Methods for manufacturing wafers and methods for manufacturing stacked device chips
By removing defective devices from the wafer and embedding good devices, and forming a stacked device chip using laser processing and resin filling, the problem of reduced yield caused by defective devices is solved, and the yield of stacked device chips is improved.
Patent Information
- Application Number
- CN202111345633.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-11-18
- Filing Date
- 2021-11-15
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2041-11-15
AI Technical Summary
In the process of manufacturing stacked device chips, the presence of defective devices leads to a decrease in yield. Existing technologies are unable to effectively remove defective devices and ensure a high yield.
By removing defective device areas on the wafer and embedding good semiconductor devices in their locations, a laser beam is used to process along the spacer channel to form through holes and fill them with resin. Finally, the wafer is divided to form a stacked device chip.
It effectively removes defective components, improves the yield of stacked device chips, reduces the number of defective chips, and enhances the yield rate of the manufacturing process.
Smart Images

Figure CN114520164B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a method for manufacturing a wafer having multiple semiconductor devices and a method for manufacturing a stacked device chip having multiple semiconductor devices stacked on top of each other. Background Technology
[0002] In the manufacturing process of device chips, a wafer in which semiconductor devices are formed in multiple regions divided by a grid of spacers (pre-defined dividing lines) arranged in a lattice pattern is used. By dividing the wafer along the spacers, multiple device chips, each containing a semiconductor device, are obtained. These device chips are then assembled into various electronic devices such as mobile phones and personal computers.
[0003] In recent years, the technology for manufacturing device chips (stacked device chips) that have multiple semiconductor devices stacked on top of each other has been put into practical use. For example, multiple device chips are stacked and interconnected using through-silicon vias (TSVs). When using through-silicon vias, the wiring connecting the semiconductor devices can be shortened compared to wire bonding, thus enabling miniaturization of stacked device chips and increased processing speed.
[0004] As a method for manufacturing stacked device chips, a method called WoW (Wafer on Wafer) has been proposed. In this method, multiple wafers are stacked, and the semiconductor devices on each wafer are interconnected using electrodes formed in a manner that penetrates the stacked wafers, thereby forming a stacked wafer. Furthermore, the stacked wafers are diced along spacers, thereby manufacturing a stacked device chip.
[0005] However, in the manufacture of stacked device chips, the wafers used sometimes contain defective semiconductor devices. Furthermore, when the stacked wafers, formed by stacking wafers containing defective devices, are diced, stacked device chips containing defective devices are manufactured. When a portion of the semiconductor devices in a stacked device chip is defective, even if the other semiconductor devices are good, the entire stacked device chip is judged as defective (a defective chip). Therefore, in the manufacture of stacked device chips, the reduction in yield due to defective devices has a significant impact.
[0006] Therefore, before stacking multiple wafers, an inspection is performed to determine whether the semiconductor devices contained in each wafer are good or defective. Furthermore, the optimal combination of wafers used in the manufacturing of the stacked device chip is determined, for example, based on the number and arrangement of defective devices contained in each wafer (see Patent Document 1). This minimizes the number of stacked device chips containing defective devices, thereby suppressing a decrease in yield.
[0007] Patent Document 1: Japanese Patent Application Publication No. 2012-134334
[0008] As described above, even if a wafer contains defective devices, the number of stacked device chips (defective chips) containing defective devices can be minimized by determining the wafer combination based on the inspection results of semiconductor devices. However, when a wafer containing defective devices is used to manufacture stacked device chips, at least a certain number of defective chips will be produced. Therefore, there is a limit to how much the number of defective chips can be reduced. Summary of the Invention
[0009] The present invention was made in view of this problem, and its object is to provide a method for manufacturing a wafer capable of suppressing the reduction in yield of stacked device chips and a method for manufacturing a stacked device chip using the wafer.
[0010] According to one aspect of the present invention, a method for manufacturing a wafer is provided, wherein the method comprises the following steps: a wafer preparation step, preparing a wafer in which semiconductor devices are formed in multiple regions divided by multiple intersecting spacers; a removal step, separating a defective device region from the wafer, the defective device region including a semiconductor device identified as defective among a plurality of semiconductor devices formed in the wafer; and an embedding step, embedding a device chip having a good semiconductor device and capable of being embedded into a through-hole formed by separating the defective device region from the wafer into the through-hole, the good semiconductor device having the same function as the semiconductor device identified as defective, wherein in the removal step, a laser beam is irradiated along the spacers surrounding the semiconductor device identified as defective.
[0011] Furthermore, preferably, in this removal step, with the focal point of the laser beam of a wavelength that is transparent to the wafer positioned inside the wafer, the laser beam is irradiated along the spacer channel, thereby forming a modified layer along the spacer channel that functions as the starting point for separation of the defective device region. Alternatively, preferably, in this removal step, with the focal point of the laser beam of a wavelength that is absorbent to the wafer positioned inside the spacer channel, the laser beam is irradiated along the spacer channel, thereby removing the region of the wafer along the spacer channel. Alternatively, preferably, in this removal step, with the focal point of the laser beam of a wavelength that is absorbent to the wafer positioned inside the liquid column formed by spraying liquid toward the wafer, the laser beam is irradiated along the spacer channel via the liquid column, thereby removing the region of the wafer along the spacer channel.
[0012] In addition, the preferred method for manufacturing the wafer also includes the following grinding step: before performing the removal step, a protective member is attached to the first side of the wafer on which the semiconductor device is formed, and the second side of the wafer located on the opposite side of the first side is ground to thin the wafer to a specified thickness.
[0013] In addition, it is preferable that, in the removal step, the second side of the wafer, located opposite to the first side where the semiconductor device is formed, is ground, thereby exposing the processed area or the cracks that developed from the processed area by the laser beam on the second side of the wafer.
[0014] Furthermore, it is preferable that, in this removal step, an etching solution is provided to the processed area or the cracks that have developed from the processed area after being irradiated by the laser beam. Additionally, it is preferable that, in this removal step, a plasma-entrained gas is provided to the processed area or the cracks that have developed from the processed area after being irradiated by the laser beam.
[0015] In addition, the preferred method for manufacturing the wafer also includes the following steps: a resin filling step, in which resin is filled into the gap between the device chip and the wafer after the embedding step is performed; and a resin grinding step, in which the resin formed on the outside of the gap is ground after the resin filling step is performed.
[0016] Furthermore, according to another aspect of the present invention, a method for manufacturing a stacked device chip is provided, wherein the method comprises the following steps: a wafer preparation step, preparing a first wafer and a second wafer, wherein semiconductor devices are formed on the first wafer and the second wafer respectively in multiple regions divided by multiple intersecting spacers; a removal step, separating a defective device region from the first wafer, the defective device region comprising semiconductor devices identified as defective among the multiple semiconductor devices formed on the first wafer; and an embedding step, embedding a semiconductor device having good semiconductor devices and capable of... A device chip of the size embedded in a through-hole formed by separating the defective device region from the first wafer is embedded in the through-hole, the good semiconductor device having the same function as the semiconductor device identified as defective; a wafer stacking step, whereby the second wafer is stacked on the first wafer, thereby forming a stacked wafer; and a dicing step, whereby the stacked wafer is diced along the spacer, thereby forming a stacked device chip having a plurality of stacked semiconductor devices, in which a laser beam is irradiated along the spacer surrounding the semiconductor device identified as defective.
[0017] In one aspect of the wafer manufacturing method of the present invention, a defective device region containing a semiconductor device identified as a defective product is removed from the wafer, and a device chip having a good semiconductor device is embedded in the gap formed by removing the defective device region. This allows the manufacture of a wafer free of defective devices. Furthermore, by stacking wafers free of defective devices to form a stacked wafer and then dividing the stacked wafer, a stacked device chip free of defective devices can be manufactured. As a result, the yield reduction of the stacked device chip can be suppressed. Attached Figure Description
[0018] Figure 1 (A) is a three-dimensional view showing the wafer. Figure 1 (B) is a cross-sectional view showing the wafer. Figure 1 (C) is a three-dimensional view showing a semiconductor device.
[0019] Figure 2 This is a front view showing the grinding apparatus.
[0020] Figure 3 (A) is a cross-sectional view showing the wafer during the removal step. Figure 3 (B) is a perspective view showing a wafer with through holes formed.
[0021] Figure 4 (A) is a cross-sectional view showing a wafer being irradiated by a laser beam. Figure 4 (B) is a cross-sectional view showing a wafer with a modified layer formed thereon. Figure 4 (C) is a cross-sectional view showing a modified layer containing multiple modified regions.
[0022] Figure 5 (A) is a top view showing the path of the rounded quad shape. Figure 5 (B) is a top view showing a rectangular path. Figure 5 (C) is a top view showing multiple straight paths.
[0023] Figure 6 It is a cross-sectional view showing the wafer after grinding.
[0024] Figure 7 (A) is a cross-sectional view showing a wafer undergoing plasma etching. Figure 7 (B) is a cross-sectional view showing the wafer after plasma etching.
[0025] Figure 8 (A) is a cross-sectional view of the wafer during the pretreatment of the adhesive layer. Figure 8 (B) is a cross-sectional view of the wafer showing the separation of defective device areas.
[0026] Figure 9This is a cross-sectional view showing the ultrasonic irradiation unit.
[0027] Figure 10 (A) is a cross-sectional view showing a wafer being irradiated by a laser beam. Figure 10 (B) is a cross-sectional view showing a wafer with grooves formed.
[0028] Figure 11 (A) is a cross-sectional view showing a wafer fixed to a support substrate. Figure 11 (B) is a cross-sectional view showing the wafer after grinding.
[0029] Figure 12 (A) is a cross-sectional view showing a wafer being irradiated by a laser beam. Figure 12 (B) is a cross-sectional view showing the wafer fixed to the support substrate.
[0030] Figure 13 (A) is a cross-sectional view showing a wafer irradiated by a laser beam through a liquid column. Figure 13 (B) is a cross-sectional view showing the wafer fixed to the support substrate.
[0031] Figure 14 (A) is a cross-sectional view showing a wafer with a mask layer formed on it. Figure 14 (B) is a cross-sectional view showing a wafer undergoing plasma etching. Figure 14 (C) is a cross-sectional view showing the wafer after plasma etching.
[0032] Figure 15 (A) is a perspective view showing a wafer prepared for the device chip. Figure 15 (B) is a perspective view showing a wafer divided into multiple device chips.
[0033] Figure 16 This is a perspective view showing the wafer during the embedding process.
[0034] Figure 17 (A) is a cross-sectional view showing a wafer with embedded device chips. Figure 17 (B) is a top view showing the through hole.
[0035] Figure 18 (A) is a cross-sectional view of the wafer during plasma etching of the adhesive layer. Figure 18 (B) is a cross-sectional view of a wafer showing a portion of the adhesive layer removed. Figure 18 (C) is a cross-sectional view showing a wafer with a device chip embedded with an adhesive layer attached.
[0036] Figure 19 (A) is a cross-sectional view showing the wafer during the resin filling step. Figure 19(B) is a cross-sectional view showing the wafer during the resin grinding process.
[0037] Figure 20 It is a cross-sectional view showing the stacked wafers.
[0038] Figure 21 (A) is a cross-sectional view showing the stacked wafers during the dicing step. Figure 21 (B) is a cross-sectional view showing a stacked wafer divided into multiple stacked device chips.
[0039] Figure 22 (A) is a cross-sectional view showing a wafer with grooves formed by sandblasting. Figure 22 (B) is a cross-sectional view showing a wafer with grooves formed by water jet processing. Figure 22 (C) is a cross-sectional view showing a wafer with grooves formed by drilling.
[0040] Figure 23 (A) is a cross-sectional view showing a wafer fixed to a support substrate. Figure 23 (B) is a cross-sectional view showing the wafer after grinding.
[0041] Figure 24 (A) is a cross-sectional view showing a wafer with through-holes formed by sandblasting. Figure 24 (B) is a cross-sectional view showing a wafer with through-holes formed by water jet processing. Figure 24 (C) is a cross-sectional view showing a wafer with a through hole formed by drilling.
[0042] Figure 25 This is a cross-sectional view showing a wafer fixed to a support substrate.
[0043] Figure 26 This is a cross-sectional view showing a wafer undergoing plasma etching.
[0044] Figure 27 (A) is a top view showing the area processed by sandblasting or waterjet processing. Figure 27 (B) is a top view showing the area being processed by drilling.
[0045] Figure 28 (A) is a cross-sectional view showing a wafer being irradiated by a laser beam. Figure 28 (B) is a cross-sectional view showing a wafer with grooves formed.
[0046] Figure 29 This is a top view showing the path of the scanning laser beam.
[0047] Figure 30 (A) is a cross-sectional view showing a wafer fixed to a support substrate. Figure 30(B) is a cross-sectional view showing the wafer after grinding.
[0048] Figure 31 (A) is a cross-sectional view showing a wafer being irradiated by a laser beam. Figure 31 (B) is a cross-sectional view showing the wafer fixed to the support substrate.
[0049] Figure 32 It is a cross-sectional view showing the wafer held by the stage.
[0050] Figure 33 (A) is a cross-sectional view showing a wafer with defective device areas removed by sandblasting. Figure 33 (B) is a cross-sectional view showing the removal of defective device areas by water jet processing. Figure 33 (C) is a cross-sectional view showing a wafer in which defective device areas have been removed by drilling.
[0051] Figure 34 (A) is a cross-sectional view showing a wafer fixed to a support substrate. Figure 34 (B) is a cross-sectional view showing the wafer after grinding.
[0052] Figure 35 (A) is a cross-sectional view showing a wafer with through-holes formed by sandblasting. Figure 35 (B) is a cross-sectional view showing a wafer with through-holes formed by water jet processing. Figure 35 (C) is a cross-sectional view showing a wafer with a through hole formed by drilling.
[0053] Figure 36 This is a cross-sectional view showing a wafer fixed to a support substrate.
[0054] Figure 37 (A) is a top view showing the area processed by sandblasting or waterjet processing. Figure 37 (B) is a top view showing the area being processed by drilling.
[0055] Label Explanation
[0056] 11: Wafer; 11a: Front side (first side); 11b: Back side (second side); 11c: Defective device area; 11d: Through-hole (removal area); 13: Spacer (pre-defined dividing line); 15: Semiconductor device; 15a: Defective device; 17: Electrode; 19: Electrode (through-hole electrode, through-hole electrode); 21: Protective component; 23: Support substrate; 25: Adhesive layer; 27: Modified layer (modified layer); 27a: Modified area (modified area); 29: Crack; 31: Groove; 33: Protective component; 35: Cut; 37: Mask layer; 39: Mask; 51: Wafer; 51a: Front side (first side); 51b: Back side (second side); 53: Spacer (pre-defined dividing line); 55: Semiconductor device; 57: Electrode (through-hole electrode, through-hole electrode); 59: Device chip; 61: Gap; 63: Adhesive layer; 65: Resin; 71: Wafer; 71a: Front side (first side); 71b: Back side (second side); 73: Spacer (pre-defined dividing line); 75: Semiconductor device; 77: Electrode (through-hole electrode, through-hole electrode); 79: Stacked wafer; 81: Stacked device chip; 91: Protective layer; 93: Groove; 95: Through-hole; 97A, 97B, 9 7C, 97D: Area (processed area); 101: Groove (removal area); 103: Protective component; 105: Groove (removal area); 2: Grinding device; 4: Chuck table; 4a: Holding surface; 6: Grinding unit; 8: Spindle; 10: Mounting base; 12: Grinding wheel; 14: Base; 16: Grinding tool; 18: Nozzle; 20: Grinding fluid; 30A, 30B, 30C, 30D: Laser irradiation unit; 32A, 32B, 32C, 32D: Laser beam; 34A, 34B, 34C, 34D: Path; 36: Gas (etching gas); 38: Mask; 38a: 40: Opening; 42: Energy imparting unit; 44: Ultrasonic irradiation unit; 46: Container; 48: Ultrasonic transmitter; 50: Liquid column; 52: Holding stage; 52a: Holding surface; 52b: Opening; 54: Laser irradiation unit; 56: Laser beam; 58: Gas (etching gas); 60: Gas (etching gas); 62: Cutting tool; 70: Holding stage; 70a: Holding surface; 70b, 70c: Opening; 72: Sandblasting unit; 74: Abrasive material; 76: Water jet unit; 78: Liquid; 80: Drilling unit; 82: Drill bit; 84: Gas (etching gas). Detailed Implementation
[0057] (Implementation Method 1)
[0058] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. First, an example of a wafer structure that can be used in this embodiment will be described. Figure 1 (A) is a perspective view showing chip 11. Figure 1 (B) is a cross-sectional view showing wafer 11.
[0059] For example, wafer 11 is a silicon wafer formed in the shape of a disk, having a front side (first side) 11a and a back side (second side) 11b opposite to the front side 11a. The front side 11a and the back side 11b are formed to be substantially parallel to each other.
[0060] The wafer 11 is divided into multiple rectangular regions by multiple spacer lines (predetermined dividing lines) 13 arranged in a grid pattern in an intersecting manner. Furthermore, semiconductor devices 15 such as IC (Integrated Circuit), LSI (Large Scale Integration), LED (Light Emitting Diode), and MEMS (Micro Electro Mechanical Systems) are formed in the multiple regions divided by the spacer lines 13 on the front side 11a of the wafer 11.
[0061] Furthermore, there are no restrictions on the material, shape, structure, or size of the wafer 11. For example, the wafer 11 can be formed from semiconductors other than silicon (GaAs, InP, GaN, SiC, etc.), glass, ceramics, resin, metal, etc. Additionally, there are no restrictions on the type, quantity, shape, structure, size, or arrangement of the semiconductor devices 15.
[0062] Figure 1 (C) is a perspective view showing the semiconductor device 15. For example, the semiconductor device 15 has a plurality of electrodes 17 exposed on the front side of the semiconductor device 15 and connected to other wiring, electrodes, semiconductor devices, etc. In addition, bumps or other connecting electrodes may be formed on the front side of the electrodes 17.
[0063] Furthermore, multiple electrodes (through-hole electrodes, through-hole electrodes) 19 are embedded within the multiple regions divided by the spacers 13 of the wafer 11. The electrodes 19 are formed in a columnar shape along the thickness direction of the wafer 11 and are connected to the electrodes 17 of the semiconductor device 15. In addition, there are no restrictions on the material of the electrodes 19, and metals such as copper, tungsten, and aluminum can be used.
[0064] Electrodes 19 are formed from the semiconductor device 15 toward the back surface 11b of the wafer 11, and the length (height) of the electrodes 19 is less than the thickness of the wafer 11. Therefore, the electrodes 19 are not exposed on the back surface 11b of the wafer 11, and are embedded inside the wafer 11. In addition, an insulating layer (not shown) is provided between the wafer 11 and the electrodes 19 to insulate the wafer 11 from the electrodes 19.
[0065] When the wafer 11 is thinned by grinding or etching the back side 11b, the electrode 19 is exposed on the back side 11b. Furthermore, when multiple wafers 11 with electrodes 19 exposed on the back side 11b are stacked, a stacked wafer is obtained having multiple semiconductor devices 15 stacked in an overlapping manner. The stacked semiconductor devices 15 are connected to each other via the electrodes 19.
[0066] The stacked wafers are diced along the spacer 13 by machining, laser processing, or other methods. As a result, a device chip (stacked device chip) with multiple stacked semiconductor devices 15 is manufactured.
[0067] Additionally, sometimes the wafer 11 contains a defective semiconductor device 15 (a defective device). Figure 1 (A) and Figure 1 Example (B) shows a wafer 11 containing a defective device 15a. For example, the defective device 15a corresponds to a semiconductor device 15 that does not meet a predetermined electrical characteristic reference.
[0068] When wafers 11 containing defective devices 15a are stacked to form a stacked wafer and then the stacked wafer is diced, a stacked device chip containing defective devices 15a is manufactured. Furthermore, when a portion of the semiconductor devices 15 included in the stacked device chip is a defective device 15a, even if the other semiconductor devices 15 are good, the stacked device chip as a whole will be judged as a defective product (defective chip).
[0069] Therefore, in the wafer manufacturing method of this embodiment, the defective device 15a is removed from the wafer 11. Furthermore, a good semiconductor device 15 is embedded in the removal area (gap) formed in the wafer 11 by removing the defective device 15a. Thus, a wafer 11 free of the defective device 15a is manufactured. Hereinafter, specific examples of the wafer manufacturing method of this embodiment will be described.
[0070] First, a wafer 11 in which semiconductor devices 15 are formed respectively in multiple regions divided by multiple intersecting spacers 13 is prepared (see reference). Figure 1 (A) and Figure 1 (B) (Wafer Preparation Step). Furthermore, in order to stack multiple wafers to form a stacked wafer in subsequent processes, it is preferable to prepare at least two wafers in the wafer preparation step.
[0071] Next, the wafer 11 is thinned by grinding (grinding step). In the grinding of the wafer 11, for example, a grinding apparatus is used. Figure 2This is a front view showing the grinding apparatus 2. The grinding apparatus 2 has a chuck stage 4 for holding the wafer 11 and a grinding unit 6 for grinding the wafer 11.
[0072] The upper surface of the chuck stage 4 forms a flat holding surface 4a for holding the wafer 11. The holding surface 4a is connected to a suction source (not shown) such as an ejector via a flow path (not shown) formed inside the chuck stage 4. Furthermore, a moving mechanism (not shown) is connected to the chuck stage 4 to move the chuck stage 4 in the horizontal direction. The moving mechanism may be a ball screw type moving mechanism or a rotary table that supports and rotates the chuck stage 4. Additionally, a rotary drive source (not shown), such as an electric motor, is connected to the chuck stage 4 to rotate the chuck stage 4 about a rotation axis that is approximately parallel to the vertical direction (up and down direction).
[0073] A grinding unit 6 is arranged above the chuck table 4. The grinding unit 6 has a cylindrical spindle 8 arranged along the vertical direction. A disc-shaped mounting base 10 made of metal or the like is fixed to the front end (lower end) of the spindle 8. In addition, a rotation drive source (not shown) such as an electric motor is connected to the base end (upper end) of the spindle 8 to rotate the spindle 8.
[0074] A grinding wheel 12 for grinding the wafer 11 is mounted on the lower surface of the mounting base 10. The grinding wheel 12 has an annular base 14, which is formed of a metal such as stainless steel or aluminum and has a diameter approximately the same as that of the mounting base 10. A plurality of grinding tools 16 are fixed on the lower surface of the base 14. For example, the plurality of grinding tools 16 are formed in the shape of cuboids and are arranged at approximately equal intervals along the outer periphery of the base 14.
[0075] The grinding wheel 12 rotates about a rotation axis that is substantially parallel to the vertical direction, powered by a rotation drive source transmitted through the spindle 8 and the mounting base 10. Additionally, a ball screw-type moving mechanism (not shown) is connected to the grinding unit 6 to move the grinding unit 6 up and down in the vertical direction. Furthermore, nozzles 18 are provided near the grinding unit 6 to supply grinding fluid 20, such as pure water, to the wafer 11 held by the chuck table 4 and the multiple grinding wheels 16.
[0076] The back side 11b of, for example, wafer 11 is ground using the grinding apparatus 2. In this case, a protective member 21 is first attached to the front side 11a of wafer 11 on which the semiconductor device 15 is formed. Thus, the semiconductor device 15 is protected by being covered by the protective member 21.
[0077] As the protective component 21, a circular strip (protective strip) comprising a film-like substrate and an adhesive layer (paste layer) on the substrate can be used. For example, the substrate is formed of resins such as polyolefin, polyvinyl chloride, and polyethylene terephthalate, and the adhesive layer is formed of epoxy, acrylic, or rubber adhesives. Alternatively, as the adhesive layer, a UV-curing resin that hardens upon exposure to ultraviolet light can be used.
[0078] Furthermore, the wafer 11 is held by the chuck stage 4. Specifically, the wafer 11 is arranged on the chuck stage 4 with its front side 11a (the side of the protective member 21) facing the holding surface 4a and its back side 11b exposed upwards. When a negative pressure from an attraction source is applied to the holding surface 4a in this state, the front side 11a of the wafer 11 is attracted and held by the chuck stage 4 through the protective member 21.
[0079] Next, the chuck table 4 is moved to a position below the grinding unit 6. While the chuck table 4 and the grinding wheel 12 are rotated in predetermined directions at predetermined speeds, the grinding wheel 12 is lowered toward the chuck table 4. At this time, the descent speed of the grinding wheel 12 is adjusted so that the grinding tool 16 presses against the wafer 11 with appropriate force.
[0080] When the grinding tool 16 contacts the back side 11b of the wafer 11, it scrapes the back side 11b of the wafer 11. This grinding thins the back side 11b of the wafer 11. Grinding stops when the wafer 11 is thinned to a predetermined thickness. Then, the protective member 21 is peeled off from the wafer 11 and removed.
[0081] Furthermore, before or after the grinding step, an inspection is performed on the semiconductor device 15 included in the wafer 11 to determine whether the semiconductor device 15 is a good or defective product. During the inspection of the semiconductor device 15, for example, a metal probe is brought into contact with the electrode 17 exposed on the front side of the semiconductor device 15 to measure (probe) the electrical characteristics of the semiconductor device 15. Then, based on whether the measured electrical characteristics meet a predetermined standard, the semiconductor device 15 is determined to be a good or defective product.
[0082] When a defective semiconductor device 15 (defective device 15a) is included in the wafer 11, the semiconductor device 15 is identified as defective through inspection. Furthermore, the location of the semiconductor device 15 identified as defective is recorded.
[0083] Next, the defective device region of the semiconductor device 15 (defective device 15a) that is identified as a defective product among the plurality of semiconductor devices 15 formed on the wafer 11 is removed from the wafer 11 (removal step). Figure 3 (A) is a cross-sectional view showing the wafer 11 during the removal step.
[0084] For example, in the removal step, the wafer 11 is removed along the four spacers 13 surrounding the defective device 15a. This separates the cuboid defective device region 11c containing the defective device 15a from the wafer 11. Furthermore, a cuboid through-hole (removal region) 11d is formed at the location of the defective device region 11c on the wafer 11, extending from the front side 11a to the back side 11b of the wafer 11.
[0085] Figure 3 (B) is a perspective view showing a wafer 11 with a through-hole 11d formed thereon. By removing the defective device region 11c, a wafer 11 without the defective device 15a is obtained. Furthermore, when the grinding step described above is performed before the removal step (see [reference]), Figure 2 When the wafer 11 is thinned, the defective device region 11c can be easily removed from the wafer 11. However, the grinding step can be omitted if it does not hinder the removal of the defective device region 11c.
[0086] Various methods can be used to remove the defective device region 11c. For example, a laser beam can be irradiated along the spacer 13 surrounding the defective device 15a, thereby separating the defective device region 11c from the wafer 11. Hereinafter, an example of performing laser processing on the wafer 11 in the removal step will be described.
[0087] Figure 4 (A) is a cross-sectional view showing the wafer 11 being irradiated by the laser beam 32A. In the removal step, the front side 11a of the wafer 11 is first fixed to a support substrate 23 that supports the wafer 11. For example, the support substrate 23 is a plate-shaped component made of silicon, glass, ceramic, etc., and the front side 11a of the wafer 11 is fixed to the support substrate 23 by means of an adhesive layer 25. Thus, the wafer 11 is supported by the support substrate 23 with the back side 11b exposed.
[0088] There are no restrictions on the material of the adhesive layer 25, and it can be appropriately selected according to the materials of the wafer 11 and the support substrate 23. For example, the adhesive layer 25 can be made of a thermosetting resin that hardens by heating, a thermoplastic resin that softens by heating, or an ultraviolet-curing resin that hardens by ultraviolet radiation.
[0089] Alternatively, the adhesive layer 25 can be a sheet (thermo-pressed sheet) that can be fixed to the wafer 11 and the support substrate 23 by heating and pressurizing. For example, the adhesive layer 25 is a soft sheet formed of a thermoplastic resin with a melting point lower than that of the wafer 11 and the support substrate 23, and does not contain an adhesive (paste layer). When the wafer 11 is pressed against the support substrate 23 while the thermo-pressed sheet is heated, the thermo-pressed sheet is tightly attached to the wafer 11 and the support substrate 23. Thus, the wafer 11 is fixed to the support substrate 23. Specific examples of sheets include polyolefin (PO) sheets and polyester (PE) sheets.
[0090] Polyolefin sheets are sheets formed from polymers synthesized using olefins as monomers. Examples of polyolefin sheets include polyethylene sheets, polypropylene sheets, and polystyrene sheets. Additionally, sheets formed from copolymers of propylene and ethylene, or sheets formed from olefin-based elastomers, can also be used.
[0091] Polyester sheets are sheets formed from polymers synthesized using dicarboxylic acids (compounds having two carboxyl groups) and glycols (compounds having two hydroxyl groups) as monomers. Examples of polyester sheets include polyethylene terephthalate sheets and polyethylene naphthalate sheets. Alternatively, polyethylene terephthalate sheets, polybutylene terephthalate sheets, or polybutylene naphthalate sheets can also be used.
[0092] Furthermore, when fixing the wafer 11 to the support substrate 23 using the adhesive layer 25, it is preferable not to firmly bond the adhesive layer 25 to the wafer 11 and the support substrate 23, but rather to temporarily fix the wafer 11 to the support substrate 23. Therefore, when separating the defective device region 11c from the wafer 11 in subsequent processes (see reference...), Figure 8 (B)), the defective device area 11c is easily peeled off from the adhesive layer 25.
[0093] For example, if the adhesive layer 25 is an adhesive formed of thermosetting resin, the wafer 11 is fixed to the support substrate 23 by a low-temperature or short-time heating treatment compared to the case where the thermosetting resin is completely fixed to the wafer 11 and the support substrate 23. Alternatively, if the adhesive layer 25 is an adhesive formed of thermoplastic resin, the wafer 11 is fixed to the support substrate 23 by heating the thermoplastic resin at a predetermined temperature until the thermoplastic resin softens.
[0094] When the adhesive layer 25 is an adhesive formed of UV-curable resin, the wafer 11 is fixed to the support substrate 23 without heat treatment of the UV-curable resin. Alternatively, when the adhesive layer 25 is a thermosetting bond, the wafer 11 is fixed to the support substrate 23 by a low-temperature or short-time heat treatment compared to the case where the thermosetting bond is completely fixed to the wafer 11 and the support substrate 23.
[0095] Alternatively, a strip made of resin or the like can be attached to the front side 11a of the wafer 11 instead of the support substrate 23. Examples of the strip's structure and material are similar to those of the protective component 21 (see [reference]). Figure 2 )same.
[0096] Next, laser processing is performed on the wafer 11. A laser processing apparatus is used for the laser processing of the wafer 11. The laser processing apparatus includes a chuck stage (not shown) for holding the wafer 11 and a laser irradiation unit 30A for irradiating the wafer 11 with a laser beam 32A. The laser irradiation unit 30A includes a laser oscillator that oscillates a laser beam of a predetermined wavelength and a converging lens (focusing lens) that converges the laser beam emitted from the laser oscillator.
[0097] The irradiation conditions of the laser beam 32A are set such that the area of the wafer 11 irradiated by the laser beam 32A is modified (degraded) through multiphoton absorption. Specifically, the wavelength of the laser beam 32A is set such that at least a portion of the laser beam 32A passes through the wafer 11. That is, the laser irradiation unit 30A irradiates the wafer 11 with a wavelength that is transmissible to the wafer 11. In addition, other irradiation conditions of the laser beam 32A (output, pulse width, spot diameter, repetition frequency, etc.) are also set to appropriately modify the wafer 11.
[0098] Furthermore, with the focal point of the laser beam 32A positioned inside the wafer 11, the laser beam 32A is irradiated along the four spaced paths 13 surrounding the defective device 15a. Additionally, the laser beam 32A only needs to irradiate in a manner surrounding the defective device 15a, and the specific scanning path of the laser beam 32A can be appropriately set.
[0099] exist Figure 5 (A) Figure 5 An example of the scanning path of laser beam 32A is shown in (C). Figure 5 (A) is a top view showing path 34A of the rounded quadrilateral shape. Figure 5 (B) is a top view showing the rectangular path 34B. Figure 5 (C) is a top view showing multiple straight paths 34C. Paths 34A, 34B, and multiple paths 34C are respectively set to overlap with the spacer 13.
[0100] For example, laser beam 32A scans around defective device 15a along a roughly rectangular path 34A with rounded corners. Alternatively, laser beam 32A can scan along a rectangular path 34B surrounding defective device 15a. Furthermore, when laser beam 32A scans along path 34A or path 34B, laser beam 32A continuously irradiates wafer 11 around defective device 15a (in a single, continuous stroke).
[0101] Furthermore, the laser beam 32A can scan along four straight paths 34C, which are along four spaced channels 13 surrounding the defective device 15a. Moreover, the paths 34C are not connected to each other, and the laser beam 32A irradiates the defective device 15a intermittently.
[0102] Figure 4 (B) is a cross-sectional view showing a wafer 11 with a modified layer (modified layer) 27 formed thereon. When a laser beam 32A is irradiated along the spacer channel 13 surrounding the defective device 15a, the wafer 11 is modified by multiphoton absorption, forming a modified layer 27 inside the wafer 11 along the spacer channel 13. Furthermore, the region with the modified layer 27 is more brittle than other regions of the wafer 11. Therefore, for example, when an external force is applied to the wafer 11, the wafer 11 breaks along the modified layer 27. That is, the modified layer 27 functions as the starting point (beginning) for the separation of the defective device region 11c.
[0103] Especially when along Figure 5 The path 34A shown in (A) or Figure 5 When the laser beam 32A is irradiated along path 34C as shown in (C), it is confirmed that unexpected irregular cracks (fissures) at the four corners (corners) of paths 34A and 34C are effectively suppressed. In this case, the modified layer 27 formed at the four corners of paths 34A and 34C functions correctly as a separation starting point, thereby facilitating the accurate separation of the defective device region 11c.
[0104] Alternatively, the modified layer 27 can be formed by irradiating the laser beam 32A multiple times along each spacer channel 13 while changing the height position of the focusing point of the laser beam 32A. In this case, the modified layer 27 is composed of multiple modified regions formed along the thickness direction of the wafer 11.
[0105] Figure 4 (C) is a cross-sectional view showing a modified layer 27 containing multiple modified regions (modified regions) 27a. For example, multiple modified regions 27a are formed along each spacer 13 at different depths in the thickness direction of the wafer 11 inside the wafer 11.
[0106] Furthermore, multiple modified regions 27a can be formed in a top-view non-overlapping manner. Specifically, such as... Figure 4 As shown in (C), for the multiple modified regions 27a, the modified region 27a formed on the back side 11b of the wafer 11 is formed at a position that is further away from the defective device 15a in the horizontal direction (the direction perpendicular to the thickness direction of the wafer 11). In this case, a modified layer 27 is formed that is inclined relative to the thickness direction of the wafer 11 (see Figure 1). Figure 4 (B)) In subsequent processes, the defective device region 11c can be easily separated from the wafer 11 (see reference). Figure 8 (B) However, there are no restrictions on the shape of the modified layer 27, which can be formed parallel to the thickness direction of the wafer 11.
[0107] Next, by grinding the back side 11b of the wafer 11, the processed area (modified layer 27) irradiated by the laser beam 32A, or cracks (fissures) developing from the processed area (modified layer 27), are exposed on the back side 11b of the wafer 11. In the grinding of the wafer 11, for example, using... Figure 2 The grinding device 2 shown.
[0108] The grinding tool 16 is brought into contact with the back side 11b of the wafer 11 held by the chuck stage 4, thereby grinding the back side 11b of the wafer 11. Furthermore, for example, the wafer 11 is ground and thinned until the modified layer 27 is exposed on the back side 11b of the wafer 11.
[0109] Figure 6 This is a cross-sectional view showing the ground wafer 11. When the grinding wheel 16 (see reference) is used... Figure 2 When the wafer 11 is pressed down and ground, an external force (pressure) is applied to the wafer 11, causing the wafer 11 to fracture along the modified layer 27. In addition, cracks (fissures) 29 generated in the modified layer 27 develop and reach the front side 11a of the wafer 11. As a result, the defective device region 11c is separated from the wafer 11.
[0110] Furthermore, the cracks 29 that develop from the modified layer 27 to the front side 11a of the wafer 11 sometimes also occur when the modified layer 27 is formed by irradiation with the laser beam 32A (see reference). Figure 4 (A) and Figure 4 (B) is generated. Specifically, by appropriately setting the irradiation conditions of the laser beam 32A and the position where the modified layer 27 is formed, the crack 29 generated simultaneously with the formation of the modified layer 27 can reach the front side 11a of the wafer 11.
[0111] Furthermore, it is preferable to perform an etching process on the wafer 11 after grinding. For example, plasma etching is performed on the wafer 11. In plasma etching, a plasma processing apparatus is used. The plasma processing apparatus includes: a chuck stage having a holding surface for holding the wafer 11; and a chamber (processing chamber) for housing the chuck stage.
[0112] Figure 7 (A) is a cross-sectional view showing a wafer 11 undergoing plasma etching. During plasma etching, the wafer 11 is held in place by a chuck stage, the chamber is sealed, and etching gas (etching gas) 36 is supplied into the chamber. Furthermore, the plasma processing apparatus uses a high-frequency voltage to ionize the gas 36 within the chamber, creating a plasma state containing ions and free radicals. Thus, the plasma-ionized gas 36 is supplied to the wafer 11.
[0113] For example, if wafer 11 is a silicon wafer, fluorine-based gases such as CF4 and SF6 are used as gas 36. However, the composition of gas 36 can be appropriately selected according to the material of wafer 11. Furthermore, the plasma-state gas 36 acts on wafer 11 to perform plasma etching on wafer 11.
[0114] Figure 7 (B) is a cross-sectional view showing the wafer 11 after plasma etching. When plasma-ionized gas 36 is supplied to the back side 11b of the wafer 11, the gas 36 penetrates the modifier layer 27 and the crack 29, etching the interior of the modifier layer 27 and the crack 29. As a result, the gap between the wafer 11 and the defective device region 11c is widened, reliably separating the defective device region 11c from the wafer 11.
[0115] However, gas 36 can also be plasma-ionized outside the chamber and then supplied to the chamber via a metal supply tube. In this case, as the plasma-ionized gas 36 passes through the supply tube, the ions contained in the gas are adsorbed onto the inner wall of the supply tube and do not easily reach the chamber. As a result, gas 36 with a high proportion of free radicals is introduced into the chamber and supplied to the wafer 11. Gas 36 with a high proportion of free radicals can easily enter narrow areas within the wafer 11, thus facilitating etching of the modified layer 27 and the interior of the crack 29.
[0116] Furthermore, the type of etching process is not limited to plasma etching. For example, wet etching can also be performed on the back side 11b of the wafer 11 by providing an etching solution. Specifically, when the wafer 11 is a silicon wafer, an etching solution containing potassium hydroxide (KOH), tetramethylammonium hydroxide (TMAH), etc., is provided to the wafer 11. The etching solution penetrates into the modified layer 27 and the crack 29, thereby etching the interior of the modified layer 27 and the crack 29, and the modified layer 27 and the crack 29 expand.
[0117] Additionally, the modified layer 27 (see reference) formed by irradiation with laser beam 32A Figure 4 When electrode 19 is located on the back side 11b of wafer 11, it is preferable to grind and thin wafer 11 until the modifier layer 27 is completely removed. In this case, wafer 11 is obtained that does not contain modifier layer 27 but only has cracks 29 that have developed from modifier layer 27. When modifier layer 27 is removed from wafer 11 in advance, the bending strength (flexural strength) of the device chip obtained by finally dividing wafer 11 is prevented from decreasing.
[0118] After removing the modified layer 27 from the wafer 11 as described above, the crack 29 is exposed on the back side 11b of the wafer 11 by grinding, thus separating the defective device region 11c from the wafer 11. Furthermore, plasma gas 36 or etching solution is provided to the interior of the crack 29 to propagate the crack 29.
[0119] Additionally, when the modified layer 27 is formed by irradiation with laser beam 32A (see reference) Figure 4 (A) and Figure 4 (B)), or when grinding the back side 11b of the wafer 11 (refer to) Figure 6 Sometimes, cracks (fissures) develop from the modified layer 27 toward the back side 11b of the wafer 11. In this case, when the crack is exposed on the back side 11b of the wafer 11 by grinding the wafer 11, the defective device region 11c is broken off from the wafer 11.
[0120] Next, the defective device region 11c is removed from the wafer 11. Specifically, the defective device region 11c is peeled off from the adhesive layer 25 and picked up, thereby separating the defective device region 11c from the wafer 11.
[0121] When separating the defective device region 11c from the wafer 11, it is preferable to first perform a process (pre-treatment) to locally reduce the adhesive strength of the adhesive layer 25. For example, a solution is provided to the adhesive layer 25 using the modified layer 27 and the crack 29, thereby locally reducing the adhesive strength of the adhesive layer 25 or locally removing the adhesive layer 25.
[0122] Furthermore, when the adhesive layer 25 is formed of a material whose adhesive strength is reduced by applying a specified amount of energy (heating, electromagnetic wave irradiation, etc.), the adhesive strength of the adhesive layer 25 can be reduced by applying energy to the adhesive layer 25. For example, when the adhesive layer 25 is an adhesive formed of thermoplastic resin, the adhesive strength of the adhesive layer 25 can be reduced by heating the adhesive layer 25. Additionally, when the adhesive layer 25 is an adhesive formed of ultraviolet-curing resin, the adhesive strength of the adhesive layer 25 can be reduced by irradiating the adhesive layer 25 with ultraviolet light.
[0123] Alternatively, as the adhesive layer 25, a strip comprising a film-like substrate, a thermally foamed layer disposed on one side of the substrate, and an adhesive layer disposed on the other side of the substrate may be used. This thermally foamed layer is formed by containing an expandable material in the adhesive that expands upon heating.
[0124] As adhesives for the thermally expanded foam layer, acrylic adhesives, rubber adhesives, vinyl alkyl ether adhesives, silicone adhesives, polyester adhesives, polyamide adhesives, polyurethane adhesives, etc., can be used. Furthermore, as expanding materials for the thermally expanded foam layer, microspheres that expand upon heating (thermally expandable microspheres), foaming materials that foam upon heating, etc., can be used.
[0125] Thermally expandable microspheres are constructed by encapsulating a substance that expands upon heating within elastic microcapsules. Examples of substances that expand upon heating include propane, propylene, and butene. A commercially available example of a belt containing thermally expandable microspheres is REVALPHA (registered trademark) manufactured by Nitto Denko Corporation. Furthermore, as foaming materials that foam upon heating, inorganic foaming agents such as ammonium carbonate, ammonium bicarbonate, sodium bicarbonate, ammonium nitrite, sodium borohydride, and azide compounds, or various organic foaming agents, can be used.
[0126] The aforementioned strip is attached to the wafer 11 and the support substrate 23 in such a manner that the thermally foamed layer side contacts the wafer 11 and the adhesive layer side contacts the support substrate 23. Furthermore, when the strip is heated, the expansion material contained in the thermally foamed layer expands in the heated area of the strip, forming unevenness, and the adhesive force of the strip to the wafer 11 decreases.
[0127] Figure 8 (A) is a cross-sectional view showing the wafer 11 when the adhesive layer 25 is pre-processed. For example, a mask 38 is fixed on the side of the support substrate 23 opposite to the side (upper surface) where the wafer 11 is fixed (lower surface). In addition, the mask 38 has an opening 38a that extends vertically through the mask 38, and is fixed in such a way that the opening 38a overlaps with the defective device region 11c.
[0128] Furthermore, an energy imparting unit 40 for imparting energy to the adhesive layer 25 is disposed below the support substrate 23. The energy imparting unit 40 imparts energy to the adhesive layer 25 through the opening 38a of the mask 38. In addition, the type of energy imparted to the adhesive layer 25 from the energy imparting unit 40 is selected according to the properties of the adhesive layer 25.
[0129] For example, if the adhesive layer 25 includes a strip of adhesive or thermally foamed layer formed of thermoplastic resin, a heater is used as the energy application unit 40. Additionally, an insulating component is used as the mask 38. Heat is applied from the energy application unit 40 to the region of the support substrate 23 that overlaps with the opening 38a of the mask 38, transferring heat from the support substrate 23 to the adhesive layer 25. This locally heats the region of the adhesive layer 25 that overlaps with the opening 38a of the mask 38.
[0130] Furthermore, when the adhesive layer 25 is an adhesive formed from an ultraviolet-curable resin, an ultraviolet light source (lamp) is used as the energy-applying unit 40. Additionally, a component that is translucent to ultraviolet light is used as the support substrate 23, and a component that is light-shielding to ultraviolet light is used as the mask 38. Ultraviolet light is then irradiated onto the adhesive layer 25 from the energy-applying unit 40 through the opening 38a of the mask 38 and the support substrate 23. Thus, ultraviolet light is locally irradiated onto the area of the adhesive layer 25 that overlaps with the opening 38a of the mask 38.
[0131] When energy is applied to the adhesive layer 25 from the energy application unit 40, the adhesive force in the area of the adhesive layer 25 that overlaps with the defective device region 11c is locally reduced. As a result, the defective device region 11c can be easily peeled off from the adhesive layer 25.
[0132] Figure 8 (B) is a cross-sectional view of the wafer 11 during the separation of the defective device region 11c. After pre-processing the wafer 11 as required, the defective device region 11c is held so that it leaves the wafer 11. Thus, the defective device region 11c is peeled off from the adhesive layer 25 and removed from the wafer 11.
[0133] In addition, when separating the defective device region 11c from the wafer 11, the separation of the defective device region 11c can be assisted by irradiating the wafer 11 or the support substrate 23 with ultrasonic waves. Figure 9 This is a cross-sectional view showing the ultrasonic irradiation unit 42.
[0134] The ultrasonic irradiation unit 42 has a box-shaped container 44 formed in the shape of a cuboid. A liquid 46, such as pure water, is stored inside the container 44. Furthermore, an ultrasonic transmitter 48 that emits ultrasonic waves is installed inside the container 44.
[0135] The wafer 11, with the modified layer 27 and cracks 29 formed thereon, is placed in the container 44 by immersing it in the liquid 46. At this time, the wafer 11 is arranged, for example, with the support substrate 23 facing the ultrasonic transmitter 48. When the ultrasonic transmitter 48 transmits ultrasonic waves in this state, the ultrasonic waves propagate through the liquid 46 as a medium and reach the support substrate 23, thereby imparting ultrasonic vibration to the support substrate 23.
[0136] Even when the wafer 11 has not fully fractured along the modified layer 27 and the crack 29, when ultrasonic vibration is applied to the support substrate 23, the vibration of the support substrate 23 promotes the fracture of the wafer 11. Furthermore, the vibration of the support substrate 23 weakens the adhesion between the defective device region 11c and the adhesive layer 25. As a result, the defective device region 11c is easily separated from the wafer 11. Additionally, ultrasonic waves can also be locally applied to areas in the support substrate 23 that overlap with the defective device region 11c.
[0137] This separates the defective device region 11c from the wafer 11. Furthermore, a through-hole 11d is formed at the location where the defective device region 11c originally existed on the wafer 11, penetrating the wafer 11 along the thickness direction (see reference). Figure 8 (B)
[0138] Furthermore, as an example, the method of breaking the wafer 11 along the modified layer 27 and crack 29 formed by irradiation by the laser beam 32A has been described above. However, the laser processing performed on the wafer 11 is not limited to the formation of the modified layer 27 and crack 29. For example, in the removal step, the defective device region 11c can also be separated from the wafer 11 by performing an ablation process on the wafer 11.
[0139] Figure 10 (A) is a cross-sectional view showing the wafer 11 irradiated by the laser beam 32B. When performing an ablation process on the wafer 11, a laser irradiation unit 30B is used to irradiate the wafer 11 with the laser beam 32B. Furthermore, the structure of the laser irradiation unit 30B is similar to that of the laser irradiation unit 30A (see reference 30A). Figure 4 (A) is the same.
[0140] However, the irradiation conditions of the laser beam 32B are set such that the area of the wafer 11 irradiated by the laser beam 32B is removed by an ablation process. Specifically, the wavelength of the laser beam 32B is set such that at least a portion of the laser beam 32B is absorbed by the wafer 11. That is, the laser irradiation unit 30B irradiates the laser beam 32B with a wavelength that is absorbent to the wafer 11. In addition, other irradiation conditions of the laser beam 32B are also set to appropriately perform an ablation process on the wafer 11.
[0141] For example, laser beam 32B irradiates the front side 11a of wafer 11. Specifically, wafer 11 is held by the chuck stage (not shown) of the laser processing apparatus with its front side 11a exposed. Furthermore, with the focal point of laser beam 32B positioned on the spacer 13 of wafer 11, laser beam 32B is irradiated along the four spacer 13 surrounding defective device 15a. Moreover, there are no restrictions on the scanning path of laser beam 32B. For example, along... Figure 5(A) and Figure 5 The path 34A or path 34B shown in (B) scans the laser beam 32B.
[0142] Figure 10 (B) is a cross-sectional view showing a wafer 11 with the groove 31 formed thereon. When a laser beam 32B is irradiated along the four spacers 13 surrounding the defective device 15a, the area along the spacers 13 on the front side 11a of the wafer 11 is removed by an ablation process. As a result, a rectangular groove 31 is formed on the front side 11a of the wafer 11 along the spacers 13 in plan view.
[0143] Furthermore, there are no restrictions on the shape of the groove 31. For example, the groove 31 can be formed with a constant width in the thickness direction of the wafer 11, or it can be formed as follows: Figure 10 As shown in (B), the width increases as it approaches the back side 11b of the wafer 11.
[0144] Furthermore, when forming the groove 31, a protective film can be used to cover the front side 11a of the wafer 11, and the laser beam 32B can be irradiated onto the wafer 11 through the protective film. For example, a resin tape or a film formed from a water-soluble resin such as PVA (polyvinyl alcohol) or PEG (polyethylene glycol) can be used as the protective film. When a protective film is formed on the front side 11a of the wafer 11, it can prevent processing debris (debris) generated during the ablation process from adhering to the front side 11a of the wafer 11, thereby avoiding contamination of the wafer 11 and the semiconductor device 15.
[0145] Alternatively, plasma gas or etchant can be provided to the processed area (groove 31) that has been processed by irradiation with laser beam 32B, thereby performing an etching process on the wafer 11. As a result, the groove 31 is expanded, and the fine irregularities formed on the inner wall of the groove 31 by the ablation process are removed.
[0146] When etching the wafer 11, it is preferable to form a mask covering the front side 11a of the wafer 11. This mask has openings that expose the area in the wafer 11 where the groove 31 is formed. Furthermore, plasma gas or etching solution is supplied to the wafer 11 through the mask. This protects the semiconductor device 15 formed on the front side 11a of the wafer 11.
[0147] Furthermore, there are no restrictions on the material of the mask used in the etching process. For example, a photoresist formed from a photosensitive resin can be used as a mask. Alternatively, the aforementioned protective film (PVA, PEG, etc.) formed on the front side 11a of the wafer 11 when irradiated by the laser beam 32B can also be used as a mask.
[0148] Next, the back side 11b of the wafer 11 is ground to expose the processed area (groove 31) that has been processed by the laser beam 32B on the back side 11b of the wafer 11. When grinding the wafer 11, the wafer 11 is first fixed to the support substrate. Figure 11 (A) is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. When the back side 11b of the wafer 11 is ground, the front side 11a of the wafer 11 is fixed to the support substrate 23 by means of the adhesive layer 25.
[0149] Next, through grinding device 2 (refer to...) Figure 2 The wafer 11 is ground. Specifically, the grinding tool 16 is brought into contact with the back side 11b of the wafer 11, thereby grinding the back side 11b of the wafer 11. The wafer 11 is ground and thinned until the groove 31 is exposed on the back side 11b of the wafer 11.
[0150] Figure 11 (B) is a cross-sectional view showing the wafer 11 after grinding. When the groove 31 is exposed on the back side 11b of the wafer 11, the defective device region 11c is disconnected from the wafer 11. Then, the defective device region 11c is separated from the wafer 11 as described above, and a through-hole 11d is formed on the wafer 11 (see reference). Figure 8 (A) Figure 8 (B) Figure 9 ).
[0151] Additionally, during the removal step, the wafer 11 can be cut by irradiation with a laser beam. Specifically, an ablation process is used to form a slit (cut) along the spacer 13 from the front side 11a to the back side 11b of the wafer 11.
[0152] Figure 12 (A) is a cross-sectional view showing a wafer 11 being irradiated by a laser beam 32C. During the cutting of the wafer 11, a laser irradiation unit 30C is used to irradiate the wafer 11 with the laser beam 32C. Furthermore, the structure of the laser irradiation unit 30C is similar to that of the laser irradiation unit 30A (see reference 30A). Figure 4 (A) is the same.
[0153] However, the irradiation conditions of the laser beam 32C are set to remove the area from the front side 11a to the back side 11b of the wafer 11 through an ablation process. Specifically, the wavelength of the laser beam 32C is set such that at least a portion of the laser beam 32C is absorbed by the wafer 11. That is, the laser irradiation unit 30C irradiates the laser beam 32C with a wavelength that is absorbent to the wafer 11. In addition, other irradiation conditions of the laser beam 32C are also set to remove the area from the front side 11a to the back side 11b of the wafer 11.
[0154] When the laser beam 32C is applied to the wafer 11, a protective component 33, such as a strip, is first attached to the wafer 11. For example, when the laser beam 32C is applied to the front side 11a of the wafer 11, a strip as a protective component 33 is attached to the back side 11b of the wafer 11.
[0155] Next, a laser beam 32C is irradiated onto the front side 11a of the wafer 11. Specifically, with the focal point of the laser beam 32C positioned on the spacer 13 of the wafer 11, the laser beam 32C is irradiated along the four spacer 13 surrounding the defective device 15a. Furthermore, there are no restrictions on the scanning path of the laser beam 32C. For example, along... Figure 5 (A) and Figure 5 The path 34A or path 34B shown in (B) scans the laser beam 32C.
[0156] When a laser beam 32C is irradiated along the spacer 13 surrounding the defective device 15a, the wafer 11 is removed along the spacer 13. As a result, a kerf (cut) 35 is formed on the wafer 11 along the spacer 13 from the front side 11a to the back side 11b. As a result, the defective device region 11c is separated from the wafer 11.
[0157] Furthermore, if it is difficult to form a kerf 35 reaching the back surface 11b of the wafer 11 by scanning the laser beam 32C once along the spacer 13, the laser beam 32C can be scanned multiple times along each spacer 13. Then, the defective device region 11c is separated from the wafer 11 as described above, and a through-hole 11d is formed on the wafer 11 (see reference). Figure 8 (A) Figure 8 (B) Figure 9 ).
[0158] After separating the defective device region 11c from the wafer 11, the wafer 11 is fixed to the support substrate 23. Figure 12 (B) is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. After the defective device region 11c is separated by forming a slit 35 on the wafer 11, the support substrate 23 is fixed on the front side 11a of the wafer 11 by means of an adhesive layer 25. Then, the protective member 33 is peeled off and removed from the back side 11b of the wafer 11.
[0159] Alternatively, in the removal step, the wafer 11 can also be processed by a laser beam (water laser) irradiated by a liquid. Figure 13 (A) is a cross-sectional view showing a wafer 11 irradiated by a laser beam 32C via a liquid column 50.
[0160] The laser irradiation unit 30C may have a built-in jetting unit (nozzle) for spraying liquid toward the wafer 11. In this case, liquid is continuously supplied to the wafer 11 from the jetting unit, thereby forming a liquid column 50 from the laser irradiation unit 30C to the wafer 11. The liquid column 50 is a column formed by flowing liquid and functions as a light guide for propagating the laser beam 32C. For example, water can be sprayed from the jetting unit to form a water column.
[0161] The wafer 11 is held by a holding stage 52. The upper surface of the holding stage 52 forms a flat holding surface 52a for holding the wafer 11. In addition, an opening 52b is provided on the holding stage 52, extending vertically through the holding stage 52. The opening 52b is formed into a rectangular shape when viewed from above, corresponding to the four spacers 13 surrounding the semiconductor device 15. The wafer 11 is arranged on the holding stage 52 such that the four spacers 13 surrounding the defective device 15a overlap with the opening 52b respectively.
[0162] Furthermore, liquid is ejected from the laser irradiation unit 30C to form a liquid column 50, and a laser beam 32C is irradiated from the laser irradiation unit 30C. At this time, the focusing point of the laser beam 32C is positioned inside the liquid column 50. Moreover, the laser beam 32C irradiates the wafer 11 via the liquid column 50.
[0163] When the laser beam 32C is irradiated onto the liquid column 50 as described above, the laser beam 32C can be guided to the spacer channel 13 of the wafer 11 even without strictly controlling the height of the focusing point of the laser beam 32C. In addition, the processing chips (debris) generated by the laser processing are washed away by the liquid.
[0164] Furthermore, the laser beam 32C scans along the spacer channel 13 together with the liquid column 50. As a result, a slit 35 is formed on the wafer 11 along the spacer channel 13, separating the defective device region 11c from the wafer 11. In addition, the liquid ejected from the laser irradiation unit 30C is discharged through the opening 52b provided in the holding stage 52.
[0165] Then, the wafer 11 is fixed to the support substrate. Figure 13 (B) is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. After the defective device region 11c is separated by forming a slit 35 on the wafer 11, the support substrate 23 is fixed on the front side 11a of the wafer 11 by means of an adhesive layer 25.
[0166] Alternatively, plasma gas or etching solution can be provided to the processed area (kerf 35) that has been processed by irradiation with laser beam 32C, thereby performing etching. As a result, the kerf 35 is expanded, and the fine irregularities formed on the inner wall of the kerf 35 by the ablation process are removed.
[0167] Furthermore, while the method for separating the defective device region 11c from the wafer 11 by laser processing has been described above, other methods besides laser processing can also be used for separating the defective device region 11c. For example, plasma cutting, which involves cutting the wafer 11 by plasma etching, can also be used.
[0168] In the case of plasma cutting, the support substrate 23 is first fixed on the front side 11a of the wafer 11 (see reference). Figure 4 (A)). Then, a plasma etching mask is formed on the back side 11b of the wafer 11.
[0169] Figure 14 (A) is a cross-sectional view showing a wafer 11 with a mask layer 37 formed thereon. The mask layer 37 is formed of a material that functions as a mask for plasma etching and is formed to cover the entire back side 11b of the wafer 11. For example, as the mask layer 37, a photoresist formed of a photosensitive resin, a water-soluble resin such as PVA or PEG can be used.
[0170] Next, the region in the mask layer 37 that overlaps with the four spacers 13 surrounding the defective device 15a is removed. For example, a laser beam 56 is irradiated onto the mask layer 37 from the laser irradiation unit 54, thereby removing the mask layer 37 along the spacers 13. In addition, the irradiation conditions of the laser beam 56 are set such that the mask layer 37 is removed by ablation when the laser beam 56 is irradiated onto the mask layer 37.
[0171] When the laser beam 56 irradiates the mask layer 37 along the four spacer channels 13 surrounding the defective device 15a, rectangular openings are formed on the mask layer 37 that expose the four spacer channels 13. This patterning of the mask layer 37 forms a plasma etching mask 39 (see reference). Figure 14 (B)
[0172] Next, plasma etching is performed on wafer 11 using mask 39. The plasma etching of wafer 11 is performed, for example, using the plasma processing apparatus described above.
[0173] Figure 14 (B) is a cross-sectional view showing a wafer 11 undergoing plasma etching. When plasma etching is performed, plasma-ionized etching gas (etching gas) 58 is supplied to the wafer 11 through an opening in the mask 39. As a result, etching is performed on the region of the wafer 11 along the spacing channel 13 surrounding the defective device 15a, forming a trench on the back side 11b of the wafer 11.
[0174] Figure 14(C) is a cross-sectional view showing the wafer 11 after plasma etching. When etching is performed so that the groove formed on the back side 11b of the wafer 11 reaches the front side 11a, a slit 35 is formed along the spacer 13 from the front side 11a to the back side 11b of the wafer 11, separating the defective device region 11c from the wafer 11. Then, the defective device region 11c is separated from the wafer 11, and a through-hole 11d is formed on the wafer 11 (see reference). Figure 8 (A) Figure 8 (B) Figure 9 ).
[0175] Alternatively, plasma etching can be performed by providing plasma-ionized gas 58 to the front side 11a of the wafer 11. In this case, a mask 39 is formed on the front side 11a of the wafer 11 before the wafer 11 is fixed to the support substrate 23. Gas 58 is then provided to the wafer 11 through the mask 39, forming a groove on the front side 11a of the wafer 11. When the groove reaches the back side 11b, a kerf 35 is formed, separating the defective device region 11c from the wafer 11. Then, the support substrate 23 is fixed on the front side 11a of the wafer 11.
[0176] After the above-described process, the defective device region 11c is separated from the wafer 11, and a through-hole 11d is formed on the wafer 11. The result is as follows: Figure 3 As shown in (B), a wafer 11 without defective device 15a is obtained.
[0177] Next, a device chip is prepared, which is a good semiconductor device 15 of the same type as the defective semiconductor device 15 (defective device 15a) and is sized to be embedded in the through-hole 11d. In the manufacture of the device chip, for example, a wafer with the same structure as wafer 11 is used. Figure 15 (A) is a perspective view showing the wafer 51 for preparing the device chip.
[0178] The wafer 51 is formed of the same material as the wafer 11, and has a front side (first side) 51a and a back side (second side) 51b. Furthermore, the wafer 51 is divided into multiple regions by a plurality of spacer lines (predetermined dividing lines) 53 arranged in a grid pattern in an intersecting manner. Semiconductor devices 55 are formed in each of the multiple regions divided by the spacer lines 53 on the front side 51a of the wafer 51.
[0179] Semiconductor device 55 has with Figure 1 The semiconductor device 55 has the same function as the semiconductor device 15 shown in (A). Furthermore, the structure of the semiconductor device 55 is the same as that of the semiconductor device 15, and electrodes (through-hole electrodes, through-hole electrodes) 57 are connected to the semiconductor device 55 (see reference). Figure 17 (A)). The structure and material of electrode 57 are similar to those of... Figure 1 The electrode 19 shown in (B) is the same.
[0180] The wafer 51 is diced along the spacer 53, thereby manufacturing multiple device chips, each having a semiconductor device 55. The dicing of the wafer 51 is performed, for example, by the laser processing or plasma etching described above.
[0181] Alternatively, a cutting device can be used for dicing the wafer 51. The cutting device includes a chuck stage for holding the wafer 51 and a cutting unit for cutting the wafer 51 held by the chuck stage. An annular cutting tool is mounted in the cutting unit. The cutting tool is rotated and cuts into the wafer 51, thereby dicing the wafer 51 along the spacer 53. The result is the acquisition of multiple device chips, each having a semiconductor device 55.
[0182] Figure 15 (B) is a perspective view showing a wafer 51 divided into multiple device chips 59. Furthermore, before or after the wafer 11 is divided, inspection is performed on the multiple semiconductor devices 55 formed on the wafer 51 to determine whether each semiconductor device 55 is a good product or a defective product. And, device chips 59 containing semiconductor devices 55 determined to be defective are removed from the multiple device chips 59 obtained by dividing the wafer 51.
[0183] Thus, device chip 59 is obtained, which has the same good semiconductor device 15 (refer to) formed on wafer 11. Figure 1 The semiconductor device 55 is the same as that of (A), etc. That is, the device chip 59 has a good semiconductor device 55 (a semiconductor device 55 with the functions that the defective device 15a should have), and the good semiconductor device 55 has the same functions as the defective device 15a (refer to Figure 1 (A) etc. have the same function.
[0184] Furthermore, there is no limitation on the timing of preparing the device chip 59. For example, after the preparation of the wafer 51 and the inspection of the semiconductor device 55 are carried out at the same time as the preparation of the wafer 11 and the inspection of the semiconductor device 15, the device chip 59 is manufactured by dicing the wafer 51.
[0185] Next, the device chip 59 is embedded into the through hole 11d of the wafer 11 (embedding step). Figure 16 This is a perspective view showing the wafer 11 during the embedding process.
[0186] With the front side 11a (semiconductor device 15 side) of the wafer 11 fixed to the support substrate 23, the device chip 59 is positioned such that the side on which the semiconductor device 55 is formed (front side) faces the support substrate 23. Furthermore, the device chip 59 is embedded into the through-hole 11d of the wafer 11.
[0187] Figure 17 (A) is a cross-sectional view showing a wafer 11 in which a device chip 59 is embedded. The device chip 59 is embedded in the through-hole 11d in such a way that it contacts the adhesive layer 25 exposed in the through-hole 11d. Thus, the device chip 59 is fixed to the support substrate 23 by means of the adhesive layer 25.
[0188] Furthermore, when the wafer 11 is temporarily fixed to the support substrate 23 by the adhesive layer 25, and the bonding between the wafer 11 and the support substrate 23 is weak, after the device chip 59 is inserted into the through hole 11d, a process is performed to firmly fix the wafer 11 to the support substrate 23 (formal fixing process). Thus, the wafer 11 and the device chip 59 are firmly fixed to the support substrate 23 by means of the adhesive layer 25.
[0189] For example, if the adhesive layer 25 is an adhesive formed of a thermosetting resin, the thermosetting resin is hardened by heat treatment at a higher temperature or for a longer period of time compared to temporary fixation, thereby strengthening the bond between the wafer 11 and the support substrate 23. Alternatively, if the adhesive layer 25 is an adhesive formed of a UV-curable resin, the UV-curable resin is heat-treated, thereby strengthening the bond between the wafer 11 and the support substrate 23. Furthermore, if the adhesive layer 25 is a thermosetting bonding pad, the wafer 11 and the support substrate 23 are pressed against the thermosetting bonding pad by heat treatment at a higher temperature or for a longer period of time compared to temporary fixation, thereby strengthening the bond between the wafer 11 and the support substrate 23.
[0190] In addition, during the removal step, if the wafer 11 is temporarily fixed to the support substrate 23 using an adhesive layer 25 with weaker adhesive strength, the wafer 11 and the support substrate 23 can be temporarily separated before the embedding step, and the wafer 11 can be re-fixed to the support substrate 23 using other adhesive layers with higher adhesive strength than the adhesive layer 25.
[0191] Figure 17 (B) is a top view showing the through-hole 11d. In the removal step described above, the through-hole 11d is formed to be larger than the device chip 59. Specifically, the length L of the through-hole 11d in the first direction (left-right direction on the paper) is... A1 The length L in the first direction of the device chip 59 is greater than B1 Additionally, the length L of the second direction (the direction perpendicular to the first direction, the vertical direction on the paper) of the through hole 11d A2The length L in the second direction of the device chip 59 is greater than B2 Therefore, when the device chip 59 is embedded in the through hole 11d, a gap 61 is formed between the wafer 11 and the device chip 59 in a manner that surrounds the device chip 59.
[0192] Furthermore, in a subsequent process (the resin filling step described later), resin is filled into the gap 61. Therefore, it is preferable to ensure that the width of the gap 61 (the distance between the inner wall of the through hole 11d and the side of the device chip 59) is a certain width or more. For example, the size of the through hole 11d or the device chip 59 is adjusted such that the width of the gap 61 is 2 μm or more, preferably 5 μm or more, and more preferably 10 μm or more.
[0193] The specific dimensions of the through-hole 11d can be appropriately set considering the positions of semiconductor devices 15 and 55. For example, on the front side 11a of the wafer 11, the distance between the end (inner wall) of the through-hole 11d and the end of the semiconductor device 15 is set to 2 μm or more, preferably 5 μm or more. Furthermore, on the front side 11a of the wafer 11, the end of the through-hole 11d can be positioned closer to the semiconductor device 15 than the center of the spacer channel 13 in the width direction. Additionally, as... Figure 17 As shown in (A), when the inner wall of the through hole 11d is inclined relative to the thickness direction of the wafer 11, a portion of the region on the back side 11b of the wafer 11 in the through hole 11d may overlap with a portion of the semiconductor device 15 formed on the wafer 11.
[0194] There are no restrictions on the specific size of the device chip 59, as long as it can be embedded into the through hole 11d. For example, on the front side of the device chip 59, the distance between the end of the semiconductor device 55 and the end of the device chip 59 is set to be less than 1 / 2 of the width of the spacer channel 13 set on the wafer 11.
[0195] Alternatively, in the embedding step, the device chip 59 with the adhesive layer attached can be embedded into the through hole 11d instead of fixing the device chip 59 to the adhesive layer 25. Specifically, after removing the adhesive layer 25 exposed inside the through hole 11d by processes such as plasma etching or wet etching (chemical treatment), the device chip 59 with the adhesive layer attached can be fixed to the support substrate 23 by means of the adhesive layer.
[0196] Figure 18 (A) is a cross-sectional view of the wafer 11 during plasma etching of the adhesive layer 25. For example, a plasma-ionized gas (etching gas) 60 is provided to the back side 11b of the wafer 11, thereby removing the area in the adhesive layer 25 that overlaps with the through-hole 11d.
[0197] Figure 18 (B) is a cross-sectional view of the wafer 11 showing a portion of the adhesive layer 25 removed. When the region of the adhesive layer 25 overlapping with the through-hole 11d is removed, the region of the upper surface of the support substrate 23 overlapping with the through-hole 11d is exposed. Additionally, during plasma etching of the wafer 11, a mask exposing the through-hole 11d can be formed on the back side 11b of the wafer 11.
[0198] Next, the device chip 59 with the adhesive layer attached is embedded into the through hole 11d. Figure 18 (C) is a cross-sectional view showing a wafer 11 in which a device chip 59 with an adhesive layer 63 is embedded. The adhesive layer 63 is provided on the front side (semiconductor device 55 side) of the device chip 59. In addition, the material of the adhesive layer 63 is the same as that of the adhesive layer 25. The device chip 59 is fixed to the upper surface of the support substrate 23 exposed inside the through hole 11d by means of the adhesive layer 63.
[0199] Furthermore, after the device chip 59 is filled into the through hole 11d, the adhesive layers 25 and 63 are formally fixed as needed. Thus, the wafer 11 and the device chip 59 are firmly fixed to the support substrate 23 by means of the adhesive layers 25 and 63.
[0200] Next, resin is filled into the gap 61 between the wafer 11 and the device chip 59 (resin filling step). Figure 19 (A) is a cross-sectional view showing the wafer 11 during the resin filling step.
[0201] In the resin filling step, resin 65 is formed on the back side 11b of the wafer 11. Resin 65 is formed, for example, by coating a liquid resin such as epoxy resin onto the back side 11b of the wafer 11 and allowing the liquid resin to harden. However, there are no limitations on the material of resin 65.
[0202] When liquid resin is coated on the back side 11b of wafer 11, a portion of the liquid resin flows into the gap 61 between wafer 11 and device chip 59 (see reference). Figure 17 (A) Figure 17 (B) etc., fill the gap 61. When the liquid resin is hardened in this state, the wafer 11 and the device chip 59 are bonded by means of the resin 65, and the device chip 59 is fixed to the wafer 11.
[0203] Next, the resin 65 formed on the outer side of the gap 61 is ground (resin grinding step). In the resin grinding step, the resin 65 formed on the back side 11b of the wafer 11 is removed by grinding. In the grinding of the resin 65, for example, a grinding apparatus 2 (see reference 1) is used. Figure 2 ).
[0204] Figure 19 (B) is a cross-sectional view showing the wafer 11 during the resin grinding step. For example, in the resin grinding step, the resin 65 formed on the outside of the gap 61 is removed by grinding, and the back side 11b side of the wafer 11 is ground. Furthermore, the wafer 11 is thinned until the electrodes 19 and 57 are exposed on the back side 11b side of the wafer 11.
[0205] However, there are no restrictions on the method used to expose electrodes 19 and 57. For example, after the resin 65 is ground to expose the back surface 11b side of the wafer 11 during the resin grinding step, plasma etching, wet etching, or other etching processes can be performed on the back surface 11b side of the wafer 11, thereby exposing electrodes 19 and 57. In this case, it is possible to prevent the grinding tool 16 (see reference) from being ground. Figure 2 The metal contained in electrodes 19 and 57 is scattered upon contact with them.
[0206] After the above processes, a wafer 11 with electrodes 19 and 57 exposed on the back side 11b is obtained. Thus, semiconductor devices 15 and 55, and semiconductor devices (not shown) included in other wafers stacked on the back side 11b of the wafer 11, can be connected via the electrodes 19 and 57. That is, the wafer manufacturing method of this embodiment produces a wafer 11 that can be used for the formation of stacked wafers.
[0207] Next, a specific example of a method for manufacturing a device chip (stacked device chip) having multiple stacked semiconductor devices using the aforementioned wafer 11 will be described. In manufacturing a stacked device chip, a stacked wafer having multiple stacked wafers is first formed (wafer stacking step). Figure 20 This is a cross-sectional view showing the stacked wafer 79.
[0208] In the wafer stacking step, wafer 11 (first wafer) after the resin grinding step and other wafers 71 (second wafer) prepared in the above-described wafer preparation step are used. In addition, the structure of wafer 71 is the same as that of wafer 11.
[0209] Specifically, wafer 71 is formed of the same material as wafer 11, and wafer 71 has a front side (first side) 71a and a back side (second side) 71b. Furthermore, wafer 71 is divided into multiple rectangular regions by multiple spacer lines (predetermined dividing lines) 73 arranged in a grid pattern in an intersecting manner. Semiconductor devices 75 are formed in the multiple regions divided by the spacer lines 73 on the front side 71a of wafer 71.
[0210] The structure of semiconductor device 75 is the same as that of semiconductor device 15. Additionally, electrodes (through-hole electrodes, through-hole electrodes) 77 are connected to semiconductor device 75. The structure and material of electrode 77 are the same as those of electrode 19.
[0211] Wafer 71 is stacked on wafer 11. For example, wafer 71 is attached to wafer 11 with its front side 71a facing the back side 11b facing wafer 11. Furthermore, there are no limitations on the method of attaching wafer 11 and wafer 71. For example, wafer 11 and wafer 71 can be attached by direct bonding. Specifically, the back side 11b of wafer 11 and the front side 71a of wafer 71 are bonded by surface-activated bonding.
[0212] However, wafer 11 and wafer 71 can be bonded together indirectly. For example, wafer 11 and wafer 71 can also be bonded together by laminating wafer 71 onto wafer 11 using a permanent adhesive.
[0213] Furthermore, if defective devices are included among the multiple semiconductor devices 75 formed on wafer 71, a grinding step, a removal step, an embedding step, a resin filling step, and a resin grinding step are performed on wafer 71 before or after wafer 71 is stacked on wafer 11. As a result, defective devices are removed from wafer 71, and device chips 59 containing good semiconductor devices 55 are embedded into wafer 71.
[0214] Wafer 11 and wafer 71 are bonded together such that spacers 13 and 73 overlap and the semiconductor devices 15 and 55 contained in wafer 11 overlap with the semiconductor devices 75 and 55 contained in wafer 71. As a result, the semiconductor devices 15 and 55 contained in wafer 11 and the semiconductor devices 75 and 55 contained in wafer 71 are connected by electrodes 19 and 57.
[0215] Thus, a stacked wafer 79 is formed having wafers 11 and 71 stacked on top of each other. Furthermore, in the wafer stacking step, multiple wafers 71 can be stacked on wafer 11. For example, other wafers 71 can be further stacked on the wafers 71 stacked on wafer 11. In this case, grinding, removal, embedding, resin filling, and resin grinding steps are performed on the multiple wafers 71 stacked on wafer 11 respectively. As a result, a stacked wafer 79 having three or more wafer layers is obtained.
[0216] Next, the stacked wafer 79 is divided along the spacers 13 and 73 to form a stacked device chip with multiple stacked semiconductor devices (division step). Figure 21 (A) is a cross-sectional view showing the stacked wafer 79 in the dicing step.
[0217] In the dicing step, for example, the stacked wafer 79 is cut using a cutting device. The cutting device includes a chuck table that holds the stacked wafer 79 and a cutting unit that cuts the stacked wafer 79 held by the chuck table. The cutting unit has a cylindrical spindle that rotates via a rotary drive source such as an electric motor. Furthermore, an annular cutting tool 62 for cutting the stacked wafer 79 is mounted at the front end of the spindle.
[0218] As a cutting tool 62, for example, a hub-type cutting tool (hub tool) is used. A hub tool is constructed by integrating an annular base formed of metal or the like and an annular cutting edge formed along the outer periphery of the base. The cutting edge of the hub tool is made of an electroformed abrasive, which is formed by fixing abrasive grains formed of diamond or the like with a bonding material such as nickel plating.
[0219] Alternatively, a washer-type cutting tool (washer tool) can also be used as the cutting tool 62. The washer tool consists of annular cutting edges, which are formed by fixing abrasive grains with a bonding material made of metal, ceramic, resin, etc.
[0220] The cutting tool 62 is rotated to cut into the stacked wafer 79, thereby dividing the stacked wafer 79. Specifically, with the lower end of the cutting tool 62 positioned below the front surface 11a (upper surface of the adhesive layer 25) of the wafer 11, the cutting tool 62 is rotated while the cutting tool 62 and the stacked wafer 79 are moved relative to each other in the horizontal direction, thereby causing the cutting tool 62 to cut into the stacked wafer 79 along the spacers 13 and 73. Furthermore, when the stacked wafer 79 is cut along all the spacers 13 and 73, the stacked wafer 79 is divided into multiple stacked device chips.
[0221] Figure 21 (B) is a cross-sectional view showing a stacked wafer 79 divided into multiple stacked device chips 81. Each stacked device chip 81 has a semiconductor device 15 or semiconductor device 55 (first semiconductor device) included in wafer 11 and a semiconductor device 75 or semiconductor device 55 (second semiconductor device) included in wafer 71. Furthermore, the first semiconductor device and the second semiconductor device are stacked on top of each other and connected by means of electrode 19 or electrode 57.
[0222] As described above, in the wafer manufacturing method of this embodiment, the defective device region 11c is removed from the wafer 11, and a device chip 59 having a good semiconductor device 15 is embedded in the space (removed region) formed by removing the defective device region 11c. Therefore, a wafer 11 without the defective device 15a can be manufactured. Furthermore, by stacking wafers 11 without the defective device 15a to form a stacked wafer 79 and dividing the stacked wafer 79, a stacked device chip 81 without the defective device 15a can be manufactured. As a result, the yield reduction of the stacked device chip 81 is suppressed.
[0223] (Implementation Method 2)
[0224] In Embodiment 1, an example of separating the defective device region 11c by irradiation with a laser beam during the removal step was described. However, other methods may also be used for separating the defective device region 11c. In this embodiment, the separation of the wafer preparation step and the grinding step (see [reference]) is described. Figure 2 The method for separating the defective device region 11c in the removal step by breaking the wafer 11 is then described.
[0225] In this embodiment, there are no restrictions on the crushing process used, as long as it can be used to process the wafer 11. Examples of crushing processes that can be used in the processing of the wafer 11 include sandblasting, waterjet processing, and drilling.
[0226] Figure 22 (A) is a cross-sectional view showing a wafer 11 with grooves 93 formed by sandblasting. In sandblasting, a sandblasting unit 72 is used to spray abrasive material 74. For example, the sandblasting unit 72 has a compressor that compresses and delivers a gas such as air, and a spray gun that sprays the abrasive material 74 together with the compressed gas. The abrasive material 74 sprayed from the sandblasting unit 72 collides with the wafer 11, thereby processing the wafer 11.
[0227] During the crushing process, a protective layer 91 is first formed on the wafer 11. For example, when processing the front side 11a of the wafer 11, the front side 11a of the wafer 11 is covered by the protective layer 91 to protect the semiconductor device 15. Furthermore, there are no restrictions on the material of the protective layer 91; for example, water-soluble resins such as PVA and PEG can be used. Additionally, if damage to the semiconductor device 15 due to the crushing process is unlikely, the formation of the protective layer 91 can be omitted.
[0228] Next, the wafer 11 is held by the holding stage 70. The upper surface of the holding stage 70 forms a flat holding surface 70a for holding the wafer 11. For example, the wafer 11 is arranged on the holding stage 70 with its front side 11a exposed upwards and its back side 11b facing the holding surface 70a.
[0229] Furthermore, abrasive material 74 is sprayed from the sandblasting unit 72 along the four spacers 13 surrounding the defective device 15a. As a result, a strip-shaped groove 93 is formed along the spacers 13 on the front side 11a of the wafer 11. The groove 93 is formed in a top-view rectangular shape in a manner surrounding the defective device 15a.
[0230] Figure 22 (B) is a cross-sectional view showing a wafer 11 with a groove 93 formed by waterjet processing. In waterjet processing, a waterjet unit 76 is used to spray a liquid 78 such as water. The waterjet unit 76 has a nozzle that sprays liquid 78 pressurized by a pump. In addition, abrasive particles may be contained in the liquid 78. The liquid 78 sprayed from the waterjet unit 76 collides with the wafer 11, thereby processing the wafer 11.
[0231] Specifically, liquid 78 ejected from water jet unit 76 is sprayed along four spacer channels 13 surrounding defective device 15a. As a result, a strip-shaped groove 93 is formed along the spacer channels 13 on the front side 11a of wafer 11. The groove 93 is formed in a top-view rectangular shape in a manner surrounding defective device 15a.
[0232] Figure 22 (C) is a cross-sectional view showing a wafer 11 with a groove 93 formed by drilling. In the drilling process, a drilling unit 80 with a rod-shaped drill bit 82 mounted on it is used. The drilling unit 80 has a rotation drive source such as an electric motor that rotates the drill bit 82 mounted on it. While rotating the drill bit 82, the tip of the drill bit 82 contacts the wafer 11, thereby processing the wafer 11.
[0233] Specifically, firstly, the rotating drill bit 82 contacts the area overlapping with the spacer 13 of the wafer 11, forming a cylindrical groove on the wafer 11. Next, the holding stage 70 or the drill bit 82 is moved along the spacer 13. Furthermore, the amount of movement at this time is set to be less than the diameter of the cylindrical groove formed on the wafer 11. Then, a new groove is formed on the wafer 11 using the drill bit 82. As a result, the groove already formed on the wafer 11 and the newly formed groove are connected.
[0234] Repeating the above steps, a plurality of grooves are formed along the four spacers 13 surrounding the defective device 15a. As a result, a strip-shaped groove 93 is formed along the spacers 13 on the front side 11a of the wafer 11. The groove 93 is composed of a plurality of cylindrical grooves formed in an interconnected manner.
[0235] As described above, a crushing process is performed along the spacer 13 surrounding the defective device 15a, thereby forming a groove 93 on the wafer 11. Then, the back side 11b of the wafer 11 is ground, thereby exposing the processed area (groove 93) processed by the crushing process on the back side 11b of the wafer 11.
[0236] When grinding the wafer 11, the wafer 11 is first fixed to the support substrate 23. Figure 23 (A) is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. When the back side 11b of the wafer 11 is ground, the front side 11a of the wafer 11 is fixed to the support substrate 23 by means of the adhesive layer 25.
[0237] Next, through grinding device 2 (refer to...) Figure 2 The wafer 11 is ground. Specifically, the grinding tool 16 is brought into contact with the back side 11b of the wafer 11, thereby grinding the back side 11b of the wafer 11. The wafer 11 is ground and thinned until the groove 93 is exposed on the back side 11b of the wafer 11.
[0238] Figure 23 (B) is a cross-sectional view showing the wafer 11 after grinding. When the groove 93 is exposed on the back side 11b of the wafer 11, the defective device region 11c is disconnected from the wafer 11. Then, by the same steps as in Embodiment 1, the defective device region 11c is separated from the wafer 11, and a through-hole 11d is formed on the wafer 11 (see Figure 1). Figure 8 (A) Figure 8 (B) Figure 9 ).
[0239] Additionally, during the removal step, a through-hole can be formed through the wafer 11 by a crushing process, thereby separating the defective device region 11c. Specifically, a through-hole is formed along the spacer 13 from the front side 11a to the back side 11b of the wafer 11 by a crushing process.
[0240] Figure 24 (A) is a cross-sectional view showing a wafer 11 with a through-hole 95 formed by sandblasting. When the through-hole 95 is formed by crushing, an opening 70b extending vertically through the holding stage 70 is provided on the holding stage 70. The opening 70b is formed into a rectangular shape in plan view, corresponding to the four spacer channels 13 surrounding the semiconductor device 15. Furthermore, the wafer 11 is arranged on the holding stage 70 such that the four spacer channels 13 surrounding the defective device 15a overlap with the opening 70b.
[0241] Next, abrasive material 74 is sprayed from the sandblasting unit 72 along the four spaced channels 13 surrounding the defective device 15a. In addition, the spraying conditions of the abrasive material 74 are set to form a hole in the area of the wafer 11 that is struck by the abrasive material 74, which penetrates the wafer 11 from the front side 11a to the back side 11b.
[0242] Therefore, when polishing material 74 is sprayed along the spacer 13, a strip-shaped through-hole 95 is formed on the wafer 11 along the spacer 13, running from the front side 11a to the back side 11b. This through-hole 95 is formed in a top-view rectangular shape, surrounding the defective device 15a. As a result, the defective device region 11c is disconnected from the wafer 11.
[0243] Figure 24 (B) is a cross-sectional view showing a wafer 11 with a through-hole 95 formed by water jet processing. In the case of forming the through-hole 95 by water jet processing, liquid 78 ejected from the water jet unit 76 is sprayed along four spaced channels 13 surrounding the defective device 15a. In addition, the spraying conditions of the liquid 78 are set to form a hole in the area of the wafer 11 that penetrates from the front side 11a to the back side 11b in the area where the liquid 78 collides with the wafer 11.
[0244] Therefore, when liquid 78 is sprayed along the spacer 13, a strip-shaped through-hole 95 is formed on the wafer 11 along the spacer 13, running from the front side 11a to the back side 11b. This through-hole 95 is formed in a top-view rectangular shape, surrounding the defective device 15a. As a result, the defective device region 11c is disconnected from the wafer 11.
[0245] Figure 24 (C) is a cross-sectional view of a wafer 11 in which a through hole 95 is formed by drilling. In the case of forming the through hole 95 by drilling, the drill bit 82 is first rotated and contacted with the wafer 11 to form a cylindrical hole that passes through the wafer 11 from the front side 11a to the back side 11b.
[0246] Then, the same steps are repeated to form a plurality of holes along the four spacers 13 surrounding the defective device 15a. In addition, the plurality of holes are formed to connect with the holes already formed on the wafer 11. As a result, a strip of through-holes 95 is formed on the wafer 11 along the spacers 13 from the front side 11a to the back side 11b, separating the defective device region 11c from the wafer 11.
[0247] In sandblasting (see reference) Figure 24 During the implementation of (A), the abrasive material 74 passing through the through-hole 95 of the wafer 11 is discharged through the opening 70b of the holding stage 70. Similarly, in waterjet processing (see... Figure 24When (B) is implemented, the liquid 78 that has passed through the through hole 95 of the wafer 11 is discharged through the opening 70b of the holding stage 70. Therefore, it is possible to prevent the abrasive material 74 and the liquid 78 from colliding with the holding surface 70a of the holding stage 70 and causing damage to the holding stage 70.
[0248] Additionally, in drilling (refer to...) Figure 24 When implementing (C), the front end of the drill bit 82 is inserted into the opening 70b of the retaining table 70. Therefore, it is possible to prevent the drill bit 82 from contacting the retaining table 70 and causing damage to the retaining table 70.
[0249] In addition, Figure 24 (A) Figure 24 (B) Figure 24 In (C), the case where the wafer 11 is processed from the front side 11a is shown, but the wafer 11 can also be processed from the back side 11b. That is, the abrasive material 74 or liquid 78 can collide with the back side 11b of the wafer 11, and the drill bit 82 can contact the back side 11b of the wafer 11.
[0250] Next, the protective layer 91 is removed from the wafer 11, and the defective device region 11c is separated from the wafer 11. Then, the wafer 11 is fixed to the support substrate 23. Figure 25 This is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. For example, the front side 11a of the wafer 11 is fixed to the support substrate 23 by means of an adhesive layer 25.
[0251] Alternatively, etching can be performed on the wafer 11 with through-holes 11d formed through a crushing process. For example, plasma etching can be performed on the interior of the through-holes 11d by providing a gas in a plasma state to the through-holes 11d of the wafer 11. Alternatively, wet etching can be performed on the interior of the through-holes 11d by providing an etching solution to the through-holes 11d of the wafer 11.
[0252] Figure 26 This is a cross-sectional view showing a wafer 11 undergoing plasma etching. When a plasma-ionized etching gas (etching gas) 84 is supplied to the wafer 11, plasma etching is performed on the inner wall of the through-hole 11d. As a result, the size of the through-hole 11d increases. In addition, the fine irregularities formed on the inner wall of the through-hole 11d due to the fragmentation process are removed by plasma etching.
[0253] In addition, the area where the wafer 11 is subjected to crushing processing is appropriately set in a manner that forms a through hole 11d of the desired size. Figure 27 (A) is a top view showing the area (processed area) 97A processed by sandblasting or waterjet processing. Additionally, Figure 27(B) is a top view showing the area (machined area) 97B that is being machined by drilling. Figure 27 (A) and Figure 27 In (B), there are patterns in areas 97A and 97B.
[0254] When the wafer 11 is processed by sandblasting, for example, abrasive material 74 is sprayed onto the region 97A along the outer periphery of the defective device 15a. Similarly, when the wafer 11 is processed by water jetting, for example, liquid 78 is sprayed onto the region 97A along the outer periphery of the defective device 15a. Thus, a groove 93 is formed around the defective device 15a (see reference). Figure 22 (A) and Figure 22 (B) or through hole 95 (refer to) Figure 24 (A) and Figure 24 (B)). In addition, the abrasive material 74 and liquid 78 can be sprayed in a manner that collides with a portion of the defective device 15a, or they can be sprayed onto the spacer channel 13 in a manner that does not collide with the defective device 15a.
[0255] When processing the wafer 11 by drilling, for example, drill bit 82 sequentially processes multiple regions 97B along the outer periphery of the defective device 15a. Furthermore, each of the multiple regions 97B is configured to overlap a portion of an adjacent region 97. Thus, a groove 93 is formed around the defective device 15a (see reference). Figure 22 (C) or through hole 95 (refer to) Figure 24 (C)). Alternatively, drill bit 82 may contact a portion of defective device 15a, or it may contact only the spacer 13 without contacting defective device 15a.
[0256] Furthermore, when processing the wafer 11 by drilling, the drill bit 82 can be inserted into the interior of the wafer 11 (see reference). Figure 22 (C) and Figure 24 (C) causes the drill bit 82 to rotate while moving horizontally along the spacer 13, thereby forming a groove 93 or a through hole 95. In this case, it is not necessary to perform multiple up-and-down operations on the spacer 13.
[0257] Then, an etching process (such as plasma etching, reference) is performed on the wafer 11. Figure 26 This process etches the inner wall of the through-hole 11d. As a result, the fine irregularities remaining in the fractured areas 97A and 97B are removed, and the width of the through-hole 11d is increased, forming a shape similar to... Figure 27 (A) and Figure 27The enlarged through-hole 11d is shown in (B).
[0258] As described above, in the removal step, the defective device region 11c can also be separated from the wafer 11 by a crushing process. Furthermore, the steps included in the removal step that are omitted from description in this embodiment are the same as in Embodiment 1. Additionally, in this embodiment, steps other than the removal step (wafer preparation step, grinding step, embedding step, resin filling step, resin grinding step, wafer stacking step, dicing step, etc.) can be performed in the same manner as in Embodiment 1. Furthermore, this embodiment can be appropriately combined with other embodiments.
[0259] (Implementation Method 3)
[0260] In embodiments 1 and 2, an example was described where the defective device region 11c was separated from the wafer 11 by processing the wafer 11 along the spacer 13 during the removal step. However, there are no limitations on the method for removing the defective device region 11c from the wafer 11. In this embodiment, the wafer preparation step and the grinding step (see [reference]) are described. Figure 2 The method of destroying and removing the defective device region 11c by irradiation with a laser beam in the removal step is then described.
[0261] Figure 28 (A) is a cross-sectional view showing the wafer 11 being irradiated by the laser beam 32D. In cases where the defective device region 11c is destroyed by irradiation with the laser beam, a laser irradiation unit 30D is used to irradiate the wafer 11 with the laser beam 32D. Furthermore, the structure of the laser irradiation unit 30D is similar to that of the laser irradiation unit 30A (see reference 30A). Figure 4 (A) is the same.
[0262] However, the irradiation conditions of the laser beam 32D are set to remove the area of the wafer 11 irradiated by the laser beam 32D through an ablation process. Specifically, the wavelength of the laser beam 32D is set such that at least a portion of the laser beam 32D is absorbed by the wafer 11. That is, the laser irradiation unit 30D irradiates the wafer 11 with a wavelength that is absorbent to the wafer 11. In addition, other irradiation conditions of the laser beam 32D are also set to appropriately perform an ablation process on the wafer 11.
[0263] For example, a laser beam 32D is irradiated onto the front side 11a of the wafer 11. Specifically, the laser beam 32D is irradiated with its focal point positioned inside the four spacer channels 13 surrounding the defective device 15a. This ablation process is performed on the defective device region 11c, destroying it. As a result, a groove (recess) is formed on the front side 11a of the wafer 11.
[0264] Figure 28(B) is a cross-sectional view showing the wafer 11 with the groove (removal area) 101 formed thereon. For example, the laser beam 32D scans the entire rectangular area located inside the four spacer channels 13 surrounding the defective device 15a from a top view. As a result, a cuboid groove 101 is formed on the front side 11a of the wafer 11 by ablation. In addition, the depth of the groove 101 is adjusted so that the bottom surface of the groove 101 is formed at a position lower than the lower end of the electrode 19. As a result, the defective device 15a and the electrode 19 are removed.
[0265] Figure 29 This is a top view showing the scanning path 34D of the laser beam 32D. For example, multiple paths 34D are set from one end of the defective device region 11c towards the other end. The laser beam 32D scans along the path 34D in a reciprocating manner between one end and the other of the defective device region 11c. Thus, the laser beam 32D illuminates the entire area of the defective device region 11c, removing the defective device region 11c. However, as long as the defective device region 11c can be removed, there are no restrictions on the scanning path of the laser beam 32D.
[0266] Furthermore, when forming the groove 101, a protective film can be used to cover the front side 11a of the wafer 11, and the laser beam 32D can be irradiated onto the wafer 11 through the protective film. For example, a resin tape or a film formed from water-soluble resins such as PVA or PEG can be used as the protective film. When a protective film is formed on the front side 11a of the wafer 11, it can prevent processing debris (debris) generated during the ablation process from adhering to the front side 11a of the wafer 11, thereby avoiding contamination of the wafer 11 and the semiconductor device 15.
[0267] Next, the back side 11b of the wafer 11 is ground, thereby exposing the processed area (groove 101) that has been processed by the laser beam 32D on the back side 11b of the wafer 11. When grinding the wafer 11, the wafer 11 is first fixed to the support substrate. Figure 30 (A) is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. When the back side 11b of the wafer 11 is ground, the front side 11a of the wafer 11 is fixed to the support substrate 23 by means of the adhesive layer 25.
[0268] Next, through grinding device 2 (refer to...) Figure 2 The wafer 11 is ground. Specifically, the grinding tool 16 is brought into contact with the back side 11b of the wafer 11, thereby grinding the back side 11b of the wafer 11. The wafer 11 is ground and thinned until the groove 101 is exposed on the back side 11b of the wafer 11.
[0269] Figure 30(B) is a cross-sectional view showing the wafer 11 after grinding. When the groove 101 is exposed on the back side 11b of the wafer 11, a through hole 11d is formed on the wafer 11 from the front side 11a to the back side 11b.
[0270] In addition, during the removal step, the through-hole 11d can be formed directly by irradiation with a laser beam 32D. Specifically, the through-hole 11d is formed from the front side 11a to the back side 11b of the wafer 11 through an ablation process.
[0271] Figure 31 (A) is a cross-sectional view showing the wafer 11 being irradiated by the laser beam 32D. First, a protective component 103, such as a strip, is attached to the wafer 11. For example, when the laser beam 32D is irradiated to the front side 11a of the wafer 11, the protective component 103 is attached to the back side 11b of the wafer 11. Furthermore, an example of the material of the protective component 103 is shown in the image (see image 21). Figure 2 )same.
[0272] Furthermore, the laser beam 32D is irradiated with its focal point positioned inside the four spaced channels 13 surrounding the defective device 15a. Additionally, there are no restrictions on the scanning path of the laser beam 32D. For example, along... Figure 29 The path shown is 34D scanning laser beam 32D.
[0273] The irradiation conditions of the laser beam 32D are set to remove the area of the wafer 11 from the front side 11a to the back side 11b by ablation. Therefore, when the irradiation of the wafer 11 by the laser beam 32D is completed, a through hole 11d is formed that extends from the front side 11a to the back side 11b of the wafer 11.
[0274] Then, the wafer 11 is fixed to the support substrate. Figure 31 (B) is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. After a through hole 11d is formed on the wafer 11, the support substrate 23 is fixed to the front side 11a of the wafer 11 by means of an adhesive layer 25. Then, the protective member 103 is peeled off from the front side 11a of the wafer 11.
[0275] Alternatively, an aqua laser (water laser) irradiated by liquid can be used in the formation of the through hole 11d. In this case, a jetting unit that sprays liquid onto the laser irradiation unit 30D is provided. Furthermore, a liquid column 50 is formed by spraying liquid from the laser irradiation unit 30D (see reference). Figure 13 (A)) and a laser beam 32D is irradiated from the laser irradiation unit 30D. At this time, the focusing point of the laser beam 32D is located inside the liquid column 50. And, the laser beam 32D irradiates the defective device region 11c through the liquid column 50. As a result, the defective device region 11c is removed.
[0276] Additionally, a wafer 11 with a through-hole 11d formed by damaging the defective device region 11c (see reference) can be used. Figure 30 (B) and Figure 31 Etching is performed on (A). For example, plasma etching is performed on the interior of the through-hole 11d by providing a gas in a plasma state to the through-hole 11d of the wafer 11. Alternatively, wet etching is performed on the interior of the through-hole 11d by providing an etching solution to the through-hole 11d of the wafer 11.
[0277] As described above, in the removal step, the defective device region 11c is destroyed by irradiation with a laser beam, thus removing the defective device region 11c from the wafer 11. Furthermore, the steps included in the removal step that are omitted from description in this embodiment are the same as in Embodiment 1. Additionally, in this embodiment, steps other than the removal step (wafer preparation step, grinding step, embedding step, resin filling step, resin grinding step, wafer stacking step, dicing step, etc.) can be performed in the same manner as in Embodiment 1. Furthermore, this embodiment can be appropriately combined with other embodiments.
[0278] (Implementation Method 4)
[0279] In Embodiment 3, an example of destroying the defective device region 11c by irradiation with a laser beam during the removal step was described, but there are no limitations on the method for destroying the defective device region 11c. In this embodiment, the wafer preparation step and the grinding step (see [reference]) are described. Figure 2 The method of destroying and removing the defective device region 11c by crushing process in the removal step will then be described.
[0280] In this embodiment, there are no restrictions on the crushing process used, as long as it is possible to process the wafer 11. Hereinafter, as a specific example of crushing, a sandblasting unit 72 (see reference 72) is used. Figure 22 Sandblasting of (A) etc., using water jet unit 76 (see reference) Figure 22 (B) etc.) waterjet processing, using drilling unit 80 (refer to) Figure 22 The drilling process of (C) etc. will be explained.
[0281] Figure 32 This is a cross-sectional view showing the wafer 11 held by the stage 70. During the crushing process, a protective layer 91 is first formed on the wafer 11. For example, when processing is performed from the front side 11a of the wafer 11, the front side 11a of the wafer 11 is covered by the protective layer 91 to protect the semiconductor device 15. Alternatively, if damage to the semiconductor device 15 due to the crushing process is unlikely, the formation of the protective layer 91 can be omitted.
[0282] Next, the wafer 11 is held by the holding stage 70. For example, the wafer 11 is arranged on the holding stage 70 with its front side 11a exposed upwards and its back side 11b facing the holding surface 70a. Then, the wafer 11 held by the holding stage 70 is subjected to crushing processing.
[0283] Figure 33 (A) is a cross-sectional view showing the wafer 11 with the defective device region 11c removed by sandblasting. In the case of sandblasting, the defective device 15a (see reference 72) is removed from the sandblasting unit 72. Figure 32 Abrasive material 74 is sprayed inside the four spacer channels 13 of the wafer 11. As a result, the area struck by the abrasive material 74 of the wafer 11 is destroyed, and a cuboid groove (removal area) 105 is formed on the front side 11a of the wafer 11.
[0284] Figure 33 (B) is a cross-sectional view showing the wafer 11 with the defective device region 11c removed by water jet processing. In the case of performing water jet processing, water jet units 76 are used to process the defective device 15a (see reference 15a). Figure 32 Pressurized liquid 78 is sprayed into the inner side of the four spacer channels 13 of the wafer 11. As a result, the area hit by the liquid 78 of the wafer 11 is destroyed, and a cuboid groove 105 is formed on the front side 11a of the wafer 11.
[0285] Furthermore, the groove 105 is formed at least over the entire area where the defective device 15a is formed. Additionally, the depth of the groove 105 is adjusted such that the bottom surface of the groove 105 is formed below the lower end of the electrode 19. As a result, the defective device 15a and the electrode 19 are removed.
[0286] Figure 33 (C) is a cross-sectional view showing the wafer 11 with the defective device region 11c removed by drilling. In the case of drilling, a rotating drill bit 82 is positioned around the defective device 15a (see reference 15a). Figure 32 The four spacer channels 13 are contacted on the inner side to form a plurality of columnar grooves on the wafer 11. Furthermore, the plurality of grooves are interconnected throughout the entire area where the defective device 15a is formed. Additionally, the depth of the plurality of grooves is adjusted such that the bottom surface of the groove 105 is formed below the lower end of the electrode 19. As a result, the groove 105, composed of the interconnected plurality of grooves, is formed on the front side 11a of the wafer 11, removing the defective device 15a and the electrode 19.
[0287] As described above, a crushing process is performed on the inner side of the spacer 13 surrounding the defective device 15a, thereby destroying the defective device 15a. As a result, the defective device 15a is removed from the wafer 11.
[0288] Next, the back side 11b of the wafer 11 is ground, thereby exposing the processed area (groove 105) that has been processed by the crushing process on the back side 11b of the wafer 11. When grinding the wafer 11, the wafer 11 is first fixed to the support substrate 23. Figure 34 (A) is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. When the back side 11b of the wafer 11 is ground, the front side 11a of the wafer 11 is fixed to the support substrate 23 by means of the adhesive layer 25.
[0289] Next, through grinding device 2 (refer to...) Figure 2 The wafer 11 is ground. Specifically, the grinding tool 16 is brought into contact with the back side 11b of the wafer 11, thereby grinding the back side 11b of the wafer 11. The wafer 11 is ground and thinned until the groove 105 is exposed on the back side 11b of the wafer 11.
[0290] Figure 34 (B) is a cross-sectional view showing the wafer 11 after grinding. When the groove 105 is exposed on the back side 11b of the wafer 11, a cuboid through hole 11d is formed on the wafer 11 from the front side 11a to the back side 11b.
[0291] Alternatively, during the removal step, the through-hole 11d can be formed directly by a crushing process. Specifically, the through-hole 11d is formed from the front side 11a to the back side 11b of the wafer 11 by a crushing process.
[0292] Figure 35 (A) is a cross-sectional view showing a wafer 11 with a through-hole 11d formed by sandblasting. When the through-hole 11d is formed on the wafer 11 by crushing, an opening 70c extending vertically through the holding stage 70 is provided on the holding stage 70. Furthermore, the wafer 11 is positioned on the holding stage 70 such that the area inside the four spacer channels 13 surrounding the defective device 15a overlaps with the opening 70c.
[0293] Next, from the sandblasting unit 72, the defective device 15a (see reference) is surrounded. Figure 32 Abrasive material 74 is sprayed onto the entire area inside the four spacers 13 of the wafer 11. Furthermore, the spraying conditions of the abrasive material 74 are set to remove the area struck by the abrasive material 74 from the front side 11a to the back side 11b of the wafer 11. As a result, defective device areas 11c are removed, and through-holes 11d are formed on the wafer 11.
[0294] Figure 35(B) is a cross-sectional view showing a wafer 11 with a through-hole 11d formed by water jet processing. In the case of water jet processing, liquid 78 ejected from the water jet unit 76 is sprayed onto the defective device 15a (see reference 15a). Figure 32 The liquid 78 is sprayed over the entire area inside the four spacers 13 of the wafer 11. Furthermore, the liquid 78 is sprayed under conditions that remove the area of the wafer 11 impacted by the liquid 78 from the front side 11a to the back side 11b. As a result, the defective device area 11c is removed, and a through-hole 11d is formed on the wafer 11.
[0295] Figure 35 (C) is a cross-sectional view showing a wafer 11 with a through hole 11d formed by drilling. In the case of drilling, a rotating drill bit 82 is positioned around the defective device 15a (see reference 15a). Figure 32 The inner side of the four spacer channels 13 of the wafer 11 is in contact with the wafer 11 to form multiple columnar grooves.
[0296] Drill bit 82 processes wafer 11 until the lower end of drill bit 82 reaches the back surface 11b of wafer 11. As a result, multiple slots are formed to penetrate wafer 11 from front surface 11a to back surface 11b. Furthermore, the multiple slots are interconnected over the entire area where at least the defective device 15a is formed. This results in the formation of a through-hole 11d consisting of the interconnected multiple slots.
[0297] Additionally, in sandblasting (see...) Figure 35 In the implementation of (A), the abrasive material 74 passing through the through hole 11d of the wafer 11 is discharged through the opening 70c of the holding stage 70. Similarly, in waterjet processing (see... Figure 35 In the implementation of (B), the liquid 78 that has passed through the through hole 11d of the wafer 11 is discharged through the opening 70c of the holding stage 70. Therefore, it is possible to prevent the abrasive material 74 or the liquid 78 from colliding with the holding surface 70a of the holding stage 70 and causing damage to the holding stage 70.
[0298] Additionally, in drilling (refer to...) Figure 35 When implementing (C), the front end of the drill bit 82 is inserted into the opening 70c of the retaining table 70. Therefore, it is possible to prevent the drill bit 82 from contacting the retaining table 70 and causing damage to the retaining table 70.
[0299] In addition, Figure 35 (A) Figure 35 (B) Figure 35In (C), the case where the wafer 11 is processed from the front side 11a is shown, but the wafer 11 can also be processed from the back side 11b. That is, the abrasive material 74 or liquid 78 can collide with the back side 11b of the wafer 11, and the drill bit 82 can contact the back side 11b of the wafer 11.
[0300] Then, the wafer 11, with the defective device area 11c removed and the through hole 11d formed, is fixed to the support substrate 23. Figure 36 This is a cross-sectional view showing the wafer 11 fixed to the support substrate 23. For example, the front side 11a of the wafer 11 is fixed to the support substrate 23 by means of an adhesive layer 25.
[0301] Alternatively, etching can be performed on the wafer 11 with through-holes 11d formed through a crushing process. For example, plasma etching can be performed on the interior of the through-holes 11d by providing a plasma-state gas to the through-holes 11d of the wafer 11 (see reference). Figure 26 Additionally, by providing etching solution to the through-hole 11d of the wafer 11, wet etching is performed on the interior of the through-hole 11d. By performing etching on the wafer 11, the size of the through-hole 11d is increased, and the fine irregularities formed on the inner wall of the through-hole 11d due to the fragmentation process are removed.
[0302] The area where the wafer 11 is subjected to crushing processing is at least around the defective device 15a (see reference). Figure 32 The four spacers 13 are appropriately positioned such that through holes 11d are formed on the inner side of each spacer. Figure 37 (A) is a top view showing the area (processed area) 97C processed by sandblasting or waterjet processing. Additionally, Figure 37 (B) is a top view showing the area (machined area) 97D that is being machined by drilling. Figure 37 (A) and Figure 37 In (B), there are patterns in areas 97C and 97D.
[0303] When processing the wafer 11 by sandblasting, abrasive material 74 is sprayed onto the region 97C containing the entire defective device 15a. Similarly, when processing the wafer 11 by water jetting, liquid 78 is sprayed onto the region 97C containing the entire defective device 15a, for example. Thus, a groove 105 is formed in a manner that removes the defective device 15a (see reference). Figure 33 (A) and Figure 33 (B) or through hole 11d (refer to) Figure 35 (A) and Figure 35 (B)). In addition, the abrasive material 74 and liquid 78 can be sprayed in a manner that collides with a portion of the spacer channel 13 surrounding the defective device 15a.
[0304] When processing wafer 11 by drilling, drill bit 82 sequentially processes multiple regions 97D that overlap with defective device 15a. Furthermore, each of the multiple regions 97D is configured to overlap with a portion of another adjacent region 97D. Thus, a groove 105 is formed in a manner that removes defective device 15a (see reference). Figure 33 (C)) or through hole 11d (refer to) Figure 35 (C)). In addition, drill bit 82 can contact a portion of the spacer channel 13 surrounding defective device 15a.
[0305] Furthermore, when processing the wafer 11 by drilling, the drill bit 82 can be inserted into the interior of the wafer 11 (see reference). Figure 33 (C) and Figure 35 (C) causes the drill bit 82 to rotate while moving horizontally, thereby forming a groove 105 or a through hole 11d. In this case, it is not necessary to raise and lower the drill bit 82 multiple times.
[0306] Then, an etching process (such as plasma etching, reference) is performed on the wafer 11. Figure 26 This process etches the inner wall of the through-hole 11d. As a result, the fine irregularities remaining in the fractured areas 97C and 97D are removed, and the width of the through-hole 11d is increased, forming a shape similar to... Figure 37 (A) and Figure 37 The enlarged through-hole 11d is shown in (B).
[0307] As described above, in the removal step, the defective device region 11c can be removed from the wafer 11 by breaking it up through a crushing process. Furthermore, the steps included in the removal step that are omitted from description in this embodiment are the same as in Embodiment 1. Additionally, in this embodiment, steps other than the removal step (wafer preparation step, grinding step, embedding step, resin filling step, resin grinding step, wafer stacking step, dicing step, etc.) can be performed in the same manner as in Embodiment 1. Furthermore, this embodiment can be appropriately combined with other embodiments.
[0308] (Implementation Method 5)
[0309] In this embodiment, the relationship between the process of removing the defective device region 11c from the wafer 11 (removal step) and the process of fixing the wafer 11 to the support substrate 23 (support substrate fixing step) will be explained. Specifically, in this embodiment, the process of fixing the wafer 11 to the support substrate 23 after removing the defective device region 11c from the wafer 11 will be described in detail.
[0310] First, the wafer 11 prepared in the preparation step is ground as needed (see reference). Figure 2 (Grinding step). Furthermore, the defective device region 11c is removed from the wafer 11 by performing laser processing, crushing processing, or other processing (removal step). Then, the wafer 11 with the through hole 11d formed by removing the defective device region 11c is fixed to the support substrate 23 (support substrate fixing step).
[0311] Laser processing can be used to remove the defective device region 11c. For example, the defective device region 11c can be separated from the wafer 11 by laser processing (see reference). Figure 12 (A) Figure 13 (A) etc.), and then the wafer 11 is fixed to the support substrate 23 (see reference). Figure 12 (B) Figure 13 (B) etc.). Additionally, for example, defective device region 11c can be destroyed by laser processing (see [reference]). Figure 31 (A) etc.), and then the wafer 11 is fixed to the support substrate 23 (see reference). Figure 31 (B) etc.
[0312] Alternatively, a crushing process can be used to remove the defective device region 11c. For example, the defective device region 11c can be separated from the wafer 11 by a crushing process (see reference). Figure 24 (A) Figure 24 (B) Figure 24 (C) etc.), and then the wafer 11 is fixed to the support substrate 23 (see reference). Figure 25 (etc.). Additionally, for example, the defective device region 11c can be destroyed by a crushing process (see...). Figure 35 (A) Figure 35 (B) Figure 35 (C) etc.), and then the wafer 11 is fixed to the support substrate 23 (see reference). Figure 36 wait).
[0313] Furthermore, a device chip 59 is embedded in the through-hole 11d of the wafer 11 fixed to the support substrate 23 (embedding step, see reference). Figures 16-18 (C, etc.). Thus, a wafer 11 without defective device 15a is manufactured.
[0314] As described above, when the support substrate fixing step is performed after the removal step, the defective device region 11c has already been removed from the wafer 11 when the wafer 11 is fixed to the support substrate 23. Therefore, after the wafer 11 is fixed to the support substrate 23, it is not necessary to perform processing for removing the defective device region 11c. As a result, it is possible to prevent the debris (processing debris) generated by the processing of the wafer 11 from adhering to the support substrate 23, and to prevent the processing debris adhering to the support substrate 23 from hindering the insertion of the device chip 59 into the through hole 11d.
[0315] Furthermore, there are no limitations on the method for fixing the wafer 11 to the support substrate 23. For example, the wafer 11 can be fixed to the support substrate 23 by means of an adhesive layer 25. As described above, the adhesive layer 25 can be, for example, an adhesive formed of a thermosetting resin, an adhesive formed of a thermoplastic resin, an adhesive formed of a UV-curable resin, a sheet (thermo-pressed sheet) that does not contain adhesive and can be fixed to the wafer 11 and the support substrate 23 by heating and pressurizing, a strip with a thermally foamed layer, etc.
[0316] Then, the resin filling steps are performed sequentially (refer to...). Figure 19 (A)), resin grinding steps (refer to) Figure 19 (B)), wafer stacking steps (refer to) Figure 20 ), Segmentation steps (refer to) Figure 21 (A)). Thus, a stacked device chip 81 having multiple stacked semiconductor devices is manufactured (see reference). Figure 21 (B)
[0317] As described above, by performing the support substrate fixing step after the removal step, it is possible to prevent processing debris from adhering to the support substrate 23, and the operation of embedding the device chip 59 in the wafer 11 can be performed smoothly. Furthermore, the steps in each of the removal step and the support substrate fixing step that are omitted from description in this embodiment are the same as in Embodiment 1. Additionally, in this embodiment, steps other than the removal step and the support substrate fixing step (wafer preparation step, grinding step, embedding step, resin filling step, resin grinding step, wafer stacking step, dicing step, etc.) can be performed in the same manner as in Embodiment 1. Furthermore, this embodiment can be appropriately combined with other embodiments.
[0318] (Implementation Method 6)
[0319] In this embodiment, the relationship between the process of removing the defective device region 11c from the wafer 11 (removal step) and the process of fixing the wafer 11 to the support substrate 23 (support substrate fixing step) will be explained. Specifically, in this embodiment, the process of removing the defective device region 11c from the wafer 11 after fixing the wafer 11 to the support substrate 23 will be described in detail.
[0320] First, the wafer 11 prepared in the preparation step is ground as needed (see reference). Figure 2 (Grinding step). Then, the wafer 11 is fixed to the support substrate 23 (support substrate fixing step). Then, the wafer 11 is subjected to laser processing, crushing processing and other processing, thereby removing the defective device area 11c from the wafer 11 (removal step).
[0321] Laser processing can be used to remove defective device regions 11c. For example, laser processing can be performed on the wafer 11 fixed to the support substrate 23 (see reference). Figure 4 (A) etc.), and then the defective device region 11c is separated from the wafer 11 (refer to (A) etc.). Figure 8 (B) etc. Additionally, for example, plasma etching is performed on the wafer 11 fixed to the support substrate 23 (see [reference]). Figure 14 (B) etc.), and then remove the defective device region 11c from the wafer 11 (refer to Figure 8 (B) etc.
[0322] Additionally, for example, a wafer 11 with grooves formed by laser processing or crushing is fixed to a support substrate 23 (see reference). Figure 11 (A) Figure 23 (A), etc. Then, the wafer 11 is ground (see reference). Figure 11 (B) Figure 23 (B) etc., remove defective device region 11c from wafer 11.
[0323] Furthermore, there are no limitations on the method for fixing the wafer 11 to the support substrate 23. For example, the wafer 11 can be fixed to the support substrate 23 by means of an adhesive layer 25. As described above, the adhesive layer 25 can be, for example, an adhesive formed of a thermosetting resin, an adhesive formed of a thermoplastic resin, an adhesive formed of a UV-curable resin, a sheet (thermo-pressed sheet) that does not contain adhesive and can be fixed to the wafer 11 and the support substrate 23 by heating and pressurizing, a strip with a thermally foamed layer, etc.
[0324] Furthermore, a device chip 59 is embedded in the through-hole 11d of the wafer 11 fixed to the support substrate 23 (embedding step, see reference). Figures 16-18 (C)). Thus, a wafer 11 without defective device 15a is manufactured.
[0325] As described above, when the removal step is performed after the support substrate fixing step, the wafer 11 is supported on the support substrate 23 after the defective device region 11c has been removed from the wafer 11. Therefore, the embedding step can be performed continuously thereafter, and the embedding of the device chip 59 can be performed smoothly.
[0326] Furthermore, if a removal step is performed after the support substrate fixing step, a grinding process for separating the defective device region 11c from the wafer 11 is performed after the operation of fixing the wafer 11 to the support substrate 23 (see reference). Figure 11 (B) Figure 23 (B, etc.). Therefore, it is not necessary to transport and attach the thin and easily deformable wafer 11 to the support substrate 23, which can improve work efficiency and prevent wafer breakage.
[0327] Then, the resin filling steps are performed sequentially (refer to...). Figure 19 (A)), resin grinding steps (refer to) Figure 19 (B)), wafer stacking steps (refer to) Figure 20 ), Segmentation steps (refer to) Figure 21 (A)). Thus, a stacked device chip 81 having multiple stacked semiconductor devices is manufactured (see reference). Figure 21 (B)
[0328] As described above, by performing the removal step after the support substrate fixing step, the transition to the subsequent embedding step can be smoothly achieved. Furthermore, the steps included in the support substrate fixing and removal steps that are omitted from description in this embodiment are the same as in Embodiment 1. Additionally, in this embodiment, steps other than the support substrate fixing and removal steps (wafer preparation step, grinding step, embedding step, resin filling step, resin grinding step, wafer stacking step, dicing step, etc.) can be performed in the same manner as in Embodiment 1. Furthermore, this embodiment can be appropriately combined with other embodiments.
[0329] Furthermore, the structures and methods of the above-described embodiments can be appropriately modified and implemented as long as they do not depart from the scope of the present invention.
Claims
1. A method for manufacturing a wafer, characterized in that, The manufacturing method of this wafer includes the following steps: The wafer preparation step involves preparing a wafer in which semiconductor devices are formed in multiple regions divided by intersecting multiple spacers. The removal step separates the defective device region from the wafer, the defective device region comprising the semiconductor devices identified as defective among the plurality of semiconductor devices formed on the wafer; as well as The embedding step involves embedding a device chip, which has a good semiconductor device and is sized to fit into a through-hole formed by separating the defective device region from the wafer, into the through-hole. The good semiconductor device has the same function as the semiconductor device that was determined to be defective. The removal step includes the following steps: by continuously irradiating the laser beam along four straight paths and stopping the irradiation after each irradiation, the laser beam is intermittently irradiated along the spacer surrounding the semiconductor device that is determined to be defective, and the four straight paths are along the four spacer surrounding the semiconductor device that is determined to be defective.
2. The method for manufacturing a wafer according to claim 1, characterized in that, In this removal step, with the focal point of the laser beam of a wavelength that is transparent to the wafer positioned inside the wafer, the laser beam is irradiated along the spacer, thereby forming a modified layer along the spacer that functions as the starting point for separation of the defective device region.
3. The method for manufacturing a wafer according to claim 1, characterized in that, In this removal step, with the focal point of the laser beam of a wavelength that is absorbent to the wafer positioned on the spacer, the laser beam is irradiated along the spacer, thereby removing the area of the wafer along the spacer.
4. The method for manufacturing a wafer according to claim 1, characterized in that, In this removal step, with the focal point of the laser beam having an absorptive wavelength for the wafer positioned inside a liquid column formed by spraying liquid toward the wafer, the laser beam is irradiated along the spacer via the liquid column, thereby removing the area of the wafer along the spacer.
5. The method for manufacturing a wafer according to any one of claims 1 to 4, characterized in that, The wafer manufacturing method also includes the following grinding step: before performing the removal step, a protective member is attached to the first side of the wafer on which the semiconductor device is formed, and the second side of the wafer located on the opposite side of the first side is ground to thin the wafer to a specified thickness.
6. The method for manufacturing a wafer according to any one of claims 1 to 4, characterized in that, In this removal step, the second side of the wafer, located opposite to the first side where the semiconductor device is formed, is ground, thereby exposing the processed area or cracks that have developed from the processed area by the laser beam on the second side of the wafer.
7. The method for manufacturing a wafer according to any one of claims 1 to 4, characterized in that, In this removal step, an etching solution is provided to the processed area or the cracks that develop from the processed area after being irradiated by the laser beam.
8. The method for manufacturing a wafer according to any one of claims 1 to 4, characterized in that, In this removal step, a plasma-entrained gas is provided to the processed area or the cracks that develop from the processed area after being irradiated by the laser beam.
9. The method for manufacturing a wafer according to any one of claims 1 to 4, characterized in that, The manufacturing method of this chip also includes the following steps: The resin filling step involves filling the gap between the device chip and the wafer with resin after the embedding step; and The resin grinding step involves grinding the resin formed on the outside of the gap after the resin filling step.
10. A method for manufacturing a stacked device chip, characterized in that, The method for manufacturing this stacked device chip includes the following steps: The wafer preparation step involves preparing a first wafer and a second wafer, wherein semiconductor devices are formed on the first wafer and the second wafer in multiple regions divided by multiple intersecting spacers. The removal step separates the defective device region from the first wafer, the defective device region comprising the semiconductor devices identified as defective among the plurality of semiconductor devices formed on the first wafer; In the embedding step, a device chip having a good semiconductor device and being able to be embedded into a through-hole formed by separating the defective device region from the first wafer is embedded into the through-hole, the good semiconductor device having the same function as the semiconductor device that was judged to be defective. In the wafer stacking step, the second wafer is stacked on the first wafer, thereby forming a stacked wafer; as well as The dicing step involves dicing the stacked wafer along the spacer, thereby forming a stacked device chip having multiple stacked semiconductor devices. The removal step includes the following steps: by continuously irradiating the laser beam along four straight paths and stopping the irradiation after each irradiation, the laser beam is intermittently irradiated along the spacer surrounding the semiconductor device that is determined to be defective, and the four straight paths are along the four spacer surrounding the semiconductor device that is determined to be defective.
Citation Information
Patent Citations
Method for manufacturing laminated device
JP2012134334A
System and method for providing 3D wafer assembly with known-good-dies
US20170186730A1
Wafer dicing methods
US20180233410A1