A ceramic plate cleaning liquid and its preparation method and application
By preparing epoxy succinate and end-capped polyether copolymers with high acidity and good water solubility, the problems of slow reaction speed and poor cleaning effect of ceramic plate cleaning solutions are solved, achieving fast and efficient cleaning of ceramic plates and avoiding the need for ceramic plate cleaning. Plate etching significantly improves the cleaning effect.
Patent Information
- Application Number
- CN202210328242.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-31
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-03-31
AI Technical Summary
The existing ceramic plate cleaning solutions have slow reaction speed and poor cleaning effect, and commonly used metal ion complexing agents and organic acids can easily etch the ceramic plate during the cleaning process, affecting the smoothness.
Maleic anhydride is used as raw material, epoxy succinate is prepared through epoxidation reaction, and free radical copolymerization is carried out with end-capped polyether to prepare a ceramic plate cleaning solution with high acidity and good water solubility, and utilizes its good Solubility and anti-scaling properties for ceramic plate cleaning.
It achieves rapid cleaning of ceramic plates with high cleanliness and avoids etching of ceramic plates. The cleaning fluid has good solubility for oil-soluble and water-soluble impurities, significantly improving the cleaning effect.
Smart Images

Figure CN114621082B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of ceramics, and more specifically, relates to a ceramic plate cleaning liquid and a preparation method and application thereof. Background Art
[0002] In TFT-LCD manufacturing, in processes such as dry etching and PECVD, ceramic plates are often used to isolate the reaction chamber to prevent the byproducts of the reaction between the upper electrode and the frame from falling and causing product defects. However, the high-energy fluorine-containing plasma in the reaction process will corrode the equipment cavity and the components in the cavity, shortening the service life of the components. At the same time, the non-volatile fluorides produced during the corrosion process are deposited on the surface of the components and finally fall off as impurity particles, affecting the cleanliness of the chamber. Therefore, these components, including ceramic plates, must be cleaned regularly. At the same time, the non-volatile fluorides produced during the corrosion process not only exist on the surface of the ceramic plate, but also enter the interior of the ceramic plate. In this way, general ceramic cleaning methods such as grinding and polishing are difficult to achieve the purpose of thorough cleaning, so it is necessary to explore a liquid that can achieve thorough cleaning of ceramic plates in plasma chambers.
[0003] At present, the method of cleaning ceramic plates is to first scrape with a scraper and then clean with alkali. This method is easy to cause scratches on the surface of the ceramic plate, breakage of the micropore edges, long cleaning time, low production efficiency, and difficulty in cleaning the inner wall of the micropores.
[0004] After searching, the patent publication number is CN108410590A, and the publication date is August 17, 2018. The invention discloses a cleaning agent and its application in cleaning ceramic filter plates. The cleaning agent mainly includes the following components: a metal ion complexing agent, an organic penetrant, a main agent A and a main agent B. The main agent A is at least one of the water-soluble organic acids, and the main agent B is a soluble salt corresponding to the main agent A. The main agent B in this cleaning agent can promote the dissolution of the insoluble metal salt of the main agent A in the aqueous solution, thereby enhancing the cleaning effect. The metal ion complexing agent and the organic penetrant can produce a synergistic effect, dissolve the fine-grained metal minerals that block the filter pores, and clean the insoluble attachments and organic agents. The disadvantage is that the metal ion complexing agent and the organic acid will inevitably etch the surface of the ceramic filter plate while removing the impurity particles on the ceramic plate, thereby affecting the smoothness of the ceramic plate.
[0005] In addition, Chen Yiyi [Chen Yiyi, Synthesis and Performance Research of Biodegradable Polyether Water Treatment Agent, PhD Dissertation, Southeast University, 2019.] disclosed that maleic anhydride (MA) was used as raw material, hydrogen peroxide was used as oxidant, sodium tungstate was used as catalyst, and sodium epoxysuccinate (ESA) monomer was synthesized by epoxidation reaction, and then water was used as reaction solvent, ammonium persulfate was used as initiator, ESA and oxalic acid end-capped polyether (APEM) or 2-acrylamide-2-methylpropanesulfonic acid (AMPS), allyl polyoxyethylene ammonium sulfonate (APES) were used as monomers, and biodegradable polyether water treatment agents ESA-APEM and ESA-AMPS-APES were prepared by free radical copolymerization, which were used in the scale inhibition of calcium carbonate and calcium sulfate. However, the polymer has weak acidity, and there are problems of slow reaction speed and poor cleaning effect when used in the cleaning process of ceramic plates. Summary of the invention
[0006] 1. Problem to be solved
[0007] In view of the problems of slow reaction speed and poor cleaning effect of existing ceramic plate cleaning liquid, the present invention provides a ceramic plate cleaning liquid and a preparation method and application thereof. The prepared ceramic plate cleaning liquid has high acidity and good water solubility, is applied to the cleaning of ceramic plates, has a fast cleaning speed and a high degree of cleanliness.
[0008] 2. Technical solution
[0009] In order to solve the above problems, the technical solution adopted by the present invention is as follows:
[0010] The invention uses maleic anhydride as a raw material, performs an epoxidation reaction under the action of an oxidant and a solid acid catalyst to prepare epoxy succinate; uses a polyacid to end-cap the olefin ether to prepare an end-capped polyether; uses epoxy succinate and the end-capped polyether as monomers, performs a free radical copolymerization reaction in the presence of an initiator to prepare a ceramic plate cleaning liquid.
[0011] The structural formula of the polymer of epoxy succinate and end-capped polyether is Wherein, x=1-5, y=1-3, and the values of x and y are adjusted by controlling the addition amount of epoxy succinate and end-capped polyether. Where n = 1-5,
[0012] The present invention provides a method for preparing a ceramic plate cleaning liquid:
[0013] Step a, preparing epoxy succinate: at room temperature, based on the molar amount of maleic anhydride, the molar ratio of sodium alcohol to maleic anhydride (5-10): 1, maleic anhydride is slowly added dropwise to the sodium alcohol solution, the molar ratio of solid acid catalyst to maleic anhydride (0.1-0.3): 1, the solid acid catalyst is continuously added, the molar ratio of oxidant to maleic anhydride (0.5-2): 1, the oxidant is continuously added, the reaction is carried out at 60-120° C. for 6-24 hours, the reaction is cooled to room temperature after completion, suction filtered, washed with ethanol solution for multiple times and then dried to obtain epoxy succinate;
[0014] Step b, preparing the blocked polyether: at room temperature, in a N2 atmosphere, based on the molar amount of the blocked ether, the polyacid and the blocked ether are added into a reaction kettle at a molar ratio of (5-8):1, and reacted at 50-90° C. for 0.5-6 h. After the reaction is completed, the blocked polyether is cooled to room temperature to obtain the blocked polyether;
[0015] Step c, preparing a ceramic plate cleaning solution: at room temperature, based on the molar amount of epoxy succinate, according to the molar ratio of the blocked polyether to the epoxy succinate of 0.2 to 5:1, add the epoxy succinate and the blocked polyether to the reactor, according to the molar ratio of the initiator to the epoxy succinate of 0.01 to 0.05:1, add the initiator dropwise to the reactor, react at 60 to 150° C. for 2 to 8 hours, cool to room temperature after the reaction, and obtain a ceramic plate cleaning solution.
[0016] Wherein, the sodium alcohol in step a is selected from any one or more of sodium methoxide, sodium ethoxide, and sodium n-propoxide, wherein sodium ethoxide and sodium n-propoxide are preferred. Maleic anhydride can be better miscible with sodium ethoxide and sodium n-propoxide, which is beneficial to increase the reaction rate and reduce the occurrence of side reactions.
[0017] The solid acid catalyst is selected from any one or more of aluminum chloride, Y molecular sieve, and sodium tungstate. The use of aluminum chloride as a catalyst is conducive to improving the reaction rate, the use of Y molecular sieve as a catalyst has high selectivity for the target product, and the catalyst is easy to separate after the reaction.
[0018] The oxidant is selected from one or more of hydrogen peroxide, ozone, and potassium permanganate, preferably ozone and potassium permanganate, wherein ozone is a gaseous oxidant and potassium permanganate is a solid oxidant. Compared with liquid hydrogen peroxide oxidizing agent, the reaction is easier to control, and excess oxidant is easy to separate from the reaction system, thereby avoiding damage to the surface of the ceramic plate by excess oxidant in the cleaning solution.
[0019] The polyacid in step b is selected from one or more of oxalic acid, adipic acid, and trisaccharic acid. Different polyacids can adjust the type of end-capping functional groups in the end-capped polyether, thereby adjusting the cleaning ability of the cleaning solution, and preparing corresponding cleaning solutions for ceramic plates with different degrees of contamination.
[0020] The N2 or inert gas is used to provide an inert environment. The inert gas is Ar, and may also be replaced by other inert gases such as He.
[0021] The enol ether is selected from one or more of allyl polyoxyethylene ether, vinyl ether, and polyethylene ether. By adjusting the type of enol ether, the dissolution and cleaning ability of the cleaning liquid on lipophilic impurities is changed, and corresponding cleaning liquids are prepared for ceramic plates with different degrees of contamination.
[0022] The initiator is selected from one or more of ammonium persulfate, azobisisobutyronitrile, and benzoyl peroxide, preferably azo and benzoyl peroxide organic initiators, which have the advantages of high initiation efficiency, uniform decomposition, few side reactions, few residues, and easy control of the relative molecular weight of the product.
[0023] The above-mentioned ceramic plate cleaning liquid is used to clean the ceramic plate, and the cleaning process includes the following steps:
[0024] Step S1, preparing a ceramic plate cleaning solution; in the cleaning solution, the mass fraction of the polymer of epoxy succinate and the blocked polyether is 5%-25%, the mass fraction of epoxy succinate is 0.01%-3%, the mass fraction of the polyacid is 0.01%-8%, the mass fraction of the olefin ether is 0.01%-5%, the mass fraction of the blocked polyether is 0.01%-8%, and the deionized water is 51%-94.96%.
[0025] Step S2, placing the contaminated ceramic plate in a cleaning solution and heating and soaking it, the soaking temperature is 35-50° C., and the soaking time is 60-90 minutes;
[0026] Step S3: After soaking, take out the ceramic plate, wash it with water and then blow it dry.
[0027] Existing ceramic cleaning methods such as grinding and polishing of ceramic plate cleaning liquids are difficult to achieve the purpose of thorough cleaning. The metal ion complexing agent and organic acid in the ceramic plate cleaning liquid in the prior art will inevitably etch the surface of the ceramic filter plate while removing the impurity particles on the ceramic plate, affecting the smoothness of the ceramic plate. Therefore, the present invention prepares a cleaning liquid containing epoxy succinate and a polymer of a blocked polyether. However, the simple epoxy succinate and blocked polyether polymers have weak acidity, insufficient water solubility, and insufficient solubility in oil-soluble stains, so the cleaning reaction speed of the ceramic plate is slow and the effect is poor. Therefore, the present invention adds epoxy succinate and polyacid to accelerate the reaction speed, thereby achieving safe and efficient removal of dirt on the ceramic plate contaminated by fluoride ions in the plasma chamber, and uses olefin ether to remove oil-soluble stains on the ceramic plate to restore the original color of the ceramic plate. The proportion of components in the cleaning solution is controlled to be 5%-25% by mass of the polymers of epoxysuccinate and end-capped polyether, 0.01%-3% by mass of epoxysuccinate, 0.01%-8% by mass of polyacid, 0.01%-5% by mass of olefin ether, 0.01%-8% by mass of end-capped polyether, and 51%-94.96% by mass of deionized water. If there is too much polymer, the viscosity of the cleaning solution will be too high. The cleaning liquid will have poor fluidity. Too little will lead to poor cleaning effect due to the small number of active functional groups. Too much epoxysuccinate will cause cations in the cleaning liquid to remain on the surface of the ceramic plate. Too little will cause phase separation in the cleaning liquid, affecting the cleaning speed. Too much polyacid will cause the cleaning liquid to be more acidic, causing the ceramic plate to be etched. Too little will lead to insufficient acidic functional groups in the cleaning liquid, poor cleaning effect and slow reaction speed. Too much olefin ether will reduce the water solubility of the cleaning liquid. Too little will lead to poor cleaning effect on the oily substances on the surface of the ceramic plate. Too much end-capped polyether will reduce the proportion of acidic functional groups in the cleaning liquid. Too little will lead to poor scale and corrosion inhibition effect.
[0028] The present invention carries out molecular structure design and function matching according to the cleaning requirements of ceramic plates. By adjusting the ratio of epoxy succinate and polymer of blocked polyether, epoxy succinate, polyacid, olefin ether and blocked polyether in the cleaning liquid, a large number of carboxyl groups in the polyether molecule and the polyacid molecular structure are used to dissolve fluorine impurities on the contaminated ceramic plate, and the cleaning liquid is used to clean the surface pollution of the ceramic plate by utilizing the good solubility of the cleaning liquid for water-soluble and oil-soluble impurities. The good solubility of the cleaning liquid for oil-soluble and water-soluble impurities and the good scale inhibition and corrosion inhibition characteristics of the polyether molecules are coordinated, and epoxy succinate and polyacid are added at the same time to accelerate the reaction speed and achieve good cleaning ability of the ceramic plate. Therefore, the cleaning liquid of the present invention has the advantages of good cleaning effect, small amount of use, easy wastewater treatment and little damage to the surface of the ceramic plate.
[0029] Some non-volatile fluorides, such as aluminum fluoride, will be deposited on the surface of the ceramic plate during the corrosion process. The surface component of the ceramic plate is aluminum oxide, which has aluminum hydroxyl groups. During the cleaning process, the cleaning liquid uses the dissolution properties of epoxysuccinate and end-capped polyether polymers on fluorine impurities in the ceramic plate contaminated by fluoride ions, converting the fluoride in the contaminated ceramic plate into soluble water-washable impurities, making it easier to remove the pollutants.
[0030] In addition, the polymers of epoxysuccinate and end-capped polyether of the present invention retain acidic groups such as carboxyl groups in the molecular structure to ensure the cleaning effect of the cleaning solution, and increase functional groups such as ester groups and ether groups. Compared with the prior art that uses metal ion complexing agents and organic acids to remove impurity particles on the ceramic plate, the surface of the ceramic filter plate is inevitably etched, affecting the smoothness of the ceramic plate. The components of the present invention avoid further etching of the ceramic plate by the acidity of the carboxyl group, thereby ensuring the smoothness of the ceramic plate.
[0031] All components of the cleaning solution of the present invention are environmentally friendly products, are easily degradable, are friendly to the human body and the environment, are simple to prepare, convenient to use and operate, and have stable effects. The cleaning solution is used for cleaning ceramic plates in a plasma chamber, has good cleaning effects, and causes little damage to the surface of the ceramic plates.
[0032] 3. Beneficial effects
[0033] Compared with the prior art, the present invention has the following beneficial effects:
[0034] (1) The present invention improves acidity and water solubility by adding epoxysuccinate and polyacid, accelerates the reaction speed, and achieves safe and efficient removal of dirt from ceramic plates contaminated by fluoride ions in a plasma chamber, and uses olefin ether to remove oil-soluble stains from ceramic plates, thereby restoring the original color of the ceramic plates;
[0035] (2) The cleaning liquid of the present invention is designed with molecular structure and functions matched according to the cleaning requirements of ceramic plates. By adjusting the ratio of epoxy succinate and polymer of blocked polyether, epoxy succinate, polyacid, olefin ether and blocked polyether in the cleaning liquid, a large number of carboxyl groups in the polyether molecule and the polyacid molecular structure are used to dissolve fluorine impurities on the contaminated ceramic plate, and the cleaning liquid is used to clean the surface pollution of the ceramic plate by using its good solubility for water-soluble and oil-soluble impurities. The good solubility of the cleaning liquid for oil-soluble and water-soluble impurities and the good scale inhibition and corrosion inhibition characteristics of the polyether molecule show good ceramic plate cleaning ability.
[0036] (3) The ceramic plate cleaning liquid of the present invention has good water solubility. The large amount of carboxyl groups in the components have good solubility for fluorine impurities in the ceramic plate contaminated by fluorine ions. The good hydrogen bonding and ion exchange properties of the epoxy succinate and the blocked polyether polymer to fluorine are utilized to convert the fluoride in the contaminated ceramic plate into soluble water-washable impurities, thereby facilitating the removal of the pollutants.
[0037] (4) The polymer molecular structure of the present invention relies on the combined action of chelation solubilization and lattice distortion, and the carboxyl group chelates the scale-forming cations (such as Ca 2+ ,Mg 2+ etc.), thereby preventing it from interacting with scaling anions (such as CO3 2- , SO4 2- The polyether structure in the molecular chain segment prevents the growth of crystal nuclei and inhibits scaling; it has a certain adsorption effect on the insoluble oxides in the wastewater of ceramic plate cleaning, avoids the accumulation of oxides, and enhances the cleaning effect of ceramic plates;
[0038] (5) The cleaning liquid components of the ceramic plate of the present invention contain a large number of ether bonds and carboxyl groups. The lone pairs of electrons in a large number of oxygen atoms will form covalent bonds with the surface of the ceramic plate, forming chemical adsorption or coordination adsorption; at the same time, the groups composed of C and H elements are hydrophobic, forming a hydrophobic protective film. A large number of carboxylic acid groups in the molecular structure of the cleaning liquid will chelate with the surface of the ceramic plate to form an organic complex protective film, thereby avoiding the etching of the ceramic surface by excessive acid sites in the cleaning agent, and having a good corrosion inhibition effect, which can not only slow down the corrosion of the ceramic plate substrate, but also reduce the consumption of the cleaning liquid;
[0039] (6) The polymer molecular structure of the present invention has both hydrophilic and lipophilic properties and is a good surfactant. The surfactant properties greatly enhance the washing effect of the ceramic plate cleaning solution;
[0040] (7) The polymer of the present invention inserts oxygen atoms into the structure through molecular design, which not only increases the biodegradability of the main chain, but also realizes the multifunctionality of the ceramic plate cleaning liquid; the preparation process of the ceramic plate cleaning liquid uses easily biodegradable raw materials, discards toxic and harmful reagents, does not produce toxic and harmful by-products, and is environmentally friendly; adopts a "one-pot" reaction method, and the products after the reaction do not need to be separated, which reduces the post-processing cost, is simple to prepare, easy to use and easy to operate, and has a stable effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] The technical solution of the present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments, but it should be understood that these drawings are designed only for explanation purposes and are not intended to limit the scope of the present invention. In addition, unless otherwise specified, these drawings are intended only to conceptually illustrate the structural configurations described herein and are not necessarily drawn to scale.
[0042] Figure 1 is the structural formula of a ceramic plate cleaning liquid of the present invention;
[0043] Figure 2 is the reaction formula for preparing the polymer of epoxy succinate and end-capped polyether of the present invention;
[0044] Figure 3 is the structural formula of the polymer of epoxy succinate and end-capped polyether of Example 1 of the present invention;
[0045] Figure 4 is the structural formula of the polymer of epoxy succinate and end-capped polyether of Example 2 of the present invention;
[0046] Figure 5 is the structural formula of the polymer of epoxysuccinate and end-capped polyether of Example 3 of the present invention;
[0047] Figure 6 This is a diagram showing the cleaning effect of the ceramic plate according to Example 1 of the present invention;
[0048] Figure 7 This is a diagram showing the cleaning effect of the ceramic plate of Comparative Example 1 of the present invention. DETAILED DESCRIPTION
[0049] The following detailed description of exemplary embodiments of the present invention refers to the accompanying drawings, which form a part of the description, and in which exemplary embodiments of the present invention that can be implemented are shown as examples. Although these exemplary embodiments are described in sufficient detail to enable those skilled in the art to implement the present invention, it should be understood that other embodiments can be implemented and various changes can be made to the present invention without departing from the spirit and scope of the present invention. The following more detailed description of the embodiments of the present invention is not intended to limit the scope of the claimed invention, but is only for the purpose of illustrating and not limiting the description of the characteristics and features of the present invention, so as to propose the best mode for performing the present invention and to enable those skilled in the art to implement the present invention. Therefore, the scope of the present invention is limited only by the appended claims.
[0050] Table 1 Mass fraction (wt%) of the ceramic plate cleaning solution of each embodiment of the present invention
[0051]
[0052]
[0053] Table 2 Experimental parameters of various embodiments of the present invention
[0054]
[0055] Table 3 Application process parameters of various embodiments of the present invention
[0056]
[0057]
[0058] Table 4 Performance parameters of the ceramic plates after cleaning in various embodiments of the present invention
[0059] Example 1 Example 2 Example 3 Comparative Example 1 Cleanliness Clean Clean Clean A bit dirty Determination 99% 99% 99% 85%
[0060] The structural formula of the polymer of epoxy succinate and end-capped polyether prepared in Examples 1-3 of the present invention is as follows: Figure 3-5 shown.
[0061] The ceramic plate cleaning solution of Comparative Example 1 of the present invention was applied to the cleaning of ceramic plates. The results showed that the ceramic plate cleaning solution containing epoxy succinate and the polymer with end-capped polyether exhibited a stronger cleaning effect. Figure 6-7 As shown, under the same preparation conditions, compared with the ceramic plate cleaning liquid of Comparative Example 1 in which no epoxysuccinate and blocked polyether polymer are added, Example 1 shows a higher degree of cleanliness and a faster decontamination speed after being immersed in the cleaning liquid at 60°C for 90 minutes, and the oil removal rate reaches 99%, while that of Comparative Example 1 is only 85%, and there are dirty spots on the ceramic plate.
Claims
1. An application of a ceramic plate cleaning liquid in cleaning a ceramic plate, characterized in that: The cleaning process includes the following steps: Step S1, preparing a ceramic plate cleaning solution; Step S2, placing the contaminated ceramic plate in a ceramic plate cleaning solution for heating and soaking; Step S3, after soaking, take out the ceramic plate, wash it with water and blow it dry; The ceramic plate cleaning solution comprises components and mass fractions thereof: 5%-25% of epoxy succinate and polymer of end-capped polyether, 0.01%-3% of epoxy succinate, 0.01%-8% of polyacid, 0.01%-5% of olefin ether, 0.01%-8% of end-capped polyether, and 51%-94.96% of deionized water. The structural formula of the polymer of epoxy succinate and end-capped polyether is: , where x=1-5, y=1-3, , where n=1-5, or or , the polyacid is selected from one or more of oxalic acid, adipic acid, and trisaccharic acid, the olefin ether is allyl polyoxyethylene ether, and the ceramic plate contains fluorine impurities, The preparation method of the ceramic plate cleaning liquid specifically comprises the following steps: Step a, preparing epoxy succinate: at room temperature, slowly drop maleic anhydride into a sodium alcohol solution, add a solid acid catalyst and an oxidant in sequence, heat to react for a period of time, cool to room temperature after the reaction is completed, filter, wash and dry to obtain epoxy succinate; Step b, preparing the blocked polyether: adding the olefin ether and the polyacid into a reaction kettle at room temperature in a N2 or inert gas atmosphere, heating and reacting for a period of time, and cooling to room temperature after the reaction to obtain the blocked polyether; Step c, preparing a ceramic plate cleaning solution: at room temperature, adding epoxy succinate and blocked polyether into a reactor, dropping an initiator into the reactor, heating and reacting for a period of time, cooling to room temperature after the reaction is completed, and obtaining a ceramic plate cleaning solution containing epoxy succinate and blocked polyether polymers.
2. The use according to claim 1, characterized in that: In step a, the molar ratio of sodium alcohol to maleic anhydride is (5-10):1; the molar ratio of solid acid catalyst to maleic anhydride is (0.1-0.3):1; the molar ratio of oxidant to maleic anhydride is (0.5-2):1, the reaction temperature is 60-120°C, and the reaction time is 6-24 h.
3. The use according to claim 2, characterized in that: In step b, the molar ratio of the polyacid to the olefin ether is (5-8):1, the reaction temperature is 50-90°C, and the reaction time is 0.5-6 h.
4. The use according to claim 3, characterized in that In step c, the molar ratio of the end-capped polyether to the epoxy succinate is (0.2-5):1, the molar ratio of the initiator to the epoxy succinate is (0.01-0.05):1, the reaction temperature is 60-150°C, and the reaction time is 2-8 h.
5. The use according to claim 4, characterized in that: In step S2, the soaking temperature is 35-50°C, and the soaking time is 60-90 minutes.
Citation Information
Patent Citations
Cleaning agent and application thereof to cleaning of ceramic filter plates
CN108410590A
Ceramic plate cleaning liquid medicine for plasma chamber and application thereof
CN112358920A
Process for the preparation of oxodisuccinates useful as detergent builders