A method for recovering coolant-contaminated membrane electrode
Through the method of low current density loading and high current density constant operation, the problem of low recovery efficiency of coolant-contaminated membrane electrodes in fuel cells is solved, achieving rapid and effective recovery of membrane electrodes, and mitigating the damage to performance caused by long-term coolant contamination. .
Patent Information
- Application Number
- CN202111630375.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-28
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2041-12-28
AI Technical Summary
When existing technologies deal with coolant contamination of membrane electrodes in fuel cells, the gas purge efficiency is low and the membrane electrode performance cannot be fully restored, especially when the coolant is contaminated for a long time.
Using low current density loading and high current density constant operation, air and hydrogen are introduced into the cathode and anode of the membrane electrode respectively, and the low current density is loaded at 10 to 200 mA/cm2 for 10 to 30 minutes, and then It operates continuously for 0.5 to 2 hours at a high current density of 1000 to 2000 mA/cm2, the temperature is 65 to 85°C, the metering ratio of air and hydrogen is 1.5 to 2.5, the humidification is 60 to 100% RH, and the pressure is normal pressure.
It effectively and quickly recovers the membrane electrode contaminated by the coolant, improves the recovery efficiency, prevents the damage to battery performance caused by long-term coolant contamination, and ensures the performance recovery of the membrane electrode.
Smart Images

Figure CN114388839B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of fuel cells, and in particular to a method for recovering a coolant-contaminated membrane electrode. Background Art
[0002] During the operation of the fuel cell, due to problems such as sealing failure, the coolant may leak to the membrane electrode surface, causing contamination of the membrane electrode. Currently, most methods used to treat membrane electrode coolant contamination are gas purging, that is, the ethylene glycol on the membrane electrode surface is removed by the flow of gas. Experiments have found that when the membrane electrode is contaminated by the coolant for a short time, the recovery strategy of gas purging can solve the problem of coolant contamination, but there is a problem of low efficiency; when the coolant is contaminated for a long time, the coolant will penetrate into the catalyst layer of the membrane electrode. The performance of the membrane electrode cannot be restored by simply using the gas purging method. Summary of the invention
[0003] According to the above technical problem that the efficiency of restoring coolant-contaminated membrane electrodes by gas purging is low, and when the coolant is contaminated for a long time, the performance of the membrane electrode cannot be fully restored by simply using the gas purging method, a method for restoring coolant-contaminated membrane electrodes is provided, and a method of low current density loading and high current density constant operation is proposed, which not only ensures the improvement of efficiency, but also alleviates the damage to battery performance caused by long-term coolant contamination.
[0004] The technical means adopted by the present invention are as follows:
[0005] A method for recovering a coolant-contaminated membrane electrode specifically comprises the following steps: introducing air and hydrogen into the cathode and anode of the coolant-contaminated membrane electrode respectively, first loading the coolant-contaminated membrane electrode at a low current density for a period of time, and then operating it at a high current density for a period of time.
[0006] Furthermore, the low current density range is 10-200 mA / cm 2 .
[0007] Furthermore, the low current density loading time is 10 to 30 minutes.
[0008] Furthermore, the high current density range is 1000~2000mA / cm 2 .
[0009] Furthermore, the constant operating time at high current density is 0.5 to 2 h.
[0010] Furthermore, the membrane electrode contaminated by the coolant during the recovery process meets the following conditions: temperature is 65-85°C; cathode air stoichiometric ratio is 1.5-2.5; anode hydrogen stoichiometric ratio is 1.5-2.0; the air and hydrogen introduced into the cathode and anode are humidified to 60-100% RH, and the pressure is normal pressure.
[0011] Compared with the prior art, the present invention has the following advantages:
[0012] The method for recovering a coolant-contaminated membrane electrode provided by the present invention can effectively and quickly recover the membrane electrode contaminated by the coolant, mainly adopting a low current density loading and high current density constant operation mode, and has the advantages of being more effective and faster.
[0013] Based on the above reasons, the present invention can be widely promoted in the fields of fuel cells and the like. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0015] Figure 1 This is a graph showing the open circuit voltage recovery time of the coolant-contaminated membrane electrode in Comparative Example 1 and Example 1 of the present invention.
[0016] Figure 2 These are the polarization curves of the coolant-contaminated membrane electrode after recovery in Comparative Example 1 and Example 1 of the present invention, and the polarization curve of the membrane electrode in Comparative Example 3.
[0017] Figure 3 This is a diagram showing the open circuit voltage recovery time of the coolant-contaminated membrane electrode in Comparative Example 2 and Example 2 of the present invention.
[0018] Figure 4 These are the polarization curves of the coolant-contaminated membrane electrode after recovery in Example 2 of the present invention and the polarization curves of the membrane electrode in Comparative Example 3.
[0019] Figure 5 Comparative polarization curves of the coolant-contaminated membrane electrode after recovery in Comparative Example 2 and Example 2 of the present invention. DETAILED DESCRIPTION
[0020] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present invention and its application or use. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0021] The present invention provides a method for recovering a coolant-contaminated membrane electrode, which specifically comprises the following steps: introducing air and hydrogen into the cathode and anode of the coolant-contaminated membrane electrode respectively, firstly loading the coolant-contaminated membrane electrode at a low current density for a period of time to restore the open circuit voltage of the membrane electrode to above 0.9V, and then operating it constantly at a high current density for a period of time.
[0022] Furthermore, the low current density range is 10-200 mA / cm 2 .
[0023] Furthermore, the low current density loading time is 10 to 30 minutes.
[0024] Furthermore, the high current density range is 1000~2000mA / cm 2 .
[0025] Furthermore, the constant operating time at high current density is 0.5 to 2 h.
[0026] Furthermore, the membrane electrode contaminated by the coolant during the recovery process meets the following conditions: temperature is 65-85°C; cathode air stoichiometric ratio is 1.5-2.5; anode hydrogen stoichiometric ratio is 1.5-2.0; the air and hydrogen introduced into the cathode and anode are humidified to 60-100% RH, and the pressure is normal pressure.
[0027] Coolant contamination will cause the membrane electrode open circuit voltage to be below 0.6V. The specific reason is: From the ethylene glycol anodic oxidation formula (1), it can be seen that when the potential is higher than -0.008V, ethylene glycol will be oxidized to CO2 on the catalyst Pt surface, but the intermediate product CHO generated during the electro-oxidation process ads / CO ads This will cause the catalyst Pt surface to be poisoned and lose its catalytic reaction activity.
[0028] In order to eliminate the intermediate CHO ads / CO ads To convert the poisoning effect of Pt into the final product CO2 without poisoning the catalyst, it is necessary to increase the OH adssurface coverage.
[0029] C2H6O2+2H2O→2CO2+10H + +10e - E=-0.008V(vs.SHE) (1)
[0030] CHO ads +OH ads →CO2+2H + +2e - (2)
[0031] CO ads +OH ads →CO2+H + +2e - (3)
[0032] The present invention provides a method for recovering a coolant-contaminated membrane electrode. First, a low current is applied to increase the OH on the Pt surface. ads The surface coverage of the Pt electrode is increased to oxidize the poisoned intermediates on the Pt surface and restore the open circuit voltage to above 0.9 V. The electrode is then operated at a high current density and the high flux of gas and water removes the ethylene glycol and other intermediates and the final product CO2 remaining in the membrane electrode micropores to prevent secondary pollution. This effectively solves the problem of performance recovery of the membrane electrode after long-term contamination by the coolant and improves the efficiency of performance recovery of the membrane electrode.
[0033] The following specifically describes the recovery effect of the method provided by the present invention on the membrane electrode contaminated by the coolant in combination with Examples 1-2 and Comparative Examples 1-3.
[0034] The coolant used in Examples 1-2 and Comparative Examples 1-2 is a mixture of ethylene glycol and deionized water, and the ethylene glycol concentration is about 20% to 80%. As shown in Table 1, the membrane electrodes used in Examples 1-2 and Comparative Examples 1-2 are all membrane electrodes contaminated by coolants. The difference is that they are immersed in coolants with different ethylene glycol contents for different time periods and different recovery methods are used. Comparative Example 1-2 first purges and then continuously loads the current density to 1000 to 1500 mA / cm 2 The recovery method of the present invention is used in Examples 1-2. Comparative Example 3 is a membrane electrode that has not been contaminated by ethylene glycol.
[0035] Table 1: Examples 1-2 and Comparative Examples 1-3
[0036] serial number Ethylene glycol content in coolant / % Coolant immersion time / h Recovery method Example 1 80% 0.5h Low current density loading, high current density operation Example 2 60% 20h Low current density loading, high current density operation Comparative Example 1 80% 0.5h Purge, Load Comparative Example 2 20% 20h Purge, Load Comparative Example 3 0 0 --
[0037] The open circuit voltage recovery time of the membrane electrode is Figure 1 and Figure 3As shown, when the membrane electrode is contaminated by the coolant for a short time, both methods can restore the open circuit voltage, but the open circuit voltage can be restored to above 0.9V faster using the method provided by the present invention; when the membrane electrode is contaminated by the coolant for a long time, the recovery method used in Example 1-2 cannot restore the open circuit voltage of the membrane electrode to above 0.9V.
[0038] Polarization curve tests were conducted on the uncontaminated membrane electrode of Comparative Example 3 and the restored membrane electrodes of Examples 1-2 and Comparative Examples 1-2 under 100% RH conditions. The test results are as follows: Figure 2 , 4 , 5 as shown; from Figure 2 It can be seen from the figure that when the coolant contaminates the membrane electrode for a short time, the recovery method used in Comparative Example 1 and the method provided by the present invention can restore the contaminated membrane electrode to its initial performance; however, when the coolant contaminates the membrane electrode for a long time, such as Figure 4 , 5 As shown, the recovery method used in Comparative Example 2 cannot restore the performance of the membrane electrode.
[0039] In summary, the present invention adopts low current density loading and high current density constant operation mode, which is of great significance for the effective and rapid recovery of fuel coolant contaminated membrane electrode.
[0040] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for recovering a coolant-contaminated membrane electrode, characterized in that: The coolant is a mixture of ethylene glycol and deionized water; the specific steps include: introducing air and hydrogen into the cathode and anode of the membrane electrode contaminated by the coolant respectively, the open circuit voltage of the membrane electrode contaminated by the coolant is below 0.6V, firstly loading the membrane electrode contaminated by the coolant at a low current density for a period of time, and then operating it at a high current density for a period of time; the low current density range is 10~200mA / cm 2 ; Low current density loading time is 10~30min; High current density range is 1000~2000mA / cm 2 ; The constant operating time at high current density is 0.5~2h; the membrane electrode contaminated by the coolant during the recovery process meets the following conditions: temperature is 65~85℃; cathode air stoichiometric ratio is 1.5~2.5; anode hydrogen stoichiometric ratio is 1.5~2.0; the air and hydrogen introduced into the cathode and anode are humidified to 60~100%RH, and the pressure is normal pressure.
Citation Information
Patent Citations
Fuel batter with proton exchange film disabled membrane electrode recovery regenerated method
CN101140997A
In-situ fuel cell stack reconditioning
CN102044689A
Membrane electrode assembly for improving performance of integrated regenerative fuel cell and preparation method of membrane electrode assembly
CN103474683A
Fuel cell activation method and method for preventing / improving membrane dryness
CN110571446A
Fuel cell regeneration control method and fuel cell system
CN111525164A