Battery cell manufacturing method

By setting a solder layer on the surface of the tabs of the battery core and using induction welding technology, the problem of metal slag generated in the welding of full-lug cylindrical battery cores is solved, an efficient and environmentally friendly welding process is achieved, the production efficiency is improved and the cost is reduced. .

CN114530673BActive Publication Date: 2024-10-11GUANGZHOU XIAOPENG MOTORS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210156825.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-02-21
Publication Date
2024-10-11
Estimated Expiration
2042-02-21

AI Technical Summary

Technical Problem

During the welding process of the tabs and current collecting plates of full-lug cylindrical batteries, a large amount of metal slag is produced, which has become a problem in the electric vehicle power battery industry.

Method used

By setting a solder layer on the surface of the tab, the current collecting plate and the tab are inductively welded together using the solder layer to avoid the generation of metal slag. Tin powder slurry is used as the solder, and the tin powder layer is formed by coating, and is achieved through eddy current welding. welding.

Benefits of technology

It achieves a welding process without metal slag, improves production efficiency and reduces costs, while avoiding chemical reactions between tin and electrolyte, ensuring environmental protection and stable performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114530673B_ABST
    Figure CN114530673B_ABST
Patent Text Reader

Abstract

An embodiment of the present invention provides a method for manufacturing a battery cell. The method comprises: providing a winding core including a pole piece, wherein the pole piece comprises an electrode and a pole ear protruding from one side of the electrode, and a solder layer is provided on the surface of the pole ear; abutting a current collector plate against the pole ear; and induction welding the current collector plate and the pole ear together through the solder layer. In the method, the process flow of welding the current collector plate and the pole ear does not generate metal slag, and the production efficiency is high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of batteries, and in particular to a method for manufacturing a battery cell. Background Art

[0002] With the development of society and people's increasing attention to environmental protection, electric vehicles have been more and more widely used. The power batteries used in electric vehicles usually use lithium-ion batteries, which have the characteristics of high energy density and large single-cell energy.

[0003] As electric vehicles further improve their requirements for power output performance, higher requirements are placed on the single cells that provide power: high power and high energy density. In order to achieve high power output, uniform current density, and fast heat dissipation, multi-pole and full-pole batteries are currently developed. Full-pole cylindrical cells have the advantages of low internal resistance and welds that can withstand high-rate charge and discharge shocks, and are a development direction for power batteries in the future. However, the welding between the pole tabs and the collector plates of full-pole cylindrical cells has problems such as the generation of more metal slag, which has become a problem for the industry. Summary of the invention

[0004] The object of the present invention is to provide a method for manufacturing a battery core, which can prevent metal slag from being generated during the welding process between a current collecting plate and a pole ear of the battery core.

[0005] In one aspect of the present invention, there is provided a method for manufacturing a battery cell, comprising:

[0006] A winding core including a pole piece is provided, wherein the pole piece includes an electrode and a pole ear protruding from one side of the electrode, and a solder layer is provided on a surface of the pole ear;

[0007] Abutting the current collecting plate against the pole ear;

[0008] The current collecting plate and the tab are induction welded together through a solder layer.

[0009] The above-mentioned process flow of welding the current collecting plate and the pole ear does not generate metal slag, and has high production efficiency and low cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 A schematic diagram of a process for manufacturing a battery cell according to an embodiment of the present invention;

[0011] Figure 2 It is a schematic diagram of the structure of the solder layer at the anode tab of an unwound anode sheet;

[0012] Figure 3 It is a schematic diagram of the structure of the solder layer at the cathode ear of an unwound cathode sheet;

[0013] Figure 4 for Figure 1A schematic diagram of the structure when the current collecting plate and the pole ear are connected in the battery cell manufacturing method shown;

[0014] Figure 5 It is a schematic diagram of the winding core structure after the tab is shaped and before welding;

[0015] Figure 6 for Figure 1 A schematic diagram of the cross-sectional structure when the anode current collector plate and the anode tab are in contact with each other in the battery cell manufacturing method shown;

[0016] Figure 7 for Figure 1 A schematic diagram of the cross-sectional structure when the cathode current collector and the cathode tab abut against each other in the battery cell manufacturing method shown; and

[0017] Figure 8 for Figure 1 A schematic diagram of the cross-sectional structure of a battery cell produced by the battery cell manufacturing method shown. DETAILED DESCRIPTION

[0018] In order to further explain the technical methods and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention are described in detail below in conjunction with the accompanying drawings and embodiments.

[0019] Figure 1 The figure is a flow chart of a method for manufacturing a battery cell according to an embodiment of the present invention. The method for manufacturing a battery cell according to an embodiment of the present invention comprises the following steps:

[0020] S11, providing a winding core including a pole piece, wherein the pole piece includes an electrode and a pole ear protruding from one side of the electrode, and a solder layer is provided on a surface of the pole ear;

[0021] S13, contacting the current collecting plate with the pole ear;

[0022] S15, induction welding the collector plate and the tab together through the solder layer.

[0023] In step S11, the tab protrudes from one side of the electrode, so that the tab protrudes from the end of the winding core. Specifically, a plurality of tabs are arranged at intervals on one side of the electrode, so that the manufactured battery cell is a full-tab or tab-free battery cell; the winding core also includes a diaphragm, and the pole piece and the diaphragm are stacked and wound to form a cylindrical winding core, so the manufactured battery cell is a cylindrical battery cell.

[0024] In this embodiment, the above step S11 further includes the following steps:

[0025] S112, coating solder on the pole lug of the pole piece to form a solder layer.

[0026] Specifically, the solder may be a tin powder paste, which includes tin powder, an adhesive and a solvent. The solder layer formed in this way is a tin powder layer 119 (see Figure 2 or 3). Specifically, the tin powder paste includes PVDF (polyvinylidene fluoride), tin powder and NMP (N-methylpyrrolidone). More specifically, the components of the tin powder paste include 5% to 18% by mass of PVDF, 15% to 30% by mass of tin powder and 65% to 75% by mass of NMP. More specifically, in one embodiment, the components of the tin powder paste include 5% by mass of PVDF, 25% by mass of tin powder and 70% by mass of NMP; in another embodiment, the components of the tin powder paste include 10% by mass of PVDF, 20% by mass of tin powder and 70% by mass of NMP.

[0027] Specifically, the particle size of the tin powder can be 3 microns to 5 microns. PVDF plays the role of an adhesive and a stabilizer, and NMP is used as a solvent. By setting the components of the tin powder slurry, the tin powder can be evenly and stably coated. It is understood that the tin powder slurry can also be replaced by other types of solder, such as copper-zinc alloy, silver-copper alloy, etc. Specifically, the thickness of the tin powder layer 119 can be 40±10 microns.

[0028] S114, stacking and winding the pole pieces and the diaphragm to form a cylindrical winding core.

[0029] In this embodiment, the electrode sheet includes an anode sheet and a cathode sheet. Figure 2 The anode sheet includes an anode 112 and an anode tab 117, and a plurality of anode tabs 117 are arranged at intervals on one side edge of the anode 112; please refer to Figure 3 The cathode sheet includes a cathode 114 and a cathode tab 118 , and a plurality of cathode tabs 118 are arranged at intervals on one side edge of the cathode 114 .

[0030] The first active material 123 is coated on the surface of the anode 112 (see Figure 5 ), a second active material 125 is coated on the surface of the cathode 114 (see Figure 5 ). Specifically, for a lithium-ion battery, the first active material 123 may be graphite, and the second active material 125 may be a lithium composite metal oxide such as lithium manganate or lithium iron phosphate. Under the action of the electrolyte, ions between the first active material 123 and the second active material 125 of the lithium-ion battery migrate to achieve charging and discharging.

[0031] Please refer again Figure 2 and Figure 3 For example, a ceramic layer 121 is coated at the junction of the cathode tab 118 and the cathode 114 at one side edge of the cathode 114, a solder is coated on the anode tab 117, and a solder is coated on the surface of the cathode tab 118 outside the edge of the ceramic layer 121. Specifically, the material of the ceramic layer 121 may be AT9 or AT11, and the main components of AT9 and AT11 may be Al2O3.

[0032] Please refer to Figure 4 and Figure 5 In this embodiment, the separator 116 is stacked between the anode sheet and the cathode sheet and wound to form a cylindrical winding core 11. Specifically, when stacked, the anode tab 117 of the anode sheet faces one side, and the cathode tab 118 of the cathode sheet faces the opposite other side, so that the anode tab 117 and the cathode tab 118 are respectively located at the two ends of the winding core 11 after winding.

[0033] Before step S13, the tabs are shaped so that the tabs are bent toward the center of the winding core. Figure 5 , the anode tab 117 and the cathode tab 118 are shaped so that the anode tab 117 and the cathode tab 118 are bent toward the center of the winding core 11. More specifically, the bending angle of the anode tab 117 and the cathode tab 118 can be 5° to 45°, that is, the angle between the anode tab 117 and the cathode tab 118 and the axial direction of the winding core 11 can be 5° to 45°. Bending the anode tab 117 and the cathode tab 118 at a certain angle can facilitate the tabs to abut against the current collecting plate.

[0034] In this embodiment, please refer to Figure 6 and Figure 7 , step S13 specifically includes: providing an anode current collector plate 13 and a cathode current collector plate 15, abutting the anode current collector plate 13 with the anode pole ear 117, and abutting the cathode current collector plate 15 with the cathode pole ear 118. The anode current collector plate 13 and the anode pole ear 117 can be clamped together by a clamp, and the cathode current collector plate 15 and the cathode pole ear 118 can be clamped together. Specifically, the clamp is made of a non-metallic material. Specifically, the thickness of the anode current collector plate 13 and the cathode current collector plate 15 is less than 0.5 mm, so that excessive heat can be prevented from being conducted to the coating area of ​​the first active material 123 of the anode 112 and the second active material 125 of the cathode 114, thereby affecting the performance of the first active material 123 and the second active material 125.

[0035] Specifically, in step S13, the current collecting plate is brought into contact with the pole ear. It is understandable that the current collecting plate can also be brought into close contact with the pole ear, and the pole ear will be squeezed to a certain extent, which will make the electrical connection performance between the current collecting plate and the pole ear better. Specifically, after the anode current collecting plate 13 is in close contact with the anode pole ear 117, and the cathode current collecting plate 15 is in close contact with the cathode pole ear 118, the bent anode pole ear 117 and cathode pole ear 118 are squeezed into a shape with a circular arc cross section. The anode pole ear 117 and the cathode pole ear 118 are squeezed to form a certain rebound effect, which can ensure that the pole ear is in good contact with the current collecting plate and ensure good electrical connection performance.

[0036] In this embodiment, step S15 is specifically as follows: Figure 8, the anode current collector plate 13 and the anode pole ear 117, the cathode current collector plate 15 and the cathode pole ear 118 are respectively induction welded together through the solder layer. Induction welding can melt the solder layer, thereby welding the anode current collector plate 13 and the anode pole ear 117, and the cathode current collector plate 15 and the cathode pole ear 118 together. Specifically, induction welding includes eddy current welding. Of course, induction welding can also be other feasible methods known in the art. When performing eddy current welding, please refer to Figure 6 and Figure 7 , place the anode current collector plate 13 and the anode pole ear 117 in the coil 30 of the eddy current welding machine, and place the cathode current collector plate 15 and the cathode pole ear 118 in the coil 30 of the eddy current welding machine. During the eddy current welding process, induced eddy currents are generated on the surface of the anode current collector plate 13, the anode pole ear 117 and the tin powder layer 119, and the temperature can reach 240°C within 0.2 seconds. The tin powder layer 119 melts, and the anode current collector plate 13 and the anode pole ear 117 can be welded together. The same is true for welding the cathode current collector plate 15 and the cathode pole ear 118, which will not be repeated here. Specifically, during welding, the area of ​​the anode 112 coated with the first active material 123 and the area of ​​the cathode 114 coated with the second active material 125 are located outside the magnetic field of the coil 30 to avoid affecting the performance of the first active material 123 and the second active material 125.

[0037] In this embodiment, when the solder is tin powder paste, the battery cell manufacturing method embodiment further includes the following steps:

[0038] Before step S15, the solder layer is dried to remove the solvent, leaving only the adhesive and tin powder in the solder layer.

[0039] In the battery cell manufacturing method of the embodiment of the present invention, the process flow of welding the current collecting plate and the pole ear does not produce metal slag and has high production efficiency. At the same time, environmentally friendly tin is used as the welding medium. Tin does not chemically react with the electrolyte, is pollution-free, has low cost, and can be used on a large scale.

[0040] The above are only preferred embodiments of the present invention, and are not intended to limit the present invention in any form. Although the present invention has been disclosed as above in preferred embodiments, it is not intended to limit the present invention. Any technician familiar with the profession can make some changes or modifications to equivalent embodiments of equivalent changes using the technical contents disclosed above without departing from the scope of the technical solution of the present invention. However, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A method for manufacturing a battery cell, characterized in that: The battery cell manufacturing method comprises: A winding core comprising a pole piece is provided, wherein the pole piece comprises an electrode and a pole ear protruding from one side of the electrode, a solder layer is provided on a surface of the pole ear, the pole piece comprises an anode piece and a cathode piece, the anode piece comprises an anode (112) and an anode pole ear (117), and the cathode piece comprises a cathode (114) and a cathode pole ear (118); Abutting the current collecting plate against the pole ear; Induction welding the current collecting plate and the tab together through a solder layer, wherein the solder layer is melted by the induction welding during the induction welding process; Before the current collecting plate is brought into contact with the pole lug, the anode pole lug (117) and the cathode pole lug (118) are bent toward the center of the winding core; The step of abutting the current collecting plate against the pole ear is specifically as follows: providing an anode current collecting plate (13) and a cathode current collecting plate (15), abutting the anode current collecting plate (13) against the anode pole ear (117), and abutting the cathode current collecting plate (15) against the cathode pole ear (118), so that the bent anode pole ear (117) and the cathode pole ear (118) are extruded into a shape with a circular arc cross section.

2. The method for manufacturing a battery cell according to claim 1, wherein: The induction welding includes eddy current welding.

3. The method for manufacturing a battery cell according to claim 1 or 2, characterized in that: The step of providing a winding core including a pole piece further comprises: Applying solder on the tab to form the solder layer; The pole pieces and the separator are stacked and wound to form a cylindrical winding core.

4. The method for manufacturing a battery cell according to claim 3, wherein: A first active material (123) is coated on the surface of the anode (112), and a second active material (125) is coated on the surface of the cathode (114).

5. The method for manufacturing a battery cell according to claim 4, characterized in that: A plurality of anode tabs (117) are arranged at intervals on one side edge of the anode (112), and a plurality of cathode tabs (118) are arranged at intervals on one side edge of the cathode (114); A ceramic layer (121) is coated on the junction of the cathode electrode (118) and the cathode (114), the solder is coated on the anode electrode (117), and the solder is coated on the surface of the cathode electrode (118) outside the edge of the ceramic layer (121).

6. The method for manufacturing a battery cell according to claim 3, characterized in that: The solder includes tin powder slurry, which includes tin powder, an adhesive and a solvent. Polyvinylidene fluoride is used as an adhesive, and N-methylpyrrolidone is used as a solvent. The components of the tin powder slurry include 5% to 18% of the polyvinylidene fluoride, 15% to 30% of the tin powder and 65% to 75% of the N-methylpyrrolidone in mass percentage.

7. The method for manufacturing a battery cell according to claim 6, wherein: Before the current collecting plate and the pole tab are welded together, the solder layer is dried to remove the solvent.

8. The method for manufacturing a battery cell according to claim 3, characterized in that: The solder layer is a tin powder layer (119), and the thickness of the tin powder layer (119) is 40±10 micrometers; the thickness of the current collecting plate is less than 0.5 millimeters.