Systems and methods for high temperature synthesis of monoatomic and polyatomic dispersions
Stable single-atom and polyatomic dispersions are synthesized on the substrate through a high-temperature heating pulse process, which solves the problem of poor stability of single-atom catalysts at high temperatures, improves the catalytic performance of multi-element interactions, and is suitable for a variety of catalytic applications.
Patent Information
- Application Number
- CN202080055909.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-06-14
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2040-06-14
AI Technical Summary
Single-atom catalysts have poor stability at high temperatures, and existing technologies are difficult to achieve high-temperature synthesis. They are limited to single-element catalysts, fail to take advantage of the synergy between different atoms, and lack new functions brought about by multi-element interactions.
High-temperature synthesis of single-atomic or polyatomic dispersions through heating pulses, utilizing dispersion on the substrate and stable atom-substrate bonds to achieve single-atomic or polyatomic dispersion of elements, using high-temperature heating pulse process (HTHP) between 500K and 4000K Periodic switching heating of short on-state and long off-state is performed at a temperature to prevent atomic aggregation and substrate degradation.
It achieves the synthesis of stable single-atom and poly-atom dispersions on the substrate, improves the thermal stability and catalytic performance of single-atom catalysts, and can form new functions brought about by multi-element interactions. It is suitable for biomass conversion, oxidation, Hydrogenation, electrochemical catalysis and other applications.
Smart Images

Figure CN114502276B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims the benefit of and priority to U.S. Provisional Patent Application Serial No. 62 / 861,639, filed on June 14, 2019, the entire contents of which are incorporated herein by reference. Background Art Technical Field
[0004] The present disclosure relates to the synthesis of atomic dispersions, and more particularly, to the high temperature synthesis of monoatom dispersions or polyatom dispersions.
[0005] Related technologies
[0006] Single-atom catalysts offer optimal atom utilization efficiency and unique coordination environment and are of great significance for improving the catalytic performance of many reactions, such as biomass conversion, oxidation, hydrogenation, and electrocatalysis. However, the stability of single-atom catalysts remains a challenge due to thermodynamically driven atom aggregation and the corresponding performance degradation.
[0007] Various approaches attempt to improve the thermal stability of single atoms by enhancing metal-substrate absorption, using kinetic or steric confinement, or forming strong metal-substrate bonds. In general, atomic dispersion can be achieved in wet chemical synthesis by confinement and coordination of atoms to the substrate, thereby preventing atomic aggregation. Successful synthesis of single atom catalysts at higher temperatures provides higher thermal stability, but high-temperature synthesis is difficult to achieve and is incompatible with many temperature-sensitive methods and materials.
[0008] Furthermore, existing technologies are mostly limited to single-element single-atom catalysts, which do not realize the potential synergistic effects between different atoms, which outperform single-atom catalysts and provide new functions derived from multi-element interactions. Summary of the invention
[0009] The present disclosure relates to high temperature synthesis of single atom dispersions or polyatom dispersions by heat pulses.Aspects of the present disclosure provide dispersed and stable single atom and / or polyatom populations on a substrate with stable atom-substrate bonding.
[0010] According to aspects of the present disclosure, a method for synthesizing an atomic dispersion includes: arranging a loading substrate, the loading substrate including a substrate loaded with at least one of a precursor of an element or an element cluster; applying one or more temperature pulses to the loading substrate, wherein the pulses of the one or more temperature pulses apply a target temperature within a duration, wherein the target temperature is between 500K and 4000K and includes the end values, and the duration is between 1 millisecond and 1 minute and includes the end values; maintaining a cooling period after the pulse; and providing single atoms of the element dispersed on the substrate after the one or more temperature pulses.
[0011] In various embodiments of the method, the method includes dispersing at least a portion of the single atoms of the element on the substrate during the pulse and forming atom-substrate bonds to stabilize the single atoms of the element on the substrate.
[0012] In various embodiments of the method, each of the one or more temperature pulses applies a target temperature for a duration, and the method includes maintaining a cooling period after each of the one or more temperature pulses.
[0013] In various embodiments of the method, the method includes dispersing at least a portion of the single atoms of the element on the substrate during each of at least one temperature pulse; and forming atom-substrate bonds to stabilize the single atoms of the element on the substrate.
[0014] In various embodiments of the method, the method includes performing at least one iteration of: loading the substrate with at least one of a precursor of an additional element or a cluster of an additional element; applying one or more additional temperature pulses to the loaded substrate, wherein each of the one or more additional temperature pulses applies a target temperature for a duration; after each of the one or more additional temperature pulses, maintaining a cooling cycle; and after the one or more additional temperature pulses, providing a polyatomic dispersion of the element and the additional element on the substrate.
[0015] In various embodiments of the method, the element and the further element are one of: the same element or different elements.
[0016] In various embodiments of the method, the element is one of Pt, Ru or Co.
[0017] In various embodiments of the method, the substrate includes at least one of a carbon-based material, a metal, a ceramic, a polymer, a composite material, or an oxide.
[0018] In various embodiments of the method, the substrate includes at least one of carbon, C3N4, TiO2, or CO2 activated carbon nanofibers.
[0019] According to aspects of the present disclosure, a system for synthesizing atomic dispersions includes: a loading substrate, the loading substrate including a substrate loaded with at least one of a precursor of an element or a cluster of an element; one or more heating elements; and a controller, the controller being configured to: control the one or more heating elements to apply one or more temperature pulses to the loading substrate, wherein the pulse of the one or more temperature pulses applies a target temperature within a duration, wherein the target temperature is between 500K and 4000K (including the end value), and the duration is between 1 millisecond and 1 minute (including the end value), and a cooling period is maintained after the pulse. After the one or more temperature pulses, single atoms of the element are dispersed on the substrate.
[0020] In various embodiments of the system, the pulses cause at least a portion of the single atoms of the element on the substrate to disperse and cause atom-substrate bonds to form to stabilize the single atoms of the element on the substrate.
[0021] In various embodiments of the system, the one or more heating elements are configured to apply one of: direct Joule heating, conductive heating, radiative heating, microwave heating, laser heating, or plasma heating.
[0022] In various embodiments of the system, the controller is configured to control the one or more heating elements to apply a target temperature for a duration for each of the one or more temperature pulses and to maintain a cooling period after each of the one or more temperature pulses.
[0023] In various embodiments of the system, the system includes a conveyor carrying a loaded substrate, wherein a controller is configured to control the conveyor to transport the loaded substrate for heating by at least one heating element, wherein controlling the one or more heating elements to apply one or more temperature pulses to the loaded substrate includes: controlling the one or more heating elements to maintain a temperature, and controlling a speed of the conveyor to expose multiple portions of the loaded substrate to each of the one or more heating elements for a duration.
[0024] In various embodiments of the system, the one or more heating elements include a plurality of heating elements, wherein the plurality of heating elements are spaced apart such that conveyance of the plurality of portions of the loaded substrate on the conveyor between each of the plurality of heating elements effects a cooling cycle.
[0025] In various embodiments of the system, the loaded substrate is a continuous strip and the conveyor continuously conveys the continuous strip of loaded substrate.
[0026] In various embodiments of the system, the loaded substrate is in one of a powder form or a droplet form, and the system includes a projection device for projecting the loaded substrate through one or more heating elements, wherein controlling at least one heating element to apply at least one temperature pulse to the loaded substrate includes: controlling at least one heating element to maintain a temperature, and controlling a projection speed of the projection device to expose the loaded substrate to each of the at least one heating element for a duration.
[0027] In various embodiments of the system, the at least one heating element comprises a plurality of heating elements, wherein the plurality of heating elements are spaced apart such that travel of the projected loaded substrate between each of the plurality of heating elements effects a cooling cycle.
[0028] In various embodiments of the system, the element is one of Pt, Ru or Co.
[0029] In various embodiments of the system, the substrate includes at least one of a carbon-based material, a metal, a ceramic, a polymer, a composite material, or an oxide.
[0030] In various embodiments of the system, the substrate includes at least one of carbon, C3N4, TiO2, or CO2 activated carbon nanofibers.
[0031] According to aspects of the present disclosure, a structure includes a substrate, single atoms of an element dispersed on the substrate, and bonding between the single atoms and the substrate.
[0032] In various embodiments of the structure, the bonding includes at least one or more of the following: a metallic bond, a covalent bond, an ionic bond, or a Van der Waals force.
[0033] In various embodiments of the structure, the element is one of Pt, Ru or Co.
[0034] In various embodiments of the structure, the substrate includes at least one of a carbon-based material, a metal, a ceramic, a polymer, a composite material, or an oxide.
[0035] In various embodiments of the structure, the substrate includes at least one of carbon, C3N4, TiO2, or CO2 activated carbon nanofibers.
[0036] In various embodiments of the structures, the single atom is a catalyst for at least one of: biomass conversion, oxidation, hydrogenation, thermochemical catalysis, electrochemical catalysis, photochemical catalysis, or fundamental studies of atom manipulation.
[0037] According to aspects of the present disclosure, a structure includes a substrate, a polyatomic group dispersed on the substrate, and a bond between the polyatomic group and the substrate. Each of the polyatomic groups includes at least two atoms, wherein at least two atoms are the same element or at least some of the at least two atoms are different elements. The polyatomic group is selected from the group consisting of a diatomic group, a triatomic group, a tetraatomic group, or a group of more than four atoms.
[0038] In various embodiments of the structure, the bonding includes one or more of the following: metallic bonds, covalent bonds, ionic bonds, or van der Waals forces.
[0039] In various embodiments of the structure, the polyatom group includes Pt-Ru diatoms.
[0040] In various embodiments of the structure, the polyatom group includes Pt-Co diatoms.
[0041] In various embodiments of the structure, the substrate includes at least one of carbon nanofibers, reduced graphene oxide, or C3N4.
[0042] In various embodiments of the structures, the polyatom group is a catalyst for at least one of: biomass conversion, oxidation, hydrogenation, thermochemical catalysis, electrochemical catalysis, photochemical catalysis, or fundamental studies of atom manipulation.
[0043] Further details and aspects of exemplary embodiments of the present disclosure are described in more detail below with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] The above and other aspects and features of the present disclosure will become more apparent from the following detailed description taken in conjunction with the accompanying drawings, wherein like reference numerals designate similar or identical elements, and:
[0045] FIG. 1 is a diagram of an exemplary control of a high temperature heating pulse according to aspects of the present disclosure;
[0046] Figure 2 is a diagram of an exemplary individual high temperature heating pulse according to aspects of the present disclosure;
[0047] Figure 3 is a diagram of an exemplary heating configuration for applying high temperature heating pulses according to aspects of the present disclosure;
[0048] Figure 4 is a diagram of an exemplary process for synthesizing a single atom dispersion using a high temperature heating pulse according to aspects of the present disclosure;
[0049] Figure 5 is a diagram of an exemplary process for synthesizing a polyatomic group using a high temperature heating pulse according to aspects of the present disclosure;
[0050] Figure 6 is a graph of exemplary results with 3-atom groups according to aspects of the present disclosure;
[0051] Figure 7 is a graph of exemplary results with multi-atom groups according to aspects of the present disclosure;
[0052] Figure 8 is a diagram of an exemplary heating configuration having multiple heating elements and a conveyor according to aspects of the present disclosure;
[0053] Fig. 9 Graphs and images related to applying a high temperature heating pulse (HTHP) process to synthesize Pt atoms on a CO2 activated carbon nanofiber (CA-CNF) substrate according to aspects of the present disclosure are shown;
[0054] Fig.10 shows diagrams and images related to single-atom bond structures according to aspects of the present disclosure;
[0055] Fig.11Figures and images related to applying HTHP processes to various atoms and substrates and for various applications according to aspects of the present disclosure are shown;
[0056] Fig.12 shows graphs and images related to the formation of Pt-Ru diatoms on carbon nanofibers by a HTHP process according to aspects of the present disclosure;
[0057] Fig.13 shows high resolution atomic images of diatoms formed on carbon and C3N4 substrates by a HTHP process according to aspects of the present disclosure; and
[0058] Fig.14 is a diagram of an exemplary heating configuration for applying a HTHP process to micron-sized powder or droplet substrate particles according to aspects of the present disclosure. DETAILED DESCRIPTION
[0059] The present disclosure relates to the high temperature synthesis of monoatomic dispersions or polyatomic dispersions by heating pulses. Aspects of the present disclosure provide dispersed and stable monoatomic and / or polyatomic groups on a substrate having stable atom-substrate bonds. Temperatures represented by the letter "K" will be understood to refer to degrees Kelvin, while temperatures represented by the letter "C" will be understood to refer to degrees Celsius.
[0060] The synthesis process disclosed herein may be referred to as high temperature heat pulse ("HTHP"). The HTHP process synthesizes and stabilizes single atoms at high temperatures and can be achieved using programmable periodic switching heat pulses with a short on-state (e.g., ~1500K, ≤55 milliseconds) and a longer off-state (e.g., 10 times longer than the on-state time, close to room temperature). In various embodiments, the on-state provides activation energy for the single-atom dispersion by forming atom-substrate bonds that can naturally withstand high temperature annealing. The longer off-state achieves overall dispersion stability by preventing atomic aggregation, metal vaporization, and substrate degradation caused by extended heating. The switching heat pulse causes atomic dispersion during high temperature exposure while keeping the substrate stable.
[0061] As will be described later in this article, the HTHP process can be used to synthesize polyatomic groups or atomic alloys composed of the same or different elements, wherein each element is a single atom and is bonded to each other and the substrate. As used herein, the term "polyatomic group" refers to and includes groups of two or more atoms on a substrate produced by the continuous application of the HTHP process, such as groups of two atoms, groups of three atoms, groups of four atoms, or groups of other numbers of atoms. The atoms in the polyatomic group can be the same element, or different elements. For example, all atoms in the polyatomic group can be the same element, or all atoms in the polyatomic group can be different elements, or some atoms in the polyatomic group can be different elements while some atoms in the group are the same element. Examples of polyatomic groups will be described later in this article in conjunction with Figure 5-7 Give a description.
[0062] Portions of this disclosure refer to U.S. Provisional Patent Application No. 62 / 861,639, filed on June 14, 2019, the entire contents of which are incorporated herein by reference and may be referred to herein as “Supplemental Text.”
[0063] refer to Figure 1 , an exemplary control diagram for a high temperature heating pulse is shown. Figure 1 The illustration is not intended to be drawn to scale. The heating pulses may be controlled to achieve a heating on-state target temperature T 高 In various embodiments, the various pulses may not reach the temperature T precisely 高 and may have a value higher or lower than T 高 temperature, and different pulses may reach different temperatures. During the heating off state, the process can be controlled to achieve T 低 In various embodiments, the various shutdown states may not precisely reach the temperature T 低 and may have a value higher or lower than T 低 The temperature of the off state may reach different temperatures during different off state cycles. 低 This may be, for example, room temperature or ambient temperature.
[0064] To achieve Figure 1 The temperature pulse controlled heating configuration is combined below Figure 3 Now, note that the temperature T 高 and T 低 It is sufficient that the temperature T is sensed by one or more temperature sensors, which can sense the temperature of the heating element or sense the temperature of the environment near the heated material, among other possibilities. In various embodiments, the temperature T can be inferred based on the predetermined heating characteristics of the heating element and the heating environment. 高 and T低 , for example where no temperature sensor is used at all or where no temperature sensor is used in a desired location.
[0065] Figure 1 The control diagrams are exemplary and variations are considered within the scope of the present disclosure. For example, although a number of n pulses are shown, the HTHP process may be implemented with only a single pulse (n=1) in various cases. In addition, the pulse control is programmable and different control modes may be implemented. For example, in various embodiments, various pulses may have different target temperatures. Such variations are considered within the scope of the present disclosure.
[0066] Figure 2 is a diagram of an exemplary single high temperature heating pulse. Figure 2 The illustration is not intended to be drawn to scale. The heating pulse can be controlled to have a heating rate R 加热 The heating rate may or may not be constant and may be, for example, between 10 K / min and 10 7 K / min (including the end value). When the target temperature T is reached 高 When the duration t 高 In various embodiments, the target temperature T 高 can be between 500K and 4000K (inclusive), and the duration t for maintaining the target temperature 高 It can be between 1 millisecond and 1 minute (inclusive). For example, for a target temperature T between 1500K and 2000K 高 , the duration of maintaining the target temperature is t 高 It can be about 55 milliseconds. As mentioned above, the actual temperature reached may not be the exact T 高 , which may be above or below the target temperature.
[0067] The temperature is controlled at the target temperature for a duration of t 高 After that, the temperature can be controlled to cool at a rate R 冷却 The cooling rate may or may not be constant, for example, it may be -10K / min and -10 7 K / min (including the end value). When the target temperature T is reached 低 When the duration t 低 In various embodiments, the target temperature T 低 It can be room temperature or ambient temperature, and the duration t used to maintain the target temperature 低 It can be the duration t 高In various embodiments, the duration t is approximately ten times greater than t, for example, between 10 milliseconds and 10 minutes (inclusive). 低 Probably not the duration t 高 For example, for a duration t of about 55 milliseconds 高 , duration t 低 It may be about 550 milliseconds. As mentioned above, the actual temperature reached may not be the exact T 低 , which may be above or below the target temperature.
[0068] Figure 2 The illustrations are exemplary and variations are considered within the scope of the present disclosure. For example, although the heating rate R 加热 and cooling rate R 冷却 are shown as constant rates, but they can be variable rates controlled according to a programmed schedule. 加热 and cooling rate R 冷却 May be very different from each other, for example when the cooling rate is passively achieved. In various embodiments, the cooling rate can be achieved by active cooling. Such or other variations are considered within the scope of the present disclosure.
[0069] refer to Figure 3 , a diagram showing an exemplary heating configuration for applying a high temperature heating pulse. According to various aspects of the present disclosure, if it is possible to Figure 1 and Figure 2 Any heating configuration may be used if the temperature pulses are controlled in the manner described. For example, Figure 3 Six possible configurations are shown, including direct Joule heating, conduction heating, radiation heating, microwave heating, laser heating, and plasma heating. However, other heating configurations not shown or described herein may be used. Various configurations may be implemented with cooling mechanisms (not shown), such as, but not limited to, cooling by radiation and conduction, active cooling by conduction and convection, and / or active cooling by physical or chemical transformation of absorbed heat, and other possibilities. Depending on which heating configuration is implemented, one or more temperature sensors (not shown) may be deployed at one or more locations, as described above. In various embodiments, the temperature may be inferred based on the predetermined heating characteristics of the heating element and the heating environment, such as when a temperature sensor is not used at all or when a temperature sensor is not used at a desired location.
[0070] The heating arrangement may include a controller (not shown) that is implemented or programmed to Figure 1 and Figure 2The heating pulses are controlled in a manner described in the relevant description. The controller may include, for example, one or more of a central processing unit, a microcontroller, a digital signal processor, a field programmable gate array (FPGA), a programmable logic device (PLD) and / or an application specific integrated circuit (ASIC) and other types of processors and circuits. The heating configuration may also include other components, such as but not limited to a power supply, a fuel source, a motor, a housing, an insulator and / or other sensors, and other components. These components are not shown in order to provide a clearer description, but they will be understood and recognized by those skilled in the art.
[0071] Figure 4 is a diagram of an exemplary process for synthesizing a single atom dispersion using a high temperature heating pulse. The precursors or atomic clusters 410 of the elements are loaded onto a substrate 420, and the HTHP process is applied to the loaded substrate. Figure 3 The loaded substrate 410 / 420 is processed using the heating configuration shown in FIG. 1 . The HTHP process converts the precursor 410 into the desired atoms 430 and / or disperses the atomic clusters 410. The high temperature on-state of the HTHP process promotes dispersion and stabilization of single atoms 430 through strong atom-substrate bonds, while the off-state achieves overall stability by preventing overheating-induced atomic aggregation and substrate degradation. During high temperature exposure, the switching heating pulses result in an atomic dispersion 430 on the substrate 420 while keeping the substrate 420 stable. The single atom dispersion achieved by the HTHP process may not disperse every cluster, but may retain some clusters after the HTHP process.
[0072] In various embodiments, single atom 430 can be any single atom, including but not limited to Pt, Ru or Co. In various embodiments, substrate 420 can be a carbon-based material, a metal, a ceramic, a polymer, a composite material, an oxide, and / or a combination thereof. For example, substrate 420 can be a carbon, C3N4 or TiO2 substrate, or a CO2 activated carbon nanofiber (CA-CNF) substrate. As used herein, the term "defect" is a feature of a substrate, and it refers to and includes irregularities in the substrate structure and / or a regular structure that deviates from / deviates from the substrate. As described above, defects in the substrate serve to stabilize the single atoms on the substrate. Figure 4 The illustration is exemplary and not drawn to scale. For example, single atoms 430 may be unevenly or irregularly spaced on substrate 420. In various embodiments, single atoms 430 may have uneven or irregular spacing. In addition, not every atom of an element on substrate 420 is a single atom, and portions of substrate 420 may include groups of multiple atoms of an element.
[0073] Figure 5is a diagram of an exemplary process for synthesizing a polyatomic group using a high temperature heating pulse. A precursor or cluster 510 of element A is loaded onto a substrate 520, and a HTHP process is applied to the loaded substrate to provide a single atom dispersion and a stable body 530. Next, a precursor or cluster 540 of element B is further loaded onto the substrate 520, and a HTHP process is applied to the further loaded substrate to provide a single atom dispersion and a stable body of atom B 542. Through this process, atom B 542 can be dispersed and stabilized on the substrate 520 at the same position as atom A 512, thereby forming a polyatomic group, and / or can be dispersed and stabilized on the substrate 520 at a different position from atom A 512. In various embodiments, atom A and atom B can be the same element, or atom A and atom B can be different elements.
[0074] Figure 5 The illustration is exemplary and is not intended to be drawn to scale. For example, single atoms and polyatomic groups may be unevenly or irregularly spaced on the substrate. In various embodiments, single atoms or polyatomic groups may have uneven or irregular spacing. In various embodiments, not every atom A 512 can be grouped with atom B 542, and not every atom B 542 can be grouped with atom A 512. In addition, some groups on substrate 520 may include groups of multiple atoms A 512 or multiple atoms B 542. In other words, the single atom dispersion achieved by the HTHP process may not disperse each cluster, but may retain some clusters after the HTHP process. In various embodiments, single atoms 512, 542 can be any single atoms, including but not limited to Pt, Ru and / or Co. In various embodiments, substrate 520 can be a carbon-based material, a metal, a ceramic, a polymer, a composite material, an oxide, and / or a combination thereof. For example, the substrate 520 may be a carbon, C3N4 or TiO2 substrate, or a CO2 activated carbon nanofiber (CA-CNF) substrate.
[0075] The process of further loading the substrate with precursors or clusters of another element can be repeated to form larger groups of multiple atoms. Figure 6 is a diagram of an exemplary result with a 3-atom group (formed by atom A 610, atom B 620, and atom C 630) on a substrate 640, Figure 7 is a diagram of an exemplary result of n polyatom groups of atoms formed on a substrate 740 (from atom A 710, atom B 720, up to atom n 730). The obtained result can be obtained by sequentially / iteratively loading a substrate and applying the HTHP process to the loaded substrate. Figure 6 and 7The result. The atoms in each group can be the same element or can include different elements. In various embodiments, the single atom can be any single atom, including but not limited to Pt, Ru or Co. The substrate can be a carbon-based material, a metal, a ceramic, a polymer, a composite material, an oxide and / or a combination thereof. For example, the substrate can be a carbon, C3N4 or TiO2 substrate, or a CO2 activated carbon nanofiber (CA-CNF) substrate.
[0076] The resulting substrates with single-atom dispersions and / or multi-atom dispersions can be used in various applications, such as but not limited to basic research on biomass conversion, oxidation, hydrogenation, thermochemical catalysis, electrochemical catalysis, photochemical catalysis and / or atom manipulation.
[0077] Thus, the above are examples of systems and methods for implementing high temperature heat pulses.Examples of specific systems or examples of specific materials and substrates processed by high temperature heat pulses are described below.
[0078] Figure 8 A diagram showing an exemplary heating configuration with multiple heating sources / heating elements 810 and a conveyor 820 that transports one or more loaded substrates 830 that are heated by the heating elements 810 is shown. The heating elements 810 may remain heated and their temperature may not need to be ramped up or down. Instead, the speed of the conveyor 820 may be configured to be at a speed corresponding to the number of substrates 830 that are heated by the heating elements 810. Figure 2 The duration of the on-state t 高 The loaded substrate 830 is exposed to individual heating elements 810 within the chamber. The positions of the heating elements 810 can be configured so that the travel time of the substrate 830 between the heating elements 810 corresponds to Figure 2 The duration of the closed state t 低 When the configuration shown is used with a continuous strip of substrate 830 loaded with elemental precursors or clusters, the HTHP process can be applied continuously to synthesize single-atom or polyatom dispersions 840 at a high synthesis rate.
[0079] refer to Fig.14, shows a diagram of an exemplary heating configuration for applying a HTHP process to micron-sized powder or droplet base particles according to aspects of the present disclosure. The illustrated heating configuration includes a plurality of heating elements 1410 through which micron-sized powder or droplet base particles 1420 (e.g., atomized) may be projected by a projection device (not shown), such as by a sprayer or blower. In various embodiments, the micron-sized powder or droplet base particles 1420 may have a substrate having a carbon-based material, a metal, a ceramic, a polymer, a composite material, an oxide, and / or combinations thereof. The micron-sized powder or droplet base particles 1420 may be loaded with precursors of elements or clusters of elements. The heating elements 1410 may remain heated and their temperature may not need to be ramped up or down. Instead, the speed at which the micron-sized powder or droplet base particles 1420 are projected may be configured to be at a speed corresponding to a predetermined temperature. Figure 2 The duration of the on-state t 高 The loaded powder or droplet substrate particles 1420 are exposed to individual heating elements 1410. The positions of the heating elements 1410 can be configured so that the travel time of the substrate 1420 between the heating elements 1410 corresponds to Figure 2 The duration of the closed state t 低 When the illustrated configuration is used with a continuous flow of micron-sized powder or droplet substrate particles 1420 loaded with elemental precursors or clusters, the HTHP process can be continuously applied to synthesize single-atom dispersions or polyatom dispersions 1430 on the micron-sized substrate particles at a high synthesis rate.
[0080] The following will describe the application of the HTHP process to specific atoms and substrates. In the following description, any heating configuration may be used, such as Figure 3 , Figure 8 or Fig.14 Any heating configuration.
[0081] Fig. 9 Figures and images related to the synthesis of Pt atoms on CO2 activated carbon nanofiber (CA-CNF) substrates using HTHP process are shown. Fig. 9 In the figure, part (a) is a schematic diagram showing the HTHP synthesis and dispersion process involving carbon atoms, metal precursors, and metal atoms. Part (b) shows the temperature evolution and detailed heating / cooling pattern during the HTHP synthesis process. The inset shows the light emitted by the material at high temperature. Part (c) shows the heating pattern of 10 pulses, showing consistent temperatures in each cycle with a high-temperature on-state and a low-temperature off-state. Parts (d) and (e) show the temperature evolution of the HTHP process (0.01 μmol / cm 2) High-angle annular dark field (HAADF) images of Pt single atoms after 1 and 10 cycles. Part (f) shows the extended X-ray absorption fine structure (EXAFS) curves of Pt single atoms on CA-CNF after 1 and 10 cycles of the HTHP process (without phase correction).
[0082] like Fig. 9 As schematically shown in part (a) of FIG. 5 , the ethanol-based salt precursor (H 2 PtCl 6 ) is loaded onto the defective CA-CNF with good wettability (e.g., loading 0.01 μmol / cm 2 , normalized to the geometric area). The precursor-loaded CA-CNF films were then subjected to HTHP treatment using an electric Joule heating process that can be programmed in terms of temperature, on-off duration, and repeated cycles (Supplementary text, Fig. S1). Thermal images captured by a high-speed camera showed a uniform spatial temperature distribution during the shock heating treatment (Supplementary text, Fig. S2). Fig. 9 Part (b) shows the temperature evolution of a pulse that heats to ∼1500 K in 55 ms and then is rapidly quenched 10 times longer by directly cutting off the input current, resulting in an average temperature of ∼400 K over the entire process. Fig. 9 Part (c) shows the temperature profiles for 10 heating cycles at a period of 6 s, indicating that relatively stable temperatures can be repeatedly reached during the heating process. Furthermore, temperatures as high as ∼3000 K can be achieved (Supplementary Text, Figure S2c), allowing the synthesis of thermally stable single atoms at high temperatures.
[0083] Fig. 9 Parts (d) and (e) of Figure 3 show high-angle annular dark field (HAADF) images of Pt dispersed on a CA-CNF substrate after 1 and 10 heat pulses at 1500 K. For a single heat pulse, the surface of the CA-CNF is dispersed with a high density of single atoms, although Pt clusters are also visible ( Fig. 9 , part (d); and Supplementary Text, Fig. S3a). However, after 10 pulses, the substrate showed a relatively uniform distribution of single atoms ( Fig. 9 , part (d); and Supplementary Text, Figure S3b), indicating that the clusters are further decomposed into single atoms during the continuous HTHP process. The macroscopic extended X-ray absorption fine structure (EXAFS) ( Fig. 9 , part (f)) and X-ray near-edge structure (XANES) analysis (Supplementary Text, Figure S3c) confirmed the single-atom dispersion. The EXAFS spectrum of the sample after 1 cycle is shown in (corresponding to the Pt-Pt bond), while The main peak at represents the Pt-substrate bonds (Pt-C bonds, as described below), revealing the structure of Pt nanoclusters mixed with single atoms. After 10 cycles, almost no Pt-Pt bonds remain, indicating the dominance of single-atom dispersions by decomposing the remaining clusters. The surface area of the CA-CNF substrate is ∼56 m 2 / g, and the Pt loading was measured to be ∼0.24 wt %. By varying the metal loading, nanoclusters can be formed at higher loadings (see Supplementary Text, Figure S4 for 0.05 and 0.1 μmol / cm 2 ), because of the limited number of stable sites.
[0084] To characterize the dispersion mechanism, control samples were examined using different heating strategies (Supplementary Text, Fig. S5a-c). Low-temperature synthesis may lack the activation energy to effectively disperse these atoms and bind them to the substrate (i.e., poor dispersion and stability), while high-temperature annealing can lead to unacceptable particle agglomeration due to overheating-induced graphitization of the carbon substrate (i.e., loss of defects) and long-range atomic diffusion. The HTHP process utilizes high temperatures for single-atom synthesis, but each pulse is short enough to avoid degradation of the substrate, thereby maintaining the stability of the single-atom dispersion.
[0085] As mentioned above, substrate defects help to bind mobile single atoms to the substrate and improve their structural stability. (See Supplementary Text, Fig. S5d-f). Applying the HTHP process on relatively crystalline CNFs (without CO2 activation) produces nanoclusters mixed with single atoms due to limited defect sites. In contrast, after activation, the increased defect aggregation and the presence of micropores (i.e., carbon vacancies) on CA-CNFs (Supplementary Text, Figs. S6-S7) lead to a high density of single-atom dispersions. Therefore, substrates with more defects can accommodate a high density of single atoms. Therefore, this illustrates the role of high-temperature heating pulses and defects on the substrate for effective single-atom dispersion and stabilization.
[0086] The single atoms synthesized by the HTHP process are structurally stable, especially when synthesized at high temperatures of 1500 K, as confirmed by in situ scanning transmission electron microscopy (STEM) from room temperature to 1273 K. The samples were allowed to stabilize for at least 30 min before taking pictures. Figure 2As shown in a, Pt single atoms show uniform and high-density single-atom dispersion at each temperature up to 1273 K after being held for 60 min. In addition, the stability of Pt single atoms can be confirmed by ex situ thermal annealing at 1073 K for 1 h in a furnace with Ar flow (Supplementary text, Figure S8). Since the HTHP process can utilize temperatures up to 3000 K (Supplementary text, Figure S2c), the HTHP process can even synthesize single atoms at higher temperatures. For example, the HTHP process can be used to synthesize single atoms at 1800 K and 2000 K (using a smaller 0.005 μmol / cm 2 Single atoms were synthesized with 200 Å loading and stable single-atom dispersions were observed by STEM and EXAFS measurements (Supplementary text, Figure 2 c and Figure S9).
[0087] For comparison, in the supplementary text Figure 2 In d, reports of single atoms synthesized using various methods are shown. Most wet chemical methods use mild temperatures, and the resulting single atoms are fragile under subsequent high-temperature annealing, especially when not properly bonded or coordinated to the substrate. Furnace heating or annealing at 1073-1173K can significantly improve the thermal stability of single atoms by producing strong and stable metal-substrate bonds through atom trapping and substrate anchoring. However, the much higher temperatures of the HTHP process exceed the ability of furnaces to heat and synthesize single atoms at 1500-2000K. In addition, higher temperature synthesis provides much shorter processing durations (e.g., <10 seconds) for ultrafast dynamics of single-atom dispersion and offers higher efficiency than low-temperature methods.
[0088] For the single-atom bond structure, the thermal stability induced by the HTHP process comes from the ability of the Pt-substrate bond to resist high-temperature annealing. Fig.10 Figures related to the single-atom bond structure are shown. Part (a) shows the Fourier transformed first shell model EXAFS fit at the Pt L3 edge of the Pt-1500K-10 cycle sample, showing a bond distance of The coordination number is 2.8. Part (b) shows the bond distances in the Pt-C3, Pt-N3 and Pt-O2C2 configurations calculated by density functional theory (DFT). Part (c) shows molecular dynamics (MD) simulations of single atom dispersion (I-III) and subsequent annealing (IV) at 1500K. Part (d) shows the identified Pt-Pt bonds (type 1) and Pt-C bonds (types 2-10) in the dispersed system. Part (e) shows the statistical distribution of bond configurations before (I) and after shock wave synthesis (III): weak bonds become strong Pt-C bonds. Part (f) shows the energy analysis of Pt atoms detached from the Pt-30 cluster by forming thermodynamically stable Pt-C bonds (type 10). Part (g) shows the time required for single atom dispersion, and part (h) shows the associated bond configurations at different synthesis temperatures. High temperature provides activation energy for bond formation, showing higher dispersion efficiency and more stable Pt-C bonds (types 5-10) at higher synthesis temperatures.
[0089] Continue to refer Fig.10 , the bond structure can be analyzed by fitting the EXAFS profile using the first-shell model to obtain the nearest-neighbor coordination number and the local structure of the Pt single atom (Supplementary Text, Table 1 and Fig. S10). Fig.10 Part (a) shows the EXAFS fitting of a single Pt atom at 1500K, showing The bond length is longer than that of the Pt-O bond reported in the literature. and Pt-N bonds is much shorter, but similar to the calculated The bond lengths of the Pt-C bonds are very consistent. In addition, based on this Pt-X3 bond model, the bond distances of Pt-C in Pt-C3, Pt-N in Pt-N3, and Pt-O in Pt-O2C2 can be calculated using density functional theory (DFT). The calculated Pt-C bond in the Pt-C3 configuration shows The bond distances of Pt-N and Pt-O are much larger ( Fig.10 , part (b)), which confirms the Pt-C bond structure in the sample.
[0090] The DFT results also show that the bond energy of the Pt-C bond is higher than that of the Pt-N bond under similar bond configurations (Pt-X3 and Pt-X4) (Supplementary text, Figure S11a). In addition, the charge density difference map further illustrates the difference between the Pt-C and Pt-N bonds: in the Pt-C bond, a large amount of charge transfer occurs between the Pt and C atoms, and the charge density is mainly concentrated in the center, which indicates a strong covalent bond nature; while in the Pt-N bond, the transferred electrons mainly circulate around the Pt and N atoms, which indicates an ionic bond (Supplementary text, Figure S11b). Therefore, compared with the Pt-N bond with similar bond configuration, the Pt-C bond exhibits higher binding energy and unique covalent properties.
[0091] To understand the atomic origin of the high temperature-induced dispersion and stabilization, molecular dynamics (MD) simulations were performed using the reaction force field (ReaxFF) potential (see Supplementary Text, SI Methods section). Defects on graphene consisted of randomly etched carbon vacancies to mimic the surface of CA-CNFs. Fig.10 Part (c) of Figure 3 depicts the dispersion of Pt clusters into single atoms as the heating cycle increases at 1500 K (from I to III), and also depicts the dispersion stability during thermal annealing at 1500 K (IV). The agglomeration and atomization of Pt atoms can be seen, and the atomization can only be stabilized when energetically favorable Pt-C bonds are formed ( Fig.10 Types 4-10, part (d)). Fig.10 Part (e) shows the evolution of the bond structure before and after the HTHP process at 1500K, where all the initial weak bonds (Pt-Pt and Pt-C of types 1-3) are transformed into strong Pt-C bonds (types 4-10) with higher binding energy, which clarifies the atomic origin of why single atoms synthesized by the HTHP process are more thermally stable than Pt clusters. The simulation clearly reproduces the synthesis process of the initial Pt clusters weakly attached to the substrate, but with more HTHP heating, the clusters break down into single atoms by forming strong Pt-C bonds that can withstand high temperature annealing. This also suggests that defects play a role in stabilizing single atoms and determining the dispersion density.
[0092] In this process, high temperature is used to provide sufficient activation energy for atomic dispersion and overcome the energy barrier of bond formation. For example, when a single Pt atom separated from a Pt-30 cluster forms a Pt-C bond, there is a kinetic energy barrier (e.g., 1.48 eV) that hinders dispersion, which can be overcome at high temperature ( Fig.10, part (f), and Supplementary Text, Fig. S12). HTHP dispersions at other temperatures can also be simulated: 500 K, 1000 K, 2000 K, and 2500 K (Supplementary Text, Fig. S13). Despite applying similar HTHP heating pulse patterns (on / off ratios and number of cycles), the temperatures of 500 K and 1000 K failed to sufficiently disperse the Pt clusters within a given repetitive cycle. In contrast, higher HTHP heating pulse temperatures have improved kinetics and achieve single-atom dispersion much faster, i.e., much higher dispersion efficiency ( Fig.10 , part (g). In addition, the Pt-C bond distribution in these single atoms at higher synthesis temperatures shows an increased proportion of more stable type 5-10 bonds, indicating improved thermal stability ( Fig.10 , part (h)). Therefore, the high temperature synthesis for single atom dispersion and stabilization provides activation energy, accelerates the dispersion process, and promotes the formation of more stable bonds. For clarity, it should be noted that the single atom dispersion achieved by the HTHP process may not disperse every cluster, and some clusters may remain after the HTHP process.
[0093] The above paragraphs describe the application of the HTHP process to synthesize Pt atoms. The HTHP synthesis process is generally applicable to other metals and substrates. In this HTHP synthesis process, the high temperature enables the atoms to disperse by forming stable metallic defect bonds, while the HTHP pulse heating helps to maintain the overall stability. Since the HTHP temperature is high enough compared to the thermal decomposition temperature of most metal precursors, the HTHP process can be used to generate single-atom dispersions of most metals, including Ru and Co single atoms on CA-CNF, which is Fig.11 and mentioned in Figure S14 of the supplementary text.
[0094] Fig.11 Figures and images related to the application of HTHP processes to various atoms and substrates and for various applications are shown. Part (a) shows Co single atoms synthesized on CA-CNF, which is confirmed by EXAFS curves and HAADF images (inset). Parts (b) and (c) show Pt single atoms (~0.5wt%) synthesized on C3N4 and TiO2 substrates by radiation and conducted shock wave synthesis. Part (d) is a light-off curve, and part (e) shows the Arrhenius plot of Pt single atoms before and after steam treatment at 973K for 4 hours for CO oxidation reaction, which shows stable performance after hydrothermal treatment. Part (f) shows the stable performance of Pt single atoms during CO oxidation at 493K for 50 hours. Part (g) shows high-temperature direct CH4 conversion of Pt single atoms and Pt IMP samples at 973K for 50 hours. Part (h) shows the reaction turnover frequency (TOF) compared with the literature.
[0095] In addition, continue to refer to Fig.11 , the shock wave approach can be extended to other substrates such as conductive reduced graphene oxide, semiconducting C3N4, and oxides such as TiO2, but using different heating methods (Supplementary text, Figure S15) and forming different bonds with the substrate (Supplementary text, Figure S16). Radiative HTHP heating can be used for powder samples by depositing the precursor-loaded powder underneath a carbon film that can be Joule heated in HTHP pulse mode. The high temperatures reached in the film also heat the C3N4 powder and lead to a high density of single-atom dispersions ( Fig.11 , part (b). In addition, HTHP pulse heating maintains the structural integrity of C3N4, which would otherwise be easily carbonized by prolonged heating (Supplementary Text, Figure S17). Non-contact radiative heating can also be scaled up for continuous production ( Figure 8 , and Fig. S18 in the Supplementary Text). As oxides have poor thermal conductivity for efficient radiative heating, Pt single atoms on TiO2 substrates can alternatively be achieved by depositing a thin layer (~2.5 nm) of TiO2 on the nanofibers in CA-CNF films by atomic layer deposition (Supplementary Text, Fig. S15c). HTHP pulse heating of CA-CNF films also heats the TiO2 layer by conductive heating and induces single-atom dispersion on TiO2 ( Fig.11 , part (c). These results demonstrate the general applicability of the HTHP process for the synthesis of thermally stable single-atom dispersions, suggesting great potential for scalable nanofabrication.
[0096] In order to test the stability of single atoms synthesized by HTHP, the partial H2O pressure was 10 -3 In situ hydrothermal testing of Pt single atoms on CA-CNF was performed in an environmental TEM (ETEM) at 400 mbar from 300 K to 773 K (the upper limit to avoid equipment corrosion), with each investigated temperature maintained for at least 30 min. As shown in Supplementary Text Figure S19, no nanoclusters appeared during the in situ measurements up to 773 K, indicating that the HTHP-synthesized single atoms are stable. In addition, the performance stability of Pt HT-SAs in CO oxidation reactions before and after hydrothermal treatment with 5% H2O at 973 K for 4 h can be confirmed, confirming the hydrothermal stability of Pt single atoms ( Fig.11 , part (d). Arrhenius diagram ( Fig.11, part (e), measured by kinetic studies) showed that the apparent reaction energies of the Pt single atom catalyst before and after steam pretreatment were very similar (50.7 kJ / mol vs. 53.2 kJ / mol). In addition, multiple cycles of CO oxidation measurements (Supplementary Text, Figure S20) and stability tests over 50 h at 493 K confirmed the high stability of Pt single atoms ( Fig.11 , part (f)).
[0097] Furthermore, it can be demonstrated that HTHP-synthesized single atoms can be used for reduction catalysis applications in direct methane conversion, where the single-atom catalysts show good performance in terms of coke resistance by preventing catalytic CC coupling. Control samples can be synthesized by a conventional impregnation (i.e., IMP) method using the same materials but thermally reduced at 573 K for 1 h (Supplementary Text, Fig. S21). Fig.11 Part (g) and Figure S22 in the Supplementary Text show that Pt IMP (T s =573K) and HTHP synthesized Pt single atoms (T s =1500K) at 973K for direct conversion of CH4 to various products (e.g., ethylene, ethane, propylene, propane, butenes, and benzene among the total hydrocarbon products). The product distribution shows high selectivity (>90%) for C2H4, C2H6, and C6H6 for Pt single atoms and no coke formation. In contrast, the Pt IMP sample shows severe coke formation even within the first hour of the reaction, which can be attributed to the continuous aggregation and agglomeration of Pt sites at high temperature (973K). Fig.11 Part (h) shows the excellent stability of HTHP-synthesized Pt single atoms in CH4 conversion, which has a stable turnover frequency (TOF) within 50 hours, which is in contrast to the rapid decline in TOF of the Pt IMP sample (due to its dispersion instability at high temperatures). Under similar conditions, the TOF of HTHP-synthesized single atoms is about 1000 times higher than the TOF of Pt nanoclusters supported on SiO2 catalysts reported in the literature, which indicates the high efficiency of single-atom catalysts. These practical results demonstrate that single atoms synthesized by the HTHP process have excellent thermal stability and great potential in catalytic applications.
[0098] Reference now Fig.12, showing graphs and images related to the formation of Pt-Ru diatoms on carbon nanofibers by HTHP process. Part (a) shows simulation work illustrating the dispersion of Pt-Ru into single atoms and the formation of bimetallic alloy. Part (b) shows a high-resolution image of the atomic dispersion of Pt-Ru diatoms without obvious segregation. Part (c) shows the X-ray absorption curves of Pt edge and Ru edge, indicating that the Pt-Ru in Pt-Ru diatoms is different from that of the metal foil alone, indicating the formation of Pt-Ru alloy bonds.
[0099] Fig.13 High-resolution atomic images of diatomic formation on carbon and C3N4 substrates by HTHP process are shown. Part (a) shows Pt-Co diatomic dispersion on carbon nanofibers (CNF). Part (b) shows Pt-Fe diatomic dispersion on reduced graphene oxide (RGO). Part (c) shows Pt-Co diatomic dispersion on C3N4 substrate. No cluster formation is clearly visible in each image / sample.
[0100] Thus, the present disclosure provides a high temperature heating pulse process for synthesizing single atom dispersions and polyatom dispersions on a substrate. The high temperature pulse is used to disperse clusters on a substrate and synthesize single atom dispersions. The single atoms are stabilized by defects on the substrate and by binding to the substrate. For clarity, it should be noted that the single atom dispersion achieved by the HTHP process may not disperse every cluster, and some clusters may remain after the HTHP process.
[0101] HTHP pulse configuration and mode are flexible, such as Figure 2 As shown, the high temperature (T 高 ), low temperature (T 低 ), heating duration (t 高 )、Cooling time(t 低 ), heating rate (R 加热 ), cooling rate (R 冷却 ) and the number of cycles (n) for the HTHP process.
[0102] The heating configuration is also flexible and may include, but is not limited to, direct Joule heating, conduction heating, radiation heating, microwave heating, laser heating, and / or plasma heating, such as Figure 3 , Figure 8 and Fig.14 Furthermore, different cooling processes may be implemented, including but not limited to cooling by radiation and conduction, active cooling by conduction and convection, and / or active cooling by physical or chemical transformation of absorbed heat.
[0103] The polyatomic groups / atomic alloys can be formed by sequentially / iteratively applying the HTHP process, which can achieve a single atomic dispersion of one species at a time. In such a process, the atoms in the polyatomic group can be different or the same, and can be pure metals or compounds thereof. The substrate can be a carbon-based material, a metal, a ceramic, a polymer, a composite material, an oxide and / or a combination thereof.
[0104] General atomic alloys with different element combinations can be synthesized by applying the HTHP process of different elements sequentially in each iteration. In this process, the single atoms can be any element that can be dispersed into atomic form (including their compound form). The substrate can be carbon-based materials, metals, ceramics, polymers, composites, oxides and / or combinations thereof.
[0105] The synthesized single atoms and multi-atom groups / atomic alloys can be used in many different applications, including but not limited to thermochemical, electrochemical and photochemical catalysis. In addition, the synthesis of single atoms and atomic alloys can be used for fundamental research on atom manipulation.
[0106] The embodiments disclosed herein are examples of the present disclosure and can be implemented in various forms. For example, although some embodiments herein are described as separate embodiments, each embodiment herein can be combined with one or more of the other embodiments herein. The specific structures and functional details disclosed herein should not be interpreted as restrictive, but as the basis of the claims, and as a representative basis for teaching those skilled in the art to use the present disclosure in a diversified manner with substantially any appropriate detailed structure. In the description of the entire drawings, similar reference numerals may refer to similar or identical elements.
[0107] The phrases “in one embodiment,” “in an embodiment,” “in various embodiments,” “in some embodiments,” or “in other embodiments” may each refer to one or more of the same or different embodiments according to the present disclosure. A phrase in the form “A or B” means “(A), (B), or (A and B).” A phrase in the form “at least one of A, B, or C” means “(A); (B); (C); (A and B); (A and C); (B and C); or (A, B, and C)”
[0108] It should be understood that the above description is only for illustrating the present invention. Those skilled in the art can design various substitutions and modifications without departing from the present disclosure. Therefore, the present disclosure is intended to cover all such substitutions, modifications and variations. The embodiments described with reference to the accompanying drawings are only used to show certain examples of the present disclosure. The embodiments described and illustrated herein are exemplary, and variations are expected to be within the scope of the present disclosure. The various embodiments disclosed herein can be combined in a manner not explicitly described herein, and these combinations are considered to be within the scope of the present disclosure. Other elements, steps, methods and techniques that are not substantially different from those in the above and / or appended claims are also intended to fall within the scope of the present disclosure.
Claims
1. A method for synthesizing an atomic dispersion, wherein include: arranging a loaded substrate, the loaded substrate comprising a substrate loaded with at least one of the following: a precursor of an element or a cluster of an element; applying at least one temperature pulse to the loaded substrate, wherein a pulse of the at least one temperature pulse applies a target temperature for a duration, wherein the target temperature is between 500 K and 4000 K, inclusive, and wherein the duration is between 1 millisecond and 1 minute, inclusive; After the pulse, a cooling cycle is maintained; and After at least one temperature pulse, single atoms of the element are provided dispersed on the substrate.
2. The method of claim 1 , further comprising, during the pulse: Dispersing the elements on the substrate at least partially monoatomically; and Atom-substrate bonds are formed to stabilize single atoms of the element on the substrate.
3. The method of claim 1, wherein each of the at least one temperature pulse applies a target temperature for a duration, the method further comprising: include: After each of the at least one temperature pulse, a cooling period is maintained.
4. The method of claim 3, further comprising, during each of the at least one temperature pulse: Dispersing the elements on the substrate at least partially monoatomically; and Atom-substrate bonds are formed to stabilize single atoms of the element on the substrate.
5. The method according to claim 1, further comprising: include: Perform at least one iteration of the following: loading the substrate with at least one of: a precursor of an additional element or a cluster of an additional element; applying at least one additional temperature pulse to the loaded substrate, wherein each of the at least one additional temperature pulse applies a target temperature for a duration; After each of the at least one additional temperature pulse, maintaining a cooling cycle; and providing a polyatomic dispersion of the element and the further element on the substrate after at least one further temperature pulse; Therein, the element and the further element are one of the following: the same element or different elements.
6. The method according to any one of claims 1 to 5, in, The element is one of Pt, Ru or Co.
7. The method according to any one of claims 1 to 5, in, The substrate includes at least one of a carbon-based material, a metal, a ceramic, a polymer, a composite material, or an oxide.
8. The method according to any one of claims 1 to 5, in, The substrate includes carbon, C 3 N 4 、TiO 2 or CO 2 At least one of the activated carbon nanofibers.
9. A system for synthesizing atomic dispersions, wherein include: A loaded substrate, the loaded substrate comprising a substrate loaded with at least one of the following: a precursor of an element or a cluster of an element; at least one heating element; and The controller is configured as: controlling at least one heating element to apply at least one temperature pulse to the loading substrate, wherein a pulse of the at least one temperature pulse applies a target temperature for a duration, wherein the target temperature is between 500 K and 4000 K, inclusive, and wherein the duration is between 1 millisecond and 1 minute, inclusive; and After the pulse, a cooling cycle is maintained. In this case, after at least one temperature pulse, single atoms of the element are dispersed on the substrate.
10. The system of claim 9, wherein the pulses cause at least partial monoatom dispersion of elements on the substrate and cause formation of atom-substrate bonds to stabilize monoatomic atoms on the substrate.
11. The system according to claim 9, in, The at least one heating element is configured to apply one of: direct Joule heating, conductive heating, radiative heating, microwave heating, laser heating, or plasma heating.
12. The system of claim 9, wherein the controller is configured to: controlling at least one heating element to apply a target temperature for a duration for each of the at least one temperature pulse, and After each of the at least one temperature pulse, a cooling cycle is maintained.
13. The system of claim 12, further comprising a conveyor carrying the loaded substrate, wherein the controller is configured to control the conveyor to convey the loaded substrate for heating by at least one heating element, wherein at least one heating element is controlled to apply at least one temperature pulse to the loading substrate include: controlling at least one heating element to maintain the temperature, and The speed of the conveyor is controlled to expose the plurality of portions of the loaded substrate to each of the at least one heating element for a duration.
14. The system of claim 13, wherein the at least one heating element comprises a plurality of heating elements, in, The plurality of heating elements are spaced apart such that a cooling cycle is achieved between each of the plurality of heating elements for conveyance of the plurality of portions of the loaded substrate on the conveyor.
15. The system according to claim 14, in, The loading substrate is a continuous strip, wherein the conveyor continuously conveys the loading substrate in a continuous strip.
16. The system according to claim 12, in, The loaded substrate is in one of a powder form or a droplet form, and the system further comprises a projection device for projecting the loaded substrate through at least one heating element, Wherein controlling at least one heating element to apply at least one temperature pulse to the loaded substrate comprises: controlling at least one heating element to maintain the temperature, and The delivery speed of the delivery device is controlled to expose the loaded substrate to each of the at least one heating element for a duration.
17. The system of claim 16, wherein the at least one heating element comprises a plurality of heating elements, in, The plurality of heating elements are spaced apart such that travel of the projected loaded substrate between each of the plurality of heating elements effects a cooling cycle.
18. A system according to any one of claims 9 to 17, in, The element is one of Pt, Ru or Co.
19. A system according to any one of claims 9 to 17, in, The substrate includes at least one of a carbon-based material, a metal, a ceramic, a polymer, a composite material, or an oxide.
20. The system according to any one of claims 9 to 17, in, The substrate includes carbon, C 3 N 4 、TiO 2 or CO 2 At least one of the activated carbon nanofibers.
Citation Information
Patent Citations
Metal / alpha-MoC1-x loaded monatomic dispersion catalyst, synthesis method and application thereof
CN107008479A
High-load precious metal monatomic catalyst as well as preparation method and application of high-load precious metal monatomic catalyst
CN108906113A