layer 3 that is doped in an anti-type manner to the active area 12; forming a second groove 32, wherein the second groove 32 penetrates the polysilicon layer and a portion of the semiconductor substrate 1, and retains a portion of the inverted polysilicon layer 3 located on the side of the second groove 32; and forming a buried word line structure in the second groove 32.

[0030] like Figure 2-Figure 101 is a cross-sectional view of each step of a method for manufacturing a semiconductor device 100 according to an embodiment of the present invention.

[0031] like Figure 2 As shown, a semiconductor substrate 1 is provided. The material of the semiconductor substrate 1 can be silicon (Si), germanium (Ge), silicon germanium (GeSi), or silicon carbide (SiC); it can also be silicon on insulator (SOI), germanium on insulator (GOI); or it can also be other materials, such as III-V group compounds such as gallium arsenide.

[0032] The semiconductor substrate 1 has a trench isolation structure 11, and the trench isolation structure 11 isolates a plurality of active regions 12 in the semiconductor substrate 1, wherein the trench isolation structure 11 may include a trench and an insulating material filled in the trench, and the insulating layer material may be silicon dioxide, etc. The active region 12 may be doped with ions to form a P-type active region or an N-type active region through ion implantation or diffusion process, and the active region 12 forms an active region and a drain region, and the source region and the drain region are doped inversely to the active region 12. For example, if the active region 12 is formed as a P-type active region 12, the source region and the drain region are N-type doped, and if the active region 12 is formed as an N-type active region 12, the source region and the drain region are P-type doped.

[0033] like Figure 3 As shown, a first groove 31 is formed in the active area 12. Before forming the first groove 31, a patterned mask layer 4 may be formed on the surface of the semiconductor substrate 1. The active area 12 of the semiconductor substrate 1 is patterned by the mask layer 4 to form the first groove 31 in the active area 12. The first groove 31 may be multiple, for example, Figure 2 As shown, two first grooves 31 may be formed. As for the mask layer 4, the material of the mask layer 4 may be silicon nitride, and the method of forming the mask layer 4 may be chemical vapor deposition, etc., but is not limited thereto.

[0034] Alternatively, if Figure 3 As shown, the depth of the first groove 31 may be 20nm-150nm, and the width of the first groove 31 may be 30nm-100nm, that is, the width of the first groove 31 may be D1, and the depth of the first groove 31 may be H1, then D1 satisfies 30nm≤D1≤100nm, and H1 satisfies 20nm≤H1≤150nm.

[0035] like Figure 4As shown, an inverted polysilicon layer 3 with an anti-type doping to the active area 12 is filled in the first groove 31. Specifically, a polysilicon layer filling the first groove 31 is formed on the surface of the semiconductor substrate 1, and the polysilicon layer is ion-doped to form an inverted polysilicon layer 3, wherein the ion doping of the inverted polysilicon layer 3 is anti-type to the ion doping of the active area 12. For example, if the active area 12 is formed as a P-type active area 12, the inverted polysilicon layer 3 is doped with N-type ions, such as arsenic or antimony; if the active area 12 is formed as an N-type active area 12, the inverted polysilicon layer 3 is doped with P-type ions, such as boron or indium. Then, the inverted polysilicon layer 3 on the upper surface of the mask layer 4 is removed, and the inverted polysilicon layer 3 located in the first groove 31 is retained.

[0036] like Figure 5 As shown, a second groove 32 is formed, and the second groove 32 penetrates the inverted polysilicon layer 3 and a portion of the semiconductor substrate 1, and a portion of the inverted polysilicon layer 3 located on the side of the second groove 32 is retained. The depth of the second groove 32 is 50nm-300nm, and the width of the second groove 32 is 20nm-50nm, that is, Figure 5 As shown, the width of the second groove 32 may be D2, and the depth of the second groove 32 may be H2, then D2 satisfies 20nm≤D2≤50nm, and H2 satisfies 50nm≤H2≤300nm.

[0037] Specifically, the second groove 32 is formed in the first groove 31, by etching the inverted polysilicon layer 3, and continuing to etch the semiconductor substrate 1 downward in a direction perpendicular to the semiconductor substrate 1 to form the second groove 32, the depth of the second groove 32 is greater than the first groove 31, and the width of the second groove 32 is less than the first groove 31, so that the sidewall of the second groove 32 is formed by part of the inverted polysilicon layer 3 and part of the semiconductor substrate 1, as shown in FIG. Figure 5 The inverted polysilicon layer 3 is formed on the upper portion of the second groove 32 .

[0038] like Figure 6-Figure 10 As shown, a buried word line structure is formed in the second groove 32, wherein the buried word line structure is formed in the lower part of the second groove 32, and the inverted polysilicon layer 3 is formed in the upper part of the second groove 32 and is located on the side of the buried word line structure, so that the source / drain region of the active area 12 is formed on the side of the inverted polysilicon layer 3 away from the buried word line structure, and the source / drain region can be separated from the buried word line structure by the inverted polysilicon layer 3, and the inverted polysilicon layer 3 and the source / drain region are doped the same, for example, both are P-type or N-type, so that a certain electric field can be formed between the drain region and the inverted polysilicon layer 3, thereby reducing the electric field strength between the drain region and the buried word line structure, reducing the GIDL current, and improving the turn-on speed of the transistor.

[0039] In some embodiments of the present invention, the steps of forming a buried word line structure include: forming a gate oxide layer 21 on the surface of the second groove 32; forming a gate barrier layer 22 on the surface of the gate oxide layer 21, the gate barrier layer 22 covers the bottom surface and part of the side surface of the gate oxide layer 21; forming a gate conductive layer 23 on the surface of the gate barrier layer 22, the gate conductive layer 23 fills part of the second groove 32; forming an insulating filling layer 24 on the gate barrier layer 22 and the gate conductive layer 23, the insulating filling layer 24 fills the remaining second groove 32.

[0040] Specifically, Figure 6 As shown, a gate oxide layer 21 is formed on the inner wall surface of the second groove 32, and the gate oxide layer 21 covers the inner wall surface of the second groove 32, is flush with the upper surface of the inverted polysilicon layer 3, and does not fill the second groove 32. Figure 7 As shown, a primary barrier layer 26 is deposited on the surface of the gate oxide layer 21 and the surface of the mask layer 4, as shown in FIG. Figure 8 As shown, a primary conductive layer 25 is formed on the surface of the primary barrier layer 26 and fills the second groove 32. Fig. 9 As shown, the primary barrier layer 26 and the primary conductive layer 25 on the surface of the mask layer 4 are removed, and the primary barrier layer 26 and the primary conductive layer 25 in the second groove 32 are retained, and the primary barrier layer 26 and the primary conductive layer 25 in the second groove 32 can be etched back to remove part of the primary barrier layer 26 and the primary conductive layer 25 in the second groove 32, and the part of the primary barrier layer 26 and the primary conductive layer 25 at the bottom of the second groove 32 is retained to form the gate barrier layer 22 and the gate conductive layer 23. The material of the gate barrier layer 22 can be titanium nitride, and can be formed by atomic layer deposition. The thickness of the gate barrier layer 22 can be 2nm-7nm, for example, 2nm, 4nm, 5nm or 6nm, 7nm, etc.

[0041] In the step of removing part of the primary conductive layer 25 and the primary barrier layer 26, the height of the removed part of the primary conductive layer 25 and the primary barrier layer 26 is 20nm-150nm, that is, the height of the removed primary conductive layer 25 and the primary barrier layer 26 located in the second groove 32 is greater than or equal to 20 nanometers and less than or equal to 150 nanometers, so that the height of the removed part of the primary conductive layer 25 and the primary barrier layer 26 is not more than the height of the inverted polysilicon layer 3, so that the upper surface of the formed gate conductive layer 23 and the gate barrier layer 22 is not lower than the lower surface of the inverted polysilicon layer 3.

[0042] The primary conductive layer 25 may be formed by chemical vapor deposition or the like, and the upper portion of the primary conductive layer 25 and the primary barrier layer 26 may be planarized by chemical mechanical polishing. In the step of removing the portion of the primary conductive layer 25 and the primary barrier layer 26 located above the mask layer 4 and in the second groove 32, the primary conductive layer 25 and the primary barrier layer 26 may be etched back by dry etching, and the residual primary barrier layer 26 on the dry-etched sidewall may be removed by wet etching.

[0043] like Fig.10 As shown, the upper surfaces of the gate conductive layer 23 and the gate barrier layer 22 are flush, and the upper surface of the gate barrier layer 22 is not lower than the lower surface of the portion of the inverted polysilicon layer 3 located on the side of the second groove 32, that is, the lower surface of the inverted polysilicon layer 3 is flush with or lower than the upper surfaces of the gate barrier layer 22 and the gate conductive layer 23, so that the source / drain region can be completely separated from the inverted polysilicon layer 3 by the inverted polysilicon layer 3, and the inverted polysilicon layer 3 is formed in the overlapping area of ​​the buried word line structure and the source / drain region, so that the GIDL current can be further reduced.

[0044] like Fig.10 As shown, after removing part of the primary conductive layer 25 and the primary barrier layer 26 in the second groove 32 to form the gate conductive layer 23 and the gate barrier layer 22, an insulating filling layer 24 filling the upper part of the second groove 32 is formed above the gate barrier layer 22 and the gate conductive layer 23 in the second groove 32. The material of the insulating filling layer 24 can be silicon nitride, which can be deposited by chemical vapor deposition. After the insulating filling layer 24 is formed, a chemical mechanical polishing (CMP) process can be performed to planarize the surface of the semiconductor device 100.

[0045] A semiconductor device 100 according to an embodiment of the present invention will be described below with reference to the accompanying drawings. The semiconductor device 100 is formed by using the method for manufacturing the semiconductor device according to the above embodiment.

[0046] like Fig.10 As shown, a semiconductor device 100 according to an embodiment of the present invention may include a semiconductor substrate 1 , a buried word line structure and an inversion polysilicon layer 3 .

[0047] The semiconductor substrate 1 can be silicon (Si), germanium (Ge), silicon germanium (GeSi), or silicon carbide (SiC); it can also be silicon on insulator (SOI), germanium on insulator (GOI); or it can also be other materials, such as III-V group compounds such as gallium arsenide.

[0048] An active area 12 and a trench isolation structure 11 located between the active areas 12 are provided in the semiconductor substrate 1, wherein a plurality of trench isolation structures 11 are provided in the semiconductor substrate 1, and the plurality of trench isolation structures 11 define a plurality of active areas 12 in the semiconductor substrate 1, and the trench isolation structure 11 may include a trench and an insulating material filled in the trench, and the insulating material may be silicon dioxide or the like.

[0049] A plurality of gate structures are formed in the active area 12. In an embodiment of the present invention, the gate structure may be a buried word line structure, and the buried word line structure is formed in the active area 12. The inverted polysilicon layer 3 is disposed in the active area 12 and formed on the side of the buried word line structure and is inversely doped with the active area 12. Specifically, the active area 12 may be doped by ion implantation or diffusion process, and different doping may form an N-type active area 12 or a P-type active area 12. The inverted polysilicon layer 3 and the active area 12 are inversely doped with each other. For example, if the active area 12 is P-doped, the polysilicon layer is formed as an N-type doped polysilicon layer. If the active area 12 is N-doped, the polysilicon layer is formed as a P-doped polysilicon layer.

[0050] Source / drain regions are formed on both sides of the buried word line structure in the active area 12 to serve as the source and drain of the buried word line structure. The source / drain and the buried word line structure have an overlapping area. The inverted polysilicon layer 3 is formed on the side of the buried word line structure and between the buried word line structure and the source / drain regions, and is doped with the same type as the source / drain regions, thereby reducing the GIDL current formed by the drain and the buried word line structure, reducing the leakage current of the semiconductor device 100, and improving the performance of the semiconductor device 100.

[0051] like Fig.10 As shown, the buried word line structure may include: a gate oxide layer 21, a gate barrier layer 22, a gate conductive layer 23 and an insulating filling layer 24, the gate barrier layer 22 is located on the surface of the gate conductive layer 23, the insulating filling layer 24 is located above the gate conductive layer 23 and the gate barrier layer 22, and the gate oxide layer 21 is located on the surface of the gate barrier layer 22 and the insulating filling layer 24.

[0052] Optionally, the upper surface of the gate barrier layer 22 is flush with the upper surface of the gate conductive layer 23 and is not lower than the lower surface of the inverted polysilicon layer 3. In other words, the lower surface of the inverted polysilicon layer 3 is flush with or lower than the upper surfaces of the gate barrier layer 22 and the gate conductive layer 23, so that the source / drain region can be completely separated from the inverted polysilicon layer 3 by the inverted polysilicon layer 3, and the inverted polysilicon layer 3 is formed in the overlapping area of ​​the buried word line structure and the source / drain region, so that the GIDL current can be further reduced.

[0053] Optionally, the upper surface of the inversion polysilicon layer 3 is flush with the upper surface of the gate oxide layer 21, and the thickness of the inversion polysilicon layer 3 is 5nm-25nm. For example, the thickness of the inversion polysilicon layer 3 can be 5nm, 10nm, 15nm, 20nm, etc., and the height of the inversion polysilicon layer 3 is 20nm-150nm. For example, the height of the inversion polysilicon layer 3 can be 20nm, 40nm, 70nm, 100nm, 130nm, etc.

[0054] Optionally, the thickness of the gate barrier layer 22 is 2 nm-7 nm, for example, the thickness of the gate barrier layer 22 may be 2 nm, 4 nm, 5 nm, 6 nm, etc.

[0055] The above are only preferred embodiments of the present invention. It should be pointed out that ordinary technicians in this technical field can make several improvements and modifications without departing from the principles of the present invention. These improvements and modifications should also be regarded as the protection scope of the present invention.

Claims

1. A method for preparing a semiconductor device, characterized in that: include: Providing a semiconductor substrate, wherein an active region and a trench isolation structure located between the active regions are formed in the semiconductor substrate; forming a first groove in the active area; Filling the first groove with an inversion polysilicon layer that is doped in an opposite manner to the active region; forming a second groove, wherein the second groove penetrates the inverted polysilicon layer and a portion of the semiconductor substrate, and retains a portion of the inverted polysilicon layer located on a side of the second groove; forming a buried word line structure in the second groove; Wherein, forming the buried word line structure comprises: forming a gate oxide layer on a surface of the second groove; forming a gate barrier layer on the surface of the gate oxide layer, wherein the gate barrier layer covers the bottom surface and part of the side surface of the gate oxide layer; forming a gate conductive layer on the surface of the gate barrier layer, wherein the gate conductive layer fills a portion of the second groove; forming an insulating filling layer on the gate barrier layer and the gate conductive layer, wherein the insulating filling layer fills the remaining second groove; Wherein, the steps of forming a gate barrier layer and forming a gate conductive layer include: forming a primary barrier layer on the surface of the gate oxide layer; forming a primary conductive layer on the surface of the primary barrier layer and filling the second groove; Part of the primary conductive layer and the primary barrier layer is removed, and part of the primary conductive layer and the primary barrier layer located in the bottom area of ​​the second groove is retained to form the gate barrier layer and the gate conductive layer, wherein the height of the removed part of the primary conductive layer and the primary barrier layer is 20nm-150nm.

2. The method for preparing a semiconductor device according to claim 1, wherein: Before the step of forming the first groove in the active area, the following steps are included: forming a patterned mask layer on the surface of the semiconductor substrate.

3. The method for preparing a semiconductor device according to claim 1, characterized in that: The depth of the first groove is 20nm-150nm, and the width of the first groove is 30nm-100nm.

4. The method for preparing a semiconductor device according to claim 1, wherein: The depth of the second groove is 50nm-300nm, and the width of the second groove is 20nm-50nm.

5. The method for preparing a semiconductor device according to claim 1, characterized in that: The upper surfaces of the gate conductive layer and the gate barrier layer are flush, and the upper surface of the gate barrier layer is not lower than the lower surface of the portion of the inversion polysilicon layer located at the side of the second groove.

6. A semiconductor device, characterized in that: include: A semiconductor substrate, wherein the semiconductor substrate is provided with active regions and a trench isolation structure located between the active regions; A buried word line structure, the buried word line structure is located in the active area, the buried word line structure comprises: a gate oxide layer, a gate barrier layer, a gate conductive layer and an insulating filling layer, the gate barrier layer is located on the surface of the gate conductive layer, the insulating filling layer is located above the gate conductive layer and the gate barrier layer, and the gate oxide layer is located on the surface of the gate barrier layer and the insulating filling layer; An inverted polysilicon layer, wherein the inverted polysilicon layer is located on the side of the buried word line structure and is inversely doped with the active area, the upper surface of the inverted polysilicon layer is flush with the upper surface of the gate oxide layer, the thickness of the inverted polysilicon layer is 5nm-25nm, and the height of the inverted polysilicon layer is 20nm-150nm.

7. The semiconductor device according to claim 6, characterized in that The upper surface of the gate barrier layer is flush with the upper surface of the gate conductive layer and is not lower than the lower surface of the inversion polysilicon layer.

8. The semiconductor device according to claim 6, characterized in that The thickness of the gate barrier layer is 2nm-7nm.