A method and device for testing the sharpness of an antique sword

By cutting the fixed material at a constant speed and recording the cutting process, the depth and work of the antique sword's cutting and breaking are calculated, which solves the accuracy and damage problems of the antique sword sharpness test in the existing technology, and realizes the precision of the antique sword's sharpness. Monitor and accurately analyze.

CN114965136BActive Publication Date: 2024-10-22TSINGHUA SHENZHEN INTERNATIONAL GRADUATE SCHOOL +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210464125.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-29
Publication Date
2024-10-22
Estimated Expiration
2042-04-29

AI Technical Summary

Technical Problem

The existing technology cannot accurately evaluate the sharpness of antique swords, and the cutting test method causes impact stress and damage to the sword's edge, making it impossible to achieve precise monitoring and accurate analysis.

Method used

The method of cutting fixed materials at a constant speed is used, the cutting process is recorded through a high-speed camera, the force is recorded by a force measuring instrument, the cutting depth and work when cutting in and breaking are calculated, the sharpness of the antique sword is calculated, and the feeding mechanism and materials controlled by a stepper motor are used Height adjustment device ensures cutting stability and precision.

Benefits of technology

It achieves accurate analysis of the sharpness of antique swords, reduces damage to the sword during testing, ensures stability and fine monitoring of the cutting process, obtains multiple evaluation parameters, and improves the accuracy and efficiency of the test.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114965136B_ABST
    Figure CN114965136B_ABST
Patent Text Reader

Abstract

The invention provides a method for testing the sharpness of an antique sword, comprising: driving the antique sword to cut a material at a uniform speed, wherein the speed range is 2-10 mm / min, the height of the cut material is the same as the cutting height of the antique sword, and the Shore hardness of the material is 40-70A; recording images of the process of the antique sword cutting the material changing with time by a high-speed camera; recording the force of the process of the antique sword cutting the material changing with time by a dynamometer; obtaining the cutting depth at the time of cutting in and at the time of breaking based on the images of the process of the antique sword cutting the material changing with time, calculating the cutting work and the breaking work; and finally calculating the sharpness of the antique sword; the method of the invention can ensure that the cutting angle between the cut material and the designated position of the sword is stable, realize quasi-static cutting, eliminate the damage that the impact stress may cause to the cutting edge of the antique sword, reduce the damage to the antique sword during the testing process, and carry out fine monitoring during the material cutting process, obtain various physical quantities during the cutting process, and analyze the sharpness more accurately.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of sword craft testing, in particular to a method and device for testing the sharpness of an antique sword. Background Art

[0002] Antique swords are collectible handicrafts that imitate the forms of ancient Chinese and foreign weapons. Sharpened antique swords are sharper than unsharpened ones. my country regulates sharpened swords and daggers, mainly stipulating the overall length of the swords and the angle of the tip. Due to the different shapes of ancient cold weapons, the blades of antique swords have various shapes, and the sharpness of different positions of the same sword is also different. The geometric standard alone is not enough to fully evaluate the sharpness and danger of antique swords. It is necessary to propose a standardized sharpness measurement method and equipment to achieve a quantitative evaluation of the sharpness of specific positions of antique swords.

[0003] At present, the method of evaluating the sharpness of the blade edge is mainly based on the cutting depth: the cutting depth method refers to using a certain pressure to press the cutting medium (usually paper or metal foil) to make the medium contact with the antique sword, and characterize the sharpness by recording the fracture depth of the medium (or the number of layers of multi-layer media). The above cutting depth test applies impact stress to the antique sword, causing damage to the surface of the antique sword.

[0004] Currently, the main method for testing edge sharpness is to use a wider medium to press down and make a macroscopic evaluation of the entire edge of the antique sword. It is impossible to finely monitor the material cutting process, and thus it is impossible to achieve accurate sword sharpness analysis. Summary of the invention

[0005] The main purpose of the present invention is to overcome the above-mentioned defects in the prior art and to propose a method and device for testing the sharpness of an antique sword. The present invention can ensure the stability of the cutting angle between the cut material and the specified position of the sword, realize quasi-static cutting, eliminate the damage that the impact stress may cause to the edge of the antique sword, reduce the damage to the antique sword during the testing process, and perform fine monitoring during the material cutting process, obtain various physical quantities during the cutting process, and perform a more accurate analysis of its sharpness.

[0006] A method for testing the sharpness of an antique sword, comprising:

[0007] The antique sword is driven to cut the fixed material at a uniform speed, wherein the speed range is 2-10 mm / min, the height of the cut material is the same as the cutting height of the antique sword, and the Shore hardness of the fixed material is 40-70A;

[0008] The images of the material cutting process of the antique sword changing over time were recorded by a high-speed camera;

[0009] The force applied by the antique sword during the material cutting process is recorded with a dynamometer over time;

[0010] Based on the image of the material cutting process of the antique sword changing with time, the cutting time point and the breaking time point are obtained, and the cutting depth at the time of cutting in and breaking is calculated according to the cutting time point and the breaking time point and the speed of the antique sword;

[0011] Based on the time-varying force of the antique sword in the process of cutting materials and the cutting depth at the time of cutting and breaking, the cutting work and breaking work are calculated;

[0012] The sharpness of antique swords is calculated based on the cutting depth at the time of penetration and fracture, as well as the cutting work and fracture work.

[0013] Specifically, based on the force that changes over time during the cutting process of the antique sword and the cutting depth at the time of cutting in and breaking, the cutting work and breaking work are calculated, specifically:

[0014]

[0015]

[0016] Among them, d1 is the cutting depth during cutting, d2 is the cutting depth during forging, F is the force that changes with time during the process of cutting materials by the antique sword, W1 is the cutting work, and W2 is the breaking work.

[0017] Specifically, the sharpness of the antique sword is calculated based on the cutting depth at the time of cutting and breaking, as well as the cutting work and breaking work, which is:

[0018]

[0019]

[0020] S = Index1*Index2

[0021] Among them, Index1 represents the dimensionless parameter characterizing the sharpness based on cutting, Index2 represents the dimensionless parameter characterizing the sharpness based on fracture, t is the thickness of the workpiece being cut, K is the fracture toughness of the material being cut, and S is the sharpness of the antique sword.

[0022] Another embodiment of the present invention provides an antique sword sharpness testing device, comprising: an antique sword feeding mechanism, an antique sword clamping device, a material height adjustment device, a material fixing device, a laser tool setting device, a dynamometer and a high-speed camera;

[0023] The antique sword clamping device is arranged on the antique sword feeding mechanism, and the antique sword feeding mechanism drives the antique sword to move at a low speed. The antique sword clamping device is on the slider of the antique sword feeding mechanism. The material fixing device is arranged on the moving block of the material height adjustment device, and the material height adjustment device drives and adjusts the relative height between the antique sword and the cutting material. The laser tool setting device is fixed above the center line of the antique sword feeding mechanism. The dynamometer is installed between the slider of the antique sword feeding mechanism and the antique sword clamping device. The high-speed camera is installed at the end of the material height adjustment device and is perpendicular to the cutting surface. The dynamometer and the high-speed camera signals are connected to a computer. The feeding mechanism, the laser tool setting device, the dynamometer and the high-speed camera are independently powered.

[0024] Specifically, the antique sword feeding mechanism is realized by controlling the screw transmission through a stepping motor, the dynamometer mounting seat is fixed to the slider of the screw, the antique sword clamping device is connected to the dynamometer mounting seat through a guide column, and the antique sword is manually adjusted and connected to the antique sword clamping device.

[0025] Specifically, the material height adjustment device is realized by a stepper motor control rod transmission, the moving blocks of the material fixing device on both sides are fixed to the control rod by bolts, the cut material is placed on the material fixing device symmetrically along the center line of the material height adjustment device, the material pressing sheet is placed on the cut material and fixedly connected to the material fixing device by bolts.

[0026] Specifically, the slider and the clamping device of the antique sword feeding mechanism make linear motion together, the slider movement range is 100-300 mm, the movement accuracy is not more than 0.02 mm, and the movement speed is not more than 10 mm per minute.

[0027] Specifically, the moving block of the material height adjustment device and the material fixing device move linearly together, and the movement accuracy of the moving block is no more than 0.05 mm.

[0028] Specifically, the thickness of the cut material is between 2 mm and 10 mm, the length is between 50 mm and 100 mm, and the width is between 25 mm and 40 mm.

[0029] It can be seen from the above description of the present invention that, compared with the prior art, the present invention has the following beneficial effects:

[0030] (1) The present invention provides a method for testing the sharpness of an antique sword, comprising: driving the antique sword to cut a fixed material at a uniform speed, wherein the speed range is 2-10 mm / min, the height of the cut material is the same as the cutting height of the antique sword, and the Shore hardness of the fixed material is 40-70A; recording the image of the antique sword cutting the material over time by a high-speed camera; recording the force of the antique sword cutting the material over time by a dynamometer; obtaining the cutting-in time point and the breaking time point based on the image of the antique sword cutting the material over time, and calculating the cutting speed according to the cutting-in time point, the breaking time point and the speed of the antique sword. The cutting depth at the time of cutting and breaking; based on the force changing with time in the process of cutting materials by the antique sword and the cutting depth at the time of cutting and breaking, the cutting work and the breaking work are calculated; the sharpness of the antique sword is calculated according to the cutting depth at the time of cutting and breaking and the cutting work and the breaking work; the method provided by the present invention can ensure the stability of the cutting angle between the cut material and the specified position of the sword, realize quasi-static cutting, eliminate the damage that the impact stress may cause to the cutting edge of the antique sword, reduce the damage to the antique sword during the testing process, and carry out fine monitoring during the material cutting process, obtain various physical quantities in the cutting process, and conduct a more accurate analysis of its sharpness.

[0031] (2) The present invention provides a device for testing the sharpness of an antique sword. The feeding mechanism of the antique sword is realized by controlling the screw drive through a stepping motor. The dynamometer mounting seat is fixed to the slider of the screw. The antique sword clamping device is connected to the dynamometer mounting seat through a guide column. The antique sword and the antique sword clamping device are manually adjusted and connected. This can ensure that the blade of the tested part of the antique sword is perpendicular to the plane of the test table and cuts orthogonally to the cut material, thereby eliminating the damage that the impact stress may cause to the cutting edge of the antique sword.

[0032] (3) The present invention provides a device for testing the sharpness of an antique sword. The material height adjustment device is realized by a stepper motor control rod transmission. The moving blocks of the material fixing device and the control rod are fixed by bolts on both sides. The cut material is symmetrically placed on the material fixing device along the center line of the material height adjustment device. The material pressing sheet is placed on the cut material and fixedly connected to the material fixing device by bolts. This ensures that the cut material is perpendicular to the blade at a fixed position of the antique sword. During the cutting process, the material pressing sheet and the cut material other than the pressing sheet are completely fixed. Only the material in the middle position is deformed due to the influence of the cutting force, thereby providing a basis for accurate sharpness analysis.

[0033] (4)) The method provided by the present invention is simple and convenient. A single operation only requires clamping the workpiece and the antique sword, and the blade test position is precisely controlled by a screw rod. The data is acquired accurately, and the zero point alignment is acquired by comparing a high-speed camera with a dynamometer. The parameters acquired are diverse, and multiple evaluation parameters can be acquired in one cutting, thereby reducing the randomness that may occur in the judgment of a single parameter. The response speed is fast, and only the key frames of the camera's entry point and break point need to be manually judged, and the calculation is completed with the assistance of a computer. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 A flow chart of a method for testing the sharpness of an antique sword provided by an embodiment of the present invention;

[0035] Figure 2 A schematic diagram of the structure of an antique sword sharpness testing device provided by an embodiment of the present invention;

[0036] Figure 3 A schematic diagram of the structure of the antique sword clamping and the dynamometer position provided by an embodiment of the present invention;

[0037] Figure 4 A schematic diagram of the structure of a workpiece clamping device provided by an embodiment of the present invention;

[0038] Figure 5 A schematic diagram of a pressure-displacement curve provided in an embodiment of the present invention;

[0039] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. DETAILED DESCRIPTION

[0040] In the claims, description and the above-mentioned drawings of this specification, unless otherwise explicitly defined, the use of terms such as "first", "second" or "third" etc. are intended to distinguish different objects rather than to describe a specific order.

[0041] In the claims, specification and the above-mentioned drawings of this specification, unless otherwise expressly defined, directional words, such as the terms "center", "lateral", "longitudinal", "horizontal", "vertical", "top", "bottom", "inside", "outside", "up", "down", "front", "back", "left", "right", "clockwise", "counterclockwise", etc., indicating directions or positional relationships are based on the directions and positional relationships shown in the drawings, and are only for the convenience of narrating this specification and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation or be constructed and operated in a specific orientation, so they cannot be understood as limiting the specific protection scope of this specification.

[0042] In the claims, description and the above drawings of this specification, unless otherwise clearly defined, the terms "fixed connection" and "fixed connection" should be understood in a broad sense, that is, any connection method without any displacement relationship and relative rotation relationship between the two parties, that is to say, including non-detachable fixed connection, detachable fixed connection, integral connection and fixed connection through other devices or elements.

[0043] In the claims, description and drawings of this specification, if the terms "include", "have" and their variations are used, they are intended to mean "including but not limited to".

[0044] like Figure 1 , is an operation flow chart of an antique sword sharpness testing method provided by an embodiment of the present invention, specifically comprising:

[0045] A method for testing the sharpness of an antique sword, comprising:

[0046] S101: driving the antique sword to cut the fixed material at a uniform speed, wherein the speed range is 2-10 mm / min, the height of the cut material is the same as the cutting height of the antique sword, and the Shore hardness of the fixed material is 40-70A;

[0047] The method provided by the present invention can ensure the stability of the cutting angle between the material being cut and the designated position of the sword, realize quasi-static cutting, eliminate the damage that the impact stress may cause to the edge of the antique sword, and reduce the damage to the antique sword during the testing process.

[0048] S102: Recording images of the process of cutting materials with the antique sword over time by a high-speed camera;

[0049] S103: recording the force applied to the antique sword during the material cutting process over time by using a dynamometer;

[0050] S104: obtaining a cutting-in time point and a breaking time point based on an image of the material cutting process of the antique sword changing with time, and calculating a cutting depth at the time of cutting-in and at the time of breaking according to the cutting-in time point and the breaking time point and the speed of the antique sword;

[0051] The material is carefully monitored during the cutting process, and various physical quantities in the cutting process are obtained, so as to make a more accurate analysis of its sharpness. The method is simple, the data is obtained accurately, and the zero point alignment is obtained by comparing the high-speed camera with the dynamometer. The parameters are obtained in a variety of ways, and multiple evaluation parameters can be obtained in one cutting, reducing the randomness that may occur in the judgment of a single parameter.

[0052] S105: calculating the cutting work and the breaking work based on the force changing with time during the cutting process of the antique sword and the cutting depth at the time of cutting and breaking;

[0053] Based on the time-varying force of the antique sword in the process of cutting materials and the cutting depth at the time of cutting in and breaking, the cutting work and breaking work are calculated, specifically:

[0054]

[0055]

[0056] Among them, d1 is the cutting depth during cutting, d2 is the cutting depth during forging, F is the force that changes with time during the process of cutting materials by the antique sword, W1 is the cutting work, and W2 is the breaking work.

[0057] S106: Calculate the sharpness of the antique sword according to the cutting depth at the time of cutting in and the time of breaking as well as the cutting work and the breaking work.

[0058] According to the cutting depth at the time of cutting and breaking, as well as the cutting work and breaking work, the sharpness of the antique sword is calculated as follows:

[0059]

[0060]

[0061] S = Index1*Index2

[0062] Among them, Index1 represents the dimensionless parameter characterizing the sharpness based on cutting, Index2 represents the dimensionless parameter characterizing the sharpness based on fracture, t is the thickness of the workpiece being cut, K is the fracture toughness of the material being cut, and S is the sharpness of the antique sword.

[0063] like Figure 2 The embodiment of the present invention provides an antique sword sharpness testing device, including an antique sword feeding mechanism 1, an antique sword clamping device 14, a material height adjustment device 2, a material fixing device 23, a laser tool setting device 4, a dynamometer 5 and a high-speed camera 3;

[0064] The antique sword clamping device 14 is arranged on the antique sword feeding mechanism 1, and the antique sword feeding mechanism 1 drives the antique sword to move at a low speed. The antique sword clamping device 14 is on the slider of the antique sword feeding mechanism 1. The material fixing device 23 is arranged on the moving block of the material height adjustment device 2, and the material height adjustment device 2 drives to adjust the relative height between the antique sword and the cutting material. The laser tool setting device 4 is fixed above the center line of the antique sword feeding mechanism 1, and the dynamometer 5 is installed between the slider of the antique sword feeding mechanism 1 and the antique sword clamping device 14. The high-speed camera 3 is installed at the end of the material height adjustment device 2 and is perpendicular to the cutting surface. The dynamometer 5 and the high-speed camera 3 signals are connected to the computer, and the antique sword feeding mechanism 1, the laser tool setting device 4, the dynamometer 5 and the high-speed camera 3 are independently powered.

[0065] like Figure 3 The feeding mechanism 1 of the antique sword is realized by controlling the screw rod 12 through a stepping motor, the mounting seat 13 of the dynamometer 1 is fixed to the slider of the screw rod 12, the clamping device 14 of the antique sword is connected to the mounting seat 13 of the dynamometer 5 through a guide column, and the antique sword 11 is manually adjusted to be connected to the clamping device 14. With this structure, it can be ensured that the blade of the tested part of the antique sword 11 is perpendicular to the plane of the test table and cuts orthogonally to the material 21 to be cut.

[0066] like Figure 4 The material height adjustment device 2 is realized by the stepping motor control rod 22, the material fixing device 23 (both sides) is fixed to the moving block of the control rod 22 by bolts, the length direction of the cut material 21 is symmetrically placed on the material fixing device 23 along the center line of the mechanism 2, and the material pressing sheet 24 is placed on the cut material 21 and fixedly connected to the material fixing device 23 by bolts. With this structure, it can be ensured that the cut material 21 is perpendicular to the blade at the fixed position of the antique sword 11, and the material pressing sheet 24 and the cut material 21 outside the pressing sheet 24 are completely fixed during the cutting process, and only the material in the middle position is affected by the cutting force and deformed.

[0067] The stepper motors of the control screw rod 12 and the control rod 22 are powered by an external power supply, and the movement of the stepper motors is controlled by a computer.

[0068] The high-speed camera 3 is fixed on the top of the structure, located just above the contact position between the antique sword 11 and the cutting material 21, and the shooting direction is vertical to the cutting material 21 and downward. The high-speed camera 3 is powered by a battery, and the captured images and videos are transmitted to the computer via a data cable.

[0069] The laser tool setting device 4 is fixed on the top of the structure, located on the center line of the antique sword movement mechanism 1, about 50 mm away from the high-speed camera 3, and the laser direction is vertical to the cut material 21 downward. The laser tool setting device 4 is powered by a battery.

[0070] The dynamometer 5 is fixed to the dynamometer 5 mounting base 13, and the probe is in contact with the antique sword clamping device 14. The dynamometer 5 is powered by an external power supply, and the mechanical signal is transmitted to the computer through the transmitter and the data line.

[0071] The structure of the embodiment of the present invention has the following advantages: accurate movement, which is completed by controlling the screw rod with a stepping motor, and the feeding speed and edge test height of the antique sword can be accurately controlled; reliable clamping can ensure that the angular position relationship between the antique sword and the cut material is correct.

[0072] In this preferred embodiment, the hardness of the cut material 21 is between 40A and 70A in Shore A hardness, the thickness is between 2 mm and 10 mm, the length is between 50 mm and 100 mm, and the width is between 25 mm and 40 mm. Preferably, the feed speed of the antique sword 11 during the cutting process is between 2 mm per minute and 10 mm per minute.

[0073] like Figures 1 to 4 , the specific operation flow of the structure of the embodiment is as follows:

[0074] Step 1, workpiece clamping. Control the stepper motor of the material height adjustment device 2 so that the placement plane of the material fixing device 23 to be cut is the same as the cutting height of the tip of the antique sword 11, so that the length direction of the material 21 to be cut is symmetrically placed on the material fixing device 23 along the center line of the material height adjustment device 2, and the material pressing sheet 24 is placed on the material 21 to be cut and fixedly connected to the material fixing device 23 to be cut by bolts, indicating that the material is tightened, and re-control the stepper motor of the material moving mechanism 2 to adjust the height of the material 21 to be cut so that it can be cut orthogonally to the designated position of the cutting edge of the antique sword 11.

[0075] Step 2, antique sword alignment. Control the stepper motor of the antique sword feeding mechanism 1 to make the antique sword 11 located at the predetermined position directly below the laser blade alignment device 4. The antique sword 11 is fixed to the antique sword clamping device 14 by means of double-sided round head screws. When the laser can cover both sides of the edge of the straight-bladed antique sword 11 where the measurement is required, tighten the round head set screws to fix the sword 11 in the antique sword clamping device 14, indicating that the blade alignment is completed. Re-control the stepper motor of the antique sword feeding mechanism 1 to make the blade close to the material position, generally set to about 1 mm.

[0076] Step 3, antique sword cutting and data recording. Open the data acquisition channels of the high-speed camera 3 and the dynamometer 5, control the stepper motor of the antique sword feeding mechanism 1, feed the cutting material 21 at a low speed until the material 21 is completely broken, and after the antique sword feeding mechanism 1 stops, remove the cutting material 21 and control the antique sword feeding mechanism 1 to move in the reverse direction back to the original position, and close the data acquisition channels of the high-speed camera 3 and the dynamometer 5.

[0077] Step 4, data fusion processing. Observe the high-speed camera 3 frame by frame and record the moment when the edge of the antique sword 11 contacts the cut material 21 as the camera zero point, the moment when the blade produces a destructive crack on the surface as the camera entry point, and the moment when the blade completely penetrates the cut material 21 as the camera break point. Take the previous data point when the dynamometer 5 displays a non-zero indication for the first time and record it as the dynamometer zero point. Correspondingly, the entry point and break point of the dynamometer curve are obtained according to the camera entry point and break point.

[0078] Step 5: Parameter calculation. Figure 5 , according to the time between the cutting point and the breaking point and the screw feed speed, the cutting depth when the surface cracks and breaks is calculated as parameters d1 and d2; according to the maximum value of the dynamometer 5 reading before the cutting point and the breaking point, the parameter F max1 、F max2 ; According to the force measurement curves from zero point to the cutting point and from zero point to the breaking point, the work done by the antique sword 11 from cutting to cutting and complete breaking is calculated as parameters W1 and W2. Generally, the test standard believes that the smaller the above parameters and the Index1 and Index2 parameters calculated by the above parameters and the formula listed in the claims are, the sharper the antique sword is.

[0079] The present invention provides a method for testing the sharpness of an antique sword, comprising: driving the antique sword to uniformly cut a fixed material, wherein the speed range is 2-10 mm / min, the height of the cut material is the same as the cutting height of the antique sword, and the Shore hardness of the fixed material is 40-70A; recording the image of the process of the antique sword cutting the material changing with time by a high-speed camera; recording the force of the process of the antique sword cutting the material changing with time by a dynamometer; obtaining the cutting-in time point and the breaking time point based on the image of the process of the antique sword cutting the material changing with time, and calculating the cutting-in time point according to the cutting-in time point, the breaking time point and the speed of the antique sword. and the cutting depth when it breaks; based on the force that changes with time during the process of cutting materials by the antique sword and the cutting depth when cutting in and when breaking, the cutting work and the breaking work are calculated; according to the cutting depth when cutting in and when breaking, the cutting work and the breaking work are calculated, the sharpness of the antique sword is calculated; the method provided by the present invention can ensure the stability of the cutting angle between the cut material and the specified position of the sword, realize quasi-static cutting, eliminate the damage that the impact stress may cause to the cutting edge of the antique sword, reduce the damage to the antique sword during the testing process, and carry out fine monitoring during the material cutting process, obtain various physical quantities in the cutting process, and conduct a more accurate analysis of its sharpness.

[0080] The present invention provides a device for testing the sharpness of an antique sword. The feeding mechanism of the antique sword is realized by controlling the screw drive through a stepping motor. The dynamometer mounting seat is fixed to the slider of the screw. The antique sword clamping device is connected to the dynamometer mounting seat through a guide column. The antique sword and the antique sword clamping device are manually adjusted and connected. It can ensure that the blade of the tested part of the antique sword is perpendicular to the plane of the test table and cuts orthogonally to the cut material, thereby eliminating the damage that the impact stress may cause to the cutting edge of the antique sword.

[0081] The present invention provides a device for testing the sharpness of an antique sword. A material height adjustment device is realized by driving a stepping motor control rod. Moving blocks of the material fixing device and the control rod are fixed by bolts on both sides. The cut material is symmetrically placed on the material fixing device along the center line of the material height adjustment device. A material pressing sheet is placed on the cut material and fixedly connected to the material fixing device by bolts. This ensures that the cut material is perpendicular to the blade at a fixed position of the antique sword. During the cutting process, the material pressing sheet and the cut material other than the pressing sheet are completely fixed, and only the material in the middle position is deformed due to the influence of the cutting force, thereby providing a basis for accurate analysis of the sharpness.

[0082] The method provided by the present invention is simple and convenient, and a single operation only requires clamping the workpiece and the antique sword, and the blade test position is accurately controlled by a screw rod; the data is accurately acquired, and the zero point alignment is acquired by comparing a high-speed camera with a dynamometer; the parameter acquisition is diverse, and a plurality of evaluation parameters can be acquired in one cutting, thereby reducing the contingency that may occur in the judgment of a single parameter; the response speed is fast, and only the key frames of the camera cut-in point and the break point need to be manually judged, and the calculation is completed with the assistance of a computer.

[0083] The above is only a specific implementation of the present invention, but the design concept of the present invention is not limited thereto. Any non-substantial changes to the present invention using this concept shall be deemed as an infringement of the protection scope of the present invention.

Claims

1. A method for testing the sharpness of an antique sword, characterized in that: include: The antique sword is driven to cut the material at a uniform speed, wherein the speed range is 2-10 mm / min, the height of the cut material is the same as the cutting height of the antique sword, and the Shore hardness of the material is 40-70A; The images of the material cutting process of the antique sword changing over time were recorded by a high-speed camera; The force applied by the antique sword during the material cutting process is recorded with a dynamometer over time; Based on the image of the material cutting process of the antique sword changing with time, the cutting time point and the breaking time point are obtained, and the cutting depth at the time of cutting in and breaking is calculated according to the cutting time point and the breaking time point and the speed of the antique sword; Based on the time-varying force of the antique sword in the process of cutting materials and the cutting depth at the time of cutting and breaking, the cutting work and breaking work are calculated; The sharpness of antique swords is calculated based on the cutting depth at the time of penetration and fracture, as well as the cutting work and fracture work.

2. The method for testing the sharpness of an antique sword according to claim 1, characterized in that: Based on the time-varying force of the antique sword in the process of cutting materials and the cutting depth at the time of cutting in and breaking, the cutting work and breaking work are calculated, specifically: Among them, d1 is the cutting depth during cutting, d2 is the cutting depth during forging, F is the force that changes with time during the process of cutting materials by the antique sword, W1 is the cutting work, and W2 is the breaking work.

3. The method for testing the sharpness of an antique sword according to claim 2, characterized in that: According to the cutting depth at the time of cutting and breaking, as well as the cutting work and breaking work, the sharpness of the antique sword is calculated as follows: S = Index1 * Index2 Among them, Index1 represents the dimensionless parameter characterizing the sharpness based on cutting, Index2 represents the dimensionless parameter characterizing the sharpness based on fracture, t is the thickness of the workpiece being cut, K is the fracture toughness of the material being cut, and S is the sharpness of the antique sword.

4. An antique sword sharpness testing device using the method described in any one of claims 1 to 3, characterized in that: include: It includes an antique sword feeding mechanism, an antique sword clamping device, a material height adjustment device, a material fixing device, a laser tool setting device, a dynamometer and a high-speed camera; The antique sword clamping device is arranged on the antique sword feeding mechanism, and the antique sword feeding mechanism drives the antique sword to move at a low speed. The antique sword clamping device is on the slider of the antique sword feeding mechanism. The material fixing device is arranged on the moving block of the material height adjustment device, and the material height adjustment device drives and adjusts the relative height between the antique sword and the cutting material. The laser tool setting device is fixed above the center line of the antique sword feeding mechanism. The dynamometer is installed between the slider of the antique sword feeding mechanism and the antique sword clamping device. The high-speed camera is installed at the end of the material height adjustment device and is perpendicular to the cutting surface. The dynamometer and the high-speed camera signals are connected to a computer. The feeding mechanism, the laser tool setting device, the dynamometer and the high-speed camera are independently powered.

5. The sharpness testing device of an antique sword according to claim 4, characterized in that: The antique sword feeding mechanism is realized by controlling the screw transmission by a stepping motor, the dynamometer mounting seat is fixed to the slider of the screw, the antique sword clamping device is connected to the dynamometer mounting seat through a guide column, and the antique sword is manually adjusted and connected to the antique sword clamping device.

6. The sharpness testing device of an antique sword according to claim 4, characterized in that: The material height adjustment device is realized by driving a stepper motor control rod. The moving blocks of the material fixing device and the control rod are fixed by bolts on both sides. The cut material is placed on the material fixing device symmetrically along the center line of the material height adjustment device. The material pressing sheet is placed on the cut material and fixedly connected to the material fixing device by bolts.

7. The sharpness testing device for an antique sword as claimed in claim 4, characterized in that: The slider and the clamping device of the antique sword feeding mechanism make linear motion together, the slider movement range is 100-300 mm, the movement accuracy is not more than 0.02 mm, and the movement speed is not more than 10 mm per minute.

8. The sharpness testing device for an antique sword as claimed in claim 4, characterized in that: The moving block of the material height adjustment device moves linearly together with the material fixing device, and the movement accuracy of the moving block is no more than 0.05 mm.