A glass-metal sealed coaxial conductor assembly for pressurized water reactor electrical penetration and a preparation method thereof
Through glass-metal sealing technology, the problem of aging of traditional coaxial conductor components under high temperature, high humidity and high radiation conditions is solved. A coaxial conductor component composed of multi-layer materials is designed to achieve high air tightness and insulation. The risk of radioactive leakage is reduced and the safety of electrical penetration parts of pressurized water reactors is enhanced.
Patent Information
- Application Number
- CN202111562956.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-20
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2041-12-20
AI Technical Summary
Traditional coaxial conductor assembly sealing materials are prone to aging under high temperature, high humidity and high irradiation conditions, and lose their sealing and insulation functions, resulting in damage to the pressure boundary integrity and safety of the electrical penetration parts of the pressurized water reactor, and increasing the risk of radioactive leakage. .
Using glass-metal sealing technology, a coaxial conductor component composed of an inner metal conductor, an inner insulating glass layer, an inner shielding metal layer, an outer insulating glass layer and an outer shielding metal layer is designed, and is sintered and sealed through a specific preparation method connection to achieve high air tightness and high insulation.
It significantly improves the airtightness, insulation and radiation resistance of coaxial conductor components, reduces the risk of sealing performance under high temperature, high humidity and high radiation conditions, and enhances the reliability and safety of components.
Smart Images

Figure CN114373575B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of nuclear reaction safety, and in particular to a glass-metal sealed coaxial conductor assembly for a pressurized water reactor electrical penetration and a preparation method thereof. Background Art
[0002] Pressurized water reactor: full name "pressurized water moderated and cooled reactor". A reactor that uses pressurized, non-boiling light water (i.e. ordinary water) as a moderator and coolant. It consists of fuel assemblies, moderators (also serving as coolant), control rod assemblies, burnable poison assemblies, neutron source assemblies, core baskets and pressure vessels. It is a type of reactor with a large number of applications and a large capacity in nuclear power plants.
[0003] The main functional components of the electrical penetration of a pressurized water reactor include the conductor assembly and the cylinder assembly. The conductor assembly runs through the entire cylinder assembly to achieve physical connection of various cables inside and outside the containment. While achieving electrical connection and signal transmission functions, it works together with the cylinder assembly of the penetration to achieve the integrity of the pressure boundary of the containment. As a key component responsible for the insulation and sealing performance of the electrical penetration, the conductor assembly not only ensures the realization of the electrical continuity of the electrical penetration, but is also an organic part of the integrity of the pressure boundary of the electrical penetration. As a conductor assembly that transmits signals inside and outside the reactor, the coaxial conductor assembly becomes even more important.
[0004] Traditional coaxial conductor assembly sealing materials are made of polymer materials. Polymer materials are inevitably prone to aging phenomena such as embrittlement and creep during long-term operation and life extension operation. After aging, if a high temperature, high humidity, or high radiation accident occurs, there is a risk of losing the sealing and insulation functions. Using glass-metal sealing technology to replace the polymer sealing materials used in coaxial conductor assemblies can improve the sealing performance of the pressure boundary under extreme working conditions and reduce the risk of radioactive leakage after an accident. Therefore, glass-metal sealed coaxial conductor assemblies are a better choice. Summary of the invention
[0005] In view of the shortcomings of the prior art, the present invention aims to provide a glass-metal sealed coaxial conductor assembly for pressurized water reactor electrical penetrations and a preparation method thereof. The coaxial conductor assembly prepared by the method has the characteristics of high air tightness, high insulation, radiation resistance, flame retardancy, etc., thereby solving the shortcomings and defects of the material itself existing in the polymer sealed coaxial conductor assembly.
[0006] The technical solution adopted by the present invention to solve the technical problem is: a glass-metal sealed coaxial conductor assembly for a pressurized water reactor electrical penetration, the assembly mainly comprising an inner metal conductor (1), an inner insulating glass layer (2), an inner shielding metal layer (3), an outer insulating glass layer (4) and an outer shielding metal layer (5) sealed together.
[0007] Furthermore, the inner metal conductor (1) is 4J29 Kovar alloy.
[0008] Furthermore, the inner insulating glass layer (2) has a thermal expansion coefficient of 8 to 10×10 -6 / K inorganic glass.
[0009] Furthermore, the inner shielding metal layer (3) is oxygen-free copper.
[0010] Furthermore, the outer insulating glass layer (4) has a thermal expansion coefficient of 17 to 18×10 -6 / K inorganic glass.
[0011] Furthermore, the outer shielding metal layer (5) is 06Cr19Ni10 stainless steel.
[0012] A method for preparing a glass-metal sealed coaxial conductor assembly for a pressurized water reactor electrical penetration, the method comprising the following steps:
[0013] Step (1), preparing an inner insulating glass layer: weighing raw materials according to a glass ratio and mixing them uniformly, melting them at high temperature and then ball milling them to obtain glass powder, dispersing the glass powder in a liquid phase consisting of a solvent, a dispersant and a binder to obtain a glass slurry, spraying and granulating the slurry to obtain granulated powder with a certain sphericity, preparing the granulated powder into a desired glass blank by pressing and molding, debinding the glass blank at 360-600° C., and vitrifying the glass blank at 650-670° C.;
[0014] Step (2), preparing an outer insulating glass layer: weighing raw materials according to a glass ratio and mixing them uniformly, melting them at a high temperature and then ball milling them to obtain glass powder, dispersing the glass powder in a liquid phase consisting of a solvent, a dispersant and a binder to obtain a glass slurry, spraying and granulating the slurry to obtain granulated powder with a certain sphericity, preparing the granulated powder into a desired glass blank by pressing and molding, debinding the glass blank at 360-600° C., and vitrifying the glass blank at 660-700° C.;
[0015] Step (3), assembling the inner metal conductor, the inner insulating glass layer, the inner shielding metal layer, the outer insulating glass layer and the outer shielding metal layer together using a sintering mold, placing them in an atmosphere protection furnace, and sealing them at a temperature of 960 to 1000° C. for a heat preservation time of 18 to 22 minutes to obtain the glass-metal sealed coaxial conductor assembly.
[0016] Furthermore, in step (1), the glass ratio, measured by weight percentage based on oxides, includes: SiO 2 :60~70%、B 2 O 3 :20~30%、Al 2 O 3:0~5%、Na 2 O: 0~3%、K 2 O: 0~3%, TiO 2 :0~3%, CaO:0~2%.
[0017] Furthermore, in step (2), the glass ratio, measured by weight percentage based on oxides, includes: SiO 2 :50~65%、B 2 O 3 :10~15%、Al 2 O 3 :5~10%、Na 2 O: 4-8%, CeO 2 :2~6%、K 2 O: 0~3%, TiO 2 :0~3%, CaO:0~2%, ZrO 2 :0~2%.
[0018] The beneficial effects of the present invention are as follows: compared with the prior art, the glass-metal sealed coaxial conductor assembly for pressurized water reactor electrical penetrations and the preparation method thereof provided by the present invention have significantly improved the air tightness, insulation, high temperature resistance, aging resistance and other properties of the coaxial conductor assembly obtained; through the above method, a high-reliability coaxial conductor assembly for a pressurized water reactor can be prepared. In addition, in the present invention, the inner metal conductor and the inner shielding metal layer are sealed by approximately matching, and the inner shielding metal layer and the outer shielding metal layer are sealed by compression, and the three metals can be sintered at the same temperature, thereby achieving the sealing of three different metal materials by sintering once. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 A schematic diagram of the sealing of the coaxial conductor assembly provided by the present invention.
[0020] Among them, 1-inner metal conductor; 2-inner insulating glass layer; 3-inner shielding metal layer; 4-outer insulating glass layer; 5-outer shielding metal layer. DETAILED DESCRIPTION
[0021] The present invention is further described below by specific examples, but these examples are only used to illustrate the present invention and are not used to limit the scope of the present invention.
[0022] Embodiments 1 to 4
[0023] (1) According to the glass ratio SiO 2 :60~70%、B 2 O 3 :20~30%、Al 2 O 3 :0~5%、Na2 O: 0~3%、K 2 O: 0~3%, TiO 2 :0-3%, CaO:0-2%, weigh the raw materials and mix them evenly, melt them at high temperature and then perform ball milling to obtain glass powder, disperse the glass powder in a liquid phase composed of solvent deionized water, dispersant sodium polyacrylate and binder polyethylene glycol to obtain glass slurry, spray granulate the slurry to obtain granulated powder with a certain sphericity, use compression molding to prepare the granulated powder into the required glass blank, debind the glass blank at 360-600°C, and vitrify the glass blank at 650-670°C to prepare the inner insulating glass layer 2.
[0024] (2) According to the glass ratio SiO 2 :50~65%、B 2 O 3 :10~15%、Al 2 O 3 :5~10%、Na 2 O: 4-8%, CeO 2 :2~6%、K 2 O: 0~3%, TiO 2 :0~3%, CaO:0~2%, ZrO 2 :0~2%, weigh the raw materials and mix them evenly, melt them at high temperature and then ball-mill them to obtain glass powder, disperse the glass powder in a liquid phase composed of solvent deionized water, dispersant sodium polyacrylate and binder carboxymethyl cellulose to obtain glass slurry, spray granulate the slurry to obtain granulated powder with a certain sphericity, use compression molding to prepare the granulated powder into the required glass blank, debind the glass blank at 360~600℃, and vitrify the glass blank at 660~700℃ to prepare the outer insulating glass layer 4.
[0025] (3) Assemble the inner metal conductor 1, the inner insulating glass layer 2, the inner shielding metal layer 3, the outer insulating glass layer 4 and the outer shielding metal layer 5 together using a graphite sintering mold, place them in an atmosphere protection furnace, and seal them at a temperature of 960 to 1000°C for 18 to 22 minutes to obtain the glass-metal sealed coaxial conductor assembly. Test the gas leakage rate, insulation resistance, withstand voltage value, withstand voltage value and other properties of the glass-metal sealed coaxial conductor assembly; wherein, the gas leakage rate is measured by a helium mass spectrometer leak detector, the insulation resistance is measured by an insulation resistance tester, the withstand voltage value is measured by a withstand voltage tester, and the withstand voltage value is measured by a high-temperature well logging pressure test chamber. The test results are summarized in the following table:
[0026]
[0027]
[0028] The above implementation modes are only used to illustrate the present invention, but not to limit the present invention. Ordinary technicians in the relevant technical field can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, all equivalent technical solutions also belong to the scope of the present invention. The patent protection scope of the present invention should be defined by the claims.
Claims
1. A glass-metal sealed coaxial conductor assembly for a pressurized water reactor electrical penetration, characterized in that: The assembly is mainly formed by sealing an inner metal conductor (1), an inner insulating glass layer (2), an inner shielding metal layer (3), an outer insulating glass layer (4) and an outer shielding metal layer (5); the inner insulating glass layer (2) has a thermal expansion coefficient of 8 to 10×10 -6 / K inorganic glass; the outer insulating glass layer (4) has a thermal expansion coefficient of 17~18×10 -6 / K inorganic glass; The method for preparing the glass-metal sealed coaxial conductor assembly for the electrical penetration of a pressurized water reactor comprises the following steps: Step (1), preparing a glass blank for the inner insulating glass layer: weighing raw materials according to the glass ratio and mixing them uniformly, melting them at high temperature and then ball milling them to obtain glass powder, dispersing the glass powder in a liquid phase consisting of a solvent, a dispersant and a binder to obtain a glass slurry, spraying and granulating the slurry to obtain granulated powder with a certain sphericity, preparing the granulated powder into a desired glass blank by pressing and molding, debinding the glass blank at 360-600° C., and vitrifying the glass blank at 650-670° C.; Step (2), preparing a glass blank for the outer insulating glass layer: weighing raw materials according to the glass ratio and mixing them uniformly, melting them at high temperature and then ball milling them to obtain glass powder, dispersing the glass powder in a liquid phase consisting of a solvent, a dispersant and a binder to obtain a glass slurry, spraying and granulating the slurry to obtain granulated powder with a certain sphericity, preparing the granulated powder into a desired glass blank by pressing and molding, debinding the glass blank at 360-600° C., and vitrifying the glass blank at 660-700° C.; Step (3), assembling the inner metal conductor, the inner insulating glass layer, the inner shielding metal layer, the outer insulating glass layer and the outer shielding metal layer together using a sintering mold, placing them in an atmosphere protection furnace, and sealing them at a temperature of 960-1000° C. for a holding time of 18-22 minutes to obtain the glass-metal sealed coaxial conductor assembly; In the step (1), the glass ratio, measured by weight percentage based on oxides, includes: SiO2: 68%, B2O3: 24%, Al2O3: 2%, Na2O: 2%, K2O: 1%, TiO2: 2%, CaO: 1%; in the step (2), the glass ratio, measured by weight percentage based on oxides, includes: SiO2: 55%, B2O3: 15%, Al2O3: 10%, Na2O: 8%, CeO2: 4%, K2O: 2%, TiO2: 2%, CaO: 2%, ZrO2: 2%; the inner metal conductor (1) is 4J29 Kovar alloy; the inner shielding metal layer (3) is oxygen-free copper; and the outer shielding metal layer (5) is 06Cr19Ni10 stainless steel.