Method for manufacturing semiconductor device

By using a patterned mask to remove the dielectric layer in the TOF chip manufacturing process, the problem of metal layer exposure in the deep trench isolation structure is solved, the adhesion of charged metal balls is avoided, and the yield of semiconductor devices is improved.

CN114284208BActive Publication Date: 2024-10-18WUHAN XINXIN SEMICON MFG CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202111566605.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-20
Publication Date
2024-10-18
Estimated Expiration
2041-12-20

AI Technical Summary

Technical Problem

In the TOF chip manufacturing process, the metal layer in the deep trench isolation structure is etched and exposed before the substrate, causing charged metal balls to adhere to the device surface, affecting the device yield.

Method used

By opening a first trench on the surface of the substrate and filling the first metal layer, forming a first dielectric layer to cover and forming a second trench, filling the second dielectric layer, and using a patterned mask to remove the dielectric layer to form a third trench groove to avoid exposure of the metal layer in front of the substrate.

Benefits of technology

It effectively avoids the attachment of charged metal balls and improves the yield rate of semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114284208B_ABST
    Figure CN114284208B_ABST
Patent Text Reader

Abstract

The present invention provides a method for manufacturing a semiconductor device, comprising: providing a substrate with a first groove on its surface, the surface of a first metal layer filled in the first groove being lower than the surface of the substrate; forming a first dielectric layer covering the surface of the substrate and the surface of the first metal layer, forming a second groove in the first dielectric layer on the first metal layer; forming a second dielectric layer to at least fill the second groove; removing the second dielectric layer and the first dielectric layer, during which the second surface of the first dielectric layer is located at a temporary interface, the temporary interface is away from the first surface of the first dielectric layer, and a portion of the thickness of the second dielectric layer is retained, and after removing the portion of the thickness of the second dielectric layer, the dielectric layer on the first metal layer is removed to form a third groove exposing the first metal layer and the substrate outside the first groove. The technical solution of the present invention can avoid the generation of charged metal balls attached to the surface of the semiconductor device, thereby improving the yield of the semiconductor device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a method for manufacturing a semiconductor device. Background Art

[0002] In the manufacturing process of TOF (Time-of-Flight) chips, a deep trench isolation structure is formed in the substrate, and a trench is formed on the top of the deep trench isolation structure, and the trench exposes the substrate outside the deep trench isolation structure to electrically lead out the substrate. However, some problems arise in the existing manufacturing process.

[0003] See also Figure 1a to Figure 1e , the steps of the existing process include:

[0004] First, a high-K dielectric layer 12 is formed to cover the substrate 11, and a deep trench (not shown) is formed that penetrates the high-K dielectric layer 12 and a portion of the thickness of the substrate 11, an oxide layer 13 is formed on the inner surface of the deep trench and on the high-K dielectric layer 12, a metal layer 14 is formed to fill the deep trench and cover the oxide layer 13 on the high-K dielectric layer 12, and the metal layer 14 covering the oxide layer 13 is removed, so that the oxide layer 13 and the metal layer 14 in the deep trench constitute a deep trench isolation structure; wherein, in order to completely remove the metal layer 14 covering the oxide layer 13, the metal layer 14 is over-etched, so that the top surface of the metal layer 14 in the deep trench is lower than the top surface of the oxide layer 13 on the high-K dielectric layer 12, as shown in FIG. Figure 1a As shown;

[0005] Then, if Figure 1b As shown, a buffer oxide layer 15 is deposited to cover the metal layer 14 and the oxide layer 13; wherein, since the top surface of the metal layer 14 in the deep trench is lower than the top surface of the oxide layer 13 on the high-K dielectric layer 12, a first trench 16 is formed in the buffer oxide layer 15 on the metal layer 14;

[0006] Then, if Figure 1c to Figure 1dAs shown, a patterned photoresist layer 17 is formed on the buffer oxide layer 15, and the buffer oxide layer 15, the oxide layer 13 and the high-K dielectric layer 12 are dry-etched using the patterned photoresist layer 17 as a mask to form a second groove 18 exposing the metal layer 14 in the deep groove and the substrate 11 outside the deep groove; wherein, in the process of dry etching to form the second groove 18, since the first groove 16 is formed in the buffer oxide layer 15 on the metal layer 14, the top surface of the buffer oxide layer 15 on the metal layer 14 is lower than the top surface of the buffer oxide layer 15 on the substrate 11, resulting in the metal layer 14 being etched and exposed before the substrate 11, and the exposed metal layer 14 will continue to be etched before the substrate 11 is exposed to produce a metal-containing polymer 19 attached to the inner surface of the second groove 18, and the polymer 19 will produce charged metal balls D1 (such as Figure 1e As shown in FIG. 1 , the silicon dioxide falls on the buffer oxide layer 15 , causing abnormalities in subsequent processes.

[0007] Therefore, how to prevent the metal layer in the deep trench isolation structure from being exposed by etching before the substrate, and thus prevent the generation of charged metal balls attached to the device surface, is a problem that needs to be solved urgently. Summary of the invention

[0008] The object of the present invention is to provide a method for manufacturing a semiconductor device, which can avoid charged metal balls from adhering to the surface of the semiconductor device, thereby improving the yield of the semiconductor device.

[0009] To achieve the above object, the present invention provides a method for manufacturing a semiconductor device, comprising:

[0010] Providing a substrate, wherein a first groove is formed on the surface of the substrate, the first groove is filled with a first metal layer, and the surface of the first metal layer is lower than the surface of the substrate;

[0011] Forming a first dielectric layer covering the surface of the substrate and the surface of the first metal layer, forming a second groove in the first dielectric layer on the first metal layer, the first dielectric layer having a first surface where the contact surface with the substrate is located and a second surface opposite to the first surface;

[0012] forming a second dielectric layer, wherein the second dielectric layer at least fills the second trench;

[0013] The second dielectric layer and the first dielectric layer are removed using a patterned mask as a mask, and during the removal process, the second surface gradually approaches the first surface until it overlaps with the first surface, wherein during the removal process, the second surface is located at a temporary interface, the first dielectric layer on the side of the temporary interface away from the first surface is removed, and a partial thickness of the second dielectric layer is retained on the side of the temporary interface away from the first surface, and after removing the retained partial thickness of the second dielectric layer, the dielectric layer on the first metal layer is removed to form a third groove exposing the first metal layer and the outer peripheral base of the first groove, and the temporary interface is a horizontal surface in the first dielectric layer.

[0014] Optionally, after removing the retained partial thickness of the second dielectric layer, a newly formed surface of the dielectric layer above the first metal layer is not lower than a newly formed surface of the dielectric layer above the periphery of the first trench.

[0015] Optionally, after removing the retained second dielectric layer of partial thickness, the height difference between the newly formed surface of the dielectric layer above the first metal layer and the newly formed surface of the dielectric layer above the substrate outside the first trench is less than

[0016] Optionally, a dry etching process is used to remove the second dielectric layer and the first dielectric layer, and an etching rate of the second dielectric layer by the dry etching process is lower than an etching rate of the first dielectric layer by the dry etching process.

[0017] Optionally, an etching selection ratio between the second dielectric layer and the first dielectric layer is 1:5 to 1:2.

[0018] Optionally, the base includes a substrate and a third dielectric layer covering the substrate.

[0019] Optionally, the bottom surface of the second groove is not lower than the surface of the third dielectric layer, and the temporary interface is the surface where the bottom surface of the second groove is located;

[0020] After removing the reserved second dielectric layer of partial thickness, the dielectric layer above the first metal layer includes the first dielectric layer filled in the first trench;

[0021] The third dielectric layer and / or a portion of the substrate and the dielectric layer above the first metal layer are removed to form a third trench exposing the first metal layer and the substrate.

[0022] Optionally, the bottom surface of the second groove is lower than the surface of the third dielectric layer, and the temporary interface is the surface where the first surface is located;

[0023] After removing the reserved second dielectric layer of partial thickness, the dielectric layer above the first metal layer includes the first dielectric layer filled in the first groove and the second dielectric layer in the second groove wrapped by the first dielectric layer in the first groove;

[0024] The third dielectric layer and / or a portion of the substrate and the dielectric layer above the first metal layer are removed to form a third trench exposing the first metal layer and the substrate.

[0025] Optionally, the second dielectric layer is a bottom anti-reflection material, and a coating process is used to fill the second dielectric layer in the second groove.

[0026] Optionally, the method for manufacturing the semiconductor device further includes:

[0027] A second metal layer is formed to fill the third trench.

[0028] Compared with the prior art, the method for manufacturing a semiconductor device of the present invention, when the surface of the first metal layer filled in the first groove opened on the surface of the substrate is lower than the surface of the substrate, after forming a first dielectric layer covering the surface of the substrate and the surface of the first metal layer, a second groove is formed in the first dielectric layer on the first metal layer. The method for manufacturing a semiconductor device provided by the present invention forms a second dielectric layer that at least fills the second groove, and removes the second dielectric layer and the first dielectric layer using a patterned mask as a mask. During the removal process, the second surface of the first dielectric layer gradually approaches the first surface of the first dielectric layer until it overlaps with the first surface, wherein the second surface is located at a temporary interface during the removal process. The first dielectric layer on the side of the temporary interface away from the first surface is removed and a second dielectric layer with a partial thickness is retained on the side of the temporary interface away from the first surface. After removing the retained second dielectric layer with a partial thickness, the dielectric layer on the first metal layer is removed to form a third groove exposing the first metal layer and the substrate outside the first groove. The temporary interface is a horizontal plane in the first dielectric layer, so that the first metal layer can be exposed after the substrate outside the first groove or exposed at the same time as the substrate outside the first groove, avoiding the first metal layer from being exposed before the substrate outside the first groove, thereby avoiding the generation of charged metal balls attached to the surface of the semiconductor device, thereby improving the yield of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1a to Figure 1e It is a schematic diagram of a device during the manufacturing process of a semiconductor device;

[0030] Figure 2 is a flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present invention;

[0031] Figure 3a to Figure 3i yes Figure 2 A schematic diagram of a device in a method for manufacturing a semiconductor device is shown.

[0032] Among them, Figure 1a to Figure 3i The reference numerals are described as follows:

[0033] 11-substrate; 12-high-K dielectric layer; 13-oxide layer; 14-metal layer; 15-buffer oxide layer; 16-first trench; 17-patterned photoresist layer; 18-second trench; 19-polymer;

[0034] 21 - substrate; 221 - first trench; 222 - fourth dielectric layer; 223 - first metal layer; 231 - high-K dielectric layer; 232 - oxide layer; 24 - first dielectric layer; 241 - second trench; 25 - second dielectric layer; 26 - patterned photoresist layer; 261 - opening; 27 - third trench. DETAILED DESCRIPTION

[0035] In order to make the purpose, advantages and features of the present invention more clear, the manufacturing method of the semiconductor device proposed by the present invention is further described in detail below. It should be noted that the drawings are all in a very simplified form and are not in precise proportions, which are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.

[0036] An embodiment of the present invention provides a method for manufacturing a semiconductor device. Figure 2 , Figure 2 1 is a flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present invention, wherein the method for manufacturing a semiconductor device comprises:

[0037] Step S1, providing a substrate, wherein a first groove is formed on the surface of the substrate, the first groove is filled with a first metal layer, and the surface of the first metal layer is lower than the surface of the substrate;

[0038] Step S2, forming a first dielectric layer covering the surface of the substrate and the surface of the first metal layer, forming a second groove in the first dielectric layer on the first metal layer, the first dielectric layer having a first surface where the contact surface with the substrate is located and a second surface opposite to the first surface;

[0039] Step S3, forming a second dielectric layer, wherein the second dielectric layer at least fills the second trench;

[0040] Step S4, using a patterned mask as a mask to remove the second dielectric layer and the first dielectric layer, during the removal process, the second surface gradually approaches the first surface until it overlaps with the first surface, wherein during the removal process, the second surface is located at a temporary interface, the first dielectric layer on the side of the temporary interface away from the first surface is removed and a partial thickness of the second dielectric layer is retained on the side of the temporary interface away from the first surface, and after removing the retained partial thickness of the second dielectric layer, the dielectric layer on the first metal layer is removed to form a third groove exposing the first metal layer and the outer base of the first groove, and the temporary interface is a horizontal plane in the first dielectric layer.

[0041] See below Figure 3a to Figure 3i The method for manufacturing the semiconductor device provided in this embodiment is described in more detail. Figure 3a to Figure 3i It is also a schematic diagram of a longitudinal cross-section of a semiconductor device.

[0042] According to step S1 , a substrate is provided, a first groove 221 is formed on the surface of the substrate, the first groove 221 is filled with a first metal layer 223 , and the surface of the first metal layer 223 is lower than the surface of the substrate.

[0043] A fourth dielectric layer 222 is formed on the inner surface of the first trench 221 . The fourth dielectric layer 222 is located between the first metal layer 223 and the substrate. The fourth dielectric layer 222 and the first metal layer 223 form a trench isolation structure.

[0044] The base may include a substrate 21 and a third dielectric layer covering the substrate 21 , and a surface of the first metal layer 223 is lower than a surface of the third dielectric layer.

[0045] The third dielectric layer may be a single-layer structure or a stacked structure of at least two layers.

[0046] See also Figure 3a and Figure 3bTaking the third dielectric layer including a stacked high-K dielectric layer 231 and an oxide layer 232 as an example, the steps of forming the trench isolation structure may include: first, sequentially covering the high-K dielectric layer 231 and the oxide layer 232 on the substrate 21; then, etching the oxide layer 232, the high-K dielectric layer 231 and the substrate 21 to form a first trench 221 penetrating the oxide layer 232, the high-K dielectric layer 231 and a portion of the thickness of the substrate 21; then, forming a fourth dielectric layer 222 on the inner surface of the first trench 221; then, filling the first metal layer 223 in the first trench 221, and the first metal layer 223 also covers the oxide layer 232 and the fourth dielectric layer 222 in the first trench 221; then, removing the first metal layer 223 covering the oxide layer 232 and the fourth dielectric layer 222 in the first trench 221 by an etching process, and only retaining the first metal layer 223 in the first trench 221. In order to completely remove the first metal layer 223 covering the oxide layer 232 and the fourth dielectric layer 222 in the first groove 221 , the first metal layer 223 is over-etched, so that the surface of the first metal layer 223 in the first groove 221 is lower than the surface of the oxide layer 232 .

[0047] The surface of the first metal layer 223 may be lower or higher than the surface of the substrate 21, or the surface of the first metal layer 223 may be flush with the surface of the substrate 21. Figure 3b In the illustrated embodiment, the surface of the first metal layer 223 is lower than the surface of the substrate 21 .

[0048] It should be noted that the fourth dielectric layer 222 may also cover the oxide layer 232 , and then the fourth dielectric layer 222 on the oxide layer 232 , the oxide layer 232 and the high-K dielectric layer 231 together constitute the third dielectric layer.

[0049] The material of the substrate 21 can be any suitable base material known to those skilled in the art, for example, it can be at least one of the following materials: silicon, germanium, silicon germanium, carbon silicon, carbon germanium silicon, indium arsenide, gallium arsenide, indium phosphide, etc.

[0050] The K (dielectric constant) value of the high-K dielectric layer 231 is preferably greater than 7. The material of the high-K dielectric layer 231 may include nitride or metal oxide, for example, silicon nitride, silicon oxynitride, titanium dioxide, tantalum pentoxide, etc.; the material of the oxide layer 232 may be silicon oxide or silicon oxynitride, etc.; the material of the fourth dielectric layer 222 may be at least one of silicon oxide, silicon nitride, tetraethyl orthosilicate, borosilicate glass, phosphosilicate glass, borophosphosilicate glass and silicon oxynitride, etc.; the material of the first metal layer 223 may include at least one of tungsten, nickel, aluminum, silver, gold and titanium.

[0051] According to step S2, refer to Figure 3c , a first dielectric layer 24 is formed to cover the surface of the substrate and the surface of the first metal layer 223, a second groove 241 is formed in the first dielectric layer 24 on the first metal layer 223, and the first dielectric layer 24 has a first surface A1 where the contact surface of the substrate is located and a second surface A2 opposite to the first surface A1. Since the surface of the first metal layer 223 is lower than the surface of the substrate, when the first dielectric layer 24 is formed by a deposition process, a second groove 241 is formed in the first dielectric layer 24 on the first metal layer 223.

[0052] The bottom surface of the second groove 241 may be higher than the surface of the substrate 21; or, the bottom surface of the second groove 241 may be higher or lower than the surface of the third dielectric layer, or the bottom surface of the second groove 241 is flush with the surface of the third dielectric layer.

[0053] exist Figure 3c In the illustrated embodiment, the first dielectric layer 24 covers the oxide layer 232, the first metal layer 223 and the fourth dielectric layer 222; since the surface of the first metal layer 223 in the first groove 221 is lower than the surface of the oxide layer 232, the second groove 241 is formed in the first dielectric layer 24 on the first metal layer 223, and the bottom surface of the second groove 241 is flush with the surface of the oxide layer 232.

[0054] The material of the first dielectric layer 24 may include at least one of silicon oxide, silicon nitride, tetraethyl orthosilicate, borosilicate glass, phosphosilicate glass, borophosphosilicate glass, silicon oxynitride and the like.

[0055] According to step S3, refer to Figure 3d , forming a second dielectric layer 25 , wherein the second dielectric layer 25 at least fills up the second trench 241 .

[0056] The second dielectric layer 25 is a bottom anti-reflection material, which may be a polymer or a photoresist. The second dielectric layer 25 may be filled in the second groove 241 by a coating process, and the bottom anti-reflection material may also cover the first dielectric layer 24 outside the second groove 241. Due to the coating process, the second dielectric layer 25 fills the second groove 241, and the surface of the second dielectric layer 25 on the first dielectric layer 24 outside the second groove 241 is kept flush with the surface of the second dielectric layer 25 on the second groove 241.

[0057] Alternatively, the second dielectric layer 25 is an insulating material such as silicon oxide, silicon oxynitride or silicon nitride, and the second dielectric layer 25 can be filled in the second groove 241 by a deposition process, and the second dielectric layer 25 can also cover the first dielectric layer 24 outside the second groove 241. Wherein, due to the existence of the second groove 241, the surface of the second dielectric layer 25 on the first dielectric layer 24 outside the second groove 241 is not flush with the surface of the second dielectric layer 25 on the second groove 241, so after the deposition process, the surface of the second dielectric layer 25 can be planarized by a chemical mechanical polishing process, so that the surface of the second dielectric layer 25 on the first dielectric layer 24 outside the second groove 241 is flush with the surface of the second dielectric layer 25 on the second groove 241.

[0058] The coating process is simpler than the deposition process, and the surface of the second dielectric layer 25 formed by the coating process is directly flat, without the need to continue to use a chemical mechanical polishing process for planarization. Therefore, the coating process can reduce costs.

[0059] According to step S4, refer to Figure 3e to Figure 3i , using a patterned mask as a mask to remove the second dielectric layer 25 and the first dielectric layer 24, during which the second surface A2 gradually approaches the first surface A1 until it overlaps with the first surface A1, Figure 3f The direction indicated by the arrow in is the movement direction of the second surface A2 gradually approaching the first surface A1; wherein, during the removal process, the second surface A2 is located at a temporary interface, the first dielectric layer 24 on the side of the temporary interface away from the first surface A1 is removed, and a partial thickness of the second dielectric layer 25 is retained on the side of the temporary interface away from the first surface A1, after removing the retained partial thickness of the second dielectric layer 25, the dielectric layer on the first metal layer 223 is removed to form a third groove 27 exposing the first metal layer 223 and the outer base of the first groove 221, and the temporary interface is a horizontal plane in the first dielectric layer 24.

[0060] In addition, after removing the retained partial thickness of the second dielectric layer 25 , the newly formed surface of the dielectric layer above the first metal layer 223 is not lower than the newly formed surface of the dielectric layer above the outer peripheral substrate of the first trench 221 .

[0061] The patterned mask has an opening 261 corresponding to the third groove 27, and the second dielectric layer 25, the first dielectric layer 24 and the third dielectric layer in the patterned mask opening 261 are etched away by a dry etching process. If the first metal layer 223 is exposed before the substrate 21 outside the first groove 221 during the process of forming the third groove 27 by a dry etching process, the exposed first metal layer 223 will continue to be etched before the substrate 21 is exposed to produce a polymer containing metal attached to the inner surface of the third groove 27, and the polymer will produce charged metal balls (i.e., Figure 1e The metal ball D1 shown falls on the various layers of the substrate 21, causing abnormalities in subsequent processes. Therefore, the first metal layer 223 is exposed after the substrate 21 outside the first trench 221 or the first metal layer 223 and the substrate 21 outside the first trench 221 are exposed at the same time.

[0062] If the bottom surface of the second groove 241 is higher than the surface of the third dielectric layer or the bottom surface of the second groove 241 is flush with the surface of the third dielectric layer, the temporary interface is the surface where the bottom surface of the second groove 241 is located; after removing the reserved second dielectric layer 25 of partial thickness, the dielectric layer above the first metal layer 223 includes the first dielectric layer 24 filled in the first groove 221; the third dielectric layer and / or part of the substrate 21 and the dielectric layer above the first metal layer 223 are removed to form a third groove 27 exposing the first metal layer 223 and the substrate 21. After removing the reserved second dielectric layer 25 of partial thickness, the newly formed surface of the dielectric layer above the first metal layer 223 is the remaining surface of the first dielectric layer 24 covering the first metal layer 223, and the newly formed surface of the dielectric layer above the first metal layer 223 is an arc convex upward; the newly formed surface of the dielectric layer above the outer base of the first groove 221 is the surface of the oxide layer 232, and the newly formed surface of the dielectric layer above the outer base of the first groove 221 is a plane.

[0063] The step of forming the third groove 27 exposing the first metal layer 223 and the substrate 21 outside the first groove 221 includes: first, etching the second dielectric layer 25 in the second groove 241 and the first dielectric layer 24 on the substrate 21 outside the first groove 221 to remove a portion of the thickness of the second dielectric layer 25 in the second groove 241 and the first dielectric layer 24 on the substrate 21 outside the first groove 221 that is higher than the bottom surface of the second groove 241 (i.e., the temporary interface), and retaining a portion of the thickness of the second dielectric layer 25 in the second groove 241 and the first dielectric layer 24 on the substrate 21 outside the first groove 221 that is lower than the bottom surface of the second groove 241; then, removing the remaining thickness of the second dielectric layer 25 and the first dielectric layer 24 covering the third dielectric layer; then, removing the third dielectric layer on the substrate 21 outside the first groove 221 and / or a portion of the substrate 21 and the first dielectric layer 24 on the first metal layer 223 to form the third groove 27.

[0064] For example, the bottom surface of the second groove 241 is flush with the surface of the third dielectric layer, and the second dielectric layer 25 also covers the first dielectric layer 24 outside the second groove 241. Figure 3e to Figure 3i The step of forming the third trench 27 of the substrate 21 exposing the first metal layer 223 and the periphery of the first trench 221 includes: first, Figure 3e As shown, a patterned photoresist layer 26 (i.e., a patterned mask) is formed on the second dielectric layer 25, and the patterned photoresist layer 26 has an opening 261 that exposes the second dielectric layer 25 above the trench isolation structure and above the substrate 21 surrounding the trench isolation structure; then, as shown Figure 3f As shown, the patterned photoresist layer 26 is used as a mask to etch the second dielectric layer 25 exposed by the opening 261 until the first dielectric layer 24 around the second trench 241 is exposed; then, as shown Figure 3g As shown, the patterned photoresist layer 26 is continued to be used as a mask to etch away a portion of the thickness of the second dielectric layer 25 in the second trench 241 and the first dielectric layer 24 on the oxide layer 232 outside the second trench 241; then, as shown Figure 3h As shown, the remaining thickness of the second dielectric layer 25 in the second groove 241 is removed; then, as shown Figure 3iAs shown, the patterned photoresist layer 26 is continued to be used as a mask to etch and remove the exposed oxide layer 232, the high-K dielectric layer 231, a partial thickness of the substrate 21, the first dielectric layer 24 on the first metal layer 223, and the fourth dielectric layer 222 above the surface of the first metal layer 223 to form the third groove 27. The third groove 27 just exposes the surface of the first metal layer 223 and extends into the substrate 21.

[0065] If the bottom surface of the second groove 241 is lower than the surface of the third dielectric layer, the temporary interface is the surface where the first surface A1 is located; after removing the reserved second dielectric layer 25 of partial thickness, the dielectric layer above the first metal layer 223 includes the first dielectric layer 24 filled in the first groove 221 and the second dielectric layer 25 in the second groove 241 wrapped by the first dielectric layer 24 in the first groove 221, and the newly formed surface of the first metal layer 223 is the first dielectric layer 24 filled in the first groove 221 and the second dielectric layer 25 in the second groove 241 wrapped by the first dielectric layer 24 in the first groove 221. The surface formed by the second dielectric layer 25 in the second groove 241 wrapped by the first dielectric layer 24 in the groove 221, the newly formed surface of the first metal layer 223 is an arc convex upward; the newly formed surface of the dielectric layer above the outer substrate of the first groove 221 is the surface of the oxide layer 232, and the newly formed surface of the dielectric layer above the outer substrate of the first groove 221 is a plane; the third dielectric layer and / or part of the substrate 21 and the dielectric layer above the first metal layer 223 are removed to form a third groove 27 exposing the first metal layer 223 and the substrate 21.

[0066] The step of forming the third groove 27 of the substrate 21 exposing the first metal layer 223 and the periphery of the first groove 221 includes: first, etching the second dielectric layer 25 in the second groove 241 and the first dielectric layer 24 on the substrate 21 outside the first groove 221 to remove a portion of the thickness of the second dielectric layer 25 in the second groove 241 and the entire thickness of the first dielectric layer 24 on the substrate 21 outside the first groove 221 (that is, removing the first dielectric layer 24 on the surface where the first surface A1 is located), and retaining a portion of the thickness of the second dielectric layer 25, and the surface of the remaining thickness of the second dielectric layer 25 is higher than the first surface A1 and is located between the surface where the first surface A1 is located and the second groove 241. 1 is wrapped by the first dielectric layer 24 in the first groove 221; then, the remaining thickness of the second dielectric layer 25 higher than the first surface A1 and the partial thickness of the third dielectric layer (for example, the partial thickness of the oxide layer 232) on the substrate 21 outside the first groove 221 are removed; then, the remaining thickness of the third dielectric layer (for example, the remaining thickness of the oxide layer 232) on the substrate 21 outside the first groove 221 and / or part of the substrate 21 and the first dielectric layer 24 filled in the first groove 221 and the second dielectric layer 25 in the second groove 241 wrapped by the first dielectric layer 24 in the first groove 221 are removed to form the third groove 27.

[0067] Optionally, after removing the retained second dielectric layer 25 of a partial thickness, the height difference between the newly formed surface of the dielectric layer above the first metal layer 223 and the newly formed surface of the dielectric layer above the outer substrate of the first trench 221 is less than In the process of removing the remaining thickness of the second dielectric layer 25 in the second groove 241, the third dielectric layer, the fourth dielectric layer 222, and the first dielectric layer 24 on the first metal layer 223 that are exposed outside the remaining thickness of the second dielectric layer 25 are also etched a small amount, so that after removing the remaining thickness of the second dielectric layer 25 in the second groove 241, the surface of the first dielectric layer 24 on the bottom surface of the second dielectric layer 25 in the second groove 241 is slightly higher than the surfaces of the third dielectric layer, the fourth dielectric layer 222, and the first dielectric layer 24 on the first metal layer 223 outside the second groove 241, and then, it is also slightly higher than the surface of the third dielectric layer on the substrate 21 outside the first groove 221, and the height difference can be, for example, less than

[0068] Furthermore, it should be noted that, in the step of forming the third groove 27, the etching rate of the second dielectric layer 25 by the dry etching process is controlled to be lower than the etching rate of the first dielectric layer 24 by the dry etching process, so that when the first dielectric layer 24 (or the first dielectric layer 24 and a part of the thickness of the third dielectric layer) on the substrate 21 outside the first groove 221 and higher than the bottom surface of the second groove 241 is etched away, only a part of the thickness of the second dielectric layer 25 in the second groove 241 is etched away. For example, the etching selectivity ratio of the second dielectric layer 25 to the first dielectric layer 24 can be 1:5 to 1:2.

[0069] Then, in other embodiments, the etching rate of the second dielectric layer 25 can also be controlled to be equal to the etching rate of the first dielectric layer 24, so that the first dielectric layer 24 (or the first dielectric layer 24 and a third dielectric layer with a partial thickness) on the substrate 21 outside the first groove 221 and higher than the bottom surface of the second groove 241 and the second dielectric layer 25 in the second groove 241 are etched away at the same time, and then the surface of the first dielectric layer 24 on the bottom surface of the second dielectric layer 25 in the second groove 241 is flush with the surface of the third dielectric layer on the substrate 21 outside the first groove 221.

[0070] In addition, the first metal layer 223 may be prevented from being exposed before the substrate 21 at the periphery of the first groove 221 by controlling the etching rates of the third dielectric layer and the first dielectric layer 24. For example, if the surface of the first metal layer 223 is lower than the surface of the substrate 21, the etching rate of the third dielectric layer may be greater than, equal to, or less than the etching rate of the first dielectric layer 24; if the surface of the first metal layer 223 is flush with the surface of the substrate 21, the etching rate of the third dielectric layer may be greater than or equal to the etching rate of the first dielectric layer 24; if the surface of the first metal layer 223 is higher than the surface of the substrate 21, the etching rate of the third dielectric layer is greater than the etching rate of the first dielectric layer 24.

[0071] Therefore, it can be seen from the above content that in order to avoid the first metal layer 223 being exposed before the substrate 21 outside the first groove 221, it can be achieved by controlling the etching rates of the third dielectric layer, the first dielectric layer 24 and the second dielectric layer 25, and combining the height difference between the surface of the first metal layer 223 and the surface of the substrate 21.

[0072] The method for manufacturing the semiconductor device further includes: removing the patterned photoresist layer 26 and the second dielectric layer 25 above the substrate 21 .

[0073] The method for manufacturing the semiconductor device further includes: forming a second metal layer (not shown) to fill the third trench 27, wherein the second metal layer is electrically connected to the first metal layer 223 and the substrate 21 for subsequent testing and other processes.

[0074] In summary, when the surface of the first metal layer filled in the first groove opened on the surface of the substrate is lower than the surface of the substrate, after forming a first dielectric layer covering the surface of the substrate and the surface of the first metal layer, a second groove is formed in the first dielectric layer on the first metal layer. The method for manufacturing a semiconductor device provided by the present invention forms a second dielectric layer that at least fills the second groove, and removes the second dielectric layer and the first dielectric layer using a patterned mask as a mask. During the removal process, the second surface of the first dielectric layer gradually approaches the first surface of the first dielectric layer until it coincides with the first surface. During the removal process, the second surface is located at a temporary interface, and the temporary interface is away from the first dielectric layer. The first dielectric layer on one side of the first surface is removed and a second dielectric layer with a partial thickness is retained on a side of the temporary interface away from the first surface. After removing the retained second dielectric layer with a partial thickness, the dielectric layer on the first metal layer is removed to form a third groove exposing the first metal layer and the substrate outside the first groove. The temporary interface is a horizontal plane in the first dielectric layer, so that the first metal layer can be exposed after the substrate outside the first groove or at the same time as the substrate outside the first groove, avoiding the first metal layer from being exposed before the substrate outside the first groove, thereby avoiding the generation of charged metal balls attached to the surface of the semiconductor device, thereby improving the yield of the semiconductor device.

[0075] The above description is only a description of the preferred embodiments of the present invention, and is not intended to limit the scope of the present invention. Any changes or modifications made by a person skilled in the art in the field of the present invention based on the above disclosure shall fall within the scope of protection of the claims.

Claims

1. A method for manufacturing a semiconductor device, characterized in that: include: Providing a substrate, wherein a first groove is formed on the surface of the substrate, the first groove is filled with a first metal layer, and the surface of the first metal layer is lower than the surface of the substrate; Forming a first dielectric layer covering the surface of the substrate and the surface of the first metal layer, forming a second groove in the first dielectric layer on the first metal layer, the first dielectric layer having a first surface where the contact surface with the substrate is located and a second surface opposite to the first surface; forming a second dielectric layer, wherein the second dielectric layer at least fills the second trench; The second dielectric layer and the first dielectric layer are removed using a patterned mask as a mask, wherein the second surface gradually approaches the first surface until it overlaps with the first surface during the removal process, wherein the second surface is located at a temporary interface during the removal process, and the etching selectivity ratio of the first dielectric layer and the second dielectric layer is adjusted so that the first dielectric layer on the side of the temporary interface away from the first surface is removed and a partial thickness of the second dielectric layer is retained on the side of the temporary interface away from the first surface, and after removing the retained partial thickness of the second dielectric layer, the dielectric layer on the first metal layer is removed to form a third groove exposing the first metal layer and the outer peripheral base of the first groove, and the temporary interface is a horizontal surface in the first dielectric layer.

2. The method for manufacturing a semiconductor device according to claim 1, wherein: After removing the retained partial thickness of the second dielectric layer, the newly formed surface of the dielectric layer above the first metal layer is not lower than the newly formed surface of the dielectric layer above the periphery of the first trench.

3. The method for manufacturing a semiconductor device according to claim 2, wherein: After removing the retained partial thickness of the second dielectric layer, the height difference between the newly formed surface of the dielectric layer above the first metal layer and the newly formed surface of the dielectric layer above the periphery of the first groove is less than 120Å.

4. The method for manufacturing a semiconductor device according to claim 1, wherein: The second dielectric layer and the first dielectric layer are removed by a dry etching process, wherein an etching rate of the second dielectric layer by the dry etching process is lower than an etching rate of the first dielectric layer by the dry etching process.

5. The method for manufacturing a semiconductor device according to claim 4, wherein: The etching selection ratio of the second dielectric layer to the first dielectric layer is 1:5-1:

2.

6. The method for manufacturing a semiconductor device according to claim 1, wherein: The base comprises a substrate and a third dielectric layer covering the substrate.

7. The method for manufacturing a semiconductor device according to claim 6, wherein: The bottom surface of the second groove is not lower than the surface of the third dielectric layer, and the temporary interface is the surface where the bottom surface of the second groove is located; After removing the reserved second dielectric layer of partial thickness, the dielectric layer above the first metal layer includes the first dielectric layer filled in the first trench; The third dielectric layer and / or a portion of the substrate and the dielectric layer above the first metal layer are removed to form a third trench exposing the first metal layer and the substrate.

8. The method for manufacturing a semiconductor device according to claim 6, wherein: The bottom surface of the second groove is lower than the surface of the third dielectric layer, and the temporary interface is the surface where the first surface is located; After removing the reserved second dielectric layer of partial thickness, the dielectric layer above the first metal layer includes the first dielectric layer filled in the first trench and the second dielectric layer in the second trench wrapped by the first dielectric layer in the first trench; The third dielectric layer and / or a portion of the substrate and the dielectric layer above the first metal layer are removed to form a third trench exposing the first metal layer and the substrate.

9. The method for manufacturing a semiconductor device according to claim 1, wherein: The second dielectric layer is a bottom anti-reflection material, and a coating process is used to fill the second dielectric layer in the second groove.

10. The method for manufacturing a semiconductor device according to claim 1, wherein: The method for manufacturing the semiconductor device further includes: A second metal layer is formed to fill the third trench.

Citation Information

Patent Citations

  • Method of making source electrode and semiconductor device

    CN108376683A

  • Integrated circuit air bridge structures and methods of fabricating same

    EP0812016A1

  • Manufacturing method of semiconductor device

    JP2006135234A

  • Multiple-depth sti trenches in integrated circuit fabrication

    SG130345A1

  • Process for forming a damascene structure

    US20030100190A1